High-temperature-resistant lithium battery film with overvoltage protection
By introducing ventilation holes and pressure relief films into the lithium battery film, the overvoltage problem caused by overheating of the lithium battery is solved, preventing explosions, and the service life of the film is improved through the wear-resistant and anti-static layer, achieving the safety and stability of the lithium battery. run.
Patent Information
- Application Number
- CN202410789538.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-19
- Publication Date
- 2024-10-18
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing lithium battery films can easily cause overvoltage when lithium battery components overheat, which may cause explosion or damage, and lack an effective overvoltage protection mechanism.
A high-temperature resistant lithium battery film with overvoltage protection is designed, including a wear-resistant layer, an anti-static layer and a high-temperature resistant layer. The main body of the film is provided with ventilation holes and a pressure relief film. The pressure relief film is made of polyethylene material. A pressure relief film is fixed on the inner wall of the pore to ensure that gas can be discharged through the pressure relief film when the lithium battery overheats to prevent explosion.
It effectively prevents lithium batteries from exploding or being damaged due to overvoltage, prolongs the service life of the film, improves the wear resistance and anti-static effect of the film through the wear-resistant layer and anti-static layer, and ensures the safe and stable operation of lithium batteries.
Smart Images

Figure CN118789905A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium battery film production, in particular to a high temperature resistant lithium battery film with overvoltage protection. Background Art
[0002] With the development of science and technology, lithium batteries have become mainstream, and the preparation of lithium batteries has received more and more attention. Lithium batteries are primary batteries that use lithium metal or lithium alloy as negative electrode materials and non-aqueous electrolyte solutions. They are different from rechargeable lithium-ion batteries and lithium-ion polymer batteries. The inventor of lithium batteries is Edison. Due to the very active chemical properties of lithium metal, the processing, storage and use of lithium metal have very high environmental requirements. Therefore, lithium batteries have not been used for a long time. With the development of microelectronics technology at the end of the 20th century, miniaturized devices have increased day by day, which puts high demands on power sources. Lithium batteries have entered a large-scale practical stage.
[0003] In the structure of lithium batteries, the diaphragm is one of the key internal components. It is located between the positive and negative electrodes. Its main function is to separate the positive and negative active materials to prevent the two electrodes from short-circuiting due to contact. In addition, during the electrochemical reaction, it can maintain the necessary electrolyte and form a channel for ion movement. High-quality diaphragms can improve the overall performance of batteries.
[0004] When the existing lithium battery film is wrapped on a lithium battery component, when the heat dissipated from the lithium battery component is too high, excessive pressure gas will be generated. Since the lithium battery component is wrapped by the film, the pressure on the lithium battery component cannot be released, which can easily cause the lithium battery to explode. In view of this, a high-temperature resistant lithium battery film with overpressure protection is proposed. Summary of the invention
[0005] The object of the present invention is to provide a high temperature resistant lithium battery film with overvoltage protection to solve the problems raised in the above background technology.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a high-temperature resistant lithium battery film with overpressure protection, comprising a film body, wherein the film body comprises a wear-resistant layer, and the wear-resistant layer can achieve a good wear-resistant effect and extend the service life of the film body, an antistatic layer and a high-temperature resistant layer, wherein the wear-resistant layer is arranged on the outermost layer, the high-temperature resistant layer is arranged on the innermost side, and the antistatic layer is arranged between the wear-resistant layer and the high-temperature resistant layer. Vents are provided on the film body, and exhaust can be carried out by setting the vents. A pressure relief membrane is fixed on the inner wall of the vent. By setting the vents, when the lithium battery is overheated and generates excessive pressure gas, the pressure relief membrane is easy to tear because the thickness of the pressure relief membrane is thinner than that of the film body, and the pressure relief membrane is made of polyethylene material, so that the pressure relief membrane is easy to tear, and the pressure gas will first break through the pressure relief membrane, and then pass through the vents, thereby releasing pressure on the lithium battery and preventing the lithium battery from exploding or being damaged.
[0007] Preferably, the ventilation holes are provided in a plurality of groups, and the plurality of ventilation holes are opened on the film body at equal distances.
[0008] Preferably, the pressure relief membranes are provided in a plurality of groups, and the plurality of groups of pressure relief membranes are arranged at equal distances on the film body.
[0009] Preferably, the wear-resistant layer is made of butadiene rubber, and the diameter thickness of the wear-resistant layer is 15 to 20 μm. By setting the wear-resistant layer, the film body can have good wear resistance, which can increase the service life of the film body and prevent the film body from being damaged and affecting the use of the lithium battery body. By setting the friction convex ball, the film body will not be directly touched and rubbed, thereby increasing the service life of the film body.
[0010] Preferably, the antistatic layer is made of polyimide, and the diameter thickness of the antistatic layer is 13-15 μm. By using polyimide as the main material of the antistatic layer, a good antistatic effect can be achieved, and static electricity generated by friction on the surface of the film body can be reduced.
[0011] Preferably, the high temperature resistant layer is made of polyetheretherketone, epoxy resin and PET plastic, and the diameter thickness of the high temperature resistant layer is 18 to 20 μm. Polyetheretherketone is a polymer composed of repeating units containing one ketone bond and two ether bonds in the main chain structure. It is a special polymer material with good high temperature resistance.
[0012] Preferably, the pressure relief membrane is made of polyethylene material, and the diameter thickness of the pressure relief membrane is 2-4 μm.
[0013] Preferably, the outer wall of the wear-resistant layer is fixed with multiple groups of friction convex balls at equal distances, and the friction convex balls are made of butadiene rubber. By arranging the friction convex balls, the film body will not be directly touched and rubbed, thereby increasing the service life of the film body.
[0014] Preferably, the film body is made by the following process:
[0015] S1. Weigh the following raw materials in parts by weight: 10-20 parts of butadiene rubber, 10-20 parts of polyimide, 10-20 parts of polyetheretherketone, 50-100 parts of epoxy resin, 10-15 parts of polyethylene and 80-150 parts of PET plastic;
[0016] S2, through the screening machine, the above device is cleaned, the impurities contained in the raw materials are removed, and then the epoxy resin and PET plastic are sliced;
[0017] S3, pre-crystallizing and drying the slices of PET plastic and epoxy resin, the temperature of pre-crystallizing and drying the PET plastic and epoxy resin is controlled at 120-150°C, the drying time is 2-3 hours, and the moisture content of the PET plastic after drying is required to be controlled below 45ppm. The pre-crystallization and drying treatment can increase the softening point of the polymer and prevent the resin particles from sticking to each other and agglomerating during the drying and melt extrusion process; at the same time, the epoxy resin raw material is dehydrated to prevent the ester-containing polymer from being hydrolyzed and degraded and generating bubbles during the melt extrusion process;
[0018] S4. After the PET plastic and epoxy resin are dried, polyimide, polyetheretherketone, butadiene rubber, epoxy resin, polyethylene and PET plastic are added into the reactor, the temperature is set to 80°C, the speed is set to 600r / min, and the stirring is performed for 3-4h to fully mix the raw materials and mix the raw materials evenly;
[0019] S5. Let the mixed raw materials stand for 24 hours, and then pour the raw materials into a twin-screw extruder. The twin-screw extruder is driven by a motor and is divided into a feeding section, a compression section and a metering section according to its efficiency. The raw materials are first compressed in the feeding section, and then enter the compression section to melt using the shear heat generated by the melt film on the inner wall of the equipment, and then heated and melted for plasticization. Subsequently, the metering section breaks the raw materials that are not completely melted into fine particles and completely melts them in the subsequent flow. The heating and melting temperature is 200°C-225°C. After the melting is completed, the raw materials are transferred to the insulation equipment for insulation treatment, and the insulation time is set to 30min-45min; the raw materials obtained after melting are passed through a metering pump and a filtering device and then enter the die head, extruded and plasticized, and blown to obtain a high-temperature resistant lithium battery film with overpressure protection, wherein during the granulation process, the temperature of the low temperature zone is 90-100°C, the temperature of the high temperature zone is 130-140°C, and the speed of the twin-screw extruder is 30r / min;
[0020] S6. A thick sheet is obtained by heating and melt extrusion through a twin-screw extruder, and the thick sheet is stretched longitudinally and transversely by a certain multiple in an appropriate temperature range above the glass transition temperature and below the melting point through a longitudinal stretching machine and a transverse stretching machine under the action of external force. The film obtained after stretching is passed into a film correcting machine, and the film correcting machine is controlled to cut and correct the film, and then rolled onto a reel to complete the film production process.
[0021] Compared with the prior art, the present invention provides a high temperature resistant lithium battery film with overvoltage protection, which has the following beneficial effects:
[0022] 1. The high-temperature resistant lithium battery film with overpressure protection is provided with vents. When the lithium battery is overheated and generates excessive pressure gas, the thickness of the pressure relief film is thinner than the thickness of the film body, and the pressure relief film is made of polyethylene material, so the pressure relief film is easy to tear, and the pressure gas will first break through the pressure relief film and then pass through the vents, thereby relieving the pressure on the lithium battery and preventing the lithium battery from exploding or being damaged.
[0023] 2. The high-temperature resistant lithium battery film with overpressure protection can provide a wear-resistant layer to make the film body have good wear resistance, thereby increasing the service life of the film body and preventing the film body from being damaged and affecting the use of the lithium battery body. In addition, by providing friction convex balls, the film body will not be directly touched and rubbed, thereby increasing the service life of the film body.
[0024] 3. The high-temperature resistant lithium battery film with overvoltage protection adopts polyimide as the main material of the anti-static layer, which can achieve good anti-static effect and reduce static electricity generated by friction on the surface of the film body. The high-temperature resistant layer is made of polyetheretherketone raw material. Polyetheretherketone is a polymer composed of repeating units containing one ketone bond and two ether bonds in the main chain structure. It is a special polymer material with good high-temperature resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a structural schematic diagram of the present invention as a whole;
[0026] Figure 2 It is a schematic diagram of the overall internal structure of the present invention;
[0027] Figure 3 For the present invention Figure 2 A magnified schematic diagram of the A structure.
[0028] In the figure: 1. film body; 11. wear-resistant layer; 12. antistatic layer; 13. high temperature resistant layer; 2. vent hole; 3. pressure relief membrane; 4. friction convex ball. DETAILED DESCRIPTION
[0029] like Figure 1-Figure 3As shown, the present invention provides a technical solution: a high temperature resistant lithium battery film with overvoltage protection, including a film body 1, the film body 1 includes a wear-resistant layer 11, an antistatic layer 12 and a high temperature resistant layer 13, the wear-resistant layer 11 is arranged on the outermost layer, and the wear-resistant layer 11 is made of butadiene rubber, which is a synthetic rubber with a regular structure formed by the polymerization of butadiene, and its cis structure content is more than 95%. According to different catalysts, it can be divided into nickel-based, cobalt-based, titanium-based and rare earth-based butadiene rubbers. Butadiene rubber has good wear resistance and cold resistance. By setting the wear-resistant layer 11, the film body 1 can have good wear resistance, which can improve the service life of the film body 1, prevent the film body 1 from being damaged, causing damage to the lithium battery body, and affect the use of the lithium battery body. The diameter thickness of the wear-resistant layer 11 is 15 to 20 μm, and the high temperature resistant layer 13 is arranged on the innermost side. The high temperature resistant layer 13 is made of polyetheretherketone, epoxy resin and PET plastic. Polyetheretherketone is a polymer composed of repeating units containing one ketone bond and two ether bonds in the main chain structure. It is a special polymer material with good high temperature resistance. The diameter and thickness of the high temperature resistant layer 13 are 18-20 μm. The antistatic layer 12 is arranged between the wear-resistant layer 11 and the high temperature resistant layer 13. The antistatic layer 12 is made of polyimide. By using polyimide as the main material of the antistatic layer 12, a good antistatic effect can be achieved, which can reduce the static electricity generated by friction on the surface of the film body. The diameter of the antistatic layer 12 is 18-20 μm. The thickness is 13-15 μm. A vent hole 2 is provided on the film body 1. The vent holes 2 are provided in multiple groups. The multiple groups of vent holes 2 are provided in the film body 1 at equal distances. A pressure relief membrane 3 is fixed on the inner wall of the vent hole 2. The pressure relief membrane 3 is provided in multiple groups. By providing the vent holes 2, when the lithium battery is overheated and generates excessive pressure gas, the pressure relief membrane 3 is thinner than the thickness of the film body 1, and the pressure relief membrane 3 is made of polyethylene material, so that the pressure relief membrane 3 is easy to tear, and the pressure gas will first break through the pressure relief membrane 3 and then pass through the vent holes 2. , and then the lithium battery can be depressurized to prevent the lithium battery from exploding or being damaged, and multiple groups of pressure relief membranes 3 are equidistantly arranged on the film body 1, the pressure relief membrane 3 is made of polyethylene material, and the diameter thickness of the pressure relief membrane 3 is 2 to 4 μm, and the outer wall of the wear-resistant layer 11 is fixed with multiple groups of friction convex balls 4 at equal distances, and the material of the friction convex balls 4 is also made of butadiene rubber, so that the friction convex balls 4 have good wear resistance, and by setting the friction convex balls 4, the film body 1 will not be directly touched and rubbed, thereby improving the service life of the film body 1.
[0030] The film body 1 is made by the following process:
[0031] S1. Weigh the following raw materials in parts by weight: 10-20 parts of butadiene rubber, 10-20 parts of polyimide, 10-20 parts of polyetheretherketone, 50-100 parts of epoxy resin, 10-15 parts of polyethylene and 80-150 parts of PET plastic;
[0032] S2, through the screening machine, the above device is cleaned, the impurities contained in the raw materials are removed, and then the epoxy resin and PET plastic are sliced;
[0033] S3, pre-crystallizing and drying the slices of PET plastic and epoxy resin, the temperature of pre-crystallizing and drying the PET plastic and epoxy resin is controlled at 120-150°C, the drying time is 2-3 hours, and the moisture content of the PET plastic after drying is required to be controlled below 45ppm. The pre-crystallization and drying treatment can increase the softening point of the polymer and prevent the resin particles from sticking to each other and agglomerating during the drying and melt extrusion process; at the same time, the epoxy resin raw material is dehydrated to prevent the ester-containing polymer from being hydrolyzed and degraded and generating bubbles during the melt extrusion process;
[0034] S4. After the PET plastic and epoxy resin are dried, add polyimide, polyetheretherketone, butadiene rubber, epoxy resin, polyethylene and PET plastic into the reactor, set the temperature to 80°C, the speed to 600r / min, stir and mix for 3-4h, fully mix the raw materials, mix the raw materials evenly, and through mixing and stirring, the quality of the film produced can be better;
[0035] S5. Let the mixed raw materials stand for 24 hours, and then pour the raw materials into a twin-screw extruder. The twin-screw extruder is driven by a motor and is divided into a feeding section, a compression section and a metering section according to its efficiency. The raw materials are first compressed in the feeding section, and then enter the compression section to melt using the shear heat generated by the melt film on the inner wall of the equipment, and then heated and melted for plasticization. Subsequently, the metering section breaks the raw materials that are not completely melted into fine particles and completely melts them in the subsequent flow. The heating and melting temperature is 200°C-225°C. After the melting is completed, the raw materials are transferred to the insulation equipment for insulation treatment, and the insulation time is set to 30min-45min; the raw materials obtained after melting are passed through a metering pump and a filtering device and then enter the die head, extruded and plasticized, and blown to obtain a high-temperature resistant lithium battery film with overpressure protection, wherein during the granulation process, the temperature of the low temperature zone is 90-100°C, the temperature of the high temperature zone is 130-140°C, and the speed of the twin-screw extruder is 30r / min;
[0036] S6. Extrusion is performed through a twin-screw extruder. The die head extrude the raw material onto the surface of the chill roller. The surface temperature of the chill roller is controlled at 18.5-20.5°C. The softened water with a relatively low temperature circulates at a high speed in the chill roller to exchange heat with the chill roller. After the chill roller maintains a relatively low temperature, the molten raw material falls onto the surface of the chill roller and is quickly cooled and formed. When the melt is cast, a strip electrode is installed above the melt, and a DC voltage of 7.5KV-9KV is passed through the strip electrode, so that the high voltage ionizes the air to generate positive and negative ions. Because the quench roller is connected to the ground through the equipment, a large number of ions will flow toward the quench roller. While the ions are flowing, the raw material melt is firmly attached to the surface of the quench roller; thus, the thick sheet is completed, and the thick sheet is stretched a certain multiple in the longitudinal and transverse directions in the appropriate temperature range above the glass transition temperature and below the melting point through a longitudinal stretching machine and a transverse stretching machine under the action of external force. The film obtained after stretching is passed into a film correction machine, which controls the film correction machine to cut and correct the film and then roll it on a reel to complete the film production process.
[0037] As an application of this embodiment:
[0038] When the temperature of the lithium battery components is too high, the lithium battery will generate excessive pressure gas. Since the thickness of the pressure relief membrane 3 is much smaller than the thickness of the film body 1, the gas pressure will break the pressure relief membrane 3, and the gas pressure will be discharged from the vent 2, thereby achieving the effect of pressure relief, releasing the gas pressure on the lithium battery body, and preventing the lithium battery components from being wrapped by the film body 1, so that the gas pressure on the lithium battery cannot be released, which may cause the lithium battery to explode or be damaged.
[0039] The above generally describes the present invention in detail, but it is obvious to a person skilled in the art that some modifications or improvements can be made to the present invention. Therefore, modifications or improvements that do not depart from the spirit of the present invention are within the scope of protection of the present invention.
Claims
1. A high temperature resistant lithium battery film with overvoltage protection, comprising a film body (1), characterized in that: The film body (1) comprises a wear-resistant layer (11), an antistatic layer (12) and a high temperature resistant layer (13); the wear-resistant layer (11) is arranged on the outermost layer, the high temperature resistant layer (13) is arranged on the innermost layer, and the antistatic layer (12) is arranged between the wear-resistant layer (11) and the high temperature resistant layer (13); a vent hole (2) is opened on the film body (1), and a pressure relief membrane (3) is fixed to the inner wall of the vent hole (2).
2. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The ventilation holes (2) are provided in a plurality of groups, and the plurality of ventilation holes (2) are arranged at equal distances on the film body (1).
3. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The pressure relief membranes (3) are arranged in multiple groups, and the multiple groups of pressure relief membranes (3) are arranged at equal distances on the film body (1).
4. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The wear-resistant layer (11) is made of butadiene rubber, and the diameter thickness of the wear-resistant layer (11) is 15 to 20 μm.
5. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The antistatic layer (12) is made of polyimide, and the diameter and thickness of the antistatic layer (12) are 13 to 15 μm.
6. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The high temperature resistant layer (13) is made of polyetheretherketone, epoxy resin and PET plastic, and the diameter and thickness of the high temperature resistant layer (13) are 18 to 20 μm.
7. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The pressure relief membrane (3) is made of polyethylene material, and the diameter thickness of the pressure relief membrane (3) is 2 to 4 μm.
8. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The outer wall of the wear-resistant layer (11) is fixed with a plurality of groups of friction convex balls (4) at equal distances.
9. The high temperature resistant lithium battery film with overvoltage protection according to claim 1, characterized in that: The film body (1) is made by the following process: S1. Weigh the following raw materials in parts by weight: 10-20 parts of butadiene rubber, 10-20 parts of polyimide, 10-20 parts of polyetheretherketone, 50-100 parts of epoxy resin, 10-15 parts of polyethylene and 80-150 parts of PET plastic; S2, through the screening machine, the above device is cleaned, the impurities contained in the raw materials are removed, and then the epoxy resin and PET plastic are sliced; S3, pre-crystallizing and drying the slices of PET plastic and epoxy resin, the temperature of pre-crystallizing and drying the PET plastic and epoxy resin is controlled at 120-150°C, the drying time is 2-3 hours, and the moisture content of the PET plastic after drying is required to be controlled below 45ppm. The pre-crystallization and drying treatment can increase the softening point of the polymer and prevent the resin particles from sticking to each other and agglomerating during the drying and melt extrusion process; at the same time, the epoxy resin raw material is dehydrated to prevent the ester-containing polymer from being hydrolyzed and degraded and generating bubbles during the melt extrusion process; S4. After the PET plastic and epoxy resin are dried, polyimide, polyetheretherketone, butadiene rubber, epoxy resin, polyethylene and PET plastic are added into the reactor, the temperature is set to 80°C, the speed is set to 600r / min, and the stirring is performed for 3-4h to fully mix the raw materials and mix the raw materials evenly; S5. Let the mixed raw materials stand for 24 hours, and then pour the raw materials into a twin-screw extruder. The twin-screw extruder is driven by a motor and is divided into a feeding section, a compression section and a metering section according to its efficiency. The raw materials are first compressed in the feeding section and then enter the compression section to be melted by the shear heat generated by the melt film on the inner wall of the equipment, and then heated and melted for plasticization. Subsequently, the metering section breaks the raw materials that are not completely melted into fine particles and completely melts them in the subsequent flow. The heating and melting temperature is 200℃-225℃. After the melting is completed, it is transferred to the insulation equipment for insulation treatment, and the insulation time is set to 30min-45min; the raw materials obtained after melting pass through a metering pump and a filtering device and enter the die head, extruded and plasticized, and blown to obtain a high-temperature resistant lithium battery film with overpressure protection. During the granulation process, the temperature in the low-temperature zone is 90-100℃, the temperature in the high-temperature zone is 130-140℃, and the speed of the twin-screw extruder is 30r / min. S6. A thick sheet is obtained by heating and melt extrusion through a twin-screw extruder, and the thick sheet is stretched longitudinally and transversely by a certain multiple in an appropriate temperature range above the glass transition temperature and below the melting point through a longitudinal stretching machine and a transverse stretching machine under the action of external force. The film obtained after stretching is passed into a film correcting machine, and the film correcting machine is controlled to cut and correct the film, and then rolled onto a reel to complete the film production process.