Preparation method of 3DMEMS probe and probe
By etching sharp grooves and forming a sharp head in the MEMS probe card, combined with the design of the beam part and copper pillars, the problem of the chip being crushed by the probe card and the signal transmission problem are solved, and three-dimensional contact and elasticity are achieved. Rebound ensures the normal transmission of detection signals and the safety of the chip.
Patent Information
- Application Number
- CN202410898410.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-10-18
AI Technical Summary
The probes of existing MEMS probe cards are cylindrical or sheet-shaped, which causes the contact force between the probe and the chip to increase, easily crushing the chip, and due to point-to-point or face-to-face two-dimensional contact, it is difficult to transmit detection signals normally, especially in the presence of an oxide layer.
By etching sharp grooves in the first pattern area of the silicon wafer, sputtering the seed layer and performing electroplating to form the pointed portion, combined with the electroplating in the second pattern area to form the beam portion, and using a wire bonding process A copper pillar is bonded to the end of the beam far away from the tip to form a 3DMEMS probe, which achieves three-dimensional contact with the tip piercing the oxide layer, and increases the distance between the chip and the target PCB board through the copper pillar to avoid structural interference.
The pointed head can penetrate the oxide layer of the chip pin to ensure the normal transmission of the detection signal, and avoid crushing the chip through elastic rebound, ensuring accurate detection of chip performance.
Smart Images

Figure CN118795188A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of probe cards, and in particular to a 3D MEMS probe preparation method and a 3D MEMS probe. Background Art
[0002] MEMS probe cards are key components in the IC chip packaging and testing process and are used for testing IC products before packaging. With the development of semiconductor manufacturing technology, the complexity of IC chips continues to increase, and this type of probe card can improve the efficiency of one-time testing.
[0003] However, the shape of the probe of the MEMS probe card used for chip testing in the prior art is generally a columnar structure or a sheet structure. When the probe moves down and contacts the pin of the chip, on the one hand, the contact force between the probe and the chip increases, which can easily damage the chip; on the other hand, the contact between the bottom surface of the probe and the pin of the chip is a point-to-point or face-to-face two-dimensional contact, and when there is an oxide layer on the pin, the detection signal cannot be transmitted normally.
[0004] Therefore, it is urgent to provide a 3D MEMS probe preparation method and a 3D MEMS probe to solve the above problems. Summary of the invention
[0005] The purpose of the present invention is to provide a 3DMEMS probe preparation method and a 3DMEMS probe, which not only enables the 3DMEMS probe to pierce the oxide layer of the chip pin to achieve three-dimensional contact and ensure the normal transmission of the detection signal, but also enables the 3DMEMS probe to elastically rebound to avoid crushing the chip.
[0006] In order to achieve the above objectives, the following technical solutions are provided:
[0007] A 3DMEMS probe preparation method comprises the following steps:
[0008] S1, etching a groove with a sharp point in a first pattern area of a silicon wafer;
[0009] S2, sputtering a seed layer on the surface of the silicon wafer and the inner wall surface of the groove;
[0010] S3, performing electroplating on the first pattern area of the silicon wafer, so that the groove is fully plated with metal and a pointed portion is formed;
[0011] S4, performing electroplating on the second pattern area of the silicon wafer to form a beam portion in the second pattern area;
[0012] S5. Bond a copper pillar on the end of the beam portion away from the pointed portion using a wire bonding process.
[0013] As an optional solution of the 3DMEMS probe preparation method, the 3DMEMS probe preparation method further includes the following steps:
[0014] S6, coating a fourth photoresist of a set thickness on the silicon wafer, and grinding and flattening the silicon wafer to make the copper column reach a target length.
[0015] As an optional solution of the 3DMEMS probe preparation method, the 3DMEMS probe preparation method further includes the following steps:
[0016] S7, welding the target PCB board to an end of the copper column away from the beam portion;
[0017] S8. Remove the silicon wafer, the seed layer and the fourth photoresist in sequence.
[0018] As an optional solution of the 3DMEMS probe preparation method, in step S1:
[0019] A first photoresist is coated on the silicon wafer, and the first pattern area is exposed after exposure and development steps.
[0020] As an optional solution of the 3DMEMS probe preparation method, in step S1:
[0021] The groove is obtained by wet etching in the first pattern area, and then the first photoresist is removed.
[0022] As an optional solution of the 3DMEMS probe preparation method, in step S2:
[0023] The seed layer is formed by a magnetron sputtering process.
[0024] As an optional solution of the 3DMEMS probe preparation method, in step S3:
[0025] A second photoresist is coated on the silicon wafer, and the first pattern area is exposed through exposure and development. After electroplating is completed, the second photoresist is removed.
[0026] As an optional solution of the 3DMEMS probe preparation method, in step S4:
[0027] A third photoresist is coated on the silicon wafer, and the second pattern area is exposed through exposure and development. After electroplating is completed, the third photoresist is removed.
[0028] As an optional solution of the 3D MEMS probe preparation method, the pointed portion is a pyramid structure, and the crossbeam portion of the probe is a straight line, a curve or a bending structure.
[0029] A 3D MEMS probe is manufactured using the 3D MEMS probe manufacturing method as described above, wherein the 3D MEMS probe comprises a pointed portion, a beam portion and a copper column, wherein the pointed portion is arranged at one end of the beam portion, and the copper column is arranged at the other end of the beam portion.
[0030] Compared with the prior art, the present invention has the following beneficial effects:
[0031] The 3DMEMS probe preparation method provided by the present invention comprises the following steps: etching a groove with a sharp point in the first pattern area of a silicon wafer, forming a sharp head capable of piercing an oxide layer in the groove, sputtering a seed layer on the surface of the silicon wafer and the inner wall of the groove, wherein the seed layer is conductive and convenient for the electroplating process in the subsequent steps, electroplating is performed in the first pattern area of the silicon wafer, so that the groove is fully plated with metal and a sharp head is formed, electroplating is performed in the second pattern area of the silicon wafer, so that a crossbeam is formed in the second pattern area, and the crossbeam can produce elastic deformation after being subjected to force, and a copper column is bonded on one end of the crossbeam away from the sharp head by a wire bonding process, and the copper column is used to connect a target PCB board. Since the copper column is additionally provided, the spacing between the chip and the target PCB board can be increased, and structural interference with the target PCB board after the crossbeam is deformed can be avoided. The sharp head can pierce the oxide layer of the chip pin to achieve three-dimensional contact, ensure the normal transmission of the detection signal, and the 3DMEMS probe can elastically rebound to avoid crushing the chip.
[0032] The 3D MEMS probe provided by the present invention can achieve three-dimensional contact to ensure normal transmission of detection signals, and can elastically rebound to avoid crushing the chip, thereby ensuring accurate detection of chip performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.
[0034] Figure 1 Flow chart of a method for preparing a 3DMEMS probe in an embodiment of the present invention;
[0035] Figure 2 This is a flow chart of step S1 in an embodiment of the present invention;
[0036] Figure 3 This is a schematic diagram of a process in which a seed layer is provided on a silicon wafer in an embodiment of the present invention;
[0037] Figure 4 Schematic diagram of the process of step S3 in an embodiment of the present invention;
[0038] Figure 5 Schematic diagram of the process of step S4 in an embodiment of the present invention;
[0039] Figure 6 It is a schematic diagram of the structure of the copper pillar bonded to the beam portion in an embodiment of the present invention;
[0040] Figure 7 Schematic diagram of the process of step S6 in an embodiment of the present invention;
[0041] Figure 8 Schematic diagram of the process of step S7 and step S8 in the embodiment of the present invention;
[0042] Fig. 9 This is a schematic diagram of the structure of the first 3DMEMS probe in an embodiment of the present invention;
[0043] Fig.10 This is a schematic diagram of the structure of a second 3DMEMS probe in an embodiment of the present invention;
[0044] Fig.11 Schematic diagram of the structure of the third 3DMEMS probe in an embodiment of the present invention.
[0045] Reference numerals:
[0046] 100, 3DMEMS probe; 101, pointed part; 102, beam part; 103, copper pillar;
[0047] 1. Silicon wafer; 11. Groove; 2. First photoresist; 3. First pattern area; 4. Seed layer; 5. Second photoresist; 6. Third photoresist; 7. Second pattern area; 8. Fourth photoresist; 9. Target PCB board. DETAILED DESCRIPTION
[0048] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0049] In the description of the present invention, it should be noted that the terms "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or are the positions or positional relationships in which the inventive product is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance. In the description of the present invention, unless otherwise specified, "multiple" means two or more.
[0050] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "disposed" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0051] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0052] In order to enable the 3D MEMS probe to penetrate the oxide layer of the chip pin to achieve three-dimensional contact, ensure the normal transmission of the detection signal, and enable the 3D MEMS probe to elastically rebound to avoid crushing the chip, this embodiment provides a 3D MEMS probe preparation method and a 3D MEMS probe. Figures 1 to 11 The specific contents of this embodiment are described in detail.
[0053] like Figures 1 to 6 The 3DMEMS probe preparation method in this embodiment includes the following steps: S1, etching a groove 11 with a sharp point in the first pattern area 3 of the silicon wafer 1; S2, sputtering a seed layer 4 on the surface of the silicon wafer 1 and the inner wall of the groove 11; S3, electroplating the first pattern area 3 of the silicon wafer 1, so that the groove 11 is fully plated with metal and a sharp head 101 is formed; S4, electroplating is performed on the second pattern area 7 of the silicon wafer 1, so that the second pattern area 7 forms a beam part 102; S5, bonding a copper column 103 to one end of the beam part 102 away from the sharp head 101 by a wire bonding process. Exemplarily, the diameter of the copper column 103 is 50um-200um, the height is 4mm-8mm, and the angle between the copper column 103 and the horizontal plane is controlled to be 89 degrees-90 degrees.
[0054] In short, the 3D MEMS probe preparation method provided by the present invention etches a groove 11 with a sharp point in the first pattern area 3 of the silicon wafer 1, and the groove 11 is used to form a sharp head 101 that can pierce the oxide layer. The seed layer 4 is sputtered on the surface of the silicon wafer 1 and the inner wall of the groove 11. The seed layer 4 is conductive and convenient for the electroplating process in the subsequent steps. The first pattern area 3 of the silicon wafer 1 is electroplated to make the groove 11 full of metal and form the sharp head 101. The second pattern area 7 of the silicon wafer 1 is electroplated to form a beam part 102 in the second pattern area 7. The beam part 102 can produce elastic deformation after being subjected to force. A copper column 103 is bonded to one end of the beam part 102 away from the sharp head 101 by a wire bonding process. The copper column 103 is used to connect the target PCB board 9. Since the copper column 103 is added, the distance between the chip and the target PCB board 9 can be increased to avoid structural interference between the beam part 102 and the target PCB board 9 after deformation. The pointed portion 101 can penetrate the oxide layer of the chip pin to achieve three-dimensional contact, thereby ensuring normal transmission of the detection signal. In addition, the 3D MEMS probe 100 can elastically rebound to avoid crushing the chip.
[0055] Furthermore, if Figure 7 As shown, the 3DMEMS probe preparation method also includes the following steps: S6, coating a fourth photoresist 8 of a set thickness on the silicon wafer 1, grinding and flattening the upper surface of the entire (including the fourth photoresist 8 and the copper pillar 103) to make the copper pillar 103 to a target length. Before grinding the copper pillar 103, the fourth photoresist 8 needs to be applied, and the fourth photoresist 8 wraps the copper pillar 103 to prevent the copper pillar 103 from swinging during the grinding process.
[0056] Furthermore, if Figure 8 As shown, the 3DMEMS probe preparation method also includes the following steps: S7, welding the target PCB board 9 to the end of the copper column 103 away from the beam portion 102; S8, sequentially removing the silicon wafer 1, the seed layer 4 and the fourth photoresist 8 to obtain a probe card. The target PCB board 9 in this embodiment has a circuit for detecting chip performance. Potassium hydroxide solution or BOE (buffered oxide etchant) solution is used to completely remove the silicon wafer 1, and the metal of the seed layer 4 is wet-etched. It can be understood that in other implementations, the seed layer 4 can also be called a metal conductive layer.
[0057] For example, Figure 1 Combination Figure 2 As shown, in step S1: a first photoresist 2 is coated on the entire surface of a silicon wafer 1, and after exposure and development steps, a first pattern area 3 is exposed. In this embodiment, the first pattern area 3 is a square of 50um-150um.
[0058] For example, Figure 1 Combination Figure 2 As shown, in step S1: potassium hydroxide or other chemical agents are used to wet-etch the first pattern area 3 according to the crystal phase of the silicon wafer 1 to obtain a groove 11, and then the first photoresist 2 is removed by dry stripping or wet stripping. The groove 11 is pyramid-shaped and has a depth of 25um-75um.
[0059] Optionally, if Figures 1 to 3 As shown, in step S2: a magnetron sputtering process is used to form a seed layer 4. The seed layer 4 in this embodiment has a thickness of 200nm-500nm, covering the surface of the silicon wafer 1 and the inner surface of the pyramid-shaped groove 11.
[0060] For example, Figures 1 to 4 As shown, in step S3: the second photoresist 5 is coated on the entire surface of the silicon wafer 1, and the first pattern area 3 and the groove 11 are exposed by exposure and development, and the groove 11 is filled with metal. After the electroplating is completed, the second photoresist 5 is removed.
[0061] For example, Figures 1 to 5 As shown, in step S4: a third photoresist 6 is coated on the silicon wafer 1, and the second pattern area 7 is exposed by exposure and development, and the beam portion 102 is obtained after electroplating, and then the third photoresist 6 is removed. In this embodiment, the thickness of the beam portion 102 is 50um-200um in a side view. In a top view, the width of the beam portion 102 is 50um-150um.
[0062] It should be noted that the pointed portion 101 and the cross beam portion 102 in this embodiment are both made of metal.
[0063] For example, Figures 9 to 11 As shown, the pointed part 101 is a pyramid structure, and the cross beam part 102 of the probe is a straight line, a curve or a bend structure. The various designs of the cross beam part 102 meet the design requirements of various spaces, and the unique contact tip design has a better piercing effect.
[0064] This embodiment also provides a 3DMEMS probe 100, which is made by the above-mentioned 3DMEMS probe preparation method, and includes a pointed portion 101, a beam portion 102, and a copper column 103, wherein the pointed portion 101 is disposed at one end of the beam portion 102, and the copper column 103 is disposed at the other end of the beam portion 102. The 3DMEMS probe 100 can penetrate the oxide layer of the chip pin to achieve three-dimensional contact, thereby ensuring normal transmission of the detection signal, and the 3DMEMS probe 100 can elastically rebound to avoid crushing the chip.
[0065] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for preparing a 3DMEMS probe, characterized in that: The following steps are involved: S1, etching a groove (11) with a sharp point in a first pattern area (3) of a silicon wafer (1); S2, sputtering a seed layer (4) on the surface of the silicon wafer (1) and the inner wall surface of the groove (11); S3, performing electroplating on the first pattern area (3) of the silicon wafer (1) so that the groove (11) is fully plated with metal and a pointed portion (101) is formed; S4, performing electroplating on the second pattern area (7) of the silicon wafer (1), so that the second pattern area (7) forms a beam portion (102); S5. Bonding a copper pillar (103) to an end of the beam portion (102) away from the pointed portion (101) using a wire bonding process.
2. The method for preparing a 3D MEMS probe according to claim 1, characterized in that: The 3DMEMS probe preparation method further comprises the following steps: S6, coating a fourth photoresist (8) of a set thickness on the silicon wafer (1), and grinding and flattening the silicon wafer (1), so that the copper pillar (103) reaches a target length.
3. The method for preparing a 3D MEMS probe according to claim 2, characterized in that: The 3DMEMS probe preparation method further comprises the following steps: S7, welding the target PCB board (9) to an end of the copper column (103) away from the crossbeam portion (102); S8, removing the silicon wafer (1), the seed layer (4) and the fourth photoresist (8) in sequence.
4. The method for preparing a 3DMEMS probe according to claim 1, characterized in that: In step S1: A first photoresist (2) is coated on the silicon wafer (1), and the first pattern area (3) is exposed after exposure and development steps.
5. The method for preparing a 3DMEMS probe according to claim 4, characterized in that: In step S1: The groove (11) is obtained by wet etching in the first pattern area (3), and then the first photoresist (2) is removed.
6. The method for preparing a 3D MEMS probe according to claim 1, characterized in that: In step S2: The seed layer (4) is formed by a magnetron sputtering process.
7. The method for preparing a 3D MEMS probe according to claim 1, characterized in that: In step S3: A second photoresist (5) is coated on the silicon wafer (1), the first pattern area (3) is exposed through exposure and development, and after electroplating is completed, the second photoresist (5) is removed.
8. The method for preparing a 3D MEMS probe according to claim 1, characterized in that: In step S4: A third photoresist (6) is coated on the silicon wafer (1), and the second pattern area (7) is exposed through exposure and development. After electroplating is completed, the third photoresist (6) is removed.
9. The method for preparing a 3D MEMS probe according to claim 1, characterized in that: The pointed portion (101) is a pyramid structure, and the crossbeam portion (102) of the probe is a straight line, curved line or bent structure. 10.3DMEMS probe, characterized in that: The 3D MEMS probe is manufactured by the preparation method of any one of claims 1 to 9, wherein the 3D MEMS probe comprises a pointed portion (101), a beam portion (102) and a copper column (103), wherein the pointed portion (101) is arranged at one end of the beam portion (102), and the copper column (103) is arranged at the other end of the beam portion (102).
Citation Information
Patent Citations
Method for preparing silicon carbide (SiC) micro-nano needle tips
CN102642805A
3D-MEMS probe and preparation method thereof
CN116654863A
Micro coaxial radio frequency cantilever probe structure and application
CN117686753A