Cold core sand pretreatment boiling heating process and automatic batching and sand mixing method
By arranging heat exchange coils and hot air circulation devices in the boiler, combined with automated batching and sand mixing methods, the problems of poor uniformity and low batching efficiency during the heating process of cold core sand are solved, and efficient and uniform heating and mixing are achieved. Improved casting quality and production efficiency.
Patent Information
- Application Number
- CN202411042183.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-10-22
AI Technical Summary
The poor uniformity of the cold core sand during the heating process and the low efficiency of the sand mixing operation lead to problems such as low casting accuracy and strength, poor quality stability, long production cycle, and high sand mixing costs.
The cold core sand pretreatment boiling heating process is used. By setting up a heat exchange coil and a hot air circulation device in the boiler, the temperature and sand core image are monitored in real time, and the heating power is dynamically adjusted according to the boiling temperature, real-time temperature and thermal conductivity coefficient, combined with automation. The batching and sand mixing method accurately controls the batching amount and mixing time.
It achieves even distribution of heat in the boiler, improves the quality of core sand, reduces the scrap rate, shortens the production cycle, reduces energy consumption, and improves production efficiency and casting consistency.
Smart Images

Figure CN118808548A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of sand core processing technology, in particular to a cold core sand pretreatment boiling heating process and an automatic batching and sand mixing method. Background Art
[0002] Cold core sand is a material used in the casting process, mainly used to make the core of the casting. Its main function is to form complex cavities or channels inside the casting, and improve the precision and surface quality of the casting. Cold core sand has good strength and workability, can harden at room temperature, shorten the production cycle and reduce energy consumption, thereby improving production efficiency and economic benefits.
[0003] At present, the traditional cold core sand processing method shows several significant challenges, especially the unevenness of the heating process and the low efficiency of the batching and sand mixing operation. These problems directly affect the stability of the casting quality, resulting in frequent surface defects and internal structural problems of the casting. In addition, the uneven heating can easily cause local overheating or incomplete hardening of the core sand, further reducing the precision and strength of the casting. Inefficient batching and sand mixing operations not only increase labor and time costs, but are also prone to inaccurate batching and uneven mixing, affecting the consistency and reliability of castings. At the same time, these shortcomings also lead to an extension of the production cycle and an increase in energy consumption, which is not conducive to the economic benefits and environmental protection of the enterprise.
[0004] Therefore, it is urgent to invent a cold core sand processing process to solve the problems in the prior art of poor uniformity in the heating process of the cold core sand, low efficiency of the primary ingredient sand mixing operation, resulting in low casting precision and strength, poor stability of casting quality, long casting production cycle, and high sand mixing cost. Summary of the invention
[0005] In view of this, the present invention proposes a cold core sand pretreatment boiling heating process and an automated batching and sand mixing method, aiming to solve the problems in the current technology of poor uniformity in the cold core sand heating process and low efficiency of the first-level batching and sand mixing operation, resulting in low casting precision and strength, poor stability of casting quality and long casting production cycle, as well as high sand mixing cost.
[0006] The present invention proposes a cold core sand pretreatment boiling heating process, comprising:
[0007] A heat exchange coil and a hot air circulation device are arranged inside the boiler;
[0008] Acquiring the real-time temperature and sand core image inside the boiler, as well as the thermal conductivity coefficient of the sand core;
[0009] Obtaining the boiling temperature of the sand core, and determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core and the real-time temperature inside the boiler;
[0010] The heating power and heating power of the heat exchange coil and the hot air circulation device are obtained, and adjusted according to the sand core image and the thermal conductivity coefficient of the sand core material.
[0011] Further, when determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core, the real-time temperature inside the boiler and the thermal conductivity coefficient of the sand core material, it includes:
[0012] Obtain the temperature ratio between the boiling temperature of the sand core and the real-time temperature inside the boiler, and determine the heating power of the heat exchange coil and the hot air circulation device according to the relationship between the temperature ratio and the preset temperature ratio:
[0013] Wherein, a first preset temperature ratio and a second preset temperature ratio are preset, and the first preset temperature ratio is smaller than the second preset temperature ratio;
[0014] When the temperature ratio is greater than the second preset temperature ratio, it is determined that the heating power of the heat exchange coil is M3, and the heating power of the hot air circulation device is N3;
[0015] When the temperature ratio is less than or equal to the second preset temperature ratio, and the temperature ratio is greater than the first preset temperature ratio, it is determined that the heating power of the heat exchange coil is M2, and the heating power of the hot air circulation device is N2;
[0016] When the temperature ratio is less than the first preset temperature ratio, it is determined that the heating power of the heat exchange coil is M1, and the heating power of the hot air circulation device is N1;
[0017] Furthermore, 10%<M1<M2<M3<55%, and 10%<N1<N2<N3<55%.
[0018] Further, when determining the heating power of the heat exchange coil as Mi and the heating power of the hot air circulation device as Ni, i=1, 2, 3, and adjusting according to the sand core image and the thermal conductivity coefficient of the sand core material, it includes:
[0019] The thermal conductivity of the sand core material is obtained, and according to the relationship between the thermal conductivity and the preset thermal conductivity, it is determined whether to adjust the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device:
[0020] When the thermal conductivity is consistent with the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device are not adjusted;
[0021] When the thermal conductivity is greater than or less than the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device need to be adjusted, and the thermal conductivity ratio between the thermal conductivity and the preset thermal conductivity is obtained, and the adjustment coefficient when adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device is determined according to the thermal conductivity ratio.
[0022] Further, when determining the adjustment coefficient of the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device according to the thermal conductivity ratio, it includes:
[0023] Presetting a first preset thermal conductivity ratio and a second preset thermal conductivity ratio, wherein the first preset thermal conductivity ratio is smaller than the second preset thermal conductivity ratio;
[0024] The adjustment coefficient is determined according to the relationship between the thermal conductivity ratio and each preset thermal conductivity ratio, wherein:
[0025] When the thermal conductivity ratio is less than the first preset thermal conductivity ratio, the adjustment coefficient is determined to be L1;
[0026] When the thermal conductivity ratio is greater than or equal to the first preset thermal conductivity ratio, and the thermal conductivity ratio is less than the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L2;
[0027] When the thermal conductivity ratio is greater than or equal to the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L3;
[0028] Moreover, L1<L2<L3<1.
[0029] Further, when the adjustment coefficient Li of the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device is determined, i=1, 2, 3, it includes:
[0030] According to the sand core image inside the boiler, the real-time height of the sand core inside the boiler is obtained, and according to the relationship between the real-time height and the preset height, it is determined whether to correct the adjustment coefficient Li;
[0031] When the real-time altitude is less than or equal to the preset altitude, it is determined that the adjustment coefficient Li is not corrected;
[0032] When the real-time altitude is greater than the preset altitude, the altitude difference between the real-time altitude and the preset altitude is obtained, and the adjustment coefficient is determined as a correction coefficient for Li according to the altitude difference.
[0033] Further, when determining the adjustment coefficient as a correction coefficient for Li according to the height difference, it includes:
[0034] Presetting a first preset height difference value and a second preset height difference value, wherein the first preset height difference value is smaller than the second preset height difference value;
[0035] According to the relationship between the height difference value and each preset height difference value, the adjustment coefficient is determined to be a correction coefficient for correction by Li, wherein:
[0036] When the height difference is less than or equal to the first preset height difference, the correction coefficient is determined to be K1;
[0037] When the height difference is greater than the first preset height difference, and the height difference is less than or equal to the second preset height difference, the correction coefficient is determined to be K2;
[0038] When the height difference is greater than the second preset height difference, the correction coefficient is determined to be K3;
[0039] Moreover, K1<K2<K3<1.
[0040] Compared with the prior art, the beneficial effect of the present invention is that through the combined use of the heat exchange coil and the hot air circulation device, the heat can be evenly distributed inside the boiler, avoiding local overheating or insufficient heating, thereby improving the overall quality of the core sand. Secondly, by obtaining the temperature and sand core image inside the boiler in real time, as well as the thermal conductivity coefficient of the sand core, the heating process can be accurately controlled. This real-time monitoring and feedback mechanism allows the process parameters to be dynamically adjusted according to actual conditions, ensuring that each batch of sand cores can achieve the ideal heating effect. This precise control not only improves the quality stability of the sand core, but also reduces the scrap rate caused by uneven heating, thereby improving production efficiency. Then, based on the boiling temperature and real-time temperature of the sand core, determining the heating power of the heat exchange coil and the hot air circulation device is another key advantage of the process. Sand cores of different materials and shapes have different boiling temperatures and thermal conductivity coefficients. By accurately calculating and controlling the heating power, customized heating can be performed for different sand core materials to ensure that each sand core can reach the best hardening state. This flexibility and customized heating method enable the process to adapt to different casting needs and improve the adaptability and flexibility of production. Finally, by adjusting the heating power of the heat exchange coil and the hot air circulation device, combined with the sand core image and the thermal conductivity of the material, the uniformity and efficiency of heating can be further improved. Real-time image monitoring can intuitively reflect the state of the sand core during the heating process. Combined with the calculation of the thermal conductivity coefficient, the heating parameters can be accurately adjusted to ensure the uniform distribution of heat inside the sand core. This intelligent control mechanism not only improves the efficiency of the heating process, but also significantly reduces energy consumption, which helps to achieve the goals of green production and energy conservation and emission reduction.
[0041] On the other hand, the present application also provides an automated batching and sand mixing method for a cold core sand pretreatment boiling heating process, comprising:
[0042] Obtaining the sand core temperature and the sand core weight inside the boiler, and determining the weight of the ingredients to be added according to the sand core weight and the sand core temperature;
[0043] According to the determined weight of the ingredients to be added, the ingredients are added into the boiler and stirred with the sand core for 25-40 seconds.
[0044] Further, when the weight of the ingredients to be added is determined according to the weight and temperature of the sand core, it includes:
[0045] The real-time weight of the sand core is obtained, and the weight of the ingredients is determined according to the weight ratio between the real-time weight and the preset weight, wherein:
[0046] Presetting a first preset weight ratio and a second preset weight ratio, wherein the first preset weight ratio is smaller than the second preset weight ratio;
[0047] When the weight ratio is less than or equal to the first preset weight ratio, the weight of the ingredient to be added is determined to be B1;
[0048] When the weight ratio is greater than the first preset weight ratio and the weight ratio is less than or equal to the second preset weight ratio, the weight of the ingredient to be added is determined to be B2;
[0049] When the weight ratio is greater than the second preset weight ratio, the weight of the ingredient to be added is determined to be B3;
[0050] Moreover, B1<B2<B3.
[0051] Further, when the weight of the ingredient to be added is determined as Bi, i=1, 2, 3, including:
[0052] Acquire the real-time temperature of the sand core, and acquire the sand core temperature difference between the real-time temperature of the sand core and a preset sand core temperature, and determine whether to adjust the weight Bi of the ingredient to be added according to the sand core temperature difference;
[0053] Wherein, a first preset sand core temperature difference and a second preset sand core temperature difference are preset, and the first preset sand core temperature difference is smaller than the second preset sand core temperature difference;
[0054] When the sand core temperature difference is less than the first preset sand core temperature, and the sand core temperature difference is greater than or equal to zero, it is determined that the weight Bi of the ingredient to be added is not adjusted;
[0055] When the sand core temperature is greater than or equal to the first preset sand core temperature, and the sand core temperature is less than the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is adjusted is determined to be H1;
[0056] When the sand core temperature is greater than or equal to the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is adjusted is determined to be H2;
[0057] Moreover, H1<H2<1.
[0058] Furthermore, the ingredients to be added are: phenolic resin and isocyanate.
[0059] Compared with the prior art, the beneficial effect of the present invention is that by obtaining the temperature and weight of the sand core inside the boiler, the weight of the ingredients to be added is accurately determined according to these parameters, and the mixing is carried out within a stirring time of 25-40 seconds. The beneficial effect of this method is that it can achieve precise control and uniform mixing of the ingredients, ensure the accurate proportion of the various components of the sand core, and improve the quality consistency and stability of the sand core. In addition, the automated batching and sand mixing process reduces the errors of human operation, improves production efficiency, optimizes the production process, further shortens the production cycle and reduces costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0060] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0061] Figure 1 A flowchart of a cold core sand pretreatment boiling heating process provided by an embodiment of the present invention;
[0062] Figure 2 A flowchart of an automated batching and sand mixing method for a cold core sand pretreatment boiling heating process provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0063] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0064] like Figure 1 As shown, in some embodiments of the present application, this embodiment provides a cold core sand pretreatment boiling heating process, comprising:
[0065] Step S110: Arrange a heat exchange coil and a hot air circulation device inside the boiler.
[0066] Step S120, obtaining the real-time temperature inside the boiler and the sand core image, as well as the thermal conductivity coefficient of the sand core.
[0067] Step S130, obtaining the boiling temperature of the sand core, and determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core and the real-time temperature inside the boiler.
[0068] Specifically, when determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core, the real-time temperature inside the boiler, and the thermal conductivity coefficient of the sand core material, it includes: obtaining the temperature ratio between the boiling temperature of the sand core and the real-time temperature inside the boiler, and determining the heating power of the heat exchange coil and the hot air circulation device according to the relationship between the temperature ratio and the preset temperature ratio: wherein a first preset temperature ratio and a second preset temperature ratio are preset, and the first preset temperature ratio is less than the second preset temperature ratio. When the temperature ratio is greater than the second preset temperature ratio, the heating power of the heat exchange coil is determined to be M3, and the heating power of the hot air circulation device is determined to be N3. When the temperature ratio is less than or equal to the second preset temperature ratio, and the temperature ratio is greater than the first preset temperature ratio, the heating power of the heat exchange coil is determined to be M2, and the heating power of the hot air circulation device is determined to be N2. When the temperature ratio is less than the first preset temperature ratio, the heating power of the heat exchange coil is determined to be M1, and the heating power of the hot air circulation device is determined to be N1. Furthermore, 10%<M1<M2<M3<55%, and 10%<N1<N2<N3<55%.
[0069] It can be understood that by obtaining the boiling temperature of the sand core and the temperature inside the boiler in real time, the heating power of the heat exchange coil and the hot air circulation device is determined according to the temperature ratio between the two and the thermal conductivity coefficient of the sand core material. Specifically, different heating power intervals correspond to the preset first and second preset temperature ratios. When the temperature ratio is greater than the second preset temperature ratio, the maximum heating power (M3 and N3) is used; when the temperature ratio is between the first and second preset temperature ratios, the medium heating power (M2 and N2) is used; when the temperature ratio is less than the first preset temperature ratio, the minimum heating power (M1 and N1) is used. By dynamically adjusting the heating power in this way, the heating process can be accurately controlled to ensure uniform heating of the core sand and improve the quality of the casting, while optimizing energy efficiency and reducing energy consumption.
[0070] Step S140, obtaining the heating power and heating power of the heat exchange coil and the hot air circulation device, and adjusting them according to the sand core image and the thermal conductivity coefficient of the sand core material.
[0071] Specifically, when determining that the heating power of the heat exchange coil is Mi and the heating power of the hot air circulation device is Ni, i=1, 2, 3, and adjusting according to the sand core image and the thermal conductivity coefficient of the sand core material, it includes: obtaining the thermal conductivity of the sand core material, and determining whether to adjust the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device according to the relationship between the thermal conductivity and the preset thermal conductivity: when the thermal conductivity is consistent with the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device are not adjusted. When the thermal conductivity is greater than or less than the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device need to be adjusted, the thermal conductivity ratio between the thermal conductivity and the preset thermal conductivity is obtained, and the adjustment coefficient when adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device is determined according to the thermal conductivity ratio.
[0072] Specifically, when determining the adjustment coefficient when adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device according to the thermal conductivity ratio, it includes: presetting a first preset thermal conductivity ratio and a second preset thermal conductivity ratio, and the first preset thermal conductivity ratio is less than the second preset thermal conductivity ratio. According to the relationship between the thermal conductivity ratio and each preset thermal conductivity ratio, the adjustment coefficient is determined, wherein: when the thermal conductivity ratio is less than the first preset thermal conductivity ratio, the adjustment coefficient is determined to be L1. When the thermal conductivity ratio is greater than or equal to the first preset thermal conductivity ratio, and the thermal conductivity ratio is less than the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L2. When the thermal conductivity ratio is greater than or equal to the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L3. And, L1<L2<L3<1.
[0073] Specifically, when determining the adjustment coefficient Li for adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device, i=1,2,3, it includes: obtaining the real-time height of the sand core inside the boiler according to the image of the sand core inside the boiler, and determining whether to correct the adjustment coefficient Li according to the relationship between the real-time height and the preset height. When the real-time height is less than or equal to the preset height, it is determined that the adjustment coefficient Li is not corrected. When the real-time height is greater than the preset height, the height difference between the real-time height and the preset height is obtained, and the correction coefficient for correcting the adjustment coefficient Li is determined according to the height difference.
[0074] Specifically, when determining the correction coefficient for the adjustment coefficient Li for correction according to the height difference, it includes: presetting a first preset height difference and a second preset height difference, and the first preset height difference is less than the second preset height difference. According to the relationship between the height difference and each preset height difference, the correction coefficient for the adjustment coefficient Li for correction is determined, wherein: when the height difference is less than or equal to the first preset height difference, the correction coefficient is determined to be K1. When the height difference is greater than the first preset height difference, and the height difference is less than or equal to the second preset height difference, the correction coefficient is determined to be K2. When the height difference is greater than the second preset height difference, the correction coefficient is determined to be K3. And, K1<K2<K3<1.
[0075] It can be seen that by obtaining the thermal conductivity of the sand core material and according to its relationship with the preset thermal conductivity, it is determined whether to adjust the heating power of the heat exchange coil and the hot air circulation device. When the thermal conductivity is consistent with the preset value, the original heating power is kept unchanged; when the thermal conductivity deviates from the preset value, the adjustment coefficient is calculated by the thermal conductivity ratio, and the heating power of the heat exchange coil and the hot air circulation device is adjusted according to the coefficient. This method ensures that sand cores of different materials can achieve the best heat treatment effect during the heating process. Furthermore, by obtaining the sand core image inside the boiler, the height of the sand core inside the boiler is monitored in real time. According to the difference between the real-time height of the sand core and the preset height, the correction coefficient is calculated and the adjustment coefficient is corrected. When the real-time height of the sand core is less than or equal to the preset height, no correction is made; when the real-time height exceeds the preset height, the correction coefficient is determined by the height difference, so as to further fine-tune the heating power. This dynamic correction mechanism can effectively deal with the problem of uneven heat distribution caused by the change of the sand core height during the heating process, and ensure that the sand core is heated evenly during the heating process.
[0076] It can be understood that the adjustment coefficient of the heating power is determined by the thermal conductivity ratio, and the heating power of the heat exchange coil and the hot air circulation device is accurately adjusted according to different thermal conductivity ratios. Secondly, the adjustment coefficient is corrected by real-time height monitoring and the introduction of the correction coefficient to ensure the temperature uniformity and consistency of the sand core throughout the heating process. This multi-level adjustment and correction mechanism not only improves the accuracy and stability of the heating process, but also optimizes energy utilization, significantly improves the quality of castings and production efficiency. In addition, by accurately controlling the heating power of the heat exchange coil and the hot air circulation device, the common problems of local overheating or insufficient heating in traditional heating methods can be avoided. This precise control ensures that all parts of the sand core are heated evenly, thereby improving the overall quality and performance of the sand core, reducing the scrap rate in casting production, and reducing production costs. By optimizing energy utilization, it is also possible to significantly reduce energy consumption in the production process, achieve the goals of green production and energy conservation and emission reduction, and improve the environmental protection and economic benefits of the casting process.
[0077] In the above embodiment, the combined use of the heat exchange coil and the hot air circulation device can make the heat evenly distributed inside the boiler, avoiding local overheating or insufficient heating, thereby improving the overall quality of the core sand. Secondly, by obtaining the temperature and sand core image inside the boiler in real time, as well as the thermal conductivity coefficient of the sand core, the heating process can be accurately controlled. This real-time monitoring and feedback mechanism allows the process parameters to be dynamically adjusted according to actual conditions to ensure that each batch of sand cores can achieve the ideal heating effect. This precise control not only improves the quality stability of the sand core, but also reduces the scrap rate caused by uneven heating, thereby improving production efficiency. Then, based on the boiling temperature and real-time temperature of the sand core, determining the heating power of the heat exchange coil and the hot air circulation device is another key advantage of the process. Sand cores of different materials and shapes have different boiling temperatures and thermal conductivity coefficients. By accurately calculating and controlling the heating power, customized heating can be performed for different sand core materials to ensure that each sand core can reach the best hardening state. This flexibility and customized heating method enable the process to adapt to different casting needs and improve the adaptability and flexibility of production. Finally, by adjusting the heating power of the heat exchange coil and the hot air circulation device, combined with the sand core image and the thermal conductivity of the material, the uniformity and efficiency of heating can be further improved. Real-time image monitoring can intuitively reflect the state of the sand core during the heating process. Combined with the calculation of the thermal conductivity coefficient, the heating parameters can be accurately adjusted to ensure the uniform distribution of heat inside the sand core. This intelligent control mechanism not only improves the efficiency of the heating process, but also significantly reduces energy consumption, which helps to achieve the goals of green production and energy conservation and emission reduction.
[0078] In another preferred embodiment based on the above embodiment, Figure 2 As shown, this embodiment provides an automated batching and sand mixing method for a cold core sand pretreatment boiling heating process, comprising:
[0079] Step S210, obtaining the sand core temperature and the sand core weight inside the boiler, and determining the weight of the ingredients to be added according to the sand core weight and the sand core temperature.
[0080] Specifically, when determining the weight of the ingredients to be added according to the weight and temperature of the sand core, it includes: obtaining the real-time weight of the sand core, and determining the weight of the ingredients according to the weight ratio between the real-time weight and the preset weight, wherein: a first preset weight ratio and a second preset weight ratio are preset, and the first preset weight ratio is less than the second preset weight ratio. When the weight ratio is less than or equal to the first preset weight ratio, the weight of the ingredients to be added is determined to be B1. When the weight ratio is greater than the first preset weight ratio, and the weight ratio is less than or equal to the second preset weight ratio, the weight of the ingredients to be added is determined to be B2. When the weight ratio is greater than the second preset weight ratio, the weight of the ingredients to be added is determined to be B3. And, B1<B2<B3.
[0081] Specifically, when the weight of the ingredient to be added is determined to be Bi, i=1,2,3, including: obtaining the real-time temperature of the sand core, obtaining the sand core temperature difference between the real-time temperature of the sand core and the preset sand core temperature, and determining whether to adjust the weight Bi of the ingredient to be added according to the sand core temperature difference. Among them, the first preset sand core temperature difference and the second preset sand core temperature difference are preset, and the first preset sand core temperature difference is less than the second preset sand core temperature difference. When the sand core temperature difference is less than the first preset sand core temperature, and the sand core temperature difference is greater than or equal to zero, it is determined that the weight Bi of the ingredient to be added is not adjusted. When the sand core temperature is greater than or equal to the first preset sand core temperature, and the sand core temperature is less than the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is adjusted is determined to be H1. When the sand core temperature is greater than or equal to the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is determined to be H2. Moreover, H1<H2<1.
[0082] It can be seen that by obtaining the real-time weight and real-time temperature of the sand core inside the boiler, as well as the preset weight and temperature, the weight ratio between the real-time weight and the preset weight is calculated. According to the preset first and second weight ratios, the weight of the ingredients to be added is determined to ensure that the amount of ingredients added can be accurately controlled under different circumstances to ensure the composition ratio and quality stability of the sand core. Secondly, according to the temperature difference between the real-time temperature of the sand core and the preset temperature, it is determined whether the weight of the ingredients to be added needs to be further adjusted. By setting the first and second preset temperature differences, different adjustment situations correspond to each other: when the temperature difference is less than the first preset value, no weight adjustment is performed; when the temperature difference is between the first and second preset values, the adjustment coefficient is determined according to the temperature difference, and then the weight of the ingredients is adjusted. This adjustment ensures that the amount of ingredients can be flexibly adjusted when the temperature of the sand core changes, thereby maintaining uniform heat distribution and accurate composition ratio of the sand core during heating.
[0083] It is understandable that the precise input amount of ingredients to be added during the sand core heating process is effectively controlled through real-time monitoring and dynamic adjustment. By weighing the relationship between the weight, temperature and preset parameters of the sand core, accurate control of key steps in the casting process is achieved, ensuring the improvement of casting quality and production efficiency. In addition, by optimizing the input amount of ingredients, energy and raw materials can be effectively saved, thereby achieving sustainable development of the casting process and improving economic benefits.
[0084] Specifically, the ingredients to be added are: phenolic resin and isocyanate.
[0085] Step S220: according to the determined weight of the ingredients to be added, add the ingredients into the interior of the boiler and stir with the sand core for 25-40 seconds.
[0086] It can be understood that in the above-mentioned embodiments, an automated batching and sand mixing method for a cold core sand pretreatment boiling heating process obtains the temperature and weight of the sand core inside the boiler, accurately determines the weight of the ingredients to be added according to these parameters, and mixes them within a stirring time of 25-40 seconds. The beneficial effect of this method is that it can achieve precise control and uniform mixing of the ingredients, ensure the accurate proportion of each component of the sand core, and improve the quality consistency and stability of the sand core. In addition, the automated batching and sand mixing process reduces the error of human operation, improves production efficiency, optimizes the production process, further shortens the production cycle and reduces costs.
[0087] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment in combination with software and hardware. Moreover, the present application may adopt the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0088] The present application is described with reference to flowcharts and / or block diagrams of methods, devices (systems) and computer program products according to embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0089] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture including an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0090] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0091] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.
Claims
1. A cold core sand pretreatment boiling heating process, characterized in that: include: A heat exchange coil and a hot air circulation device are arranged inside the boiler; Acquiring the real-time temperature and sand core image inside the boiler, as well as the thermal conductivity coefficient of the sand core; Obtaining the boiling temperature of the sand core, and determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core and the real-time temperature inside the boiler; The heating power and heating power of the heat exchange coil and the hot air circulation device are obtained, and adjusted according to the sand core image and the thermal conductivity coefficient of the sand core material.
2. The cold core sand pretreatment boiling heating process according to claim 1, characterized in that: When determining the heating power of the heat exchange coil and the hot air circulation device according to the boiling temperature of the sand core, the real-time temperature inside the boiler and the thermal conductivity coefficient of the sand core material, it includes: Obtain the temperature ratio between the boiling temperature of the sand core and the real-time temperature inside the boiler, and determine the heating power of the heat exchange coil and the hot air circulation device according to the relationship between the temperature ratio and the preset temperature ratio: Wherein, a first preset temperature ratio and a second preset temperature ratio are preset, and the first preset temperature ratio is smaller than the second preset temperature ratio; When the temperature ratio is greater than the second preset temperature ratio, it is determined that the heating power of the heat exchange coil is M3, and the heating power of the hot air circulation device is N3; When the temperature ratio is less than or equal to the second preset temperature ratio, and the temperature ratio is greater than the first preset temperature ratio, it is determined that the heating power of the heat exchange coil is M2, and the heating power of the hot air circulation device is N2; When the temperature ratio is less than the first preset temperature ratio, it is determined that the heating power of the heat exchange coil is M1, and the heating power of the hot air circulation device is N1; Furthermore, 10%<M1<M2<M3<55%, and 10%<N1<N2<N3<55%.
3. The cold core sand pretreatment boiling heating process according to claim 2, characterized in that: When determining the heating power of the heat exchange coil as Mi and the heating power of the hot air circulation device as Ni, i=1, 2, 3, and adjusting according to the sand core image and the thermal conductivity coefficient of the sand core material, it includes: The thermal conductivity of the sand core material is obtained, and according to the relationship between the thermal conductivity and the preset thermal conductivity, it is determined whether to adjust the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device: When the thermal conductivity is consistent with the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device are not adjusted; When the thermal conductivity is greater than or less than the preset thermal conductivity, it is determined that the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device need to be adjusted, and the thermal conductivity ratio between the thermal conductivity and the preset thermal conductivity is obtained, and the adjustment coefficient when adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device is determined according to the thermal conductivity ratio.
4. The cold core sand pretreatment boiling heating process according to claim 3, characterized in that: When determining the adjustment coefficient of the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device according to the thermal conductivity ratio, it includes: Presetting a first preset thermal conductivity ratio and a second preset thermal conductivity ratio, wherein the first preset thermal conductivity ratio is smaller than the second preset thermal conductivity ratio; The adjustment coefficient is determined according to the relationship between the thermal conductivity ratio and each preset thermal conductivity ratio, wherein: When the thermal conductivity ratio is less than the first preset thermal conductivity ratio, the adjustment coefficient is determined to be L1; When the thermal conductivity ratio is greater than or equal to the first preset thermal conductivity ratio, and the thermal conductivity ratio is less than the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L2; When the thermal conductivity ratio is greater than or equal to the second preset thermal conductivity ratio, the adjustment coefficient is determined to be L3; Moreover, L1<L2<L3<1.
5. The cold core sand pretreatment boiling heating process according to claim 4, characterized in that: When determining the adjustment coefficient Li for adjusting the heating power Mi of the heat exchange coil and the heating power Ni of the hot air circulation device, i=1, 2, 3, it includes: According to the sand core image inside the boiler, the real-time height of the sand core inside the boiler is obtained, and according to the relationship between the real-time height and the preset height, it is determined whether to correct the adjustment coefficient Li; When the real-time altitude is less than or equal to the preset altitude, it is determined that the adjustment coefficient Li is not corrected; When the real-time altitude is greater than the preset altitude, the altitude difference between the real-time altitude and the preset altitude is obtained, and the adjustment coefficient is determined as a correction coefficient for Li according to the altitude difference.
6. The cold core sand pretreatment boiling heating process according to claim 5, characterized in that: When determining the adjustment coefficient as a correction coefficient for Li according to the height difference, it includes: Presetting a first preset height difference value and a second preset height difference value, wherein the first preset height difference value is smaller than the second preset height difference value; According to the relationship between the height difference value and each preset height difference value, the adjustment coefficient is determined to be a correction coefficient for correction of Li, wherein: When the height difference is less than or equal to the first preset height difference, the correction coefficient is determined to be K1; When the height difference is greater than the first preset height difference, and the height difference is less than or equal to the second preset height difference, the correction coefficient is determined to be K2; When the height difference is greater than the second preset height difference, the correction coefficient is determined to be K3; Moreover, K1<K2<K3<1.
7. An automated batching and sand mixing method based on the cold core sand pretreatment boiling heating process according to claim 1, characterized in that: include: Obtaining the sand core temperature and the sand core weight inside the boiler, and determining the weight of the ingredients to be added according to the sand core weight and the sand core temperature; According to the determined weight of the ingredients to be added, the ingredients are added into the boiler and stirred with the sand core for 25-40 seconds.
8. The automatic batching and sand mixing method according to claim 7, characterized in that: When the weight of the ingredients to be added is determined according to the weight of the sand core and the temperature of the sand core, it includes: The real-time weight of the sand core is obtained, and the weight of the ingredients is determined according to the weight ratio between the real-time weight and the preset weight, wherein: Presetting a first preset weight ratio and a second preset weight ratio, wherein the first preset weight ratio is smaller than the second preset weight ratio; When the weight ratio is less than or equal to the first preset weight ratio, the weight of the ingredient to be added is determined to be B1; When the weight ratio is greater than the first preset weight ratio and the weight ratio is less than or equal to the second preset weight ratio, the weight of the ingredient to be added is determined to be B2; When the weight ratio is greater than the second preset weight ratio, the weight of the ingredient to be added is determined to be B3; Moreover, B1<B2<B3.
9. The automatic batching and sand mixing method according to claim 8, characterized in that: When the weight of the ingredients to be added is determined as Bi, i=1, 2, 3, including: Acquire the real-time temperature of the sand core, and acquire the sand core temperature difference between the real-time temperature of the sand core and a preset sand core temperature, and determine whether to adjust the weight Bi of the ingredient to be added according to the sand core temperature difference; Wherein, a first preset sand core temperature difference and a second preset sand core temperature difference are preset, and the first preset sand core temperature difference is smaller than the second preset sand core temperature difference; When the sand core temperature difference is less than the first preset sand core temperature, and the sand core temperature difference is greater than or equal to zero, it is determined that the weight Bi of the ingredient to be added is not adjusted; When the sand core temperature is greater than or equal to the first preset sand core temperature, and the sand core temperature is less than the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is adjusted is determined to be H1; When the sand core temperature is greater than or equal to the second preset sand core temperature difference, it is determined that the weight Bi of the ingredient to be added is adjusted, and the adjustment coefficient when the weight Bi of the ingredient to be added is adjusted is determined to be H2; Moreover, H1<H2<1.
10. The automatic batching and sand mixing method according to claim 9, characterized in that: The ingredients to be added are: phenolic resin and isocyanate.