3D printing method and device, workpiece and computer readable storage medium

By dividing the area and adjusting the density of the scanning path at the cross-section mutation of the 3D printed workpiece, the problem of shrinkage lines at the cross-section mutation position in powder-laying 3D printing is solved, and the appearance and performance of the workpiece are improved.

CN118808672APending Publication Date: 2024-10-22SHANGHAI JIAOTONG UNIV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411085649.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

During the powder-laying 3D printing process, shrinkage lines are likely to occur at sudden changes in the cross-section, affecting the appearance and performance of the part.

Method used

By slicing the process model of the workpiece in layers, determining the cross-sectional mutation site and dividing the second area and at least one first area, controlling the energy source operation to print layer by layer, using different scanning path filling strategies to ensure that the filling density changes when the cross-section suddenly changes. The area is gradually enlarged to reduce or avoid the occurrence of shrinkage lines.

Benefits of technology

Effectively reduce or even eliminate the occurrence of shrinkage lines, improve the appearance and quality of the workpiece, and improve printing quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808672A_ABST
    Figure CN118808672A_ABST
Patent Text Reader

Abstract

The invention provides a 3D printing method and device, a workpiece and a computer readable storage medium. The 3D printing method comprises the steps that layered slicing is conducted on a process model of the workpiece; determining a section abrupt change part on the process model; a second area and at least one first area are divided on the section of the section mutation part, all the first areas jointly surround the second area, and the edges, away from the second area, of the first areas are located on the surface of the process model; the second area comprises a flexible area, and the flexible area is adjacent to the first area; controlling the energy source to operate to print layer by layer and form a workpiece; the energy source operates based on a first scanning path filling strategy when printing other parts and a first area except a section abrupt change part of the workpiece, and operates based on a second scanning path filling strategy when printing a flexible area of the workpiece; the filling density of the first scanning path filling strategy is larger than that of the second scanning path filling strategy, and the filling density of the second scanning path filling strategy is increased in the forming direction when different slices of the section abrupt change part are printed. The application of the method can effectively avoid generation of contraction lines with section mutation characteristics.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of 3D printing, and in particular relates to a 3D printing method and device, a workpiece, and a computer-readable storage medium. Background Art

[0002] According to different feeding methods, 3D printing can be of different types, such as powder spreading, powder feeding, and wire feeding. Among them, powder spreading 3D printing technology mainly includes selective laser melting (SLM), selective laser sintering (SLS), and electron beam melting (EBM). These 3D printing technologies usually use precisely focused laser spots or electron beams as energy sources to quickly melt pre-laid layers of metal or nylon powder, and can directly obtain functional parts of almost any shape. It is a rapid prototyping technology with great development prospects and has broad application prospects in aerospace, medical, automotive, mold manufacturing and other fields.

[0003] In the process of layer-by-layer printing of metal powder, a high-precision energy source sintered or melted the powder layer by layer. Then after sintering or melting, the layer will shrink to a certain extent, and the shrinkage is mainly determined by the cross-sectional area and shape of each layer. Figure 1 When there is a cross-sectional mutation in the part 10 shown in FIG. 1 , a shrinkage line 12 (such as Figure 2 As shown in the figure, the shrinkage line 12 may affect the appearance of the part at the least, or may affect the performance of the part at the worst, causing the part to be scrapped. Summary of the invention

[0004] The purpose of the present invention is to provide a 3D printing method and device, a workpiece, and a computer-readable storage medium, aiming to improve the printing quality of workpieces with cross-sectional mutation characteristics, reduce or even avoid the generation of shrinkage lines, and improve the appearance and quality of parts.

[0005] To achieve the above object, the present invention provides a 3D printing method, comprising:

[0006] The process model of the workpiece is sliced ​​in layers along the forming direction;

[0007] Determining a cross-sectional mutation location on the process model, wherein the cross-sectional mutation location includes at least one layer of the slice;

[0008] A second region and at least one first region are divided on the slice at the cross-sectional mutation site, all the first regions jointly surround the second region, and edges of the first regions away from the second regions are located on the surface of the process model; the second region includes a flexible region, and the flexible region is adjacent to the first region; and,

[0009] Controlling the energy source to print layer by layer along the forming direction until the workpiece is formed;

[0010] When printing other parts of the workpiece except the cross-sectional mutation site and the first area, the energy source operates based on the first scanning path filling strategy, and when printing the flexible area of ​​the workpiece, the energy source operates based on the second scanning path filling strategy. The filling density of the first scanning path filling strategy is greater than the filling density of the second scanning path filling strategy, and when printing different slices of the cross-sectional mutation site of the workpiece, the filling density of the second scanning path filling strategy gradually increases along the forming direction.

[0011] Optionally, the step of determining a cross-section mutation location on the process model includes:

[0012] Obtaining the cross-sectional area of ​​each slice;

[0013] Obtaining a ratio of the cross-sectional areas of two adjacent slices;

[0014] Determine whether the ratio of the cross-sectional areas of two adjacent layers of the slices is greater than or equal to 1 / n and less than or equal to n. If not, take the slice with the larger cross-sectional area among the two adjacent layers of the slices as the cross-sectional mutation site, or take the slice with the larger cross-sectional area among the two adjacent layers of the slices and several layers of the slices located on the side of the slice with the larger cross-sectional area away from the slice with the smaller cross-sectional area as the cross-sectional mutation site; n is greater than 1.

[0015] Optionally, the scanning path of the second scanning path filling strategy is a curved path or a broken line path;

[0016] When printing different slices of the cross-sectional mutation location of the workpiece, the width of the scanning path of the second scanning path filling strategy gradually increases along the forming direction, and / or the number of scanning paths of the second scanning path filling strategy gradually increases along the forming direction.

[0017] Optionally, the scanning path of the second scanning path filling strategy is a dot matrix path, and when printing different slices of the cross-sectional mutation portion of the workpiece, the dot matrix density of the dot matrix path gradually increases along the forming direction.

[0018] Optionally, when the slice at the cross-section mutation site is a solid structure, the number of the first region is one; the first region is arranged around the periphery of the second region, and an edge of the first region away from the second region is on the outer surface of the process model;

[0019] When the slice at the cross-sectional mutation site is a hollow annular structure, the number of the first regions is two; one of the two first regions is arranged on the outer periphery of the second region, and the other is arranged on the inner periphery of the second region, and an edge of the first region arranged on the outer periphery of the second region away from the second region is on the outer surface of the process model, and an edge of the first region arranged on the inner periphery of the second region away from the second region is on the inner surface of the process model.

[0020] Optionally, when the ratio of the cross-sectional areas of two adjacent layers of the slices is less than 1 / n or greater than n, the slice with the smaller area among the two adjacent layers of the slices is used as the reference slice of the corresponding cross-sectional mutation site; the ratio of the area of ​​any first region to the cross-sectional area of ​​the reference slice corresponding to the cross-sectional mutation site where the first region is located is greater than or equal to 1 / m and less than or equal to m, and m is greater than 1 and less than n.

[0021] Optionally, when the slice at the cross-sectional mutation site is an annular structure, the second region includes two flexible regions and one connecting region, and each flexible region is located between one of the first regions and the connecting region.

[0022] To achieve the above objectives, the present invention further provides a 3D printing device, comprising a control unit and an energy source, wherein the control unit is communicatively connected to the energy source and is configured to execute the 3D printing method as described in any of the preceding items.

[0023] To achieve the above-mentioned object, the present invention further provides a computer-readable storage medium having a program stored thereon, and when the program is executed, the 3D printing method as described in any of the preceding items is executed.

[0024] To achieve the above-mentioned purpose, the present invention further provides a workpiece, which is printed by the 3D printing method as described in any of the preceding items.

[0025] Compared with the prior art, the 3D printing method and device, workpiece, and computer-readable storage medium of the present invention have the following advantages:

[0026] The aforementioned 3D printing method comprises: slicing the process model of the workpiece in layers along the molding direction; determining a cross-sectional mutation site on the process model, the cross-sectional mutation site includes at least one layer of the slices; dividing a second area and at least one first area on the slices of the cross-sectional mutation site, all of the first areas together surround the second area, and the edge of the first area away from the second area is located on the surface of the process model; the second area includes a flexible area, the flexible area is adjacent to the first area; and controlling the energy source to run to print layer by layer and form the workpiece; when printing other parts of the workpiece except the cross-sectional mutation site and the first area, the energy source runs based on the first scanning path filling strategy, and when printing the flexible area of ​​the workpiece, the energy source runs based on the second scanning path filling strategy; the filling density of the first scanning path filling strategy is greater than the filling density of the second scanning path filling strategy, and when printing different slices of the cross-sectional mutation site, the filling density of the second scanning path filling strategy gradually increases along the molding direction. The 3D printing method is suitable for the molding of workpieces with cross-sectional mutations, and the application of the 3D printing method can effectively reduce or even eliminate the generation of shrinkage lines and improve the appearance and quality of the workpiece. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] The accompanying drawings are used to better understand the present invention and do not constitute an improper limitation of the present invention.

[0028] Figure 1 It is a schematic diagram of a workpiece, in which there is a sudden change in cross section of the workpiece;

[0029] Figure 2 It is formed by the 3D printing method in the existing technology. Figure 1 When the workpiece is shown, a schematic diagram of the workpiece obtained;

[0030] Figure 3 is an overall flow chart of a 3D printing method provided by the present invention according to an embodiment;

[0031] Figure 4 is a partial flow chart of a 3D printing method provided by the present invention according to an embodiment;

[0032] Figure 5 It is a schematic diagram of a process model of a workpiece printed by a 3D printing method provided by an embodiment of the present invention when applied, wherein a cross-sectional mutation site and a non-cross-sectional mutation site are identified in the diagram;

[0033] Figure 6 is a schematic diagram of a process model of another workpiece printed by the 3D printing method provided by one embodiment of the present invention when applied, wherein a cross-sectional mutation site and a non-cross-sectional mutation site are identified in the diagram;

[0034] Figure 7 is a schematic diagram of dividing a target slice into regions in a 3D printing method provided according to an embodiment of the present invention, wherein the target slice in the figure is a solid structure, and the second region is entirely a flexible region;

[0035] Figure 8 is a schematic diagram of dividing a target slice into regions in a 3D printing method provided according to an embodiment of the present invention, wherein the target slice in the figure is a solid structure, and the second region includes a flexible region and a non-flexible region;

[0036] Fig. 9 is a schematic diagram of dividing a target slice into regions in a 3D printing method provided according to an embodiment of the present invention, wherein the target slice in the figure is a ring-shaped structure, and the second region is entirely a flexible region;

[0037] Fig.10 is a schematic diagram of dividing a target slice into regions in a 3D printing method provided according to an embodiment of the present invention, wherein the target slice in the figure is a ring-shaped structure, and the second region includes two flexible regions and one connection region;

[0038] Fig.11 is a schematic diagram of printing a flexible area in a 3D printing method provided according to an embodiment of the present invention, wherein the scanning path in the figure is a zigzag path, a) is a schematic diagram of a flexible area of ​​a first target slice of two adjacent target slices, b) is a schematic diagram of a flexible area of ​​a second target slice of two adjacent target slices, and the number of welds formed in b) is greater than the number of welds formed in a);

[0039] Fig.12 is a schematic diagram of printing a flexible area in a 3D printing method provided according to an embodiment of the present invention, wherein the scanning path in the figure is a zigzag path, a) is a schematic diagram of a flexible area of ​​a first target slice of two adjacent target slices, b) is a schematic diagram of a flexible area of ​​a second target slice of two adjacent target slices, and the width of the weld formed in b) is greater than the width of the weld formed in a);

[0040] Fig.13 It is a schematic diagram of printing a flexible area in a 3D printing method provided according to an embodiment of the present invention, wherein the scanning path in the figure is a Z-shaped path, a) is a schematic diagram of the flexible area of ​​the first layer of two adjacent target slices, and b) is a schematic diagram of the flexible area of ​​the second layer of two adjacent target slices, and the number of solder joints formed in b) is greater than the number of solder joints formed in a).

[0041] [Description of reference numerals is as follows]:

[0042] 10-workpiece, 12-shrinkage line, 100-process model, 110-slice, 110a-target slice, 110b-reference slice, 101-cross-section mutation site, 11, 101a-cross-section mutation position, 111-first area, 112-second area, 112a-flexible area, 112b-non-flexible area, 112c-connection area. DETAILED DESCRIPTION

[0043] The following is an explanation of the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the illustrations provided in the present embodiment only illustrate the basic concept of the present invention in a schematic manner, and only the components related to the present invention are shown in the figure instead of being drawn according to the number, shape and size of the components in the actual implementation. The type, quantity and proportion of each component in the actual implementation can be a random change, and the component layout type may also be more complicated.

[0044] In addition, each embodiment of the following description has one or more technical features, but this does not mean that the user of the present invention must implement all the technical features in any embodiment at the same time, or can only implement part or all of the technical features in different embodiments separately. In other words, under the premise that implementation is possible, those skilled in the art can selectively implement part or all of the technical features in any embodiment according to the disclosure of the present invention and according to the design specifications or implementation requirements, or selectively implement a combination of part or all of the technical features in multiple embodiments, thereby increasing the flexibility of the implementation of the present invention.

[0045] As used in this specification, the singular forms "one", "an" and "the" include plural objects, and the plural form "multiple" includes more than two objects, unless the content clearly indicates otherwise. As used in this specification, the term "or" is usually used in the sense of including "and / or", unless the content clearly indicates otherwise, and the terms "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection. It can be a mechanical connection or an electrical connection. It can be directly connected or indirectly connected through an intermediate medium, and it can be the internal connection of two elements or the interaction relationship between two elements. Relational terms such as the terms "first", "second", etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations, nor do they indicate or imply relative importance or implicitly indicate the number of technical features indicated. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0046] The object of the present invention is to provide a 3D printing method, which is suitable for printing a workpiece with a cross-sectional mutation feature to reduce or even eliminate the shrinkage line at the cross-sectional mutation site, improve the printing quality, and improve the appearance and performance of the workpiece.

[0047] In order to make the purpose, advantages and features of the present invention more clear, the present invention is further described in detail below with reference to the accompanying drawings. It should be noted that the drawings are all in very simplified form and in non-precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. The same or similar reference numerals in the drawings represent the same or similar components.

[0048] Figure 3 The overall process of the 3D printing method is shown. Please refer to Figure 3 , the 3D printing method comprises:

[0049] Step S10: Process model 100 (such as Figure 5 or Figure 6 As shown in the figure, the plurality of slices 110 are layered to obtain the plurality of slices 110 sequentially arranged along the forming direction.

[0050] Step S20: determining a cross-sectional mutation location 101 (e.g. Figure 5 or Figure 6As shown in FIG. 1 ). It can be understood that, other parts of the process model 100 except the cross-sectional mutation part 101 are non-cross-sectional mutation parts (not marked in the figure), and each cross-sectional mutation part 101 is located between two non-cross-sectional mutation parts. The cross-sectional mutation part 101 includes at least one layer of the slice 110, and the non-cross-sectional mutation part also includes at least one layer of the slice 110. For the convenience of description, the slice 110 located at the cross-sectional mutation part 101 is referred to as the target slice 110a.

[0051] Step S30: divide each target slice 110a into regions, so as to divide each target slice 110a into a second region 112 and at least one first region 111 (such as Figures 7 to 10 All the first regions 111 surround the second region 112 together, and the edge of the first region 111 away from the second region 112 is on the surface of the process model 100. The second region 112 includes at least a flexible region 112a, and the flexible region 112a is adjacent to the first region 111.

[0052] Step S40, based on the non-cross-sectional mutation part, the first region 111, and the flexible region 112a, the energy source is controlled to operate according to a preset scanning path filling strategy, and prints layer by layer along the forming direction until the workpiece is formed.

[0053] The process model 100 is established based on the workpiece to be printed. Therefore, for the convenience of description, the same terms are used herein to describe the corresponding parts of the workpiece and the process model 100. Specifically, the part of the workpiece corresponding to the cross-sectional mutation part 101 of the process model 100 is described as the cross-sectional mutation part 101 of the workpiece, the part of the workpiece corresponding to the non-cross-sectional mutation part of the process model 100 is described as the non-cross-sectional mutation part of the workpiece, the part of the workpiece corresponding to the target slice 110a of the process model 100 is described as the target slice 110a of the workpiece, the part of the workpiece corresponding to the first area 111 of the process model 100 is described as the first area 111 of the workpiece, the part of the workpiece corresponding to the second area 112 of the process model 100 is described as the second area 112 of the workpiece, and the part of the workpiece corresponding to the flexible area 112a of the process model 100 is described as the flexible area 112a of the workpiece.

[0054] In an embodiment of the present invention, the scanning path filling strategy includes at least a first scanning path filling strategy and a second scanning path filling strategy, and when printing the non-cross-sectional mutation site of the workpiece and the first area 111 of the target slice 110a, the energy source operates based on the first scanning path filling strategy, and when printing the flexible area 112a of the target slice 110 of the workpiece, the energy source operates based on the second scanning path filling strategy. The second scanning path is different from the first scanning path filling strategy, specifically, the filling density of the second scanning path filling strategy is less than the filling density of the first scanning path filling strategy. Moreover, when the cross-sectional mutation site 101 includes a plurality of target slices 110a, for the plurality of target slices 110a of the same cross-sectional mutation site 101, the filling density of the second scanning path filling strategy gradually increases along the molding direction. In other words, when the plurality of target slices 110a of the interface mutation site 101 are numbered as the first target slice 110a, the second target slice 110a, the third target slice 110a, ... the i-th target slice 110a, respectively, along the molding direction, and the filling density in the second scanning path filling strategy when printing the flexible area 112a of the first target slice 110a of the workpiece is M1, the filling density of the second scanning path filling strategy when printing the flexible area 112a of the second target slice 110a of the workpiece is M2, the filling density of the second scanning path filling strategy when printing the flexible area 112a of the third target slice 110a of the workpiece is M3, ... the filling density of the second scanning path filling strategy when printing the i-th target slice 110a of the workpiece is Mi, M1, M2, M3, ... Mi gradually increase. i is a positive integer greater than 1, and M1, M2, M3, ... Mi are all greater than 0.

[0055] By executing the 3D printing method, the filling density of the workpiece obtained by printing at the flexible area 112a of the target slice 110 can be made smaller than the filling density at the non-cross-sectional mutation site 101 and the first area 111 of the target slice 110a. In this way, the workpiece has a certain flexibility at the flexible area 112a of the target slice 110a, and can resist the stress changes caused by the cross-sectional changes during the printing process, and further resist the shrinkage of the raw material forming the workpiece at the cross-sectional mutation site 101. When the cross-sectional mutation site 101 includes multiple target slices 110, the filling density of the second scanning path filling strategy is controlled to gradually increase along the forming direction during the process of printing different target slices 110 of the same cross-sectional mutation site 101 of the workpiece, so that the filling density of the flexible area 112a of each target slice 110a of the cross-sectional mutation site 101 gradually increases along the forming to gradually improve the density inside the mutation site 101, thereby forming a relatively uniform transition between the density of the flexible area 112a of each target slice 110a of the cross-sectional mutation site 101 and the non-mutation site after the cross-sectional mutation site 101 along the forming direction, thereby effectively avoiding the formation of a shrinkage line at the cross-sectional mutation position 112a, thereby improving the appearance and performance of the workpiece.

[0056] It can be understood that there is a cross-sectional mutation position 101a on the cross-sectional mutation part 101. The cross-sectional mutation position 101a refers to the position where the cross-sectional area change trend of the process model 100 or the workpiece perpendicular to the forming direction suddenly changes, for example Figure 5 The position where the cross-sectional area of ​​the process model 100 perpendicular to the forming direction begins to increase or changes from gradually increasing to a position where it remains unchanged, or Figure 6 The process model 100 of another workpiece shown is a position where the cross-sectional area perpendicular to the forming direction suddenly changes.

[0057] Next, each step of the 3D printing method is described in detail.

[0058] The step S10 can be directly performed using conventional methods. Figure 5 and Figure 6 The dotted line S in FIG. 1 represents a boundary line of part of the slice 110 .

[0059] The step S20 includes: determining the mutation site 101 and the non-mutation site according to the cross-sectional area of ​​each of the slices 110 .

[0060] Please refer to Figure 4, the step S20 may specifically include the following steps S21, S22 and S23.

[0061] The step S21 includes obtaining the cross-sectional area of ​​each layer of the slice 110 .

[0062] If necessary, Figure 6 As shown, when the slice 110 has a constant cross-sectional area in the molding direction, the cross-sectional area of ​​the slice 110 at any position in the molding direction is taken as the cross-sectional area of ​​the slice 110. When at least a portion of the slice 110 has different cross-sectional areas at different positions in the molding direction, the cross section of the slice 110 can be defined according to actual conditions, for example, the minimum cross-sectional area of ​​the slice 110 is defined as the cross-sectional area of ​​the slice 110, or the average of the maximum cross-sectional area and the minimum cross-sectional area of ​​the slice 110 is defined as the cross-sectional area of ​​the slice 110, or the maximum cross-sectional area of ​​the slice 110 is defined as the cross-sectional area of ​​the slice 110. Figure 5 In the process model shown, the minimum cross-sectional area of ​​the slice 110 may be defined as the cross-sectional area of ​​the slice 110 .

[0063] It should also be noted that, when the slice 110 is an annular structure, the cross-sectional area of ​​the slice 110 at a specified position (e.g., the position with the largest cross section or the position with the smallest cross section) refers to the cross-sectional area of ​​the annular structure at the specified position. For example, when the slice 110 is an annular structure, the cross-sectional area of ​​the slice 110 at the specified position has a circular first edge line and a circular second edge line, the first edge line is arranged around the periphery of the second edge line, the circle where the first edge line is located is called the first circle, and the circle where the second edge line is located is called the second circle, then the cross-sectional area of ​​the slice 110 at the specified position is equal to the difference between the area of ​​the first circle and the area of ​​the second circle. For another example, when the slice 110 is a rectangular annular structure, the slice 110 includes a rectangular first edge line and a rectangular second edge line at the specified position, the first edge line is arranged around the periphery of the second edge line, the rectangle where the first edge line is located is called the first rectangle, the rectangle where the second edge line is located is called the second edge line, and the cross-sectional area of ​​the slice 110 at the specified position is equal to the difference between the area of ​​the first rectangle and the area of ​​the second rectangle. The annular structure here can be regular, such as a circular annular structure, a rectangular annular structure, a polygonal annular structure, or irregular.

[0064] Step S22 includes obtaining the ratio of the cross-sectional areas of two adjacent layers of the slices 110, for example, the ratio of the cross-sectional area of ​​the latter layer of the slices 110 to the cross-sectional area of ​​the former layer of the slices 110. It can be understood that the latter layer and the former layer here are defined according to the molding direction. From the molding direction, the "latter layer" is behind the "previous layer". In practice, the molding direction is generally from bottom to top, so the "latter layer" is above the "previous layer" and the "previous layer" is below the "latter layer".

[0065] Step S23 includes determining whether the ratio of the cross-sectional areas of two adjacent layers of the slices 110 is greater than or equal to a first preset value and less than or equal to a second preset value. If not, the position of the slice 110 with a larger cross-sectional area among the two adjacent layers of the slices 110 is used as the mutation site 101, or the position of the slice 110 with a larger cross-sectional area among the two adjacent layers of the slices 110 and the positions of several layers of the slices 110 located on one side of the slice 110 with a larger cross-sectional area away from the slice 110 with a smaller cross-sectional area are used as the mutation site 101. Specifically, when the cross-sectional mutation site 101 includes a layer of the slice 110, the layer of the slice 110 with a larger cross-sectional area among the two adjacent layers of the slice 110 is used as the cross-sectional mutation site 101, that is, when the cross-sectional area of ​​the process model 100 suddenly increases, the cross-sectional area of ​​the latter layer of the slice 110 is larger than the cross-sectional area of ​​the former layer of the slice 110, and therefore the latter layer of the slice 110 among the two adjacent layers of the slice 110 is used as the target slice 110a; when the cross-sectional area of ​​the process model 100 suddenly decreases, the cross-sectional area of ​​the former layer of the slice 110 is larger than the cross-sectional area of ​​the latter layer of the slice 110, and at this time the former layer of the slice 110 among the two adjacent layers of the slice 110 is used as the target slice 110a. When the cross-sectional mutation site 101 includes multiple layers of slices 110, if the cross-sectional area of ​​the slice 110 of the next layer of two adjacent layers of slices 110 is larger than the cross-sectional area of ​​the slice 110 of the previous layer, the positions of the slice 110 of the next layer of the two adjacent layers of slices 110 and the multiple layers of slices 110 after the next layer of the slice 110 are taken as the cross-sectional mutation site 101, that is, the slice 110 of the next layer of the two adjacent layers of slices 110 and the multiple layers of slices 110 after the next layer of the slice 110 are taken as the cross-sectional mutation site 101. 10 are all the target slices 110a; if the cross-sectional area of ​​the latter slice 110 of two adjacent layers of the slices 110 is smaller than the cross-sectional area of ​​the former slice 110, the positions of the former slice 110 of the two adjacent layers of the slices 110 and the several layers of the slices 110 before the former slice 110 are taken as the mutation site 101, that is, the former slice 110 of the two adjacent layers of the slices 110 and the several layers of the slices 110 before the former slice 110 are all the target slice 110a.

[0066] In addition, when the judgment result of step S23 is no, the slice 110 with the smaller area of ​​the two adjacent slices 110 is used as the reference slice 110b corresponding to the cross-sectional mutation site 101 where the slice 110 with the larger cross-sectional area is located (e.g. Figure 5 shown).

[0067] The first preset value and the second preset value are set according to actual conditions, but the two are reciprocal to each other, that is, when the first preset value is 1 / n, the second preset value is n, and n is greater than 1. In other words, "whether the ratio of the cross-sectional areas of the two adjacent layers of the slices 110 is greater than or equal to the first preset value and less than or equal to the second preset value" actually refers to whether the deviation of the cross-sectional areas of the two adjacent layers of the slices 110 is greater than n times. When the ratio of the cross-sectional areas of the two adjacent layers of the slices 110 is greater than or equal to the first preset value and less than or equal to the second preset value, it indicates that the deviation of the cross-sectional areas of the two adjacent layers of the slices 110 is less than or equal to n times, and when the ratio of the cross-sectional areas of the two adjacent layers of the slices 110 is less than the first preset value or greater than the second preset value, it indicates that the deviation of the cross-sectional areas of the two adjacent layers of the slices 110 is greater than n times. Optionally, n is greater than or equal to 2, preferably n is greater than or equal to 5, and more preferably n is greater than or equal to 10.

[0068] It should also be noted that the specific number of layers of the target slices 101a in the cross-sectional mutation site 101 is determined by those skilled in the art based on the properties of the raw materials used to manufacture the workpiece and the specific deviation of the cross-sectional areas of two adjacent layers of the slices 110. Generally speaking, the greater the deviation of the cross-sectional areas of two adjacent layers of the slices 110, the more layers of the target slices 101a included in the first cross-sectional mutation site 101.

[0069] It can be understood that after the cross-sectional mutation site 101 is determined, the other sites on the process model 100 are the non-mutation sites.

[0070] In the step S30, the number of the first regions 111 is determined according to the shape of the target slice 110. In practice, the number of the first regions 111 is one or two.

[0071] Specifically, when the target slice 110 is Figure 7 and Figure 8 In the case of a solid structure as shown, the number of the first region 111 is one, and the first region 111 surrounds the periphery of the target slice 110. Thus, the edge of the first region 111 away from the second region 112 is on the outer surface of the process model 100. Fig. 9 and Fig.10In the case of the annular structure shown, the number of the first regions 111 is two, and the two first regions 111 are respectively arranged at the inner periphery and the outer periphery of the second region 112, so that the two first regions 111 jointly surround the second region 112. The edge of the first region 111 surrounding the outer periphery of the second region 112 away from the second region 112 is on the outer surface of the process model 100, and the edge of the first region 111 surrounding the inner periphery of the second region 112 away from the second region 112 is on the inner periphery of the process model 100.

[0072] The area of ​​the first region 111 is equivalent to the cross-sectional area of ​​the reference slice 110b of the cross-sectional mutation site 101 where the first region 111 is located. For example, along the molding direction, the deviation between the cross-sectional area of ​​the slice 110 of the p-1 layer and the cross-sectional area of ​​the slice 110 of the p layer is greater than n times, and the cross-sectional area of ​​the slice 110 of the p layer is greater than the cross-sectional area of ​​the slice 110 of the p-1 layer, then a cross-sectional mutation site 101 corresponding to the slice 110 of the p layer includes the slice 110 of the p layer and the slices 110 of the j layers thereafter, that is, along the molding direction, the cross-sectional mutation site 101 extends backward from the slice 110 of the p layer to the slice 110 of the q layer, and q is equal to the sum of p and j, p and q are both integers greater than 1, and j is a positive integer greater than or equal to 0. Therefore, the slice 110 of the pth layer and the slice 110 of the jth layer thereafter are the target slices 110a of the cross-sectional mutation site 101, and the slice 110 of the p-1th layer is the reference slice 110b of the cross-sectional mutation site 101. Therefore, for the cross-sectional mutation site 101, the area of ​​the first region 111 thereon is equivalent to the cross-sectional area of ​​the slice 110 of the p-1th layer. Alternatively, along the forming direction, the deviation between the cross-sectional area of ​​the slice 110 of the p-1 layer and the cross-sectional area of ​​the slice 110 of the p-1 layer is greater than n times, and the cross-sectional area of ​​the slice 110 of the p-1 layer is smaller than the cross-sectional area of ​​the slice 110 of the p-1 layer, then a cross-sectional mutation site 101 corresponding to the slice 110 of the p-1 layer includes the slice 110 of the p-1 layer and the slices 110 of the j layers before it, that is, along the forming direction, the cross-sectional mutation site 101 extends forward from the slice 110 of the p-1 layer to the slice 110 of the q layer, and q is equal to the difference between p and j, p and q are both integers greater than 1, and j is a positive integer greater than or equal to 0. Therefore, the slice 110 of the p-1 layer and the slices 110 of the j layers before it are the target slices 110a of the cross-sectional mutation site 101, and the slice 110 of the p layer is the reference slice 110b of the cross-sectional mutation site 101. Therefore, for the cross-sectional sudden change portion 101, the area of ​​the first region 111 thereon is equivalent to the cross-sectional area of ​​the p-th layer of the slice 110. In this way, the generation of shrinkage lines on the surface of the workpiece can be effectively avoided.

[0073] In the embodiment of the present invention, the “area of ​​the first region 111 is equivalent to the cross-sectional area of ​​the reference slice 110b of the cross-sectional mutation site 101 where the first region 111 is located” means that the ratio of the area of ​​the first region 111 to the cross-sectional area of ​​the reference slice 110b of the cross-sectional mutation site 101 where the first region 111 is located is not less than 1 / m and not greater than m, m is greater than 1, and m is less than n. Specifically in the above embodiment, when the cross-sectional mutation site 101 includes the slice 110 of the p-th layer and the j-th layer of the slice 110 thereafter, the ratio of the area of ​​the first region 111 on each layer of the target slice 110a of the cross-sectional mutation site 101 to the cross-sectional area of ​​the slice 110 of the p-1th layer is greater than or equal to 1 / m and less than or equal to m. When the cross-sectional protrusion 101 includes the slice 110 of the p-1 layer and the slice 110 of the j layers before it, the ratio of the area of ​​the first region 111 on each layer of the target slice 110a of the cross-sectional mutation 101 to the cross-sectional area of ​​the slice 110 of the p layer is greater than or equal to 1 / m and less than or equal to m. In practice, m may be less than or equal to n / 2, for example, when n is 10, m may be 5, 4, 3, 2, 1 or any other suitable number less than 5, and m is preferably 1 or 2.

[0074] Optionally, when the target slice 110a is Figure 7 and Figure 8 In the case of a solid structure as shown, the second region 112 is entirely the flexible region 112a (eg Figure 7 Alternatively, the second region 112 includes the flexible region 112a and the non-flexible region 112b (as shown in Fig. 9 ), the inflexible area 112b is located on the side of the flexible area 112a away from the first area 111. In the process of performing the step S40, when printing the inflexible area 112b, the energy source may be operated based on the first scanning path filling strategy, so that the filling density of the inflexible area 112b of the workpiece is the same as the filling density of the non-cross-sectional mutation part of the workpiece and the first area 111. Alternatively, when printing the inflexible area 112b of the workpiece, the energy source is operated with a third scanning path filling strategy different from the first scanning path filling strategy, so that the filling density of the inflexible area 112b of the workpiece is different from the filling density of the first area 111 and the non-cross-sectional mutation part of the workpiece.

[0075] When the target slice 110a is Fig. 9 and Fig.10 In the case of the annular structure shown in FIG. 1 , the second region 112 is the entire flexible region 112a (eg, Fig. 9As shown), or the second region 112 includes two flexible regions 112a and one connecting region 112c (as shown Fig.10 As shown in FIG. 4 ), the connection area 112c is located between the two flexible areas 112a, so that one of the flexible areas 112a is located on the inner side of the connection area 112c and is adjacent to the first area 111 surrounded by the inner periphery of the second area 112, and the other flexible area 112a is located on the outer side of the connection area 112c and is adjacent to the first area 111 surrounded by the outer periphery of the second area 112. During the execution of step S40, when printing the connection area 112c of the workpiece, the energy source may be operated based on the first scanning path filling strategy so that the filling density of the connection area 112c of the workpiece is the same as the filling density of the non-cross-sectional mutation site and the first area 111 of the workpiece. Alternatively, when printing the connection area 112c, the energy source is operated with a third scanning path filling strategy different from the first scanning path filling strategy so that the filling density of the connection area 112c of the workpiece is different from the filling density of the first area 111 and the non-cross-sectional mutation site of the workpiece.

[0076] In the step S40, the scanning path in the first scanning path filling strategy may have any suitable form, for example, it may be a straight path, a curved path, a broken line path, or a dot matrix path, which is not limited in the embodiment of the present invention.

[0077] The scanning path in the second scanning path filling strategy is a non-linear path, which may be a dot matrix path, a curved path, or a broken line path.

[0078] It can be understood that when the scanning path is a dot matrix path, the energy source forms a weld on a corresponding area of ​​the workpiece after printing the corresponding area of ​​the workpiece. The filling density refers to the percentage of the total area of ​​all welds in the scanning area to the area of ​​the corresponding scanning area. For example, when the first scanning path is a dot matrix path, for a first area 111, the filling density of the first scanning filling path is the percentage of the total area of ​​all welds on the first area 111 to the area of ​​the corresponding first area 111. When the scanning path is a curved path or a broken line path, the energy source forms a weld on the area after printing the corresponding area of ​​the workpiece. The filling density refers to the percentage of the total area of ​​all welds in the scanning area to the area of ​​the corresponding scanning area. For example, for a flexible area 112a, the filling density of the second scanning filling path is the percentage of the total area of ​​all welds on the flexible area 112a to the area of ​​the corresponding flexible area 112a.

[0079] When the scanning path in the second scanning path filling strategy is a dot matrix path, during the execution of step S40, when printing different target slices 110a of the cross-sectional mutation site 101 of the workpiece, along the molding direction, the density of the dot matrix in the second scanning path filling strategy gradually increases, so that the filling density of the flexible area 112a of each target slice 110a of the same cross-sectional mutation site 101 of the workpiece gradually increases along the molding direction. In addition, for the first layer of the target slice 110a of the cross-sectional mutation site 101, the distance between two adjacent points in the dot matrix path of the second scanning path strategy should be greater than or equal to 0.15mm, and the filling density should not be greater than 45%, so as to ensure that the flexible area 112a of the first layer of the target slice 110a has sufficient flexibility.

[0080] When the scanning path in the second scanning path filling strategy is a curved path or a broken line path, during the execution of step S40, when printing different target slices 110a of the cross-sectional mutation site 101 of the workpiece, along the forming direction, the width of the scanning path in the second scanning path filling strategy gradually increases, and / or the number of scanning paths in the second scanning path filling strategy gradually increases, so that the filling density of the flexible area 112a of each target slice 110a of the same cross-sectional mutation site 101 of the workpiece gradually increases along the forming method.

[0081] In addition, for the first layer of the target slice 110a at the cross-sectional mutation site 101, the distance between two adjacent scanning paths in the second scanning path strategy is greater than or equal to 0.15 mm, and the width of each scanning path is approximately 0.15 mm.

[0082] In the embodiment of the present invention, the optional curved path includes but is not limited to at least one of an S-shaped path and a spiral path, and the optional broken line path includes but is not limited to at least one of a Z-shaped path and a W-shaped path.

[0083] Furthermore, the present invention also provides a 3D printing device, the 3D printing device comprising a control unit and an energy source, the control unit is communicatively connected to the energy source and is configured to perform the 3D printing method as described above. The energy source includes but is not limited to any one of an electron beam generator and a laser.

[0084] Furthermore, the present invention also provides a computer-readable storage medium, on which a program is stored, and when the program is executed, the 3D printing method as described above is executed.

[0085] Furthermore, the present invention also provides a workpiece, the workpiece has a cross-sectional mutation feature, and the workpiece is printed by the aforementioned 3D printing method. Thus, the filling density of the flexible area 112a of the cross-sectional mutation site 101 on the workpiece is less than the filling density of the non-cross-sectional mutation site and the first area 111 of the cross-sectional mutation site 101, and on one cross-sectional mutation site 101, the filling density of the flexible area 112a of different target slices 110a gradually increases along the molding direction.

[0086] Although the present invention is disclosed as above, it is not limited thereto. Those skilled in the art may make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A 3D printing method, characterized in that: include: The process model of the workpiece is sliced ​​in layers along the forming direction; Determining a cross-sectional mutation location on the process model, wherein the cross-sectional mutation location includes at least one layer of the slice; A second region and at least one first region are divided on the slice at the cross-sectional mutation site, all the first regions jointly surround the second region, and edges of the first regions away from the second regions are located on the surface of the process model; the second region includes a flexible region, and the flexible region is adjacent to the first region; as well as, Controlling the energy source to operate and printing layer by layer along the forming direction until the workpiece is formed; When printing other parts of the workpiece except the cross-sectional mutation site and the first area, the energy source operates based on the first scanning path filling strategy, and when printing the flexible area of ​​the workpiece, the energy source operates based on the second scanning path filling strategy. The filling density of the first scanning path filling strategy is greater than the filling density of the second scanning path filling strategy, and when printing different slices of the cross-sectional mutation site of the workpiece, the filling density of the second scanning path filling strategy gradually increases along the forming direction.

2. The 3D printing method according to claim 1, characterized in that: The step of determining the cross-section mutation location on the process model comprises: Obtaining the cross-sectional area of ​​each slice; Obtaining a ratio of the cross-sectional areas of two adjacent slices; Determine whether the ratio of the cross-sectional areas of two adjacent layers of the slices is greater than or equal to 1 / n and less than or equal to n. If not, take the slice with the larger cross-sectional area among the two adjacent layers of the slices as the cross-sectional mutation site, or take the slice with the larger cross-sectional area among the two adjacent layers of the slices and several layers of the slices located on one side of the slice with the larger cross-sectional area away from the slice with the smaller cross-sectional area as the cross-sectional mutation site; n is greater than 1.

3. The 3D printing method according to claim 1 or 2, characterized in that: The scanning path of the second scanning path filling strategy is a curved path or a broken line path; When printing different slices of the cross-sectional mutation location of the workpiece, the width of the scanning path of the second scanning path filling strategy gradually increases along the forming direction, and / or the number of scanning paths of the second scanning path filling strategy gradually increases along the forming direction.

4. The 3D printing method according to claim 1 or 2, characterized in that: The scanning path of the second scanning path filling strategy is a dot matrix path, and when printing different slices of the cross-sectional mutation portion of the workpiece, the dot matrix density of the dot matrix path gradually increases along the forming direction.

5. The 3D printing method according to claim 2, characterized in that: When the slice at the cross-section mutation site is a solid structure, the number of the first region is one; the first region is arranged around the periphery of the second region, and an edge of the first region away from the second region is on the outer surface of the process model; When the slice at the cross-sectional mutation site is a hollow annular structure, the number of the first regions is two; one of the two first regions is arranged on the outer periphery of the second region, and the other is arranged on the inner periphery of the second region, and an edge of the first region arranged on the outer periphery of the second region away from the second region is on the outer surface of the process model, and an edge of the first region arranged on the inner periphery of the second region away from the second region is on the inner surface of the process model.

6. The 3D printing method according to claim 2 or 5, characterized in that: When the ratio of the cross-sectional areas of two adjacent layers of the slices is less than 1 / n or greater than n, the slice with the smaller area among the two adjacent layers of the slices is used as the reference slice of the corresponding cross-sectional mutation site; the ratio of the area of ​​any first region to the cross-sectional area of ​​the reference slice corresponding to the cross-sectional mutation site where the first region is located is greater than or equal to 1 / m and less than or equal to m, and m is greater than 1 and less than n.

7. The 3D printing method according to claim 5, characterized in that: When the slice at the cross-sectional mutation site is an annular structure, the second region includes two flexible regions and one connecting region, and each flexible region is located between one of the first regions and the connecting region.

8. A 3D printing device, characterized in that: It comprises a control unit and an energy source, wherein the control unit is communicatively connected with the energy source and is configured to execute the 3D printing method as described in any one of claims 1 to 7.

9. A computer-readable storage medium having a program stored thereon, characterized in that: When the program is executed, the 3D printing method according to any one of claims 1 to 7 is performed.

10. A workpiece, characterized in that: The workpiece is printed by the 3D printing method according to any one of claims 1 to 7.