Wafer laser cutting method and system
The modified layer and hidden tangent line are formed inside the wafer through the Bessel beam, and combined with the high-speed three-dimensional displacement stage and spatial light modulator, it solves the problems of material waste and insufficient equipment flexibility of the traditional cutting method, and achieves high efficiency, Precise wafer cutting, suitable for wafer processing of various materials and thicknesses.
Patent Information
- Application Number
- CN202411303414.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-19
- Publication Date
- 2024-10-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional mechanical cutting or chemical etching methods in chip manufacturing lead to easy cracking and chipping of the wafer edges, and the wide cutting path leads to material waste, affecting processing efficiency and yield. The existing ultra-short pulse laser stealth cutting process has deficiencies in equipment flexibility and stability, and is difficult to adapt to the processing of different wafer materials and thicknesses.
Bessel beam is used for laser cutting. By forming a modified layer and hidden tangent line inside the wafer, and using a high-speed three-dimensional displacement stage and a spatial light modulator to optimize the laser parameters, it achieves efficient cutting in a single laser scan. Combined with the blue film Protective and mechanical splitting device for precise separation.
It improves the processing efficiency and cutting accuracy of wafers, overcomes the problems of material waste and insufficient equipment flexibility of traditional methods, achieves efficient cutting of wafers of various materials and thicknesses, and improves the application flexibility and stability of the equipment. sex.
Smart Images

Figure CN118808941A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of wafer cutting technology, and in particular to a wafer laser cutting method. The present invention also relates to a wafer laser cutting system applied to the wafer laser cutting method. Background Art
[0002] With the rapid development of the global chip manufacturing industry, the requirements for the precision, efficiency and yield of semiconductor wafer processing technology have reached an unprecedented level. As one of the key links in the chip manufacturing process, the improvement and innovation of the wafer cutting process is directly related to the performance and cost of the final product. In the pursuit of more sophisticated and higher-integrated chip manufacturing, traditional mechanical cutting or chemical etching cutting methods have gradually revealed their limitations. For example, cracks and edge collapse are prone to occur at the edge of the wafer, which not only affects the electrical performance of the chip, but also increases the scrap rate. At the same time, the wider cutting path also limits the effective utilization of the wafer and increases the material cost.
[0003] In this context, ultrashort pulse laser stealth cutting technology came into being. The existing ultrashort pulse laser stealth cutting process uses Gaussian laser for stealth cutting, and focuses the laser tightly inside the wafer through a high numerical aperture objective lens. However, the small focal depth of this process limits the depth of modification, and requires a layered multiple scanning method, which greatly affects the processing efficiency. Bessel beams have the characteristics of long-distance non-diffraction transmission. The energy of their main lobe can remain basically unchanged over a long distance. They have an extremely long focal depth and can achieve stealth cutting of silicon carbide wafers with a single laser scan. The method of using an axicon lens to generate a Bessel beam for stealth cutting of wafers can greatly improve the efficiency of stealth cutting. However, when the type and thickness of the wafer change, the optical components in the equipment need to be replaced and debugged, which puts forward high technical requirements for the installation and debugging of the equipment, affects the flexibility and stability of the equipment application, and is not conducive to improving the processing efficiency of wafers. Summary of the invention
[0004] In view of this, the present invention aims to provide a wafer laser cutting method to improve the processing efficiency of wafers.
[0005] To achieve the above object, the technical solution of the present invention is achieved as follows: A wafer laser cutting method is used for cutting and separating wafers, the method comprising: Fixing the wafer in a film frame, and fixing the film frame on a stage; Set laser processing parameters to generate Bessel laser; Adjusting the stage so that the laser is incident from the front side of the wafer, and positioning the processing position; Performing laser cutting on the wafer to form a modified layer and hidden cutting lines inside the wafer; A protective film is applied to the front side of the wafer after laser cutting; The coated wafer is fixed on a mechanical splitting device, and the wafer is separated along the hidden tangent line direction of the wafer.
[0006] Furthermore, the step of fixing the wafer in a film frame and fixing the film frame on a stage further includes: Pasting the back side of the wafer onto the blue film; The blue film is tightened and assembled in the film frame, and the film frame is fixed on the stage.
[0007] Furthermore, the stage is a stage of a high-speed three-dimensional translation stage.
[0008] Furthermore, the laser cutting of the wafer to form a modified layer and a hidden cutting line inside the wafer also includes: Controlling the high-speed three-dimensional translation stage to move the stage along the Z direction to focus the laser on a predetermined depth inside the wafer; The high-speed three-dimensional translation stage is controlled to move the stage along the X-direction and the Y-direction at a preset speed and direction to form a modified layer and a hidden cut line in the wafer.
[0009] Furthermore, the laser cutting of the wafer to form a modified layer and a hidden cutting line inside the wafer also includes: A surface image of the wafer is acquired to monitor the cutting process of the wafer.
[0010] Furthermore, the wavelength range of the laser is 800nm-1200nm, the pulse width range of the laser is 50fs-20ps, the repetition frequency range of the laser is 10kHz-100kHz, and the scanning speed range of the laser is 100mm / s-1000mm / s.
[0011] Furthermore, the setting of laser processing parameters also includes: A holographic phase spectrum is loaded into a spatial light modulator, and the focal depth of the laser is jointly regulated by the holographic phase spectrum and objective lens parameters.
[0012] Furthermore, the wafer is made of any one of silicon, silicon carbide, glass, aluminum nitride, gallium nitride, zinc oxide, diamond or sapphire.
[0013] Furthermore, the thickness of the wafer ranges from 350 μm to 1000 μm.
[0014] Compared with the prior art, the present invention has the following advantages: The wafer laser cutting method described in the present invention optimizes the laser cutting steps and utilizes the long focal depth of the Bessel light beam to focus the Bessel focus as a whole on the inside of the wafer to be processed, so that a single laser scan can achieve a sufficient depth of the modified layer, thereby overcoming the problem that the Gaussian light beam needs to be scanned in layers multiple times to achieve invisible cutting, thereby greatly improving the processing efficiency.
[0015] By sticking the back of the wafer on the blue film, it helps to protect the surface of the wafer from scratches, and helps to improve the accuracy and consistency of cutting, facilitates operation, and is easy to peel off after processing, which can improve processing efficiency.
[0016] The high-speed three-dimensional translation stage makes it easy to adjust the spatial position of the wafer, thereby facilitating the adjustment of the processing position of the wafer and facilitating the implementation of the design.
[0017] After the laser is focused on the preset depth of the wafer, the processing direction of the wafer is adjusted, which is beneficial to the processing process of the wafer and the design implementation.
[0018] Acquiring the surface image of the wafer is conducive to monitoring the processing and cutting process of the wafer, helping to observe the processing status of the wafer, and facilitating design implementation.
[0019] By loading a holographic phase spectrum into a spatial light modulator to generate a Bessel beam, the flexibility of the wafer laser cutting method can be improved, enabling the wafer laser cutting method to be able to process wafers of various materials and thicknesses.
[0020] The present invention also provides a wafer laser cutting system, comprising: An ultrashort pulse laser, wherein the ultrashort pulse laser can output ultrashort pulse laser with Gaussian distribution; An optical path adjustment component, wherein the optical path adjustment component is capable of adjusting the optical path of the ultrashort pulse laser generated by the ultrashort pulse laser; A beam shaping component, wherein the beam shaping component is capable of adjusting an ultrashort pulse laser to generate a Bessel beam; A focusing component, wherein the focusing component is capable of focusing the laser beam shaped by the beam shaping component; An imaging component capable of providing an image of the surface of the wafer; A motion component, wherein the motion component is capable of carrying out the movement of the wafer; A control unit is configured to control the actions of the ultrashort pulse laser, the beam shaping component and the motion component.
[0021] The wafer laser cutting system described in the present invention has the same beneficial effects as the wafer laser cutting method described above compared to the prior art, so it will not be described in detail here. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings: Figure 1 This is a flow chart of a wafer laser cutting method according to an embodiment of the present invention; Figure 2 It is a schematic structural diagram of a wafer laser cutting system according to an embodiment of the present invention; Description of reference numerals: 1. Control unit; 2. Ultrashort pulse laser; 3. First reflector; 4. Optical shutter; 5. Beam expander; 6. Second reflector; 7. Third reflector; 8. Spatial light modulator; 9. Plano-convex lens; 10. First dichroic mirror; 11. Objective lens; 12. Wafer to be processed; 13. High-speed three-dimensional translation stage; 14. Second dichroic mirror; 15. Illumination light source; 16. CCD camera. DETAILED DESCRIPTION
[0023] In the following description, specific details such as specific system structures, technologies, etc. are provided for the purpose of illustration rather than limitation, so as to provide a thorough understanding of the embodiments of the present application. However, it should be clear to those skilled in the art that the present application may also be implemented in other embodiments without these specific details. In other cases, detailed descriptions of well-known systems, devices, circuits, and methods are omitted to prevent unnecessary details from obstructing the description of the present application.
[0024] It should be understood that when used in the present specification and the appended claims, the term "comprising" indicates the presence of described features, wholes, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components and / or combinations thereof.
[0025] It should also be understood that the term “and / or” used in the specification and appended claims refers to any and all possible combinations of one or more of the associated listed items, and includes these combinations.
[0026] As used in the specification and appended claims of this application, the term "if" can be interpreted as "when" or "uponce" or "in response to determining" or "in response to detecting", depending on the context. Similarly, the phrase "if it is determined" or "if [described condition or event] is detected" can be interpreted as meaning "uponce it is determined" or "in response to determining" or "uponce [described condition or event] is detected" or "in response to detecting [described condition or event]", depending on the context.
[0027] In addition, in the description of the present application specification and the appended claims, the terms "first", "second", "third", etc. are only used to distinguish the descriptions and cannot be understood as indicating or implying relative importance.
[0028] References to "one embodiment" or "some embodiments" etc. described in the specification of this application mean that one or more embodiments of the present application include specific features, structures or characteristics described in conjunction with the embodiment. Therefore, the statements "in one embodiment", "in some embodiments", "in some other embodiments", "in some other embodiments", etc. that appear in different places in this specification do not necessarily refer to the same embodiment, but mean "one or more but not all embodiments", unless otherwise specifically emphasized in other ways. The terms "including", "comprising", "having" and their variations all mean "including but not limited to", unless otherwise specifically emphasized in other ways.
[0029] The present invention will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments.
[0030] Embodiment 1 The present embodiment relates to a wafer laser cutting method, which is useful for improving wafer processing efficiency by optimizing the laser cutting steps.
[0031] Before introducing the wafer laser cutting method in this embodiment, it is necessary to briefly introduce some concepts involved in this embodiment. The wafer laser cutting in this embodiment refers to focusing the laser focus inside the wafer to form a modified layer by laser to facilitate the wafer splitting. The wafer laser cutting method in this embodiment optimizes the laser cutting steps and utilizes the characteristics of the long focal depth of the Bessel beam to focus the Bessel focus as a whole inside the wafer to be processed, so that a single laser scan can achieve sufficient depth of the modified layer, overcoming the problem that the Gaussian beam needs to be layered and scanned multiple times to achieve invisible cutting, greatly improving the processing efficiency.
[0032] In terms of overall thinking, Figure 1 As shown, the wafer laser cutting method in this embodiment includes: Step S1, fixing the wafer in a film frame, and fixing the film frame on a stage.
[0033] Wherein, in step S1, the wafer is made of any one of silicon (Si), silicon carbide (SiC), glass, aluminum nitride (AlN), gallium nitride (GaN), zinc oxide (ZnO), diamond or sapphire, and the thickness of the wafer ranges from 350μm to 1000μm. The wafer is fixed in the film frame and the film frame is fixed on the stage, which is conducive to maintaining the position of the wafer on the stage through the film frame, and protecting the wafer through the film frame to avoid scratches. Specifically, the following steps are also included: Step S11, attaching the back side of the wafer to the blue film.
[0034] Among them, in this step S11, by sticking the back side of the wafer on the blue film, it is beneficial to protect the surface of the wafer from scratches, and helps to improve the cutting accuracy and consistency, facilitate operation, and facilitate peeling after processing, which can improve processing efficiency.
[0035] Step S12, tighten the blue film and install it in the film frame, and fix the film frame on the stage.
[0036] Among them, in this step S12, the stage is a stage of a high-speed three-dimensional translation stage, and the high-speed three-dimensional translation stage is used to facilitate the adjustment of the spatial position of the wafer, thereby facilitating the adjustment of the processing position of the wafer and facilitating the design implementation.
[0037] Step S2, setting laser processing parameters to generate Bessel laser.
[0038] Wherein, in step S2, the wavelength range of the laser is 800nm-1200nm, the pulse width range of the laser is 50fs-20ps, the repetition frequency range of the laser is 10kHz-100kHz, the scanning speed range of the laser is 100mm / s-1000mm / s, and the following steps are also included: Step S21, loading the holographic phase spectrum into the spatial light modulator, and the focal depth of the laser is jointly controlled by the holographic phase spectrum and the objective lens parameters.
[0039] Among them, in step S21, the Bessel beam is generated by loading the holographic phase spectrum in the spatial light modulator, which can improve the flexibility of the wafer laser cutting method and enable the wafer laser cutting method to be able to process wafers of various materials and thicknesses.
[0040] Step S3, adjusting the stage so that the laser is incident from the front side of the wafer, and positioning the processing position.
[0041] Among them, in step S3, when positioning the processing position, the height of the wafer is first adjusted to focus the laser at a preset depth inside the wafer, and then the processing direction of the wafer is adjusted. Specifically, the following steps are also included: Step S31 , controlling the high-speed three-dimensional translation stage to move the stage along the Z direction, so as to focus the laser on a predetermined depth inside the wafer.
[0042] Step S32, controlling the high-speed three-dimensional translation stage to move the stage along the X-direction and the Y-direction at a preset speed and direction to form a modified layer and a hidden cut line in the wafer.
[0043] Among them, in step S31 and step S32, after the focus of the laser is focused on the preset depth of the wafer, the processing direction of the wafer is adjusted, which is beneficial to the processing process of the wafer and the design implementation.
[0044] Step S4: laser cutting the wafer to form a modified layer and hidden cutting lines inside the wafer.
[0045] Among them, in step S4, when the wafer is laser cut, the surface image of the wafer can also be obtained to monitor the processing process of the wafer. The device for obtaining the image can be, for example, a CCD camera. Obtaining the surface image of the wafer is conducive to monitoring the processing and cutting process of the wafer, helping to observe the processing status of the wafer, and facilitating design implementation. Step S4 also includes the following steps: Step S5, applying a protective film to the front side of the wafer after laser cutting.
[0046] In step S5, a protective film is applied to the front side of the wafer to protect the surface of the wafer from scratches during the subsequent mechanical splitting process.
[0047] Step S6, fixing the coated wafer on a mechanical splitting device, and separating the wafer along the hidden tangent line direction of the wafer.
[0048] In this step S6, the wafer can be split into pieces after laser cutting by a mechanical splitting device, thereby obtaining the split wafers.
[0049] Specifically, in this embodiment, for example, a 6-inch 500 um thick conductive 4H-SiC wafer can be used as the wafer to be processed.
[0050] The back of the cleaned 4H-SiC wafer is glued to the blue film, the blue film is stretched on the film frame, and the front side is fixed in the card slot of the high-speed three-dimensional translation stage with the front side facing up. The
[1120] and
[1100] crystal directions of the wafer are aligned with the X-axis movement direction and the Y-axis movement direction respectively.
[0051] The laser processing parameters are set as follows: pulse width of 270fs, repetition frequency of 50kHz, and laser power of 4W; the holographic phase map is loaded into the spatial light modulator, and the focal depth of the Bessel beam after being focused by the objective lens is about 250um.
[0052] The processing position of the high-speed three-dimensional translation stage is adjusted by the image of the wafer surface. After positioning at the processing position, the focus of the focused Bessel beam is embedded in the interior of the wafer. The top of the focus is 50um away from the surface of the wafer. The laser scanning path is set, the laser scanning speed is set to 500mm / s, and the wafer is laser cut according to the set program.
[0053] After the laser cutting process is completed, turn off the related equipment for laser cutting, cover the front of the cut wafer with a protective film, and fix the film frame on a mechanical splitting device. Use the visual system of the mechanical splitting device to locate the position of the hidden cutting line, and perform mechanical splitting along the direction of the hidden cutting line to achieve the splitting of the cut wafer.
[0054] The wafer laser cutting method in this embodiment optimizes the laser cutting steps, utilizes the long focal depth of the Bessel beam, and focuses the Bessel focus as a whole on the inside of the wafer to be processed, so that a single laser scan can achieve sufficient depth of the modified layer, overcoming the problem that the Gaussian beam needs to be layered and scanned multiple times to achieve invisible cutting, greatly improving the processing efficiency. At the same time, the flexibility of the laser cutting system is improved, so that the method can process wafers of various materials and thicknesses, and solves the disadvantages of the previous Bessel laser invisible cutting that requires the replacement of optical components and debugging of optical paths when changing the wafer material and thickness.
[0055] Embodiment 2 This embodiment relates to a wafer laser cutting system. The wafer laser cutting system in this embodiment is applied to the wafer laser cutting method in the first embodiment.
[0056] Specifically, the wafer laser cutting system in this embodiment includes an ultrashort pulse laser 2, an optical path adjustment component, a beam shaping component, a focusing component, an imaging component, a motion component and a control unit 1.
[0057] Among them, the ultrashort pulse laser 2 can output ultrashort pulse laser with Gaussian distribution. The optical path adjustment component can adjust the optical path of the ultrashort pulse laser generated by the ultrashort pulse laser 2. The beam shaping component can adjust the ultrashort pulse laser to generate a Bessel beam. The focusing component can focus the laser shaped by the beam shaping component. The imaging component can provide an image of the surface of the wafer 12. The motion component can undertake the movement of the wafer 12. The control unit 1 is configured to be able to control the actions of the ultrashort pulse laser, the beam shaping component and the motion component.
[0058] In more detail, the optical path adjustment component in this embodiment includes a first reflector 3, an optical gate 4, a beam expander 5, a second reflector 6 and a third reflector 7. The ultrashort pulse laser 2 outputs an ultrashort pulse laser with a Gaussian distribution, which is reflected to the optical gate 4 by the first reflector 3, then expanded by the beam expander 5, and then reflected to the beam shaping component by the second reflector 6 and the third reflector 7.
[0059] The beam shaping component in this embodiment includes a reflective spatial light modulator 8 and a plano-convex lens 9. The reflective spatial light modulator 8 can convert a Gaussian-distributed ultrashort pulse laser into a Bessel beam. The Bessel beam is converged or collimated by the plano-convex lens 9 and then reflected to the focusing component.
[0060] The focusing assembly in this embodiment includes a first dichroic mirror 10 and an objective lens 11 . The Bessel light beam is reflected by the first dichroic mirror 10 into the objective lens 11 and irradiates onto a wafer 12 on the stage.
[0061] The imaging component in this embodiment includes an illumination light source 15, a second dichroic mirror 14 and a CCD camera 16. The light of the illumination light source 15 passes through the second dichroic mirror 14, the first dichroic mirror 10 and the objective lens 11 to irradiate the surface of the wafer 12 to provide illumination for the CCD camera 16. The CCD camera 16 observes the image of the laser cutting process through the first dichroic mirror 10 and the second dichroic mirror 14 to monitor the laser cutting process of the wafer.
[0062] In more detail, the CCD camera 16, the illumination light source 15 and the laser beam are coaxially calibrated to ensure the accuracy of the imaging position of the imaging component. When in use, images of different focus depths are obtained by the CCD camera 16 to determine whether the focal length of the Bessel beam meets the requirements for cutting the wafer 12.
[0063] The motion assembly in this embodiment includes a high-speed three-dimensional displacement stage 13 having an X-axis motion platform, a Y-axis motion platform, a Z-axis motion platform and a stage, and the stage has a slot for fixing the film frame.
[0064] The control unit 1 in this embodiment is electrically connected to the ultrashort pulse laser 2, the high-speed three-dimensional translation stage 13 and the CCD camera 16. The ultrashort pulse laser 2 can be started and shut down by the control unit 1. The spatial position of the wafer 12 can be adjusted on the high-speed three-dimensional translation stage 13 by the control unit 1. The image information obtained by the CCD camera 16 is processed by the control system.
[0065] The wafer laser cutting system of this embodiment, by applying the wafer laser cutting method in the first embodiment, utilizes the long focal depth of the Bessel beam to focus the Bessel focus as a whole on the inside of the wafer 12 to be processed, so that a single laser scan can achieve a sufficient depth of the modified layer, overcoming the problem that the Gaussian beam needs to be layered and scanned multiple times to achieve invisible cutting, greatly improving the processing efficiency. At the same time, the method of using the spatial light modulator 8 to perform beam shaping to generate the Bessel beam improves the flexibility of the laser invisible cutting system, enabling it to process wafers of various materials and thicknesses, and solves the disadvantages of the previous Bessel laser invisible cutting that the optical components need to be replaced and the optical path needs to be debugged when the wafer material and thickness are changed.
[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A wafer laser cutting method for cutting and separating wafers, characterized in that: The method includes: Fixing the wafer in a film frame, and fixing the film frame on a stage; Setting laser processing parameters, loading a holographic phase map in a spatial light modulator, the focal depth of the laser is jointly controlled by the holographic phase map and objective lens parameters, and Bessel laser is generated, wherein the wavelength range of the laser is 800nm-1200nm, the pulse width range of the laser is 50fs-20ps, the repetition frequency range of the laser is 10kHz-100kHz, and the scanning speed range of the laser is 100mm / s-1000mm / s; Acquiring a surface image of the wafer to monitor a cutting process of the wafer; Adjusting the stage so that the laser is incident from the front side of the wafer, and positioning the processing position; Performing laser cutting on the wafer to form a modified layer and hidden cutting lines inside the wafer; A protective film is applied to the front side of the wafer after laser cutting; The coated wafer is fixed on a mechanical splitting device, and the wafer is separated along the hidden tangent line direction of the wafer.
2. The wafer laser cutting method according to claim 1, characterized in that: The method of fixing the wafer in a film frame and fixing the film frame on a stage further comprises: Pasting the back side of the wafer onto the blue film; The blue film is tightened and assembled in the film frame, and the film frame is fixed on the stage.
3. The wafer laser cutting method according to claim 2, characterized in that: The object stage is a high-speed three-dimensional translation stage.
4. The wafer laser cutting method according to claim 3, characterized in that: The laser cutting of the wafer to form a modified layer and a hidden cutting line inside the wafer also includes: Controlling the high-speed three-dimensional translation stage to move the stage along the Z direction to focus the laser on a predetermined depth inside the wafer; The high-speed three-dimensional translation stage is controlled to move the stage along the X-direction and the Y-direction at a preset speed and direction to form a modified layer and a hidden cut line in the wafer.
5. The wafer laser cutting method according to any one of claims 1 to 4, characterized in that: The wafer is made of any one of silicon, silicon carbide, glass, aluminum nitride, gallium nitride, zinc oxide, diamond or sapphire.
6. The wafer laser cutting method according to claim 5, characterized in that: The thickness of the wafer ranges from 350 μm to 1000 μm.
7. A wafer laser cutting system, characterized in that: include: An ultrashort pulse laser (2), wherein the ultrashort pulse laser (2) is capable of outputting ultrashort pulse laser light with a Gaussian distribution; An optical path adjustment component, wherein the optical path adjustment component is capable of adjusting the optical path of the ultrashort pulse laser generated by the ultrashort pulse laser (2); A beam shaping component, wherein the beam shaping component is capable of adjusting an ultrashort pulse laser to generate a Bessel beam; A focusing component, wherein the focusing component is capable of focusing the laser beam shaped by the beam shaping component; An imaging component capable of providing an image of a surface of a wafer (12); A motion component, the motion component being capable of receiving and moving the wafer (12); A control unit (1), wherein the control unit (1) is configured to be able to control the actions of the ultrashort pulse laser, the beam shaping component and the motion component.
Citation Information
Patent Citations
Semiconductor laser processing device
CN109604838A
Measuring instrument and laser beam machine for wafer
US20080180697A1
Apparatuses and methods for laser processing laminate workpiece stacks
US20180118603A1
Method and system for cleaving a substrate with a focused converging ring-shaped laser beam
WO2018011618A1
Cited By
Laser cutting method for lithium niobate crystal and lithium niobate crystal grain