Machining method of corrosion-resistant blade adjusting ring
During the processing of the blade adjustment ring, the appropriate positioning bushing and connecting plate combination half-ring blank is calculated and selected to form an anodized protective film, which solves the corrosion problem during the processing of the blade adjustment ring and improves the corrosion resistance and turbine shaft Engine reliability and service life.
Patent Information
- Application Number
- CN202411231864.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-09-04
AI Technical Summary
Existing blade adjustment rings are prone to corrosion during processing, resulting in low reliability and short service life of the turboshaft engine.
Two half-ring blanks arranged in half are obtained through machining, and the appropriate first positioning bushing outer diameter size range is calculated based on the positioning bushing hole diameter requirements and the measured position value, and the appropriate first positioning bushing and connection are selected The plate combines the half-ring blanks into the first ring-shaped body. After processing the mounting holes, it decomposes the half-ring blanks and undergoes sulfuric acid anodization treatment to form an anodized protective film. The second positioning bushing and the connecting plate are then combined into the second ring-shaped body. Install the slider and shouldered straight pin to obtain the blade adjustment ring.
It effectively improves the corrosion resistance of the blade adjustment ring, avoids dimensional deviations and corrosion phenomena, extends the reliability and service life of the turboshaft engine, and reduces the risk of damage to the anodized protective film during subsequent machining.
Smart Images

Figure CN118809101A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of blade adjustment ring processing, and in particular to a processing method of a corrosion-resistant blade adjustment ring. Background Art
[0002] The blade adjustment ring on the turboshaft engine is an important part of the compressor bearing casing. It is mainly used to adjust the angle of the guide vane on the compressor, thereby changing the airflow characteristics of the turboshaft engine and affecting the performance of the turboshaft engine. The side of the blade adjustment ring is provided with a mounting hole for installing a slider and a shoulder pin. It is fixed on the outer side of the axial flow casing through an adjustable slider. When the turboshaft engine is working, the guide vane is adjusted by the rocker arm fixed on the mounting hole. That is, the blade adjustment ring also plays the role of centering and providing support in the bearing casing. If the mounting hole on its side is corroded, it will directly affect the working stability of the guide vane. Therefore, the corrosion resistance of its surface is particularly important. However, the blade adjustment ring is usually a half-aluminum alloy profile structure with a thin wall thickness and high processing accuracy. It needs to be paired during the processing process, which makes the blade adjustment ring difficult to process. In addition, since the blade adjustment ring is on the outside of the turboshaft engine when working, it is greatly affected by the use environment, and the turboshaft engine is mostly used in the marine corrosive environment, so the corrosion resistance of the blade adjustment ring is required to be high.
[0003] However, in the current processing route of the blade adjustment ring, the overall surface treatment is often performed by sulfuric acid anodizing before processing the precision holes on the side to improve the corrosion resistance. This is because the two half rings need to be combined into a whole when processing the mounting holes on the side, but an interference fit positioning bushing is used when combining the two half rings, so that the combined blade adjustment ring cannot be disassembled and assembled again, otherwise the bottom hole size will be out of tolerance, and sulfuric acid anodizing will corrode the positioning bushing. Therefore, after the mounting holes on the side of the blade adjustment ring are processed, only chemical oxidation treatment can be performed. Compared with other parts that have been anodized with sulfuric acid, the corrosion resistance of the mounting holes is quite different. When used in a highly corrosive environment such as at sea, the opening where the blade adjustment ring is connected to other parts is prone to corrosion, which seriously affects the reliability and service life of the turboshaft engine. Summary of the invention
[0004] The invention provides a method for processing a corrosion-resistant blade adjustment ring, so as to solve the technical problem that the blade adjustment ring on the existing turboshaft engine is prone to corrosion, resulting in low reliability and short service life of the turboshaft engine.
[0005] According to one aspect of the present invention, a method for processing a corrosion-resistant blade adjustment ring is provided, comprising the following steps: S1, machining to obtain two half-ring blanks arranged in half, and pairing the two half-ring blanks to process a plurality of end holes; S2, calculating the outer diameter size range of a first locating bushing that meets the requirements according to the aperture requirements, position requirements and measured values of the position when the two half-ring blanks are combined, and then selecting a suitable first locating bushing according to the outer diameter size range of the first locating bushing, and then combining the two half-ring blanks into a first annular body through the first locating bushing and a connecting plate, wherein , the first positioning bushings are respectively clearance-fitted with the multiple end face holes on the two half-ring blanks; S3, after processing multiple mounting holes on the side of the first annular body, the first annular body is decomposed into two half-ring blanks; S4, the two half-ring blanks are anodized with sulfuric acid; S5, the two half-ring blanks and the end face lugs are combined into a second annular body through the second positioning bushings and the connecting plate, wherein the second positioning bushings are respectively interference-fitted with the multiple end face holes on the two half-ring blanks; S6, the sliders and the shouldered straight pins are respectively installed through the multiple mounting holes on the second annular body to obtain the blade adjustment ring.
[0006] As a further improvement of the above technical solution:
[0007] Furthermore, in step S2, the calculation process of the outer diameter size range of the first positioning bushing is as follows:
[0008]
[0009] bc≥0, c≥d;
[0010]
[0011] Among them, the positioning bushing aperture requirement is The outer diameter of the first positioning bushing The position requirement is E, the position deviation value is 2X, and the actual position value is W.
[0012] Further, a=0.012, b=0, E=0.1.
[0013] Furthermore, between step S5 and step S6, there is also a step of machining a lug hole on the end face lug.
[0014] Furthermore, in step S1, when machining the end hole, the aperture machining tolerance of the end hole is reduced according to the thickness of the anodized protective film.
[0015] Furthermore, in step S3, when the mounting hole is processed, the hole diameter processing tolerance of the mounting hole is reduced according to the thickness of the anodized protective film.
[0016] Furthermore, in step S4, the sulfuric acid anodizing treatment of the two half-ring blanks specifically includes the following steps: S41, cleaning the two half-ring blanks, and then installing the two half-ring blanks in an anodizing tank; S42, connecting the power supply to form an anodized protective film on the surface of the two half-ring blanks; S43, taking out the two half-ring blanks from the anodizing tank, cleaning the two half-ring blanks, and then drying the two half-ring blanks.
[0017] Furthermore, after step S43, the method further includes step S44, sealing the two half-ring blanks, and cleaning and drying the two half-ring blanks after the sealing process.
[0018] Further, in step S6, the slider and the direct pin with shoulder are respectively installed through the multiple mounting holes on the second annular body. The specific steps are as follows: first, the second annular body, the slider and the direct pin with shoulder are respectively cleaned, and then the second annular body is clamped, and the multiple mounting holes on the second annular body are precisely positioned, and finally the slider and the direct pin with shoulder are respectively installed on the multiple mounting holes.
[0019] Furthermore, before the step of finally installing the slider and the shouldered straight pin on the plurality of mounting holes respectively, the step also includes: applying lubricant on the mounting contact surfaces of the slider and the shouldered straight pin.
[0020] The present invention has the following beneficial effects:
[0021] The processing method of the corrosion-resistant blade adjustment ring of the present invention obtains two half-ring blanks arranged in half by machining, and after the two half-ring blanks are paired to process multiple end holes, the outer diameter size range of the first positioning bushing that meets the requirements is calculated according to the positioning bushing aperture requirements, position requirements and actual measured values of the position when the two half-ring blanks are combined, and then a suitable first positioning bushing is selected according to the outer diameter size range of the first positioning bushing, and then the two half-ring blanks are combined into a first annular body through the first positioning bushing and a connecting plate, so that multiple mounting holes can be machined on the side of the first annular body, and then the first annular body is decomposed into two half-ring blanks, and the two half-ring blanks are anodized with sulfuric acid. At this time, since the two half-ring blanks already have mounting holes, an anodized protective film will be formed in the mounting holes, and the corrosion resistance is good. The two half-ring blanks and the end face lugs are combined into a second annular body through the second positioning bushing and the connecting plate. Since when the first annular body is combined, the first positioning bushings are respectively matched with the multiple end holes on the two half-ring blanks. Therefore, after the first annular body is decomposed, the size of the end hole will not exceed the tolerance, ensuring that the interference fit of the second locating bushing with the multiple end hole holes on the two half-ring blanks can still meet the technical requirements, and the slider and the shoulder straight pin are respectively installed through the multiple mounting holes on the second annular body to obtain the blade adjustment ring. Compared with the prior art, this scheme selects a suitable first locating bushing by calculation, so as to effectively avoid the size exceeding the tolerance when the first annular body is decomposed through the first locating bushing with clearance fit, ensuring that the subsequent interference fit of the second locating bushing can still meet the technical requirements, and after the mounting hole processing is completed, sulfuric acid anodizing treatment can be performed to effectively ensure the integrity of the anodized protective film on the surface of the blade adjustment ring, improve the corrosion resistance of the blade adjustment ring, and prevent the occurrence of corrosion to the greatest extent, so that the turboshaft engine using the blade adjustment ring of this scheme has high reliability and long service life. At the same time, it also reduces the machining process after sulfuric acid anodizing treatment, reduces the risk of damaging the anodized protective film during subsequent machining, has strong practicality, and is suitable for wide promotion and application.
[0022] In addition to the above-described purposes, features and advantages, the present invention has other purposes, features and advantages. The present invention will be further described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The drawings constituting a part of this application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0024] Figure 1 It is a flowchart of the steps of a method for processing a corrosion-resistant blade adjustment ring according to a preferred embodiment of the present invention; DETAILED DESCRIPTION
[0025] The embodiments of the present invention are described in detail below with reference to the accompanying drawings. However, the present invention can be implemented in many different ways as defined and covered below.
[0026] like Figure 1 As shown, the processing method of the corrosion-resistant blade adjustment ring of this embodiment includes the following steps: S1, machining to obtain two half-ring blanks arranged in half, and pairing the two half-ring blanks to process multiple end holes; S2, calculating the outer diameter size range of the first positioning bushing that meets the requirements according to the positioning bushing aperture requirements, position requirements and actual measured values of the position when the two half-ring blanks are combined, and then selecting a suitable first positioning bushing according to the outer diameter size range of the first positioning bushing, and then combining the two half-ring blanks into a first annular body through the first positioning bushing and the connecting plate, wherein the first positioning bushing The positioning bushings are respectively clearance-fitted with the multiple end face holes on the two half-ring blanks; S3, after processing multiple mounting holes on the side of the first annular body, the first annular body is decomposed into two half-ring blanks; S4, the two half-ring blanks are anodized with sulfuric acid; S5, the two half-ring blanks and the end face lugs are combined into a second annular body through a second positioning bushing and a connecting plate, wherein the second positioning bushings are respectively interference-fitted with the multiple end face holes on the two half-ring blanks; S6, the slider and the shoulder straight pin are respectively installed through the multiple mounting holes on the second annular body to obtain a blade adjustment ring.
[0027] Specifically, the processing method of the corrosion-resistant blade adjustment ring of the present invention obtains two half-ring blanks arranged in half by machining, and after the two half-ring blanks are paired to process multiple end holes, the outer diameter size range of the first positioning bushing that meets the requirements is calculated according to the positioning bushing aperture requirements, position requirements and actual measured values of the position when the two half-ring blanks are combined, and then a suitable first positioning bushing is selected according to the outer diameter size range of the first positioning bushing, and then the two half-ring blanks are combined into a first annular body through the first positioning bushing and the connecting plate, so that multiple mounting holes can be machined on the side of the first annular body, and then the first annular body is decomposed into two half-ring blanks, and the two half-ring blanks are anodized with sulfuric acid. At this time, since the two half-ring blanks already have mounting holes, an anodized protective film will be formed in the mounting holes, which has good corrosion resistance. The two half-ring blanks and the end face lugs are combined into a second annular body through the second positioning bushing and the connecting plate. Since when the first annular body is combined, the first positioning bushings are respectively clearance-matched with the multiple end holes on the two half-ring blanks. Therefore, after the first annular body is decomposed, the size of the end hole will not exceed the tolerance, ensuring that the second locating bushing is respectively interference-fitted with the multiple end hole holes on the two half-ring blanks to still meet the technical requirements, and the slider and the shoulder straight pin are respectively installed through the multiple mounting holes on the second annular body to obtain the blade adjustment ring. Compared with the prior art, this scheme selects a suitable first locating bushing by calculation, so as to effectively avoid the size exceeding the tolerance when the first annular body is decomposed through the first locating bushing with clearance fit, ensuring that the subsequent interference-fit second locating bushing can still meet the technical requirements, and sulfuric acid anodizing treatment can be performed after the mounting hole processing is completed, so as to effectively ensure the integrity of the anodized protective film on the surface of the blade adjustment ring, improve the corrosion resistance of the blade adjustment ring, and prevent the occurrence of corrosion to the greatest extent, so that the turboshaft engine using the blade adjustment ring of this scheme has high reliability and long service life. At the same time, it also reduces the machining process after sulfuric acid anodizing treatment, reduces the risk of damaging the anodized protective film during subsequent machining, has strong practicality, and is suitable for wide promotion and application.
[0028] It should be understood that after the two half-ring blanks are paired and the processing of multiple end holes is completed, the actual measured value of the position when the two half-ring blanks are combined can be directly measured.
[0029] In this embodiment, in step S2, the calculation process of the outer diameter size range of the first positioning bushing is as follows:
[0030]
[0031] bc≥0, c≥d;
[0032]
[0033] Among them, the positioning bushing aperture requirement is The outer diameter of the first positioning bushing The position requirement is E, the position deviation value is 2X, and the actual position value is W.
[0034] It should be understood that X is the clearance value between the required hole diameter of the locating bushing and the outer diameter dimension of the first locating bushing.
[0035] Specifically, the outer diameter size range of the first locating bushing is calculated through the above calculation process, and then a suitable outer diameter size of the first locating bushing is selected from the range so that the first locating bushing can be used to respectively fit with the end hole clearances on the two half-ring blanks to avoid out-of-tolerance end hole size when the first annular body is decomposed, thereby ensuring that the interference fit of the second locating bushing meets the design requirements.
[0036] In this embodiment, a=0.012, b=0, E=0.1. Specifically, after the positioning bushing aperture requirements and position requirements are determined, the outer diameter size range of the first positioning bushing can be obtained as follows: During the processing, after the actual position value is measured, the outer diameter size range of the first positioning bushing can be calculated.
[0037] In this embodiment, between step S5 and step S6, there is also a step of machining a lug hole on the end lug. Specifically, the end lug is connected to the guide blade through the lug hole and the pin to achieve the transmission of rotation.
[0038] In this embodiment, in step S1, when the end hole is processed, the hole diameter processing tolerance of the end hole is reduced according to the thickness of the anodized protective film. Specifically, since an anodized protective film will be formed inside the end hole when the semi-ring blank is anodized with sulfuric acid, it is necessary to reduce the hole diameter processing tolerance of the end hole according to the thickness of the anodized protective film when processing the end hole, so as to improve the subsequent assembly accuracy.
[0039] It should be understood that although in the processing of a single blade adjustment ring, the end hole is processed first and then the anodized protective film is formed, the blade adjustment ring is a batch-processed part, and the aperture processing tolerance of the upper end hole of the blade adjustment ring processed in the subsequent batch can be reduced accordingly based on the thickness of the anodized protective film inside the upper end hole of the blade adjustment ring processed in the previous batch.
[0040] In this embodiment, in step S3, when the mounting hole is processed, the aperture processing tolerance of the mounting hole is reduced according to the thickness of the anodized protective film. Specifically, since an anodized protective film will be formed in the mounting hole when the semi-ring blank is anodized with sulfuric acid, it is necessary to reduce the aperture processing tolerance of the mounting hole according to the thickness of the anodized protective film when the mounting hole is processed to improve the subsequent assembly accuracy.
[0041] In this embodiment, in step S4, the sulfuric acid anodizing treatment of the two half-ring blanks specifically includes the following steps: S41, cleaning the two half-ring blanks, and then installing the two half-ring blanks in an anodizing tank; S42, connecting the power supply to form an anodized protective film on the surface of the two half-ring blanks; S43, taking out the two half-ring blanks from the anodizing tank, cleaning the two half-ring blanks, and then drying the two half-ring blanks. Specifically, after thoroughly cleaning the impurities on the surfaces of the two half-ring blanks to ensure that the surfaces of the two half-ring blanks are clean, the two half-ring blanks are installed in an anodizing tank to ensure that the two half-ring blanks are in good contact with the motor in the tank so that the current can pass evenly; a DC power supply is turned on, and under the action of electrolysis, the silver sulfate ions in the sulfuric acid electrolyte react with the aluminum atoms on the surface of the half-ring blanks to form a dense anodized protective film; after the anodized protective film is formed, the two half-ring blanks are taken out of the anodizing tank, and the two half-ring blanks are cleaned to remove the electrolyte and impurities remaining on the surface of the half-ring blanks, and then the two half-ring blanks are dried to prevent the anodized protective film from being damp or damaged.
[0042] In this embodiment, after step S43, the process further includes step: S44, sealing the two semi-ring blanks, and cleaning and drying the two semi-ring blanks after the sealing process. Specifically, the two semi-ring blanks are sealed to seal the micropores in the anodized protective film, thereby further improving the corrosion resistance of the semi-ring blanks, and the two semi-ring blanks are cleaned and dried after the sealing process to remove the processing liquid or other impurities that may remain on the surface of the semi-ring blanks, thereby ensuring the processing quality and avoiding pollution in the subsequent processing process.
[0043] In this embodiment, in step S6, the slider and the direct pin with shoulder are respectively installed through the multiple mounting holes on the second annular body. The specific steps are as follows: first, the second annular body, the slider and the direct pin with shoulder are respectively cleaned, and then the second annular body is clamped, and the multiple mounting holes on the second annular body are precisely positioned, and finally the slider and the direct pin with shoulder are respectively installed on the multiple mounting holes.
[0044] Specifically, the second annular body, the slider and the straight pin with shoulder are first cleaned respectively to ensure the cleanliness and assembly quality in the subsequent assembly process, then the second annular body is clamped, and the multiple mounting holes on the second annular body are precisely positioned to ensure that the positions of the mounting holes are accurate, and finally the slider and the straight pin with shoulder are respectively installed on the multiple mounting holes.
[0045] In this embodiment, before the slider and the shouldered straight pin are respectively installed on the plurality of installation holes, the step further includes: applying lubricant on the installation contact surfaces of the slider and the shouldered straight pin. Specifically, the lubricant is used to reduce friction and wear during the assembly process and improve assembly quality.
[0046] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for processing a corrosion-resistant blade adjustment ring, characterized in that: The following steps are involved: S1, machining to obtain two half-ring blanks arranged in half, and pairing the two half-ring blanks to machine a plurality of end holes; S2, according to the positioning bushing aperture requirements, position requirements and measured position values when the two semi-ring blanks are combined, the outer diameter size range of the first positioning bushing that meets the requirements is calculated, and then a suitable first positioning bushing is selected according to the outer diameter size range of the first positioning bushing, and then the two semi-ring blanks are combined into a first annular body through the first positioning bushing and the connecting plate, wherein the first positioning bushing is respectively matched with the multiple end holes on the two semi-ring blanks; S3, after machining a plurality of mounting holes on the side surface of the first annular body, decomposing the first annular body into two half-ring blanks; S4, performing sulfuric acid anodizing treatment on the two half-ring blanks; S5, combining the two half-ring blanks and the end face lugs into a second annular body through a second positioning bushing and a connecting plate, wherein the second positioning bushings are respectively interference-fitted with a plurality of end face holes on the two half-ring blanks; S6, respectively installing the slider and the straight pin with the shaft shoulder through the multiple mounting holes on the second annular body to obtain the blade adjustment ring.
2. The method for processing a corrosion-resistant blade adjustment ring according to claim 1, characterized in that: In step S2, the calculation process of the outer diameter size range of the first positioning bushing is as follows: bc≥0, c≥d; Among them, the positioning bushing aperture requirement is The outer diameter of the first positioning bushing The position requirement is E, the position deviation value is 2X, and the actual position value is W.
3. The method for processing a corrosion-resistant blade adjustment ring according to claim 2, characterized in that: a=0.012, b=0, E=0.
1.
4. The method for processing a corrosion-resistant blade adjustment ring according to any one of claims 1 to 3, characterized in that: The steps between step S5 and step S6 also include: The lug holes are machined on the end lugs.
5. The method for processing a corrosion-resistant blade adjustment ring according to any one of claims 1 to 3, characterized in that: In step S1, when machining the end surface hole, the hole diameter machining tolerance of the end surface hole is reduced according to the thickness of the anodized protective film.
6. The method for processing a corrosion-resistant blade adjustment ring according to any one of claims 1 to 3, characterized in that: In step S3, when machining the mounting hole, the machining tolerance of the hole diameter of the mounting hole is reduced according to the thickness of the anodized protective film.
7. The method for processing a corrosion-resistant blade adjustment ring according to any one of claims 1 to 3, characterized in that: In step S4, the sulfuric acid anodizing treatment of the two half-ring blanks specifically includes the following steps: S41, cleaning the two half-ring blanks, and then installing the two half-ring blanks in an anodizing tank; S42, connecting the power supply to form an anodized protective film on the surfaces of the two half-ring blanks; S43, taking out the two half-ring blanks from the anodizing tank, washing the two half-ring blanks, and then drying the two half-ring blanks.
8. The method for processing a corrosion-resistant blade adjustment ring according to claim 7, characterized in that: After step S43, the method further includes the following steps: S44, performing sealing processing on the two semi-ring blanks, and cleaning and drying the two semi-ring blanks after the sealing processing.
9. The method for processing a corrosion-resistant blade adjustment ring according to any one of claims 1 to 3, characterized in that: In step S6, the slider and the shouldered straight pin are respectively installed through the multiple installation holes on the second annular body. The specific steps are as follows: First, the second annular body, the slider and the straight pin with shoulder are cleaned respectively, then the second annular body is clamped, and the multiple mounting holes on the second annular body are accurately positioned, and finally the slider and the straight pin with shoulder are installed on the multiple mounting holes respectively.
10. The method for processing a corrosion-resistant blade adjustment ring according to claim 9, characterized in that: The steps include the following steps before the slider and the shoulder pin are respectively installed on the plurality of mounting holes: Apply lubricant to the mounting contact surfaces of the slide and the straight pin with shoulder.
Citation Information
Patent Citations
Guide vane mounting device for low-pressure turbine of aero-engine
CN109676562A
Assembling type buffer base and assembling and repeated positioning process method of buffer base
CN114135624A
Easily-assembled tool for repairing aero-engine axial flow casing flow channel and using method of easily-assembled tool for repairing aero-engine axial flow casing flow channel
CN116423146A
Integral machining method for ultra-thin wall easy-to-deform aluminum alloy multi-petal shunt ring of aero-engine
CN116803596A
Adjustable blade adjusting mechanism of aero-engine
CN118049285A