A method for preparing salt-free dye paste
Through the combination of ZrO(OH)2 adsorption and nanofiltration membrane, the problems of wastewater consumption and chemical introduction in the preparation of salt-free dye pulp are solved, which improves the utilization value of salt and achieves efficient dye purification and safe production.
Patent Information
- Application Number
- CN202411301344.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-18
AI Technical Summary
The prior art has problems such as high wastewater consumption, long time consumption, safety problems caused by chemical introduction of chemical substances, and low utilization value of salt when preparing salt-free dye slurry.
ZrO(OH)2 is used as the ion exchanger to adsorb SO42- in the dye, and preliminarily processed by microfiltration or ultrafiltration, combined with the concentration and washing of ceramic membranes or tube membranes, nanofiltration removes monovalent salts, and passes through high pressure Reverse osmosis recovers wastewater to achieve separation and reuse of salt.
It effectively solves the problems of wastewater consumption and time-consuming, avoids the introduction of chemical substances, improves the utilization value of salt, and realizes a loss-free ZrO(OH)2 adsorption and desorption process, ensuring efficient purification and safety of dyes.
Smart Images

Figure CN118813069B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of dyes, and in particular to a method for preparing a salt-free dye paste. Background Art
[0002] Industrial synthetic commodity dyes contain a large amount of inorganic salts such as Na2SO4 and NaCl produced by acid-base neutralization and salting out. Their high salt content, low solubility and poor filtration performance directly limit their application in the digital inkjet industry. In order to meet the application of dyes in the digital inkjet industry, the crude dyes must be purified and refined to meet the requirements of preparing digital inkjet dye pastes with good filtration performance and high stability.
[0003] There are many methods for industrial purification of crude dyes. The desalting methods mainly include solvent extraction, salting out, alcohol precipitation, membrane method, etc. At present, nanofiltration membrane is commonly used for the preparation of salt-free dyes, but the retention rate of divalent salts by nanofiltration membrane is about 85%-90%, and the removal efficiency of divalent salts is low. 2- The membrane method will produce a lot of high-color wastewater if there are more dyes. 2- The main methods include calcium method, barium method, freezing method, ion resin exchange method, etc., while chemical methods often introduce other chemical substances and the process is complicated. Efficient purification of crude dyes and removal of salt from dyes has always been a major problem that has plagued the product quality of the dye industry, and it is also a key research direction.
[0004] Patent CN108003657A discloses a preparation process of salt-free dye without wastewater discharge, comprising: (1) pre-treating a crude dye aqueous solution through an ultrafiltration membrane device to obtain a filtrate; (2) subjecting the filtrate to water-adding circulation desalination by a nanofiltration I process to obtain a permeate 1 and a concentrated solution 1; (3) desalting the permeate 1 by a nanofiltration II process to obtain a permeate 2 and a concentrated solution 2, and spray-drying the concentrated solution 2 to obtain a dye product; (4) the permeate 2 enters a reverse osmosis I process for reverse osmosis treatment to obtain a concentrated solution 3 and a permeate 3; (5) the concentrated solution 1 enters a reverse osmosis II process for reverse osmosis treatment to obtain a permeate 4 and a concentrated solution 4; (6) the concentrated solution 4 is adsorbed by a zirconium hydroxide adsorption column to obtain a permeate 5; (7) the permeate 5 is spray-dried to obtain a solid dye product. However, the process has the following problems to a certain extent: the ultrafiltration device in step (1) adopts dead-end filtration, which is easy to cause membrane fouling; the nanofiltration I process in step (2) adopts 500~1000D nanofiltration membrane, and the mass of make-up water is 5~20 times the mass of the filtrate, which requires a large amount of water and takes a long time; the permeate 1 in step (3) is a salt water containing a small amount of dye, which enters the nanofiltration II to obtain a concentrated solution with a solid content of 15~25%; the low value-added dye obtained by spray drying contains more salt, has low utilization value and high energy consumption for spray drying; the concentrated solution 3 in step (4) is a concentrated solution with a reverse osmosis operating pressure of 1.5~2.5Mpa, which does not contain too high salt concentration and contains mixed salts of NaCl and Na2SO4, which has low utilization value; the conventional reverse osmosis is used to concentrate the dye solution to a content of more than 30% in step (5), which is easy to cause membrane fouling and is not suitable for long-term operation; the zirconium hydroxide adsorption column in step (6) adsorbs SO4 2- Cl in process solution - It will increase, and the excess chloride ions need to be removed. Otherwise, after direct spray drying, the final dye will contain more chloride ions and fail to meet the standards.
[0005] Patent CN106280549A discloses a salt-free dye and its preparation method. The preparation method of the salt-free dye includes the following steps: removing divalent salts: mixing the crude dye aqueous solution with a soluble barium salt, stirring the reaction, filtering with a nano-ceramic membrane, and obtaining dye solution 1; removing monovalent salts: filtering the dye solution 1 with a nanofiltration membrane, first cyclically desalting at a pressure of 0.2~1.5MPa, replenishing water during the process, and after the chloride ion content is detected to be lower than 5ppm, increasing the pressure to 2.0~2.5MPa for concentration to obtain dye solution 2; mixing the dye solution 2 with a cosolvent and a buffer, sterilizing, adding a preservative, and then filtering to obtain a salt-free dye. In this desalination method, the process of removing divalent salts uses a chemical method to introduce a new substance, a soluble barium salt. The soluble barium salt is costly and toxic. Although barium sulfate is a poorly soluble precipitate, there will still be residual free Ba in the solution. 2+ Ions can cause safety problems for the product. Summary of the invention
[0006] The present invention aims to solve at least one of the technical problems in the related art to a certain extent. To this end, the present invention provides a method for preparing salt-free dye paste with simple operation and high efficiency. The method of the present invention shows its feasibility and superiority, solves the problem of generating a large amount of wastewater and taking a long time when washing salt directly using a nanofiltration membrane process, and avoids the safety problems caused by the introduction of chemical impurities by chemical methods. The method of the present invention consumes less water in the treatment process, recycles and reuses the wastewater, separates the inorganic salt, and obtains monovalent salt and divalent salt solutions respectively, thereby improving the utilization value of the salt. The adsorption, separation and analysis of zirconium hydroxide (ZrO(OH)2) are all realized in the membrane equipment, and the desorption and recovery process has no loss and is simple to operate.
[0007] The present invention adopts the following technical solution:
[0008] The embodiment of the present invention provides a method for preparing a salt-free dye paste, comprising the following steps:
[0009] (1) Pretreatment: Filter the crude dye liquid through a microfiltration membrane or ultrafiltration membrane to remove mechanical impurities and colloids;
[0010] (2) Adsorption reaction: ZrO(OH)2 acts as an ion exchanger to adsorb SO4 in the crude dye solution. 2- , SO4 2- Replaced by Cl - In the adsorption reaction, ZrO(OH)2 and SO4 2- The molar ratio is 4-6:1, the pH is adjusted to 2-3 with HCl, the temperature is 20-40°C, and the reaction is fully carried out for 15-30 minutes to obtain an adsorption slurry;
[0011] (3) Sedimentation, concentration and washing: The adsorption slurry in step (2) is naturally sedimented. After sedimentation, the supernatant is concentrated using a ceramic membrane or a tubular membrane to obtain a [ZrO(OH)]2SO4 concentrated slurry and a permeate. The [ZrO(OH)]2SO4 concentrated slurry is stirred and washed with water and then naturally sedimented. The natural sedimentation-supernatant concentration-[ZrO(OH)]2SO4 concentrated slurry is stirred and washed with water for 5 to 6 times. The washing is stopped when the permeate is basically colorless, and all the permeate is collected and enters the nanofiltration step;
[0012] (4) Nanofiltration: The permeate in step (3) is subjected to a nanofiltration membrane to remove monovalent salts. After the desalination is qualified, the material is concentrated to obtain a salt-free dye paste;
[0013] (5) Desalination wastewater recovery: The desalination wastewater after desalination in step (4) is concentrated by high-pressure reverse osmosis to obtain a NaCl solution with a content of 6 to 8.5 wt %. The water generated during the concentration process is reused as make-up water in step (3) or step (4);
[0014] (6) Desorption reaction: Desorb the [ZrO(OH)]2SO4 concentrated slurry in step (3), add water, add NaOH dropwise, maintain the pH value at 9-10, maintain for 15-30 minutes, dilute and wash the obtained ZrO(OH)2 concentrated slurry with water, and concentrate the supernatant using a ceramic membrane or tubular membrane to wash out SO4 2- Repeat the steps of diluting the ZrO(OH)2 concentrated slurry with water and washing - concentrating the supernatant for multiple times. When the conductivity of the permeate is lower than 20μs / cm, stop washing and return the ZrO(OH)2 concentrated slurry to the system of step (2) for adsorption;
[0015] (7) Recovery of desorption wastewater: The desorption wastewater in step (6) is concentrated by high-pressure nanofiltration to a Na2SO4 solution with a content of 12-15 wt%. The water generated during the concentration process is reused as make-up water in step (3) or step (4).
[0016] In some embodiments, the concentration of the dye in the crude dye solution is 5-45wt%.
[0017] In some embodiments, taking the crude dye after drying the crude dye liquid as 100%, the dye accounts for 50~99wt%, the salt accounts for 1~50wt%, among which Na2SO4 accounts for 1~50wt%, and NaCl accounts for 0~49wt%.
[0018] In some embodiments, the concentration of the dye in the crude dye liquid is 5~25wt%; taking the crude dye after the crude dye liquid is dried as 100%, the dye accounts for 50~85wt%, and the salt accounts for 15~50wt%, of which Na2SO4 accounts for 10~30wt%, and NaCl accounts for 5~20wt%.
[0019] In some embodiments, the dye is a water-soluble dye with a molecular weight of 300-800.
[0020] In some embodiments, based on the crude dye product after drying the crude dye product liquid as 100%, Na2SO4 accounts for 15~30wt%.
[0021] In some embodiments, the dye is one or more of CI Reactive Orange 140, CI Reactive Black 5, and CI Acid Yellow 23.
[0022] In some embodiments, in step (1), the microfiltration membrane is selected from a flat membrane, a filter element or a hollow fiber microfiltration form, with a pore size of 0.1~1.0μm, an inlet pressure of 0.10~0.30Mpa, and is carried out at room temperature, using a cross-flow method for filtration; the ultrafiltration membrane is hollow fiber ultrafiltration, with an ultrafiltration retention molecular weight of 50,000~500,000, an inlet pressure of 0.05~0.15Mpa, and is carried out at room temperature, using a cross-flow method for filtration.
[0023] In some embodiments, in step (2), the particle size of ZrO(OH)2 is 50-70 μm.
[0024] In some embodiments, in step (3), the pore size of the ceramic membrane or tubular membrane is 0.01-0.05 μm, and during the process of adding water to the [ZrO(OH)]2SO4 concentrated slurry and stirring and washing, the amount of water added each time is 0.9-1.1 times the volume of the [ZrO(OH)]2SO4 concentrated slurry.
[0025] In some embodiments, step (4) is: the permeate in step (3) is first concentrated, and then water is added at a constant volume for desalination, the amount of membrane permeate in the desalination process is kept equal to the amount of water added to the concentrated solution in the feed tank, and the monovalent salt is removed by a 300-500D nanofiltration membrane, the membrane inlet pressure is 1.0-3.0MPa, and the ion content in the concentrated solution is determined by ion chromatography. After the desalination is qualified, the material is concentrated to prepare a salt-free dye paste with a concentration of 15-40wt%.
[0026] In some embodiments, in step (5), the high-pressure reverse osmosis membrane pressure is 2.5-8.0 MPa, and the NaCl solution with a content of 6%-8.5 wt% obtained after concentration is used in the salting-out process after the dye synthesis to achieve salt reuse.
[0027] In some embodiments, in step (6), the steps of diluting the ZrO(OH)2 concentrated slurry with water and washing it - concentrating the supernatant are repeated 5 to 6 times, and the amount of water added in the step of diluting the ZrO(OH)2 concentrated slurry with water and washing it is 0.9 to 1.1 times the volume of the ZrO(OH)2 concentrated slurry.
[0028] In some embodiments, in step (7), the high-pressure nanofiltration membrane used in the high-pressure nanofiltration has a molecular weight cutoff of 500-800D, and the membrane inlet pressure is 2.0-8.0 MPa. The Na2SO4 solution with a content of 12-15 wt% obtained after concentration is used as a dyeing accelerator salt for dyeing with the dye.
[0029] The present invention has the following advantages and beneficial effects:
[0030] (1) The preparation method of the salt-free dye paste of the present invention shows its feasibility and superiority. ZrO(OH)2 adsorbs SO42- It has high efficiency, large capacity, short reaction time, high density, and rapid sedimentation. It is suitable for dyes that are difficult to desalt using membrane methods, especially small molecular weight dyes with good solubility. Because these dyes pass through the membrane more, the use of membrane methods will cause a large loss of dyes.
[0031] (2) The preparation method of the salt-free dye paste of the present invention first uses ZrO(OH)2 to absorb SO4 2- , which solves the problem of directly using nanofiltration membrane to remove Na2SO4, producing a large amount of wastewater and taking a long time, especially for dye varieties with particularly high content of divalent salts.
[0032] (3) The method for preparing the salt-free dye paste of the present invention can also avoid the safety problems caused by the introduction of chemical impurities.
[0033] (4) The preparation method of the salt-free dye paste of the present invention is green and environmentally friendly, consumes little water during the treatment process, and the wastewater is recycled and reused, without any wastewater discharge.
[0034] (5) The method for preparing the salt-free dye paste of the present invention separates the inorganic salt and separates the salt to obtain monovalent salt and divalent salt solutions, respectively, thereby improving the utilization value of the salt.
[0035] (6) In the method for preparing the salt-free dye paste of the present invention, ZrO(OH)2 is adsorbed, solid-liquid separated, desorbed and then returned for utilization, and the process is loss-free and easy to operate.
[0036] (7) The method for preparing the salt-free dye paste of the present invention has little dye loss, which can be controlled below 2.0%. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the following description of the embodiments in conjunction with the accompanying drawings, in which:
[0038] Figure 1 The present invention is a process flow chart of a method for preparing a salt-free dye paste. DETAILED DESCRIPTION
[0039] The embodiments of the present invention are described in detail below. The embodiments described below are exemplary and are only used to explain the present invention, and should not be understood as limiting the present invention.
[0040] Unless defined otherwise herein, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs.
[0041] Where values are described herein as a range, it should be understood that such disclosure includes disclosure of all possible sub-ranges within that range, as well as specific values falling within that range, regardless of whether a specific value or a specific sub-range is explicitly stated.
[0042] In this document, "multiple" and the like, unless otherwise specified, refer to a number greater than 2 or equal to 2. For example, "one or more" means one or greater than or equal to two.
[0043] In this document, the terms “preferred” and “more preferred” are only used to describe implementation methods or examples with better effects, and it should be understood that they do not constitute limitations on the scope of protection of the present invention.
[0044] In this document, the words "further" and the like are used for descriptive purposes to indicate differences in content, but should not be construed as limiting the scope of protection of the present invention.
[0045] In this article, the term "and / or" is a description of the association relationship of objects, indicating that three relationships may exist. For example, A and / or B means: A or B, or A and B.
[0046] As used herein, the term "about" means + / - 10%, preferably + / - 5%, more preferably + / - 1% of the specified value.
[0047] Unless otherwise specified, the raw materials and reagents used in the following examples are commercially available or can be prepared by known methods.
[0048] like Figure 1 As shown, an embodiment of the present invention provides a method for preparing a salt-free dye paste, comprising the following steps:
[0049] (1) Pretreatment: Filter the crude dye liquid through a microfiltration membrane or ultrafiltration membrane to remove mechanical impurities and colloids (to protect subsequent membrane separation equipment);
[0050] (2) Adsorption reaction: ZrO(OH)2 acts as an ion exchanger to adsorb SO4 in the crude dye solution. 2- , SO4 2- Replaced by Cl - In the adsorption reaction, ZrO(OH)2 and SO4 2- The molar ratio is 4-6:1, the pH is adjusted to 2-3 with HCl, the temperature is 20-40°C, and the reaction is fully carried out for 15-30 minutes to obtain an adsorption slurry;
[0051] (3) Sedimentation, concentration and washing: The adsorption slurry in step (2) is naturally sedimented. After sedimentation, the supernatant is concentrated using a ceramic membrane or a tubular membrane to obtain a [ZrO(OH)]2SO4 concentrated slurry and a permeate. The [ZrO(OH)]2SO4 concentrated slurry is stirred and washed with water and then naturally sedimented. The natural sedimentation-supernatant concentration-[ZrO(OH)]2SO4 concentrated slurry is stirred and washed with water for 5 to 6 times. The washing is stopped when the permeate is basically colorless, and all the permeate is collected and enters the nanofiltration step;
[0052] (4) Nanofiltration: The permeate in step (3) is subjected to a nanofiltration membrane to remove monovalent salts. After the desalination is qualified, the material is concentrated to obtain a salt-free dye paste;
[0053] (5) Desalination wastewater recovery: The desalination wastewater after desalination in step (4) is concentrated by high-pressure reverse osmosis to obtain a NaCl solution with a content of 6 to 8.5 wt %. The water generated during the concentration process is reused as make-up water in step (3) or step (4);
[0054] (6) Desorption reaction: Desorb the [ZrO(OH)]2SO4 concentrated slurry in step (3) by adding water and dropping NaOH, maintaining the pH value at 9-10 for 15-30 min. (At this time, [ZrO(OH)]2SO4 becomes ZrO(OH)2, SO4 2- The ZrO(OH)2 concentrated slurry is diluted and washed with water, and the supernatant is concentrated using a ceramic membrane or a tubular membrane to wash out SO4 2- Repeat the steps of diluting the ZrO(OH)2 concentrated slurry with water and washing - concentrating the supernatant for multiple times. When the conductivity of the permeate is lower than 20μs / cm, stop washing and return the ZrO(OH)2 concentrated slurry to the system of step (2) for adsorption;
[0055] (7) Recovery of desorption wastewater: The desorption wastewater in step (6) is concentrated by high-pressure nanofiltration to a Na2SO4 solution with a content of 12-15 wt%. The water generated during the concentration process is reused as make-up water in step (3) or step (4).
[0056] In some embodiments, the concentration of the dye in the crude dye liquid is 5-45wt%; taking the crude dye after the crude dye liquid is dried as 100%, the dye accounts for 50-99wt%, the salt accounts for 1-50wt%, of which Na2SO4 accounts for 1-50wt%, and NaCl accounts for 0-49wt%. The dye of the embodiment method of the present invention has a wide range of applications, and dyes with different salt contents can achieve excellent desalination effects through the embodiment method of the present invention.
[0057] Preferably, the dye is a water-soluble dye with a molecular weight of 300 to 800. The preparation method of the salt-free dye paste of the present invention shows a more excellent effect for water-soluble dyes with a molecular weight of 300 to 800, because small molecular weight dyes pass through the membrane more, and the membrane desalination using the existing technology will cause a large loss of dyes.
[0058] In some embodiments, the concentration of the dye in the crude dye liquid is 5-25wt%; taking the crude dye after the crude dye liquid is dried as 100%, the dye accounts for 50-85wt%, and the salt accounts for 15-50wt%, of which Na2SO4 accounts for 10-30wt%, and NaCl accounts for 5-20wt%. The preparation method of the salt-free dye paste in the embodiment of the present invention has a better desalination effect than the prior art when desalting dye varieties containing more divalent salts. ZrO(OH)2 adsorbs SO4 2- It has high efficiency, large capacity and short reaction time, avoiding the problem of directly using nanofiltration membrane to remove Na2SO4 in the prior art, which produces a large amount of wastewater and takes a long time.
[0059] Preferably, based on the crude dye product after drying the crude dye product liquid as 100%, the proportion of Na2SO4 is 15-30wt%.
[0060] In a specific embodiment, the dye is one or more of CI Reactive Orange 140, CI Reactive Black 5, and CI Acid Yellow 23.
[0061] In some embodiments, in step (1), the microfiltration membrane is selected in the form of a flat membrane, a filter element or a hollow fiber microfiltration, with a pore size of 0.1~1.0μm, an inlet pressure of 0.10~0.30Mpa, and is carried out at room temperature, using a cross-flow filtration method; the ultrafiltration membrane is selected in the form of a hollow fiber ultrafiltration, with an ultrafiltration retention molecular weight of 50,000~500,000, an inlet pressure of 0.05~0.15Mpa, and is carried out at room temperature, using a cross-flow filtration method; the cross-flow filtration method is not easy to cause membrane fouling.
[0062] In some embodiments, in step (2), the particle size of ZrO(OH)2 is 50-70 μm.
[0063] In some embodiments, in step (2), the adsorption reaction is maintained at a pH of 2-3 by adjusting the pH through HCl. Controlling the pH range is critical, but the pH cannot be too low, because ZrO(OH)2 is an amphoteric compound. If the pH is too low, ZrO(OH)2 will dissolve and the following reactions will occur: ZrO(OH)2+2HCl—ZrOCl2+2H2O, ZrO(OH)2+4HCl—ZrCl4+3H2O. The pH should not be greater than 3. When the pH is greater than 3, the HCl concentration is low, which affects the adsorption reaction: 2ZrO(OH)2+Na2SO4+2HCl—[ZrO(OH)]2SO4+2NaCl+2H2O. The temperature is between 20 and 40°C. The temperature of the dye system should not be too high. Some dyes will be unstable and undergo hydrolysis under high temperature conditions. According to SO4 2- The amount of ions is calculated by adding ZrO(OH)2. Theoretically, 2 mol of zirconium hydroxide adsorbs 1 mol of SO4. 2- However, the purity of commercially available ZrO(OH)2 is less than 100%, and it often exists in combination with water and will not react completely in the reaction. 2- When the adsorption is complete, ZrO(OH)2 will be added in excess, so that the addition of ZrO(OH)2 and SO4 2- The molar ratio is 4~6:1, but ZrO(OH)2 should not be added in large quantities. 2- When the molar ratio is greater than 6:1, it will cause pressure on the subsequent solid-liquid separation process. The reaction time is 15-30 minutes. Ion chromatography is used to detect SO4 2- Further, ion chromatography was used to detect SO4 2- When the content is 0, separation is performed.
[0064] In some embodiments, in step (3), the natural sedimentation time is 20-30 minutes. First, the natural sedimentation is carried out by utilizing the high density of ZrO(OH)2 and [ZrO(OH)]2SO4. About 95% of ZrO(OH)2 and [ZrO(OH)]2SO4 can be naturally precipitated. Since the particle sizes of ZrO(OH)2 and [ZrO(OH)]2SO4 are very small, small particles of ZrO(OH)2 and [ZrO(OH)]2SO4 will still be suspended in the supernatant. Then, the supernatant is concentrated by using a ceramic membrane or a tubular membrane.
[0065] In some embodiments, in step (3), the pore size of the ceramic membrane or tubular membrane is 0.01-0.05 μm, and the membrane assembly must ensure that ZrO(OH)2 and [ZrO(OH)]2SO4 can be completely retained, and the feed liquid can pass through, and the pore size should not be greater than 0.05 μm, otherwise fine particles in the solution can easily enter the membrane pores and cause the membrane pores to be blocked. Concentration is to truly separate the solid and liquid, and the permeate enters the next step to continue desalination. The concentrated [ZrO(OH)]2SO4 slurry obtained on the concentrated liquid side is returned to the sedimentation tank, added with water, stirred and washed, and then naturally precipitated. The supernatant is then concentrated by membrane. After 5 to 6 rounds of natural sedimentation - supernatant concentration - [ZrO(OH)]2SO4 concentrated slurry adding water, stirring and washing, the amount of water added each time is 0.9 to 1.1 times the volume of the [ZrO(OH)]2SO4 concentrated slurry, until the effluent is basically colorless. The purpose of washing is to wash out the dye and reduce dye loss. The effluent that passes through the membrane enters the next nanofiltration process. The pH is adjusted to the initial value of the raw material solution before entering the nanofiltration membrane. The concentrated [ZrO(OH)]2SO4 slurry is obtained on the concentrated liquid side.
[0066] In some embodiments, step (4) is: first concentrate the permeate in step (3), then add water to desalinate at a constant volume, keep the amount of permeate in the desalination process equal to the amount of water added to the concentrate in the feed tank, use a 300-500D nanofiltration membrane to remove monovalent salts, preferably 300-400D, and it is not advisable to choose too large, because the macromolecular membrane will cause a large loss of dyes, the membrane inlet pressure is 1.0-3.0MPa, use ion chromatography to determine the ion content in the concentrate, and concentrate the material after the desalination is qualified to prepare a salt-free dye paste with a concentration of 15-40wt%. Further, the qualified desalination in step (4) refers to the determination of Cl by ion chromatography. - When the ion content is 0, the desalination is qualified.
[0067] In some embodiments, in step (5), the membrane inlet pressure of the high-pressure reverse osmosis is 2.5-8.0 MPa, and the NaCl solution with a content of 6%-8.5 wt% obtained after concentration is used in the salting-out process after the dye is synthesized, thereby realizing the reuse of salt.
[0068] In some embodiments, in step (6), the steps of diluting the ZrO(OH)2 concentrated slurry with water and washing it - concentrating the supernatant are repeated 5 to 6 times, and the amount of water added in the step of diluting the ZrO(OH)2 concentrated slurry with water and washing it is 0.9 to 1.1 times the volume of the ZrO(OH)2 concentrated slurry.
[0069] In some embodiments, in step (7), the molecular weight cutoff of the high pressure nanofiltration membrane is 500-800D, the membrane inlet pressure is 2.0-8.0MPa, and the Na2SO4 solution with a content of 12-15wt% obtained after concentration is used as the accelerator salt for dyeing with the dye.
[0070] The present invention adopts a multi-step process to purify the crude dye. 2- The removal efficiency is generally low, but ZrO(OH)2 has a large specific surface area and can adsorb SO4 2- Large capacity and high removal rate, first select ZrO(OH)2 as the ion exchanger to adsorb SO4 in the crude dye liquid 2- , put SO4 2- Replaced by Cl - After the adsorption is completed, the liquid is collected and the SO4 2- The [ZrO(OH)]2SO4 concentrated slurry is desorbed and returned to play the adsorption role after analysis to achieve recycling. The principle of ion exchange:
[0071] Adsorption: 2ZrO(OH)2+Na2SO4+2HCl—[ZrO(OH)]2SO4+2NaCl+2H2O
[0072] Desorption: [ZrO(OH)]2SO4+2NaOH—2ZrO(OH)2+Na2SO4
[0073] The feed liquid after adsorption enters the next step of nanofiltration process to continue to remove monovalent salt. At this time, the nanofiltration can be selected to be 300-500D, and the dye loss of the permeate is small. After the salt is removed, the material is concentrated to prepare a salt-free dye paste of a certain concentration. The method of the present invention obtains a monovalent salt solution and a divalent salt solution respectively, and concentrates them respectively. The monovalent salt solution concentrated by high-pressure reverse osmosis can be used in the salting-out process after the synthesis of the dye to achieve salt reuse. The divalent salt solution concentrated by high-pressure nanofiltration can be used as a dyeing-accelerating salt for the dye dyeing. The water produced in the concentration process can be used for desalination and water replenishment to achieve recycling.
[0074] In the embodiment of the present invention:
[0075] The microfiltration membrane, ultrafiltration membrane, nanofiltration membrane, and reverse osmosis membrane used in the experiment were purchased from Fume Technology (Beijing) Co., Ltd.;
[0076] CI Reactive Orange 140 liquid, CI Reactive Black 5 liquid, and CI Acid Yellow 23 coarse powder were all from Tianjin Dekai Chemical Co., Ltd.;
[0077] ZrO(OH)2: particle size 50~70μm, purchased from Shijiazhuang Jinghuang Technology Co., Ltd.
[0078] Example 1
[0079] A method for preparing a salt-free dye paste comprises the following steps:
[0080] (1) Take 1000 kg (about 900 L) of CI Reactive Orange 140 liquid and use UV spectrophotometer and ion chromatography to detect. The dye content in the dried dye crude product (including dye, salt, unreacted products, by-products and mechanical impurities, etc.) is about 74.20 wt%, the dye content in the liquid is 12.40 wt%, and SO4 2- The content is 20859ppm (1kg of liquid contains 20859mg of SO4 2- ), according to a SO4 2- Corresponding to 2 Na + , the calculated mass of Na2SO4 is 30.85kg, accounting for 18.73wt% of the crude dye, Cl - The content is 5961ppm (1kg of liquid contains 5961mg of Cl - ), the calculated mass of NaCl is 9.82kg, accounting for 5.96% of the crude dye.
[0081] (2) The feed liquid in step (1) is pretreated, and the filtrate is collected by filtering with a hollow fiber microfiltration membrane. The pore size of the hollow fiber microfiltration membrane is 0.2 μm, the inlet pressure is 0.15 MPa, and the filtration is carried out at room temperature in a cross-flow manner.
[0082] (3) The filtrate in step (2) is subjected to an adsorption reaction according to SO4 2- The amount of ions is 217.28 mol, so that ZrO(OH)2 and SO4 2- The molar ratio is 5:1, and the amount of ZrO(OH)2 added is about 153.18 kg. HCl is added dropwise while stirring, and the pH value is controlled at 2-3 to allow the liquid to fully contact and react with the solid powder. The reaction lasts for 15 minutes, and a sample is taken to detect SO4 2- The content is 0, and the adsorption slurry is obtained.
[0083] (4) The adsorption slurry in step (3) was naturally settled for 30 minutes, and the supernatant was concentrated using a ceramic membrane. The pore size of the ceramic membrane was 20 nm, and the membrane assembly could completely intercept ZrO(OH)2 and [ZrO(OH)]2SO4. About 820 L of feed liquid was obtained on the effluent side, and about 80 L of concentrated slurry was obtained on the concentrated liquid side. The concentrated slurry was returned to the sedimentation tank, 80 L of water was added, stirred, and then naturally settled. The supernatant was concentrated again. After 6 rounds of sedimentation-supernatant concentration-concentrated slurry water stirring washing-sedimentation, about 480 L of water was consumed, the effluent was basically colorless, and the total volume of the effluent was about 1300 L. [ZrO(OH)]2SO4 concentrated slurry was obtained on the concentrated liquid side.
[0084] (5) The pH of the permeate in step (4) was adjusted to the initial value of the raw material solution (CI Active Orange 140 feed solution), and desalted using a 300D Dalton nanofiltration membrane with the membrane inlet pressure controlled at 2.0 MPa. The solution was first concentrated to about 500 L, and then desalted with constant volume water replenishment of about 750 L. The Cl - The ion content is 0, the desalination is qualified, and the material is concentrated to obtain about 380L (408kg) of 30wt% active orange 140 salt-free dye paste, consuming about 750L of water, and the total volume of desalination wastewater is about 1670L.
[0085] (6) The desalinated wastewater in step (5) is then concentrated by high-pressure reverse osmosis. The membrane pressure is initially 2.5 MPa and gradually increased to 8.0 MPa. After concentration, the concentrated solution is about 100 L (115 kg), with a NaCl content of 8.02 wt% and a dye concentration of 0.21 wt%. The obtained NaCl solution can be used in the salting-out process after the synthesis of the dye to achieve salt reuse. 1570 L of water is produced with a conductivity of 16.5 μs / cm, which can be reused in step (4) or step (5).
[0086] (7) Desorb the [ZrO(OH)]2SO4 concentrated slurry in step (4) by adding 15 wt% NaOH solution and stirring, maintaining the pH value at 9.5 for 20 min. At this time, [ZrO(OH)]2SO4 turns into ZrO(OH)2, SO4 2- The desorbed product enters the solution and is diluted with 80L of water. After settling for 10 minutes, the supernatant is concentrated using a ceramic membrane device, and Na2SO4 is washed out with the effluent. The ZrO(OH)2 concentrated slurry is returned, and washed with water - settled - concentrated six times until the conductivity of the effluent is less than 20μs / cm. The ZrO(OH)2 concentrated slurry is returned to step (3) for adsorption, consuming about 480L of water and collecting about 480L of desorption wastewater.
[0087] (8) The desorbed wastewater in step (7) is recovered and concentrated using a high-pressure nanofiltration membrane with a molecular weight of 500D. The membrane inlet pressure is gradually increased from 2.0 MPa to 8.0 MPa. After concentration, the concentrated solution is a Na2SO4 solution with a content of up to 14.2 wt%, about 180 L (210 kg), which can be used as a dyeing salt for dyeing the dye variety. The water produced is about 300 L, and the conductivity is 14.5 μs / cm, which can be reused in step (4) or step (5).
[0088] (9) The total water used in the above method is about 480L+750L+480L=1710L, which is about 1.90 times the volume of the raw material liquid, and the wastewater is recycled and reused. Finally, 408kg of 30wt%CI Reactive Orange 140 salt-free dye paste is detected. - Ion content is 0, SO42- The content is 0, and the dye yield is as high as 98.71%.
[0089] Example 2
[0090] A method for preparing a salt-free dye paste comprises the following steps:
[0091] (1) Take 1000 kg (about 880 L) of CI active black 5 liquid, use ultraviolet spectrophotometer to detect the content, and use ion chromatography to detect ions. It is found that the dye content of the crude dye (including dye, salt, unreacted products, by-products and mechanical impurities) obtained by drying the liquid is about 68.21 wt%, the dye content of the liquid is 16.42 wt%, and SO4 2- Content 29025ppm (1kg of liquid contains 29025mg of SO4 2- ), the calculated mass of Na2SO4 is 42.93kg, accounting for 19.56wt% of the crude dye, Cl - Content 15000ppm (1kg of liquid contains 15000mg of Cl - ), the calculated mass of NaCl is 24.70kg, accounting for 11.26wt% of the crude dye.
[0092] (2) The feed liquid in step (1) is pretreated, and the filtrate is collected by filtering with a hollow fiber ultrafiltration membrane. The hollow fiber ultrafiltration membrane has a molecular weight cutoff of 100,000 and an inlet pressure of 0.10 MPa. The filtration is carried out at room temperature and in a cross-flow manner.
[0093] (3) The filtrate in step (2) is subjected to an adsorption reaction according to SO4 2- The amount of ions is 302.34 mol, so that ZrO(OH)2 and SO4 2- The molar ratio is 5:1, and the amount of ZrO(OH)2 added is about 213.15 kg. HCl is added dropwise while stirring, and the pH value is controlled at 2-3 to allow the liquid to fully contact and react with the solid powder. The reaction lasts for 15 minutes, and a sample is taken to detect SO4 2- The content is 0, and the adsorption slurry is obtained.
[0094] (4) The adsorption slurry in step (3) was naturally settled for 30 minutes, and the supernatant was concentrated using a ceramic membrane. The pore size of the ceramic membrane was 20 nm, and the membrane assembly could completely intercept ZrO(OH)2 and [ZrO(OH)]2SO4. About 110 L of concentrated slurry was obtained on the concentrated liquid side. The concentrated slurry was returned to the sedimentation tank, 110 L of water was added, stirred, and then naturally settled. The supernatant was concentrated by membrane. After 5 cycles of sedimentation-supernatant concentration-concentrated slurry with water, stirred, washed, and settled, about 550 L of water was consumed, the effluent was basically colorless, and the total volume of the effluent was about 1320 L. [ZrO(OH)]2SO4 concentrated slurry was obtained on the concentrated liquid side.
[0095] (5) The pH of the permeate in step (4) was adjusted to the initial value of the raw material solution (CI active black 5 liquid), and desalted using a 300D nanofiltration membrane with the membrane inlet pressure controlled at 2.0 MPa. It was first concentrated to about 500 L, and then desalted with constant volume water replenishment of about 950 L. The Cl - The ion content is 0ppm, the desalination is qualified, and the material is concentrated to obtain about 390L (460kg) of 35wt% CI reactive black 5 salt-free dye paste, consuming about 950L of water, and the total volume of desalination wastewater is about 1880L.
[0096] (6) The desalinated wastewater in step (5) is then concentrated by high-pressure reverse osmosis. The membrane pressure is initially 2.5 MPa and gradually increased to 8.0 MPa. After concentration, the concentrated solution is about 300 L (340 kg), with a NaCl content of 6.95 wt% and a dye concentration of 0.19 wt%. The obtained NaCl solution can be used in the salting-out process after the synthesis of the dye to achieve salt reuse. The produced water is about 1580 L with a conductivity of 15.5 μs / cm, which can be reused in step (4) or step (5).
[0097] (7) Desorb the [ZrO(OH)]2SO4 concentrated slurry in step (4) by adding 15 wt% NaOH solution and stirring, maintaining the pH value at 9.5 for 20 min. At this time, [ZrO(OH)]2SO4 turns into ZrO(OH)2, SO4 2- The desorbed product enters the solution and is diluted with 110L of water. After settling for 10 minutes, the supernatant is concentrated using a ceramic membrane device, and Na2SO4 is washed out with the effluent. The ZrO(OH)2 concentrated slurry is returned, and washed with water - settled - concentrated five times until the conductivity of the effluent is less than 20μs / cm. The ZrO(OH)2 concentrated slurry is returned to step (3) for adsorption, consuming about 550L of water and collecting about 550L of desorption wastewater.
[0098] (8) The desorption wastewater in step (7) is recovered and concentrated using a high-pressure nanofiltration membrane with a molecular weight of 500D. The membrane inlet pressure is gradually increased from 2.0 MPa to 8.0 MPa. After concentration, the concentrated solution is about 280 L (298 kg) of a Na2SO4 solution with a content of up to 13.90 wt%, which is used as a dyeing salt in the dip dyeing and printing roller dyeing of the dye variety. The water produced is about 270 L and the conductivity is 25.5 μs / cm, which can be reused in step (4) or step (5).
[0099] (9) The total water used in the above method is about 550L+950L+550L=2050L, which is about 2.33 times the volume of the raw material liquid, and the wastewater is recycled and reused. Finally, 467kg of 35wt% active black 5 salt-free dye paste is detected, Cl -Ion content is 0, SO4 2- The content is 0 and the dye recovery rate is as high as 99.50%.
[0100] Example 3
[0101] A method for preparing a salt-free dye paste comprises the following steps:
[0102] (1) Take 100 kg of CI Acid Yellow 23 coarse powder and dissolve it in 1200 L of water to obtain CI Acid Yellow 23 liquid. Acid Yellow 23 is a small molecular weight dye with good solubility. This dye can pass through the membrane more easily. Using the membrane method will cause a large loss of the dye.
[0103] Using UV spectrophotometer and ion chromatography, it was found that the dye content in the coarse powder was about 66.33%, the dye content in the liquid was 5.10wt%, and SO4 2- Content 9603ppm (1kg of liquid contains 9603mg of SO4 2- ), calculated to contain 18.46kg of Na2SO4, accounting for 18.46wt% of the crude dye, Cl - Content 6507ppm (1kg of liquid contains 6507mg of Cl - ), the calculated mass of NaCl is 13.94kg, accounting for 13.94wt% of the crude dye.
[0104] (2) The feed liquid in step (1) is pretreated, and the filtrate is collected by filtering with a hollow fiber microfiltration membrane. The pore size of the hollow fiber microfiltration membrane is 0.2 μm, the inlet pressure is 0.2 MPa, and the filtration is carried out at room temperature in a cross-flow manner.
[0105] (3) The filtrate in step (2) is subjected to an adsorption reaction according to SO4 2- The amount of ions is 130.04 mol, so that ZrO(OH)2 and SO4 2- The molar ratio is 5:1, and the amount of ZrO(OH)2 added is about 91.68 kg. HCl is added dropwise while stirring, and the pH value is controlled at 2-3 to allow the liquid to fully contact and react with the solid powder. The reaction lasts for 15 minutes, and a sample is taken to detect SO4 2- The content is 0, and the adsorption slurry is obtained.
[0106] (4) The adsorption slurry in step (3) was naturally settled for 30 minutes, and the supernatant was concentrated using a ceramic membrane. The sedimentation volume was about 120 L. The pore size of the ceramic membrane was 20 nm. The membrane assembly could completely intercept ZrO(OH)2 and [ZrO(OH)]2SO4. About 60 L of concentrated slurry was obtained on the concentrated liquid side. The concentrated slurry was returned to the sedimentation tank, 60 L of water was added, stirred, and then naturally settled. The supernatant was concentrated by membrane. After 6 rounds of sedimentation-supernatant concentration-concentrated slurry with water, stirred, washed, and settled, the permeate was basically colorless. The pH of the permeate was adjusted to 6.5 and entered the next nanofiltration step. About 360 L of water was consumed. The permeate was basically colorless. The total volume of the permeate was about 1500 L. A [ZrO(OH)]2SO4 concentrated slurry was obtained on the concentrated liquid side.
[0107] (5) The pH of the permeate in step (4) was adjusted to the starting value of the raw material solution (CI Acid Yellow 23 solution), and desalted using a 300D nanofiltration membrane with the membrane inlet pressure controlled at 2.0 MPa. The solution was first concentrated to about 600 L, and then desalted by adding water at a constant volume of about 800 L. The Cl - The ion content was 0ppm, the desalination was qualified, and the material was concentrated to obtain about 400L (437kg) of 15wt% acid yellow 23 salt-free dye paste, and the total volume of desalination wastewater was about 1900L.
[0108] (6) The desalinated wastewater in step (5) is then concentrated by high-pressure reverse osmosis. The membrane pressure is initially 2.5 MPa and gradually increased to 8.0 MPa. After concentration, the concentrated solution is about 160 L (190 kg) and the NaCl content is 7.02 wt%. The obtained NaCl solution can be used in the salting-out process after the synthesis of the dye to achieve salt reuse. The produced water is about 1740 L and the conductivity is 17.5 μs / cm, which can be reused in step (4) or step (5).
[0109] (7) Desorb the [ZrO(OH)]2SO4 concentrated slurry in step (4) by adding 15 wt% NaOH solution and stirring, maintaining the pH value at 9.5 for 20 min. At this time, [ZrO(OH)]2SO4 turns into ZrO(OH)2, SO4 2- The desorbed product enters the solution and is diluted with 60L of water. After settling for 10 minutes, the supernatant is concentrated using a ceramic membrane device, and Na2SO4 is washed out with the effluent. The ZrO(OH)2 concentrated slurry is returned, and washed with water - settled - concentrated six times until the conductivity of the effluent is less than 20μs / cm. The ZrO(OH)2 concentrated slurry is continued to return to step (3) for adsorption, consuming about 360L of water and collecting about 360L of desorption wastewater.
[0110] (8) The desorption wastewater in step (7) is recovered and concentrated by a high-pressure nanofiltration membrane with a molecular weight of 500D. The membrane inlet pressure is gradually increased from 2.0 MPa to 8.0 MPa. After concentration, the concentrated solution is a Na2SO4 solution with a content of up to 12.94 wt%, about 110 L (140 kg), which can be used as a dyeing accelerator salt for dyeing this dye variety. The water produced is about 250 L, and the conductivity is 19.5 μs / cm, which can be reused in step (4) or step (5).
[0111] (9) The total water used in the above method is about 360L+800L+360L=1520L, which is about 1.26 times the volume of the raw material liquid, and the waste water is recycled and reused. Finally, 437kg of 15wt% acid yellow 23 salt-free dye paste is detected, Cl - Ion content is 0, SO4 2- The content is 0 and the dye recovery rate is as high as 98.82%.
[0112] In the present invention, the term "some embodiments" and the like means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0113] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A method for preparing a salt-free dye paste, It is characterized in that The steps include: (1) Pretreatment: Filter the crude dye liquid through a microfiltration membrane or ultrafiltration membrane to remove mechanical impurities and colloids; (2) Adsorption reaction: ZrO(OH) 2 As an ion exchanger, it absorbs SO in the crude dye solution. 4 2- , will SO 4 2- Replaced by Cl - , in the adsorption reaction, ZrO(OH) 2 with SO 4 2- The molar ratio is 4-6:1, the pH is adjusted to 2-3 with HCl, the temperature is 20-40°C, and the reaction is fully carried out for 15-30 minutes to obtain an adsorption slurry; (3) Sedimentation, concentration and washing: The adsorption slurry in step (2) is naturally sedimented, and after sedimentation, the supernatant is concentrated using a ceramic membrane or a tubular membrane to obtain [ZrO(OH)] 2 SO 4 Concentrate and permeate, [ZrO(OH)] 2 SO 4 The concentrated slurry is stirred and washed with water and then naturally settled. Repeat the natural sedimentation and supernatant concentration. [ZrO(OH)] 2 SO 4 The concentrated slurry is stirred and washed with water for 5 to 6 times until the permeate is basically colorless, and then the washing is stopped. All the permeate is collected and entered into the nanofiltration step; (4) Nanofiltration: The permeate in step (3) is subjected to a nanofiltration membrane to remove monovalent salts. After the desalination is qualified, the material is concentrated to obtain a salt-free dye paste; (5) Desalination wastewater recovery: The desalination wastewater after desalination in step (4) is concentrated by high-pressure reverse osmosis to obtain a NaCl solution with a content of 6 to 8.5 wt %. The water generated during the concentration process is reused as make-up water in step (3) or step (4); (6) Desorption reaction: [ZrO(OH)] 2 SO 4 The concentrated slurry was desorbed, water was added, NaOH was added dropwise, and the pH value was maintained at 9-10 for 15-30 min. 2 The concentrated slurry is diluted with water for washing, and the supernatant is concentrated using a ceramic membrane or tubular membrane to wash out the SO 4 2- , repeating ZrO(OH) 2 The concentrated slurry is diluted with water and washed - the supernatant is concentrated for multiple times. When the conductivity of the permeate is lower than 20μs / cm, the washing is stopped. ZrO(OH) 2 The concentrated slurry is then returned to the system of step (2) for adsorption; (7) Desorption wastewater recovery: The desorption wastewater in step (6) is concentrated by high-pressure nanofiltration to a concentration of 12-15 wt% Na 2 SO 4 The water produced during the concentration process is used as make-up water and then recycled to step (3) or step (4).
2. The method for preparing a salt-free dye paste according to claim 1, It is characterized in that In the crude dye solution, the concentration of the dye is 5-45wt%.
3. The method for preparing a salt-free dye paste according to claim 2, It is characterized in that The dye is a water-soluble dye with a molecular weight of 300-800.
4. The method for preparing a salt-free dye paste according to claim 2, It is characterized in that In the crude dye solution, the dye concentration is 5-25wt%; Taking the crude dye product after drying as 100%, the dye accounts for 50-85wt% and the salt accounts for 15-50wt%, among which Na 2 SO 4 The proportion is 10~30wt%, and NaCl accounts for 5~20wt%.
5. The method for preparing a salt-free dye paste according to claim 2, It is characterized in that The dye is one or more of CI Reactive Orange 140, CI Reactive Black 5 and CI Acid Yellow 23.
6. The method for preparing a salt-free dye paste according to claim 1, It is characterized in that In step (1), The microfiltration membrane is a flat membrane, a filter element or a hollow fiber microfiltration form, with a pore size of 0.1-1.0 μm, an inlet pressure of 0.10-0.30 MPa, and is carried out at room temperature in a cross-flow manner; The ultrafiltration membrane adopts hollow fiber ultrafiltration, the ultrafiltration cut-off molecular weight is 50,000-500,000, the inlet pressure is 0.05-0.15Mpa, and the filtration is carried out at room temperature in a cross-flow manner.
7. The method for preparing a salt-free dye paste according to claim 1, It is characterized in that In step (2), the ZrO(OH) 2 The particle size is 50~70μm.
8. The method for preparing a salt-free dye paste according to claim 1, It is characterized in that In step (3), the pore size of the ceramic membrane or tubular membrane is 0.01-0.05 μm, [ZrO(OH)] 2 SO 4 During the process of adding water to the concentrated slurry and stirring and washing, the amount of water added each time is [ZrO(OH)] 2 SO 4 0.9~1.1 times the volume of the concentrated slurry.
9. The method for preparing a salt-free dye paste according to claim 1, It is characterized in that Step (4) is: first concentrating the permeate of step (3), then adding water to desalinate at a constant volume, keeping the amount of membrane permeate during the desalination process equal to the amount of water added to the concentrated solution in the feed tank, using a 300-500D nanofiltration membrane to remove monovalent salt, the membrane inlet pressure is 1.0-3.0MPa, using ion chromatography to determine the ion content in the concentrated solution, and concentrating the material after the desalination is qualified to prepare a salt-free dye paste with a concentration of 15-40wt%.
10. The method for preparing a salt-free dye paste according to claim 4, It is characterized in that In step (5), the membrane inlet pressure of the high-pressure reverse osmosis is 2.5-8.0 MPa, and the NaCl solution with a content of 6%-8.5wt% obtained after concentration is used in the salting-out process after the dye is synthesized; And / or, in step (6), repeat ZrO(OH) 2 The number of steps of diluting the concentrated slurry with water and washing and concentrating the supernatant is 5 to 6 times. 2 The concentrated slurry is diluted with water. The amount of water added in the washing step is ZrO(OH) 2 0.9~1.1 times the volume of the concentrated slurry; And / or, in step (7), the high pressure nanofiltration membrane used in the high pressure nanofiltration has a molecular weight cutoff of 500-800D, the membrane inlet pressure is 2.0-8.0MPa, and the Na content obtained after concentration is 12-15wt% 2 SO 4 The solution is used as an accelerating salt for dyeing with this dye.
Citation Information
Patent Citations
Salt-free dye and preparation method thereof
CN106280549A
Sewage discharge free reparation method of salt-free dye
CN108003657A
Cationic dye wastewater separation method
CN108358371A
Method for producing organic pigment microparticles
US20180230310A1