Mooring cover and manufacturing method thereof

Through the thermoforming combination of the thermoplastic elastomer layer and the filling layer, the tethering layer is threaded and seamed on the cover body, which solves the problems of low tethering strength and poor air tightness of the tethered cover, and achieves higher bonding strength and air tightness. .

CN118816631APending Publication Date: 2024-10-22713TH RES INST OF CHINA STATE SHIPBUILDING CORP LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410880436.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-02
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing tethered caps have low tethering strength and poor air tightness, and are difficult to form by manual wet molding. The injection molding process can easily lead to local uneven glue and bubble defects.

Method used

The thermoplastic elastomer layer and the filling layer are combined by hot pressing, and the tethering layer is threaded and seamed on the cover body. The filling layer is a thermoplastic elastomer film to ensure the fixed connection between the tethering layer and the cover body, avoid separation, and improve airflow. confidentiality.

Benefits of technology

The bonding strength and air tightness of the tethering cover are improved, separation and bubble defects are avoided, and better tethering effect and sealing performance are achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118816631A_ABST
    Figure CN118816631A_ABST
Patent Text Reader

Abstract

The invention relates to a launching device for launching a projectile through a self pipe, in particular to a mooring cover and a manufacturing method thereof. According to the novel mooring cover manufacturing method, after the mooring layer containing the thermoplastic elastomer layer is laid and covers the corresponding frame opening position, the mooring layer is sewn to the cover body through the weaving line penetrating through the mooring hole, it is guaranteed that the mooring layer and the cover body are fixedly connected, and the filling layer is wrapped in the mooring layer; and then the cover body, the mooring layer and the filling layer are combined into a whole through hot press molding. The mooring cover prepared by the method not only has higher mooring strength, but also has good air tightness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a launching device for launching projectiles by using a self-tube, and in particular to a mooring cover and a manufacturing method thereof. Background Art

[0002] The launch box end cover is an important component of the launch device. Currently, the launch box covers mainly include mechanical covers, blasting covers, and composite fragile covers. Mechanical covers usually require a special power system and servo system, which increases the load of the entire launch system and takes a long time to open. Although the blasting cover is not opened by servo control and responds quickly, it has a high cost for one-time use, is complex to maintain, and the electronic components inside the launch box are easily damaged during the explosion. The composite fragile cover is the most widely used and used box cover. It has the characteristics of light weight and fast response. Its structural strength meets daily requirements, and it can be opened by ejecting the projectile or by the launch airflow and shock wave during launch, eliminating the process of electronic unpacking, greatly improving the launch efficiency, and meeting the needs for rapid launch.

[0003] The Chinese invention patent with application publication number CN104864773A discloses a directional ejection composite material fragile cover and its preparation method. The fragile cover disclosed in the patent includes a frame and an ejection body, and the junction of the frame and the ejection body is a separation zone and a connection zone respectively. The separation zone is the area where the frame and the ejection body are glued after being separated. In this area, there is a rectangular groove on the inner side of the edge of the ejection body after separation. AB glue is filled in the rectangular groove. The edge of the ejection body is glued to the edge of the frame by AB glue. The edge of the ejection body and the edge of the frame are respectively attached with inner fiber cloth strips and outer fiber cloth strips by epoxy resin glue on the inside and outside. The fragile cover in the technical solution disclosed in the patent has a simple structure, light weight, and convenient operation, and can be directional thrown under the action of airflow. However, the technical solution disclosed in the patent will throw out the fragments of the broken fragile cover, and the fragment throwing process will cause safety hazards to other equipment around the launcher.

[0004] In response to the above problems, a Chinese invention patent with application announcement number CN112644111B discloses a composite fragile cover with a mooring function and a method for preparing the same. The patent describes in detail how to prepare a mooring cover by manual wet molding. The patent discloses that the glass fiber fabric that is not impregnated with epoxy resin still has a certain flexibility to ensure that the cover can be turned over and moored to the flange after opening. However, the glass fiber fabric area that is not impregnated with resin will become the main factor affecting the air tightness of the cover. In addition, the wet molding process is also extremely difficult in actual operation. Since the resin prepolymer before curing molding is in liquid state, the flowing resin during the curing process will inevitably penetrate the reserved fiber fabric area. The fabric impregnated with resin will lose its flexibility, which will seriously affect the mooring function of the cover.

[0005] The Chinese invention patent application with application publication number CN116481379A disclosed a launch box cover, which is an improvement on the problems existing in the Chinese invention patent with application publication number CN112644111B. As shown in Figures 8-9 of the specification of the invention patent application, the launch box cover includes a regular polygonal cover body, the cover body includes a flange interface area and a body sub-petal, the body sub-petal has four and corresponds to the four sides of the regular polygonal cover body, there is a frame opening connected to the opening between adjacent body sub-petals, the edge of the body sub-petal around the frame opening has a thinned portion, and the thinned portion is provided with a retention hole. During manufacturing, fabric is covered on both sides of the cover body, and then polyurethane prepolymer is used to encapsulate the whole through an injection process, and the flowing elastic colloid prepolymer can fill the opening and the frame opening. The cured elastic colloid includes polyurethane laid in sequence along the thickness direction of the cover body and a retention layer covering the corresponding positions of the flange connection area, the elastic deformation area, and the sub-petal connection area of ​​the cover body.

[0006] However, the applicant's process test found that after the rigid cover body is encapsulated with liquid elastomer prepolymer by injection molding, bubbles of uncertain size are generally present in the finished product, which also reduces the airtightness of the cover body to a certain extent. Moreover, in some special use cases where the cover body bears a large pressure, the launch box cover body will appear to break and separate from the elastic colloid and fly out when in use. In severe cases, the body sub-petal and the elastic colloid will tear and separate at the flange connection area, and cannot achieve a good tethering effect. Summary of the invention

[0007] The purpose of the present invention is to provide a new method for manufacturing a tethered cover, so as to solve the problems of low tethering strength and poor air tightness in current tethered cover products. At the same time, the purpose of the present invention is also to provide a tethered cover made by the above-mentioned tethered cover manufacturing method, so as to solve the problems of low tethering strength and poor air tightness in existing tethered cover products.

[0008] The method for manufacturing the tethered cover of the present invention comprises the following steps: 1) Filling the frame opening of the prepared cover body with a filling layer that matches the shape of the frame opening; 2) Covering the two sides of the cover body corresponding to each frame opening with a prepared retention layer including a thermoplastic elastomer layer, and making the retention layer cover the filling layer, the thinned area at the edge of the frame opening, and the flange connection area of ​​the frame opening corresponding to the cover body; 3) Sewing the tie-down layer to the cover body by passing the weaving thread through the tie-down holes at the edge of the frame opening; 4) The tie-down layer is integrated with the cover body and the filling layer by hot pressing.

[0009] Furthermore, a thermoplastic elastomer column is filled in the mooring hole, the braided wire passes through the thermoplastic elastomer column in the mooring hole, and the mooring layer and the thermoplastic elastomer column are combined into one after hot pressing.

[0010] Furthermore, after the thermoplastic elastomer column is filled in the mooring hole and before the mooring layer is coated on the cover body, the two side surfaces of the cover body are cleaned, a structural adhesive layer is coated and a thermoplastic elastomer film is laid to cover the two side surfaces of the cover body, and then heated and cured into an integrated structure.

[0011] Furthermore, the filling layer is a thermoplastic elastomer film, and the tethering layer and the thermoplastic elastomer film are integrated into one after hot pressing.

[0012] Furthermore, the size and shape of the tethering layer corresponding to one frame opening are sufficient to enable it to bypass the flange connection area of ​​the cover body and cover the other side of the cover body after covering one side of the cover body.

[0013] Furthermore, when manufacturing the mooring layer, a redundant avoidance groove corresponding to and connected to the annular weak area is formed at the inner side of the mooring layer adjacent to the flange connection area.

[0014] Furthermore, when manufacturing the mooring layer, the aramid fabric thin layer and the thermoplastic elastomer film of the required size and shape are laid in sequence and then coated on the core mold, and the mooring layer is formed by vacuum bag hot pressing.

[0015] The present invention provides a new method for manufacturing a mooring cover. After laying a mooring layer including a thermoplastic elastomer layer to cover the corresponding frame opening position, the mooring layer is first sewn to the cover body by means of a woven thread passing through the mooring hole to ensure a fixed connection between the mooring layer and the cover body and to wrap the filling layer inside. Then, the cover body, the mooring layer and the filling layer are combined into one by means of hot pressing. The mooring cover manufactured in this way can not only hot press the mooring layer and the cover body into one, but also each interface has a high bonding strength and good air tightness. At the same time, the mooring layer and the cover body are also sewn together by means of woven thread, and the connection strength is higher. In this way, the separation of the body sub-petal and the mooring layer is avoided, and a better mooring effect is achieved.

[0016] The mooring cover of the present invention comprises a cover body, a frame opening of the cover body is filled with a filling layer with a shape-fitting shape, both sides of the cover body have mooring layers covering the flange connection area, the filling layer and the thinned area of ​​the frame opening edge, the mooring layer is sewn to the cover body by woven thread passing through the mooring holes in the thinned area, the mooring layer comprises a thermoplastic elastomer layer, and the filling layer, the mooring layer and the cover body are an integral structure formed by hot pressing.

[0017] Furthermore, the mooring hole is filled with a thermoplastic elastomer column, the woven wire passes through the thermoplastic elastomer column, and the mooring layer and the thermoplastic elastomer column are hot-pressed and combined into an integrated structure.

[0018] Furthermore, the tethered layer corresponding to one frame opening bypasses the flange connection area of ​​the cover body and covers the other side of the cover body after covering one side of the cover body.

[0019] Furthermore, a redundant avoidance groove corresponding to and connected to the annular weak area is provided at an inner side of the mooring layer adjacent to the flange connection area.

[0020] Furthermore, the filling layer is a thermoplastic elastomer film, and the mooring layer and the filling layer are hot-pressed into an integrated structure.

[0021] The present invention improves the existing mooring cover. The mooring layer can be sewn to the cover body by the woven thread passing through the mooring hole, ensuring the fixed connection between the mooring layer and the cover body and covering the filling layer. The cover body, the mooring layer and the filling layer are an integrated structure of hot pressing integrity. The mooring cover of such an integrated structure has a high bonding strength. The mooring layer and the cover body are also sewn together by the woven thread, and the connection strength is higher. In addition, due to the use of thermoplastic elastomer, the generation of manual wet molding and local glue unevenness and internal bubble defects of injection molded products is fundamentally eliminated, ensuring that the mooring cover achieves a better mooring effect while also having a high air tightness. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a front view of the first embodiment of the tethered cover of the present invention; Figure 2 A schematic diagram of a tethered cover when assembling a lightweight tethering assembly onto a cover body; Figure 3 It is a schematic diagram when making the tethered layer; Figure 4 It is a schematic diagram of hot pressing the tethering layer; Figure 5 Schematic diagram of the principle of forming a surface covering layer.

[0023] In the figure: 1. fixed ring body; 10. main body sub-petal; 11. thinning area; 12. radial thinning area; 13. annular thinning area; 100. fixed connection hole; 110. mooring hole; 2. filling layer; 3. mooring layer; 31. redundant avoidance groove; 4. weaving line; 5. surface covering layer; 60. mooring cover lower mold; 61. mooring cover upper mold; 62. side block; 7. mooring layer assembly mold; 70. flat plate lower mold; 71. flat plate upper mold: 72. mooring layer core mold: 73. forming side pressure block; 80. vacuum device bottom plate; 81. vacuum bag; 82. breathable felt; 83. demoulding cloth; 84. thermocouple; 85. pressure gauge; 86. sealing strip. DETAILED DESCRIPTION

[0024] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.

[0025] The applicant has studied the molding process of the existing mooring cover for the launch box and found that it is difficult to ensure the stability of the deformation ability of the mooring root of the product by hand lay-up molding, and it is easy to cause local uneven glue liquid and a large number of bubbles in the product due to insufficient exhaust by injection molding. These defects will become the main factors affecting the local mooring strength and air tightness of the cover. The present invention aims to solve the problem of finished product defects such as insufficient mooring strength and poor air tightness in the existing mooring cover preparation method.

[0026] Based on the above concept, more specific different embodiments are provided below for illustration.

[0027] like Figure 1-2 As shown, the mooring cover of the present invention includes a regular polygonal cover body, which includes a fixing ring body 1 at the edge and a body sub-petal 10, wherein the fixing ring body 1 has a certain number of fixing connection holes 100 so as to be fixedly connected to the end of the launch tube through the fixing connection holes 100, and the specific shape of the fixing ring body 1 can be determined according to the shape of the launch tube. The main body sub-petal is provided with a radial thinning area 12 and an annular thinning area extending along the fixed ring body 1. The thinning area is a groove structure, that is, a crackable groove structure. In this way, when the mooring cover is broken, it can be split along the crackable groove to form multiple petals, and will not form irregular fragments; the main body sub-petal is provided with a frame opening, and the frame opening is filled with a lightweight mooring component. The lightweight mooring component is fixedly connected to the fixed ring body 1 and the main body sub-petal 10, and has a foldable part extending from the fixed ring body 1 adjacent to the fixed ring body 1. The foldable part is used to turn the petals moored by the lightweight mooring component outward when the projectile is launched, and the whole makes way for the through hole of the launch tube to allow the projectile to fly out. With such a structure, when the mooring cover is broken into petals during use, each petal can be moored by the lightweight mooring component to the fixed ring body 1 fixed indirectly at the end of the launch tube, and will not fly out, thereby achieving a mooring effect.

[0028] The lightweight mooring assembly as a whole needs to fill the opening of the frame to ensure the sealing of the entire mooring cover. At the same time, it also needs to have a certain structural strength to withstand the high temperature and high pressure in the launch tube. Furthermore, the lightweight mooring assembly also needs to be able to make the petals formed after the mooring cover rupture and flip outward relative to the fixed ring body 1 to ensure smooth launch of the projectile.

[0029] In this embodiment, the lightweight mooring assembly includes a filling layer 2 and a mooring layer 3 covering the surface of the filling layer 2. The mooring layer 3 is fixedly connected to the fixed ring body 1 and the main body sub-petal 10 to fix the filling layer 2 in the frame opening between the two mooring layers 3. This method can more reliably achieve the fixed connection between the lightweight mooring assembly and the cover body, while ensuring a better sealing effect. In this embodiment, the mooring layer 3 mainly plays a mooring role. The filling layer 2 mainly plays a role of filling the frame opening and reducing weight. The mooring layer 3 has a flippable part adjacent to the fixed ring body 1.

[0030] Two side surfaces of the main body sub-petal 10 are provided with thinning areas 11 at the edge portions near the frame opening, the edge of the mooring layer 3 covers the thinning areas 11 and the outer side surface is flush with the surface of the main body sub-petal 10, and the design of the thinning areas 11 is not only to achieve the flushness of the light-weight mooring component with the surface of the cover body, but also to facilitate the connection between the mooring layer 3 and the main body sub-petal 10. Mooring holes 110 are provided on the thinning areas, and the mooring layer 3 and the main body sub-petal 10 are sewn and fixed at the thinning areas 11 by the weaving thread 4 passing through the mooring holes 110. The design of the mooring holes 110 facilitates the weaving thread 4 to pass through the hard and brittle cover body, and the number and arrangement of the mooring holes 110 are determined according to needs.

[0031] Moreover, the mooring layer 3 includes a thermoplastic elastomer layer. After the mooring layer 3 is covered on the filling layer 2 and the cover body 1, the filling layer, the mooring layer and the cover body can be hot-pressed into an integrated structure by hot pressing, thereby further ensuring the bonding strength between the mooring layer and the body sub-petal. In one embodiment, the mooring layer is a membrane structure formed by alternately laying aramid fabric layers and thermoplastic polyurethane layers and hot pressing.

[0032] Based on the above concept or the above embodiment, in another embodiment, in order to ensure the pressure-bearing seal at the mooring hole 110, in this embodiment, preferably, a thermoplastic elastomer column, such as a thermoplastic polyurethane column, is filled in the mooring hole 110, which can play a filling and sealing role and is convenient for the threading needle to pass through. In this way, the mooring layer and the thermoplastic elastomer column can also be combined into an integrated structure during hot pressing. It is ensured that at each mooring hole, not only is there a woven wire connecting the main body sub-valve and the mooring layer, but also the filled thermoplastic elastomer column and the mooring layer are hot-pressed and combined into one, and the bonding strength is higher.

[0033] Based on the above concept or the above embodiment, in another embodiment, the filling layer is a thermoplastic elastomer film, such as a polyurethane film, so that the mooring layer and the filling layer can be combined into an integrated structure during hot pressing, so that the overall integration of the main body sub-petals and the lightweight mooring assembly is better.

[0034] At the position of the frame opening of each main body sub-petal, the retention layer 3 covering the two sides can be two separate parts, and the two parts can be connected to the cover body respectively, or of course, it can be a whole. Figure 1-3 As shown, the same mooring layer 3 covers both sides of the same filling layer 2 at the same time and has a wrapping portion that bypasses the fixed ring body 1, that is, the mooring layer 3 is an integral diaphragm structure. During manufacturing, firstly, half of the mooring layer 3 is laid corresponding to the frame opening on the cover body, and then the filling layer 2 is filled on the mooring layer 3 corresponding to the frame opening, and then the other half of the mooring layer 3 is bypassed from the outside of the fixed ring body 1 to the other side of the cover body and covered on the filling layer 2, and then the mooring layer 3 and the cover body are fixedly connected. In this way, the connection between the mooring layer 3 and the cover body is more reliable, and the mooring effect is more reliable. Of course, a perforated structure for the connecting bolts to pass through needs to be provided on the mooring layer 3 at the position corresponding to the fixed connection hole 100.

[0035] The overall surface of the mooring layer 3 can be a plane, and its flexibility can be used to achieve the flipping of each petal after rupture. However, this may cause pulling interference between each petal and the fixed ring body 1, affecting the flexibility of flipping. In some experiments, it was found that when the mooring cover is under greater pressure, this part is also easy to be torn. This is also the reason why the main body sub-petals and the elastic colloid as a whole are torn and separated at the flange connection area in the prior art. As a preferred embodiment, a redundant avoidance groove corresponding to the annular weak area is provided at the inner side of the mooring layer adjacent to the flange connection area, that is, a redundant avoidance groove 31 extending along the edge of the fixed ring body 1 is provided on the mooring layer 3 at the portion adjacent to the fixed ring body 1, and the redundant avoidance groove 31 constitutes the above-mentioned foldable part, such as Figure 1-3 As shown in Figures 5 and 6, the redundant avoidance groove 31 is linear and extends along one side of the square fixed ring body 1. The redundant avoidance groove 31 can provide a certain amount of flipping avoidance space, and at the same time provide a certain amount of redundant length for the mooring layer 3, which is also convenient for flipping. It can be clearly seen from the accompanying drawings that the redundant avoidance groove 31 is just aligned with the annular thinning area, which is conducive to flipping.

[0036] In addition, as a better embodiment, in order to protect the connection structure between the mooring layer 3 and the cover body from damage, the cover body and the outer side of the mooring layer 3 are provided with a surface covering layer 5, such as a hot-pressed polyurethane film or other bonded protective film layer. In this way, on the one hand, the mooring layer 3 and the cover body are covered as a whole, and at the same time, the surface integrity of the entire mooring cover is better and the air tightness is better.

[0037] The following provides a method for manufacturing the tie-down cover of the present invention.

[0038] Specifically, the cover body, the tethering layer 3 and the filling layer 2 are manufactured separately, and then the three are assembled as a whole, and finally the surface covering layer 5 is formed on the cover body by processing.

[0039] Among them, the cover body adopts the existing manufacturing process, for example, it is made by compression molding. After the structure is formed, the surface of the cover body is roughened with 150-mesh sandpaper, and then the surface is scratched clean with anhydrous ethanol. The mooring hole 110 of the cover body is filled with a thermoplastic elastomer column, such as a 5mm diameter polyurethane column, and the mooring hole 110 is filled, and then the structural adhesive layer is coated on the upper and lower surfaces of the cover body, and at the same time, a thermoplastic elastomer film is covered, such as a single-layer polyurethane film, and the adhesive layer is cured and formed by keeping warm at 120°C for 1h, so that the overall structural consistency of the cover body is better.

[0040] The filling layer 2 is made of a thermoplastic elastomer film, such as a thermoplastic polyurethane film, and the polyurethane film can be cut into a shape that matches the shape of the frame opening.

[0041] The tethered layer 3 is a tethered layer comprising a thermoplastic elastomer layer, wherein the thermoplastic elastomer layer can also be a polyurethane layer. The following specifically provides a method for manufacturing the tethered layer, which specifically includes the following steps: Figure 3-4As shown, first, the aramid fabric and thermoplastic polyurethane film raw materials of the required size and shape are cut respectively. The mooring layer 3 is formed by hot pressing two layers of thermoplastic polyurethane and the aramid fabric arranged between the two layers of thermoplastic polyurethane films. Of course, in other embodiments, the mooring layer unit can also be formed by thermoplastic polyurethane film + thermoplastic polyurethane film + aramid fabric + thermoplastic polyurethane film + thermoplastic polyurethane film. Those skilled in the art can adjust the ratio of thermoplastic polyurethane film to aramid fabric according to actual needs. Taking a vacuum bag hot pressing molding process as an example, a cut aramid fabric is placed between two cut thermoplastic polyurethane films to form the mooring layer 3 material, and then the mooring layer 3 material is coated on the mooring layer core mold, and then the mooring layer core mold with the mooring layer material is placed on the flat lower mold 70, the molding side pressure block is installed, and the flat upper mold is covered on it. Place the assembled mooring layer assembly mold 7 on the bottom plate 80 of the vacuum device, place a thermocouple 84 for detecting temperature and a vacuum nozzle on the edge of the mooring layer assembly mold 7, and cover the mooring layer assembly mold 7 with a demoulding cloth 83, a breathable felt 82, and a vacuum bag 81. A sealed sealing strip 86 is provided on the edge of the vacuum bag 81. First, check the air tightness of the vacuum bag 81, evacuate it to below -0.095MPa, turn off the vacuum for 10 minutes to ensure that the vacuum pressure is lower than 0.01MPa, otherwise re-press and tighten the sealing strip 86 to ensure that it is tightly sealed. Wrap the demoulding cloth 83 and the breathable felt 82 on the mooring layer assembly mold 7 to ensure that no polyurethane overflows from the mold to affect the separation of the mooring layer assembly mold 7 and the vacuum bag 81. Then send the wrapped mooring layer assembly mold 7 into the vacuum bag 81 and evacuate it, and send the evacuated vacuum bag 81 into the temperature control box. The temperature of the molding process is monitored by a thermocouple 84 and the temperature of the temperature control box is adjusted according to the hot pressing process system. The temperature is raised to 130°C at a heating rate of 1-1.5°C / min and kept at that temperature for 1 hour, and then cooled to room temperature at a cooling rate of 2-4°C / min before being taken out of the box and demoulded to obtain a retention layer 3.

[0042] The assembly process of the cover body, the mooring layer 3 and the filling layer 2 is as follows: half of the mooring layer 3 is placed in a corresponding position on one side of the cover body, the trimmed filling layer 2 is filled into the corresponding frame opening, the other half of the mooring layer 3 is passed around the fixing ring body 1 and covered to the corresponding position on the other side of the cover body, so that the filling layer 2 is completely covered in the frame opening, and then the weaving thread is used to sew along the mooring hole 110, and the thread is routed back and forth for several times to complete the sewing. The weaving thread can be made of double-strand aramid yarn, etc.

[0043] Finally, to ensure the air tightness of the product, a whole piece of polyurethane film is laid on the upper and lower surfaces of the overall structure formed in the previous step, and then the whole is placed on the mooring cover lower mold 60, the side block 62 is installed, and the mooring cover upper mold 61 is covered, and then the vacuum belt is applied and placed in a temperature control box for hot pressing. The hot pressing molding steps and process parameters of this step are the same as those of the mooring layer 3. After the hot pressing is completed, the product is demoulded, the overflow around the product is cleaned, and the fixed connection hole 100 is machined.

[0044] When the mooring cover of the present invention is used, it is fixed to the launch tube through the fixed connection hole 100. When the launcher is started, the air pressure in the launch tube increases, and the air pressure causes the mooring cover to break along the crack groove, and the petals formed after the breakage are turned outward and opened, and the mooring layer 3 is stretched. Since the mooring layer 3 is formed by combining aramid fabric and thermoplastic polyurethane, and the thermoplastic polyurethane has a large deformation property, after the launcher is completed, the thermoplastic polyurethane film can drive the broken cover body to reset and close the launch tube to prevent interference with the launch of other launch tubes.

[0045] Of course, the above-mentioned manufacturing method is a manufacturing method based on an optimal embodiment of the above-mentioned mooring cover. In the manufacturing methods of some other embodiments, such as the embodiment in which the mooring hole is not filled with a thermoplastic elastomer column, it is naturally not necessary to fill the mooring hole with a thermoplastic elastomer column. In some embodiments, the filling layer can also be other lightweight filling layers, not a thermoplastic elastomer material. In some embodiments, if the mooring layer corresponding to a main body sub-valve is a split structure, that is, the two parts cover the two sides of the cover body respectively, then during manufacturing, the mooring layers are laid on both sides of the cover body to cover the filling layer and the thinned area.

[0046] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. The patent protection scope of the present invention shall be based on the claims. All equivalent structural changes made using the contents of the description and drawings of the present invention should also be included in the protection scope of the present invention.

Claims

1. A method for manufacturing a tethered cover, characterized in that: The following steps are involved: 1) Filling the frame opening of the prepared cover body with a filling layer that matches the shape of the frame opening; 2) Covering the two sides of the cover body corresponding to each frame opening with a prepared retention layer including a thermoplastic elastomer layer, and making the retention layer cover the filling layer, the thinned area at the edge of the frame opening, and the flange connection area of ​​the frame opening corresponding to the cover body; 3) Sewing the tie-down layer to the cover body by passing the weaving thread through the tie-down holes at the edge of the frame opening; 4) The tie-down layer is integrated with the cover body and the filling layer by hot pressing.

2. The method for manufacturing a tethered cover according to claim 1, wherein The mooring hole is filled with a thermoplastic elastomer column, the braided wire passes through the thermoplastic elastomer column in the mooring hole, and the mooring layer and the thermoplastic elastomer column are combined into one after hot pressing.

3. The method for manufacturing a tethered cover according to claim 2, wherein After the thermoplastic elastomer column is filled in the mooring hole, before the mooring layer is coated on the cover body, the two side surfaces of the cover body are cleaned, a structural adhesive layer is coated, and a thermoplastic elastomer film is laid to cover the two side surfaces of the cover body, and then heated and cured into an integrated structure.

4. The method for manufacturing a tethered cover according to claim 1, wherein: The filling layer is a thermoplastic elastomer film, and the tethering layer and the thermoplastic elastomer film are integrated into one after hot pressing.

5. The method for manufacturing a tethered cover according to any one of claims 1 to 4, characterized in that: The size and shape of the tethering layer corresponding to one frame opening are sufficient to enable it to bypass the flange connection area of ​​the cover body after covering one side of the cover body and cover the other side of the cover body.

6. The method for manufacturing a tethered cover according to claim 5, wherein When manufacturing the mooring layer, a redundant avoidance groove corresponding to and connected to the annular weak area is formed at the inner side of the mooring layer adjacent to the flange connection area.

7. The method for manufacturing a tethered cover according to claim 6, wherein When manufacturing the mooring layer, aramid fabric thin layers and thermoplastic elastomer films of required size and shape are laid in sequence and at intervals, and then the laid thin layers are coated on the core mold, and the mooring layer is formed by vacuum bag hot pressing.

8. A capping cover, comprising a cover body, a shape-matching filling layer in the frame opening of the cover body, and capping layers covering the flange connection area, the filling layer and the thinned area of ​​the frame opening edge on both sides of the cover body, characterized in that: The mooring layer is sewn on the cover body by weaving threads passing through the mooring holes in the thinned area. The mooring layer comprises a thermoplastic elastomer layer. The filling layer, the mooring layer and the cover body are an integrated structure formed by hot pressing.

9. The tethered cover according to claim 8, characterized in that: The tethered layer corresponding to one frame opening goes around the flange connection area of ​​the cover body and covers the other side of the cover body after covering one side of the cover body.

10. The tie-down cover according to claim 8, characterized in that: A redundant avoidance groove corresponding to and connected to the annular weak area is provided at an inner side position of the mooring layer adjacent to the flange connection area.