TSV back exposed hole structure and preparation method thereof

By simplifying the TSV backside exposure process and utilizing temporary bonding adhesive and insulation layer deposition, the problems of cumbersome process steps and high cost in the existing technology are solved, and the manufacturing efficiency and qualification rate are improved.

CN118824973APending Publication Date: 2024-10-22CHENGXIE TECHNOLOGY (SHANGHAI) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410916174.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing process steps for exposing holes on the back of TSV are cumbersome, resulting in high production costs, low pass rates, and serious machine pollution.

Method used

Temporary bonding adhesive is used to adhere the front side of the substrate to the carrier, and the insulating layer is directly deposited after thinning to simplify the process steps and form an exposed hole structure on the back of the TSV.

Benefits of technology

The process steps are simplified, the production cost is reduced, and the manufacturing efficiency and qualification rate of the exposed hole structure on the back of the TSV are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118824973A_ABST
    Figure CN118824973A_ABST
Patent Text Reader

Abstract

The invention provides a TSV back exposed hole structure and a preparation method thereof. The method is applied to the technical field of advanced packaging, and comprises the following steps: adhering the front surface of a substrate to a carrier through temporary bonding glue; thinning the back surface of the substrate until the second conductor is exposed; depositing a first insulating layer on the back surface of the thinned substrate; coating a second insulating layer on the first insulating layer; sequentially exposing and developing the second insulating layer to generate a second opening; etching the first insulating layer to generate a first opening; and forming bumps in the first opening and the second opening to obtain the TSV back exposed hole structure. In this way, the manufacturing efficiency of the TSV back exposed hole structure can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of advanced packaging technology, and in particular to a TSV backside exposed hole structure and a preparation method thereof. Background Art

[0002] In the field of integrated circuits, especially in advanced packaging such as 2.5D and 3D, through-silicon via (TSV) interconnection technology has become one of the key technologies for achieving high-performance and highly integrated chips. TSV technology realizes signal transmission and power distribution between different chip layers by manufacturing vertical electrical interconnection channels on silicon wafers, thereby effectively improving the performance and energy efficiency of chips. In recent years, with the increasing functional requirements of electronic devices, the requirements for TSV technology have become increasingly stringent, especially the innovation in the back-side exposed hole structure and its preparation method, which provides chip designers with more flexibility and functionality. Designers can use back-side exposed holes to achieve more complex interconnection designs and optimize the overall performance of the chip; the introduction of the back-side exposed hole structure allows direct interconnection between multiple chip layers, which is of great significance in realizing device integration and system integration.

[0003] At present, the existing technology usually adopts the copper-silicon etching process route when performing TSV back-side hole exposure. The process operation steps are relatively long, resulting in high production costs for TSV back-side hole exposure. In addition, the copper-silicon etching itself is prone to cause machine contamination, reducing the pass rate of the TSV back-side hole structure. Summary of the invention

[0004] The invention provides a TSV backside exposed hole structure and a preparation method thereof.

[0005] A TSV backside hole structure, comprising:

[0006] A first conductor (1), the first conductor (1) being electrically connected to a corresponding second conductor (4) via a metal wiring layer (2);

[0007] The second conductor (4) is arranged in a TSV hole corresponding to the substrate (3), and the second conductor (4) is insulated and isolated from the substrate (3) by SiO2;

[0008] The second conductor (4) is electrically connected through the first opening of the first insulating layer (5), the second opening of the second insulating layer (6) and the corresponding bump (7);

[0009] The bump (7) is insulated and isolated by the first insulating layer (5), the second insulating layer (6) and the substrate (3);

[0010] The first conductor (1) and the substrate (3) are insulated and isolated;

[0011] The first conductor (1) and the metal wiring layer (2) are adhered to the carrier (9) by means of a temporary bonding adhesive (8).

[0012] Furthermore: the structure of the second conductor (4) is cylindrical, and the diameter of the first opening is smaller than the diameter of the TSV hole.

[0013] Furthermore, the material of the first conductor (1) includes: CuNiAu or CuNiPdAu.

[0014] Furthermore, the material of the substrate (3) includes: Si.

[0015] Furthermore, the material of the bump (7) includes: CuSn, CuNiSn, CuNiCuSnAg or CuNiSnAg.

[0016] Furthermore, the material of the first insulating layer (5) includes at least one of the following: Si3N4, SiO2, SiCN and SiON.

[0017] A method for preparing a TSV backside exposed hole structure, comprising:

[0018] S1, the front side of the substrate (3) is bonded to the carrier (9) by means of a temporary bonding adhesive (8); wherein the front side of the substrate (3) is provided with a metal wiring layer (2); the metal wiring layer (2) is provided with a plurality of first conductors (1); the substrate (3) is provided with a plurality of TSV holes; a second conductor (4) is provided in the TSV hole; the second conductor (4) is electrically connected to the corresponding first conductor (1) through the metal wiring layer (2);

[0019] S2, thinning the back side of the substrate (3) until the second conductor (4) is exposed;

[0020] S3, depositing a first insulating layer (5) onto the back side of the thinned substrate (3);

[0021] S4, coating a second insulating layer (6) onto the first insulating layer (5);

[0022] S5, sequentially exposing and developing the second insulating layer (6) to form a second opening;

[0023] S6, etching the first insulating layer (5) to generate a first opening; wherein the first opening and the second opening are both cylindrical, and the diameter of the first opening is equal to the diameter of the second opening;

[0024] S7, forming bumps (7) in the first opening and the second opening, thereby obtaining the TSV backside exposed hole structure.

[0025] Furthermore, the material of the carrier (9) includes at least one of the following: glass, silicon wafer and ceramic.

[0026] Furthermore: the depth of the TSV hole is 15 μm to 200 μm

[0027] Furthermore, the method further comprises: after depositing the first insulating layer (5) onto the back side of the thinned substrate (3), coating the third insulating layer (10) onto the first insulating layer (5); sequentially exposing and developing the third insulating layer (10) to generate a third opening; etching the first insulating layer (5) to generate a fourth opening; removing the third insulating layer (10); coating the second insulating layer (6) onto the first insulating layer (5); sequentially exposing and developing the second insulating layer (6) to generate a fifth opening; forming a bump (7) in the fourth opening and the fifth opening; wherein the fourth opening and the fifth opening are both cylindrical, and the diameter of the fifth opening is greater than or equal to the diameter of the fourth opening.

[0028] Compared with the prior art, the beneficial effects of the present invention are as follows: the front side of the substrate is adhered to the carrier by temporary bonding glue, the back side of the substrate is thinned until the second conductor is exposed, and then the first insulating layer is directly deposited on the back side of the thinned substrate, thereby simplifying the process steps and improving the manufacturing efficiency of the TSV back side hole structure; the simplification of the process steps reduces the use of machines and reduces the manufacturing cost of the TSV back side hole structure; the simplification of the process steps improves the pass rate of the TSV back side hole structure.

[0029] It should be understood that the contents described in the summary of the invention are not intended to limit the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The above and other features, advantages and aspects of the embodiments of the present invention will become more apparent with reference to the following detailed description in conjunction with the accompanying drawings. The accompanying drawings are used to better understand the present invention and do not constitute a limitation of the present invention. In the accompanying drawings, the same or similar reference numerals represent the same or similar elements, wherein:

[0031] Figure 1 A schematic diagram showing a process of a method for preparing a TSV backside hole structure according to an embodiment of the present invention is shown;

[0032] Figure 2 A cross-sectional view showing the front side of the substrate being bonded to the carrier by means of a temporary bonding adhesive;

[0033] Figure 3 A cross-sectional view showing the back side of the substrate being thinned to expose the second conductor;

[0034] Figure 4 A cross-sectional view showing deposition of a first insulating layer onto the back side of a thinned substrate;

[0035] Figure 5 showing a cross-sectional view of applying a second insulating layer onto the first insulating layer;

[0036] Figure 6 A cross-sectional view showing the second opening is generated by sequentially exposing and developing the second insulating layer;

[0037] Figure 7 A cross-sectional view showing etching the first insulating layer to generate a first opening;

[0038] Figure 8 A cross-sectional view of a TSV backside hole structure according to an embodiment of the present invention is shown;

[0039] Fig. 9 A cross-sectional view of a third opening is shown in which a third insulating layer is coated on the first insulating layer, and the third insulating layer is sequentially exposed and developed to generate the third insulating layer;

[0040] Fig.10 A cross-sectional view showing etching the first insulating layer to generate a first opening;

[0041] Fig.11 shows a cross-sectional view with the third insulating layer removed;

[0042] Fig.12 showing a cross-sectional view of applying a second insulating layer onto the first insulating layer;

[0043] Fig.13 FIG. 4 is a cross-sectional view of a TSV backside hole structure according to another embodiment of the present invention. DETAILED DESCRIPTION

[0044] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0045] In addition, the term "and / or" in this article is only a description of the association relationship between the associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.

[0046] Figure 8 A schematic diagram of a TSV back-side exposed hole structure according to an embodiment of the present invention is shown, and the structure includes: a first conductor 1, which is electrically connected to a corresponding second conductor 4 through a metal wiring layer 2; the second conductor 4 is arranged in a TSV hole corresponding to a substrate 3, and the second conductor 4 is insulated and isolated from the substrate 3 by SiO2; the second conductor 4 is electrically connected to a corresponding bump 7 through an opening of a first insulating layer 5, an opening of a second insulating layer 6, respectively; the bump 7 is insulated and isolated from the substrate 3 by the first insulating layer 5, the second insulating layer 6; the first conductor 1 is insulated and isolated from the substrate 3; the first conductor 1 and the metal wiring layer 2 are adhered to a carrier 9 by a temporary bonding glue 8.

[0047] In some embodiments, the opening of the first insulating layer 5 and the opening of the second insulating layer 6 are both cylindrical, and the diameter of the opening of the first insulating layer 5 is equal to the diameter of the opening of the second insulating layer 6 .

[0048] In some embodiments, the opening of the first insulating layer 5 and the opening of the second insulating layer 6 are both square, and the side length of the opening of the first insulating layer 5 is equal to the side length of the opening of the second insulating layer 6 .

[0049] In some embodiments, the second conductor 4 is cylindrical in shape, and the diameter of the opening of the first insulating layer 5 and / or the second insulating layer 6 is smaller than the diameter of the TSV hole.

[0050] In some embodiments, the material of the first conductor 1 is CuNiAu or CuNiPdAu.

[0051] In some embodiments, the material of the substrate 3 is Si.

[0052] In some embodiments, the material of the bump 7 is one of CuSn, CuNiSn, CuNiCuSnAg or CuNiSnAg.

[0053] In some embodiments, the material of the first insulating layer 5 may be Si 3 N 4 , SiO 2 , SiCN, SiON or any combination thereof.

[0054] Figure 1 A schematic flow chart of a method for preparing a TSV backside hole structure according to an embodiment of the present invention is shown, the method comprising:

[0055] S1, the front side of the substrate 3 is bonded to the carrier 9 by means of a temporary bonding adhesive 8, as shown in FIG. Figure 2 As shown; wherein, a metal wiring layer 2 is provided on the front side of the substrate 3; the metal wiring layer 2 is provided with five first conductors 1; the substrate 3 is provided with five TSV holes; a second conductor 4 is provided in the TSV hole; the second conductor 4 is electrically connected to the corresponding first conductor 1 through the metal wiring layer 2;

[0056] In some embodiments, the depth of the TSV hole is 120 μm.

[0057] In some embodiments, the material of the carrier 9 may be glass, silicon wafer or ceramic.

[0058] S2, thinning the back side of the substrate 3 until the second conductor 4 is exposed, such as Figure 3 As shown;

[0059] In some embodiments, the substrate 3 is a Si substrate, and the back side of the substrate 3 is thinned by performing Si grinding, CMP grinding, wet etching or a combination thereof.

[0060] In some embodiments, during CMP polishing, the second conductor in the TSV hole may be flush with, recessed, or protruded from the substrate 3 .

[0061] S3, depositing the first insulating layer 5 on the back side of the thinned substrate 3, as shown in Figure 4 As shown;

[0062] In some embodiments, the first insulating layer 5 is Si 3 N 4 , and Si 3 N 4 is deposited on the back side of the thinned substrate 3 by performing a CVD process step.

[0063] S4, coating the second insulating layer 6 on the first insulating layer 5, such as Figure 5 As shown;

[0064] In some embodiments, the second insulating layer 6 is PI, and the PI is coated on the first insulating layer 5 by performing a PI coating process.

[0065] S5, exposing and developing the second insulating layer 6 in sequence to form a second opening, such as Figure 6 As shown;

[0066] S6, etching the first insulating layer 5 to form a first opening, such as Figure 7 As shown;

[0067] In some embodiments, the first insulating layer 5 is etched by using CF4, NF3, SF6, CHF3, and any combination thereof.

[0068] In some embodiments, the first opening and the second opening are both cylindrical, and the diameter of the first opening is equal to the diameter of the second opening.

[0069] S7, forming a bump 7 in the first opening and the second opening, so as to obtain a TSV backside exposed hole structure.

[0070] According to an embodiment of the present invention, the front side of the substrate is adhered to the carrier by temporary bonding glue, the back side of the substrate is thinned until the second conductor is exposed, and then the first insulating layer is directly deposited on the back side of the thinned substrate, thereby simplifying the process steps and improving the manufacturing efficiency of the TSV back side hole structure; the simplification of the process steps reduces the use of machines and reduces the manufacturing cost of the TSV back side hole structure; the simplification of the process steps improves the pass rate of the TSV back side hole structure.

[0071] Another method for preparing a TSV backside hole structure according to an embodiment of the present invention includes:

[0072] S1, the front side of the substrate 3 is bonded to the carrier 9 by means of a temporary bonding adhesive 8, as shown in FIG. Figure 2 As shown; wherein, a metal wiring layer 2 is provided on the front side of the substrate 3; the metal wiring layer 2 is provided with five first conductors 1; the substrate 3 is provided with five TSV holes; a second conductor 4 is provided in the TSV hole; the second conductor 4 is electrically connected to the corresponding first conductor 1 through the metal wiring layer 2;

[0073] In some embodiments, the depth of the TSV hole is 120 μm.

[0074] In some embodiments, the material of the carrier 9 is glass.

[0075] S2, thinning the back side of the substrate 3 until the second conductor 4 is exposed, such as Figure 3 As shown;

[0076] In some embodiments, the substrate 3 is a Si substrate, and the back side of the substrate 3 is thinned by performing Si grinding, CMP grinding, wet etching or a combination thereof.

[0077] S3, depositing the first insulating layer 5 on the back side of the thinned substrate 3, as shown in Figure 4 As shown;

[0078] In some embodiments, the first insulating layer 5 is Si 3 N 4 , and Si 3 N 4 is deposited on the back side of the thinned substrate 3 by performing a CVD process step.

[0079] S4, coating the third insulating layer 10 on the first insulating layer 5, and sequentially exposing and developing the third insulating layer 10 to form a third opening, such as Fig. 9 As shown;

[0080] In some embodiments, the third insulating layer 10 may be photoresist.

[0081] S5, etching the first insulating layer 5 to form a fourth opening, such as Fig.10 As shown;

[0082] S6, removing the third insulating layer 10, such as Fig.11 As shown;

[0083] S7, coating the second insulating layer 6 on the first insulating layer 5, such as Fig.12 As shown;

[0084] In some embodiments, the second insulating layer 6 is PI, and the PI is coated on the first insulating layer 5 by performing a PI coating process.

[0085] S8, sequentially exposing and developing the second insulating layer 6 to form a fifth opening, such as Figure 7 As shown;

[0086] S9, forming bumps 7 in the fourth opening and the fifth opening, so as to obtain a TSV backside exposed hole structure.

[0087] In some embodiments, the fourth opening and the fifth opening are both cylindrical, and the diameter of the fifth opening is greater than or equal to the diameter of the fourth opening.

[0088] Fig.13 A schematic diagram of a TSV back-side exposed hole structure according to another embodiment of the present invention is shown, and the structure includes: a first conductor 1, the first conductor 1 is electrically connected to two corresponding second conductors 4 through a metal wiring layer 2; the second conductor 4 is arranged in a TSV hole corresponding to a substrate 3, and the second conductor 4 is insulated and isolated from the substrate 3 by SiO2; the two second conductors 4 corresponding to the first conductor 1 through the metal wiring layer 2 are electrically connected to the corresponding openings of the first insulating layer 5, the corresponding openings of the second insulating layer 6 and the corresponding bumps 7; the bumps 7 are insulated and isolated from the substrate 3 by the first insulating layer 5, the second insulating layer 6; the first conductor 1 is insulated and isolated from the substrate 3; the first conductor 1 and the metal wiring layer 2 are adhered to a carrier 9 by a temporary bonding glue 8.

[0089] It should be noted that, for the above-mentioned method embodiments, for the sake of simplicity, they are all described as a series of action combinations, but those skilled in the art should know that the present invention is not limited by the described order of actions, because according to the present invention, certain steps can be performed in other orders or simultaneously. Secondly, those skilled in the art should also know that the embodiments described in the specification are all optional embodiments, and the actions and modules involved are not necessarily required by the present invention.

[0090] It should be understood that the above-mentioned various forms of processes can be used to reorder, add or delete steps. For example, the steps described in the present invention can be executed in parallel, sequentially or in different orders, as long as the desired results of the technical solution of the present invention can be achieved, and this document does not limit this.

[0091] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A TSV backside hole structure, characterized in that: include: A first conductor (1), the first conductor (1) being electrically connected to a corresponding second conductor (4) via a metal wiring layer (2); The second conductor (4) is arranged in a TSV hole corresponding to the substrate (3), and the second conductor (4) is insulated and isolated from the substrate (3) by SiO2; The second conductor (4) is electrically connected through the first opening of the first insulating layer (5), the second opening of the second insulating layer (6) and the corresponding bump (7); The bump (7) is insulated and isolated by the first insulating layer (5), the second insulating layer (6) and the substrate (3); The first conductor (1) and the substrate (3) are insulated and isolated; The first conductor (1) and the metal wiring layer (2) are adhered to the carrier (9) by means of a temporary bonding adhesive (8).

2. The TSV backside hole structure according to claim 1, characterized in that: The second conductor (4) is cylindrical in structure, and the diameter of the first opening is smaller than the diameter of the TSV hole.

3. The TSV backside hole structure according to claim 2, characterized in that: The material of the first conductor (1) includes: CuNiAu or CuNiPdAu.

4. The TSV backside hole structure according to claim 3, characterized in that: The material of the substrate (3) includes: Si.

5. The TSV backside hole structure according to claim 4, characterized in that: The material of the bump (7) includes: CuSn, CuNiSn, CuNiCuSnAg or CuNiSnAg.

6. The TSV backside hole structure according to claim 5, characterized in that: The material of the first insulating layer (5) includes at least one of the following: Si3N4, SiO2, SiCN and SiON.

7. A method for preparing a TSV backside exposed hole structure, comprising: S1, the front side of the substrate (3) is bonded to the carrier (9) by means of a temporary bonding adhesive (8); wherein the front side of the substrate (3) is provided with a metal wiring layer (2); the metal wiring layer (2) is provided with a plurality of first conductors (1); the substrate (3) is provided with a plurality of TSV holes; a second conductor (4) is provided in the TSV hole; the second conductor (4) is electrically connected to the corresponding first conductor (1) through the metal wiring layer (2); S2, thinning the back side of the substrate (3) until the second conductor (4) is exposed; S3, depositing a first insulating layer (5) onto the back side of the thinned substrate (3); S4, coating a second insulating layer (6) onto the first insulating layer (5); S5, sequentially exposing and developing the second insulating layer (6) to form a second opening; S6, etching the first insulating layer (5) to generate a first opening; wherein the first opening and the second opening are both cylindrical, and the diameter of the first opening is equal to the diameter of the second opening; S7, forming bumps (7) in the first opening and the second opening, thereby obtaining the TSV backside exposed hole structure.

8. The method for preparing the TSV backside hole structure according to claim 7, characterized in that: The material of the carrier (9) includes at least one of the following: glass, silicon wafer and ceramic.

9. The method for preparing a TSV backside hole structure according to claim 8, characterized in that: The TSV hole has a depth of 15 μm to 200 μm.

10. The method for preparing a TSV backside hole structure according to claim 7, characterized in that: The method further comprises: after depositing the first insulating layer (5) on the back side of the thinned substrate (3), coating the third insulating layer (10) on the first insulating layer (5); sequentially exposing and developing the third insulating layer (10) to generate a third opening; etching the first insulating layer (5) to generate a fourth opening; removing the third insulating layer (10); coating the second insulating layer (6) on the first insulating layer (5); sequentially exposing and developing the second insulating layer (6) to generate a fifth opening; forming a bump (7) in the fourth opening and the fifth opening; wherein the fourth opening and the fifth opening are both cylindrical, and the diameter of the fifth opening is greater than or equal to the diameter of the fourth opening.