Molten steel purification device and method
By designing a molten steel purification device and using a combined structure of a chute and a multi-layer filter plate, the problem of dross in high-temperature alloy molten steel was solved, efficient purification of molten steel was achieved, and the quality and performance of castings were improved.
Patent Information
- Application Number
- CN202411063180.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-10-25
AI Technical Summary
There is a large amount of dross in the high-temperature alloy steel liquid, which affects the cleanliness of the master alloy rod and the quality and mechanical properties of downstream precision castings.
A molten steel purification device is designed, including a chute and a purification component. The purification component is composed of slag retaining plates and multiple filter plates arranged at intervals. The filtering and removal of scum is achieved through liquid gaps and multi-layer filter plates. The filter plates The material is zirconium dioxide, the porosity gradually decreases, the tilt angle is 45°-60°, and the baking step is used to remove water vapor and preheat the chute.
It effectively blocks and filters scum, significantly improves the purity of molten steel, and improves the quality and mechanical properties of precision castings.
Smart Images

Figure CN118832150A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of molten steel filtering, and in particular to a molten steel purification device and method. Background Art
[0002] At present, the important role of steel materials in the national economy is self-evident. It plays a key role in many fields such as construction, transportation, machinery manufacturing, energy, aerospace, and national defense industry. It is crucial to promote economic development and improve people's living standards. Especially with the development of industrial technology, the demand for high-quality alloy materials has increased year by year. The most typical one is the application and development of casting master alloys, which puts forward the most stringent requirements for the preparation of alloy materials by ultra-pure smelting. Taking the K438 master alloy for casting as an example, the master alloy is smelted in a vacuum induction furnace to melt and alloy the metal, and finally cast into alloy rods. In the smelting of K438 high-temperature master alloy, more than ten alloy elements such as nickel, cobalt, chromium, tungsten, niobium, tantalum, molybdenum, zirconium, titanium, aluminum, and boron are used. These alloy elements will introduce their own oxides, by-products and non-metallic inclusions into the molten steel to varying degrees; in addition, the shedding and slag phenomenon of refractory materials in the smelting and pouring systems will also bring non-metallic oxide inclusions into the high-temperature alloy steel liquid. These inclusions will increase the slag of K438 high-temperature master alloy rods, affect the cleanliness of the master alloy rods, and ultimately affect the casting quality and mechanical properties of downstream precision castings. Summary of the invention
[0003] In order to overcome the deficiencies of the prior art, the technical problem to be solved by the present invention is: how to reduce the slag of high-temperature alloy steel liquid in the melting and pouring system.
[0004] The technical solution adopted by the present invention to solve its technical problem is:
[0005] A molten steel purification device comprises a chute, a pouring port is provided at the bottom of the chute, a purification component is provided on a side of the chute away from the pouring port, when working, mother liquid is introduced into the chute from one side of the purification component, and the mother liquid flows out from the pouring port after passing through the purification component;
[0006] The casting assembly includes a slag retaining plate and a plurality of filter plates which are detachably arranged in sequence in the casting direction. A liquid-passing gap is provided between the lower end of the slag retaining plate and the bottom wall of the chute. The plurality of filter plates divide the internal space of the chute into a plurality of cavities.
[0007] Furthermore, the upper ends of the plurality of filter plates are all inclined downward toward one side of the pouring port, and the inclination angles between the upper ends and the bottom wall of the chute are all 45°-60°.
[0008] Furthermore, the number of the above-mentioned filter plates is 3, which include the first filter plate, the second filter plate and the third filter plate in sequence from the above-mentioned slag retaining plate to the above-mentioned pouring port. The porosity of the above-mentioned first filter plate and the above-mentioned second filter plate is not greater than 20PPI, and the porosity of the third filter plate is not greater than 30PPI.
[0009] Furthermore, the width dimension of the end of the chute close to the pouring port is smaller than the width dimension of the end of the chute away from the pouring port.
[0010] Furthermore, the inner wall of the chute is provided with a first clamping groove which is clamped with the slag retaining plate, and the inner wall of the chute is also provided with a plurality of second clamping grooves which are respectively clamped with the plurality of filter plates.
[0011] Furthermore, the pouring port is truncated cone-shaped, and the upper opening size of the pouring port is larger than the lower opening size.
[0012] Furthermore, the material of the plurality of filter plates is zirconium dioxide.
[0013] The present invention also provides a method for purifying molten steel, comprising the following steps:
[0014] S1: baking chute;
[0015] S2: injecting the master alloy molten steel into the above chute, and the molten steel passes through the liquid gap and then passes through multiple filter plates in sequence to obtain purified molten steel;
[0016] S3: The purified molten steel flows from the pouring port into the mold for pouring.
[0017] Furthermore, in step S1, the baking temperature is 600° C. and the baking time is 8 hours.
[0018] The beneficial effects of the present invention are:
[0019] The master alloy molten steel is poured into the chute from the side close to the slag retaining plate. The molten steel passes through the liquid gap and the gap is sealed, ensuring that most of the slag cannot move to the side of the pouring port under the obstruction of the slag retaining plate. In addition, the slag in the molten steel passing through the liquid gap is filtered and blocked by the filter plates under the filtering action of the multi-layer filter plates, ensuring that the molten steel flowing from the pouring port to the mold cavity is of high purity, thereby improving the casting quality and mechanical properties of downstream precision castings. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the three-dimensional structure of the present invention;
[0021] Figure 2 It is a schematic cross-sectional view of the main view of the present invention;
[0022] Figure 3It is a schematic diagram of the internal structure of the chute of the present invention;
[0023] Figure 4 It is a top view schematic diagram of the present invention;
[0024] Marked in the figure are, 1-chute, 2-slag retaining plate, 3-filter plate, 4-pouring port, 5-liquid gap, 6-first clamping groove, 7-second clamping groove, 31-first filter plate, 32-second filter plate, 33-third filter plate. DETAILED DESCRIPTION
[0025] The present invention is further described below in conjunction with the accompanying drawings.
[0026] according to Figure 1-Figure 4 As shown, an embodiment of the present application proposes a molten steel purification device, including a chute 1, a pouring port 4 is provided at the bottom of the chute 1, and a purification component is provided on the side of the chute 1 away from the pouring port 4. During operation, the mother liquor is introduced into the chute 1 from one side of the purification component, and the mother liquor flows out from the pouring port 4 after passing through the purification component; the pouring component includes a slag retaining plate 2 and a plurality of filter plates 3 which are detachably arranged in sequence in the pouring direction, a liquid passing gap 5 is provided between the lower end of the slag retaining plate 2 and the bottom wall of the chute 1, and the plurality of filter plates 3 divide the internal space of the chute 1 into a plurality of cavities. The chute 1 is cast from magnesium-aluminum refractory materials, and the body is composed of the following raw materials by mass percentage: sintered magnesia 66%-85%, plate-shaped corundum powder 10%-25%, silica fume 3%-5%, aluminum powder 0.5%-2%, additives 0.5%-2%, and the additives are one or a combination of sodium polyphosphate, citric acid, explosion-proof fiber, and heat-resistant steel fiber; and in order to ensure the overall rigidity of the chute 1, a steel bar structure is arranged in the length direction and width direction of the lower end of the chute 1, and the chute 1 can be a rectangular trough design, in order to further ensure the flow of molten steel Efficiency, the width dimension of the end of the above-mentioned chute 1 close to the above-mentioned pouring port 4 is smaller than the width dimension of the end of the above-mentioned chute 1 away from the above-mentioned pouring port 4, that is, the horizontal cross-sectional profile of the chute 1 is a trapezoidal design, the side of the above-mentioned chute 1 away from the above-mentioned pouring port 4 is a long bottom side, and the side of the above-mentioned chute 1 close to the above-mentioned pouring port 4 is a short bottom side, and the bottom inner wall of the chute 1 can be inclined relative to the horizontal plane, and one side of the above-mentioned pouring port 4 is lower than one side of the slag baffle 2, and the inclination angle based on the horizontal plane is 3°~5°, so as to ensure the flow efficiency of the molten steel in the chute 1.
[0027] First of all, it should be stated that the mother alloy molten steel is poured into the chute 1 from the side close to the slag retaining plate 2, and the molten steel passes through the liquid gap 5 and the liquid gap 5 is liquid-sealed, ensuring that most of the slag cannot move to the side of the pouring port 4 under the obstruction of the slag retaining plate 2, and the molten steel passing through the liquid gap 5 is filtered and blocked by the filter plate 3 under the filtering action of the multi-layer filter plate 3, ensuring that the molten steel flowing from the pouring port 4 to the mold cavity has a high degree of purity, thereby improving the casting quality and mechanical properties of downstream precision castings.
[0028] Moreover, the upper ends of the plurality of filter plates 3 are all inclined downward toward the side of the pouring port 4, and the inclination angles between the slag retaining plate 2, the filter plate 3 and the bottom wall of the chute 1 are all 45°-60°. The inclined setting is beneficial to reducing the thermal radiation of the molten steel between the slag retaining plate 2 and the filter screen, delaying the temperature drop of the molten steel in this interval, and is beneficial to maintaining the fluidity of the molten steel and preventing the occurrence of the molten steel pouring death phenomenon.
[0029] Specifically, the inner wall of the chute 1 is provided with a first clamping groove 6 which is clamped with the slag retaining plate 2, and the inner wall of the chute 1 is also provided with a plurality of second clamping grooves 7 which are respectively clamped with the plurality of filter plates 3. The first clamping groove 6 and the second clamping groove 7 are recessed at a depth of 3mm to 10mm on the inner wall of the chute 1 to ensure that no molten steel leakage occurs at the connection between the slag retaining plate 2 and the filter plate 3 and the chute 1, and the size of the liquid gap 5 is 15mm to 30mm to ensure that the liquid seal can be achieved in time and the amount of slag passing through the liquid gap 5 is reduced; the material of the plurality of filter plates 3 can be magnesium oxide, aluminum oxide, zirconium oxide, which can be selected or used in combination. In view of the excellent high-temperature strength and stability of zirconium oxide, zirconium oxide is selected in this embodiment to prepare the slag retaining plate and the filter plate.
[0030] The pouring port 4 is truncated cone-shaped, and the upper opening of the pouring port 4 is larger than the lower opening, which can accelerate the flow of molten steel into the mold, reduce the retention of molten steel in the chute 1, and improve the efficiency of molten steel pouring.
[0031] Moreover, in this embodiment, the number of the filter plates 3 is 3, and the first filter plate 31, the second filter plate 32 and the third filter plate 33 are included in sequence from the slag retaining plate 2 to the pouring port 4. Since the first filter plate 31, the second filter plate 32 and the third filter plate 33 are all detachably arranged in the chute 1, the filter plates can be disassembled and installed to meet the filtering using one, two or all three filter plates. The first stage of filtration is to set only the first filter plate 31, and the selection of the third filter plate 33 is based on the principle that the closer to the pouring port 4, the smaller the filter plate (high PPI value) should be selected, and the farther from the pouring port 4, the larger the filter screen should be selected. That is to say, the apertures of the first filter plate 31, the second filter plate 32 and the third filter plate 33 are gradually reduced in sequence, and the principle of step-by-step filtration is adopted. Prevent large particles of slag and slag inclusions from blocking the small-aperture filter screen on a large scale, and ensure that the molten steel passes through the filter screens at all levels smoothly, so as to ensure that the master alloy of the filter device provided in this embodiment is fully filtered and reduce the secondary pollution of the molten steel by the filter screen slag.
[0032] This embodiment also provides a method for purifying molten steel, which is characterized by comprising the following steps:
[0033] S1: Baking chute 1; wherein the baking temperature is 600°C and the baking time is 8h; the baking has two functions, one is to remove water vapor in the chute body, which will cause the molten steel to splash violently when it meets the molten steel, and the other is to preheat the chute body, reduce the temperature drop of the casting molten steel, and ensure good fluidity of the molten steel.
[0034] S2: The master alloy molten steel is injected into the above-mentioned chute 1, and the molten steel passes through the liquid gap 5 and then passes through multiple filter plates 3 in sequence to obtain purified molten steel; the casting temperature is 1680°C. In this embodiment, three filter plates 3 are specifically selected, which are the first filter plate 31, the second filter plate 32 and the third filter plate 33 in sequence from the slag retaining plate 2 to the pouring port 4, wherein the selected slag retaining plate 2 has a thickness of 10mm; the first filter plate 31 has a thickness of 10mm, a porosity of 10PPI, and a hole type of through hole; the second filter plate 32 has a thickness of 10mm, a porosity of 10PPI, and a hole type of sponge; the third filter plate 33 has a thickness of 10mm, a porosity of 15PPI, and a hole type of sponge, to achieve three-stage filtration in sequence and realize the purification process of the molten steel.
[0035] S3: The purified molten steel flows from the pouring port 4 into the mold for pouring.
[0036] In summary, the embodiment of the present application proposes a molten steel purification device, including a chute 1, a pouring port 4 is opened at the bottom of the chute 1, and a purification component is arranged on the side of the chute 1 away from the pouring port 4. When working, the mother liquid is introduced into the chute 1 from one side of the purification component, and the mother liquid flows out from the pouring port 4 after passing through the purification component; the pouring component includes a slag retaining plate 2 and a plurality of filter plates 3 which are detachably arranged in sequence at intervals toward the pouring direction, and a liquid passing gap 5 is arranged between the lower end of the slag retaining plate 2 and the bottom wall of the chute 1, and the plurality of filter plates 3 divide the internal space of the chute 1 into a plurality of cavities, thereby realizing the efficient removal of metal oxide inclusions and non-metal oxide inclusions generated during the production of the master alloy, reducing the number and size of large-particle inclusions in the master alloy rod, and significantly reducing the slag level of the master alloy, thereby improving the quality of the master alloy, and can significantly improve the yield rate of downstream precision castings and the mechanical properties of the castings.
Claims
1. A molten steel purification device, characterized in that: The invention comprises a chute (1), wherein a pouring port (4) is provided at the bottom of the chute (1), and a purification component is provided on a side of the chute (1) away from the pouring port (4). When the chute (1) is in operation, mother liquid is introduced into the chute (1) from one side of the purification component, and the mother liquid flows out from the pouring port (4) after passing through the purification component. The pouring assembly comprises a slag retaining plate (2) and a plurality of filter plates (3) which are detachably arranged in sequence and spaced apart in the pouring direction, a liquid-passing gap (5) is provided between the lower end of the slag retaining plate (2) and the bottom wall of the chute (1), and the plurality of filter plates (3) divide the internal space of the chute (1) into a plurality of cavities.
2. A molten steel purification device according to claim 1, characterized in that: The upper ends of the plurality of filter plates (3) are all inclined toward one side of the pouring port (4), and the inclination angle between the filter plates (3) and the bottom wall of the chute (1) is 45°-60°.
3. A molten steel purification device according to claim 2, characterized in that: The number of the filter plates (3) is three, which include a first filter plate (31), a second filter plate (32) and a third filter plate (33) in sequence from the slag retaining plate (2) to the pouring port (4); the porosity of the first filter plate (31) and the second filter plate (32) is no more than 20 PPI, and the porosity of the third filter plate (33) is no more than 30 PPI.
4. A molten steel purification device according to claim 1, characterized in that: The width dimension of the end of the chute (1) close to the pouring port (4) is smaller than the width dimension of the end of the chute (1) away from the pouring port (4).
5. A molten steel purification device according to claim 1, characterized in that: The inner wall of the chute (1) is provided with a first clamping groove (6) which is clamped with the slag retaining plate (2), and the inner wall of the chute (1) is also provided with a plurality of second clamping grooves (7) which are respectively clamped with the plurality of filter plates (3).
6. A molten steel purification device according to claim 1, characterized in that: The pouring port (4) is arranged in a truncated cone shape, and the size of the upper opening of the pouring port (4) is larger than the size of the lower opening.
7. A molten steel purification device according to claim 1, characterized in that: The material of the plurality of filter plates (3) is all zirconium dioxide.
8. A molten steel purification device according to claim 1, characterized in that: The pores of the filter plate (3) are sponge pores.
9. A method for purifying molten steel, characterized in that: The following steps are involved: S1: baking chute (1); S2: injecting the master alloy molten steel into the chute (1), and the molten steel passes through the liquid-passing gap (5) and then sequentially passes through a plurality of filter plates (3) to obtain purified molten steel; S3: The purified molten steel flows from the pouring port (4) into the mold for pouring.
10. A method for purifying molten steel according to claim 9, characterized in that: In step S1, the baking temperature is 600° C. and the baking time is 8 hours.