Device and method for testing bonding strength of lithium battery pole piece

Through the testing device and method that combines the stage and the micron scratch meter, the qualitative and complex problems of lithium battery pole piece bonding strength testing in the existing technology are solved, and efficient, accurate quantitative measurement and good repeatability are achieved. Bonding strength testing.

CN118837293APending Publication Date: 2024-10-25ZHEJIANG CASNOVO MATERIALS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411267804.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

The existing lithium battery pole piece bonding strength testing method has insufficient qualitative evaluation, complex equipment and difficult operation. The peeling strength test data fluctuates greatly, making it impossible to achieve efficient and accurate quantitative measurement.

Method used

Using a test device and method that combines a stage and a micron scratch meter, the bonding strength is calculated by moving the micron scratch meter in the length, width and height directions of the stage, applying a load and recording the scratch length and termination load. , ensuring test repeatability and accuracy.

Benefits of technology

It achieves quantitative measurement of pole piece bonding strength, simplifies test operations, reduces volatility, improves detection accuracy, and has scalability to connect to a visual inspection system to achieve online quantitative inspection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118837293A_ABST
    Figure CN118837293A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of lithium ion batteries, in particular to a lithium battery pole piece bonding strength testing device and a testing method. Comprising an objective table (1) and a micron scratching instrument (2), the objective table (1) and the micron scratching instrument (2) are of an integrated structure or an independent structure, and the micron scratching instrument (2) can move in the length direction, the width direction and the height direction of the objective table (1). And the micron scratching instrument (2) can apply a load in the height direction of the objective table (1). The micron scratch method is used for quantitatively characterizing the bonding strength of the pole piece, the used instrument is simple, the method is convenient and efficient, meanwhile, the defect that the peel strength test is carried out on a single test pole piece is avoided, multiple tests can be carried out on the same pole piece, and the repeatability is good. And meanwhile, a visual detection system can be further accessed by the method, so that quicker online quantitative detection is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of lithium-ion batteries, and more specifically, to a lithium battery pole piece bonding strength testing device and testing method. Background Art

[0002] In lithium batteries, the electrode active material is adhered to the surface of the current collector by an adhesive. The interfacial bonding strength between the entire electrode active coating and the foil as the substrate can directly affect the electrochemical performance of the lithium battery. Therefore, quantitative evaluation of its bonding strength becomes an important indicator of the performance of the adhesive. Currently, the common electrode bonding strength test methods are: hundred-grid test, peel strength test, and laser layer cracking method. Among them, the hundred-grid test can only be qualitatively evaluated; the laser layer cracking method has complex equipment and is difficult to operate.

[0003] CN109870353A discloses a method for testing the peel strength of a lithium-ion battery pole piece, comprising the following steps: S1: sticking one side of a double-sided adhesive tape (1) to a steel plate (2), placing a first cushion film (3) on the lower part of the other side of the double-sided adhesive tape (1), and then sticking it to the front side of a dressing layer of a lithium-ion battery pole piece (4), so that the lower part of the pole piece (4) is not bonded to the lower part of the double-sided adhesive tape (1); S2: fixing the lower end of the pole piece (4) to the first end of a tensile testing instrument, and fixing the steel plate (2) to the second end of the tensile testing instrument; S3: starting the tensile testing instrument to start testing and obtaining the maximum peel strength, but the peel strength test is limited by the pole piece slitting width and the overlap degree of the test tape, and the data fluctuates greatly. Summary of the invention

[0004] A first aspect of the present invention provides a lithium battery pole piece bonding strength testing device, comprising: a stage and a micron scratch instrument, wherein the stage and the micron scratch instrument are an integrated structure or independent structures, and the micron scratch instrument can move in the length direction, width direction and height direction of the stage.

[0005] The micron scratch tester can apply a load in the height direction of the stage.

[0006] A second aspect of the present invention provides a method for testing the bonding strength of a lithium battery electrode, comprising the following steps: Step 1: Take a lithium battery electrode, straighten it horizontally, and fix both ends on the stage; Step 2: Adjust the distance between the end of the micrometer scratch tester and the surface of the electrode, and set the initial load F0, loading rate, and scratching speed of the micrometer scratch tester; Step 3: Start the scratch tester and move it in the length and height directions of the stage until the pole piece starts to expose aluminum. The length from the starting point to the point where the pole piece starts to expose aluminum is I, and a scratch with a length of L is obtained, and the end load F1 is recorded; Step 4: Calculate according to formula 1 to obtain the bonding strength F; Step 5: Move the micrometer scratch tester in the width direction of the stage and repeat steps 2-4 below the original scratch to obtain the bonding strength F'; Step 6: If the relative deviation between F and F' is not greater than 5%, the bonding strength is the average value of F and F'. If the relative deviation between F and F' is greater than 5%, repeat steps 1-6 until the relative deviation between F and F' is not greater than 5%. , formula 1.

[0007] In step 2, the end of the micrometer scratch tester contacts the surface of the electrode.

[0008] The scratch length is 10-50 mm.

[0009] The loading rate is 0.01-0.2 N / min.

[0010] Preferably, the loading rate is 0.01-0.1 N / min.

[0011] The scratching speed is 10-200 mm / min.

[0012] Preferably, the scratching speed is 30-100 mm / min.

[0013] The present application study found that the loading rate of 0.01-0.2 N / min and the scratching speed of 10-200 mm / min can improve the accuracy of the detection and may reduce the volatility of the micron scratch tester during operation.

[0014] The initial load is 5-30 mN.

[0015] Preferably, the initial load is 5-20 mN.

[0016] The end load is 40-80 mN.

[0017] Preferably, the termination load is 40-60 mN.

[0018] Beneficial effects: 1. The micron scratch method is used to quantitatively characterize the bonding strength of the electrode. The instrument is simple to use and easy to operate.

[0019] 2. The device of the present application combined with the test method can be tested multiple times on the same electrode with good repeatability.

[0020] 3. This application method is convenient and efficient, and is not limited by the electrode cutting width and the overlap degree of the test tape.

[0021] 4. The method of the present application can realize quantitative measurement of bonding strength. The loading rate is 0.01-0.2 N / min, the scratching speed is 10-200 mm / min, and the termination load is 40-80 mN, which can improve the accuracy of detection.

[0022] 5. The test method of this application is scalable and can be further connected to a visual inspection system to achieve faster online quantitative detection. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a device for testing the bonding strength of lithium battery pole pieces.

[0024] Figure 2 This is a schematic diagram before the bonding strength test of the embodiment.

[0025] Figure 3 This is a schematic diagram of the bonding strength test of the embodiment.

[0026] Among them are 1. stage; 2. micron scratch tester; 3. lithium battery pole piece. DETAILED DESCRIPTION

[0027] Example 1 A lithium battery electrode bonding strength testing device, such as Figure 1 As shown, it includes: a stage 1 and a micron scratch tester 2, wherein the stage 1 and the micron scratch tester 2 are independent structures respectively, and the micron scratch tester 2 can move in the length direction, width direction and height direction of the stage 1.

[0028] The micron scratch tester 2 can apply a load in the height direction of the stage 1 .

[0029] A method for testing the bonding strength of a lithium battery pole piece comprises the following steps: Step 1: Take a lithium battery electrode, straighten it horizontally, and fix both ends on the stage 1; Step 2: If Figure 2 As shown, the distance between the end of the micron scratch tester 2 and the surface of the electrode is adjusted so that the end of the micron scratch tester 2 contacts the surface of the electrode, and the initial load F0 of the micron scratch tester 2 is set to 10mN, the loading rate is 0.06N / min, and the scratching speed is 60mm / min; Step 3: Start the scratch tester 2 and move it in the length and height directions of the stage 1 until the electrode begins to expose aluminum. Figure 2 As shown, the length I from the starting point to the aluminum exposure point of the pole piece is 18.4 mm, the scratch length L is 40 mm, and the end load F1 is recorded as 50 mN; Step 4: According to formula 1, the bonding strength F is calculated to be 28.4 mN; Step 5: Move the micrometer scratch tester 2 in the width direction of the stage 1, repeat steps 2-4 below the original scratch, the length I from the starting point to the point where the aluminum of the pole piece begins to be exposed is 18.08 mm, the scratch length L is 40 mm, and the end load F1 is recorded as 50 mN, and the bonding strength F' is 28.08 mN; Step 6: The average value of the bonding strength is F and F' is 28.24mN; , formula 1.

[0030] Comparative Example 1 A lithium battery electrode bonding strength testing device, such as Figure 1 As shown, it includes: a stage 1 and a micron scratch tester 2, wherein the stage 1 and the micron scratch tester 2 are independent structures respectively, and the micron scratch tester 2 can move in the length direction, width direction and height direction of the stage 1.

[0031] The micron scratch tester 2 can apply a load in the height direction of the stage 1 .

[0032] A method for testing the bonding strength of a lithium battery pole piece comprises the following steps: Step 1: Take a lithium battery electrode, straighten it horizontally, and fix both ends on the stage 1; Step 2: If Figure 2 As shown, the distance between the end of the micron scratch tester 2 and the surface of the electrode is adjusted so that the end of the micron scratch tester 2 contacts the surface of the electrode, and the initial load F0 of the micron scratch tester 2 is set to 10mN, the loading rate is 0.06N / min, and the scratching speed is 60mm / min; Step 3: Start the scratch tester 2 and move it in the length and height directions of the stage 1 until the electrode begins to expose aluminum. Figure 2 As shown, the length I from the starting point to the aluminum exposure point of the pole piece is 4.2 mm, the scratch length L is 20 mm, and the end load F1 is recorded as 30 mN; Step 4: According to formula 1, the bonding strength F is calculated to be 14.2 mN; Step 5: Move the micrometer scratch tester 2 in the width direction of the stage 1, repeat steps 2-4 below the original scratch, the length I from the starting point to the aluminum exposure point of the pole piece is 3.88 mm, the scratch length L is 20 mm, and the end load F1 is recorded as 30 mN, and the bonding strength F' is 13.88 mN; Step 6: The average value of the bonding strength is F and F', which is 14.04 mN; , formula 1.

[0033] Performance Testing Methods and Data The same lithium battery electrode was tested three times with reference to the test methods of the embodiment and the comparative example, and the coefficient of variation (CV) was calculated. The data are listed in Table 1.

[0034] Table 1

Claims

1. A lithium battery pole piece bonding strength testing device, It is characterized in that include: A stage (1) and a micrometer scratch tester (2), wherein the stage (1) and the micrometer scratch tester (2) are an integrated structure or independent structures, and the micrometer scratch tester (2) can move in the length direction, width direction and height direction of the stage (1); The micrometer scratch tester (2) can apply a load in the height direction of the stage (1); The method for testing the bonding strength of a lithium battery pole piece by the device comprises the following steps: Step 1: Take a lithium battery electrode, straighten it horizontally, and fix both ends of it on the stage (1); Step 2: Adjust the distance between the end of the micrometer scratch tester (2) and the surface of the electrode, and set the initial load F of the micrometer scratch tester (2) 0 , loading rate, scratching speed; Step 3: Start the scratch tester (2) and move it in the length direction and height direction of the stage (1) until the electrode starts to expose aluminum. The length from the starting point to the point where the electrode starts to expose aluminum is I. A scratch with a length of L is obtained, and the end load F is recorded. 1 ; Step 4: Calculate according to formula 1 to obtain the bonding strength F; Step 5: Move the micrometer scratch tester (2) in the width direction of the stage (1), and repeat steps 2-4 below the original scratch to obtain the bonding strength F'; Step 6: If the relative deviation between F and F' is not greater than 5%, the bonding strength is the average value of F and F'. If the relative deviation between F and F' is greater than 5%, repeat steps 1-6 until the relative deviation between F and F' is not greater than 5%. , formula 1.

2. The lithium battery pole piece bonding strength testing device according to claim 1, It is characterized in that In step 2, the end of the micrometer scratch tester (2) contacts the surface of the electrode.

3. The device for testing the bonding strength of a lithium battery pole piece according to claim 2, It is characterized in that The scratch length is 10-50 mm.

4. The lithium battery pole piece bonding strength testing device according to claim 3, It is characterized in that The loading rate is 0.01-0.2 N / min.

5. The lithium battery pole piece bonding strength testing device according to claim 4, It is characterized in that The loading rate is 0.01-0.1 N / min.

6. The lithium battery pole piece bonding strength testing device according to claim 5, It is characterized in that The scratching speed is 10-200 mm / min.

7. The lithium battery pole piece bonding strength testing device according to claim 6, It is characterized in that The initial load is 5-30 mN.

8. The lithium battery pole piece bonding strength testing device according to claim 7, It is characterized in that The end load is 40-80 mN.