Preparation and application of hUCMSC / SVF-PEP-coated Gel

By preparing hUCMSC/SVF-PEP@Gel, we solve the problems of traditional osteoarthritis treatment being unable to effectively slow down disease progression and poor cartilage regeneration ability, achieving long-term cell survival and efficient chondrogenic differentiation, and providing an effective treatment for osteoarthritis. plan.

CN118846239APending Publication Date: 2024-10-29BEIJING REGENERATIVE BIOTECHNOLOGY RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410867043.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-01
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

Traditional osteoarthritis treatment can only provide short-term symptom relief and cannot stop or slow down the progression of the disease. Surgical treatment also has problems such as low cartilage sources, poor regeneration ability, and limited postoperative activities. There is a lack of effective drugs and means to prevent and reverse the disease.

Method used

To prepare hUCMSC/SVF-PEP@Gel, through the isolation and culture of hUCMSC, the extraction of SVF and the preparation of PEP@Gel, a thermosensitive hydrogel is formed to provide cell attachment and protection, extend the cell survival time, and through the synergy of SVF and PEP@Gel It inhibits the expression of inflammatory cytokines and induces chondrogenesis and differentiation.

Benefits of technology

The long-term survival and efficient chondrogenic differentiation of hUCMSC/SVF were achieved, providing potential applications for bone regeneration and repair, suitable for clinical treatment of osteoarthritis, significantly improving cartilage regeneration ability and alleviating inflammation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118846239A_ABST
    Figure CN118846239A_ABST
Patent Text Reader

Abstract

The invention discloses preparation and application of hUCMSC / SVF-PEP-coated Gel. The preparation method comprises the following steps: step 1, isolated culture of hUCMSC, step 2, extraction culture of SVF, step 3, preparation of X hUCMSC and 2X hUCMSC / SVF suspension, step 4, preparation of hUCMSC and hUCMSC / SVF-PEP-coated Gel, and step 5, multidirectional detection.According to the invention, co-culture of hUCMSC and PEP-coated Gel hydrogel promotes increase of the level of anti-inflammatory factors, after SVF is added, the anti-inflammatory effect is synergistically enhanced; the oxidative stress state in the OA process is relieved, so that the inflammatory state is reversed; the EP hydrogel serves as a protective carrier for hUCMSC transmission, the SVF hydrogel and the PEP hydrogel both contribute to inhibiting expression of inflammatory cytokines and inducing cartilage formation and differentiation of hUCMSC and have a synergistic effect, it is indicated that the PEP-coated Gel hydrogel serving as the protective carrier for cell transmission has a potential application prospect in OA treatment, and bone regeneration and repair are expected to be more efficiently achieved through combined application of hUCMSC / SVF and PEP-coated Gel. The method is suitable for cartilage regeneration in clinical treatment of osteoarthritis.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of biomedicine, and in particular to the preparation and use of hUCMSC / SVF-PEP@Gel. Background Art

[0002] Osteoarthritis is a joint degenerative disease caused by multiple factors. Its pathological characteristics include degeneration and destruction of articular cartilage, synovitis, subchondral bone sclerosis or cystic changes, bone hyperplasia at the joint margins, osteophyte formation and other symptoms. The onset of osteoarthritis is related to many factors such as age, trauma, inflammation, obesity, and strain. With the aging of the population and the increase in the proportion of obese people, the incidence of OA continues to rise. The incidence rate in the age group over 65 years old is as high as 80%. OA has become the fourth most disabling disease. OA will not only seriously affect the quality of life of patients, but also bring serious economic burdens to patients' families and society. At present, the mainstream treatments for OA include non-drug, drug and surgical methods.

[0003] Mesenchymal stem cell therapy has shown good application prospects in the treatment of OA. Human umbilical cord mesenchymal stem cells are adult stem cells derived from the Wharton's jelly tissue of the human umbilical cord. They have a wide range of sources and strong proliferation ability. They are recognized as the most drug-like MSC type and have received widespread attention in the field of cartilage tissue engineering. hUCMSC has broad prospects in the treatment of OA.

[0004] The injectable in situ gel-forming system exhibits a phase transition from solution, sol to gel under physiological conditions, producing a reservoir capable of providing local release of encapsulated drugs. It is widely used in the treatment of indications such as diabetes, wound healing and spinal cord injury. The preparation and application of MSC-phase change hydrogels have also been reported in the literature, which is beneficial for maintaining MSC activity and long-term survival of transplants. The adipose vascular matrix component is a cell cluster tissue rich in precursor adipocytes, bone marrow stromal cells, endothelial progenitor cells, T cells, B cells, mast cells and adipose tissue macrophages in adipose tissue. Co-transplantation of SVF and MSC prolongs the survival of MSC, which is of great significance for MSC drug development.

[0005] However, conventional osteoarthritis treatments have the following disadvantages:

[0006] Traditional intervention measures for osteoarthritis can only provide temporary symptom relief, such as short-term pain relief, but have no effect on stopping or slowing the progression of OA. Current treatment methods mainly rely on early oral medications or intra-articular injections of sodium hyaluronate to achieve short-term symptom relief; in the middle and late stages, surgical treatments such as microfracture, cartilage transplantation, and joint replacement are used, but there are many disadvantages such as a small source of cartilage, poor regeneration ability, and severe limitation of postoperative activity. Currently, there are no effective drugs or means to prevent and pathologically reverse the progression of the disease to treat osteoarthritis. Summary of the invention

[0007] The purpose of the present invention is to provide a preparation and use of hUCMSC / SVF-PEP@Gel to solve the problem that traditional osteoarthritis intervention measures proposed in the above background technology can only provide temporary symptom relief, such as short-term pain relief, but have no effect on stopping or slowing the development of OA. The current treatment methods are mainly oral medication or intra-articular injection of sodium hyaluronate in the early stage to achieve the effect of relieving symptoms in the short term; microfracture, cartilage transplantation, joint replacement and other surgical treatments are adopted in the middle and late stages, but there are many disadvantages such as small cartilage sources, poor regeneration ability, and severe limitation of postoperative activities. At present, there are no effective drugs and means to prevent and pathologically reverse the development of the disease to treat osteoarthritis.

[0008] To achieve the above object, the present invention provides the following technical solution: a preparation of hUCMSC / SVF-PEP@Gel, comprising the following steps:

[0009] Step 1, isolation and culture of hUCMSC: culture P0 hUCMSC by tissue block method, add 0.25% trypsin solution and 1mL aprotinin solution, digest, harvest the precipitate, precipitate cells, inoculate and culture for later use;

[0010] Step 2, extraction and culture of SVF: 60 ml of adipose tissue obtained by liposuction was repeatedly rinsed 2-3 times with sterile PBS until the washing solution was clear, and an equal volume of 0.075% type I collagenase was added, and the mixture was placed in a 37°C constant temperature shaker for shaking and digestion for about 40 minutes, filtered with a 60-mesh cell sieve, and the filtrate was collected and centrifuged at 400×g for 10 minutes to remove the oil layer and milky cell layer, and the clarified supernatant was carefully discarded, and resuspended into 6 ml of cell suspension with 0.9% sodium chloride injection solution, which is the SVF stock solution;

[0011] Step 3. Preparation of X hUCMSC and 2X hUCMSC / SVF suspension: Take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml 0.9% sodium chloride injection to make 2X hUCMSC for use; take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml SVF stock solution to make 2X hUCMSC / SVF suspension containing 2×10 6 / ml hUCMSC for standby use;

[0012] Step 4, preparation of hUCMSC, hUCMSC / SVF-PEP@Gel: 50g PLGA1500-PEG1200-PLGA1500 was stirred evenly by low-temperature vortex at 4°C, dispersed and dissolved in 100g pure water to prepare PEP@Gel with a volume fraction of 50%, and then 10ml of pure water, 2X hUCMSC or 2X hUCMSC / SVF suspension was added to 10ml of 50% PEP@Gel by mass, and mixed evenly to prepare PEP@Gel with a mass fraction of 25%, or hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel containing a final concentration of 1×106 / ml hUCMSC. Under the condition of 4-8°C, PEP@Gel, hUCMSC-PEP@Gel, and hUCMSC / SVF-PEP@Gel were respectively poured into a 24-well plate, 0.5ml / well, and placed at 37°C for coagulation;

[0013] Step 5. Multi-faceted detection and identification: Phase transition temperature measurement of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel, hUCMSC survival examination, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition examination, osteogenic, adipogenic, and chondrogenic differentiation potential analysis of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel, and secretory effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel.

[0014] As a preferred technical solution of the present invention, the culture system in step 1 is MSC complete culture medium DMEM / F1212400-024, GIBCO, 10% animal-free serum substitute C08003C, Stemboscience, and 0.25% trypsin solution and 1 mL aprotinin solution are added in step 1. Specifically, when the culture is cultured for 12 days, the culture bottle is gently shaken to suspend the residual tissue blocks, the culture supernatant is carefully discarded, the culture surface is washed once with PBS, and 0.25% trypsin solution T6424-1VL, Biological industries, digested at room temperature for 5 minutes, added 1mL of aprotinin solution 1A1250000, Sigma to terminate digestion, the precipitate harvested in the step one is specifically centrifuged at 400×g for 5 minutes, discarded the supernatant, and the precipitate is harvested; washed twice with PBS, filtered with a 100μm nylon cell sieve, and the filtrate is collected; centrifuged at 400×g for 5 minutes, the supernatant is discarded, and the precipitated cells are harvested, recorded as P0 generation hUCMSC, and the inoculation and culture standby in the step one is specifically resuspended in MSC complete medium, inoculated into 175cm2 tissue culture flask EasyFlask, NUNC at 6×103 / cm2, and harvested when the P1 generation hUCMSC is cultured to 70-80% confluence; the P1 generation hUCMSC is continued to be passaged to P4, and the P4 hUCMSC is resuspended in 0.9% sodium chloride injection, and the cell concentration is adjusted to 4×106 / ml for standby.

[0015] As a preferred technical solution of the present invention, the phase transition temperature of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel in step 5 is specifically determined as follows: PEP@Gel with a mass fraction of 20%, 26%, 32%, 38%, 44%, and 50% is prepared by the same method, and equal volumes of pure water, 2X hUCMSC or 2X The hUCMSC / SVF suspension was mixed evenly to prepare PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with mass fractions of 10%, 13%, 16%, 19%, 22% and 25%, which were heated from 20°C to 65°C in a constant temperature water bath, and the solution-gel-precipitation phase transition temperatures of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel were measured, and the phase transition diagram was drawn. Subsequently, the elastic modulus G′ and viscous modulus G″ of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with a volume fraction of 25% were measured using an RH-20 rheometer to determine the gelation temperature.

[0016] As a preferred technical solution of the present invention, the hUCMSC survival test in step 5 is specifically as follows: placing the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in a 6-well plate, adding 1.5 ml of 0.9% sodium chloride injection preheated at 37°C, and culturing at 37°C and 5% CO2. The medium is changed every other day. At D0, D3, D7, D14, and D30, the hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel culture groups discard the culture supernatant, let stand at 4-8°C for 30 minutes, and then transfer to 37°C and 5% CO2 for incubation for 1 hour. The three groups of samples are stained with a live and dead cell double staining kit for 30 minutes, the staining solution is discarded, and the samples are rinsed 3 times with 0.9% sodium chloride injection and observed under an inverted fluorescence microscope. Green represents live cells and red represents dead cells.

[0017] As a preferred technical solution of the present invention, the hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition test in step 5 is specifically as follows: the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C is added, and the medium is cultured at 37°C and 5% CO2. The medium is changed every other day. At D0, D3, D7, D14, and D30, the culture supernatant is aspirated and the plate is allowed to stand at 4-8°C for 30 minutes, and then transferred to 37°C and incubated at 5% CO2 for 1 hour, the culture supernatant is aspirated and fixed with 4% paraformaldehyde for 1 hour, and then washed 3 times with 4°C pre-cooled PBS, and the cells are permeabilized with 0.1% Triton X-100 at room temperature for 20 minutes, and the cells are blocked with 10% goat serum by volume for 30 minutes; an anti-human primary antibody is added and incubated overnight at 4°C, and goat anti-rabbit IgG H&L is added FITC, incubated at 37°C for 1 hour, washed three times with PBS, and observed under an inverted fluorescence microscope. Green fluorescence represents positive staining for type II collagen.

[0018] As a preferred technical solution of the present invention, the osteogenic, adipogenic, and chondrogenic differentiation potential of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in step 5 is specifically as follows: the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, allowed to stand at 4-8°C for 30 minutes, then transferred to 37°C, 5% CO2, and incubated under saturated humidity conditions for 1 hour, 1.5 ml / well of MSC complete medium is added, and the plate is incubated at 37°C, 5% CO2 , cultured for 24 hours under saturated humidity conditions, cultured according to the instructions of the osteogenic differentiation kit, adipogenic differentiation kit, and chondrogenic differentiation kit, and the medium was changed every other day. When osteogenic differentiation reached 14 days, the cells were stained with alizarin red staining. The red deposits represented callus formation, forming a positive bone differentiation. When adipogenic differentiation reached 14 days, the cells were stained with Oil Red "O" staining. The red deposits represented lipid droplet formation, forming a positive adipogenic differentiation. When chondrogenic differentiation reached 18 days, the cells were stained with Alcian blue staining. The blue-blue-green deposits represented acidic mucin extracellular matrix, forming a positive cartilage differentiation.

[0019] As a preferred technical solution of the present invention, the secretion effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in step 5 is specifically as follows: some anti-inflammatory cytokines of the cell-thermosensitive hydrogel system, including TSG-6, IL-10 and PGE-2, are evaluated by corresponding ELISA kits. In brief, hUCMSCs are inoculated into 6-well plates and routinely cultured for 72 hours, replaced with 2.5 ml of 0.9% sodium chloride injection, and incubated at 37°C, 5% Incubate under CO2 conditions, place the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in a 6-well plate, add 1.5 ml of MSC complete medium pre-warmed at 37°C, and culture at 37°C, 5% CO2 for 72 hours, replace with 2.5 ml of 0.9% sodium chloride injection, and incubate at 37°C, 5% CO2. At D0, D3, D7, D14, and D30, take the incubation supernatant and measure the absorbance OD values ​​of TSG-6, IL-10, and PGE-2 at 450 nm according to the ELISA kit. Calculate the concentrations of TSG-6, IL-10, and PGE-2 according to the standard curve.

[0020] A use of hUCMSC / SVF-PEP@Gel. The prepared SVF / hUCMSC-PEP@Gel thermosensitive hydrogel is liquid at room temperature (25°C) and turns into a semisolid gel at body temperature (37°C). It provides effective attachment for human umbilical cord mesenchymal stem cells, prevents the stem cells from being lost from the joint cavity with the solution, and prolongs the retention time of hUCMSC or hUCMSC / SVF at the injection site. The hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel cell-thermosensitive hydrogel systems are successfully prepared. After 30 days, all cells in the hUCMSC control group have died, while cells in the hUCMSC-PEP@Gel group and the hUCMSC / SVF-PEP@Gel group are still alive, indicating that the PEP thermosensitive hydrogel provides a good 3D environment and spatial support for hUCMSC / SVF, and maintains cell activity and survival time in vitro for a long time.

[0021] Compared with the prior art, the beneficial effects of the present invention are: EP hydrogel serves as a protective carrier for hUCMSC delivery, and SVF and PEP hydrogels both help to inhibit the expression of inflammatory cytokines and induce the chondrogenic differentiation of hUCMSC and have a synergistic effect, indicating that PEP@Gel hydrogel has potential application prospects in OA treatment as a protective carrier for cell delivery, and the combined application of hUCMSC / SVF and PEP@Gel is expected to achieve bone regeneration and repair more efficiently, and is suitable for cartilage regeneration in the clinical treatment of osteoarthritis. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 is a flow chart of the present invention;

[0023] Figure 2 This is a diagram showing the effect of hUCMSC and hUCMSC / SVF of the present invention on the phase transition and gelation temperature of PEP@Gel;

[0024] Figure 3 This is a survival diagram of hUCMSCs of the present invention;

[0025] Figure 4 This is the immunofluorescence staining diagram of type II collagen of the present invention;

[0026] Figure 5 The osteogenic, adipogenic and chondrogenic differentiation capabilities of hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel of the present invention are shown in FIG.

[0027] Figure 6 The figure shows the secretion of TSG-6, IL-10 and PGE-2 by hUCMSC of the present invention. DETAILED DESCRIPTION

[0028] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0029] See also Figure 1-6 The present invention provides a preparation method of hUCMSC / SVF-PEP@Gel, comprising the following steps:

[0030] Step 1, isolation and culture of hUCMSC: culture P0 hUCMSC by tissue block method, add 0.25% trypsin solution and 1mL aprotinin solution, digest, harvest the precipitate, precipitate cells, inoculate and culture for later use;

[0031] Step 2, extraction and culture of SVF: 60 ml of adipose tissue obtained by liposuction was repeatedly rinsed 2-3 times with sterile PBS until the washing solution was clear, and an equal volume of 0.075% type I collagenase was added, and the mixture was placed in a 37°C constant temperature shaker for shaking and digestion for about 40 minutes, filtered with a 60-mesh cell sieve, and the filtrate was collected and centrifuged at 400×g for 10 minutes to remove the oil layer and milky cell layer, and the clarified supernatant was carefully discarded, and resuspended into 6 ml of cell suspension with 0.9% sodium chloride injection solution, which is the SVF stock solution;

[0032] Step 3. Preparation of X hUCMSC and 2X hUCMSC / SVF suspension: Take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml 0.9% sodium chloride injection to make 2X hUCMSC for use; take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml SVF stock solution to make 2X hUCMSC / SVF suspension containing 2×10 6 / ml hUCMSC for standby use;

[0033] Step 4, preparation of hUCMSC, hUCMSC / SVF-PEP@Gel: 50g PLGA1500-PEG1200-PLGA1500 was stirred evenly by low-temperature vortex at 4°C, dispersed and dissolved in 100g pure water to prepare PEP@Gel with a volume fraction of 50%, and then 10ml of pure water, 2X hUCMSC or 2X hUCMSC / SVF suspension was added to 10ml of 50% PEP@Gel by mass, and mixed evenly to prepare PEP@Gel with a mass fraction of 25%, or hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel containing a final concentration of 1×106 / ml hUCMSC. Under the condition of 4-8°C, PEP@Gel, hUCMSC-PEP@Gel, and hUCMSC / SVF-PEP@Gel were respectively poured into a 24-well plate, 0.5ml / well, and placed at 37°C for coagulation;

[0034] Step 5. Multi-faceted detection and identification: Phase transition temperature measurement of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel, hUCMSC survival examination, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition examination, osteogenic, adipogenic, and chondrogenic differentiation potential analysis of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel, and secretory effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel.

[0035] The culture system in step 1 is MSC complete medium DMEM / F1212400-024, GIBCO, 10% animal-free serum substitute C08003C, Stemboscience, and 0.25% trypsin solution and 1 mL aprotinin solution are added in step 1. Specifically, when the culture reaches 12 days, the culture bottle is gently shaken to suspend the residual tissue pieces, the culture supernatant is carefully aspirated, the culture surface is washed once with PBS, and 0.25% trypsin solution T6424-1VL, Biological industries, digested at room temperature for 5 minutes, added 1mL of aprotinin solution 1A1250000, Sigma to terminate digestion, harvested the precipitate in step one, specifically centrifuged at 400×g for 5 minutes, discarded the supernatant, harvested the precipitate; washed twice with PBS, filtered with a 100μm nylon cell sieve, and collected the filtrate; centrifuged at 400×g for 5 minutes, discarded the supernatant, harvested the precipitated cells, and recorded as P0 generation hUCMSC, inoculated and cultured for standby in step one, specifically P0 generation hUCMSC was resuspended in MSC complete medium, inoculated into 175cm2 tissue culture flask EasyFlask, NUNC at 6×103 / cm2, and harvested P1 generation hUCMSC when cultured to 70-80% confluence; P1 generation hUCMSC continued to be passaged to P4, P4 hUCMSC was resuspended in 0.9% sodium chloride injection, and the cell concentration was adjusted to 4×106 / ml for standby.

[0036] In step 5, the phase transition temperature of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel was determined as follows: PEP@Gel with a mass fraction of 20%, 26%, 32%, 38%, 44%, and 50% was prepared by the same method, and equal volumes of pure water, 2X hUCMSC or 2X The hUCMSC / SVF suspension was mixed evenly to prepare PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with mass fractions of 10%, 13%, 16%, 19%, 22% and 25%, which were heated from 20°C to 65°C in a constant temperature water bath, and the solution-gel-precipitation phase transition temperatures of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel were measured, and the phase transition diagram was drawn. Subsequently, the elastic modulus G′ and viscous modulus G″ of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with a volume fraction of 25% were measured using an RH-20 rheometer to determine the gelation temperature.

[0037] The hUCMSC survival test in step 5 is as follows: gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, 1.5 ml of 0.9% sodium chloride injection solution pre-warmed at 37°C is added, and cultured at 37°C and 5% CO2. The medium is changed every other day. At D0, D3, D7, D14, and D30, the hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel culture groups are aspirated and the culture supernatant is discarded, and the cells are allowed to stand at 4-8°C for 30 minutes, and then transferred to 37°C and 5% CO2 for incubation for 1 hour. The three groups of samples are stained with a live and dead cell double staining kit for 30 minutes, the staining solution is aspirated and discarded, and the cells are rinsed 3 times with 0.9% sodium chloride injection solution and observed under an inverted fluorescence microscope. Green represents live cells and red represents dead cells.

[0038] In step 5, the hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition test is specifically as follows: the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C is added, and the plate is cultured at 37°C and 5% CO2. The medium is changed every other day. At D0, D3, D7, D14, and D30, the culture supernatant is aspirated and the plate is allowed to stand at 4-8°C for 30 minutes, and then the plate is transferred to 37°C and incubated at 5% CO2 for 1 hour, the culture supernatant is aspirated and fixed with 4% paraformaldehyde for 1 hour, and then washed three times with 4°C pre-cooled PBS. The cells are permeabilized with 0.1% Triton X-100 at room temperature for 20 minutes, and the cells are blocked with 10% goat serum by volume for 30 minutes; the anti-rabbit primary antibody is added and incubated overnight at 4°C, and goat anti-rabbit IgG H&L is added FITC, incubated at 37°C for 1 hour, washed three times with PBS, and observed under an inverted fluorescence microscope. Green fluorescence represents positive staining for type II collagen.

[0039] In step 5, the osteogenic, adipogenic, and chondrogenic differentiation potentials of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel are specifically as follows: the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, incubated at 4-8°C for 30 minutes, then transferred to 37°C, 5% CO2, and saturated humidity for 1 hour, MSC complete medium 1.5 ml / well is added, and incubated at 37°C, 5% CO2, and saturated humidity. The cells were cultured for 24 hours according to the instructions of the osteogenic differentiation kit, adipogenic differentiation kit, and chondrogenic differentiation kit. The medium was changed every other day. When the osteogenic differentiation reached 14 days, the cells were stained with Alizarin red staining. The red deposits represented callus formation, which was positive for bone differentiation. When the adipogenic differentiation reached 14 days, the cells were stained with Oil Red "O" staining. The red deposits represented lipid droplet formation, which was positive for adipogenic differentiation. When the chondrogenic differentiation reached 18 days, the cells were stained with Alcian blue staining. The blue-blue-green deposits represented acidic mucin extracellular matrix, which was positive for chondrogenic differentiation.

[0040] The secretion effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in step 5 is as follows: some anti-inflammatory cytokines of the cell-thermosensitive hydrogel system, including TSG-6, IL-10 and PGE-2, are evaluated by the corresponding ELISA kit. In brief, hUCMSCs are seeded into 6-well plates and cultured for 72 hours in a conventional manner, replaced with 2.5 ml of 0.9% sodium chloride injection, and incubated at 37°C and 5% CO2. The gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is then incubated with 1% 0.9% sodium chloride injection solution. F-PEP@Gel was placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C was added, and cultured at 37°C, 5% CO2 for 72 hours. Then 2.5 ml of 0.9% sodium chloride injection was replaced and incubated at 37°C, 5% CO2. At D0, D3, D7, D14, and D30, the incubation supernatant was taken and the absorbance OD values ​​of TSG-6, IL-10, and PGE-2 at 450 nm were measured on the ELISA kit according to the regulations, and the concentrations of TSG-6, IL-10, and PGE-2 were calculated according to the standard curve.

[0041] A use of hUCMSC / SVF-PEP@Gel. The prepared SVF / hUCMSC-PEP@Gel thermosensitive hydrogel is liquid at room temperature (25°C) and turns into a semisolid gel at body temperature (37°C). It provides effective attachment for human umbilical cord mesenchymal stem cells, prevents the stem cells from being lost from the joint cavity with the solution, and prolongs the retention time of hUCMSC or hUCMSC / SVF at the injection site. The hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel cell-thermosensitive hydrogel systems are successfully prepared. After 30 days, all cells in the hUCMSC control group have died, while cells in the hUCMSC-PEP@Gel group and the hUCMSC / SVF-PEP@Gel group are still alive, indicating that the PEP thermosensitive hydrogel provides a good 3D environment and spatial support for hUCMSC / SVF, and maintains cell activity and survival time in vitro for a long time.

[0042] In the present invention, P0 hUCMSCs were cultured by tissue block method, and the culture system was MSC complete medium DMEM / F1212400-024, GIBCO, 10% animal-free serum substitute C08003C, Stemboscience. When cultured for 12 days, the culture bottle was gently shaken to suspend the residual tissue blocks, and the culture supernatant was carefully discarded. The culture surface was washed once with PBS, and 0.25% trypsin solution T6424-1VL, Biological industries, was added, and digested at room temperature for 5 minutes. 1 mL of aprotinin solution 1A1250000, Sigma was added to terminate the digestion; centrifuged at 400×g for 5 minutes, the supernatant was discarded, and the precipitate was harvested; washed twice with PBS, filtered with a 100 μm nylon cell sieve, and the filtrate was collected; centrifuged at 400×g for 5 minutes, the supernatant was discarded, and the precipitated cells were harvested and recorded as P0 generation hUCMSCs; P0 generation hUCMSCs were resuspended in MSC complete medium and precipitated at 6×103 / cm 2 Inoculate to 175cm 2 Tissue culture flask EasyFlask, NUNC, harvest P1 hUCMSC when cultured to 70-80% confluence; P1 hUCMSC continue to be passaged to P4, P4 hUCMSC are resuspended in 0.9% sodium chloride injection, and the cell concentration is adjusted to 4×10 6 / ml, set aside, 60ml of adipose tissue obtained by liposuction was repeatedly rinsed 2-3 times with sterile PBS until the washing solution was clear, and an equal volume of 0.075% type I collagenase was added, and the mixture was placed in a 37°C constant temperature shaker for shaking and digestion for about 40 minutes, filtered with a 60-mesh cell sieve, and the filtrate was collected and centrifuged at 400×g for 10 minutes to remove the oil layer and milky cell layer, and the clarified supernatant was carefully discarded, and resuspended into 6ml cell suspension with 0.9% sodium chloride injection, which was the SVF stock solution, and 4×10 6 / ml hUCMSC suspension 5ml, add 5ml 0.9% sodium chloride injection to make 2XhUCMSC for use; take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml SVF stock solution to make 2X hUCMSC / SVF suspension containing 2×10 6 / ml hUCMSC for later use, 50g PLGA1500-PEG1200-PLGA1500 Sun-Lipo NanoTech, stir evenly with low temperature vortex in a medium pot at 4℃, disperse and dissolve in 100g pure water to prepare PEP@Gel with a volume fraction of 50%, and then add 10ml of pure water, 2X hUCMSC or 2X hUCMSC / SVF suspension to 10ml of PEP@Gel with a mass fraction of 50%, mix evenly, and prepare PEP@Gel with a mass fraction of 25%, or PEP@Gel with a final concentration of 1×10 6 / ml hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel were poured into 24-well plates at 0.5 ml / well under 4-8°C and placed at 37°C for coagulation. PEP@Gel with mass fractions of 20%, 26%, 32%, 38%, 44%, and 50% were prepared by the same method, and equal volumes of pure water, 2X The hUCMSC or 2XhUCMSC / SVF suspension was mixed evenly to prepare PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with mass fractions of 10%, 13%, 16%, 19%, 22% and 25%, which were heated from 20°C to 65°C in a constant temperature water bath, and the solution-gel-precipitation phase transition temperatures of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel were measured, and the phase transition diagrams were drawn. Tech, the elastic modulus G′ and the viscous modulus G″ of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with a volume fraction of 25% were measured in a medium pot to determine the gelation temperature, the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel was placed in a 6-well plate, 1.5 ml of 0.9% sodium chloride injection solution preheated at 37°C was added, and cultured at 37°C and 5% CO2. The medium was changed every other day, and the temperature was 0. At D1, D3, D7, D14, and D30, the culture supernatant of the hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel culture groups was discarded, the cells were allowed to stand at 4-8°C for 30 min, and then transferred to 37°C and 5% CO2 for incubation for 1 hour. The three groups of samples were stained with the Live and Dead Cell Double Staining Kit 3106135, Supelco for 30 min, the staining solution was discarded, and the cells were rinsed three times with 0.9% sodium chloride injection solution and observed under an inverted fluorescence microscope. Green represents live cells and red represents dead cells.

[0043] The gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel was placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C was added, and the cells were cultured at 37°C and 5% CO2. The medium was changed every other day. At D0, D3, D7, D14, and D30, the culture supernatant was aspirated and the cells were allowed to stand at 4-8°C for 30 minutes. After being transferred to 37°C and incubated at 5% CO2 for 1 hour, the culture supernatant was aspirated and fixed with 4% paraformaldehyde for 1 hour, and then washed three times with 4°C pre-cooled PBS. The cells were permeabilized with 0.1% Triton X-100 at room temperature for 20 minutes, and the cells were blocked with 10% goat serum for 30 minutes; the rabbit anti-human primary antibody ab34712 was added, and incubated overnight at 4°C, and goat anti-rabbit IgG H&L FITC was added ab6717, Abcam, incubated at 37℃ for 1 hour, washed with PBS 3 times, observed under an inverted fluorescence microscope, green fluorescence represents positive type II collagen staining, gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel was placed in a 6-well plate, incubated at 4-8℃ for 30 minutes, and then transferred to 37℃, 5% CO2, saturated humidity conditions for 1 hour, MSC complete medium 1.5ml / well was added, and cultured at 37℃, 5% CO2, saturated humidity conditions for 24 hours, cultured according to the instructions of osteogenic differentiation kit A1007201, GIBCO, adipogenic differentiation kit A1007001, GIBCO, chondrogenic differentiation kit A1007101, GIBCO, cultured every other day, osteogenic differentiation to 14 days, stained with Alizarin red staining, red deposition represents callus formation, bone differentiation is positive, adipogenic differentiation is positive, At 14 days of differentiation, the red deposits represented lipid droplet formation, which was positive for adipogenic differentiation. At 18 days of chondrogenic differentiation, the blue-blue-green deposits represented acidic mucin-like extracellular matrix, which was positive for chondrogenic differentiation. Some anti-inflammatory cytokines of the cell-thermosensitive hydrogel system, including TSG-6, IL-10 and PGE-2, were evaluated by corresponding ELISA kits. In brief, hUCMSCs were seeded into 6-well plates and cultured conventionally for 72 hours, replaced with 2.5 ml of 0.9% sodium chloride injection, and incubated at 37°C and 5% CO2. The gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel was placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C was added, and cultured at 37°C and 5% CO2 for 72 hours, replaced with 2.5 ml of 0.9% sodium chloride injection.5ml, incubate at 37℃, 5% CO2, take the incubation supernatant at D0, D3, D7, D14, D30, and measure the absorbance OD value of TSG-6, IL-10 and PGE-2 at 450nm according to the ELISA kit, and calculate the concentration of TSG-6, IL-10 and PGE-2 according to the standard curve.

[0044] SPSS 25.0 was used for statistical analysis, and the data were Indicates that the means were compared using independent sample t-test, P<0.05 was statistically significant. The effects of hUCMSC and SVF / hUCMSC on the phase transition and gelation temperature of PEP@Gel: The PLGA-PEG-PLGA PEP triblock copolymer with a mass fraction of 25% was liquid at room temperature. When heated to 37°C, the triblock copolymer solution automatically cross-linked to form a gel. Above the critical gel concentration, as the temperature increased, the polymer aqueous solution experienced three physical states: sol, gel, and sol suspension. The thermal coagulation properties of the 25wt% thermosensitive hydrogel aqueous solution were further evaluated using dynamic rheological analysis. The PEP polymer 25wt% exhibited a temperature-dependent solution-gel transition behavior, which exhibited solution-like behavior at 4°C and room temperature 25°C, and formed a gel at body temperature (37°C) (combined with the instructions attached). Figure 2 A), after adding hUCMSC and hUVMSC / SVF cells, the sol-gel-precipitation phase transition point of PEP polymer was observed to change, but it still showed solution-like behavior at 4°C and room temperature (25°C), and formed gel at body temperature (37°C), but the gelation temperature was increased. This is because the heat required after loading cells is large to transform the spatial structure of the polymer into gel (combined with the attached manual Figure 2 B and the attached manual Figure 2 C), combined with the instructions Figure 2 We monitored the changes in the elastic modulus (G') and viscous modulus (G") of the polymer aqueous solution after heating. For example, G' represents the elastic behavior and energy storage of the sample when it is deformed, while G" represents the viscous behavior. At low temperatures, G" is higher than G', indicating that it is in a free-flowing liquid state with good injectability. As the temperature increases, both increase, but G' increases faster. The modulus-temperature curing shows that the highest modulus temperature of the polymer solution (25wt%) is 32.6℃ (combined with the attached manual Figure 2 C), after adding hUCMSC and hUVMSC / SVF cells, the sol-gel transition points of PEP polymer were observed at 33.6°C and 33.9°C, respectively. At this time, G′ was equal to G″, which was higher than that of PEP polymer gelation temperature and longer gelation time (Figure 2). Figure 2 E and 1 are attached to the instruction manual Figure 2F), although the gelation temperature increased, it was still below the body temperature of 37°C, indicating that the phase change performance of this polymer thermosensitive gel is suitable for intra-articular injection of the polymer solution. After entering the joint cavity, the polymer solution quickly forms a gel due to the increase in temperature. The addition of hUCMSC and hUVMSC / SVF cells has little effect on its thermosensitive characteristics. A: Phase change diagram of PEP@Gel thermosensitive gel; B: Phase change diagram of PEP@Gel loaded with hUCMSC; C: Phase change diagram of PEP@Gel loaded with hUCMSC / SVF; D: The gelation temperature of 25wt% PEP polymer solution is 32.6°C; E: The gelation temperature of hUCMSC-PEP system is 33.6°C; F: The gelation temperature of hUCMSC / SVF-PE system is 33.9°C;

[0045] Effects of SVF and PEP on the viability of hUCMSC: During the 0-3 day culture period, there was little difference in the cell viability, cell state and cell shape between the hUCMSC, hUCMSC-PEP@Gel group and hUCMSC / SVF-PEP@Gel group (see the instruction manual). Figure 3), after 7 days of culture, only a few cells survived in the hUCMSC group, i.e., the control group. The survival rate of cells in the hUCMSC-PEP@Gel group was higher on the 7th day, and some cells were spindle-shaped and existed in an independently dispersed state, while the cells in the hUCMSC / SVF-PEP@Gel group showed a typical spindle-shaped morphology and were arranged in a vortex manner, indicating that the connectivity between cells improved. At 14 days, all the cells in the hUCMSC group had died, and the number of live cells (green fluorescence) and dead cells (red fluorescence) in the hUCMSC-PEP@Gel group were close. The number of live cells (green fluorescence) in the hUCMSC / SVF-PEP@Gel group was significantly more than the number of dead cells (red fluorescence). At 30 days, Green fluorescence can still be observed in the hUCMSC-PEP@Gel group, and very few cells still survive in an independently dispersed state. The cells in the hUCMSC / SVF-PEP@Gel group still grow well, and some cells die. The results of cell viability assay in this study show that PEP@Gel enhances the cell viability of hUCMSC, and SVF and 25% PEP@Gel have a synergistic enhancing effect on cell viability. hUCMSC still survive in SVF+PEP thermosensitive hydrogel for more than 30 days or even longer, indicating that the proportion of PEP@Gel thermosensitive hydrogel used in this study is suitable for supporting the growth of hUCMSC and providing space and support for cell proliferation. VF and PEP thermosensitive gels have a synergistic effect on h Effect of UCMSC on chondrogenic differentiation: On day 0 of cell differentiation culture, the ratio of type II collagen positive cells in the hUCMSC / SVF-PEP@Gel group (0.19±0.07) and the ratio of type II collagen positive cells in the hUCMSC+SVF group (0.17±0.05) were significantly higher than those in the hUCMSC control group (0.00±0.00) (P<0.05). There was no significant difference in the ratio of type II collagen positive cells between the hUCMSC / SVF-PEP@Gel group and the hUCMSC-PEP@Gel group (P>0.05). On day 3 of cell differentiation culture, the ratio of type II collagen positive cells in the hUCMSC / SVF-PEP@Gel group (0.26±0.11 ) and hUCMSC+SVF groups (0.22±0.09) were significantly higher than those in the hUCMSC control group (0.00±0.00) (P<0.05). There was no significant difference in the type II collagen positive cell ratios between the hUCMSC / SVF-PEP@Gel group and the hUCMSC-PEP@Gel group (P>0.05). After 7 days of differentiation culture, the type II collagen positive cell ratios in the hUCMSC / SVF-PEP@Gel group (0.39±0.13) and hUCMSC+SVF group (0.31±0.08) were significantly higher than those in the hUCMSC control group (0.00±0.00) (P<0.05), there was no significant difference in the ratio of type II collagen positive cells between the hUCMSC / SVF-PEP@Gel group and the hUCMSC-PEP@Gel group (P>0.05). After 14 days of differentiation culture, the ratio of type II collagen positive cells in the hUCMSC / SVF-PEP@Gel group and the hUCMSC-PEP@Gel group was significantly higher than that in the hUCMSC control group (0.15±0.03) (P<0.05). The ratio of type II collagen positive cells in the hUCMSC / SVF-PEP@Gel group (0.57±0.12) was significantly higher than that in the hUCMSC-PEP@Gel group (0.69±0.13). l group type II collagen positive cell ratio (0.32±0.10) (P<0.05, at 30 days of differentiation culture, the type II collagen positive cell ratios of hUCMSC / SVF-PEP@Gel group and hUCMSC-PEP@Gel group were significantly higher than those of hUCMSC control group (0.19±0.07) (P<0.05), and the type II collagen positive cell ratio of hUCMSC / SVF-PEP@Gel group (0.76±0.13) was significantly higher than that of hUCMSC-PEP@Gel group (0.43±0.09) (P<0.05), the instructions are attached. Figure 4 The results of quantitative analysis of type II collagen immunofluorescence staining showed that type II collagen was green fluorescent, and the number of positive cells stained with green fluorescence in the hUCMSC / SVF-PEP@Gel group and hUCMSC-PEP@Gel group was significantly higher than that in the hUCMSC control group; from 14 days of differentiation culture to the end of the experiment, the ratio of type II collagen positive cells in the hUCMSC / SVF-PEP@Gel group (0.57±0.12) was significantly higher than that in the hUCMSC-PEP@Gel group, and hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel had significant differences in osteogenesis, adipogenesis and chondrogenesis. The potential of hUCMSC, hUCMSC / SVF and PEP@Gel is different: Comparison of osteogenic potential: After 14 days of osteogenic differentiation culture after fusion, the cell structure in the center of the cell nodule gradually lost, calcium nodules were formed, and red nodules were seen by alizarin red staining. A large number of red nodules were seen in both hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel osteogenic differentiation groups, and the number of red nodules formed in the hUCMSC / SVF-PEP@Gel osteogenic differentiation group was significantly more than that in the hUCMSC-PEP@Gel osteogenic differentiation group, whether observed by gross observation or under a 40x microscope (see the instruction manual). Figure 5 A), Comparison of adipogenic potential: After 14 days of adipogenic differentiation culture, a large number of red grape-like lipid droplets appeared in the hUCMSC-PEP@Gel group, which showed a stronger adipogenic ability than the hUCMSC / SVF-PEP@Gel adipogenic differentiation group (see the instruction manual). Figure 5B), Comparison of chondrogenic potential: After 18 days of chondrogenic differentiation culture, blue staining of the extracellular matrix was observed in both the hUCMSC-PEP@Gel group and the hUCMSC / SVF-PEP@Gel chondrogenic differentiation group, indicating the secretion of acidic mucopolysaccharide; more chondrocytes were observed in the sections of the hUCMSC-PEP@Gel chondrogenic differentiation group and the hUCMSC / SVF-PEP@Gel chondrogenic differentiation group, proving that hUCMSC / SVF-PEP@Gel has a stronger chondrogenic ability (see Appendix for instructions). Figure 5 C), combined with the instructions Figure 6, PEP@Gel hydrogel inhibits the expression of anti-inflammatory cytokines in hUCMSCs: ELISA test results of TSG-6: The TSG-6 concentrations (ng / ml) of the hUCMSC / SVF-PEP@Gel group at D7 (28.16±2.35), D14 (31.52±2.09) and D30 (30.74±1.65) and the hUCMSC-PEP@Gel group at D7 (28.47±1.83), D14 (28.68±1.91) and D30 (27.23±2.12) were significantly higher than those of the hUCMSC control group at D7 (25.62±2.12), D14 (24.45±1.26), D30 (25.11±2.21). The concentration of TSG-6 (ng / ml) in the hUCMSC / SVF-PEP@Gel group at D14 (31.52±2.09) and D30 (30.74±1.65) was significantly higher than that in the hUCMSC-PEP@Gel group at D14 (28.68±1.91) and D30 (27.23±2.12) (P<0.05). The results of ELISA test of IL-10: the concentration of IL-10 in the hUCMSC / SVF-PEP@Gel group at D7 (101.23±3.78) and the hUCMSC-PEP@Gel group at D7 (98.25±4.18) were significantly higher than those in the hUCMSC-PEP@Gel group at D7 (101.23±3.78) (P<0.05). g / ml) were significantly higher than those of the hUCMSC control group at D7 (88.22±4.78) (P<0.05); the IL-10 concentrations (pg / ml) of the hUCMSC / SVF-PEP@Gel group at D14 (105.73±4.21) and D30 (99.81±3.09) were significantly higher than those of the hUCMSC-PEP@Gel group at D14 (93.58±3.67) and D30 (83.31±4.02) and the hUCMSC control group at D14 (85.69±3.66) and D30 (76.28±4.12) (P<0.05). Test results: The PGE-2 concentration (pg / ml) of hUCMSC / SVF-PEP@Gel group D7 (500.31±33.11) and hUCMSC-PEP@Gel group D7 (492.23±31.35) was significantly higher than that of hUCMSC control group D7 (463.89±37.46) (P<0.05); the PGE-2 concentration (pg / ml) of hUCMSC / SVF-PEP@Gel group D14 (510.26±18.52) and D30 (506.34±26.78) was significantly higher than that of hUCMSC control group D14 (459.74±23.52) and D30 (455.37±7.66) (P<0.05); the PGE-2 concentration (pg / ml) of the hUCMSC-PEP@Gel group at D14 (485.11±33.27) was significantly higher than that of the hUCMSC control group at D14 (459.74±23.52) (P<0.05); the PGE-2 concentration (pg / ml) of the hUCMSC / SVF-PEP@Gel group at D30 (506.34±26.78) was significantly higher than that of the hUCMSC-PEP@Gel group at D30 (473.53±24.51) (P<0.05). .

[0046] The manufacture of injectable sol-gel systems for biomedical applications is increasing. Therapeutic drugs, growth factors or cells pre-doped in liquid sol-gel solutions are directly injected into the desired tissue, organ or body cavity in a minimally invasive manner, and then form a gel scaffold in situ. To date, most research on injectable materials has focused on biopolymers. Hydrogels are cross-linked amphiphilic polymer networks with elastic solid properties, deformability and softness. Due to their high water content, biocompatibility and permeability to a variety of biomolecules, hydrogels are widely used in tissue engineering, drug delivery and biological research. hUCMSC and SVF have gradually become hot topics in recent years and have been applied to the treatment of different types of diseases in various fields. Both CMSC and SVF have different degrees of differentiation and proliferation ability, different immune phenotypes, different gene expressions, and even different tissue dynamics, and differentiate into bone cells, chondrocytes, and adipocytes under different induction environments. Although biomaterial-based hydrogels effectively encapsulate MSCs and improve long-term cell survival, insufficient retention of MSCs in the injected defect site is still the main obstacle to the successful outcome of MSCs treatment of cartilage defects. To date, various methods have been proposed to overcome this problem. Among the different methods used to prolong cell survival and retention in tissue defect sites, thermosensitive hydrogels have been widely used to improve cell retention due to their simple operation. Thermosensitive hydrogels are three-dimensional (3D) networks composed of triblock polymers. , whose physical and chemical properties are similar to those of the extracellular matrix (ECM), and are suitable for repairing or regenerating tissues and quickly restoring the biomechanical function of tissues. The injected polymer biomaterial microbeads not only prevent the shear force generated by cells during delivery, but also form a strong niche at the injection site, allowing the paracrine factors to be concentrated. At present, we have tried for the first time to prepare hUCMSC, hUCMSC / SVF and thermosensitive hydrogel into a cell-thermosensitive hydrogel system for intra-articular injection treatment of OA, and to explore the effect of hUCMSC, SVF / hUCMSC combined with PEP gel to effectively improve long-term cell survival and chondrogenic differentiation. The SVF / hUCMSC-PEP@Gel thermosensitive hydrogel prepared in this study, at room temperature ( At 25℃, it is liquid, and at body temperature (37℃), it turns into a semi-solid gel, which provides effective attachment for human umbilical cord mesenchymal stem cells, prevents the loss of stem cells from the joint cavity with the solution, and prolongs the retention time of hUCMSC or hUCMSC / SVF at the injection site. We successfully prepared hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel cell-thermosensitive hydrogel systems. After 30 days, all cells in the hUCMSC control group had died, while cells in the hUCMSC-PEP@Gel group and hUCMSC / SVF-PEP@Gel group were still alive, indicating that PEP thermosensitive hydrogel provides a good 3D environment and spatial support for hUCMSC / SVF.Long-term maintenance of cell activity and survival time in vitro and realization of directional osteogenic differentiation of stem cells are the key to bone regeneration. We studied the osteogenic differentiation effect of PEP@Gel on hUCMSC and hUCMSC / SVF in vitro by detecting the ratio of intracellular type II collagen (a key factor for cartilage differentiation). After 14 and 30 days of co-culture, the ratio of intracellular type II collagen in the hUCMSC / SVF-PEP@Gel group and hUCMSC-PEP@Gel group was significantly higher than that in the hUCMSC control group, and the ratio of intracellular type II collagen in the hUCMSC / SVF-PEP@Gel group was significantly higher than that in the hUCMSC-PEP@ Gel group, proving that SVF, PEP@Gel and SVF / PEP@Gel co-cultured with hUCMSC all enhanced the chondrogenic differentiation ability of cells. This study also verified through experiments that hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel had strong osteogenic and chondrogenic differentiation abilities. After 14 days of osteogenic differentiation culture, scattered red positive nodules were observed under the naked eye and microscope by alizarin red staining. The red nodules in the hUCMSC / SVF-PEP@Gel group were significantly more than those in the hUCMSC-PEP@Gel group, proving that hUCMSC / SVF-PEP@Gel has strong osteogenic and chondrogenic differentiation abilities. It has strong osteogenic differentiation ability in vitro. In the experiment, hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel were also induced to adipogenesis and chondrogenesis. In adipogenesis, hUCMSC-PEP@Gel showed stronger adipogenesis ability, which reversely proved the advantage of hUCMSC / SVF-PEP@Gel in osteogenic induction. hUCMSC / SVF-PEP@Gel also showed strong advantages in chondrogenic induction, proving that hUCMSC / SVF-PEP@Gel hydrogel retains hUCMSC and its multiple differentiation potentials of stem cells at the same time. The osteogenic and chondrogenic differentiation ability of hUCMSCs was enhanced. In addition, PEP@Gel hydrogel reversed OA inflammation by promoting the expression of anti-inflammatory cytokines paracrine by hUCMSCs. The analysis proved that excessive ROS participated in multiple signaling pathways, activated various cytokines, enhanced the inflammatory response, hindered cell viability and inhibited cartilage formation in OA. Mesenchymal stem cells regulate immune responses and inhibit inflammation by secreting cytokines, such as inhibiting the body's inflammatory response by upregulating TSG6, IL-10, and PGE2. Here, the cultured hUCMSCs and their secretions were collected, and the cytokine expression was determined by ELISA, such as, Figure 6As shown in AC, when cells were treated with PEP@Gel (hUCMSC-PEP@Gel group), the expression of anti-inflammatory factors TSG6, IL-10, and PGE2 was significantly upregulated; after the addition of SVF (hUCMSC / SVF-PEP@Gel group), the expression of anti-inflammatory factors TSG6, IL-10, and PGE2 were also significantly enhanced, and at some time points, there were significant differences in the upregulation of TSG6, IL-10, and PGE2 between the hUCMSC / SVF-PEP@Gel group and the hUCMSC-PEP@Gel group, indicating that the co-culture of hUCMSC and PEP@Gel hydrogel promoted the increase in the level of anti-inflammatory factors, and the addition of SVF had a synergistically enhanced anti-inflammatory effect, which alleviated the oxidative stress state in the process of OA and thus reversed the inflammatory state.

[0047] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A preparation method of hUCMSC / SVF-PEP@Gel, characterized in that: The following steps are involved: Step 1, isolation and culture of hUCMSC: culture P0 hUCMSC by tissue block method, add 0.25% trypsin solution and 1mL aprotinin solution, digest, harvest the precipitate, precipitate cells, inoculate and culture for later use; Step 2, extraction and culture of SVF: 60 ml of adipose tissue obtained by liposuction was repeatedly rinsed 2-3 times with sterile PBS until the washing solution was clear, and an equal volume of 0.075% type I collagenase was added, and the mixture was placed in a 37°C constant temperature shaker for shaking and digestion for about 40 minutes, filtered with a 60-mesh cell sieve, and the filtrate was collected and centrifuged at 400×g for 10 minutes to remove the oil layer and milky cell layer, and the clarified supernatant was carefully discarded, and resuspended into 6 ml of cell suspension with 0.9% sodium chloride injection solution, which is the SVF stock solution; Step 3. Preparation of X hUCMSC and 2X hUCMSC / SVF suspension: Take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml0.9% sodium chloride injection to make 2X hUCMSC for use; take 4×10 6 / ml hUCMSC suspension 5ml, add 5ml SVF stock solution to make 2X hUCMSC / SVF suspension containing 2×10 6 / ml hUCMSC for standby use; Step 4, preparation of hUCMSC, hUCMSC / SVF-PEP@Gel: 50g PLGA1500-PEG1200-PLGA1500 was stirred evenly with a low-temperature vortex at 4°C, dispersed and dissolved in 100g pure water to prepare PEP@Gel with a volume fraction of 50%, and then 10ml of pure water, 2X hUCMSC or 2X hUCMSC / SVF suspension was added to 10ml of 50% PEP@Gel by mass, and mixed evenly to prepare PEP@Gel with a mass fraction of 25%, or hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel containing a final concentration of 1×106 / ml hUCMSC. Under the condition of 4-8°C, PEP@Gel, hUCMSC-PEP@Gel, and hUCMSC / SVF-PEP@Gel were respectively perfused into a 24-well plate, 0.5ml / well, and placed at 37°C for coagulation; Step 5. Multi-faceted detection and identification: Phase transition temperature measurement of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel, hUCMSC survival examination, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition examination, osteogenic, adipogenic, and chondrogenic differentiation potential analysis of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel, and secretory effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel.

2. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The culture system in step 1 is MSC complete culture medium DMEM / F1212400-024, GIBCO, 10% animal-free serum substitute C08003C, Stemboscience, and 0.25% trypsin solution and 1 mL aprotinin solution are added in step 1. Specifically, when the culture is cultured for 12 days, the culture bottle is gently shaken to suspend the residual tissue blocks, the culture supernatant is carefully discarded, the culture surface is washed once with PBS, and 0.25% trypsin solution T6424-1VL, Biological industries, digested at room temperature for 5 minutes, added 1mL of aprotinin solution 1A1250000, Sigma to terminate digestion, the precipitate harvested in the step one is specifically centrifuged at 400×g for 5 minutes, discarded the supernatant, and the precipitate is harvested; washed twice with PBS, filtered with a 100μm nylon cell sieve, and the filtrate is collected; centrifuged at 400×g for 5 minutes, the supernatant is discarded, and the precipitated cells are harvested, recorded as P0 generation hUCMSC, and the inoculation and culture standby in the step one is specifically resuspended in MSC complete medium, inoculated into 175cm2 tissue culture flask EasyFlask, NUNC at 6×103 / cm2, and harvested when the P1 generation hUCMSC is cultured to 70-80% confluence; the P1 generation hUCMSC is continued to be passaged to P4, and the P4 hUCMSC is resuspended in 0.9% sodium chloride injection, and the cell concentration is adjusted to 4×106 / ml for standby.

3. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The phase transition temperature determination of hUCMSC-PEP@Gel and hUCMSC / SV-PEP@Gel in step 5 is as follows: PEP@Gel with a mass fraction of 20%, 26%, 32%, 38%, 44%, and 50% is prepared by the same method, and equal volumes of pure water, 2X hUCMSC or 2X The hUCMSC / SVF suspension was mixed evenly to prepare PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with mass fractions of 10%, 13%, 16%, 19%, 22% and 25%, which were heated from 20°C to 65°C in a constant temperature water bath, and the solution-gel-precipitation phase transition temperatures of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel were measured, and the phase transition diagram was drawn. Subsequently, the elastic modulus G′ and viscous modulus G″ of PEP@Gel, hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel with a volume fraction of 25% were measured using an RH-20 rheometer to determine the gelation temperature.

4. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The hUCMSC survival test in step 5 is specifically as follows: placing the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in a 6-well plate, adding 1.5 ml of 0.9% sodium chloride injection pre-warmed at 37°C, culturing at 37°C and 5% CO2, changing the medium every other day, and at D0, D3, D7, D14, and D30, the hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel culture groups discard the culture supernatant, let stand at 4-8°C for 30 minutes, and then transfer to 37°C and 5% CO2 for incubation for 1 hour. The three groups of samples are stained with a live and dead cell double staining kit for 30 minutes, the staining solution is discarded, and the samples are rinsed 3 times with 0.9% sodium chloride injection and observed under an inverted fluorescence microscope. Green represents live cells and red represents dead cells.

5. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel type II collagen deposition test in step 5 is specifically as follows: placing the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in a 6-well plate, adding 1.5 ml of MSC complete medium pre-warmed at 37°C, culturing at 37°C and 5% CO2, changing the medium every other day, discarding the culture supernatant at D0, D3, D7, D14, and D30, standing at 4-8°C for 30 minutes, and then transferring to 37°C and incubating at 5% CO2 for 1 hour, discarding the culture supernatant, fixing with 4% paraformaldehyde for 1 hour, then washing 3 times with 4°C pre-cooled PBS, permeabilizing the cells with 0.1% Triton X-100 at room temperature for 20 minutes, and blocking the cells with 10% goat serum by volume for 30 minutes; adding rabbit anti-human primary antibody and incubating at 4°C overnight, adding goat anti-rabbit IgGH&L FITC, incubated at 37°C for 1 hour, washed three times with PBS, and observed under an inverted fluorescence microscope. Green fluorescence represents positive staining for type II collagen.

6. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The osteogenic, adipogenic and chondrogenic differentiation potential of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in step 5 is specifically as follows: the gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is placed in a 6-well plate, incubated at 4-8°C for 30 minutes, then transferred to 37°C, 5% CO2, saturated humidity and incubated for 1 hour, 1.5 ml / well of MSC complete medium is added, and the plate is incubated at 37°C, 5% CO2, saturated humidity and incubated for 1 hour. After 24 hours of culture, the cells were cultured according to the instructions of the osteogenic differentiation kit, adipogenic differentiation kit, and chondrogenic differentiation kit. The medium was changed every other day. On the 14th day of osteogenic differentiation, the cells were stained with Alizarin red staining. The red deposits represented callus formation, which was positive for osteogenic differentiation. On the 14th day of adipogenic differentiation, the cells were stained with Oil Red "O" staining. The red deposits represented lipid droplet formation, which was positive for adipogenic differentiation. On the 18th day of chondrogenic differentiation, the cells were stained with Alcian blue staining. The blue-blue-green deposits represented acidic mucin extracellular matrix, which was positive for chondrogenic differentiation.

7. The preparation of hUCMSC / SVF-PEP@Gel according to claim 1, characterized in that: The secretion effect of hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel in step 5 is specifically as follows: some anti-inflammatory cytokines of the cell-thermosensitive hydrogel system, including TSG-6, IL-10 and PGE-2, are evaluated by corresponding ELISA kits. In brief, hUCMSCs are seeded into 6-well plates and cultured for 72 hours in a conventional manner, replaced with 2.5 ml of 0.9% sodium chloride injection, and incubated at 37°C and 5% CO2. The gelled hUCMSC-PEP@Gel or hUCMSC / SVF-PEP@Gel is then incubated with 1% 0.9% sodium chloride injection solution. VF-PEP@Gel was placed in a 6-well plate, 1.5 ml of MSC complete medium pre-warmed at 37°C was added, and cultured at 37°C, 5% CO2 for 72 hours. Then 2.5 ml of 0.9% sodium chloride injection was replaced and incubated at 37°C, 5% CO2. At D0, D3, D7, D14, and D30, the incubation supernatant was taken and the absorbance OD values ​​of TSG-6, IL-10, and PGE-2 at 450 nm were measured on the ELISA kit according to the regulations, and the concentrations of TSG-6, IL-10, and PGE-2 were calculated according to the standard curve.

8. The use of hUCMSC / SVF-PEP@Gel according to any one of claims 1 to 7, characterized in that: The prepared SVF / hUCMSC-PEP@Gel thermosensitive hydrogel is liquid at room temperature (25°C) and turns into a semisolid gel at body temperature (37°C), which provides effective attachment for human umbilical cord mesenchymal stem cells, prevents the stem cells from being lost from the joint cavity with the solution, and prolongs the retention time of hUCMSC or hUCMSC / SVF at the injection site. The hUCMSC-PEP@Gel and hUCMSC / SVF-PEP@Gel cell-thermosensitive hydrogel systems were successfully prepared. After 30 days, all the cells in the hUCMSC control group had died, while the cells in the hUCMSC-PEP@Gel group and the hUCMSC / SVF-PEP@Gel group were still alive, indicating that the PEP thermosensitive hydrogel provides a good 3D environment and spatial support for hUCMSC / SVF, and maintains cell activity and survival time in vitro for a long time.