Component for a delivery system and method and apparatus for producing a component for a delivery system

By embedding tubular elements of fiber material and wrinkle patterns that enhance the surface area into the cigarette holders of tobacco industry products, the problem of the cigarette holder temperature rising after the aerosol is heated is solved, achieving better aerosol cooling and use experience.

CN118870993APending Publication Date: 2024-10-29NICOVENTURES TRADING LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202280088668.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2021-12-29
Filing Date
2022-12-29
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

In the aerosol generated when existing tobacco industry products are heated, the aerosol-forming agent material is aerosolized after being heated, causing the temperature of the cigarette holder to rise and affecting the user experience.

Method used

Using a cigarette holder made of fiber material, first and second tubular elements are embedded therein so that they are distributed circumferentially and longitudinally of the fiber material to form a cavity to cool the aerosol, and to enhance the surface area of ​​the material through a wrinkle pattern for absorption Moisture reduces the temperature of the cigarette holder.

Benefits of technology

It effectively reduces the temperature of the cigarette holder, improves the cooling effect of the aerosol, improves the use experience, and reduces the heat transfer to the user's mouth.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118870993A_ABST
    Figure CN118870993A_ABST
Patent Text Reader

Abstract

A component (2) for use in or as an article (1) of an aerosol providing system (100) is provided, the component (2) comprising a body (4) of fibrous material. The first and second tubular elements (4a, 4b) extend substantially along a common axis through the body (4) of fibrous material, and the first and second tubular elements (4a, 4b) are each circumferentially surrounded by said fibrous material. There is also described a component (2) for use in or as an article (1) of an aerosol providing system, the component (2) comprising a body (4) of fibrous material and a tubular element (4a, 4b) embedded within the body (4) such that it is circumferentially and longitudinally surrounded by the fibrous material forming said body (4). There is also described an article (1) for use in or as an aerosol providing system, the article (1) having a downstream end (2b) and comprising a body (4) of fibrous material and a tubular element (4a) circumferentially surrounded by said fibrous material, wherein the tubular element (4a) extends to a first longitudinal end (2a) of the body (4) and is spaced apart from a second longitudinal end (2b) of the body, and wherein the longitudinal end (2a) of the body to which the tubular element (4a) extends is spaced apart from the downstream end (2b) of the article (1). A method for forming a component (2) and an apparatus configured for producing a component (2) are also described.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to components for or used as aerosol providing systems. The present disclosure also relates to articles for or used as aerosol providing systems, and methods and apparatus for producing components for aerosol providing systems. Background Art

[0002] Some tobacco industry products generate an aerosol when used, which is inhaled by the user. For example, a tobacco heating device heats an aerosol generating substrate such as tobacco to form an aerosol by heating but not burning the substrate. These tobacco industry products typically include a mouthpiece through which the aerosol passes to reach the user's mouth. Summary of the invention

[0003] According to the embodiments described herein, according to a first aspect, a component for use in an aerosol providing system or as an article of an aerosol providing system is provided, the component comprising a fibrous material body, and a first tubular element and a second tubular element, the first tubular element and the second tubular element extending through the body substantially along a common axis and each being circumferentially surrounded by the fibrous material.

[0004] According to the embodiments described herein, according to a second aspect, a component for use in an aerosol providing system or as an article for an aerosol providing system is provided, the component comprising a fibrous material body and a tubular element embedded in the body, such that the tubular element is circumferentially and longitudinally (in the length direction, longitudinally) surrounded by the fibrous material forming the body.

[0005] According to the embodiments described herein, according to a third aspect, there is provided an article for use in an aerosol providing system or as an aerosol providing system, the article having a downstream end, and the article comprising a fibrous material body and a tubular element circumferentially surrounded by the fibrous material, wherein the tubular element extends to a first longitudinal end of the body and is spaced apart from a second longitudinal end of the body, and wherein the longitudinal end of the body to which the tubular element extends is spaced apart from the downstream end of the article.

[0006] According to an embodiment described herein, according to a fourth aspect, there is provided a method for forming a component of an article for use in an aerosol providing system, the method comprising applying a pleat pattern to a sheet material, the pleat pattern comprising a series of substantially parallel ridges and grooves, providing a supply of tubular elements, and gathering the sheet material around the tubular elements to form a material body, wherein at least one tubular element extends through the body substantially along a common axis and the at least one tubular element is circumferentially surrounded by the fibrous material.

[0007] According to the embodiments described herein, according to a fifth aspect, there is provided an apparatus configured for producing a component according to the fourth aspect, the apparatus comprising a crimping roller for applying a corrugation pattern to a sheet, the corrugation pattern comprising a series of substantially parallel ridges and grooves, a feed mechanism for a tubular element, and a garniture assembly for gathering the sheet around the tubular element to form a material body, wherein at least one tubular element extends through the body substantially along a common axis and the at least one tubular element is circumferentially surrounded by the fibrous material. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Embodiments of the present invention will now be described, by way of non-limiting example only, with reference to the accompanying drawings, in which:

[0009] Figure 1 is a side cross-sectional view of an article for use as or with a non-flammable aerosol providing device, the article comprising a mouthpiece;

[0010] Figure 1B — is formed Figure 1 A side view of a sheet of first material body of the illustrated article.

[0011] Figure 2 is a side cross-sectional view of another embodiment of an article for use as or with a non-flammable aerosol providing device;

[0012] Figure 3 is a side cross-sectional view of another embodiment of an article for use as or with a non-flammable aerosol providing device;

[0013] Figure 4 is a side cross-sectional view of another article used as or in conjunction with a non-flammable aerosol providing device;

[0014] Figure 5- is a side cross-sectional view of another article used as or in conjunction with a non-flammable aerosol providing device;

[0015] Figure 6 Is used from Figures 1 to 5 A perspective view of a non-flammable aerosol providing device for generating an aerosol from an aerosol-generating material of the article shown;

[0016] Figure 7 Shows the outer cover removed and no product present Figure 6 The device shown;

[0017] Figure 8 yes Figure 7 a partially cut-away side view of the device shown;

[0018] Fig. 9 yes Figure 7 an exploded view of the device shown, with the housing omitted;

[0019] Fig. 10A yes Figure 7 a cross-sectional view of a portion of the device shown; and

[0020] Fig. 10B yes Fig. 10A A close-up illustration of an area of ​​the device shown. DETAILED DESCRIPTION

[0021] In the figures described herein, like reference numerals are used to describe equivalent features, articles, or components.

[0022] Figure 1 is a side cross-sectional view of an article 1 for use with a non-flammable aerosol delivery system.

[0023] The article 1 comprises a mouthpiece 2 and a cylindrical rod of an aerosol-generating material 3 (in the case of the present invention, a tobacco material) connected to the mouthpiece 2. The aerosol-generating material 3 provides an aerosol when heated, for example, in a non-flammable aerosol providing device as described herein (e.g., a non-flammable aerosol providing device comprising a coil), thereby forming a system. In other embodiments, the article 1 may include its own heat source, thereby forming an aerosol providing system that does not require a separate aerosol providing device.

[0024] The mouthpiece 2 of the article 1 comprises an upstream end 2a adjacent to the aerosol generating material 3 and a downstream end 2b distal to the aerosol generating material 3 .

[0025] The aerosol-generating material 3 (also referred to herein as the aerosol-generating substrate 3) includes at least one aerosol-former material. In an example of the present invention, the aerosol-former material is glycerol. In an alternative example, the aerosol-former material may be another material or a combination thereof as described herein. It has been found that the aerosol-former material improves the sensory properties of the product by helping to transfer compounds such as flavor compounds from the aerosol-generating material to the consumer. However, a problem with adding such an aerosol-former material to the aerosol-generating material in the product for the non-flammable aerosol providing system may be that when the aerosol-former material is aerosolized after heating, it may increase the mass of the aerosol delivered by the product, and this increased mass may maintain a higher temperature as it passes through the mouthpiece. As it passes through the mouthpiece, the aerosol transfers heat to the mouthpiece, which warms the outer surface of the mouthpiece, including the area in contact with the consumer's lips during use. Mouthpiece temperatures may be significantly higher than what consumers are accustomed to when smoking (eg, conventional cigarettes), and this may be an undesirable effect caused by the use of such aerosol former materials.

[0026] In the example of the present invention, the mouthpiece comprises a first material body 4, in which a first tubular element 4a and a second tubular element 4b are embedded. The first tubular element and the second tubular element are embedded in the material body 4 and are circumferentially surrounded by the material forming the body 4. The first material body is wrapped in a first plug wrap 7 (high-speed filter plug wrap).

[0027] In an embodiment of the present invention, the body 4 is a filter. However, it should be appreciated that in other embodiments, the body 4 may be provided solely to function as a carrier or support for the first and second tubular elements 4a, 4b without substantially filtering the inhalant of the article 1.

[0028] The first material body 4 is formed of a fibrous material. In an example of the present invention, the first material body 4 is formed of a sheet 14. The sheet 14 can be folded to form the material body 4. The material body 4 can be formed by a continuous web of a sheet. In an example of the present invention, the sheet 14 is gathered in a manner similar to a "crepe filter" to form the material body 4. The first tubular element 4a and the second tubular element 4b are embedded and circumferentially surrounded by the gathered sheet to form the first material body 4.

[0029] In the example of the present invention, the first tubular element 4a is positioned at the longitudinal end of the material body 4 and extends to the longitudinal end of the body. The second tubular element 4b is positioned downstream of the first tubular element 4a, and the material body 4 extends outside the second tubular element 4b, so that the second tubular element is circumferentially and longitudinally surrounded by the first material body 4. Advantageously, this arrangement can simplify the production process because the cavity and the filter portion can be formed in the same material body 4. Alternatively, other objects can be embedded in the material body 4, such as an aerosol modifier (aerosol-modifying agent) release component.

[0030] In an example of the present invention, the first tubular element 4a and the second tubular element 4b are separated by a gap of about 1mm to form an effectively continuous tubular portion. In the embodiment in which the first tubular element 4a and the second tubular element 4b are intended to form an effectively continuous tubular portion, the tubular element can be suitably separated by a gap of 0.5mm to 6mm, for example a gap of 1mm to 3mm, or a gap of 2mm to 5mm. In an example of the present invention, the air gap in the cigarette holder is defined by the tubular portion formed by the first tubular element 4a and the second tubular element 4b, and this air gap is used as a cooling section. In other embodiments, a single tubular element in tubular element 4a, 4b can form a tubular portion for aerosol cooling, and another in the tubular element can be positioned at other positions in the body 4.

[0031] The air gap provides a chamber through which the heated volatile components generated by the aerosol generating material 3 flow. The tubular elements 4a, 4b are hollow to provide a chamber for aerosol accumulation, but are rigid enough to withstand axial pressure and bending moments that may be generated during production and when the article 1 is in use. The tubular portion formed by the first tubular element 4a and the second tubular element 4b provides a physical displacement between the aerosol generating material 3 and the downstream portion of the mouthpiece 2. The physical displacement provided by the tubular portion will provide a thermal gradient over the length of the first material body 4.

[0032] Preferably, the combined internal volume of the tubular elements 4a, 4b is greater than 100 mm 3. It has been found that providing a cavity of at least this volume enables an improved aerosol to be formed. Such a cavity size provides sufficient space within the mouthpiece 2 to allow heated volatile components to cool, thereby allowing the aerosol generating material 3 to be exposed to higher temperatures than would otherwise be possible, as the latter might result in overheating of the aerosol. In examples of the present invention, the cavity is formed by adjacent tubular elements 4a, 4b, but in alternative arrangements the cavity may be formed by a single tubular element 4a. More preferably, the mouthpiece 2 comprises a cavity, for example formed by adjacent tubular elements 4a, 4b, having a volume greater than 120 mm 3 The internal volume is more preferably greater than 150 mm 3 In some examples, the internal cavity includes about 110 mm 3 To about 600mm 3 volume, and preferably, about 120 mm 3 To about 500mm 3 In the example of the present invention, the inner cavity formed by adjacent tubular elements 4a, 4b has a volume of about 250mm 3 Alternatively, where a single tubular element is arranged to provide the cooling section, the tubular element preferably has an internal volume as described above.

[0033] The cavity may be configured to provide a temperature difference of at least 40 degrees Celsius between the heated volatile components entering the first upstream end of the cavity and the heated volatile components exiting the second downstream end of the cavity. The cavity may be configured to provide a temperature difference of preferably at least 60 degrees Celsius, preferably at least 80 degrees Celsius, and more preferably at least 100 degrees Celsius between the heated volatile components entering the first upstream end of the cavity and the heated volatile components exiting the second downstream end of the cavity. Such a temperature difference over the length of the cavity may protect temperature sensitive components of the mouthpiece downstream of the cavity from the high temperature of the aerosol generating material 3 when the aerosol generating material 3 is heated.

[0034] Preferably, the length of the tubular portion is less than about 50 mm. More preferably, the length of the tubular portion is less than about 40 mm. Still more preferably, the length of the tubular portion is less than about 35 mm. Additionally or alternatively, the length of the tubular portion is preferably at least about 10 mm. Preferably, the length of the tubular portion is at least about 15 mm.

[0035] In some preferred embodiments, the length of the tubular portion is about 15mm to about 35mm, more preferably about 16mm to about 30mm, even more preferably about 18mm to about 25mm, most preferably about 23mm. In examples of the present invention, the length of the tubular portion is 23mm. In examples of the present invention, the tubular portion comprises a first tubular element 4a and a second tubular element 4b, which have a length of 11mm respectively and are separated by a gap of 1mm. As described herein, alternatively, the tubular portion can comprise a single tubular element 4a with a length as described above.

[0036] In other embodiments, the first and second tubular elements may be disposed at other locations within the body of material 4, or the body of material 4 itself may be disposed at different locations within the article, as described below.

[0037] In the example of the present invention, the first tubular element 4a and the second tubular element 4b have the same specifications, that is, the length, wall thickness and inner diameter of each tubular element are the same. Alternatively, the first tubular element and the second tubular element may have different specifications, for example, to provide different internal cavity volumes or ventilation at different locations in the mouthpiece.

[0038] In the examples of the present invention, the tubular elements 4a, 4b are each formed from a plurality of paper layers that are wound in parallel with butt joints to form a hollow tube. In the examples of the present invention, the first and second paper layers are arranged as a two-ply tube, but in other examples, 3, 4 or more paper layers may be used to form a 3, 4 or more layer tube. Other configurations may be used, such as spirally wound paper layers, cardboard tubes, paper tubes formed using a papier-mâché process, or a plurality of paper layers wound in parallel with each other to form a hollow tube. type process), molded or extruded plastic pipe, or the like.

[0039] In some embodiments, the tubular elements preferably have a wall thickness of at least about 50 μm and at most about 1 mm, preferably 50 μm to 500 μm, and more preferably 60 μm to 130 μm. In an example of the present invention, the tubular elements have a wall thickness of about 130 μm. The "wall thickness" of the tubular element corresponds to the thickness of the wall of the tubular element in the radial direction, excluding the surrounding material in which the tubular element is embedded. This can be measured, for example, using a caliper.

[0040] In some embodiments, the wall thickness of the tubular elements 4a, 4b is at least 50 microns, and preferably, at least 75, 80, 85, 90, 95, 100 or 105 microns. In some embodiments, the wall thickness of the tubular elements is at least 100 or 110 microns.

[0041] In some embodiments, the wall thickness of the tubular elements 4a, 4b is less than 1000 microns, and preferably less than 500 microns.

[0042] In some embodiments, the tubular elements 4a, 4b are each formed of a paper having a basis weight ranging from 40 gsm to 100 gsm. For example, the basis weight of the paper is 60 gsm to 80 gsm.

[0043] The combined thickness of the tubular elements 4a, 4b and the surrounding body of material 4 means that the tubular portion has a greater thermal mass, which has been found to help reduce the temperature of the aerosol passing through the tubular portion and reduce the surface temperature of the mouthpiece at a location downstream of the tubular portion. This is thought to be because the greater thermal mass of the tubular portion allows the tubular portion to absorb more heat from the aerosol than a tubular portion with a thinner wall thickness. The increased thickness of the tubular portion also allows the aerosol to be transported from the center within the mouthpiece, so that less heat is transferred from the aerosol to the outside of the mouthpiece, such as the outside of the body of material.

[0044] In some embodiments, the material of the wall of the tubular elements 4a, 4b has a permeability of at least 100 Cronaster units, and preferably, at least 200, 500 or 1000 Cronaster units.

[0045] It has been found that the relatively high permeability of the tubular elements 4a, 4b increases the amount of heat transferred from the aerosol to the tubular portion, and thus reduces the temperature of the aerosol. It has also been found that the permeability of the tubular elements 4a, 4b increases the amount of moisture transferred from the aerosol to the tubular portion, which has been found to improve the feel of the aerosol in the user's mouth. The high permeability of the tubular elements 4a, 4b also means that ventilation into the portion of the material body 4 surrounding the tubular portion can pass through the walls of the tubular elements 4a, 4b and into the aerosol stream without the need to cut through all the external plug wrapping paper and tipping paper, the material of the body 4 and the vents of the tubular elements forming the tubular portion, thereby reducing the complexity of production.

[0046] In some examples, the sheet 14 may be provided with cutout portions (e.g., punched areas) to reduce the density of the body of material 4. In some examples, the cutout portions may be provided in the portion of the sheet forming the portion of the body of material 4 surrounding the hollow tubular elements 4a, 4b. Advantageously, by providing the cutout portions in the sheet 14 forming the portion of the body, the amount of material that is perforated to provide ventilation into the tubular elements 4a, 4b may be reduced.

[0047] In some embodiments, the permeability of the material of the wall of hollow tubular element 8 is provided by the perforations formed in the material. In some instances, the material is non-porous paper, and permeability is provided by the perforations formed in the material. In other instances, the material is porous paper, which may or may not include perforations. In the case where perforations are provided, they may, for example, be set to one or more perforation lines extending through the wall of hollow tubular element. Perforations may be set to perforated belts or perforated rings through the wall of hollow tubular element. In this case, perforations may be set at the position towards the upstream end of hollow tubular element, for example, from about 8mm to about 2mm of the upstream end of hollow tubular element, or about 5mm to about 2mm.

[0048] The material body 4 may be produced using a CU-20 filter production machine produced by Decouflé (TM). However, a person skilled in the art will appreciate that other machines may be used to produce the first material body 4.

[0049] In some embodiments, the width of sheet 14 is at least 60 mm, and preferably, at least 70, 80, 90, 100, 110 or 120 mm.

[0050] In some embodiments, the width of the sheet 14 is at most 240 mm, and preferably, at most 230, 220, 210, 200, 190, 180, 170, 160 or 150 mm.

[0051] In some embodiments, the width of the sheet 14 is less than 180 mm, and preferably less than 170, 160, 150, 140 or 130 mm.

[0052] In some embodiments, the width of the sheet 14 is in the range of 60 to 240 mm, and preferably in the range of 80 to 240 mm, in the range of 90 to 200 mm, or in the range of 100 to 170 mm.

[0053] In an example of the present invention, sheet 14 includes cellulose. In an example of the present invention, sheet 14 is paper. However, sheet 14 may include different materials in addition or as an alternative. For example, in some embodiments, sheet 14 includes reconstituted tobacco (reconstituted tobacco) forming a sheet 14 arranged to form a material body 4. The reconstituted tobacco includes cellulose. The reconstituted tobacco may optionally be paper reconstituted tobacco. In other embodiments, sheet 14 includes different materials, such as cotton; tobacco, lyocell fiber; polyvinyl alcohol (PVOH), polylactic acid (PLA), poly (ε-caprolactone) (PCL), poly (1-4 butylene glycol succinate) (PBS), poly (butylene adipate-co-butylene terephthalate) (PBAT), starch-based materials, aliphatic polyester materials, polysaccharide polymers and / or fabrics or nonwoven materials. Sheet 14 may be biodegradable. In one embodiment, sheet 14 may be a non-plastic material or may be plastic. In some embodiments, sheet 14 does not include cellulose acetate.

[0054] In one embodiment, the sheet 14 comprises paper having a basis weight in the range of 15 to 80 gsm, and preferably in the range of 20 to 50 gsm.

[0055] In some embodiments, the basis weight of sheet 14 is at least 15 gsm, and preferably at least 20 gsm, 25 gsm, 30 gsm, 35 gsm, 40 gsm, 45 gsm, 50 gsm, 55 gsm, or 60 gsm.

[0056] In some embodiments, the basis weight of sheet 14 is 100 gsm or less, and preferably, 90 gsm or less, 80 gsm or less, 70 gsm or less, 60 gsm or less, 50 gsm or less, or 40 gsm or less or 30 gsm or less. In some embodiments, the basis weight of sheet 14 is 20 gsm or less.

[0057] In some embodiments, the basis weight of sheet 14 is in the range of 20 to 100 gsm, and preferably in the range of 25 to 80 gsm or in the range of 30 to 65 gsm.

[0058] In an example of the present invention, the sheet 14 is wrinkled before being arranged in the material body 4. For example, the sheet 14 can pass through a pair of crimping rollers. In an example of the present invention, the first material body 4 includes a wrinkled sheet 14 formed with a wrinkle pattern, and the wrinkle pattern includes a series of substantially parallel ridges and grooves. The wrinkles can make the sheet 14 easier to gather to form the material body 4. The wrinkles can also increase the length of the sheet 14 that can be used to form a material body 4 with a specific volume. Increasing the amount of sheet 14 in the material body 4 can increase the surface area of ​​the sheet in contact with the aerosol passing through the material body 4, and thus increase the amount of moisture absorbed by the sheet 14 from the aerosol.

[0059] Biodegradability can be measured according to the procedure specified in ISO 14855.

[0060] As described herein, the tubular elements 4a, 4b, 4a', 4b', 4a", 4b" and the first and second material bodies 4, 4', 4", 6 can achieve greater than 50% biodegradation within 30 days when exposed to fresh or sea water.

[0061] It may be desirable to form different portions of the material body 4 from different amounts of sheet material, which may be achieved by applying different degrees of pleating to the sheet material 14 forming the portion. For example, it may be desirable to form the longitudinal ends of the body 4 from longer sheets, so that the sheets are more densely arranged, and when viewed from the longitudinal ends, the longitudinal ends of the body 4 appear more similar to conventional filter elements to the consumer, and additionally or alternatively, have a higher firmness. Therefore, it may be advantageous to apply a higher amount of pleating to the sheet material 14 forming the longitudinal end portions of the body relative to the longitudinal center portion of the body. Similarly, it may be advantageous to form a portion of the body 4 from a shorter length of sheet material, where it is desired that the sheet material has a less dense packing arrangement. For example, in the case where an object is embedded in the body 4, it may be desirable to apply fewer pleats to the sheet material 14 forming the longitudinal portion of the body into which the object is embedded, so as to have a lower density of sheet material 14 around the embedded object. This arrangement may advantageously prevent the longitudinal portion of the body from having an undesirable high pressure drop.

[0062] The level of wrinkles applied to the sheet can contribute to the hardness of the body formed by the sheet. Advantageously, the hardness of the body of material can be varied along its length by varying the crimp factor of the sheet 14 applied to form the body of material. For example, a portion of the body of material formed by a sheet having a higher level of wrinkles may have a hardness of approximately 88% to 92%. A portion of the body of material having a hardness of 88% to 92% may be appropriately formed at the distal end of the body to improve the appearance of the body when viewed from that end and to provide improved stability of the longitudinal end portion of the component. Similarly, other portions of the body may be formed by sheets having a lower level of wrinkles and having a hardness of at least 80%.

[0063] In an example of the present invention, the average spacing between adjacent ridges of the sheet 14 is greater than about 0.3 mm. Additionally, in an example of the present invention, the amplitude of the folds is less than about 0.7 mm.

[0064] The wrinkle amplitude (also called "wrinkle factor") refers to the depth of the grooves formed by the wrinkles in the sheet 14 forming the body. Figure 1B As shown, when viewed from a first side of the sheet 14, the corrugated sheet 14 produces a plurality of peaks and valleys in the sheet 14, wherein the corrugation amplitude "A" is the depth of the valley measured from the peak. The corrugations may be formed in a "zigzag" form or another shape. In some instances, adjacent grooves of the corrugated sheet 14 are spaced a distance apart, or have a pitch "P" in the range of 0.3 to 2 mm, and preferably, in the range of 0.4 to 1 mm. In some embodiments, adjacent grooves of the corrugated sheet are spaced a distance apart in the range of 0.1 to 3 mm, and preferably, in the range of 0.2 to 2 mm. In some embodiments, adjacent grooves of the corrugated sheet 10 are spaced a distance apart of at least 0.1 mm, and preferably, at least 0.2, 0.5, 0.7, 1, 1.5, 2, 2.5 or 3 mm. In some embodiments, adjacent grooves of the corrugated sheet are spaced apart by a distance of at most 3 mm, and preferably, by a distance of at most 2.5, 2, 1, 1.5, 0.7, 0.5, 0.2, or 0.1 mm. For example, the sheet 14 can have corrugations having a corrugation amplitude of less than 500 μm and a spacing between peaks (or valleys) of at least 300 μm, at least 400 μm, or at least 500 μm.

[0065] In some embodiments, the sheet 14 is heated as it is crimped. For example, the sheet 14 may be passed between crimping rollers, one or both of which are heated. For example, one or both of the rollers may be heated to a temperature of up to 100 degrees Celsius, such as a temperature of 50 degrees Celsius or 60 degrees Celsius. The amount of pressure applied to the sheet passing between the rollers may also vary. Heating the rollers or applying a higher level of pressure to the sheet may result in a higher level of crimping.

[0066] Advantageously, it has been found that sheets 14 (e.g., paper) having the above-described pleat pitches and / or amplitudes exhibit improved performance when used as components of an aerosol delivery system. Specifically, these relatively low levels of pleat pitches and amplitudes unexpectedly result in a body of material or a portion of a body of material having a lower pressure drop than a body or a portion of a body formed from a sheet 14 having a higher level of pleats.

[0067] In any of these examples, the average density of the body of material may be from about 0.1 to about 0.25 mg / mm 3 The density of the body of material can be measured by separating the body from the article and surrounding plug wrap and / or tipping paper and removing any embedded objects, but including any additives added to the sheet 14. The density can be calculated as a bulk density based on the weight of the sheet 14 and any additives added to the sheet 14 and the total volume occupied by the sheet 14. For example, the total volume of the body of material 4 measured within the plug wrap 7.

[0068] In the example of the present invention, the density of the material body 4 is about 0.19 mg / mm 3 In some embodiments, body 4 has a density of at least 0.1 mg / mm 3 , 0.12mg / mm 3 or 0.15mg / mm 3 Alternatively or in addition, the material body 4 may have a density of less than about 0.3 mg / mm 3 , less than about 0.25mg / mm 3 or less than about 0.22 mg / mm 3 Advantageously, the density of the material body may be about 0.15 mg / mm 3 To about 0.25mg / mm 3 As described above, different portions of the body of material 4 may have different densities based on the level of wrinkling and gathering applied to the sheet 14 that forms the portion. These values ​​include any additives included in the body of material 4. Prior to wrinkling and forming the body of material, the density of the sheet 14 may be about 0.2 to 0.5 mg / mm 3 , for example, about 0.25, 0.30 or 0.35 mg / mm 3 .

[0069] The dimensions given for sheet 14 refer to the dimensions of the sheet before it is wrinkled or gathered to form a body of material. The dimensions of sheet 14 can be measured by stretching sheet 14 to the point where no visible wrinkles remain therein.

[0070] In the example of the invention, a lower level of corrugation is applied to the sheet 14 forming the portion of the body 4 of material in which the tubular elements 4a, 4b are embedded, whereas a higher level of corrugation is applied to the sheet 14 forming the distal end of the body 4.

[0071] In some embodiments, the sheet 14 is crumpled to a corrugation amplitude of at least 0.1 mm, and preferably, at least 0.3 mm, 0.4 mm, or 0.5 mm.

[0072] In some embodiments, the sheet 14 is crumpled to a corrugation amplitude of at most 1 mm, and preferably, a corrugation amplitude of at most 0.8 mm, 0.6 mm, or 0.5 mm.

[0073] In some embodiments, the sheet 14 includes at least one slit extending in a direction substantially perpendicular to the longitudinal axis of the body 4. The at least one slit is positioned so that when the sheet 14 is assembled into the body 4, the slit allows the sheet 14 located on a first side (e.g., downstream side) of an object (e.g., the second tubular element 4b) embedded in the body to be gathered together so that the slit forms an inner edge in the body 4 that at least partially defines a boundary of a space containing the embedded object.

[0074] The inner edge formed by the slit allows the sheet 14 to be gathered together on one side of the embedded object to at least partially or completely define a boundary to prevent the object from moving out of the first end of the space in which it is embedded. This improves the positioning of the embedded object within the body 4. In addition, because the sheet 14 is gathered together, it helps to conceal the embedded object when viewed from the longitudinal end of the body 4, which can improve the aesthetics of the mouthpiece 2. Advantageously, the slit achieves these benefits without requiring a separate component, such as a cellulose acetate plug, to be provided downstream of the embedded object or downstream of the body 4.

[0075] The article 1 has a ventilation level of about 75% of the aerosol inhaled through the article. In alternative embodiments, the article may have a ventilation level of 20% to 80%, for example, 65% to 75%, of the aerosol inhaled through the article. Ventilation at these levels helps to slow the flow of the aerosol inhaled through the mouthpiece 2, thereby allowing the aerosol to be fully cooled before reaching the downstream end 2b of the mouthpiece 2. Ventilation is provided directly into the mouthpiece 2 of the article 1. In examples of the present invention, ventilation is provided into the tubular portion, which has been found to be particularly beneficial in assisting the aerosol generation process. Ventilation is provided by a first row and a second row of parallel ventilation holes 12, which in the case of the present invention are formed as laser perforations, respectively located 17.925 mm and 18.625 mm downstream of the mouth end 2b of the mouthpiece 2. In examples of the present invention, these ventilation holes 12 pass through the tipping paper 5, the filter plug wrapping paper 7 and the second tubular element 4b. In alternative embodiments, ventilation may be provided into the mouthpiece at other locations.

[0076] Alternatively, ventilation may be provided to the portion of the article where the tubular portion is located by a single row of ventilation holes (e.g., laser perforated). This has been found to result in improved aerosol formation, which is believed to be due to the airflow through the ventilation holes being more uniform than through multiple rows of ventilation holes for a given ventilation level.

[0077] It has been found that aerosol temperature generally increases with decreasing ventilation levels. However, the relationship between aerosol temperature and ventilation level does not appear to be linear, for example, changes in ventilation due to production tolerances have a smaller effect at lower target ventilation levels. For example, with a ventilation tolerance of ±15%, for a target ventilation level of 75%, the aerosol temperature may increase by about 6°C at the lower limit of ventilation (60% ventilation). However, with a target ventilation level of 60%, the aerosol temperature may only increase by about 3.5°C at the lower limit of ventilation (45% ventilation). Therefore, the target ventilation level for the article may be in the range of 40% to 70%, for example, in the range of 45% to 65%. The average ventilation level of at least 20 articles may be 40% to 70%, for example, 45% to 70% or 51% to 59%.

[0078] In some examples, the aerosol-generating material 3 described herein is a first aerosol-generating material, and the first tubular element 4a and / or the second tubular element 4b may include a second aerosol-generating material. In one example, the inner wall of the tubular element 4a includes the second aerosol-generating material. For example, the second aerosol-generating material may be arranged on the inner surface of the tubular element 4a.

[0079] The second aerosol generating material comprises at least one aerosol former material, and may further comprise at least one aerosol modifier or other sensing material.The aerosol former material and / or aerosol modifier may be any aerosol former material or aerosol modifier as described herein, or a combination thereof.

[0080] When the aerosol generated from the aerosol generating material 3 (referred to herein as the first aerosol) is inhaled through the first tubular element 4a of the mouthpiece, the heat from the first aerosol can aerosolize the aerosol-forming material of the second aerosol generating material to form a second aerosol. The second aerosol may include a flavorant that can add or supplement the flavor of the first aerosol.

[0081] Providing a second aerosol generating material on the first tubular element 4a or the second tubular element 4b may result in the generation of a second aerosol that enhances or complements the flavour or visual appearance of the first aerosol.

[0082] In other embodiments, the first and second tubular elements 4a, 4b may be embedded in a rod of aerosol-generating material. In these embodiments, the tubular elements may be formed from paper as described above, or from a reconstituted tobacco sheet.

[0083] In an example of the present invention, the article 1 has an outer circumference of about 21 mm (i.e., the article is in a semi-slender form). Preferably, the article 1 has an aerosol-generating material rod having a circumference greater than 19 mm. It has been found that this provides a circumference sufficient to produce an improved and lasting aerosol than the conventional aerosol generation process preferred by consumers. When the article is heated, heat is transferred through the aerosol-generating material rod 3 to volatilize the components of the rod, and it has been found that a circumference greater than 19 mm is particularly effective for generating aerosols in this manner. Since the article is heated to release the aerosol, improved heating efficiency can be achieved using an article having a circumference less than about 23 mm. In order to achieve an improved aerosol by heating while maintaining an appropriate product length, a rod circumference greater than 19 mm and less than 23 mm is preferred. In some instances, the circumference of the rod can be 20 mm to 22 mm, which has been found to provide a good balance between providing effective aerosol delivery and allowing effective heating.

[0084] The outer circumference of the mouthpiece 2 is substantially the same as the outer circumference of the aerosol generating material rod 3 so that there is a smooth transition between these components. In the example of the present invention, the outer circumference of the mouthpiece 2 is approximately 20.8mm.

[0085] In some examples, the tipping paper 5 includes a citrate, such as sodium citrate or potassium citrate. In these examples, the tipping paper 5 may have a citrate content of 2% by weight or less, or 1% by weight or less. Reducing the citrate content of the tipping paper 5 is believed to help reduce the charring effect that may occur during use.

[0086] In the examples of the present invention, the tipping paper 5 extends 5 mm over the aerosol generating material rod 3, but alternatively it may extend 3 to 10 mm, or more preferably 4 to 6 mm, over the rod 3 to provide a secure connection between the mouthpiece 2 and the rod 3. The basis weight of the tipping paper 5 may be higher than the basis weight of the plug wrap paper used in the article 1, for example, a basis weight of 40 to 80 gsm, more preferably a basis weight of 50 to 70 gsm, and in the examples of the present invention, a basis weight of 58 gsm. These basis weight ranges have been found to result in a tipping paper having an acceptable tensile strength while being sufficiently flexible to be wrapped around the article 1 and adhered to itself along the longitudinal lap seam on the paper. Once wrapped around the mouthpiece 2, the outer circumference of the tipping paper 5 is about 21 mm.

[0087] In some embodiments, the first plug wrap 7 has a basis weight of less than 50 gsm, more preferably a basis weight of about 20 gsm to 40 gsm. However, it should be appreciated that the basis weight of the first plug wrap 7 may be higher to increase the stiffness of the mouthpiece. For example, the basis weight of the first plug wrap 7 may be at least 50, 60, 70, 80, 90 or 100 gsm. In some embodiments, the basis weight of the first plug wrap 7 is in the range of 50 to 110 gsm, or in the range of 60 to 100 gsm.

[0088] In some embodiments, the first plug wrap 7 has a basis weight of at least 20 gsm or at least 30 gsm.

[0089] In some embodiments, the first plug wrap 7 has a basis weight of at most 120, 110 or 100 gsm.

[0090] In some embodiments, the basis weight of the first plug wrap 7 is in the range of 20 to 120 gsm, and preferably in the range of 30 to 100 gsm.

[0091] Preferably, the thickness of the first plug wrap 7 is 30 μm to 60 μm, more preferably 35 μm to 45 μm. However, it will be appreciated that the thickness weight of the first plug wrap 7 may be higher to increase the stiffness of the mouthpiece. In some embodiments, for example, the thickness of the first plug wrap 7 may be at least 40, 50, 60, 70, 80, 90 or 100 microns. In some embodiments, the thickness of the first plug wrap 7 is in the range of 40 to 120 microns, or in the range of 50 to 100 microns.

[0092] Preferably, the first plug wrap 7 is a non-porous plug wrap, e.g. having a permeability of less than 100 Korast units, e.g. less than 50 Korast units. However, in other embodiments, the first plug wrap 7 may be a porous plug wrap, e.g. having a permeability of more than 200 Korast units.

[0093] The pressure drop or pressure differential (also referred to as the resistance to draw) across the mouthpiece (e.g., the portion of the article 1 downstream of the aerosol generating material 3) is preferably less than about 40 mmH2O. It has been found that such a pressure drop allows sufficient aerosol (including desired compounds, such as flavor compounds) to reach the consumer through the mouthpiece 2. More preferably, the pressure drop across the mouthpiece 2 is less than about 20 mmH2O. In some embodiments, particularly improved aerosols have been achieved using a mouthpiece 2 having a pressure drop of less than 15 mmH2O, such as about 6 mmH2O, about 10 mmH2O, or about 14 mmH2O. Alternatively or in addition, the mouthpiece pressure drop may be at least 3 mmH2O, preferably at least 4 mmH2O, and more preferably at least 5 mmH2O. In some embodiments, the mouthpiece pressure drop may be from about 5 mmH2O to 20 mmH2O, and preferably from 5 mmH2O to 15 mmH2O. These values ​​enable the mouthpiece 2 to slow the aerosol as it passes through the mouthpiece 2 , thereby allowing the temperature of the aerosol time to decrease before reaching the downstream end 2 b of the mouthpiece 2 .

[0094] In an example of the present invention, the aerosol generating material 3 is wrapped in a wrapper 10. The wrapper 10 can be, for example, a paper or paper-backed foil wrapper. In an example of the present invention, the wrapper 10 is substantially airtight. In an alternative embodiment, the wrapper 10 preferably has a permeability of less than 100 korast units, more preferably less than 60 korast units. It has been found that low permeability wrappers (e.g., wrappers with a permeability of less than 100 korast units, more preferably less than 60 korast units) cause an improvement in aerosol formation in the aerosol generating material 3. Without wishing to be bound by theory, it is believed that this is due to a reduction in the loss of aerosol compounds through the wrapper 10. The permeability of the wrapper 10 can be measured according to ISO 2965:2009 (on the determination of the air permeability of materials used as cigarette paper, filter plug wrapping paper and filter tip connecting paper).

[0095] In an embodiment of the present invention, the wrapper 10 includes an aluminum foil. It has been found that the aluminum foil is particularly effective in enhancing the formation of aerosols in the aerosol-generating material 3. In an example of the present invention, the aluminum foil has a metal layer with a thickness of about 6 μm. In an example of the present invention, the aluminum foil has a paper backing. However, in an alternative arrangement, the aluminum foil can be other thicknesses, for example, a thickness of 4 μm to 16 μm. The aluminum foil does not need to have a paper backing either, but can have a backing formed by other materials, for example, to help provide the foil with appropriate tensile strength, or it can have no backing material. Metal layers or foils other than aluminum can also be used. The total thickness of the wrapper is preferably 20 μm to 60 μm, more preferably 30 μm to 50 μm, which can provide a wrapper with appropriate structural integrity and heat transfer properties. The tension that can be applied to the wrapper before the wrapper breaks can be greater than 3000 grams of force, for example, 3000 to 10000 grams of force or 3000 to 4500 grams of force.

[0096] In some examples, the wrapper 10 surrounding the aerosol generating material 3 has a high level of permeability, for example, a permeability greater than about 1000 korast units, or greater than about 1500 korast units, or greater than about 2000 korast units. The permeability of the wrapper 10 can be measured according to ISO 2965:2009 (Determination of the air permeability of materials used as cigarette papers, filter plug wrappers and filter tie papers).

[0097] The wrapper 10 may be formed from a material having a high inherent permeability level, an inherently porous material, or may be formed from a material having any inherent permeability level, wherein the final permeability level is achieved by providing the wrapper 10 with permeable strips or permeable zones. Providing a permeable wrapper 10 provides a path for air to enter the article. The wrapper 10 may be provided with a certain permeability so that the amount of air entering through the aerosol generating material rod is relatively greater than the amount of air entering the article through the ventilation holes 12 in the mouthpiece. An article having such an arrangement may produce a more flavorful aerosol, which may be more satisfying to the user.

[0098] In an example of the present invention, the aerosol-forming material added to the aerosol-generating substrate 3 accounts for 14% by weight of the aerosol-generating substrate 3. Preferably, the aerosol-forming material accounts for at least 5% by weight of the aerosol-generating substrate, more preferably at least 10%. Preferably, the aerosol-forming material accounts for less than 25% by weight of the aerosol-generating substrate, more preferably less than 20%, for example, 10% to 20%, 12% to 18%, or 13% to 16%.

[0099] Preferably, the aerosol-generating material 3 is provided as a cylindrical aerosol-generating material rod. Regardless of the form of the aerosol-generating material, it preferably has a length of about 10 mm to 100 mm. In some embodiments, the length of the aerosol-generating material is preferably in the range of about 25 mm to 50 mm, more preferably in the range of about 30 mm to 45 mm, and even more preferably in the range of about 30 mm to 40 mm.

[0100] In some examples, the article 1 may be configured so that there is a spacing (ie, a minimum distance) between the heater and the first tubular element 4a of the non-flammable aerosol providing device 100. This prevents heat from the heater from damaging the material forming the first tubular element 4a.

[0101] The minimum distance between the heater of the non-flammable aerosol providing device 100 and the first tubular element 4a can be 3 mm or more. In some examples, the minimum distance between the heater of the non-flammable aerosol providing device 100 and the first tubular element 4a can be in the range of 3 mm to 10 mm, for example, 3 mm, 4 mm, 5 mm, 6 mm, 7 mm, 8 mm, 9 mm or 10 mm.

[0102] The spacing between the heater and the first tubular element 4a of the non-flammable aerosol providing device 100 can be achieved by, for example, adjusting the length of the rod of the aerosol generating material 3.

[0103] The volume of the aerosol generating material 3 provided may be from about 200 mm 3 Changed to about 4300mm 3 , preferably from about 500 mm 3 Change to 1500mm 3 , more preferably from about 1000 mm 3 Changed to about 1300mm 3 The volume of the aerosol generating material is provided, for example, about 1000 mm 3 To about 1300mm 3 , have advantageously been shown to achieve superior aerosols having greater visibility and sensory properties than aerosols achieved with volumes selected from the lower end of the range.

[0104] The mass of the provided aerosol generating material 3 may be greater than 200 mg, for example, about 200 mg to 400 mg, preferably about 230 mg to 360 mg, more preferably about 250 mg to 360 mg. It has been advantageously found that providing a higher mass of aerosol generating material results in improved sensory performance compared to an aerosol generated by a lower mass of tobacco material.

[0105] Preferably, the aerosol-generating material or substrate is formed from a tobacco material as described herein, including a tobacco component.

[0106] In the tobacco materials described herein, the tobacco component preferably contains paper reconstituted tobacco. The tobacco component may also contain leaf tobacco, extruded tobacco and / or ribbon cast tobacco.

[0107] Aerosol generating material 3 can comprise the reconstituted tobacco material of density being less than about 700 milligrams / cubic centimeters (mg / cc).It has been found that compared with more dense material, this tobacco material is particularly effective in providing the aerosol generating material that can be heated quickly to release aerosol.For example, the inventor has tested multiple aerosol generating materials, such as the property of belt-type flow casting reconstituted tobacco material and paper reconstituted tobacco material when heating.It has been found that for each given aerosol generating material, there is a specific zero heat flow temperature, below this temperature, net heat flow is heat absorption, in other words, the heat of entering material is more than the heat of leaving material, and above this temperature, net heat flow is exothermic, in other words, when heat is applied to material, the heat of leaving material is more than the heat of entering material.The material with density less than 700mg / cc has lower zero heat flow temperature.Because most of the heat flow of outflowing material is carried out by the formation of aerosol, therefore having lower zero heat flow temperature has a beneficial effect on the required time of first release aerosol from aerosol generating material. For example, aerosol generating materials having a density less than 700 mg / cc were found to have a zero heat flow temperature less than 164°C, compared to materials having a density greater than 700 mg / cc having a zero heat flow temperature greater than 164°C.

[0108] The density of the aerosol generating material also has an effect on the rate at which heat is conducted through the material, with lower densities (eg, densities below 700 mg / cc) causing heat to be conducted more slowly through the material and therefore enabling a more sustained release of the aerosol.

[0109] Preferably, the aerosol-generating material 3 comprises a reconstituted tobacco material, such as a paper reconstituted tobacco material, having a density of less than about 700 mg / cc. More preferably, the aerosol-generating material 3 comprises a reconstituted tobacco material having a density of less than about 600 mg / cc. Alternatively or in addition, the aerosol-generating material 3 preferably comprises a reconstituted tobacco material having a density of at least 350 mg / cc, which is believed to allow a sufficient amount of heat conduction through the material.

[0110] Tobacco material can provide with cut rag tobacco (cut rag tobacco) form. Cut rag tobacco can have the cutting width of at least 15 cuts per inch (about 5.9 cuts per cm, equivalent to the cutting width of about 1.7mm). Preferably, the cutting width of cut rag tobacco is at least 18 cuts per inch (about 7.1 cuts per cm, equivalent to the cutting width of about 1.4mm), more preferably at least 20 cuts per inch (about 7.9 cuts per cm, equivalent to the cutting width of about 1.27mm). In an example, cut rag tobacco has the cutting width of 22 cuts per inch (about 8.7 cuts per cm, equivalent to the cutting width of about 1.15mm). Preferably, the cutting width of cut rag tobacco is 40 per inch or less (about 15.7 cuts per cm, equivalent to the cutting width of about 0.64mm). It has been found that a cut width of 0.5 mm to 2.0 mm, such as 0.6 mm to 1.5 mm, or 0.6 mm to 1.7 mm, results in a tobacco material that is preferred in terms of surface area to volume ratio, particularly when heated, and in terms of overall density and pressure drop of the substrate 3. Cut tobacco may be formed from a mixture of a variety of tobacco material forms, such as a mixture of one or more of paper reconstituted tobacco, tobacco leaf, extruded tobacco, and ribbon cast tobacco. Preferably, the tobacco material comprises paper reconstituted tobacco or a mixture of paper reconstituted tobacco and tobacco leaf.

[0111] In tobacco material described herein, tobacco material can contain filler component. Filler component is non-tobacco component normally, does not include the component of the composition that derives from tobacco. Filler component can be non-tobacco fiber, such as wood fiber or pulp or wheat fiber. Filler component can also be inorganic material, such as chalk, perlite, vermiculite, diatomaceous earth, colloidal silica, magnesium oxide, magnesium sulfate, magnesium carbonate. Filler component can also be non-tobacco casting material or non-tobacco extrusion material. Filler component can exist with the amount of 0 to 20% by tobacco material weight, or exist with the amount of 1 to 10% by composition weight. In some embodiments, filler component does not exist.

[0112] In tobacco material described herein, tobacco material contains aerosol forming agent material.In this background, " aerosol forming agent material " is a kind of reagent that promotes aerosol generation.Aerosol forming agent material can promote aerosol generation by promoting gas initial vaporization and / or condensation as inhalable solid and / or liquid aerosol.In some embodiments, aerosol forming agent material can improve the sending of flavoring agent from aerosol generating material.Usually, any suitable aerosol forming agent material or reagent can be included in aerosol generating material of the present invention, including those described herein. Other suitable aerosol forming agent materials include, but are not limited to: polyols, such as sorbitol, glycerol and glycols (such as propylene glycol or triethylene glycol); non-polyols, such as monohydric alcohols; high boiling hydrocarbons; acids, such as lactic acid; glycerol derivatives; esters, such as diacetin, triacetin, triethylene glycol diacetate, triethyl citrate or myristate (including ethyl myristate and isopropyl myristate); and aliphatic carboxylic acid esters, such as methyl stearate, dimethyl dodecanedioate and dimethyl tetradecanedioate. In some embodiments, the aerosol forming agent material can be a mixture of glycerol, propylene glycol or glycerol and propylene glycol. Glycerol can be present in an amount of 10 to 20% by weight of tobacco material, for example, 13 to 16% by weight of composition, or about 14% or 15% by weight of composition. If present, propylene glycol can be present in an amount of 0.1 to 0.3% by weight of composition.

[0113] The aerosol forming agent material can be included in any component of the tobacco material, for example in any tobacco component, and / or if present, can be included in the filler component. Alternatively or in addition, the aerosol forming agent material can be added to the tobacco material separately. In either case, the total amount of the aerosol forming agent material in the tobacco material can be as defined herein.

[0114] The tobacco material may contain from 10% to 90% tobacco leaf by weight, wherein the aerosol former material is provided in an amount of up to about 10% by weight of the tobacco leaf. In order to achieve an overall level of aerosol former material of from 10% to 20% by weight of the tobacco material, it has been advantageously found that this may be added to another component of the tobacco material, such as reconstituted tobacco material, at a higher weight percentage.

[0115] Tobacco material described herein contains nicotine.Nicotine content is 0.5 to 1.75% by tobacco material weight, and for example, can be 0.8 to 1.5% by tobacco material weight.In addition or alternatively, tobacco material contains 10% to 90% tobacco leaf by weight, and its nicotine content is greater than 1.5% by tobacco leaf weight.Advantageously found to use nicotine content higher than 1.5% tobacco leaf and lower nicotine base material such as paper reconstructed tobacco combination to provide with suitable nicotine level, but than using paper reconstructed tobacco alone, there is the tobacco material of better organoleptic properties.The nicotine content of tobacco leaf such as cut tobacco can for example be 1.5% to 5% by tobacco leaf weight.

[0116] Tobacco material described herein can contain aerosol modifier, such as any flavoring agent described herein. In one embodiment, tobacco material contains menthol, thereby forms the product containing menthol. Tobacco material can contain 3mg to 20mg menthol, preferably 5mg to 18mg, and more preferably 8mg to 16mg menthol. In an example of the present invention, tobacco material contains 16mg menthol. Tobacco material can contain 2% to 8% menthol by weight, preferably 3% to 7% menthol by weight, and more preferably 4% to 5.5% menthol by weight. In one embodiment, tobacco material includes 4.7% menthol by weight. Using high percentage of reconstituted tobacco material, for example, greater than 50% of tobacco material by weight, this high level of menthol loading can be achieved. Alternatively or in addition, using high volume of aerosol generation material (such as tobacco material) can improve achievable menthol loading level, for example, when using greater than about 500mm 3 or suitably greater than about 1000 mm 3 In the case of aerosol generating materials (such as tobacco materials).

[0117] In compositions described herein, when equivalents are given with % by weight, in order to avoid doubt, this refers to dry basis weight, unless specifically indicated to the contrary. Therefore, in order to determine % by weight, any moisture that may exist in tobacco material or any component thereof is not considered at all. The water content of tobacco material described herein can change, for example, can be 5 to 15% by weight. The water content of tobacco material described herein can be changed according to the temperature, pressure and humidity conditions of, for example, maintaining the composition. As known to those skilled in the art, water content can be determined by Karl-Fisher analysis. On the other hand, in order to avoid doubt, even if aerosol forming agent material is a component in liquid phase (such as glycerine or propylene glycol), any component except water is included in the weight of tobacco material. However, when providing aerosol forming agent material in the tobacco component of tobacco material, or providing aerosol forming agent material in the filler component (if present) of tobacco material, substitute or except being added to tobacco material separately, described aerosol forming agent material is not included in the weight of tobacco component or filler component, but is included in the weight of " aerosol forming agent material " with % by weight as defined herein. All other ingredients present in the tobacco component are included in the weight of the tobacco component, even those of non-tobacco origin (eg, non-tobacco fibers in the case of paper reconstituted tobacco).

[0118] In one embodiment, tobacco material comprises tobacco component as defined herein and aerosol forming agent material as defined herein. In one embodiment, tobacco material is substantially composed of tobacco component as defined herein and aerosol forming agent material as defined herein. In one embodiment, tobacco material is composed of tobacco component as defined herein and aerosol forming agent material as defined herein.

[0119] Paper reconstructed tobacco is present in the tobacco component of tobacco material described herein with the amount of 10% to 100% by tobacco component weight. In an embodiment, paper reconstructed tobacco is present in the amount of 10% to 80% by tobacco component weight, or 20% to 70% by weight. In other embodiments, tobacco component is basically composed of paper reconstructed tobacco or is composed of paper reconstructed tobacco. In a preferred embodiment, tobacco leaf is present in the tobacco component of tobacco material with the amount of at least 10% by tobacco component weight. For example, tobacco leaf can exist with the amount of at least 10% by tobacco component weight, and the remainder of tobacco component comprises the combination of paper reconstructed tobacco, belt-cast reconstructed tobacco or belt-cast reconstructed tobacco and another form of tobacco (such as tobacco particles).

[0120] Paper reconstituted tobacco refers to tobacco material formed by the following process, wherein the tobacco raw material is extracted with a solvent to provide an extract of solubles and a residue containing fibrous material, and then the extract (usually after concentration and optionally after further processing) is recombined with fibrous material from the residue (usually after the fibrous material is refined and a portion of non-tobacco fibers are optionally added) by deposition of the extract on the fibrous material. The process of recombining is similar to the papermaking process.

[0121] The paper reconstituted tobacco can be any type of paper reconstituted tobacco known in the art. In one embodiment, the paper reconstituted tobacco is made from a raw material comprising one or more of tobacco rods, tobacco stems, and whole tobacco leaves. In other embodiments, the paper reconstituted tobacco is made from a raw material consisting of tobacco rods and / or whole tobacco leaves and tobacco stems. However, in other embodiments, alternatively or in addition, fragments, fines, and winnowing materials can be used in the raw material.

[0122] Paper reconstituted tobacco for use in the tobacco materials described herein can be prepared by methods known to those skilled in the art for preparing paper reconstituted tobacco.

[0123] Figure 2 is a side cross-sectional view of another article 1' comprising a mouthpiece 2' comprising a body of material 4'. The mouthpiece 2' is substantially the same as the mouthpiece 2 described above, except that a first tubular element 4a' is disposed at the upstream end of the body of material 4' and is separated from a second tubular element 4b' by a gap filled with material forming said body 4', and the second tubular element 4b' is disposed at the downstream end of said body 4'.

[0124] In an example of the present invention, the first tubular element 4a' and the second tubular element 4b' are separated by a gap of 10mm. Alternatively, the first tubular element 4a' and the second tubular element 4b' are separated by a gap of other distances, for example, 5mm to 15mm, or 6mm to 12mm, or about 6mm, about 7mm, about 8mm or about 9mm. The material body 4' extends into the gap. In an example of the present invention, the material forming the material body 4' extends across the entire width of the material body 4' in the gap between the first tubular element 4a' and the second tubular element 4b'. In an example of the present invention, the sheet 14 forming the body 4' comprises two slits, which are respectively positioned at the downstream end and the upstream end of the first tubular element 4a' and the second tubular element 4b'. The slits are positioned so that when the sheets 14 are assembled into the body 4', they release the sheets 14 therebetween to extend into the gap between the first and second tubular elements 4a', 4b' to allow the central portion of the body 4' of material to extend completely across the gap between the two tubular elements.

[0125] In an example of the invention, the first tubular element 4a' provides a tubular portion as described above, which acts as a cavity for aerosol cooling. In an example of the invention, the first tubular element 4a' has a length of about 15 mm. Alternatively, the first tubular element 4a' may have a length as described above for the tubular portion.

[0126] The second tubular element 4b' is embedded in the material body 4' at the downstream end of the material body 4' and extends to the longitudinal end of the body 4'. It has been advantageously found that providing the tubular element at this position significantly reduces the temperature of the outer surface of the mouthpiece 2' at the downstream end 2b of the mouthpiece that contacts the consumer's mouth when the article 1' is used. In addition, it has been found that the use of the tubular portion significantly reduces the temperature of the outer surface of the mouthpiece 2' even located upstream of the tubular portion. Without wishing to be bound by theory, it is believed that this is due to the tubular portion conveying the aerosol closer to the center of the mouthpiece 2' and thus reducing the transfer of heat from the aerosol to the outer surface of the mouthpiece 2'. In addition, it has been found that the material body 4' filling the gap between the first tubular element 4a' and the second tubular element 4b' removes moisture from the aerosol generated by the aerosol generating material 3 when the aerosol passes through the material body 4' of the mouthpiece 2, which makes the aerosol feel cooler in the user's mouth.

[0127] Forming a mouthpiece comprising a body of material 4' comprising a first tubular element 4a' and a second tubular element 4b' embedded at opposite ends of the body of material 4' advantageously results in a mouthpiece having a concave mouth end and a cavity for aerosol cooling at the upstream end of the mouthpiece, the mouthpiece being surrounded by a plug wrap of less thickness than would normally be required for such a construction, since both cavities are provided by tubular elements embedded in the same body of material, thereby eliminating the need for separate plug wraps and combination wrappers for different components. In addition to simplifying the production of the mouthpiece by reducing the number of components, ventilation holes can also be more easily formed at desired locations in the body of material 4', since the plug wrap to be perforated is of less thickness.

[0128] In an example of the present invention, the wall thickness of the second tubular element 4b' is greater than the wall thickness of the first tubular element 4a', and the length of the second tubular element 4b' is less than the length of the first tubular element 4a', so that the cavity provided by the second tubular element 4b' at the mouth end 2b of the mouthpiece is smaller than the cavity formed by the tubular element 4a'. In other examples, the wall thickness of the first tubular element 4a' may be greater than the wall thickness of the second tubular element 4b'. Advantageously, different wall thicknesses, inner diameters and / or lengths are selected for the first tubular element 4a' and the second tubular element 4b', respectively, to allow the cavity provided at either end of the material body 4' to be optimized for aerosol cooling and / or aerosol transport through the mouthpiece, based on their position in the mouthpiece, as desired.

[0129] Preferably, the length of the second tubular element 4b' is less than about 20mm. More preferably, the length of the second tubular element 4b' is less than about 15mm. Still more preferably, the length of the second tubular element 4b' is less than about 10mm. In addition or as an alternative, the length of the second tubular element 4b' is at least about 5mm. Preferably, the length of the second tubular element 4b' is at least about 6mm. In some preferred embodiments, the length of the second tubular element 4b' is about 5mm to about 20mm, more preferably about 6mm to about 10mm, even more preferably about 6mm to about 8mm, most preferably about 6mm, 7mm or about 8mm. In examples of the present invention, the length of the second tubular element 4b' is 6mm.

[0130] In the example of the present invention, each of the first tubular element 4a' and the second tubular element 4b' has the same outer diameter and is surrounded by a body of material 4' of the same thickness.

[0131] As described above, different levels of wrinkles may be applied to the sheet 14 to form different portions of the body 4 of material. In the example of the present invention, a higher level of wrinkles is applied to the sheet forming the mouth end portion of the body 4' in which the second tubular element 4b' is embedded, compared to the wrinkle level of the sheet 14 forming the portion of the body 4' in which the first tubular element 4a' is embedded and the sheet 14 filling the gap between the first tubular element 4a' and the second tubular element 4b'. Advantageously, applying a higher level of wrinkles to the sheet 14 around the second tubular element 4b' can give the mouthpiece a more desirable firmness at the mouth end 2b and an improved appearance when viewed from the mouth end of the mouthpiece.

[0132] Figure 3 is a side cross-sectional view of another article 1", which includes a mouthpiece 2", which includes a material body 4". In the example of the present invention, the material body 4" does not substantially extend beyond the second tubular element 4b. In the example of the present invention, the mouthpiece 2" includes a second material body 6 located downstream of the first material body 4", and in this embodiment, the second material body 6 is adjacent to and in abutting relationship with the first material body 4". The first material body 4" and the second material body 6 respectively define an overall outer shape that is substantially cylindrical and share a common longitudinal axis. In the example of the present invention, the same level of pleats is applied to the entire sheet 14 forming the material body 4".

[0133] The second body of material 6 is formed of a sheet material, as described with respect to the first body of material 4. The second body of material 6 can be formed of the same sheet material 14 as the first body of material 4, or of a sheet material having a different composition or other properties (such as a level of wrinkles). In some examples, the second body of material 6 can have the same density as the first body of material 4.

[0134] Preferably, the length of the second material body 6 is less than about 20 mm. In the example of the present invention, the length of the second material body 6 is 16 mm.

[0135] In some embodiments, the axial length of the second material body 6 is in the range of 10 to 20 mm.

[0136] In some embodiments, an aerosol former material is applied to the second body of material 6. For example, the aerosol former material may be applied to the sheet before the sheet is folded to form the second body of material 6. The aerosol former material may be sprayed onto the sheet, or applied by brush or by dipping the sheet into the aerosol former material.

[0137] In some embodiments, the aerosol former material may include one or more of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, 1,3-butylene glycol, erythritol, meso-erythritol, ethyl vanillate, ethyl dodecanoate, diethyl suberate, triethyl citrate, glyceryl triacetate, a mixture of diacetates, benzyl benzoate, benzyl phenylacetate, tributyrin, lauryl acetate, lauric acid, myristic acid, and propylene carbonate.

[0138] In some embodiments, at least 0.02 mg of aerosol former material is applied to the second material body per 1 mm of axial length of the second material body 6. Preferably, at least 0.03, 0.04 or 0.05 mg of aerosol former material is applied to the second material body per 1 mm of axial length of the material body.

[0139] In some embodiments, 0.5 mg or less of aerosol forming material is applied to the second material body 6 per 1 mm of the axial length of the material body. Preferably, 0.4 mg or less, 0.3 mg or less, 0.2 mg or less, or 0.1 mg or less of aerosol forming material is applied to the second material body 6 per 1 mm of the axial length of the material body.

[0140] As the aerosol passes through the second body of material 6, at least some of the aerosol former material combines with the aerosol and helps make the aerosol feel less dry in the mouth of the user.

[0141] In some embodiments, the second material body 6 has a thickness of at least 115 mm. 3In the example of the present invention, the second material body 6 is generally cylindrical and thus has a generally cylindrical outer volume. It should be appreciated that in other embodiments, the second material body 6 may have an outer volume less than 115 mm. 3 of the external volume.

[0142] It has been found that when the aerosol passes through the second material body 6 of the mouthpiece 2", comprising cellulose and having a diameter of at least 115 mm 3 The bulk of the second material body 6 helps remove moisture from the aerosol generated by the aerosol generating material 3. That is, the cellulose-containing sheet forming the second material body 6 absorbs water from the aerosol. Removing moisture from the aerosol makes the aerosol feel cooler in the user's mouth.

[0143] In other examples described herein, the body of material 4, 4' extends beyond the first tubular element 4a, and a portion of the body of material 4, 4' extends across the entire width of the body 4, 4'. In these examples, an aerosol former may be applied to a portion of the body 4, 4' as described above for the second body of material 6. In these examples, the portion may provide the functionality of the body of material 6 described above without providing a separate body of material.

[0144] The second body of material is surrounded by a second plug wrap 8. The second plug wrap 8 may have any of the specifications as described for the plug wrap 7.

[0145] In some embodiments, the second material body 6 has a thickness of at least 19 mm per mm of the material body axial length. 3 volume, and preferably at least 25 mm per mm of axial length 3 Or at least 30mm per mm 3 For example, if the second material body 6 has an axial length of 19 mm per mm 3 volume and 10mm in length, the volume of the material body will be 190mm 3 .

[0146] A larger volume of the second body of material 6 will generally be more effective in removing moisture from the aerosol. In some examples, the outer volume of the body of material 6 is at least 200, at least 300, at least 400, at least 500, at least 600, at least 700, at least 800, at least 900, or at least 1000 mm 3 .

[0147] In some embodiments, the axial length of the second body of material 6 is at least 4 mm, at least 5 mm, at least 6 mm, at least 7 mm, at least 8 mm, at least 9 mm, or at least 10 mm.

[0148] In some embodiments, the axial length of the second body of material 6 is in the range of about 5 to 20 mm, and preferably, 6 to 15 mm, and preferably, 6 to 10 mm.

[0149] In some embodiments, the width of the second body of material 6 is at least 4 mm, at least 5 mm, at least 6 mm, at least 7 mm, at least 8 mm, or at least 9 mm.

[0150] In some embodiments, the circumference of the second body of material 6 is at least 16 mm, at least 18 mm, at least 20 mm, at least 22 mm, at least 25 mm, or at least 28 mm.

[0151] In some embodiments, the pressure drop across the second body of material 6 is at least 2 WGmm, and preferably at least 3 mmWG, and preferably at least 4 mmWG. The pressure drop across the body of material may be at least 5, 6, 7, 8, 9, 10 or 11 mmWG.

[0152] In some embodiments, the pressure drop across the second body of material 6 is less than 20 mmWG, and possibly less than 16 mmWG, and preferably less than 15, 14, 13 or 12 mmWG.

[0153] In some embodiments, the pressure drop across the second body of material 6 is about 4.4, 8.1, or 11.9 mmWG.

[0154] In some embodiments, the pressure drop across the second body of material 6 is in the range of 3 to 15 mmWG, and preferably, in the range of 4 to 12 mmWG.

[0155] In some embodiments, the pressure drop across the second material body 6 is at least 0.2 mmWG per mm of the axial length of the second material body 6, and preferably, at least 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0 or 1.1 mmWG per mm of the axial length of the second material body 6.

[0156] In some embodiments, the pressure drop across the second material body 6 is less than 2 mm WG per mm of the axial length of the second material body 6 , and preferably, less than 1.6, 1.5, 1.4, 1.3 or 1.2 mm WG per mm of the axial length of the second material body 6 .

[0157] In some embodiments, the pressure drop across the second material body 6 is in the range of 0.3 to 1.5 mmWG per mm of the axial length of the second material body 6 , and preferably, in the range of 0.4 to 1.2 mmWG per mm of the axial length of the second material body 6 .

[0158] In some embodiments, the pressure drop across the second material body 6 is at least 2 mmWG, and preferably, at least 3 mmWG, and preferably, at least 4 mmWG, at least 6 mmWG, at least 8 mmWG, at least 10 mmWG, or at least 11 mmWG, or at least 12 mmWG, or at least 15 mmWG, or at least 20 mmWG, or at least 23 mmWG.

[0159] In some embodiments, the pressure drop across the second material body 6 is less than 25 mmWG, and preferably, less than 23 mmWG, less than 20 mmWG, less than 15 mmWG, less than 14 mmWG, and preferably, less than 12 mmWG or less than 10 mmWG.

[0160] In some embodiments, the pressure drop across the second body of material 6 is in the range of 10 to 25 mmWG, and preferably, in the range of 12 to 23 mmWG or 13 to 20 mmWG.

[0161] In some embodiments, the pressure drop across the second material body 6 is at least 0.2 mmWG per mm of material body axial length, and preferably, at least 0.3, 0.4, 0.6 or 0.8 mmWG per mm of material body axial length, and preferably, at least 1, 1.1, 1.2, 1.5, 2 or 2.33 mmWG per mm of material body axial length.

[0162] In some embodiments, the pressure drop across the second body of material 6 is less than 2.5 mm WG per mm of the body of material axial length, and preferably, less than 2.3, 2, 1.5, 1.4, 1.2 or 1 mm WG per mm of the body of material axial length.

[0163] In some embodiments, the pressure drop across the second material body 6 is in the range of 1 to 2.5 mmWG per mm of second material body axial length, and preferably, in the range of 1.2 to 2.3 or 1.3 to 2 mmWG per mm of second material body axial length.

[0164] In some embodiments having any of the above pressure drop values, second body of material 6 has an axial length of about 10 mm.

[0165] In some of these embodiments, the mass of the second body of material 6 is at least 20 mg, and preferably, at least 30 mg, at least 40 mg, at least 50 mg, at least 55 mg or at least 60 mg. It has been advantageously found that providing a higher mass of the second body of material 6 increases the amount of moisture absorbed from the aerosol. In an example of the present invention, the mass of the second body of material is about 44 mg.

[0166] In some of these embodiments, the mass of the second material body 6 is less than 150 mg, and preferably, less than 100 mg, less than 75 mg, less than 55 mg, less than 50 mg, or less than 45 mg.

[0167] In some embodiments, the second body of material 6 has a weight of at least 2 mg per mm of axial length of the body of material, and preferably, at least 3 mg per mm of axial length or at least 4 mg per mm of axial length.

[0168] In the example of the present invention, the second material body 6 has a weight of about 4.4 mg per mm. That is, if the material body 6 has an axial length of 10 mm, as in the example of the present invention, the mass will be about 44 mg.

[0169] In some embodiments, second body of material 6 is a solid cylindrical body of material.

[0170] In the example of the present invention, the first body of material 4 and the second body of material 6 are combined using a third plug wrap 9 which is wrapped around the two sections. The tipping paper 5 surrounds the entire length of the mouthpiece 2 and wraps over a portion of the aerosol generating material 3 rod, and has an adhesive on its inner surface to connect the mouthpiece 2 and the rod 3.

[0171] Preferably, the third plug wrap 9 has a basis weight of less than 50 gsm, more preferably a basis weight of about 20 gsm to 45 gsm. However, it will be appreciated that the basis weight of the third plug wrap 9 may be higher to increase the stiffness of the mouthpiece. For example, the basis weight of the third plug wrap 9 may be at least 50, 60, 70, 80, 90 or 100 gsm. In some embodiments, the basis weight of the third plug wrap 9 is in the range of 50 to 110 gsm, or in the range of 60 to 100 gsm.

[0172] In some embodiments, the third plug wrap 9 has a basis weight of at least 10 gsm, or at least 15 gsm, or at least 20 gsm, or at least 25 gsm.

[0173] In some embodiments, the third plug wrap 9 has a basis weight of less than 40, less than 35 or less than 30 gsm.

[0174] In some embodiments, the basis weight of the third plug wrap 9 is in the range of 10 to 40 gsm, and preferably in the range of 15 to 35 gsm, or in the range of 20 to 30 gsm, or in the range of 25 to 30 gsm. In some embodiments, the basis weight of the third plug wrap 9 is about 27 gsm.

[0175] Preferably, the third plug wrap 9 has a thickness of 30 μm to 60 μm, more preferably 35 μm to 45 μm. However, it will be appreciated that the thickness weight of the third plug wrap 9 may be higher to increase the stiffness of the mouthpiece. In some embodiments, for example, the thickness of the third plug wrap 9 may be at least 40, 50, 60, 70, 80, 90 or 100 microns. In some embodiments, the thickness of the third plug wrap 9 is in the range of 40 to 120 microns, or in the range of 50 to 100 microns.

[0176] The third plug wrap 9 is preferably a non-porous plug wrap having a permeability of less than 100 Korast units, for example less than 50 Korast units. However, in alternative embodiments, the third plug wrap 9 may be a porous plug wrap, for example having a permeability of more than 200 Korast units.

[0177] In the example of the invention, the second body of material 6 forms the mouth end of the component. Alternatively, further parts may be provided downstream of the second body of material 6.

[0178] Figure 4 is a side cross-sectional view of another article 1''' including a mouthpiece 2'''. The mouthpiece 2''' includes a first material body 4''' located at the mouth end of the mouthpiece, in which a first tubular element 4a'' and a second tubular element 4b'' are embedded. The first material body 4''' and the first tubular element 4a'' and the second tubular element 4b'' are substantially the same as the first material body 4 and the first tubular element 4a and the second tubular element 4b, except that they are constructed for provision at the mouth end of the mouthpiece. As described above, it may be desirable to apply a higher level of wrinkles to the sheet to form a material body or a portion of a material body visible from the mouth end of the mouthpiece, so that the material body has a desired appearance when viewed from the mouth end.

[0179] In an example of the present invention, a certain level of wrinkling is applied to the material body 4'" surrounding the first tubular element 4a' and the second tubular element 4b', which results in a densely compressed arrangement of the sheet material around the first tubular element 4a'' and the second tubular element 4b''. Advantageously, this can result in a portion of the body formed by the sheet material having this level of wrinkling having a desired hardness. For example, in the area circumferentially surrounding the first tubular element 4a'' and the second tubular element 4b'', the hardness of the material body 4''' can be greater than about 82%.

[0180] In the present example, the body of material 4'' does not extend beyond the ends of the first tubular element 4a'' and the second tubular element 4b''. Alternatively, Figure 1In a manner similar to the embodiments described in , the first material body 4"' can extend further than the first tubular element 4a" to form a portion of the material body 4" upstream of the first tubular element 4a", which extends across the entire width of the first material body 4"'. In these embodiments, the portion of the first material body 4"' located upstream of the first tubular element 4a" can provide the function of the second material body 6, and the second material body 6 can be omitted.

[0181] In the example of the present invention, the first tubular element 4a" and the second tubular element 4b" have the same specifications. The first tubular element 4a" and the second tubular element 4b" may have any suitable specifications as described above with respect to the first tubular element 4a and the second tubular element 4b.

[0182] Preferably, the length of the first material body 4'' is less than about 20mm. More preferably, the length of the first material body 4'' is less than about 15mm. Still more preferably, the length of the first material body 4'' is less than about 10mm. Additionally or alternatively, the length of the first material body 4'' is at least about 5mm. Preferably, the length of the first material body 4'' is at least about 6mm. In some preferred embodiments, the length of the first material body 4'' is from about 5mm to about 20mm, more preferably from about 6mm to about 10mm, even more preferably from about 6mm to about 8mm, most preferably about 6mm, 7mm or about 8mm. In an example of the present invention, the length of the first material body 4'' is 6mm. In an example of the present invention, each of the first hollow tubular element 4a'' and the second hollow tubular element 4b'' has a length of about 2.5mm and is separated by a gap of about 1mm. Alternatively, the first tubular element and the second tubular element may be separated by a gap of 0.5mm to 5mm, for example, 0.75mm to 1.5mm, or 1mm to 3mm.

[0183] The first hollow tubular element 4a" and the second hollow tubular element 4b" preferably have an inner diameter greater than 3.0 mm, respectively. A diameter smaller than this may cause the speed at which the aerosol passes through the mouthpiece 2"' and reaches the consumer's mouth to increase more than desired, causing the aerosol to become overheated, for example, to a temperature greater than 40°C or greater than 45°C. More preferably, the first hollow tubular element 4a" and the second hollow tubular element 4b" have an inner diameter greater than 3.1 mm, respectively, and even more preferably greater than 3.5 mm or 3.6 mm. In one embodiment, the inner diameter of each of the first hollow tubular element 4a" and the second hollow tubular element 4b" is about 3.9 mm.

[0184] In the example of the invention, the tubular portion is formed by a hollow tubular element 13. The hollow tubular element 13 may have any suitable specifications as described above for the first tubular element 4a and the second tubular element 4b.

[0185] Figure 5 2 is a side cross-sectional view of another article 1"" comprising a mouthpiece 2". The mouthpiece 2"" comprises a first material body 4"" in which a first tubular element 4a is embedded so as to be longitudinally and circumferentially surrounded by the material forming the first material body 4"". In the example of the present invention, the first tubular element 4a is disposed relative to the Figure 1 The first tubular element 4a described is identical but disposed at different locations. In the example of the invention, the first tubular element 4a is disposed at a substantially central position in the body of material 4"" so that the body of material 4"" extends beyond the upstream and downstream longitudinal ends of the tubular element 4a. As described above, the sheet forming the body of material may include a slit positioned so that when the sheet 14 is assembled into the body 4, the slit allows the sheet 14 located on the first side (e.g., the downstream side) of the object embedded in the body to come together so that the slit forms an inner edge in the body 4 that at least partially defines the boundary of the space containing the embedded object. In the example of the invention, the sheet 14 includes two slits positioned so that when the sheet is assembled into the body 4, the slits are adjacent to the upstream and downstream ends of the tubular element 4a. Providing the slits in the sheet 14 positioned at each end of the tubular element 4a allows the sheet 14 to be released to fully extend across the width of the body of material 4"" without deforming around the embedded tubular element.

[0186] Advantageously, the material body 4"" can be provided as the sole filter component of the mouthpiece 2"" since the tubular element and the material body together provide the desired cooling and filtering of the aerosol, wherein the material body 4"" has the tubular element 4a embedded in a position whereby the tubular element is longitudinally and circumferentially surrounded by the material body. Providing the body 4"" as the sole filter component of the mouthpiece can advantageously simplify the production of the mouthpiece 2"".

[0187] According to the present invention, the "aerosol providing system" includes both a flammable aerosol providing system and a non-flammable aerosol providing system.

[0188] According to the present disclosure, a "combustible" aerosol providing system is a system in which the constituent aerosol generating material (or components thereof) of the aerosol providing system burns or burns during use to facilitate delivery of at least one substance to a user.

[0189] In some embodiments, the delivery system is a combustible aerosol providing system, such as a system selected from the group consisting of a cigarette, a cigarillo, and a cigar.

[0190] In some embodiments, the present disclosure relates to components for use in a combustible aerosol delivery system, such as a filter, a filter rod, a filter segment, a tobacco rod, a spill, an aerosol regulator release component such as a capsule, a thread or a bead, or a paper such as a plug wrap, a tipping paper or a cigarette paper.

[0191] According to the present disclosure, a "non-flammable" aerosol providing system is one in which the constituent aerosol generating materials (or components thereof) of the aerosol providing system do not burn or burn to facilitate delivery of at least one substance to a user.

[0192] In some embodiments, the delivery system is a non-flammable aerosol providing system, such as a powered non-flammable aerosol providing system.

[0193] In some embodiments, the non-flammable aerosol providing system is an electronic cigarette, also known as an electronic cigarette (vaping) device or an electronic nicotine delivery system (END), but it should be noted that the presence of nicotine in the aerosol generating material is not a requirement.

[0194] In some embodiments, the non-flammable aerosol providing system is an aerosol generating material heating system, also known as a heat-not-burn system. An example of such a system is a tobacco heating system.

[0195] In some embodiments, the non-flammable aerosol providing system is a hybrid system that uses a combination of aerosol generating materials to generate an aerosol, one or more of which can be heated. Each aerosol generating material can be, for example, in solid, liquid or gel form, and may or may not contain nicotine. In some embodiments, the hybrid system comprises a liquid or gel aerosol generating material and a solid aerosol generating material. The solid aerosol generating material can include, for example, tobacco or non-tobacco products.

[0196] Generally, a non-flammable aerosol providing system may include a non-flammable aerosol providing device and consumables for use with the non-flammable aerosol providing device.

[0197] In some embodiments, the present disclosure relates to consumables that contain aerosol-generating materials and are configured for use with non-flammable aerosol-providing devices. Throughout the invention disclosure, these consumables are sometimes referred to as articles.

[0198] In some embodiments, the non-flammable aerosol providing system, such as the non-flammable aerosol providing device thereof, may include an energy source and a controller. The energy source may be, for example, a power source or a heat generating energy source. In some embodiments, the heat generating energy source includes a carbon matrix that can be excited to distribute energy in the form of heat to the aerosol generating material or to a heat transfer material close to the heat generating energy source.

[0199] In some embodiments, the non-flammable aerosol providing system may include an area for housing consumables, an aerosol generator, an aerosol generating region, a housing, a mouthpiece, a filter, and / or an aerosol modifier.

[0200] In some embodiments, consumables for use with a non-flammable aerosol providing device may include an aerosol generating material, an aerosol generating material storage area, an aerosol generating material delivery component, an aerosol generator, an aerosol generating area, a shell, a wrapping paper, a filter, a mouthpiece and / or an aerosol regulator.

[0201] In some embodiments, the substance to be delivered comprises an active substance.

[0202] As used herein, active substances can be physiologically active materials, which are materials intended to achieve or improve physiological responses. The active substances can be, for example, selected from nutrients, nootropics, psychoactive agents. The active substances can be naturally occurring or synthetically obtained. The active substances can include, for example, nicotine, caffeine, taurine, caffeine, vitamins such as B6 or B12 or C, melatonin or their components, derivatives or combinations. The active substances can include one or more components, derivatives or extracts of tobacco or another botanical.

[0203] In some embodiments, the active substance comprises nicotine. In some embodiments, the active substance comprises caffeine, melatonin or vitamin B12.

[0204] As mentioned herein, the active substance may include or be derived from one or more botanicals or components, derivatives or extracts thereof. As used herein, the term "botanical" includes any material derived from a plant, including but not limited to extracts, leaves, bark, fibers, rods, roots, seeds, flowers, fruits, pollen, skins, shells, etc. Alternatively, the material may include active compounds naturally present in plants and obtained synthetically. Examples of botanicals are tobacco, eucalyptus, anise, cocoa, fennel, lemongrass, peppermint, green mint, rooibos, chamomile, flax, ginger, ginkgo, hazelnut, hibiscus, laurel, licorice (licorice), matcha, holly tea, orange peel, papaya, rose, sage, tea such as green tea or black tea, thyme, cloves, cinnamon, coffee, anise (fennel), basil, bay leaf, cardamom, coriander, cumin, nutmeg, oregano, red pepper, rosemary, Saffron, lavender, lemon peel, mint, juniper, elderflower, vanilla, basil, turmeric, turmeric, sandalwood, cilantro, bergamot, orange blossom, myrtle, black currant, valerian, chili, nutmeg, damien, oregano, olive, lemon balm, lemon basil, chives, caraway, verbena, tarragon, geranium, mulberry, ginseng, theanine, theophylline, maca, ashwagandha, pistacia, cocoa, chlorophyll, baobab, or any combination thereof. The mint may be selected from the following mint varieties: wild mint (Mentha arventis), mint cultivar (Mentha ac.v.), Egyptian mint (Mentha niliaca), peppermint (Mentha piperita), peppermint lemon mint cultivar (Mentha piperita citrata cv), peppermint cultivar (Mentha piperita cv), wrinkled green mint (Mentha spicata crispa), madder mint (Mentha cordifolia), European peppermint (Mentha longifolia), variegated pineapple mint (Mentha suaveolens variegata), pomegranate (Mentha pulegium), spearmint cultivar (Memtha spicata cv) and apple mint (Mentha suaveolens).

[0205] In some embodiments, the active substance comprises or is derived from one or more botanicals or components, derivatives or extracts thereof, and the botanical is tobacco.

[0206] In some embodiments, the active ingredient comprises or is derived from one or more botanicals or components, derivatives or extracts thereof, and the botanicals are selected from eucalyptus, star anise and cocoa.

[0207] In some embodiments, the active ingredient comprises or is derived from one or more botanicals or components, derivatives or extracts thereof, and the botanicals are selected from Rooibos and Fennel.

[0208] In some embodiments, the substance to be delivered comprises a flavorant.

[0209] As used herein, the terms "flavoring agent" and "flavoring agent" refer to materials that can be used to produce a desired taste, aroma or other physical sensation in adult consumer products, where permitted by local regulations. They can include naturally occurring flavoring materials, botanicals, extracts of botanicals, synthetically obtained materials, or combinations thereof (e.g., tobacco, licorice (licorice), hydrangea, eugenol, Japanese white bark magnolia leaf, chamomile, fenugreek, cloves, maple, matcha, menthol, Japanese mint, aniseed (fennel), cinnamon, turmeric, Indian spices, Asian spices, vanilla, wintergreen, cherry, berry, cranberry, cranberry, peach, apple, orange, mango, tangerine, lemon, sour lemon, tropical fruit, papaya, rhubarb, grape, durian, pitaya, cucumber, blueberry, mulberry, citrus fruit, honey whiskey, bourbon whiskey, Scotch whiskey, whisky, gin, tequila, rum, spearmint, peppermint, lavender, aloe, cardamom, celery, quinoa, nutmeg, sandalwood, bergamot, geranium, khat, naswar, betel nut, hookah, pine, honey essence, rose oil, vanilla, lemon oil, orange oil, orange blossom, cherry blossom, cinnamon, caraway, cognac, jasmine, ylang-ylang, sage, fennel, chamomile, allspice, ginger, coriander, coffee, mint oil from any species of the genus Mentha, eucalyptus, anise, cocoa, lemongrass, rooibos, flax, ginkgo, hazelnut, hibiscus, laurel, wintergreen tea, orange peel, rose, tea such as green or black, thyme, juniper, elderflower, basil, bay leaf, cumin, oregano, red pepper, rosemary, saffron, lemon peel, mint, basil, turmeric, cilantro, myrtle, black currant, valerian, chili pepper, nutmeg, damien, oregano, olive, The invention relates to a method for preparing a mouthwash comprising: preparing a mouthwash comprising: preparing a mouthwash comprising: a balm, lemon basil, chives, caraway, verbena, tarragon, limonene, thymol, camphene), flavor enhancers, bitter taste receptor site blockers, sensory receptor site activators or stimulators, sugars and / or sugar substitutes (e.g., sucralose, acesulfame potassium, aspartame, saccharin, cyclamate, lactose, sucrose, glucose, fructose, sorbitol or mannitol), and other additives such as activated carbon, chlorophyll, minerals, plants or breath fresheners. They can be simulated, synthetic or natural ingredients or blends thereof. They can be in any suitable form, for example, liquids such as oils, solids such as powders, or gases.

[0210] In some embodiments, the flavoring agent comprises menthol, spearmint and / or peppermint. In some embodiments, the flavoring agent comprises the flavor components of cucumber, blueberry, citrus fruit and / or cranberry. In some embodiments, the spice comprises eugenol. In some embodiments, the flavoring agent comprises the flavor components extracted from tobacco.

[0211] In some embodiments, the flavoring agent may include sensates that are intended to achieve a somatic sensation that is typically chemically induced and sensed by stimulation of the fifth cranial nerve (trigeminal nerve) in addition to or in lieu of the aroma or taste nerves, and these may include agents that provide a hot, cool, tingling, numbing effect. Suitable hot acting agents may be, but are not limited to, vanillyl ethyl ether, and suitable cooling agents may be, but are not limited to, eucalyptol, WS-3.

[0212] Aerosol generating materials are materials that can generate aerosols, for example, when heated, irradiated, or powered in any other way. Aerosol generating materials can be, for example, in solid, liquid, or gel form, which may or may not contain active substances and / or flavoring agents. In some embodiments, the aerosol generating material may comprise an "amorphous solid", which may alternatively be referred to as a "monolithic solid" (i.e., non-fibrous). In some embodiments, the amorphous solid may be a xerogel. The amorphous solid is a solid material that can retain some fluid, such as a liquid, inside it. In some embodiments, the aerosol generating material may, for example, comprise about 50wt%, 60wt%, or 70wt% of an amorphous solid to about 90wt%, 95wt%, or 100wt% of an amorphous solid.

[0213] The aerosol-generating material may comprise one or more active substances and / or flavouring agents, one or more aerosol former materials and optionally one or more other functional materials.

[0214] The aerosol forming agent material may include one or more components capable of forming an aerosol. In some embodiments, the aerosol forming agent material may include one or more of glycerol, glycerine, propylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, 1,3-butylene glycol, erythritol, meso-erythritol, ethyl vanillate, ethyl dodecanoate, diethyl suberate, triethyl citrate, glyceryl triacetate, diacetate glyceryl mixture, benzyl benzoate, benzyl phenylacetate, tributyrin, lauryl acetate, lauric acid, myristic acid, and propylene carbonate.

[0215] The one or more other functional materials may include one or more of a pH adjuster, a colorant, a preservative, a binder, a filler, a stabilizer and / or an antioxidant.

[0216] The material may be present on or in a support to form a substrate. The support may, for example, be or include paper, paper card, paperboard, cardboard, a reconstructed material, a plastic material, a ceramic material, a composite material, glass, a metal or a metal alloy. In some embodiments, the support includes a susceptor. In some embodiments, the susceptor is embedded in the material. In some alternative embodiments, the susceptor is located on one side or either side of the material.

[0217] A consumable is an article comprising or consisting of an aerosol generating material, some or all of which is intended to be consumed by a user during use. A consumable may comprise one or more other components, such as an aerosol generating material storage area, an aerosol generating material delivery component, an aerosol generating area, a housing, a wrapper, a cigarette holder, a filter and / or an aerosol modifier. A consumable may also comprise an aerosol generator, such as a heater, which emits heat during use to cause the aerosol generating material to generate an aerosol. The heater may, for example, comprise a combustible material, a material that is heatable by electrical conduction, or a base.

[0218] The susceptor is a material that is heatable by penetration of a changing magnetic field, such as an alternating magnetic field. The susceptor may be a conductive material, such that penetration of the changing magnetic field into it results in inductive heating of the heating material. The heating material may be a magnetic material, such that penetration of the changing magnetic field into it results in hysteresis heating of the heating material. The susceptor may be both conductive and magnetic, such that the susceptor is heatable by two heating mechanisms. In this article, a device configured to generate a changing magnetic field is referred to as a magnetic field generator.

[0219] An aerosol modifier is a substance configured to modify the aerosol produced, for example, by changing the taste, flavor, acidity or another characteristic of the aerosol.The aerosol modifier may be provided in an aerosol modifier release component that is operable to selectively release the aerosol modifier.

[0220] The aerosol modifier may be, for example, an additive or an adsorbent. The aerosol modifier may, for example, contain one or more of a flavoring agent, a colorant, water, and a carbon adsorbent. The aerosol modifier may, for example, be a solid, a liquid, or a gel. The aerosol modifier may be in the form of a powder, a thread, or a granule. The aerosol modifier may not contain a filter material.

[0221] An aerosol generator is a device configured to cause an aerosol to be generated from an aerosol generating material. In some embodiments, the aerosol generator is a heater configured to subject the aerosol generating material to thermal energy, thereby releasing one or more volatile substances from the aerosol generating material to form an aerosol. In some embodiments, the aerosol generator is configured to cause an aerosol to be generated from an aerosol generating material without heating. For example, the aerosol generator can be configured to subject the aerosol generating material to one or more of vibration, pressure rise, or electrostatic energy.

[0222] The articles are often named according to their length, e.g., those in rod form: "regular" (typically in the range of 68-75 mm, e.g., about 68 mm to about 72 mm), "short" or "micro" (68 mm or less), "jumbo" (typically in the range of 75-91 mm, e.g., about 79 mm to about 88 mm), "long" or "extra jumbo" (typically in the range of 91-105 mm, e.g., about 94 mm to about 101 mm), and "extra long" (typically in the range of about 110 mm to about 121 mm).

[0223] They are also named according to the product circumference: "Regular" (about 23-25 ​​mm), "Wide" (greater than 25 mm), "Slim" (about 22-23 mm), "Semi-Slim" (about 19-22 mm), "Extra-Slim" (about 16-19 mm) and "Micro-Slim" (less than about 16 mm).

[0224] Thus, a giant, ultra-thin version of the article would, for example, have a length of about 83 mm and a circumference of about 17 mm.

[0225] Various forms with different lengths of mouthpieces can be produced. The mouthpiece length will be from about 30 mm to 50 mm. The tipping paper connects the mouthpiece to the aerosol generating material and will typically have a length greater than the mouthpiece, for example, 3 to 10 mm longer than the mouthpiece, so that the tipping paper covers the mouthpiece and overlaps the aerosol generating material, for example, in the form of a rod of substrate material, thereby connecting the mouthpiece to the rod.

[0226] The articles described herein, and their aerosol-generating materials and mouthpieces, may be prepared in any of the above-described forms, but are not limited to any of the above-described forms.

[0227] As used herein, the terms "upstream" and "downstream" are relative terms defined relative to the direction of the mainstream aerosol inhaled through the article or device in use.

[0228] The filamentary tow material described herein can include cellulose acetate fiber tow. It is also possible to use other materials for forming fibers to form filamentary tows, such as polyvinyl alcohol (PVOH), polylactic acid (PLA), polycaprolactone (PCL), poly (1-4 butylene glycol succinate) (PBS), poly (butylene adipate-co-butylene terephthalate) (PBAT), starch-based materials, cotton, aliphatic polyester materials and polysaccharide polymers or combinations thereof. The filamentary tow can be plasticized by a plasticizer (such as triacetin) suitable for the tow, wherein the material is cellulose acetate tow, or the tow can be a non-plastic material. The tow can have any suitable specifications, such as having a "Y" shape or other cross-section, such as an "X" shape, a single fiber denier value of 2.5 to 15 single filament deniers, for example, 8.0 to 11.0 single filament deniers, and a total denier value of 5,000 to 50,000, such as 10,000 to 40,000 fibers.

[0229] As used herein, the term "tobacco material" refers to any material that comprises tobacco or its derivative or substitute. The term "tobacco material" can include one or more of tobacco, tobacco derivatives, expanded tobacco, reconstituted tobacco or tobacco substitutes. The tobacco material can include one or more of tobacco dust, tobacco fiber, shredded tobacco, extruded tobacco, tobacco stems, tobacco flakes, reconstituted tobacco and / or tobacco extract.

[0230] Figure 6 An example of a non-flammable aerosol providing device 100 for generating an aerosol from an aerosol generating medium / material, such as an aerosol generating material 3 of any of the articles 1, 1', 1", 1"', 1"" described herein is shown. Generally, the device 100 can be used to heat a replaceable article 110 containing an aerosol generating medium, such as the articles 1, 1', 1", 1"', 1"" described herein, to generate an aerosol or other inhalable medium that is inhaled by a user of the device 100. The device 100 and the replaceable article 110 together form a system.

[0231] The device 100 includes a housing 102 (in the form of a cover) that encloses and contains the various components of the device 100. The device 100 has an opening 104 at one end through which an article 110 can be inserted for heating by the heating assembly. In use, the article 110 can be fully or partially inserted into the heating assembly, where it can be heated by one or more components of the heater assembly.

[0232] When the article 110 is inserted into the device 100, the minimum distance between one or more components of the heater assembly and the tubular body 4a of the article 110 can be in the range of 3mm to 10mm, for example 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm or 10mm.

[0233] The device 100 of this example includes a first end member 106, which includes a cover 108 that is movable relative to the first end member 106 so as to close the opening 104 when no article 110 is in place. Figure 6 In FIG. 1 , the cover 108 is shown in an open configuration, but the cover 108 can be moved to a closed configuration. For example, the user can slide the cover 108 in the direction of arrow "B".

[0234] The device 100 may also include a user-operable control element 112, such as a button or switch, which, when pressed, operates the device 100. For example, by operating the switch 112, the user may turn the device 100 on.

[0235] The device 100 may also include electrical components, such as a socket / port 114, which may accept an electrical cord to charge a battery of the device 100. For example, the socket 114 may be a charging port, such as a USB charging port.

[0236] Figure 7 The outer cover 102 is removed and the article 110 is not present. Figure 6 The device 100 is shown. The device 100 defines a longitudinal axis 134.

[0237] like Figure 7 As shown, the first end member 106 is disposed at one end of the device 100, and the second end member 116 is disposed at the opposite end of the device 100. The first end member 106 and the second end member 116 together at least partially define an end surface of the device 100. For example, the bottom surface of the second end member 116 at least partially defines the bottom surface of the device 100. The edge of the housing 102 can also define a portion of the end surface. In this example, the cover 108 also defines a portion of the top surface of the device 100.

[0238] The end of the device closest to the opening 104 can be referred to as the proximal end (or mouth end) of the device 100 because, in use, it is closest to the user's mouth. In use, the user inserts the article 110 into the opening 104, operates the user control 112 to begin heating the aerosol-generating material and inhales the aerosol generated in the device. This causes the aerosol to flow through the device 100 along a flow path toward the proximal end of the device 100.

[0239] The other end of the device farthest from the mouth 104 can be referred to as the distal end of the device 100 because it is the end farthest from the user's mouth in use. When the user inhales the aerosol generated in the device, the aerosol flows out of the distal end of the device 100.

[0240] The device 100 also includes a power source 118. The power source 118 can be, for example, a battery, such as a rechargeable battery or a non-rechargeable battery. Examples of suitable batteries include, for example, lithium batteries (such as lithium ion batteries), nickel batteries (such as nickel cadmium batteries), and alkaline batteries. The battery is electrically connected to the heating assembly to provide power to heat the aerosol generating material when needed and under the control of a controller (not shown). In this example, the battery is connected to a central support 120 that holds the battery 118 in place.

[0241] The device also includes at least one electronic module 122. The electronic module 122 may include, for example, a printed circuit board (PCB). The PCB 122 may support at least one controller, such as a processor, and a memory. The PCB 122 may also include one or more electrical tracks to electrically connect multiple electronic components of the device 100 together. For example, a battery terminal may be electrically connected to the PCB 122 so that power can be distributed throughout the device 100. The socket 114 may also be electrically coupled to the battery via the electrical tracks.

[0242] In the example device 100, the heating assembly is an induction heating assembly and includes a plurality of components to heat the aerosol generating material of the article 110 by an induction heating process. Induction heating is a process of heating a conductive object (such as a susceptor) by electromagnetic induction. The induction heating assembly may include an induction element, for example, one or more induction coils, and a device for passing a varying current (such as an alternating current) through the induction element. The varying current in the induction element generates a varying magnetic field. The varying magnetic field penetrates a susceptor appropriately positioned relative to the induction element and generates eddy currents inside the susceptor. The susceptor has a resistance to the eddy currents, and thus the flow of the eddy currents to the resistance causes the susceptor to be heated by Joule heating. In the case where the susceptor includes a ferromagnetic material such as iron, nickel or cobalt, heat may also be generated by hysteresis losses in the susceptor, i.e., changes in the orientation of magnetic dipoles in the magnetic material caused by the alignment of the magnetic dipoles in the magnetic material by a varying magnetic field. In induction heating, heat is generated inside the susceptor, allowing rapid heating, compared to heating by conduction, for example. Furthermore, no physical contact is required between the induction heater and the base, allowing for increased freedom in construction and application.

[0243] The induction heating assembly of the example device 100 includes a base arrangement 132 (referred to herein as a "base"), a first induction coil 124, and a second induction coil 126. The first induction coil 124 and the second induction coil 126 are made of a conductive material. In an example of the present invention, the first induction coil 124 and the second induction coil 126 are made of a Litz wire / cable wound in a spiral manner to provide a spiral induction coil 124, 126. The Litz wire is designed to reduce skin effect losses in the conductor. In the example device 100, the first induction coil 124 and the second induction coil 126 are made of copper Litz wire having a rectangular cross-section. In other examples, the Litz wire may have a cross-section of other shapes, for example, a circle.

[0244] The first induction coil 124 is configured to generate a first changing magnetic field to heat a first portion of the base 132, and the second induction coil 126 is configured to generate a second changing magnetic field to heat a second portion of the base 132. In this example, the first induction coil 124 is adjacent to the second induction coil 126 in the direction along the longitudinal axis 134 of the device 100 (that is, the first induction coil 124 and the second induction coil 126 do not overlap). The base arrangement 132 can include a single base, or two or more separate bases. The ends 130 of the first induction coil 124 and the second induction coil 126 can be connected to the PCB 122.

[0245] It should be understood that in some examples, the first induction coil 124 and the second induction coil 126 may have at least one characteristic that is different from each other. For example, the first induction coil 124 may have at least one characteristic that is different from the second induction coil 126. More specifically, in one example, the first induction coil 124 may have a different induction value than the second induction coil 126. Figure 8 In the embodiment, first induction coil 124 and second induction coil 126 have different lengths, so that first induction coil 124 is wound around a smaller portion of base 132 than second induction coil 126. Therefore, first induction coil 124 can include a different number of turns than second induction coil 126 (assuming that the spacing between the turns is substantially the same). In yet another example, first induction coil 124 can be made of a different material than second induction coil 126. In some examples, first induction coil 124 and second induction coil 126 can be substantially identical.

[0246] In this example, the first induction coil 124 and the second induction coil 126 are wound in opposite directions. This can be useful when the induction coils are activated at different times. For example, initially, the first induction coil 124 can be operated to heat a first section / portion of the article 110, and subsequently, the second induction coil 126 can be operated to heat a second section / portion of the article 110. When used in conjunction with certain types of control circuits, winding the coils in opposite directions helps reduce the current induced in the inactive coils. Figure 7 In the embodiment, the first induction coil 124 is a right-handed spiral, and the second induction coil 126 is a left-handed spiral. However, in another embodiment, the induction coils 124, 126 can be wound in the same direction, or the first induction coil 124 can be a left-handed spiral and the second induction coil 126 can be a right-handed spiral.

[0247] The base 132 of this embodiment is hollow and thus defines a container in which the aerosol-generating material is contained. For example, the article 110 may be inserted into the base 132. In this example, the base 120 is tubular, having a circular cross-section.

[0248] The base 132 may be made of one or more materials. Preferably, the base 132 comprises carbon steel with a nickel or cobalt coating.

[0249] In some examples, the base 132 may include at least two materials that can be heated at two different frequencies for selective aerosolization of the at least two materials. For example, the first section of the base 132 (which is heated by the first induction coil 124) may include a first material, and the second section of the base 132 (which is heated by the second induction coil 126) may include a second different material. In another example, the first section may include a first material and a second material, wherein the first material and the second material may be heated differently based on the operation of the first induction coil 124. The first material and the second material may be adjacent along an axis defined by the base 132, or may form different layers within the base 132. Similarly, the second section may include a third material and a fourth material, wherein the third material and the fourth material may be heated differently based on the operation of the second induction coil 126. The third material and the fourth material may be adjacent along an axis defined by the base 132, or may form different layers within the base 132. For example, the third material may be the same as the first material, and the fourth material may be the same as the second material. Alternatively, each material may be different. For example, the base may comprise carbon steel or aluminum.

[0250] Figure 7The device 100 also includes an insulating member 128, which can be generally tubular and at least partially surround the base 132. The insulating member 128 can be made of any insulating material, such as, for example, plastic. In this specific example, the insulating member is made of polyetheretherketone (PEEK). The insulating member 128 can help to isolate the various components of the device 100 from the heat generated in the base 132.

[0251] The thermal insulation member 128 may also fully or partially support the first induction coil 124 and the second induction coil 126. Figure 8 As shown, the first induction coil 124 and the second induction coil 126 are positioned around the insulating member 128 and in contact with the radially outward surface of the insulating member 128. In some examples, the insulating member 128 does not abut the first induction coil 124 and the second induction coil 126. For example, a small gap may exist between the outer surface of the insulating member 128 and the inner surface of the first induction coil 124 and the second induction coil 126.

[0252] In a specific example, the base 132 , the insulating member 128 , and the first and second induction coils 124 , 126 are coaxial about a central longitudinal axis of the base 132 .

[0253] Figure 8 A partial cross-sectional side view of the device 100 is shown. In this example the housing 102 is present. The rectangular cross-sectional shape of the first induction coil 124 and the second induction coil 126 is more clearly visible.

[0254] The device 100 also includes a support 136 that engages one end of the base 132 to hold the base 132 in place. The support 136 is connected to the second end member 116.

[0255] The device may also include a second printed circuit board 138 incorporated within the control element 112 .

[0256] The device 100 also includes a second cover / cap 140 and a spring 142 disposed toward the distal end of the device 100. The spring 142 allows the second cover 140 to open to provide access to the base 132. The user can open the second cover 140 to clean the base 132 and / or the support 136.

[0257] The device 100 also includes an expansion chamber 144 that extends away from the proximal end of the base 132 toward the opening 104 of the device. A retaining clip 146 is at least partially located within the expansion chamber 144 to abut and retain the article 110 when the article 110 is received within the device 100. The expansion chamber 144 is connected to the end member 106.

[0258] Fig. 9yes Figure 8 An exploded view of the device 100 is shown with the housing 102 omitted.

[0259] Fig. 10A Shows Fig. 9 A cross-section of a portion of the device 100 is shown. Fig. 10B Shows Fig. 10A A close-up of the area. Fig. 10A and 10B The article 110 is shown contained within a base 132, wherein the dimensions of the article 110 are such that the outer surface of the article 110 abuts the inner surface of the base 132. This ensures that heating is most effective. The article 110 of this example includes an aerosol generating material 110a. The aerosol generating material 110a is located within the base 132. The article 110 may also include other components, such as a filter, packaging material, and / or a cooling structure.

[0260] Fig. 10B The outer surface of the base 132 is shown separated from the inner surfaces of the induction coils 124, 126 by a distance 150, which is measured in a direction perpendicular to the longitudinal axis 158 of the base 132. In one specific example, the distance 150 is about 3 mm to 4 mm, about 3-3.5 mm, or about 3.25 mm.

[0261] Fig. 10B It is further shown that the outer surface of the insulation 128 is separated from the inner surface of the induction coils 124, 126 by a distance 152, which is measured in a direction perpendicular to the longitudinal axis 158 of the base 132. In one specific example, the distance 152 is about 0.05 mm. In another example, the distance 152 is substantially 0 mm, so that the induction coils 124, 126 abut and contact the insulation 128.

[0262] In one example, the base 132 has a wall thickness 154 of about 0.025 mm to 1 mm, or about 0.05 mm.

[0263] In one example, the base 132 has a length of about 40 mm to 60 mm, about 40 mm to 45 mm, or about 44.5 mm.

[0264] In one example, the insulation 128 has a wall thickness 156 of approximately 0.25 mm to 2 mm, 0.25 mm to 1 mm, or approximately 0.5 mm.

[0265] In use, the articles 1, 1', 1", 1"', 1"" described herein may be inserted into a non-flammable aerosol providing device, such as the one described in reference Figures 6 to 10BThe described device 100. At least a portion of the mouthpiece 2, 2', 2", 2"', 2"" of the article 1, 1', 1", 1"" extends from the non-flammable aerosol providing device 100 and can be placed in the mouth of a user. An aerosol is generated by heating an aerosol generating material 3 using the device 100. The aerosol generated by the aerosol generating material 3 passes through the mouthpiece 2 to reach the mouth of the user.

[0266] A method for forming a mouthpiece 2, 2', 2", 2'", 2"', 2"" as described herein may suitably include the following steps: applying a corrugation pattern to a sheet, the corrugation pattern comprising a series of substantially parallel ridges and grooves; providing a supply of tubular elements; and gathering the sheet of fibrous material around the tubular elements to form a body of material, wherein at least one tubular element extends through the body substantially along a common axis and is circumferentially surrounded by the sheet of fibrous material. In some examples, the method further includes positioning the at least one tubular element so that the at least one tubular element is embedded in the body, so that the at least one tubular element is circumferentially and longitudinally surrounded by the fibrous material forming the body.

[0267] Apparatus configured for producing components as described herein may suitably include: a crimping roller for applying a corrugation pattern to a sheet of fibrous material, the corrugation pattern comprising a series of substantially parallel ridges and grooves; a feed mechanism for tubular elements; and a matching assembly for gathering the sheet of fibrous material around the tubular elements to form a material body, wherein at least one tubular element extends through the body substantially along a common axis and is circumferentially surrounded by the fibrous material.

Claims

1. A component for use in an aerosol delivery system or as an article of an aerosol delivery system, the component comprising: A fiber material body; as well as A first tubular element and a second tubular element extend through the body substantially along a common axis and are each circumferentially surrounded by a fiber material.

2. A component according to claim 1, wherein the component forms a mouthpiece of a single article.

3. The component according to claim 1 or 2, wherein the fiber material is a first cellulose-based material.

4. The component of claim 3, wherein the first cellulose-based material is paper.

5. The component of claim 4, wherein the paper is formed from wood pulp.

6. The component of claim 3, wherein the first cellulose-based material is a reconstituted tobacco sheet.

7. A component according to any one of claims 1 to 6, wherein the first and second tubular elements are separated by a gap of 0.5 mm to 5 mm, or 0.75 mm to 1.5 mm, or 1 mm to 3 mm.

8. A component according to any one of claims 1 to 6, wherein the first and second tubular elements are separated by a gap of 5 mm to 15 mm, or 6 mm to 12 mm, or 8 mm to 11 mm.

9. The component of claim 8, wherein the body of fibrous material extends into the gap.

10. A component according to any one of claims 1 to 9, wherein the first tubular element and / or the second tubular element extends to a longitudinal end of the component.

11. A component according to any one of claims 1 to 10, wherein a first pleat factor is applied to a first longitudinal region of the body of fibrous material and a second pleat factor is applied to a second longitudinal region of the body of fibrous material.

12. The component of claim 11, wherein the first and second wrinkle factors are one of depth, spacing, pressure, or temperature.

13. The component according to any one of claims 1 to 12, wherein the first tubular element and / or the second tubular element is formed from a second cellulose-based material.

14. The component of claim 13, wherein the second cellulose-based material is paper.

15. The component of claim 14, wherein the paper is formed from wood pulp.

16. The component of claim 15, wherein the second cellulose-based material is a reconstituted tobacco sheet.

17. A component according to any one of claims 1 to 16, wherein the body of fibrous material is formed from one or more sections of sheet material.

18. A component for use in an aerosol delivery system or as an article of an aerosol delivery system, the component comprising: A fiber material body; as well as A tubular element is embedded within the body such that the tubular element is circumferentially and longitudinally surrounded by the fibrous material forming the body.

19. A component according to claim 18, wherein the component forms the mouthpiece of a single article.

20. The component of claim 18 or 19, wherein the fiber material is a first cellulose-based material.

21. The component of claim 20, wherein the first cellulose-based material is paper.

22. The component of claim 21 wherein the paper is formed from wood pulp.

23. The component of claim 20, wherein the first cellulose-based material is a reconstituted tobacco sheet.

24. A component according to any one of claims 18 to 23, wherein the proximal end of the tubular element is spaced at least 5 mm, or at least 8 mm, or at least 10 mm from the longitudinal end of the component.

25. A component according to any one of claims 18 to 23, wherein the tubular element extends to a longitudinal end of the component.

26. A component according to any one of claims 18 to 25, wherein a first pleat factor is applied to a first longitudinal region of the body of fibrous material and a second pleat factor is applied to a second longitudinal region of the body of fibrous material.

27. The component of claim 26, wherein the first and second wrinkle factors are one of depth, spacing, pressure, or temperature.

28. A component according to any one of claims 18 to 27, wherein the tubular element is formed from a second cellulose-based material.

29. A component according to any one of claims 18 to 28, wherein the body of fibrous material is formed from one or more sections of sheet material.

30. An article for use in or as an aerosol delivery system, the article having a downstream end, the article comprising: A fiber material body; as well as A tubular element circumferentially surrounded by a fibrous material, wherein the tubular element extends to a first longitudinal end of the body and is spaced from a second longitudinal end of the body, and wherein the longitudinal end of the body to which the tubular element extends is spaced from the downstream end of the article.

31. The article of claim 30, wherein the fiber material is a third cellulose-based material.

32. The article of claim 31 , wherein the third cellulose-based material is paper.

33. The article of claim 32, wherein the paper is formed from wood pulp.

34. The article of claim 33, wherein the third cellulose-based material is a reconstituted tobacco sheet.

35. An article according to any one of claims 30 to 34, wherein the proximal end of the tubular element is spaced at least 5 mm, or at least 8 mm, or at least 10 mm from a longitudinal end of the article.

36. An article according to any one of claims 30 to 35, wherein the tubular element extends to a longitudinal end of the article.

37. An article according to any one of claims 30 to 36, wherein a first pleat factor is applied to a first longitudinal region of the body of fibrous material and a second pleat factor is applied to a second longitudinal region of the body of fibrous material.

38. The article of claim 37, wherein the first and second wrinkle factors are one of depth, spacing, pressure, or temperature.

39. The article of any one of claims 30 to 38, wherein the tubular element is formed from a second cellulose-based material.

40. An article according to any one of claims 30 to 39, wherein the body of fibrous material is formed from one or more sections of sheet material.

41. An article comprising a component according to any one of claims 1 to 29.

42. A method for forming a component of an article for use in an aerosol delivery system, the method comprising: applying a corrugation pattern to a sheet of fibrous material, the corrugation pattern comprising a series of substantially parallel ridges and grooves; providing a supply of tubular elements; as well as The sheets of fibrous material are gathered around the tubular elements to form a body of material, wherein at least one tubular element extends through the body substantially along a common axis and is circumferentially surrounded by the sheets of fibrous material.

43. The method of claim 41 further comprising positioning the at least one tubular element so that the at least one tubular element is embedded within the material body, thereby the at least one tubular element is circumferentially and longitudinally surrounded by the fibrous material sheet forming the material body.

44. An apparatus configured for producing a component according to any one of claims 1 to 39, comprising: a crimping roller for imparting a crimp pattern to the sheet of fibrous material, the crimp pattern comprising a series of substantially parallel ridges and troughs; a feeding mechanism for tubular elements; as well as A kit for gathering the sheets of fibrous material around the tubular elements to form a body of material, wherein at least one tubular element extends through the body substantially along a common axis and is circumferentially surrounded by fibrous material.

Citation Information

Patent Citations

  • Filtered cigarette comprising a tubular element in filter

    CN103763949A

  • Method and apparatus for manufacturing variable crimped web material

    CN105473010A

  • Aerosol generating article for use with an aerosol generating device

    CN113518561A

  • An article for use in an aerosol provision system and an article for use in a non-combustible aerosol provision system

    WO2021123843A1