Electrochromic dimming structure and traffic equipment

CN118871852AActive Publication Date: 2024-10-29BOE TECHNOLOGY GROUP CO LTD +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202380007963.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-02-28
Publication Date
2024-10-29
Estimated Expiration
2043-02-28

AI Technical Summary

Technical Problem

The existing color-changing canopy in new energy vehicles has slow dimming speed, poor user experience, and high cost. Moreover, the suspended particle canopy consumes a lot of power and has poor thermal insulation performance. The principle of EC technology is complex and difficult to implement in large-area applications. Efficient discoloration.

Method used

An electrochromic dimming structure is adopted, which includes a substrate, an electrochromic device and a protective layer. The electrochromic device is composed of a whole layer of light-transmitting electrode layer, an electrochromic layer and a metal electrode. The metal electrode is electrically connected to the electrode layer. Reduce the sheet resistance of the electrode and improve the speed and uniformity of color change.

Benefits of technology

It significantly improves the color-changing speed and uniformity of the electrochromic light-emitting structure, improves the experience of the color-changing canopy, and is suitable for canopy applications in new energy vehicles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118871852A_ABST
    Figure CN118871852A_ABST
Patent Text Reader

Abstract

The invention discloses an electrochromic dimming structure and traffic equipment. The electrochromic dimming structure comprises a substrate, an electrochromic device and a first protective layer. The electrochromic device is located on the substrate and comprises a first electrode layer, an electrochromic layer and a second electrode layer which are sequentially arranged in a stacked mode, the first electrode layer is located between the electrochromic layer and the substrate, and the first electrode layer and the second electrode layer are both whole-layer light-transmitting electrode layers. At least one of the first electrode layer and the second electrode layer comprises an oxide material; the first protective layer covers the electrochromic device. The electrochromic device further comprises a metal electrode which is located on at least one of the side, away from the second electrode layer, of the first electrode layer and the side, away from the first electrode layer, of the second electrode layer, and the metal electrode is electrically connected with at least one of the first electrode layer and the second electrode layer. By arranging the metal electrodes, the electrochromism speed and the electrochromism uniformity of the large-area electrochromism dimming structure are effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Electrochromic lighting structures and traffic equipment Technical Field

[0001] The embodiments of the present disclosure relate to an electrochromic light-emitting structure and traffic equipment. Background Art

[0002] Currently, electrochromic glass is widely used in automotive and aviation glass, as well as in building materials. Electrochromism is a phenomenon in which a material's optical properties (such as reflectivity, transmittance, and absorptivity) undergo a stable, reversible color change under the influence of an applied electric field. This phenomenon manifests itself as a reversible change in color and transparency. Materials exhibiting electrochromic properties are called electrochromic materials, and devices made with them are called electrochromic devices.

[0003] Summary of the Invention

[0004] The embodiments of the present disclosure provide an electrochromic light-emitting structure and a traffic device. The electrochromic light-emitting structure includes: a substrate, an electrochromic device, and a first protective layer. The electrochromic device is located on the substrate, and the electrochromic device includes a first electrode layer, an electrochromic layer, and a second electrode layer stacked in sequence, the first electrode layer is located between the electrochromic layer and the substrate, the first electrode layer and the second electrode layer are both whole light-transmitting electrode layers, and at least one of the first electrode layer and the second electrode layer includes an oxide material; the first protective layer covers the electrochromic device. The electrochromic device also includes a metal electrode located on at least one of a side of the first electrode layer away from the second electrode layer and a side of the second electrode layer away from the first electrode layer, and the metal electrode is electrically connected to at least one of the first electrode layer and the second electrode layer.

[0005] For example, according to an embodiment of the present disclosure, the metal electrode includes at least one of a metal grid electrode and a metal thin layer, and the thickness of the metal thin layer is 1 to 20 nanometers; along a direction perpendicular to the substrate, the metal electrode overlaps with the electrochromic layer.

[0006] For example, according to an embodiment of the present disclosure, the electrovariable dimming structure further includes: an antenna structure, which is arranged in the same layer as at least a portion of the metal electrode and is spaced apart from the antenna structure.

[0007] For example, according to an embodiment of the present disclosure, the metal electrode includes a first metal electrode and a second metal electrode, the first metal electrode is located on a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal electrode is located on a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; the antenna structure is arranged on the same layer as the first metal electrode, and the thickness of the antenna structure is greater than the thickness of the second metal electrode.

[0008] For example, according to an embodiment of the present disclosure, the first metal electrode includes a first metal grid electrode or a first metal thin layer, and the second metal electrode includes a second metal thin layer.

[0009] For example, according to an embodiment of the present disclosure, the metal grid electrode includes a first metal grid electrode and a second metal grid electrode, the first metal grid electrode is located on a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal grid electrode is located on a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; the overlap rate of the orthographic projection of the first metal grid electrode on the substrate and the orthographic projection of the second metal grid electrode on the substrate is greater than 90%; the antenna structure is arranged on the same layer as one of the first metal grid electrode and the second metal grid electrode.

[0010] For example, according to an embodiment of the present disclosure, at least 90% of the orthographic projection of the first electrode layer on the substrate overlaps with the orthographic projection of the metal thin layer on the substrate; the metal thin layer includes a first metal thin layer and a second metal thin layer, the first metal thin layer is located on a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal thin layer is located on a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; the antenna structure is arranged on the same layer as one of the first metal thin layer and the second metal thin layer.

[0011] For example, according to an embodiment of the present disclosure, the antenna structure includes a solid structure, and along a direction perpendicular to the substrate, the antenna structure does not overlap with the electrochromic layer.

[0012] For example, according to an embodiment of the present disclosure, the antenna structure includes a grid structure, and along a direction perpendicular to the substrate, the antenna structure overlaps or does not overlap with the electrochromic layer.

[0013] For example, according to an embodiment of the present disclosure, the antenna structure includes a main body portion, the main body portion is in the shape of an octagon, and the angle between at least two adjacent sides of the octagon is 135 degrees.

[0014] For example, according to an embodiment of the present disclosure, the antenna structure includes a main body portion, the main body portion includes the grid structure, the grid structure includes a first strip portion extending along a first direction and a second strip portion extending along a second direction, and the first direction intersects with the second direction.

[0015] For example, according to an embodiment of the present disclosure, the antenna structure includes a main body portion, the main body portion includes the grid structure, and the grid structure includes a plurality of strip portions arranged radially starting from a point in a central area of ​​the main body portion.

[0016] For example, according to an embodiment of the present disclosure, the thickness of the electrode layer electrically connected to the metal electrode in the first electrode layer and the second electrode layer is 10 nanometers to 10 micrometers.

[0017] For example, according to an embodiment of the present disclosure, the thickness of the metal grid electrode is 100 to 5000 nanometers, and the line width of the metal grid electrode is 1 to 5 micrometers.

[0018] For example, according to an embodiment of the present disclosure, the electrovariable dimming structure further includes: a second protective layer covering the second electrode layer. At least a portion of the second metal grid electrode and the antenna structure are located on a side of the second protective layer away from the substrate. The second protective layer includes a groove configured to expose the second electrode layer, and the second metal grid electrode is electrically connected to the second electrode layer through the groove. The second protective layer is further provided with an electrode portion on a side away from the second electrode layer, and the electrode portion is electrically connected to the second metal grid electrode. The first protective layer covers the second metal grid electrode and the antenna structure.

[0019] For example, according to an embodiment of the present disclosure, the antenna structure is arranged in the same layer as the first metal grid electrode, and the first protective layer covers the antenna structure; the first metal grid electrode includes two metal layers, and the material of the antenna structure is the same as the material of the metal layer of the two metal layers away from the substrate.

[0020] For example, according to an embodiment of the present disclosure, the second electrode layer includes a first film layer, a second film layer and a third film layer that are stacked, the first film layer and the third film layer are made of the same material, the thickness ratio of the first film layer to the third film layer is 0.9 to 1.1, and the thickness of the second film layer is less than the thickness of the first film layer.

[0021] For example, according to an embodiment of the present disclosure, the electrochromic layer includes an electrochromic material layer, an electrolyte layer, and a storage layer stacked in sequence, and the electrochromic material layer is located between the electrolyte layer and the first electrode layer.

[0022] For example, according to an embodiment of the present disclosure, the electrochromic material layer includes one of an inorganic electrochromic material and an organic electrochromic material, and the electrolyte layer includes one of a solid electrolyte and a liquid electrolyte.

[0023] The present disclosure provides a traffic device including a skylight, wherein the skylight includes any one of the above-mentioned electrochromic dimming structures. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings of the embodiments will be briefly introduced below. Obviously, the drawings in the following description only relate to some embodiments of the present disclosure, rather than limiting the present disclosure.

[0025] FIG1 is an electrochromic dimming structure.

[0026] FIG2 is a schematic diagram of a partial structure of an electrochromic dimming structure provided according to an example of an embodiment of the present disclosure.

[0027] 3 to 5 are schematic diagrams of planar structures of metal grid electrodes in different examples.

[0028] FIG. 6 is a light transmittance curve diagram of the metal grid electrode shown in FIG. 4 .

[0029] FIG. 7 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0030] FIG8 is a graph showing how the transmittance of the electrochromic dimming structure shown in FIG7 changes with wavelength.

[0031] 9 and 10 are schematic diagrams of electrochromic dimming structures provided according to different examples of the embodiments of the present disclosure.

[0032] FIG. 11 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0033] FIG12 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0034] FIG13 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0035] FIG. 14 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0036] 15 to 17 are planar structural diagrams of antenna structures in different examples according to embodiments of the present disclosure.

[0037] FIG18 is a gain comparison diagram of the antenna structures shown in FIG15 to FIG17 .

[0038] FIG19 is a gain diagram of the antenna structure shown in FIG15 in different radiation directions.

[0039] FIG20 is a gain diagram of the antenna structure shown in FIG16 in different radiation directions.

[0040] FIG21 is a gain diagram of the antenna structure shown in FIG17 in different radiation directions.

[0041] FIG. 22 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0042] FIG. 23 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure.

[0043] FIG24 is a schematic block diagram of a traffic device. DETAILED DESCRIPTION

[0044] To make the purpose, technical solutions, and advantages of the embodiments of the present disclosure more clear, the technical solutions of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the accompanying drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.

[0045] Unless otherwise defined, the technical or scientific terms used in this disclosure should have the ordinary meaning understood by a person of ordinary skill in the art to which this disclosure belongs. The terms "first," "second," and similar terms used in this disclosure do not indicate any order, quantity, or importance, but are simply used to distinguish different components. The terms "include" or "comprises" and similar terms mean that the element or object preceding the term includes the elements or objects listed after the term and their equivalents, without excluding other elements or objects. The characteristics of "parallel," "perpendicular," and "same" used in the embodiments of this disclosure include the characteristics of "parallel," "perpendicular," and "same" in the strict sense, as well as "approximately parallel," "approximately perpendicular," and "approximately the same" that include certain errors, taking into account the errors associated with the measurement of specific quantities (for example, the limitations of the measurement system), and represent the acceptable deviation range for a specific value determined by a person of ordinary skill in the art. For example, "approximately" can mean within one or more standard deviations, or within 10% or 5% of the stated value. When the number of a component is not specifically specified below in the embodiments of this disclosure, it means that the component can be one or more, or can be understood as at least one. "At least one" means one or more, and "a plurality" means at least two. The “same-layer arrangement” referred to in the present disclosure refers to a structure in which two (or more) structures are formed by the same deposition process and patterned by the same patterning process, and their materials may be the same or different.

[0046] Figure 1 shows an electrochromic dimming structure. As shown in Figure 1, the electrochromic dimming structure includes glass 1, an electrochromic device, and a protective layer 7 covering the electrochromic device. The electrochromic device includes a lower electrode 2, a color-changing layer 3, an electrolyte layer 4, an ion storage layer 5, and an upper electrode 6, which are stacked in sequence. The lower electrode 2 and the upper electrode 6 are both transparent conductive films that form the entire layer of the electrochromic device, such as indium tin oxide (ITO). The color-changing layer is the core layer of the electrochromic device and is also the layer where the color change reaction occurs. The material of the color-changing layer can be divided into inorganic electrochromic materials and organic electrochromic materials according to type.

[0047] New energy vehicles are attracting significant attention as a new economic growth driver. However, battery range has become a major constraint on interior space design, making mechanically opening and panoramic sunroofs difficult to adopt in new energy vehicles. Consequently, color-changing skylights are increasingly being adopted in new energy vehicles.

[0048] Currently, color-changing skylights primarily utilize electrochromic (EC) technology, polymer dispersed liquid crystals (PDLC) technology, and suspended particle devices (SPD) technology. PDLC and SPD are physical dimming technologies, while EC utilizes electrochemical dimming. PDLC skylights primarily switch between transparent and fogged states by altering the arrangement of liquid crystal molecules within the glass. For example, upon power failure, ordinary PDLC glass immediately transforms to a fogged state and does not maintain its high light transmittance. Furthermore, its thermal insulation performance is inferior. SPD skylights incorporate suspended particles within the glass interlayer. When power is lost, the Brownian motion of these particles randomly arranges them, allowing them to absorb over 99% of visible light. These skylights are power-hungry, requiring a 110V voltage to operate. They return to a dark state upon power failure, have a maximum operating temperature of 60°C, and are more expensive. EC technology works by allowing ions to pass through the electrolyte layer and enter the electrochromic layer, where they react with the materials within the layer to produce a chemical reaction, resulting in the glass's color change.

[0049] During the research, the inventors of this application discovered that the color-changing skylight includes the electrochromic dimming structure shown in Figure 1. Since at least one of the upper electrode and the lower electrode of the electrochromic dimming structure adopts indium tin oxide (ITO), whose square resistance is 50 ohms / square, the color-changing speed of the dimming screen using the electrochromic dimming structure is slow. For example, it takes several minutes to adjust the dimming screen from high transmittance to low transmittance, and the larger the area of ​​the dimming screen, the slower the color-changing speed of the dimming screen, thereby greatly reducing the experience of the color-changing skylight.

[0050] The present disclosure provides an electrochromic light-emitting structure and a traffic device. The electrochromic light-emitting structure includes a substrate, an electrochromic device, and a first protective layer. The electrochromic device is located on the substrate, and the electrochromic device includes a first electrode layer, an electrochromic layer, and a second electrode layer stacked in sequence. The first electrode layer is located between the electrochromic layer and the substrate. The first electrode layer and the second electrode layer are both whole light-transmitting electrode layers, and at least one of the first electrode layer and the second electrode layer includes an oxide material; the first protective layer covers the electrochromic device. The electrochromic device also includes a metal electrode located on at least one of a side of the first electrode layer away from the second electrode layer and a side of the second electrode layer away from the first electrode layer, and the metal electrode is electrically connected to at least one of the first electrode layer and the second electrode layer.

[0051] The electrochromic dimming structure provided by the present invention greatly reduces the overall square resistance of at least one of the first electrode layer and the second electrode layer by providing a metal electrode electrically connected to at least one of the first electrode layer and the second electrode layer, effectively improving the electrochromic speed and color change uniformity of the large-area electrochromic dimming structure. When the electrochromic dimming structure is applied to a color-changing skylight, it is beneficial to improve the experience effect of the color-changing skylight.

[0052] The electrochromic light-emitting structure and traffic equipment provided by the present disclosure are described below with reference to the accompanying drawings.

[0053] FIG2 is a partial structural diagram of an electrochromic light-emitting structure according to an example of an embodiment of the present disclosure. As shown in FIG2 , the electrochromic light-emitting structure includes a substrate 100 , an electrochromic device 200 , and a first protective layer 300 .

[0054] For example, as shown in FIG. 2 , the substrate 100 may include a light-transmitting material such as glass.

[0055] As shown in Figure 2, the electrochromic device 200 is located on the substrate 100. The electrochromic device 200 includes a first electrode layer 210, an electrochromic layer 230 and a second electrode layer 220 stacked in sequence. The first electrode layer 210 is located between the electrochromic layer 230 and the substrate 100. The first electrode layer 210 and the second electrode layer 220 are both whole-layer light-transmitting electrode layers. At least one of the first electrode layer 210 and the second electrode layer 220 includes an oxide material.

[0056] For example, the material of the first electrode layer 210 may include indium tin oxide (ITO), fluorine-doped tin dioxide (FTO), etc. For example, the material of the second electrode layer 220 may be the same as that of the first electrode layer 210. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 10 nanometers to 10 micrometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 15 to 800 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 20 to 500 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 25 to 400 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 30 to 300 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 40 to 200 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 50 to 100 nanometers. For example, the thickness of the first electrode layer 210 and the second electrode layer 220 may be 60 to 90 nanometers. When the first electrode layer and the second electrode layer are made of oxide materials, it is beneficial to minimize the impact of the first electrode layer and the second electrode layer on the electrochromic layer.

[0057] For example, the first electrode layer 210 and the second electrode layer 220 may also be formed of thin metal layers, and the thickness of the thin metal layers may be less than 50 nanometers. For example, the material of the thin metal layers may include gold (Au), copper (Cu), silver (Ag), nickel (Ni), chromium (Cr), molybdenum (Mo), and aluminum (Al).

[0058] In some examples, as shown in FIG2 , the electrochromic layer 230 includes an electrochromic material layer 231, an electrolyte layer 232, and a storage layer 233, which are sequentially stacked. The electrochromic material layer 231 is located between the electrolyte layer 232 and the first electrode layer 210. For example, the electrochromic material layer 231 may be made of a cathode-discoloring material, and the storage layer 233 may be made of an anode-discoloring material.

[0059] In some examples, as shown in FIG. 2 , the material of the electrochromic material layer 231 may include an inorganic electrochromic material and an organic electrochromic material.

[0060] For example, organic electrochromic materials include polyaniline and its derivatives, polypyrrole and its derivatives, polythiophene and its derivatives, viologens, tetrathiafulvalene, metal phthalocyanine compounds, and the like.

[0061] For example, inorganic electrochromic materials include tungsten trioxide (WO3), titanium dioxide (TiO2), niobium pentoxide (Nb2O5), molybdenum trioxide (MoO3), tantalum pentoxide (Ta2O5), etc. For example, when the electrochromic material layer 231 is made of tungsten trioxide (WO3), its electrochromic mechanism can be the injection and extraction of electrons and ions.

[0062] For example, tungsten trioxide (WO3) can be prepared by reactive sputtering, during which the flow ratio of argon (Ar) and oxygen (O2) can be 1:1, the working power can be 100W, and the thickness of the prepared electrochromic material layer 231 can be 300 nanometers.

[0063] In some examples, as shown in FIG2 , the material of the electrolyte layer 232 includes at least one of a fully solid polymer electrolyte, a gel polymer electrolyte, and a composite polymer electrolyte. For example, a variety of high molecular weight polymer materials are used in the preparation of polymer electrolytes, among which the most representative polymer electrolyte matrix materials include polyether (mainly PEO), polyacrylonitrile (PAN), polyvinylidene fluoride (PVdF), and polymethyl methacrylate (PMMA).

[0064] For example, solid-state electrolytes include lithium phosphorus oxynitride (LiPON), lithium phosphorus silicon oxynitride (LiSiPON), lithium lanthanum zirconium oxide (LLZO), lithium lanthanum titanate (LLTO), tantalum-doped lithium lanthanum zirconium oxide (LLZTO), lithium polymer (LiPO), tantalum pentoxide (Ta2O5), lithium niobate (LiNbO3), lithium tantalate (LiTaO3), silicon oxide (SiO2), etc.

[0065] For example, during the preparation of lithium phosphorus oxynitride (LiPON), nitrogen (N2) may be introduced with a volume flow rate of 60 sccm, a working power of 100 W, and a thickness of the formed electrolyte layer of 300 nanometers.

[0066] For example, the material of the storage layer 233 includes nickel oxide (NiO), iridium oxide (IrO2), manganese dioxide (MnO2), cobalt oxide (Co3O4), etc. For example, the storage layer 233 can be called a counter electrode. For example, the storage layer 233 can store ions and balance charges.

[0067] For example, nickel oxide (NiO) can be prepared by reactive sputtering, during which the flow ratio of argon (Ar) and oxygen (O2) can be 8:1, the working power can be 100W, and the thickness of the prepared electrochromic material layer 231 can be 300 nanometers.

[0068] For example, the electrochromic material layer 231 and the storage layer 233 may be prepared by a sol-gel method, screen printing, doctor blade coating, slit coating, or injection molding method to form a colloidal film layer.

[0069] For example, inorganic electrochromic materials can be divided into cathode and anode coloring materials based on their coloring properties. For example, oxides containing tungsten (W), molybdenum (Mo), niobium (Nb), tantalum (Ta), and titanium (Ti) are cathode coloring materials. Anodic electrochromic materials are primarily Group VIII transition metal oxides, such as nickel (Ni), cobalt (Co), manganese (Mn), and iridium (Ir), as well as their hydrated oxides. These materials fade when reduced and become colored when oxidized. The Prussian blue system is also an anodic coloring material. Materials that exhibit dual coloration in both oxidized and reduced states, such as vanadium pentoxide (V2O5), rhodium oxide (Rh2O3), and CoOx, are also anodic coloring materials.

[0070] For example, as shown in FIG2 , the surface of the first electrode layer 210 contacts the surface of the electrochromic material layer 231, the surface of the electrochromic material layer 231 contacts the surface of the electrolyte layer 232, the surface of the electrolyte layer 232 contacts the surface of the storage layer 233, and the surface of the storage layer 233 contacts the surface of the second electrode layer 220. When a voltage is applied between the first electrode layer 210 and the second electrode layer 220 to generate a voltage difference, ions in the storage layer 233 pass through the electrolyte layer 232 and enter the electrochromic material layer 231, where they combine with substances in the electrochromic material layer 231 to produce a chemical reaction, causing the color of the electrochromic material layer 231 to change and its transparency to decrease. When there is no voltage difference between the first electrode layer 210 and the second electrode layer 220, the ions are extracted from the electrochromic material layer 231 and return to the storage layer, causing the electrochromic material layer 231 to return to a transparent state.

[0071] As shown in FIG2 , in the electrochromic dimming structure, the first protective layer 300 covers the electrochromic device 200. For example, the first protective layer 300 covers the surface of the electrochromic device 200 away from the substrate 100 and the side surface of the electrochromic device 200. The first protective layer 300 wraps the electrochromic device 200 to protect it.

[0072] For example, the first protection layer 300 may be composed of a single layer or a stack of layers of lithium phosphorus oxynitride (LiPON), polydimethylsiloxane (PDMS), silicon nitride (SiN), silicon oxynitride (SiON), silicon oxide (SiO), etc.

[0073] As shown in Figure 2, the electrochromic device 200 also includes a metal electrode 240, which is located on at least one of the side of the first electrode layer 210 away from the second electrode layer 220 and the side of the second electrode layer 220 away from the first electrode layer 210, and the metal electrode 240 is electrically connected to at least one of the first electrode layer 210 and the second electrode layer 220.

[0074] In some examples, as shown in FIG2 , the thickness of the electrode layer electrically connected to the metal electrode 240 in the first electrode layer 210 and the second electrode layer 220 is no greater than 100 nanometers. For example, the thickness of the electrode layer is no greater than 90 nanometers. For example, the thickness of the electrode layer is no greater than 80 nanometers.

[0075] The electrochromic dimming structure provided by the present disclosure can greatly reduce the resistance of the first electrode layer and / or the second electrode layer and the metal electrode as a whole electrode by providing a metal electrode electrically connected to at least one of the first electrode layer and the second electrode layer in the electrochromic device, thereby effectively improving the electrochromic speed of the large-area electrochromic dimming structure. Therefore, when the electrochromic dimming structure is applied to a color-changing sky curtain, it is beneficial to improve the experience effect of the color-changing sky curtain.

[0076] In addition, by providing an oxide electrode layer and a metal electrode together as electrodes of the electrochromic dimming structure, it is possible to prevent the metal electrode from directly contacting the electrochromic layer and affecting the performance of the electrochromic layer, and it is also possible to reduce the thickness of the electrode layer. Thus, while reducing the overall resistance of the electrode as the electrochromic dimming structure, the electrochromic dimming structure will not have a larger thickness or affect the performance of the electrochromic layer due to the addition of the metal electrode.

[0077] 3 to 5 are schematic diagrams of planar structures of metal grid electrodes in different examples.

[0078] In some examples, as shown in FIG. 2 to FIG. 5 , the metal electrode 240 includes a metal grid electrode 241 , and the metal grid electrode 241 overlaps the electrochromic layer 230 along a direction perpendicular to the substrate 100 (the Y direction shown in FIG. 2 ).

[0079] For example, the material of the metal grid electrode 241 can be gold (Au), platinum (Pt), copper (Cu), molybdenum (Mo), silver (Ag), aluminum (Al), etc.

[0080] For example, as shown in Figures 3 to 5 , the metal grid electrode 241 includes a hollow region 242 , which can be uniformly arranged. For example, the pattern of the hollow region 242 can include regular patterns such as polygons, circles, and ovals, or can include other irregular shapes, such as wavy patterns. For example, polygons can include triangles, quadrilaterals, pentagons, hexagons, octagons, and the like.

[0081] In some examples, as shown in Figures 2 to 5 , the thickness of the metal grid electrode 241 is 100 to 5000 nanometers, and the line width of the metal grid electrode 241 is 1 to 5 micrometers. For example, the metal grid electrode includes a plurality of strip electrodes, and the distance between adjacent strip electrodes is greater than 1 micrometer. For example, the distance between adjacent strip electrodes is greater than 2 micrometers.

[0082] For example, when the line width of the metal grid electrode 241 is relatively wide, such as 2 to 5 microns, the line width will not be comparable to the wavelength, and thus no interference fringes will be generated. For example, when the line width of the metal grid electrode 241 is relatively narrow, such as 1 micron, and the spacing between the metal grid electrodes 241 is large, such as greater than 1 micron, no interference will be generated.

[0083] For example, the thickness of the metal grid electrode 241 is 150 to 1000 nanometers. For example, the thickness of the metal grid electrode 241 is 400 to 900 nanometers. For example, the thickness of the metal grid electrode 241 is 400 to 900 nanometers. For example, the thickness of the metal grid electrode 241 is 500 to 800 nanometers. For example, the thickness of the metal grid electrode 241 is 200 to 300 nanometers.

[0084] For example, the line width of the metal grid electrode 241 is 1.5 to 4.5 micrometers. For example, the line width of the metal grid electrode 241 is 2.5 to 3.5 micrometers. For example, the line width of the metal grid electrode 241 is 2 to 3 micrometers.

[0085] In the electrochromic material layer shown in Figure 1, when the first electrode layer and the second electrode layer are not electrically connected to the metal electrode, the square resistance of the first electrode layer and the second electrode layer is 50 ohms / square; in the electrochromic dimming structure provided in the present application, at least one of the first electrode layer and the second electrode layer is electrically connected to the metal electrode, such as forming the electrochromic dimming structure shown in Figure 2. By setting the metal electrode, the square resistance of the electrode layer and the electrode jointly formed by the metal electrode can be significantly reduced, such as not more than 10 ohms / square, thereby effectively improving the electrochromic speed of the large-area electrochromic dimming structure.

[0086] FIG6 is a graph showing the transmittance of the metal grid electrode shown in FIG4 . For example, the line width of the metal grid electrode 241 shown in FIG4 can be 5 microns. For example, as shown in FIG4 and FIG6 , the transmittance of the metal grid electrode 241 is not less than 90% in the visible light band. For example, the transmittance of the metal grid electrode 241 is not less than 91%. For example, the transmittance of the metal grid electrode 241 is not less than 92%. For example, the transmittance of the metal grid electrode 241 is not less than 93%. For example, the above transmittance refers to the average transmittance of the entire metal grid electrode, which is related to the line width of the metal grid electrode.

[0087] By setting the line width of the metal grid electrode, the transmittance of the metal grid electrode to light can be improved, such as not less than 90%. The metal grid electrode can be regarded as a transparent electrode, so as to reduce the resistance of the electrode of the electrochromic dimming structure while minimizing the impact on the light transmission effect of the electrode.

[0088] Figure 2 schematically shows that the surface of the first electrode layer 210 away from the metal grid electrode is flat. In actual products, since a metal grid electrode is provided between the first electrode layer 210 and the substrate 100, the surface of the first electrode layer 210 away from the metal grid electrode will have a protrusion corresponding to the metal grid electrode. The electrochromic dimming structure provided in the present application, by setting the thickness of the metal grid electrode to be thinner, is conducive to reducing the height of the protrusion of the first electrode layer away from the substrate, which is conducive to preventing the protrusion from affecting the performance of the electrochromic layer.

[0089] FIG2 schematically shows that the metal grid electrode is located between the first electrode layer and the substrate, but the present invention is not limited thereto. The metal grid electrode may also be located on a side of the second electrode layer away from the substrate.

[0090] FIG7 is a schematic diagram of an electrovariable dimming structure according to another example of an embodiment of the present disclosure. As shown in FIG7 , the metal grid electrode 241 includes a first metal grid electrode 2411 and a second metal grid electrode 2412. The first metal grid electrode 2411 is located on a side of the first electrode layer 210 away from the second electrode layer 220 and is electrically connected to the first electrode layer 210. The second metal grid electrode 2412 is located on a side of the second electrode layer 220 away from the first electrode layer 210 and is electrically connected to the second electrode layer 220. The first electrode layer 210 and the first metal grid electrode 2411 together serve as electrodes on one side of the electrovariable dimming structure, while the second electrode layer 220 and the second metal grid electrode 2412 together serve as electrodes on the other side of the electrovariable dimming structure.

[0091] By providing a first metal grid electrode electrically connected to the first electrode layer and a second metal grid electrode electrically connected to the second electrode layer, the resistance of the electrodes on both sides of the electrochromic dimming structure can be greatly reduced, effectively improving the electrochromic speed of the large-area electrochromic dimming structure.

[0092] For example, the power supply for applying voltage to the electrochromic light may be directly connected to the metal grid electrode, but not limited thereto, the power supply for applying voltage to the electrochromic light may also be directly connected to the first electrode layer and the second electrode layer.

[0093] In some examples, as shown in FIG7 , the overlap rate of the orthographic projection of the first metal grid electrode 2411 on the substrate 100 and the orthographic projection of the second metal grid electrode 2412 on the substrate 100 is greater than 90%. For example, the overlap rate of the orthographic projection of the first metal grid electrode 2411 on the substrate 100 and the orthographic projection of the second metal grid electrode 2412 on the substrate 100 is greater than 92%. For example, the overlap rate of the orthographic projection of the first metal grid electrode 2411 on the substrate 100 and the orthographic projection of the second metal grid electrode 2412 on the substrate 100 is greater than 95%. For example, the overlap rate of the orthographic projection of the first metal grid electrode 2411 on the substrate 100 and the orthographic projection of the second metal grid electrode 2412 on the substrate 100 is greater than 98%. For example, the orthographic projection of the first metal grid electrode 2411 on the substrate 100 and the orthographic projection of the second metal grid electrode 2412 on the substrate 100 completely overlap.

[0094] The arrangement of the orthographic overlapping relationship between the first metal grid electrode and the second metal grid electrode on the substrate is beneficial for improving the light transmittance of the electrode of the electrovariable dimming structure.

[0095] For example, as shown in FIG. 7 , the material of the second metal grid electrode 2412 may be the same as that of the first metal grid electrode 2411 , such as gold (Au), platinum (Pt), copper (Cu), molybdenum (Mo), silver (Ag), aluminum (Al), etc.

[0096] 7 , the second metal grid electrode 2412 and the first metal grid electrode 2411 may have the same thickness, such as 100 to 5000 nanometers. For example, the thickness of the first metal grid electrode 2411 and the second metal grid electrode 2412 may both be 1 micrometer.

[0097] 7 , the line width of the second metal grid electrode 2412 and the first metal grid electrode 2411 may be the same, such as 1 to 5 microns. For example, the line width of the first metal grid electrode 2411 and the second metal grid electrode 2412 may both be 3 microns.

[0098] For example, as shown in FIG. 7 , metal grid electrodes, such as the first metal grid electrode 2411 and the second metal grid electrode 2412 , may be deposited by using a DC magnetron sputtering method and patterned as needed.

[0099] For example, as shown in FIG7 , a high-precision exposure machine can be used to pattern the first metal grid electrode 2411 and the second metal grid electrode 2412 to set the line width of the metal grid electrode as small as possible, such as less than 3 microns, such as 2 microns, such as 1 micron, which helps to further reduce the visual presence of the metal grid electrode.

[0100] Figure 8 shows the variation of light transmittance of the electrovariable dimming structure shown in Figure 7 with wavelength. As shown in Figure 8 , when the electrovariable dimming structure is in a nearly transparent state, such as the faded state, the transmittance of light with a wavelength of 550 nanometers is approximately 64.0%. When the electrovariable dimming structure is in a color-changing state, such as the tinted state, the transmittance of light with a wavelength of 550 nanometers is approximately 15.2%. Therefore, the modulation degree of the electrovariable dimming structure for light with a wavelength of 550 nanometers is 48.8%.

[0101] Figures 9 and 10 are schematic diagrams of electrochromic dimming structures according to different examples of the present disclosure. The difference between the electrochromic dimming structure shown in Figure 9 and the electrochromic dimming structure shown in Figure 10 lies in whether the limiting structure 023 is provided.

[0102] For example, as shown in Figures 9 and 10, the first metal grid electrode 2411 includes two metal layers, such as metal layer 021 and metal layer 022. For example, metal layer 022 can be an electroplating seed layer that can be patterned into a metal grid structure; metal layer 021 can be a film layer grown on metal layer 022 using electroplating. For example, the material of metal layer 021 can be molybdenum, and the material of metal layer 022 can be copper. For example, the thickness of metal layer 022 can be 300 nanometers, and the thickness of metal layer 021 can be greater than 1 micron. Electroplating can form metal grid electrodes with a relatively thick thickness (e.g., 1 to 100 microns, such as 2 to 5 microns, such as 3 to 4 microns) at a low cost.

[0103] For example, as shown in FIG10 , the hollow region 242 of the first metal grid electrode 2411 is provided with a defining structure 023 for defining the thickness of the metal layer 022. For example, the defining structure 023 can be made of a transparent organic material, such as polyimide (PI) or acrylic adhesive. For example, the defining structure 023 can also be made of a transparent inorganic material, such as silicon oxide or silicon nitride. For example, the thickness of the defining structure 023 can be 1.5 to 2.5 microns. For example, the thickness of the defining structure 023 can be 2 microns.

[0104] For example, after forming the definition structure 023 , the definition structure 023 and the metal layer 023 may be placed in an electroplating solution to electroplate the metal layer 022 .

[0105] Figure 11 is a schematic diagram of an electrochromic dimming structure according to another embodiment of the present disclosure. The other structures of the electrochromic dimming structure shown in Figure 11, except for the second electrode layer, may have the same features as the corresponding structures in the above examples, and will not be described in detail here.

[0106] In some examples, as shown in Figure 11, the second electrode layer 220 includes a first film layer 221, a second film layer 222 and a third film layer 223 that are stacked together. The first film layer 221 and the third film layer 223 are made of the same material, the thickness ratio of the first film layer 221 to the third film layer 223 is 0.9 to 1.1, and the thickness of the second film layer 222 is less than the thickness of the first film layer 221.

[0107] For example, the first film layer 221 and the third film layer 223 have the same thickness. For example, the material of the first film layer 221 and the third film layer 223 can be aluminum-doped zinc oxide (AZO), and the material of the second film layer 222 can be silver (Ag). For example, the material of the first film layer 221 and the third film layer 223 can be indium tin oxide (ITO), and the material of the second film layer 222 can be silver (Ag).

[0108] For example, the thickness of the first film layer 221 and the third film layer 223 may both be 50 nanometers, and the thickness of the second film layer 222 may be 30 nanometers. For example, the second electrode layer 220 may have a sandwich structure including a thin silver layer.

[0109] By utilizing the optical microcavity effect, the heating effect of the infrared band of the solar spectrum energy on the electrochromic light-emitting structure is reduced, which is beneficial to improving the reliability and cycle characteristics of the electrochromic light-emitting structure.

[0110] FIG12 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure. The electrochromic dimming structure shown in FIG12 differs from the electrochromic dimming structure shown in FIG7 in that the electrochromic dimming structure shown in FIG12 further includes an antenna structure 400 disposed in the same layer as at least a portion of the metal electrode and spaced apart therefrom. The substrate 100, first electrode layer 210, second electrode layer 220, electrochromic layer 230, and first protective layer 300 in the electrochromic dimming structure shown in FIG12 may have the same features as the corresponding structures in any of the examples shown in FIG2 through FIG11 and are not further described herein.

[0111] The electrochromic light-emitting structure provided by the present disclosure utilizes an antenna structure disposed on at least a portion of the same layer as the metal electrode. This reduces the resistance of the electrodes in the electrochromic device, effectively increasing the electrochromic speed of the large-area electrochromic light-emitting structure while enabling the reception and transmission of microwave signals without adding additional film layers. For example, the antenna structure can be used for satellite communications. For example, the antenna structure can enable the transmission and reception of microwave signals for 4G and 5G networks.

[0112] For example, Figure 12 schematically shows that the metal grid electrode 241 includes a first metal grid electrode 2411 and a second metal grid electrode 2412, but is not limited to this. The metal grid electrode 241 may also include only one layer of structure, such as only one layer of grid electrode electrically connected to the first electrode layer, or only one layer of grid electrode electrically connected to the second electrode layer.

[0113] In some examples, as shown in FIG. 12 , the antenna structure 400 is disposed in the same layer as one of the first metal grid electrode 2411 and the second metal grid electrode 2412 .

[0114] In some examples, as shown in FIG12 , the antenna structure 400 is disposed in the same layer as the first metal grid electrode 2411, and the first protective layer 300 covers the antenna structure 400. The first protective layer is used to protect the antenna structure.

[0115] In some examples, as shown in FIG. 12 , the shape of the antenna structure 400 is the same as the shape of at least a portion of the metal grid electrode 241 , and the antenna structure 400 may overlap or not overlap the electrochromic layer 230 along a direction perpendicular to the substrate 100 .

[0116] 12 , the antenna structure 400 and the first metal grid electrode 2411 can be formed in the same patterning process, and the antenna structure 400 is shaped like a metal grid. For example, the antenna structure 400 and the first metal grid electrode 2411 can have the same material, thickness, and line width.

[0117] Figure 12 schematically shows that the antenna structure and the electrochromic layer do not overlap to reduce mutual interference between the electrochromic device and the antenna structure. When the electrochromic dimming structure is applied to the sunroof of transportation equipment, the antenna structure can be stuck in the groove, which is a groove for locking the edge of the sunroof.

[0118] Of course, the embodiments of the present disclosure are not limited to this. The antenna structure having the same shape as that of at least part of the metal grid electrode can be overlapped with the electrochromic layer. Since the antenna structure has good light transmittance, overlapping the electrochromic layer and the antenna structure can help increase the area of ​​the electrochromic device.

[0119] FIG13 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure. The electrochromic dimming structure shown in FIG13 differs from the electrochromic dimming structure shown in FIG10 in that the electrochromic dimming structure shown in FIG13 further includes an antenna structure 400 disposed in the same layer as the metal grid electrode and spaced apart. The substrate 100, first electrode layer 210, second electrode layer 220, electrochromic layer 230, and first protective layer 300 in the electrochromic dimming structure shown in FIG13 may have the same features as the corresponding structures in any of the examples shown in FIG2 to FIG11, and will not be described in detail here. For example, as shown in FIG13, the first protective layer 300 covers the antenna structure 400.

[0120] In some examples, as shown in FIG13 , first metal grid electrode 2411 includes two metal layers 021 and 022, and the material of antenna structure 400 is the same as the material of metal layer 021, one of the two metal layers 021 and 022, which is farther from substrate 100. Antenna structure 400 shown in FIG13 may have the same features as antenna structure 400 shown in FIG12 , and further description thereof is omitted.

[0121] FIG14 is a schematic diagram of an electrochromic dimming structure provided according to another example of an embodiment of the present disclosure. The electrochromic dimming structure shown in FIG14 differs from the electrochromic dimming structure shown in FIG7 in that the electrochromic dimming structure shown in FIG14 further includes an antenna structure 400 disposed in the same layer as the metal grid electrode and spaced apart. For example, the number of antenna structures 400 can be 1, 2, or more. The substrate 100, first electrode layer 210, second electrode layer 220, and electrochromic layer 230 in the electrochromic dimming structure shown in FIG12 can have the same features as the corresponding structures in any of the examples shown in FIG2 to FIG11, and will not be repeated here.

[0122] In some examples, as shown in FIG14 , the electrochromic dimming structure further includes a second protective layer 600 covering the second electrode layer 220. For example, the second protective layer 600 may cover the surface of the second electrode layer 220 away from the substrate 100, the electrochromic layer 230, and the side surface of the first electrode layer 210. For example, the second protective layer 600 may be made of the same material as the first protective layer 300, such as silicon dioxide. For example, the thickness of the portion of the second protective layer 600 located on the side of the second electrode layer 220 away from the substrate 100 may be 80 to 120 nanometers. For example, the thickness of the portion of the second protective layer 600 located on the side of the second electrode layer 220 away from the substrate 100 may be 100 nanometers.

[0123] In some examples, as shown in FIG14 , at least a portion of the second metal grid electrode 2412 and the antenna structure 400 are located on a side of the second protective layer 600 away from the substrate 100. The second protective layer 600 includes a groove 610 configured to expose the second electrode layer 220. The second metal grid electrode 2412 is electrically connected to the second electrode layer 220 through the groove 610. For example, the second protective layer 600 can be dry-etched using a reactive ion etching (RIE) or inductively coupled plasma (ICP) device to pattern the grid-shaped grooves 610. For example, the shape of the grooves 610 can be the same as that of the second metal grid electrode 2412.

[0124] In some examples, as shown in FIG14 , an electrode portion 500 is further provided on a side of the second protective layer 600 away from the second electrode layer 220 . The electrode portion 500 is electrically connected to the second metal mesh electrode 2412 . For example, the electrode portion 500 may include a first electrode portion 510 and a second electrode portion 520 . By applying different voltages to the first electrode portion 510 and the second electrode portion 520 to form a voltage difference, the second metal mesh electrode 2412 generates heat when the voltage is applied by the electrode portion 500 . This can, for example, de-ice or defog the electro-variable dimming structure. For example, when the electro-variable dimming structure is used in a sunroof of transportation equipment, applying a voltage to the second metal mesh electrode through the electrode portion causes the second metal mesh electrode to function as a heater, thereby promoting snow melting in winter, evaporating water film on the sunroof, and defogging.

[0125] For example, as shown in Figure 14, when the electrochromic dimming structure is used for dimming, only one electrode portion in the electrode portion 500 is configured to apply a voltage to the second metal grid electrode 2412 to achieve color change of the electrochromic layer; when the second metal grid electrode 2412 is used for heating, a voltage is applied to both electrode portions in the electrode portion 500, while no voltage is applied to the first metal grid electrode 2411. At this time, the electrochromic dimming structure does not work.

[0126] In some examples, as shown in FIG. 14 , the first protection layer 300 covers the second metal grid electrode 2412 and the antenna structure 400 to protect the electrochromic device and the antenna structure.

[0127] Figures 15 to 17 are planar structural diagrams of the antenna structure provided according to the embodiments of the present disclosure in different examples, Figure 18 is a gain comparison diagram of the antenna structures shown in Figures 15 to 17, Figure 19 is a gain diagram of the antenna structure shown in Figure 15 in different radiation directions, Figure 20 is a gain diagram of the antenna structure shown in Figure 16 in different radiation directions, and Figure 21 is a gain diagram of the antenna structure shown in Figure 17 in different radiation directions.

[0128] Any antenna structure in the examples shown in FIG. 15 to FIG. 17 can be applied to the antenna structure in the electrovariable dimming structure shown in FIG. 12 to FIG. 14 .

[0129] In some examples, the metal electrode includes a first metal electrode and a second metal electrode, the first metal electrode is located on a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal electrode is located on a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; the antenna structure is arranged in the same layer as the first metal electrode, and the thickness of the antenna structure is greater than the thickness of the second metal electrode.

[0130] In some examples, the first metal electrode includes a first metal mesh electrode or a first metal thin layer, and the second metal electrode includes a second metal thin layer.

[0131] In some examples, as shown in Figures 12 to 15 , the antenna structure 400 comprises a solid structure, and in a direction perpendicular to the substrate 100, the antenna structure 400 does not overlap with the electrochromic layer 230. For example, the antenna structure 400 may have a polygonal outline, where the solid structure refers to the portion of the antenna structure 400 surrounded by the polygonal outline being a solid structure and not hollowed out.

[0132] For example, as shown in Figures 12 to 15, the shape of the antenna structure 400 can be different from the shape of the metal grid electrode provided in the same layer. For example, in the direction parallel to the line width of the metal grid electrode, the size of the antenna structure 400 is larger than the line width of the metal grid electrode. For example, the size of the octagon along the V direction can be 2 to 3 mm, such as 2.3 mm. For example, the size of the octagon along the V direction determines the range of the resonant frequency and gain. For example, at this size, it resonates around 28 GHz and the highest gain is at 27 GHz. For example, the resonant frequency and gain range of the antenna structure will change as the size of the octagon changes.

[0133] In some examples, as shown in FIG15 , antenna structure 400 includes a main body 401 having an octagonal shape, wherein the angle between at least two adjacent sides of the octagon is 135 degrees. For example, main body 401 is the portion that transmits and receives microwave signals. For example, the two adjacent sides are directly connected.

[0134] For example, when the antenna structure is rectangular, the electrical length of radiation is the distance between the top and bottom edges (assuming the bottom edge of the rectangle is connected to the feeder and the top and bottom edges are perpendicular to the feeder). Therefore, the current can only oscillate within a fixed electrical length, thus generating radiation. The left and right edges of the rectangle (the left and right edges are parallel to the feeder) do not participate in radiation. For example, the antenna structure can be a microstrip transmission line, where the ratio of its physical length to the wavelength of the transmitted electromagnetic wave is the electrical length. For example, when the antenna structure is octagonal, due to the presence of hypotenuses, such as those with a 135-degree angle, the electrical length is not constant. Only the edges parallel to the feeder do not participate in radiation (the resulting current oscillation is very small and can be ignored). The other edges perpendicular to the feeder or at a certain angle can participate in radiation. Therefore, the electrical length varies. Compared to a structure with a constant electrical length, the octagon has more edges participating in radiation, and the electrical length varies to a certain extent. Therefore, its radiation gain is slightly increased compared to the rectangular structure. For example, the bandwidth of a rectangular structure is generally 10% of the center frequency, while that of an octagon can be extended to 10%-20%. The bandwidth of high frequency bands (especially millimeter waves) determines their transmission capacity, so high frequency antennas are generally required to be broadband or ultra-wideband.

[0135] For example, taking the V direction shown in FIG15 as a reference direction, the extension direction of one of the two adjacent sides is parallel or perpendicular to the V direction, and the angle between the extension direction of the other side and the V direction is +45 degrees or -45 degrees. For example, as shown in FIG15, the octagon includes two sides, the angle between the extension direction of one of the two sides and the V direction is +45 degrees, and the angle between the extension direction of the other of the two sides and the V direction is -45 degrees. For example, the antenna structure adopts dual-polarization antenna technology, which combines antennas with mutually orthogonal polarization directions of +45 degrees and -45 degrees and operates in transmit and receive duplex mode at the same time, thereby saving the number of antennas.

[0136] The main body of the antenna structure provided in the embodiment of the present disclosure adopts an octagonal outline, and the sides of the octagonal outline can resonate. The octagonal antenna structure has more resonant sides, which is beneficial to maximizing the gain while achieving the miniaturization of the antenna structure; and setting the angle between at least two adjacent sides of the octagon to 135 degrees is beneficial to increasing the bandwidth and is suitable for high-frequency requirements.

[0137] Of course, the embodiments of the present disclosure are not limited thereto, and the main body of the antenna structure may also be in the shape of a quadrilateral, such as a rectangle or square, or a hexagon or other polygon.

[0138] For example, as shown in FIG15 , the antenna structure 400 further includes two electrode portions 402 electrically connected to the main portion 401. For example, the two electrode portions 402 are configured to receive different electrical signals. For example, the electrode portions 402 and the main portion 401 may be integrally provided. For example, the two electrode portions 402 may be respectively connected to two inclined sides of an octagon.

[0139] For example, as shown in Figure 15 , the end of the electrode portion 402 away from the main body portion 401 includes a binding portion 4021, which has a trapezoidal shape. This binding portion 4021 is used to bind to a circuit board and can provide impedance matching. For example, if the printed circuit board (FPC) has thin traces, the trapezoidal shape of the binding portion 4021 can reduce trace width variations during the binding process, preventing poor port parameters, compared to a rectangular shape.

[0140] By setting the shapes of the main body and the electrode part of the antenna structure, it is beneficial to improve the radiation effect of the antenna structure while improving the signal transmission effect.

[0141] For example, as shown in Figures 18 and 19, by setting the antenna structure to an octagonal solid structure using dual-polarization antenna technology as shown in Figure 15, it is beneficial to improve the radiation effect of the antenna structure. For example, the maximum gain of the antenna structure is approximately 6dBi; the maximum gain of the antenna structure in each radiation direction at a phase of 0 degrees at a frequency of 28GHz is approximately 4.4dBi, and the maximum gain of the antenna structure in each radiation direction at a phase of 90 degrees at a frequency of 28GHz is approximately 3dBi.

[0142] For example, as shown in Figures 12 to 15, the thickness of the antenna structure 400 can be the same as the thickness of the first metal grid electrode 2411 provided in the same layer, or when the first metal grid 2411 has multiple film layers, the thickness of the antenna structure 400 can be the same as the thickness of the film layer farthest from the substrate 100. In the electrochromic dimming structure provided by the present disclosure, the antenna structure and a layer of metal grid are formed in the same patterning process. The thickness of the antenna structure can be set to be the same as the thickness of the metal grid layer, or the same as the thickness of at least one film layer of the metal grid layer. At the same time, the antenna structure is set as a solid structure and does not overlap with the electrochromic device. This can prevent the electrochromic device from affecting the radiation effect of the antenna structure and help the antenna structure have a better radiation effect. When the electrochromic dimming structure including the above-mentioned antenna structure is applied to the sunroof of transportation equipment, the antenna structure can be stuck in a groove, which is a groove for setting the sunroof, to prevent the antenna structure from affecting the light transmission effect of the electrochromic dimming structure.

[0143] In some examples, as shown in Figures 16 and 17 , the antenna structure 400 includes a mesh structure. For example, the main body 401 of the antenna structure 400 includes a mesh structure. Figures 12 to 14 schematically illustrate that the antenna structure 400 does not overlap with the electrochromic layer 230 in a direction perpendicular to the substrate 100. However, this is not limiting. When the antenna structure includes a mesh structure, the antenna structure has a better light transmission effect, and the antenna structure can overlap with the electrochromic layer, which helps to increase the area of ​​the electrochromic device used for color change.

[0144] The outlines of the antenna structures shown in FIG. 16 and FIG. 17 may be the same as the outline of the antenna structure shown in FIG. 15 , and are not described again here.

[0145] In some examples, as shown in FIG16 , the main body 401 of the antenna structure 400 includes multiple contour edges 440 surrounding a mesh structure. The mesh structure includes a first strip portion 410 extending along a first direction and a second strip portion 420 extending along a second direction, where the first direction intersects the second direction. For example, the first direction may be the X direction in the figure, and the second direction may be the Y direction in the figure. The first and second directions may be interchangeable. For example, but not limited to this, the angle between the first and second directions may be 30 to 120 degrees, 45 to 100 degrees, or 60 to 80 degrees. For example, the angle between the first strip portion 410 and at least one contour edge 440 is 45 degrees, and the angle between the second strip portion 420 and at least one contour edge 440 is 45 degrees.

[0146] For example, as shown in FIG16 , the first strip portion 410 may be connected to the connection point of two adjacent contour edges 440. The angle between the first strip portion 410 and one of the contour edges 440 may be 45 degrees, and the angle between the first strip portion 410 and the other contour edge 440 may be 90 degrees. With reference to the extension direction of the contour edge of the antenna structure 400 in FIG15 , the first strip portion 410 and the second strip portion 420 in the antenna structure 400 shown in FIG16 can form a dual-polarized antenna with mutually orthogonal polarization directions of +45 degrees and -45 degrees, thereby reducing the number of antennas.

[0147] For example, as shown in FIG16 , the number of first strips 410 and second strips 420 is the same to achieve symmetry. In this case, the performance in both polarization directions is the same, such as the isolation S21 and S12 are the same, and the two channels can be switched arbitrarily. Of course, the disclosed embodiments are not limited to this, and the number of first strips and second strips can also be different. In this case, the performance of the two channels may differ significantly, such as the isolation S21 and S12 being different. If performance requirements are met, the two channels cannot be switched arbitrarily.

[0148] For example, the line widths of the first stripe 410 and the second stripe 420 can be the same as the line width of the metal grid electrode to facilitate manufacturing. For example, the line width of the contour edge 440 can be the same as the line width of the metal grid electrode. For example, the first stripe 410, the second stripe 420, and the contour edge 440 can be an integrated structure.

[0149] For example, both ends of the first strip portion 410 are connected to the contour edge 440 , and both ends of the second strip portion 420 are connected to the contour edge 440 .

[0150] For example, Figure 16 schematically shows that the number of first strips 410 and second strips 420 is 2, but it is not limited to this. When the antenna structure does not overlap with the electrochromic layer, the number of first strips and second strips can be appropriately increased to improve the radiation effect of the antenna structure; when the antenna structure overlaps with the electrochromic layer, the number of first strips and second strips needs to be set taking into account the light transmission effect and radiation effect of the antenna structure.

[0151] For example, as shown in Figures 18 and 20, by setting the antenna structure to a grid structure using dual-polarization antenna technology as shown in Figure 16, it is beneficial to improve the radiation effect of the antenna structure. For example, the maximum gain of the antenna structure is approximately 2dBi; the maximum gain of the antenna structure in each radiation direction at a phase of 0 degrees at a frequency of 28GHz is approximately -0.61dBi, and the maximum gain of the antenna structure in each radiation direction at a phase of 90 degrees at a frequency of 28GHz is approximately -2.5dBi.

[0152] For example, FIG16 only illustrates the grid structure in the main body portion, and the electrode portion of the antenna structure may also be configured as a grid structure.

[0153] In some examples, as shown in FIG17 , antenna structure 400 includes multiple contour edges 440 surrounding a mesh structure. The mesh structure includes multiple strips 430 arranged radially, originating from a point within a central region 450 of main body 401. The central region may refer to an area centered at the center of an octagonal outline, for example, with a radius of 1 / 4 to 3 / 4 the length of the octagon's diagonal. For example, the origin of the multiple radial strips 430 may be the center point of the central region.

[0154] For example, as shown in FIG17 , at least one strip 430 may terminate at a point connected to a contour edge 440 . For example, each strip 430 may terminate at a point connected to a contour edge 440 . For example, a strip 430 may terminate at one end of a contour edge 440 or at any point along the contour edge 440 . For example, the strip 430 and the contour edge 440 may be integrally formed. For example, the line widths of the strip 430 and the contour edge 440 may be the same as the line width of the metal mesh electrode to facilitate manufacturing.

[0155] For example, FIG17 only illustrates the grid structure in the main body portion, and the electrode portion of the antenna structure may also be configured as a grid structure.

[0156] For example, Figure 17 schematically shows that the number of strips 430 is 8, but is not limited to this. When the antenna structure does not overlap with the electrochromic layer, the number of strips can be appropriately increased to improve the radiation effect of the antenna structure; when the antenna structure overlaps with the electrochromic layer, the number of strips needs to be set taking into account the light transmission effect and radiation effect of the antenna structure.

[0157] For example, as shown in Figures 18 and 21, by setting the antenna structure to a grid structure using dual-polarization antenna technology as shown in Figure 17, the radiation effect of the antenna structure is improved. For example, the maximum gain of the antenna structure is approximately 1.5dBi; the maximum gain of the antenna structure in each radiation direction at a phase of 0 degrees at a frequency of 28GHz is approximately -1.8dBi, and the maximum gain of the antenna structure in each radiation direction at a phase of 90 degrees at a frequency of 28GHz is approximately -4.3dBi.

[0158] For example, as shown in Figure 18, the radiation effect of a solid antenna structure is better than that of an antenna structure with a mesh structure. Comparing the antenna structures with mesh structures shown in Figures 16 and 17, it is found that the mesh structure shown in Figure 16 is conducive to uniform current distribution, allowing the current to flow smoothly and the resonance to achieve stronger radiation.

[0159] FIG22 is a schematic diagram of an electrochromic dimming structure according to another example of an embodiment of the present disclosure. The electrochromic dimming structure shown in FIG22 differs from the electrochromic dimming structure shown in FIG12 in that the structure of the metal electrode 240 is different.

[0160] In some examples, as shown in FIG22 , the metal electrode 240 includes at least one of a metal grid electrode and a metal thin layer 243 . The metal thin layer 243 has a thickness of 1 to 20 nanometers and overlaps the electrochromic layer 230 in a direction perpendicular to the substrate 100 . For example, the metal thin layer 243 has a thickness of 2 to 10 nanometers. For example, the metal thin layer 243 has a thickness of 3 to 6 nanometers. For example, the metal thin layer 243 has a thickness of 4 to 9 nanometers. For example, the metal thin layer 243 has a thickness of 5 to 8 nanometers. For example, the metal thin layer 243 has a thickness of 7 to 15 nanometers. For example, the metal thin layer 243 has a thickness of 12 to 18 nanometers.

[0161] In some examples, as shown in FIG22 , the metal electrode 240 includes a first metal grid electrode 2411 and a second metal thin layer 2432. The first metal grid electrode 2411 is located on a side of the first electrode layer 210 away from the second electrode layer 220 and is electrically connected to the first electrode layer 210. The second metal thin layer 2432 is located on a side of the second electrode layer 220 away from the first electrode layer 210 and is electrically connected to the second electrode layer 220. The antenna structure 400 is provided in the same layer as the first metal grid electrode 2411, and the thickness of the antenna structure 400 is greater than the thickness of the second metal thin layer 2432. For example, the antenna structure 400 may have the same features as any of the antenna structures 400 shown in FIG15 to FIG17 , and no further description is given here.

[0162] The electrochromic dimming structure provided by the present invention is beneficial to improving the conductive effect while reflecting sunlight, such as reflecting the infrared band in sunlight, to reduce the thermal effect, and provide a better working environment for the electrochromic dimming structure by setting the metal electrode on the side of the second electrode layer away from the first electrode layer as a metal thin layer; at the same time, the metal electrode on the side of the first electrode layer away from the second electrode layer is set as a metal grid electrode with a thickness greater than the metal thin layer, and the thickness of the antenna structure manufactured in the same patterning process as the metal grid electrode is set to be thicker and solid structure, which is beneficial to improving the radiation effect of the antenna structure.

[0163] For example, the first metal grid electrode shown in FIG. 22 may have the same features as the first metal grid electrode in the above example, and details thereof will not be repeated here.

[0164] 22 , at least 90% of the orthographic projection of the second electrode layer 220 on the substrate 100 overlaps with the orthographic projection of the second metal thin layer 2432 on the substrate 100. For example, more than 95% of the orthographic projection of the second electrode layer 220 on the substrate 100 overlaps with the orthographic projection of the second metal thin layer 2432 on the substrate 100. For example, the orthographic projection of the second electrode layer 220 on the substrate 100 completely overlaps with the orthographic projection of the second metal thin layer 2432 on the substrate 100.

[0165] For example, the first metal grid electrode shown in Figure 22 can adopt the first metal grid electrode shown in Figures 9 and 10, that is, as shown in Figure 13, if a thicker metal grid is formed by electroplating, then the antenna structure and the first metal grid electrode can be formed in a synchronous patterning process, and the antenna structure can have a thicker thickness, such as more than 1 micron.

[0166] FIG23 is a schematic diagram of an electrochromic dimming structure according to another example of an embodiment of the present disclosure. The electrochromic dimming structure shown in FIG23 differs from the electrochromic dimming structure shown in FIG22 in that the structure of the metal electrode 240 is different.

[0167] In some examples, as shown in FIG23 , at least 90% of the orthographic projection of the first electrode layer 210 on the substrate 100 overlaps with the orthographic projection of the metal thin layer 243 on the substrate 100. For example, more than 95% of the orthographic projection of the first electrode layer 210 on the substrate 100 overlaps with the orthographic projection of the metal thin layer 243 on the substrate 100. For example, the orthographic projection of the first electrode layer 210 on the substrate 100 completely overlaps with the orthographic projection of the metal thin layer 243 on the substrate 100.

[0168] In some examples, as shown in FIG23 , the metal thin layer 243 includes a first metal thin layer 2431 and a second metal thin layer 2432 . The first metal thin layer 2431 is located on a side of the first electrode layer 210 away from the second electrode layer 220 and is electrically connected to the first electrode layer 210 . The second metal thin layer 2432 is located on a side of the second electrode layer 220 away from the first electrode layer 210 and is electrically connected to the second electrode layer 220 . The antenna structure 400 is provided on the same layer as one of the first metal thin layer 2431 and the second metal thin layer 2432 . Providing the antenna structure on the same layer as the metal electrode helps save space and reduce costs. FIG23 schematically illustrates the antenna structure 400 being provided on the same layer as the first metal thin layer 2431 , but the present invention is not limited thereto. The antenna structure can also be provided on the same layer as the second metal thin layer.

[0169] For example, as shown in FIG23 , the thickness of the first metal thin layer 2431 is greater than the thickness of the second metal thin layer 2432 , and the thickness of the antenna structure 400 is the same as the thickness of the first metal thin layer 2431 , so as to maximize the thickness of the antenna structure and improve the radiation effect of the antenna structure.

[0170] The first metal thin layer or the first metal grid electrode in the electrovariable dimming structure shown in Figures 22 and 23 above can be called the first metal electrode, and the second metal thin layer in the electrovariable dimming structure shown in Figures 22 and 23 above can be called the second metal electrode. By setting the thickness of the antenna structure arranged on the same layer as the first metal electrode to be greater than that of the second metal electrode, the thickness of the antenna structure is greater than that of the first metal electrode, and the thickness of the antenna structure can be increased as much as possible to improve the radiation effect of the antenna structure; the second metal electrode adopts the second metal thin layer, which is conducive to reflecting more sunlight, reducing the heating effect of the infrared band of the solar spectrum energy on the electrovariable dimming structure, and is conducive to improving the reliability and cycle characteristics of the electrovariable dimming structure.

[0171] The electrochromic devices in the examples shown in the above figures can be interchangeable. For example, the second electrode layer with three film layers shown in Figure 11 can be applied to the electrochromic dimming structure shown in Figures 22 to 23 to further reduce the warming effect of the infrared band of the solar spectrum energy on the electrochromic dimming structure.

[0172] The first metal grid electrode in the examples shown in the above figures can be applied to the electrovariable dimming structure shown in FIG. 22 .

[0173] Another embodiment of the present disclosure provides a traffic device, and Figure 24 is a schematic block diagram of the traffic device. As shown in Figure 24, the traffic device includes a skylight, and the skylight has any of the above-mentioned electrovariable dimming structures.

[0174] For example, the traffic equipment includes a slot for engaging the sunroof, and the antenna structure can be set to a solid and thick structure and placed in the slot, which will not affect the light transmittance of the sunroof and can greatly improve the radiation characteristics of the antenna structure.

[0175] For example, the first electrode layer is closer to the interior space of the traffic equipment than the second electrode layer.

[0176] For example, the transportation equipment may be various appropriate transportation tools, such as various types of land transportation equipment such as cars, or water transportation equipment such as ships.

[0177] There are a few points to note:

[0178] (1) The drawings of the embodiments of the present disclosure only involve structures related to the embodiments of the present disclosure, and other structures can refer to general designs.

[0179] (2) In the absence of conflict, features in the same embodiment and different embodiments of the present disclosure may be combined with each other.

[0180] The foregoing description is merely an exemplary embodiment of the present disclosure and is not intended to limit the scope of protection of the present disclosure. The scope of protection of the present disclosure is determined by the appended claims.

Claims

1. An electrochromic dimming structure, comprising: substrate; An electrochromic device, located on the substrate, comprising a first electrode layer, an electrochromic layer and a second electrode layer stacked in sequence, wherein the first electrode layer is located between the electrochromic layer and the substrate, the first electrode layer and the second electrode layer are both whole light-transmitting electrode layers, and at least one of the first electrode layer and the second electrode layer comprises an oxide material; A first protective layer, covering the electrochromic device; The electrochromic device further comprises a metal electrode located on at least one of a side of the first electrode layer away from the second electrode layer and a side of the second electrode layer away from the first electrode layer, and the metal electrode is electrically connected to at least one of the first electrode layer and the second electrode layer.

2. The electrochromic dimming structure according to claim 1, wherein: The metal electrode comprises at least one of a metal grid electrode and a metal thin layer, and the thickness of the metal thin layer is 1 to 20 nanometers; Along a direction perpendicular to the substrate, the metal electrode overlaps the electrochromic layer.

3. The electrochromic light-emitting structure according to claim 2, further comprising: The antenna structure is in the same layer as at least part of the metal electrode and is spaced apart from the metal electrode.

4. The electrochromic dimming structure according to claim 3, wherein: The metal electrode comprises a first metal electrode and a second metal electrode, the first metal electrode is located at a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal electrode is located at a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; The antenna structure is arranged in the same layer as the first metal electrode, and the thickness of the antenna structure is greater than the thickness of the second metal electrode.

5. The electrochromic dimming structure according to claim 4, wherein: The first metal electrode includes a first metal mesh electrode or a first metal thin layer, and the second metal electrode includes a second metal thin layer.

6. The electrochromic dimming structure according to claim 3, wherein: The metal grid electrode comprises a first metal grid electrode and a second metal grid electrode, the first metal grid electrode is located at a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal grid electrode is located at a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; The orthographic projection of the first metal grid electrode on the substrate is parallel to the orthographic projection of the second metal grid electrode The overlap rate of the orthographic projections on the substrate is greater than 90%; The antenna structure is disposed in the same layer as one of the first metal grid electrode and the second metal grid electrode.

7. The electrochromic dimming structure according to claim 3, wherein: At least 90% of the orthographic projection of the first electrode layer on the substrate overlaps with the orthographic projection of the metal thin layer on the substrate; The metal thin layer comprises a first metal thin layer and a second metal thin layer, the first metal thin layer is located on a side of the first electrode layer away from the second electrode layer and is electrically connected to the first electrode layer, and the second metal thin layer is located on a side of the second electrode layer away from the first electrode layer and is electrically connected to the second electrode layer; The antenna structure is disposed in the same layer as one of the first metal thin layer and the second metal thin layer.

8. The electrochromic dimming structure according to any one of claims 3 to 7, wherein: The antenna structure comprises a solid structure, and along a direction perpendicular to the substrate, the antenna structure does not overlap with the electrochromic layer.

9. The electrochromic dimming structure according to claim 5 or 6, wherein: The antenna structure includes a grid structure, and along a direction perpendicular to the substrate, the antenna structure overlaps or does not overlap with the electrochromic layer.

10. The electrochromic dimming structure according to any one of claims 3 to 9, wherein: The antenna structure includes a main body, the main body is in an octagonal shape, and the angle between at least two adjacent sides of the octagon is 135 degrees.

11. The electrochromic dimming structure according to claim 9, wherein: The antenna structure includes a main body, the main body includes the mesh structure, the mesh structure includes a first stripe portion extending along a first direction and a second stripe portion extending along a second direction, the first direction intersecting the second direction.

12. The electrochromic dimming structure according to claim 9, wherein: The antenna structure includes a main body, the main body includes the grid structure, and the grid structure includes a plurality of strips arranged radially starting from a point in a central area of ​​the main body.

13. The electrochromic dimming structure according to any one of claims 1 to 12, wherein: The thickness of the electrode layer electrically connected to the metal electrode in the first electrode layer and the second electrode layer is 10 nanometers to 10 micrometers.

14. The electrochromic dimming structure according to claim 2, wherein: The thickness of the metal grid electrode is 100 to 5000 nanometers, and the line width of the metal grid electrode is 1 to 5 micrometers.

15. The electrochromic light-emitting structure according to claim 6, further comprising: a second protective layer, covering the second electrode layer; Wherein, at least a portion of the second metal grid electrode and the antenna structure are located on a side of the second protective layer away from the substrate, the second protective layer includes a groove configured to expose the second electrode layer, and the second metal grid electrode is electrically connected to the second electrode layer through the groove; An electrode portion is further provided on a side of the second protective layer away from the second electrode layer, and the electrode portion is electrically connected to the second metal mesh electrode; The first protective layer covers the second metal grid electrode and the antenna structure.

16. The electrochromic dimming structure according to claim 6, wherein: The antenna structure is arranged in the same layer as the first metal grid electrode, and the first protective layer covers the antenna structure; The first metal grid electrode includes two metal layers, and the material of the antenna structure is the same as the material of the metal layer of the two metal layers that is far away from the substrate.

17. The electrochromic dimming structure according to any one of claims 1 to 16, wherein: The second electrode layer includes a first film layer, a second film layer and a third film layer which are stacked, the first film layer and the third film layer are made of the same material, and the thickness ratio of the first film layer to the third film layer is 0.9~1.1, and the thickness of the second film layer is less than the thickness of the first film layer.

18. The electrochromic dimming structure according to any one of claims 1 to 17, wherein: The electrochromic layer includes an electrochromic material layer, an electrolyte layer and a storage layer which are stacked in sequence, and the electrochromic material layer is located between the electrolyte layer and the first electrode layer.

19. The electrochromic dimming structure according to claim 18, wherein: The electrochromic material layer includes one of an inorganic electrochromic material and an organic electrochromic material, and the electrolyte layer includes one of a solid electrolyte and a liquid electrolyte.

20. A traffic device comprising a skylight, wherein: The skylight comprises the electrochromic dimming structure according to any one of claims 1-19.

Citation Information

Patent Citations

  • All-solid-state electrochromic glass

    CN107621737A

  • Electrochromic device

    CN109154755A

  • Electronic equipment and housing assembly

    CN112835238A

  • Electrochromic glass , doubling glass and cavity glass that discolour fast

    CN208766430U

  • All-solid-state reflective dimming electrochromic element sealed with protective layer, and dimming member comprising the same

    US20130010347A1