Barbecue net processing technology and barbecue net assembly
Through aluminum alloy extrusion molding and anodizing treatment, the existing grilling nets are solved, and a light, stable and durable grilling net design is achieved, which improves the use effect and life of grilling nets.
Patent Information
- Application Number
- CN202411020568.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-01
AI Technical Summary
The existing grilled nets are heavy, inconvenient for processing and use, and have poor thermal conductivity, which leads to the grilled nets being easily shaken during the barbecue process, affecting the uniform heating effect of the food.
The aluminum alloy blank is extruded to form the aluminum grilling main board and side bracket. The grilling design is punched and riveted, combined with anodizing treatment, to improve the lightweight, stability and corrosion resistance of the grilling net.
It improves the processing efficiency and service life of the grilled net, ensures uniform heating and hygiene standards of food, and enhances the stability and aesthetics of the grilled net.
Smart Images

Figure CN118873016A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of barbecue grills and grilling nets, and in particular to a grilling net processing technology and a barbecue grilling net component. Background Art
[0002] Barbecue is a common cooking method, widely used in outdoor and indoor cooking occasions. At present, the grills used in ovens on the market are usually made of stainless steel or iron. These materials are resistant to high temperatures and corrosion, and are suitable for long-term use in high temperature environments. However, these materials are heavy, inconvenient to carry, assemble and process, and have low processing efficiency. It is also very laborious for users to use them outdoors, and the thermal conductivity and heat dissipation performance are very poor. In addition, the grill may be uneven during processing. Such a grill cannot evenly fit the surface of the oven, causing the grill to move or shake during the barbecue process, thereby affecting the uniform heating and cooking effect of the food, and further affecting the user experience. Summary of the invention
[0003] The object of the present invention is to provide a grilling net processing method and a barbecue grilling net assembly which can improve processing efficiency, is light in use, has good stability, and has a long service life.
[0004] A grill processing method comprises the following steps: extruding an aluminum alloy blank into an aluminum grill profile; cutting the aluminum grill profile to form an aluminum grill main board; punching oil-leaking strip holes on the aluminum grill main board; punching square holes at both ends of the aluminum grill main board; assembling two aluminum grill side brackets and riveting them at both ends of the aluminum grill main board to form an aluminum grill assembly; and performing surface anodizing on the aluminum grill assembly.
[0005] In the above scheme, the aluminum alloy billet is extruded into a wavy aluminum mesh profile. The extrusion process can increase the structural strength of the aluminum material while maintaining its lightweight. The aluminum grill main board and the aluminum grill side bracket are both light in weight, which reduces the labor intensity of transportation and assembly and can improve the processing efficiency. The aluminum grill main board is punched with oil-leaking strip holes and square holes, which helps the grill to discharge food grease and impurities during use, thereby maintaining the quality and hygiene standards of baked food. The two aluminum grill side brackets are assembled and riveted at both ends of the aluminum grill main board. This assembly method is simple and can ensure the stability of the aluminum grill main board during use. The surface anodizing treatment improves the corrosion resistance of the aluminum grill assembly, extends its service life, and makes its appearance more beautiful.
[0006] Furthermore, the aluminum grill main board includes a first protrusion and a second protrusion with opposite protrusion directions, and the first protrusion and the second protrusion are continuously and alternately connected.
[0007] In the above scheme, the food contacts the first protrusion, and the first protrusion can evenly conduct heat to the surface of the food to heat the food. The grease, sauce, etc. generated during the heating of the food drip into the second protrusion, preventing the grease, sauce, etc. from excessively accumulating on the grill, thereby improving the health and taste of the food. The first protrusion and the second protrusion are continuously and alternately arranged to ensure the grilling effect. In addition, a zebra crossing shape can be formed on the surface of the food, making the food beautiful.
[0008] Furthermore, the method of punching the oil leakage strip holes on the aluminum grill main board includes the following steps: placing the aluminum grill main board with the protrusion direction of the first protrusion facing upward and the protrusion direction of the second protrusion facing downward on the first positioning groove of the first stamping machine, and making one end of the aluminum grill main board close to the first positioning column on the first stamping machine; pressing the first stamping machine downward to punch a plurality of strip holes on the second protrusion, and the strip holes are used for oil leakage.
[0009] In the above scheme, by placing the aluminum grill main board on the first positioning groove of the first stamping machine and using the first positioning column for positioning, the accuracy of the stamping process can be ensured. The protruding direction of the first protrusion is upward and the protruding direction of the second protrusion is downward to avoid deformation of the aluminum grill main board during stamping. A plurality of strip holes are punched on the second protrusion, and these holes can effectively discharge the grease generated during the food heating process.
[0010] Furthermore, punching square holes at both ends of the aluminum grill main board includes the following steps: placing one end of the aluminum grill main board on the second positioning groove of the second stamping machine, so that the protruding direction of the first protrusion faces downward, and the protruding direction of the second protrusion faces upward; placing one end of the aluminum grill main board against the second positioning column on the second stamping machine, and pressing the second stamping machine downward to punch a first square hole at one end of the second protrusion; taking out the aluminum grill main board and placing the other end of it on the second positioning groove of the second stamping machine, and the protruding directions of the first protrusion and the second protrusion remain unchanged; pressing the second stamping machine downward to punch a second square hole at one end of the second protrusion.
[0011] In the above scheme, one end of the aluminum grill main board is placed on the second positioning groove of the second punching machine, ensuring that the protrusion of the first protrusion is facing downward and the protrusion of the second protrusion is facing upward, and one end of the aluminum grill main board is abutted against the second positioning column on the second punching machine to ensure stability and precise positioning. The second punching machine presses down to punch one end of the second protrusion to form the first square hole, and the aluminum grill main board is taken out and the other end is placed on the second positioning groove of the second punching machine. During the repositioning process, ensure that the orientation of the first protrusion and the second protrusion remains unchanged to ensure the consistency and accuracy of the hole position. These square holes are convenient for discharging larger grease residues.
[0012] Furthermore, the two aluminum grilling grid side brackets are assembled and riveted to the two ends of the aluminum grilling grid main board to form an aluminum grilling grid assembly, including the following steps: respectively passing the two ends of the first protrusion through the connecting holes on the first panels of the two aluminum grilling grid side brackets; and stamping and expanding the first protrusion passing through the first panel of the aluminum grilling grid side bracket so that the first protrusion is riveted to the aluminum grilling grid side bracket.
[0013] In the above solution, the first protrusions at the two ends of the aluminum grill main board are respectively passed through the connection holes on the first panels of the two aluminum grill side brackets. This step ensures the initial connection and positioning between the aluminum grill side brackets and the aluminum grill main board. The first protrusions passing through the first panels of the aluminum grill side brackets are subjected to a stamping and expansion operation so that the first protrusions are riveted together with the aluminum grill side brackets. This riveting method can ensure that the aluminum grill side brackets are firmly fixed on the aluminum grill main board, thereby enhancing the stability and durability of the overall structure.
[0014] Furthermore, after punching square holes at both ends of the aluminum grill main board, the aluminum grill main board is also polished and wired, and the polishing machine is equipped with a wire drawing wheel, and the polishing machine is pushed back and forth along the aluminum grill main board twice.
[0015] In the above scheme, raised burrs will appear after punching the strip holes and square holes on the aluminum grill main board, so the aluminum grill main board needs to be polished and brushed. After completion, the surface of the aluminum grill main board is smooth and has brushed lines, which is not only beautiful, but also increases the texture and touch of the product.
[0016] Furthermore, before the surface of the aluminum grill assembly is anodized, the aluminum grill assembly is fully cleaned and inspected, and a clean cloth moistened with white gasoline is used to wipe the aluminum grill assembly to inspect the appearance of the aluminum grill assembly.
[0017] In the above scheme, anodizing is an electrochemical process used to form a protective oxide film on the surface of aluminum alloy. If there is oil, dust or other impurities on the surface of the aluminum grill component, these impurities may affect the formation and quality of the oxide layer. By cleaning, you can ensure a smooth surface and provide a basis for the formation of a high-quality oxide layer.
[0018] Furthermore, the surface of the aluminum grill assembly is anodized, and the thickness of the anodization is between 40 μm and 60 μm.
[0019] In the above scheme, the anodized layer thickness in the range of 40 μm to 60 μm can provide good corrosion resistance and effectively prevent the aluminum grill assembly from being damaged by oxidation during use. At the same time, it also has a high hardness, increasing the ability to resist scratches and wear.
[0020] A barbecue grill assembly is manufactured using the grill processing method described in the above scheme, comprising an aluminum grill main board and an aluminum grill side bracket, wherein the two aluminum grill side brackets are respectively connected to the two ends of the aluminum grill main board, and an oxide layer is formed on the surface of the aluminum grill main board and the aluminum grill side bracket, and the oxide layer is a hard anodized layer.
[0021] In the above scheme, the aluminum grill main board and the aluminum grill side bracket are made of aluminum, which is light in weight, reduces the labor intensity of assembly and transportation, and makes outdoor grill assembly more convenient. The aluminum grill side bracket can ensure the stability of the grill installed on the grill, so that the aluminum grill main board remains flat. Since a hard anodized layer is formed on the surface of the aluminum grill assembly, this oxide layer can effectively block the intrusion of water and oxygen, thereby greatly improving the corrosion resistance of the entire grill assembly and extending its service life.
[0022] Furthermore, the cross section of the first protrusion is in an inverted U shape, the protrusion direction of the second protrusion is opposite to the protrusion direction of the first protrusion, and the cross section of the second protrusion is in a V shape.
[0023] In the above scheme, the inverted U-shaped first raised portion is in contact with the food, which is conducive to firmly supporting the food, improving the uniformity and efficiency of heating, ensuring that the food can be fully heated, and achieving better cooking results; the grease, sauce, etc. generated during the heating of the food drip into the second raised portion, and the V-shaped second raised portion facilitates the discharge of the grease, sauce, etc., to avoid affecting the health and taste of the food.
[0024] The grilling net processing method and grilling net assembly of the present invention have the beneficial effects of improving processing efficiency, being light and stable when in use, and having a long service life. The aluminum alloy billet is extruded into a wavy aluminum net profile. The aluminum material can be made lightweight while increasing its structural strength through the extrusion process. The aluminum grilling net main board and the aluminum grilling net side bracket are both light in weight, which reduces the labor intensity of transportation and assembly and can improve processing efficiency. The aluminum grilling net main board is punched with oil strip holes and square holes, which helps the grilling net to discharge food grease and impurities during use and maintain the quality and sanitation standards of the baked food. The two aluminum grilling net side brackets are assembled and riveted at both ends of the aluminum grilling net main board. This assembly method is simple and can ensure the stability of the aluminum grilling net main board when in use. The surface anodizing treatment improves the corrosion resistance of the aluminum grilling net assembly, prolongs its service life, and makes its appearance more beautiful. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 The present invention is a flow chart of the grill processing method.
[0026] Figure 2 This is a flow chart of step S300 of the present invention.
[0027] Figure 3 This is a flow chart of step S400 of the present invention.
[0028] Figure 4 This is a flow chart of step 600 of the present invention.
[0029] Figure 5 The figure is a schematic structural diagram of a barbecue grill assembly according to an embodiment.
[0030] Figure 6 FIG. 1 is a schematic structural diagram of a first protrusion and a second protrusion in one embodiment.
[0031] Figure 7 The figure is a schematic diagram of the aluminum grill side bracket structure according to one embodiment.
[0032] Figure 8 The figure is a schematic diagram of the connection structure between the aluminum grill side bracket and the aluminum grill main board according to one embodiment.
[0033] Explanation of the accompanying drawings: 1. Aluminum grill main board; 11. First protrusion; 12. Second protrusion; 2. Aluminum grill side bracket; 21. First panel; 3. Strip hole; 4. Square hole; 5. Connecting hole. DETAILED DESCRIPTION
[0034] The following will further describe in detail a grilling net processing method and a barbecue grilling net assembly of the present invention in conjunction with specific embodiments and drawings.
[0035] like Figures 1 to 8 As shown, in a preferred embodiment, a grill processing method of the present invention comprises the following steps: Step S100, extruding the aluminum alloy billet into an aluminum mesh profile. Extruding the aluminum alloy billet into a wavy aluminum mesh profile can increase the structural strength of the aluminum material while maintaining its lightness through the extrusion process.
[0036] Step S200, cutting the aluminum mesh profile to form an aluminum grill mainboard 1.
[0037] like Figure 5 and Figure 6 As shown, in some embodiments, the aluminum grill main board 1 includes a first protrusion 11 and a second protrusion 12 with opposite protrusion directions, and the first protrusion 11 and the second protrusion 12 are continuously and alternately connected. The food contacts the first protrusion 11, and the first protrusion 11 can evenly conduct heat to the surface of the food to heat the food. The grease, sauce, etc. generated during the heating of the food drip into the second protrusion 12, which prevents the grease, sauce, etc. from excessively accumulating on the grill, thereby improving the health and taste of the food. The first protrusion 11 and the second protrusion 12 are continuously and alternately arranged to ensure the grilling effect, and can also form a zebra crossing shape on the surface of the food, making the food beautiful.
[0038] Step S300, flushing the aluminum grill main board 1 with the oil-draining strip holes 3. The strip holes 3 can ensure that the oil is smoothly discharged from the aluminum grill main board 1, avoiding excessive accumulation of oil on the aluminum grill main board 1, and improving the healthiness and taste of food.
[0039] In one embodiment, step S300 specifically includes: Step S310, the aluminum grill main board 1 with the first protrusion 11 facing upward and the second protrusion 12 facing downward is placed on the first positioning groove of the first stamping machine, and one end of the aluminum grill main board 1 is close to the first positioning column of the first stamping machine. By placing the aluminum grill main board 1 on the first positioning groove of the first stamping machine and positioning it with the first positioning column, the accuracy of the stamping process can be ensured. The purpose of placing the first protrusion 11 facing upward and the second protrusion 12 facing downward is to avoid deformation of the aluminum grill main board 1 during stamping.
[0040] Step S320, the first punching machine presses down to punch a plurality of strip holes 3 on the second raised portion 12, and the strip holes 3 are used for oil leakage. By using a punching machine for batch production, the production efficiency can be significantly improved. This automated production method reduces the complexity and time cost of manual operation, making the production process more efficient and reliable. Punching a plurality of strip holes 3 on the second raised portion 12 can effectively discharge the grease generated during the heating process of food. This design not only helps to keep the grill clean, but also prevents grease from accumulating on the grill, thereby improving the hygiene standard and taste of the food.
[0041] Step S400, punching square holes at both ends of the aluminum grill main board 1.
[0042] In one embodiment, step S400 specifically includes: Step S410, placing one end of the aluminum grill main board 1 on the second positioning groove of the second punching machine, so that the protruding direction of the first protruding portion 11 faces downward, and the protruding direction of the second protruding portion 12 faces upward.
[0043] Step S420, one end of the aluminum grill main board 1 is leveled against the second positioning column on the second punching machine, and the second punching machine presses down to punch the first square hole 4 on one end of the second protrusion 12. One end of the aluminum grill main board 1 is placed on the second positioning groove of the second punching machine, ensuring that the protrusion of the first protrusion 11 faces downward and the protrusion of the second protrusion 12 faces upward, and one end of the aluminum grill main board 1 is abutted against the second positioning column on the second punching machine to ensure stability and precise positioning, and the second punching machine presses down to punch one end of the second protrusion 12 to form the first square hole 4.
[0044] Step S430, taking out the aluminum grill main board 1 and placing the other end thereof on the second positioning groove of the second punching machine, and the protruding directions of the first protrusion 11 and the second protrusion 12 remain unchanged.
[0045] Step S440, the second punching machine presses down to punch a second square hole 4 at one end of the second protrusion 12. Take out the aluminum grill main board 1, and place its other end on the second positioning groove of the second punching machine. During the repositioning process, ensure that the orientation of the first protrusion 11 and the second protrusion 12 remains unchanged to ensure the consistency and accuracy of the position of the square hole 4.
[0046] In the above embodiment, the square holes 4 at both ends of the aluminum grill main board 1 are effectively punched through precise positioning and punching operations, which not only improves the assembly efficiency and quality of the product, but also enhances its stability and reliability during use. When grilling, some food residues may fall onto the second protrusion 12. The strip holes 3 at the bottom of the second protrusion 12 can only pass a part of the grease, so the larger grease residues need to be discharged through the square holes 4. The square holes 4 help to keep the oil guide groove clean, thereby improving the cooking effect and the taste of the food. The square holes 4 are also convenient for cleaning the aluminum grill main board 1.
[0047] Step S500, grinding and drawing the aluminum grill main board 1, the grinding machine is equipped with a drawing wheel, and the grinding machine is pushed back and forth twice along the aluminum grill main board 1. After punching the strip holes 3 and the square holes on the aluminum grill main board 1, burrs will appear, so the aluminum grill main board 1 needs to be ground and drawn. After completion, the surface of the aluminum grill main board 1 is smooth and has a drawing texture, which is not only beautiful, but also can increase the texture and touch of the product.
[0048] Step S600, assemble and rivet the two aluminum grill side brackets 2 at both ends of the aluminum grill main board 1 to form an aluminum grill assembly. Assemble and rivet the two aluminum grill side brackets 2 at both ends of the aluminum grill main board 1. This assembly method is simple and can ensure the stability of the aluminum grill main board 1 when in use. The aluminum grill main board 1 and the aluminum grill side brackets 2 are both light in weight, which reduces the labor intensity of transportation and assembly and can improve processing efficiency.
[0049] In one embodiment, step S600 specifically includes: Step S610 , passing two ends of the first protrusion 11 through the connection holes 5 on the first panels 21 of the two aluminum grill side brackets 2 .
[0050] Step S620 , punching and expanding the first protruding portion 11 of the first panel 21 passing through the aluminum grill side bracket 2 so that the first protruding portion 11 is riveted to the aluminum grill side bracket 2 .
[0051] In the above embodiment, the first protrusions 11 at the two ends of the aluminum grill main board 1 are respectively passed through the connection holes 5 on the first panels 21 of the two aluminum grill side brackets 2. This step ensures the initial connection and positioning between the aluminum grill side brackets 2 and the aluminum grill main board 1. The first protrusions 11 passing through the first panels 21 of the aluminum grill side brackets 2 are subjected to a stamping and expansion operation, so that the first protrusions 11 are riveted together with the aluminum grill side brackets 2. This riveting method can ensure that the aluminum grill side brackets 2 are firmly fixed on the aluminum grill main board 1, thereby enhancing the stability and durability of the overall structure.
[0052] Step S700, clean and inspect the aluminum grill assembly, wipe the aluminum grill assembly with a clean cloth moistened with white spirit to inspect the appearance of the aluminum grill assembly. Anodizing is an electrochemical process used to form a protective oxide film on the surface of aluminum alloy. If there is oil, dust or other impurities on the surface of the aluminum grill assembly, these impurities may affect the formation and quality of the oxide layer. By cleaning, the surface can be ensured to be smooth, providing a basis for the formation of a high-quality oxide layer.
[0053] Step S800, anodize the surface of the aluminum grill assembly. Surface anodizing improves the corrosion resistance of the aluminum grill assembly, extends its service life, and makes it more beautiful. After the surface anodizing is completed, tensile test, salt spray test, heat resistance test and coating thickness test are required. During the tensile test, a load of 110KG needs to be vertically hung under the aluminum grill assembly for one minute. The product is not loose or detached, the front appearance is good, and the contact point of the back hanging rope is slightly deformed, which is considered qualified; during the salt spray test, the rust area of 5% salt spray for 336 hours is less than 0.1%, which is considered qualified; during the temperature resistance test, the temperature is 425C° (800 °F), and after 1 hour, it is sprinkled with normal temperature water, and there is no blistering, cracking or deformation.
[0054] The thickness of anodizing is between 40 μm and 60 μm. The thickness of anodizing layer between 40 μm and 60 μm can provide good corrosion resistance and effectively prevent the aluminum grill components from being damaged by oxidation during use. At the same time, it also has a higher hardness, which increases the ability to resist scratches and wear.
[0055] like Figures 5 to 8As shown, in a preferred embodiment, a barbecue grill assembly is made by the grill processing method of the above scheme, including an aluminum grill main board 1 and an aluminum grill side bracket 2, and the two aluminum grill side brackets 2 are respectively connected to the two ends of the aluminum grill main board 1. An oxide layer is formed on the surface of the aluminum grill main board 1 and the aluminum grill side bracket 2, and the oxide layer is a hard anodized layer. The aluminum grill main board 1 and the aluminum grill side bracket 2 are both made of aluminum, which is light in weight, reduces the labor intensity of assembly and transportation, and makes outdoor assembly of the oven more convenient. The aluminum grill side bracket 2 can ensure the stability of the grill installed on the oven, so that the aluminum grill main board 1 remains flat. Since a hard anodized layer is formed on the surface of the aluminum grill assembly, this oxide layer can effectively block the intrusion of water and oxygen, thereby greatly improving the corrosion resistance of the entire grill assembly and extending the service life.
[0056] like Figure 6 As shown, in some embodiments, the cross section of the first protrusion 11 is inverted U-shaped, the direction of the second protrusion 12 is opposite to the direction of the first protrusion 11, and the cross section of the second protrusion 12 is V-shaped. The inverted U-shaped first protrusion 11 is in contact with the food, and the first protrusion 11 is conducive to firmly supporting the food, improving the uniformity and efficiency of heating, ensuring that the food can be fully heated, and the cooking effect is better; the grease, sauce, etc. generated during the heating of the food drip into the second protrusion 12, and the V-shaped second protrusion 12 facilitates the discharge of the grease, sauce, etc. to avoid affecting the health and taste of the food.
[0057] The present invention discloses a grill processing method and a working principle and process of a grill assembly. First, an aluminum grill main board 1 and a side bracket are manufactured. They are usually made of aluminum material and are cut, formed and processed to form a desired structure. Then, the aluminum grill main board 1 is punched to make the oil leakage strip holes 3 and square holes. The grinding machine is equipped with a wire drawing wheel, and the grinding machine is pushed back and forth along the aluminum grill main board 1 twice to grind the raised burrs at the strip holes 3 and the square holes. Then, two aluminum grill side brackets 2 are assembled and riveted at both ends of the aluminum grill main board 1 to form an aluminum grill assembly. The two aluminum grill side brackets 2 are assembled and riveted at both ends of the aluminum grill main board 1, and then the aluminum grill assembly is wiped with a clean cloth wetted with white kerosene to detect the appearance of the aluminum grill assembly. After the appearance meets the requirements, the aluminum grill assembly is surface anodized.
[0058] In the description of the present invention, it is necessary to understand that terms such as "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0059] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0060] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0061] Although the present invention is described in conjunction with the above specific embodiments, it is obvious that those skilled in the art can make many substitutions, modifications and changes according to the above content. Therefore, all such substitutions, improvements and changes are included in the spirit and scope of the appended claims.
Claims
1. A method for processing a grill, characterized in that: The steps include: Extruding the aluminum alloy billet into an aluminum mesh profile; Cut the aluminum mesh profile to form an aluminum grill mainboard; Punch out oil-leaking strip holes on the main board of the aluminum grill; Punch square holes at both ends of the aluminum grill mainboard; Assemble and rivet two aluminum grill side brackets to the two ends of the aluminum grill main board to form an aluminum grill assembly; The aluminum grill assembly is surface anodized.
2. The method for processing a grill according to claim 1, characterized in that: The aluminum grill main board comprises a first protrusion and a second protrusion with opposite protrusion directions, and the first protrusion and the second protrusion are continuously and alternately connected.
3. The method for processing a grill according to claim 2, characterized in that: The method of punching the oil-leaking strip holes on the main board of the aluminum grill comprises the following steps: Place the aluminum grill main plate with the first protrusion facing upward and the second protrusion facing downward on the first positioning groove of the first stamping machine, and make one end of the aluminum grill main plate close to the first positioning column of the first stamping machine; The first punching machine presses down to punch a plurality of strip holes on the second protrusion, and the strip holes are used for oil leakage.
4. The method for processing a grill according to claim 2, characterized in that: Punching square holes at both ends of the aluminum grill mainboard includes the following steps: Place one end of the aluminum grill mainboard on the second positioning groove of the second punching machine, so that the protruding direction of the first protruding portion faces downward and the protruding direction of the second protruding portion faces upward; Place one end of the aluminum grill mainboard against the second positioning column on the second punching machine, and press the second punching machine downward to punch a first square hole on one end of the second raised portion; Take out the aluminum grill main board and place the other end of it on the second positioning groove of the second punching machine, and the protruding directions of the first protrusion and the second protrusion remain unchanged; The second punching machine tool presses down to punch a second square hole at one end of the second protrusion.
5. The method for processing a grill according to claim 2, characterized in that: The step of assembling and riveting two aluminum grilling grid side brackets to the two ends of the aluminum grilling grid main board to form an aluminum grilling grid assembly includes the following steps: Pass both ends of the first protrusion through the connection holes on the first panels of the two aluminum grill side brackets respectively; The first protrusion of the first panel passing through the aluminum grilling grid side bracket is punched and expanded so that the first protrusion is riveted to the aluminum grilling grid side bracket.
6. The method for processing a grill according to claim 1, characterized in that: After punching square holes at both ends of the aluminum grill main board, the aluminum grill main board is also polished and brushed. The polisher is equipped with a wire drawing wheel and is pushed back and forth along the aluminum grill main board twice.
7. The method for processing a grill according to claim 6, characterized in that: Before the surface of the aluminum grill assembly is anodized, the aluminum grill assembly is fully cleaned and inspected. The aluminum grill assembly is wiped with a clean cloth moistened with white gasoline to inspect the appearance of the aluminum grill assembly.
8. The method for processing a grill according to claim 1, characterized in that: The surface of the aluminum grill assembly is anodized, and the thickness of the anodization is between 40 μm and 60 μm.
9. A barbecue grill assembly, characterized in that: The grill is manufactured by the grill processing method according to any one of claims 1 to 8, and comprises an aluminum grill main board and an aluminum grill side bracket, wherein the two aluminum grill side brackets are respectively connected to the two ends of the aluminum grill main board, and an oxide layer is formed on the surface of the aluminum grill main board and the aluminum grill side bracket, and the oxide layer is a hard anodized layer.
10. The barbecue grill assembly according to claim 9, characterized in that: The cross section of the first protrusion is in an inverted U shape, the protrusion direction of the second protrusion is opposite to the protrusion direction of the first protrusion, and the cross section of the second protrusion is in a V shape.