High-precision form and location tolerance machining process for composite pipe shell

Through pre-processing, hydrogen burning and adjustment of the central position process path, the problem of coaxiality in composite tube shell processing is solved, and high-precision shape and position tolerance processing is achieved to meet the precision assembly needs of traveling wave tubes.

CN118875655AActive Publication Date: 2024-11-01NANJING SANLE GROUP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411009423.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-01
Estimated Expiration
2044-07-26

AI Technical Summary

Technical Problem

After the composite tube shell is slowly wiping, the coaxial tolerance exceeds the difference, making it difficult to achieve the Φ0.01mm accuracy required by the design, mainly due to factors such as linearity difference, stress and correction error.

Method used

The process path of pre-processing inner diameter, measuring form and position tolerance, calculating hydrogen, and adjusting the center position after measurement, including processing pre-holes inside the composite tube shell, measuring coaxiality, calculating hydrogen to eliminate stress, and adjusting the center after measurement and straightening The position is processed by a slow wire cutting machine to retain the processing allowance for subsequent adjustment.

Benefits of technology

It effectively improves the coaxial accuracy of the composite tube shell, reaching Φ0.01mm, meets the high-precision assembly requirements of the traveling wave tube, and improves the overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118875655A_ABST
    Figure CN118875655A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of low-speed wire feeding machining, and provides a composite tube shell high-precision form and location tolerance machining technology which comprises the steps that a pre-hole is machined in a composite tube shell, and stress is released; measuring the coaxiality form and location tolerance of the pre-processed composite tube shell; the composite tube shell is straightened through hydrogen burning, and meanwhile stress is eliminated; the form and location tolerance of the straightened composite tube shell is measured, and the high-low point position change position of coaxiality measurement on the pole shoe is recorded; according to the recorded high and low point positions of the coaxiality, the center position of the machined composite pipe shell is adjusted; according to the machining method, in the machining process of the composite tube shell, through the technological modes of increasing the pre-machining inner diameter, measuring the form and location tolerance, conducting hydrogen burning and straightening on the composite tube shell, measuring the form and location tolerance after straightening and adjusting the position of a machining center, the high-precision form and location tolerance precision of the composite tube shell is achieved, and the coaxiality reaches phi 0.01 mm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of slow-wire machining, in particular to a high-precision shape and position tolerance machining process for a composite tube shell. Background Art

[0002] As a vacuum microwave power amplifier, the traveling wave tube has the advantages of wide bandwidth, large gain, and high output power. As an important device in the traveling wave tube, the slow wave system plays a role in standing wave interaction and forming the electron beam trajectory channel structure. In order to meet the performance index of the electron beam flow rate of a certain band traveling wave tube exceeding 98%, an integrated composite tube shell slow wave structure is designed, such as Figure 1 The figure shows the composite shell structure in a traveling wave tube, which is characterized by a length to aperture ratio (L: ΦD1) of 45. The composite shell is usually assembled and welded by magnetic screens, pole shoes, connecting rings and other parts. It is necessary to ensure that the coaxiality between the inner hole of the composite shell and the reference meets the requirement of φ0.01mm after the final processing. In order to realize the processing of an integrated composite shell with a large aspect ratio, it is necessary to improve the coaxiality form and position tolerance accuracy during the processing process.

[0003] At present, due to factors such as the straightness difference of the composite tube shell parts exceeding 0.04mm, stress inside the composite tube shell, and correction errors between the composite tube shell and the tooling, the composite tube shell with an aspect ratio of 45 is measured to have a coaxiality of Φ0.06-Φ0.1mm after one-time forming by wire-cutting. Therefore, the present invention proposes a high-precision form and position tolerance processing technology for the composite tube shell, which can solve the problem of coaxial form and position tolerance out-of-tolerance caused by one-time processing and forming through process paths such as pre-processing the inner diameter, measuring the form and position tolerance size, straightening the composite tube shell by hydrogen burning, measuring the form and position tolerance after straightening, adjusting the center position of the composite tube shell for final processing, etc., so that the form and position tolerance of the one-piece composite tube shell can reach high precision and meet the final coaxiality requirement of Φ0.01mm. Summary of the invention

[0004] The invention provides a high-precision shape and position tolerance processing technology for a composite tube shell, so as to solve the problem of excessive coaxial shape and position tolerances that is easily caused by one-time processing in the background technology.

[0005] The technical solution of the present invention is as follows:

[0006] A high-precision shape and position tolerance processing technology for a composite tube shell, comprising a magnetic shield, a pole shoe, a connecting ring, and an adapter constituting the composite tube shell, characterized in that it comprises the following steps:

[0007] S1: Pre-holes are machined inside the composite tube shell to release stress;

[0008] S2: Measure the coaxiality form and position tolerance of the composite tube shell after pre-processing;

[0009] S3: Burn hydrogen to straighten the composite tube shell and eliminate stress at the same time;

[0010] S4: Measure the shape and position tolerance of the composite tube shell after straightening, and record the change position of the high and low points on the pole shoe when measuring the coaxiality;

[0011] S5: According to the recorded high and low points of coaxiality, adjust the center position of the processed composite tube shell;

[0012] In S1, the composite tube shell is welded on the positioning core rod with ΦD as the positioning and clamping reference, and the tooling center is corrected to ensure the uniformity of the reference surface, which is conducive to improving the coaxiality of the composite tube shell. Then the ΦD1 size is processed and cut twice by a slow wire cutting machine, and a 0.1-0.3mm margin is reserved during processing to leave a processing margin for subsequent position adjustment;

[0013] In S2, the composite tube shell is supported by the ejectors at both ends of the coaxiality measuring instrument, and the outer contour surface of the pole shoe is measured with a dial indicator. The composite tube shell is rotated to read the coaxiality measurement data and recorded in the inspection card;

[0014] In S3, the composite tube shell is straightened in a hydrogen furnace using a mold used for welding the composite tube shell, which can eliminate the welding stress inside the composite tube shell and achieve the purpose of straightening by using the mold;

[0015] In S4, the outer contour surface of the pole shoe is measured again with a dial indicator, and the composite tube shell is rotated to read the coaxiality measurement data. At the same time, the positions of the highest point and the lowest point of the coaxiality on the outer circular contour of the pole shoe are marked during the measurement to provide an adjustment reference for subsequent operations;

[0016] In S5, the composite tube shell is welded on the positioning core rod with ΦD as the positioning and clamping reference, the tooling center is corrected, and according to the measurement results in S4, it is adjusted in the same direction at the position B where the coaxiality high point exists.

[0017] Preferably, the wire cutting machine in S1 uses a wire of Φ0.1 mm, the wire material is molybdenum wire, and the feed speed is 0.002-0.003 mm.

[0018] Preferably, the dial indicator head in S2 lightly contacts the measured surface so that the head has a compression of 1-2 mm, the composite tube shell is rotated 2-3 times, and the average value is recorded and calculated.

[0019] Preferably, the temperature in the hydrogen furnace in S3 is 450°C to 480°C.

[0020] Preferably, the mold in S3 includes a welding upper mold and a welding lower mold.

[0021] Preferably, the distance Δ value adjusted in S5 is 1 / 2× the coaxiality dimension.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. The present invention solves the problem of coaxiality out-of-tolerance in composite tube shell processing by adopting the methods of pre-processing inner diameter, measuring coaxiality after pre-processing, straightening the composite tube shell by burning hydrogen, measuring coaxiality after straightening, and adjusting the position of the processing center, so that the overall coaxiality of the composite tube shell reaches Φ0.01mm, meeting the design requirements, and plays a key role in the subsequent centering and assembly of the collector components, centering and assembly of the electron gun components, centering and assembly of the high-frequency band internal clamping rod and the spiral wire, etc. Under the premise of the high-precision assembly requirements of the traveling wave tube, the process path of the present invention can effectively improve the performance of the entire traveling wave tube. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 is a structural diagram of the composite tube shell of the present invention;

[0025] Figure 2 It is a schematic diagram of measuring the coaxiality of a pre-processed hole according to the present invention;

[0026] Figure 3 is a schematic diagram of the straightening composite tube shell of the present invention;

[0027] Figure 4 It is a schematic diagram of measuring the coaxiality deviation point of the present invention;

[0028] Figure 5 It is a flow chart of the process of the present invention.

[0029] In the figure:

[0030] 1. Pole shoe; 2. Ejector; 3. Dial indicator; 4. Welding upper die; 5. Welding lower die. DETAILED DESCRIPTION

[0031] The following embodiments of the present invention are described in further detail in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0032] Embodiment 1:

[0033] A high-precision shape and position tolerance processing technology for a composite tube shell comprises the following steps:

[0034] Step 1: Pre-holes are machined inside the composite tube shell to release stress; Figure 1 As shown, the composite tube shell is welded on the positioning core rod with ΦD as the positioning and clamping reference, and the tooling center is corrected to ensure the uniformity of the reference surface, which is beneficial to improve the coaxiality of the composite tube shell. Then the ΦD1 size is processed and cut twice by a slow-feed wire cutting machine, and a radial allowance of 0.1-0.3mm is retained during processing to leave a processing allowance for subsequent position adjustment.

[0035] Step 2: Measure the coaxiality and geometric tolerance of the composite tube shell after pre-processing; Figure 2 As shown, with ΦD1 as the reference axis, the ejector pins 2 at both ends of the coaxiality measuring instrument are pressed against the two ends of the pre-holes of the composite tube shell, and the dial indicator 3 head is lightly touched to the outer contour surface of the pole shoe 1, so that the head has a compression of 1-2mm, slowly rotate the composite tube shell 2-3 times and read the coaxiality measurement data, and record it in the inspection card, repeat the above steps, measure at different positions of the workpiece to obtain multiple data points, and calculate the average value.

[0036] Step 3: Burn hydrogen to straighten the composite tube shell and eliminate stress at the same time; Figure 3 As shown, the composite tube shell is straightened in a hydrogen furnace at 450℃~480℃ using the mold used for welding the composite tube shell: the composite tube shell is placed in a hydrogen furnace for preheating. The preheating temperature should be lower than the phase change temperature of the material to avoid excessive thermal stress. During the preheating process, pay attention to the deformation of the composite tube shell to prepare for the subsequent straightening operation; when the composite tube shell is preheated to the appropriate temperature, quickly install the welding upper mold 4 and the welding lower mold 5 on the tube shell, pay attention to the close fit between the mold and the composite tube shell to avoid new deformation; use the supporting force of the mold and Due to the thermoplasticity of the composite tube shell material, the composite tube shell is straightened. During the straightening process, force should be applied gradually to avoid excessive force at one time causing the tube shell to break. After the straightening is completed, the composite tube shell is kept warm in the hydrogen furnace for a period of time to make the internal structure of the composite tube shell fully stable. After the insulation is completed, the composite tube shell is taken out of the hydrogen furnace for natural cooling or controlled cooling. During the cooling process, rapid temperature changes should be avoided to avoid generating new thermal stress. This process can not only eliminate the internal welding stress of the composite tube shell, but also use the mold to achieve the purpose of straightening.

[0037] Step 4: Measure the form and position tolerances of the composite tube shell after straightening, and record the changes in the high and low points of the coaxiality measurement on the pole shoe 1; again use the dial indicator 3 head to gently touch the outer contour surface of the pole shoe 1, slowly rotate the tube shell 2-3 circles and read the coaxiality measurement data. Unlike S2, it is necessary to mark the highest and lowest points of the coaxiality on the outer contour of the pole shoe 1 during the measurement. This method provides an adjustment reference for subsequent operations.

[0038] Step 5: According to the high and low points of the recorded coaxiality, adjust the center position of the processed composite tube shell; Figure 4 As shown, the positioning and clamping method is consistent with that in S1. Figure 1The ΦD in S4 is used as the reference axis to calibrate the center position of the tooling. According to the measurement results in S4, the coaxiality error is calculated. The position B where the coaxiality high point exists is adjusted in the same direction. The adjustment distance Δ is 1 / 2× the coaxiality size. For example, the overall coaxiality of the composite tube shell measured at position B is Φ0.03mm, that is, the adjustment Δ value at position B is 0.015mm. The adjusted position is used as the center position of the composite tube shell for processing. Through this process, the shape and position tolerance accuracy of the composite tube shell can be effectively improved to meet the design requirement of Φ0.01mm.

[0039] like Figure 1-5 As shown, this embodiment adopts the method of pre-machining the inner diameter, measuring the coaxiality after pre-machining, straightening the composite tube shell by burning hydrogen, measuring the coaxiality after straightening, and adjusting the position of the machining center, which solves the problem of excessive coaxiality of the composite tube shell processing, so that the overall coaxiality of the tube shell reaches Φ0.01mm, meeting the design requirements.

[0040] The embodiments of the present invention are provided for the purpose of illustration and description. Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A high-precision geometric tolerance processing technology for a composite tube shell, comprising a pole shoe (1) constituting the composite tube shell, characterized in that: The following steps are involved: S1: Pre-holes are machined inside the composite tube shell to release stress; S2: Measure the coaxiality form and position tolerance of the composite tube shell after pre-processing; S3: Burn hydrogen to straighten the composite tube shell and eliminate stress at the same time; S4: measuring the shape and position tolerance of the composite tube shell after straightening, and recording the high and low point position changes of the coaxiality measurement on the pole shoe (1); S5: According to the recorded high and low points of coaxiality, adjust the center position of the processed composite tube shell; The step S1 includes: welding the composite tube shell onto the positioning core rod with ΦD as the positioning and clamping reference, correcting the tooling center, ensuring the uniformity of the reference surface, which is conducive to improving the coaxiality of the composite tube shell, and then processing the ΦD1 size, cutting it twice by a slow-feed wire cutting machine, and retaining a radial margin of 0.1-0.3mm during processing, so as to leave a processing margin for subsequent position adjustment; S2 comprises: using the ejector pins (2) at both ends of the coaxiality measuring instrument to support the composite tube shell, and using a dial indicator (3) to measure the outer contour surface of the pole shoe (1), rotating the composite tube shell to read the coaxiality measurement data, and recording it in the inspection card; S3 includes: using the mold used for welding the composite tube shell to perform a straightening treatment on the composite tube shell in a hydrogen furnace, which can not only eliminate the welding stress inside the composite tube shell, but also use the mold to achieve the purpose of straightening; The step S4 comprises: measuring the outer contour surface of the pole shoe (1) again with a dial indicator (3), rotating the composite tube shell to read the coaxiality measurement data, and marking the positions of the highest point and the lowest point of the coaxiality on the outer contour of the pole shoe (1) during the measurement to provide an adjustment reference for subsequent operations; The step S5 includes: welding the composite tube shell onto the positioning core rod with ΦD as the positioning and clamping reference, correcting the tooling center, and adjusting in the same direction at the position B where the coaxiality high point exists according to the measurement result in S4.

2. The high-precision shape and position tolerance processing technology of the composite tube shell according to claim 1, characterized in that: The S1 medium slow wire cutting machine uses a Φ0.1 mm wire, the wire material is molybdenum wire, and the feed speed is 0.002-0.003 mm.

3. The high-precision shape and position tolerance processing technology of the composite tube shell according to claim 1, characterized in that: The dial gauge (3) in S2 is lightly brought into contact with the surface to be measured, so that the gauge has a compression of 1-2 mm, the composite tube shell is rotated 2-3 times, and the average value is recorded and calculated.

4. The high-precision shape and position tolerance processing technology of the composite tube shell according to claim 1, characterized in that: The temperature in the hydrogen furnace in S3 is 450°C to 480°C.

5. The high-precision shape and position tolerance processing technology of the composite tube shell according to claim 1, characterized in that: The mold in S3 comprises a welding upper mold (4) and a welding lower mold (5).

6. The high-precision geometric tolerance processing technology for composite tube shells according to claim 1, characterized in that: The distance Δ value in S5 is adjusted to 1 / 2× the coaxiality dimension.

Citation Information

Patent Citations

  • Method for processing tungsten helical line of millimeter wave traveling-wave tube

    CN101694825A

  • Machining technology of stainless steel seamless steel tube for high-precision machine

    CN107378399A

  • Manufacturing method of high-thermal-conductivity and high-electric-conductivity corrosion-resistant composite board and composite board

    CN116175086A

  • Straightening method and mould for magnesium alloy thin-wall micropipe

    CN116274508A

  • Composite tube shell clamp for Q-band space traveling wave tube

    CN215787285U