Pressurizing equipment and process for injection molding production of plastic bucket
By designing injection molding parts, compensation parts and pressurization parts in plastic barrel injection molding production, and using components such as screw conveyor rods, springs and magnets, the problems of pressure leakage and pressure fluctuation of injection molding materials are solved, and adaptive compensation for pressure stability and Active pressurization improves molding quality.
Patent Information
- Application Number
- CN202410912701.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-11-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing plastic barrel injection molding production, the pressure of the injection molding material leaks and insufficient pressure progress, resulting in insufficient pressure fluctuations and affecting the molding quality.
A plastic barrel injection molding production and pressurization equipment including injection molding part, compensation part and pressurization part is designed. Through components such as screw conveying rod, spring, magnet and electromagnet, adaptive compensation and active pressurization of leakage pressure are achieved. Ensure pressure stability during injection molding.
It effectively avoids the formation of voids caused by pressure leakage, improves the pressure holding quality and injection efficiency, and ensures the stability and molding quality of the injection pressure.
Smart Images

Figure CN118876367A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plastic barrel processing, in particular to a plastic barrel injection molding production pressurizing device and process. Background Art
[0002] Plastic barrels are processed by injection molding. The injection molding process is often the gap between the inner mold and the outer mold. The injection molding material is injected into the gap to form a product.
[0003] According to the Chinese patent publication number CN220075414U, the patent provides a plastic barrel production pressurized mold, including a bracket, an outer mold, an inner mold, a feed pipe, an adjustment device 1 for driving the outer mold to move and an adjustment device 2 for driving the inner mold to move, the feed pipe is connected to the outer mold, and the bottom of the bracket is provided with a clearance hole opposite to the outer mold. The adjustment device 1 includes a driving part 1, a transmission wheel 1, a transmission wheel 2, a transmission belt, a transmission screw and a transmission nut 1. The driving part 1 is connected to the bracket, and the two transmission screws are rotatably connected to both sides of the bracket. The driving part 1 in the adjustment device 2 provides power for adjusting the height position of the outer mold. The driving part 1 drives the transmission wheel 1 and the transmission wheel 2 to rotate, and then drives the two transmission screws to rotate at the same time. The transmission screw drives the transmission nut 1 and the outer mold to adjust the upper and lower positions, and then adjusts the relative gap between the outer mold and the inner mold, which is convenient for adjusting the processing of plastic barrels with different heights and bottom thicknesses.
[0004] When the size of the above mold is adjusted, the cavity will change, so there will inevitably be a gap when the mold is docked, which will reduce the sealing when the injection port is connected to the mold, and then the pressure of the injection material will leak and the injection progress will be insufficient. There may be gaps in the molten plastic, affecting the molding quality. At the same time, the pressure fluctuations during the pressure holding period of the injection head will also be caused by pressure relief, which is not stable enough. Therefore, a plastic barrel injection production pressurization equipment and process are proposed to solve the above problems. Summary of the invention
[0005] 1. Technical issues to be solved
[0006] In view of the deficiencies in the prior art, the present invention provides a plastic barrel injection molding production pressurizing equipment and process, which solves the problem of pressure leakage and insufficient pressing of injection molding materials, resulting in unstable pressure fluctuations.
[0007] (II) Technical solution
[0008] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a plastic barrel injection molding production pressurizing equipment, including a horizontal injection molding machine and a barrel, the injection molding part is used to convey molten plastic for injection molding, the compensation part is used to adaptively compensate for leakage pressure during the molten plastic holding pressure period, the pressure holding part is used to adaptively hold pressure during the injection molding of the molten plastic, and the pressurizing part is used to automatically pressurize the molten plastic during injection molding.
[0009] Preferably, the injection molding part includes an injection molding head, which is attached to the inner wall of the barrel, and a material guide groove is provided on the outer wall of the injection molding head, and a through hole one is provided on the injection molding head, and a cross groove is provided on the inner wall of each through hole one, and an inner groove corresponding to the through hole one is provided on the inner wall of the injection molding head, and each of the inner grooves is connected with the corresponding through hole one, and each of the inner grooves is connected with the corresponding cross groove, and the middle part of each of the inner grooves is connected with each other, and a through hole two is provided in the middle part of the injection molding head, and a slide groove is provided in the middle part of the inner groove and is connected with the through hole two through the slide groove, and the slide groove is aligned with the through hole two, and a mounting groove is provided at one end of the injection molding head away from the through hole two.
[0010] Preferably, the inner wall of the mounting groove is connected with a screw conveying rod, the screw conveying rod is attached to the inner wall of the barrel, an output device is installed on the horizontal injection molding machine, the output device is connected to the barrel, and the screw conveying rod is installed on a motor in the output device.
[0011] Preferably, the compensation part is installed in the injection molding part, and the compensation part includes a limit plate 1, the limit plate 1 is connected to the inner wall of the through hole 1, a sliding rod 1 slides through the limit plate 1, a piston head is connected to one end of the sliding rod 1, the piston head fits the inner wall of the through hole 1, a steel ball is connected to the other end of the sliding rod 1, a spring 1 is elastically connected between the steel ball and the limit plate 1, and the steel ball fits the inner wall of the through hole 1.
[0012] Preferably, the number of the compensation parts is equal to the number of the second through holes, and each of the compensation parts is installed in the corresponding second through hole.
[0013] Preferably, the pressure-maintaining part is installed in the second through hole, and the pressure-maintaining part includes a second limiting plate, and the second limiting plate is connected to the inner wall of the second through hole. A sliding rod second slides through the second limiting plate, and one end of the second sliding rod is connected to a magnet and is sleeved with a sealing sleeve, and the other end of the second sliding rod is connected to a magnet, and a spring second is elastically connected between the second magnet and the second limiting plate.
[0014] Preferably, the outer wall of the magnet two is surrounded and connected with telescopic rods corresponding to the number of inner grooves, and the inner rod of each telescopic rod is connected with a sliding column, and each sliding column is slidably connected in the corresponding through hole one, and each sliding column is respectively abutted against the steel ball adjacent to itself, and each sliding column is connected with a cross slider, and each cross slider is slidably connected in the corresponding cross groove, and the inner wall of the slide groove is connected with magnet three, and the magnet three and magnet two repel each other with the same polarity.
[0015] Preferably, the pressurizing part includes a nozzle shell, a plastic injection port is opened in the middle of the nozzle shell, the inner wall of the plastic injection port is connected to a support rod, the support rod is connected to an electromagnet, the electromagnet is connected to an electric wire, the electric wire passes through the support rod and the nozzle shell to extend outward, the electromagnet is inserted into the inner wall of the through hole two and is attracted to the opposite sex of magnet one.
[0016] Preferably, the electromagnet is provided with a central opening, the outer wall of the barrel is provided with a heater, the nozzle shell is installed at the end of the heater, the nozzle shell is connected with the barrel through a spray port, a hopper is installed on the heater, the hopper is connected with the barrel, and the nozzle shell is installed on the clamping device of a horizontal injection molding machine.
[0017] A plastic barrel injection molding production pressurization process comprises the following steps:
[0018] S1. High-pressure polyethylene and polypropylene raw materials are mixed and melted, and composite particles for making plastic barrels are prepared by vacuum drying, so that the water content of the composite particles is reduced to between 0.06% and 0.09%;
[0019] S2, putting composite particles and additives from a hopper into a barrel, using a screw conveyor rod to convey the raw materials, and using a heater to heat the composite particles inside to plasticize them into a molten composite material melt, wherein the additives are plasticizers, antioxidants, antistatic agents, and lubricants;
[0020] S3, the temperature of the initial section of the barrel is between 145℃-180℃, the temperature of the middle section of the barrel is between 220℃-285℃, and the temperature of the front section of the barrel to the nozzle is between 235℃-300℃. The preload force of the spring 1 in the compensation part is used to drive the piston head to extrude the composite melt in the area from the front section of the barrel to the nozzle, thereby compensating for the loss pressure during the holding period. The pressure in the holding stage is between 10-20MPa;
[0021] S4. Use an electromagnet to attract the magnet to force the pressure-holding part to drive the compensation part to reset, and then actively apply pressure during injection, so that the composite material melt is stably injected from the injection port through the injection head into the clamping device for cooling and molding. The clamping temperature is between 20℃-60℃, the injection pressure is between 50-150MPa, and the pressure is increased by 1-10MPa based on the injection pressure.
[0022] (III) Beneficial effects
[0023] Compared with the prior art, the present invention provides a plastic barrel injection molding production pressurization equipment and process, which has the following beneficial effects:
[0024] 1. The pressurizing equipment and process for injection molding production of plastic barrels adopts the centrifugal force of the spiral conveying rod to increase the capacity of the through hole to absorb the molten liquid. The spring loses the centrifugal drive and converts it into its own internal preload force to drive the steel ball to reset, and provides a certain thrust to the molten plastic in the through hole, compensating for the pressure relief of the molten plastic in the front section of the barrel, avoiding the formation of gaps in the molten plastic due to pressure leakage and reducing the pressure holding quality.
[0025] 2. The plastic barrel injection molding production pressurizing equipment and process adopts magnet three to always repel magnet two with the same polarity to generate reverse thrust. Under the influence of the repulsive force, the sliding column is driven to slide toward the steel ball through the telescopic rod, thereby forming an extrusion force on the steel ball, improving the contraction efficiency of spring one, and increasing the pressure of the piston head on the molten plastic. The piston head and the sliding column are used to pressurize the molten plastic twice in succession, thereby improving the efficiency of pressure compensation and avoiding the problem of irreparable pressure loss due to pressure relief.
[0026] 3. The plastic barrel injection molding production pressurizing equipment and process adopts repulsive force to push magnet 2 away from magnet 3. Spring 2 contracts under the action of its own internal preload and pushes magnet 1 to reset through slide bar 2. Magnet 1 is blocked from resetting due to the pressure of molten plastic, thereby generating thrust pressurization. At the same time, repulsive force will also improve the contraction efficiency of spring 2, further prompting magnet 1 to pressurize the molten plastic, again improving the problem of insufficient pressure caused by pressure relief. The adaptive pressure relief volume compensates the pressure of the molten plastic in the front section of the barrel, making the material tight and tight during the pressure holding process.
[0027] 4. The plastic barrel injection molding production pressurizing equipment and process adopts an electromagnet inserted into the through hole two, forcibly adsorbing magnet one so that magnet one is forced to reset and drive the sliding column to force reset, the sliding column forcibly squeezes the steel ball to force the piston head to reset, and then the molten plastic in the through hole one and the through hole two is forced to be squeezed outward, thereby producing an active pressurizing effect, increasing the injection pressure during injection molding, further improving the injection efficiency, and at the same time further compensating for the pressure relief caused by the mold splicing gap during injection molding, ensuring the stability of the injection pressure, and improving the injection quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 This is a schematic diagram of the overall structure of a plastic barrel injection molding production pressurizing equipment proposed by the present invention;
[0029] Figure 2 A cross-sectional view of a heater and a barrel of a pressurizing device for injection molding of a plastic barrel proposed by the present invention;
[0030] Figure 3 This is a structural schematic diagram of a nozzle shell and an injection molding head of a plastic barrel injection molding production pressurizing equipment proposed by the present invention;
[0031] Figure 4 A cross-sectional view of an injection molding head of a pressurizing equipment for injection molding of a plastic barrel proposed by the present invention;
[0032] Figure 5 This is a connection diagram of an injection molding head and a spiral conveying rod of a plastic barrel injection molding production pressurizing equipment proposed by the present invention;
[0033] Figure 6 A plastic barrel injection molding production pressurizing equipment proposed by the present invention Figure 5 A magnified view of middle;
[0034] Figure 7 This is a structural schematic diagram of a compensating part of a plastic barrel injection molding production pressurizing equipment proposed by the present invention;
[0035] Figure 8 This is a connection diagram of the compensation part and pressure-holding part of a plastic barrel injection molding production pressurizing equipment proposed by the present invention and the injection molding head.
[0036] In the figure: 1. horizontal injection molding machine; 2. output device; 3. heater; 4. barrel; 5. injection molding part; 51. injection molding head; 52. material guide groove; 53. through hole 1; 54. cross groove; 55. inner groove; 56. through hole 2; 57. slide groove; 58. installation groove; 6. screw conveying rod; 7. compensation part; 71. limit plate 1; 72. slide bar 1; 73. piston head; 74. steel ball; 75. spring 1; 8. pressure holding part; 81. limit plate 2; 82. slide bar 2; 83. magnet 1; 84. magnet 2; 85. spring 2; 86. telescopic rod; 87. slide column; 88. cross slide block; 89. magnet 3; 9. pressurizing part; 91. nozzle shell; 92. spray nozzle; 93. support rod; 94. electromagnet; 95. wire; 10. hopper. DETAILED DESCRIPTION
[0037] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0038] See also Figure 1-8The present invention provides a technical solution: a plastic barrel injection molding production pressurizing equipment, including a horizontal injection molding machine 1 and a barrel 4, the barrel 4 is one of the components of the horizontal injection molding machine 1, the injection molding part 5 is used to convey molten plastic for injection molding, the compensation part 7 is used to adaptively compensate for the leakage pressure during the molten plastic holding pressure period, the pressure holding part 8 is used to adaptively hold the leakage pressure during the molten plastic injection molding, and the pressurizing part 9 is used to automatically pressurize the molten plastic during the injection molding.
[0039] In the present invention, in order to increase the capacity of the molten plastic in the pressure holding zone of the barrel 4 and use the extra capacity to achieve the purpose of pressurization, the injection molding part 5 of this case includes an injection molding head 51, and the injection molding head 51 is attached to the inner wall of the barrel 4. The outer wall of the injection molding head 51 is surrounded by a guide groove 52, and the guide groove 52 is used to guide the molten plastic to flow to the front section of the barrel 4. The guide groove 52 adopts a wedge-shaped structure and an arc surface structure, which can effectively reduce the problem of adhesion and hysteresis of the molten plastic. A through hole 53 is surrounded on the injection molding head 51, and a larger capacity of molten plastic is stored in the through hole 53. A cross groove 54 is opened on the inner wall of each through hole 53. An inner groove 55 corresponding to the through hole 53 is opened on the inner wall of the injection molding head 51. Each inner groove 55 is connected to the corresponding through hole 53, and each inner groove 55 is connected to the corresponding cross groove 54. The middle part of each inner groove 55 is connected to each other. A through hole 56 is provided in the middle of the injection molding head 51, and a larger capacity of molten plastic is stored in the through hole 56. A slide groove 57 is provided in the middle of the inner groove 55 and is connected to the through hole 56 through the slide groove 57. The slide groove 57 is aligned with the through hole 56. A mounting groove 58 is provided at one end of the injection molding head 51 away from the through hole 56. A screw conveying rod 6 is connected to the inner wall of the mounting groove 58. A check valve is installed on the screw conveying rod 6, which is a matching component of the prior art structure. Its purpose is to prevent the molten plastic from flowing back. Therefore, it is not described in detail in this case. The screw conveying rod 6 is attached to the inner wall of the barrel 4. An output device 2 is installed on the horizontal injection molding machine 1. The output device 2 is one of the components of the horizontal injection molding machine 1. The output device 2 is connected to the barrel 4. The screw conveying rod 6 is installed on the motor in the output device 2, and is connected and driven by the motor and the screw conveying rod 6.
[0040] In this embodiment, in order to ensure the pressure stability of the molten plastic in the pressure holding area of the barrel 4, the compensation part 7 of this case is installed in the injection molding part 5, and the compensation part 7 includes a limit plate 71, and the limit plate 71 is fixedly connected to the inner wall of the through hole 53. A slide rod 72 slides through the limit plate 71, and a piston head 73 is connected to one end of the slide rod 72. The piston head 73 fits the inner wall of the through hole 53. The piston head 73 slides against the inner wall of the through hole 53 to prevent the molten plastic from flowing into the inner groove 55. The other end of the slide rod 72 A steel ball 74 is connected to one end, and the weight of the steel ball 74 is greater than the weight of the piston head 73. The centrifugal force of the spiral conveying rod 6 can generate a force for oblique upward movement. A spring 75 is elastically connected between the steel ball 74 and the limiting plate 71. The steel ball 74 fits on the inner wall of the through hole 1 53. The number of compensation parts 7 is equal to the number of through holes 2 56. Each compensation part 7 is respectively installed in the corresponding through hole 2 56. Each through hole 2 56 can store molten plastic, and the pressure on the molten plastic is increased through each piston head 73.
[0041] It is worth noting that in order to further improve the pressure stability of the molten plastic during the pressure holding period, the pressure holding part 8 of this case is installed in the second through hole 56, and the pressure holding part 8 includes a second limiting piece 81, and the second limiting piece 81 is connected to the inner wall of the second through hole 56. A second slide bar 82 slides through the second limiting piece 81, and one end of the second slide bar 82 is connected to a magnet 83 and is covered with a sealing sleeve. The sealing sleeve prevents liquid from invading the inner groove 55. The other end of the second slide bar 82 is connected to a second magnet 84, and a second spring 85 is elastically connected between the second magnet 84 and the second limiting piece 81. The outer wall of the second magnet 84 is surrounded by telescopic rods 86 corresponding to the number of the inner grooves 55, and each telescopic rod 86 has a The inner rods are all connected with sliding posts 87. When sliding posts 87 slide under the centrifugal force, they can automatically drive the telescopic rod 86 to perform telescopic adjustment to avoid the sliding posts 87 getting stuck on the inner wall of the through hole 2 56. Each sliding post 87 is respectively slidably connected in the corresponding through hole 1 53. Each sliding post 87 is respectively abutted against the steel ball 74 adjacent to itself. Each sliding post 87 is connected with a cross slider 88. Each cross slider 88 is respectively slidably connected in the corresponding cross groove 54. The inner wall of the slide groove 57 is connected with magnet 3 89. Magnet 3 89 and magnet 2 84 repel each other with the same polarity. The repulsive force generated by the same polarity improves the contraction efficiency of spring 2 85, prompting magnet 1 83 to pressurize the molten plastic.
[0042] It is worth noting that in order to further reduce the problem of unstable pressure caused by pressure relief during injection of molten plastic, the pressurizing part 9 of the present invention includes a nozzle shell 91, a spray port 92 is provided in the middle of the nozzle shell 91, and the spray port 92 is the injection port for injecting molten plastic into the mold cavity. The inner wall of the spray port 92 is connected to a support rod 93, and an electromagnet 94 is connected to the support rod 93. The support rod 93 is used to suspend and fix the electromagnet 94 and will not block the spray port 92. The electromagnet 94 is connected to an electric wire 95, which passes through the support rod 93 and the nozzle shell 91 to extend outward, and the electric wire 95 passes through the support rod 93 and the nozzle shell 91 to extend outward. The external power supply provides power to the electromagnet 94, and the electromagnet 94 is inserted into the inner wall of the through hole 2 56 and is attracted to the magnet 1 83 by opposite charges. The suction force generated by the opposite charges can force the magnet 1 83 to be adsorbed and force the spring 2 85 to be tightened. The middle part of the electromagnet 94 is provided with an opening, and the outer wall of the barrel 4 is provided with a heater 3. The nozzle shell 91 is installed at the end of the heater 3. The nozzle shell 91 is connected to the barrel 4 through the injection port 92. The heater 3 is provided with a hopper 10, and the hopper 10 is connected to the barrel 4. The nozzle shell 91 is installed on the clamping device of the horizontal injection molding machine 1.
[0043] A plastic barrel injection molding production pressurization process comprises the following steps:
[0044] S1. High-pressure polyethylene and polypropylene raw materials are mixed and melted, and composite particles for making plastic barrels are prepared by vacuum drying, so that the water content of the composite particles is reduced to between 0.06% and 0.09%;
[0045] S2, putting composite particles and additives from the hopper 10 into the barrel 4, using the screw conveying rod 6 to convey the raw materials, and heating the composite particles inside the barrel 3 to plasticize them into a molten composite material melt, wherein the additives are plasticizers, antioxidants, antistatic agents, and lubricants;
[0046] S3, the temperature of the initial section of the barrel 4 is between 145°C and 180°C, the temperature of the middle section of the barrel 4 is between 220°C and 285°C, and the temperature of the front section of the barrel 4 to the nozzle is between 235°C and 300°C. The preload force of the spring 75 in the compensation part 7 is used to drive the piston head 73 to extrude the composite melt in the area from the front section of the barrel 4 to the nozzle, thereby compensating for the loss pressure during the holding period. The pressure in the holding stage is between 10-20MPa;
[0047] S4. The electromagnet 94 is used to attract the magnet 83 to force the pressure holding part 8 to drive the compensation part 7 to reset, and then actively pressurize during injection, and then the composite material melt is stably injected into the clamping device from the injection port 92 through the injection head 51 for cooling and molding. The clamping temperature is between 20°C and 60°C, the injection pressure is between 50-150MPa, and the pressure is increased by 1-10MPa based on the injection pressure.
[0048] Working principle: composite particles for making plastic barrels are prepared through vacuum drying, and the composite particles and additives are put into the barrel 4 from the hopper 10. The output device 2 is used to control the screw conveying rod 6 to convey the raw materials. The output device 2 is one of the components of the horizontal injection molding machine 1 in the prior art. The motor is used to control the screw conveying rod 6 to work, so no further description is given in this case. The heater 3 heats the composite particles inside the barrel 4 to plasticize them into a molten composite material melt. The screw conveying rod 6 rotates to drive the injection head 51 to rotate, thereby generating centrifugal force in the through hole 53. The elasticity of the spring 75 is used to drive the steel ball 74 to move obliquely upward in the through hole 53 under the drive of the centrifugal force, and then the piston head 73 is driven by the slide rod 72 to rise obliquely in the through hole 53. At this time, the piston head 73 is away from the inner angle of the through hole 53, thereby increasing the volume that the liquid in the through hole 53 can enter. The molten plastic continuously fills the front section of the barrel 4 to the nozzle area, thereby squeezing the screw conveying rod 6 to make its rear The molten plastic will fill the front section of the barrel 4 and continue to flow into each through hole 53. Different from the prior art, the present invention utilizes the through hole 53 to increase the liquid capacity between the barrel 4 and the injection head 51, and continues to pull the piston head 73 to slide under the action of centrifugal force, further increasing the capacity of the through hole 53 to absorb the molten liquid. As a result, after the spiral conveying rod 6 stops rotating, the spring 75 loses the centrifugal drive and is converted into its own inherent preload force to drive the steel ball 74 to reset, and then pushes the piston head 73 to reset to the angle inside the through hole 53 through the slide rod 72. However, at this time, since the front section of the barrel 4 is filled with molten plastic, the liquid in the through hole 53 is in a state of being blocked by pressure, and the piston head 73 cannot be completely reset, but continuously contracts the spring 75 and provides a certain thrust to the molten plastic in the through hole 53. The pressure generated under the thrust can compensate for the pressure relief of the molten plastic in the front section of the barrel 4, thereby avoiding the formation of gaps in the molten plastic and reducing the pressure holding quality due to pressure leakage.
[0049] While the compensation part 7 is used to perform pressure compensation to maintain the pressure holding quality, the magnet three 89 in the pressure holding part 8 always repels the magnet two 84 with the same polarity and generates a reverse thrust. In the state without centrifugal force, the magnet two 84 is affected by the repulsive force and drives the sliding column 87 to slide toward the steel ball 74 through the telescopic rod 86, thereby forming an extrusion force on the steel ball 74, further improving the contraction efficiency of the spring one 75, and then increasing the pressure of the piston head 73 on the molten plastic. Different from the prior art, the present case utilizes the piston head 73 and the sliding column 87 to pressurize the molten plastic twice in a row, thereby improving the efficiency of pressure compensation and avoiding the problem of irreparable pressure loss due to pressure relief. At the same time, the elastic force of the spring one 75 and the repulsive force generated between the magnet two 84 and the magnet three 89 are used as the power, which replaces the traditional mode that needs to rely on other load equipment to achieve the pressurization effect, further reducing load loss and saving energy.
[0050] The pressure-maintaining portion 8 is also affected by the centrifugal force when the spiral conveying rod 6 rotates. The cross slider 88 slides in the cross groove 54 and drives the slide column 87 to tilt and rise, thereby pulling the telescopic rod 86 to extend, and then pulling the spring 2 85 through the magnet 2 84, so that the magnet 2 84 is constantly approaching the magnet 3 89 under the action of the centrifugal force. According to the above reasoning, the liquid in the through hole 2 56 can enter the capacity due to the increase in the sliding of the magnet 1 83, and the sealing sleeve prevents the liquid from invading the inner groove 55. Under the action of the centrifugal force, the slide column 87 will tilt and rise synchronously with the steel ball 74, so there will be no problem that the steel ball 74 is restricted and cannot slide. On the other hand, when the spiral conveying rod 6 is stopped, the centrifugal force disappears, and the repulsive force causes the magnet 83 to move. Iron 2 84 is away from magnet 3 89, spring 2 85 contracts under the action of its own internal preload and pushes magnet 1 83 to reset through slide bar 2 82. Magnet 1 83 is blocked from resetting due to the pressure of the molten plastic, thereby generating thrust pressurization. At the same time, repulsion will also increase the contraction efficiency of spring 2 85, further prompting magnet 1 83 to pressurize the molten plastic. On the basis of the above-mentioned two pressurizations of the molten plastic by the piston head 73 and the slide column 87, magnet 1 83 will also produce two pressurization processes for the molten plastic under the influence of spring 2 85 and repulsion, once again improving the problem of insufficient pressure caused by pressure relief. The adaptive pressure relief amount compensates the pressure of the molten plastic in the front section of the barrel 4, so that the material is tight and tight during the pressure holding process.
[0051] During injection molding, the movable mold and the fixed mold in the prior art mold clamping device are combined to connect the mold cavity to the injection port 92. The spiral conveying rod 6 does not rotate and slides in the barrel 4 to push the molten plastic in the pressure holding state, so that the molten plastic enters the mold cavity through the injection port 92 for filling and cooling. When the injection head 51 approaches the nozzle shell 91, the electromagnet 94 is inserted into the second through hole 56. The middle opening of the second through hole 56 can promote the molten plastic in the second through hole 56 to flow out smoothly without causing the problem of sealing blockage. The electromagnet 94 penetrates into the hole and approaches the magnet 1 83, and passes the wire 95 When electricity is connected, the magnetism of the electromagnet 94 is increased, thereby forcibly adsorbing the magnet 1 83, so that the magnet 1 83 is forced to reset and drives the slide column 87 to reset. At the same time, the slide column 87 forces the steel ball 74 to force the piston head 73 to reset, and then the molten plastic in the through hole 1 53 and the through hole 2 56 is forced to be squeezed outward, thereby producing an active pressurization effect, increasing the injection pressure during injection molding, further improving the injection efficiency, and further compensating for the pressure relief caused by the mold splicing gap during injection molding, ensuring the stability of the injection pressure, and improving the injection quality.
[0052] In this case, the temperature of the barrel 4 does not exceed 300°C. The magnets involved in this case can be neodymium iron boron magnets, cobalt steel magnets, etc., and their Curie temperatures are at least between 310°C and 875°C, thus fully meeting the basic requirements for use during injection molding in this case.
[0053] On the other hand, plasticizers can increase the softness, extensibility, and plasticity of plastics by weakening the van der Waals forces between polymer molecules, thereby increasing the mobility of polymer molecular chains and reducing the crystallinity of polymer molecular chains, while reducing the flow temperature and hardness of plastics, which is beneficial to the molding of plastic products.
[0054] Antioxidants are a class of chemical substances that, when present in a small amount in a polymer system, can delay or inhibit the oxidation process of the polymer, thereby increasing the service life of the polymer.
[0055] Generally, they have the characteristics of surfactants, with both polar and non-polar groups in their structure, which can guide and eliminate the accumulated harmful charges so that they do not cause inconvenience or harm to production or life.
[0056] Lubricants can improve the friction and adhesion between the particles of each layer of plastic and between the melt and the metal surface of the processing equipment, increase the fluidity of the resin, and achieve adjustable resin plasticization time.
[0057] The quality of the finished plastic barrel can be improved by mixing the above additives with the composite particles for melt injection molding.
[0058] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "including one..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.
Claims
1. A plastic barrel injection molding production pressurizing equipment, characterized in that: include: Horizontal injection molding machine (1); Barrel (4); An injection molding section (5) for conveying molten plastic for injection molding; A compensation part (7) is used to adaptively compensate for leakage pressure during the period of holding pressure of the molten plastic; A pressure holding portion (8) is used to adaptively hold the leakage pressure during the injection of molten plastic; The pressurizing part (9) is used to automatically pressurize the molten plastic during injection molding.
2. A plastic barrel injection molding production pressurizing equipment according to claim 1, characterized in that: The injection molding part (5) comprises an injection molding head (51), the injection molding head (51) is attached to the inner wall of the barrel (4), the outer wall of the injection molding head (51) is surrounded by a material introduction groove (52), the injection molding head (51) is surrounded by a through hole (53), the inner wall of each through hole (53) is provided with a cross groove (54), the inner wall of the injection molding head (51) is surrounded by an inner groove (55) corresponding to the through hole (53), each of the inner grooves (55) is respectively connected to the corresponding through hole (53). The inner grooves (55) are connected to the corresponding cross grooves (54), and the middle parts of the inner grooves (55) are connected to each other. The middle part of the injection head (51) is provided with a second through hole (56). The middle part of the inner grooves (55) is provided with a slide groove (57) and is connected to the second through hole (56) through the slide groove (57). The slide groove (57) is aligned with the second through hole (56), and the injection head (51) is provided with a mounting groove (58) at one end away from the second through hole (56).
3. A plastic barrel injection molding production pressurizing equipment according to claim 2, characterized in that: The inner wall of the mounting groove (58) is connected to a screw conveying rod (6), and the screw conveying rod (6) is attached to the inner wall of the barrel (4). An output device (2) is installed on the horizontal injection molding machine (1), and the output device (2) is connected to the barrel (4), and the screw conveying rod (6) is installed on a motor in the output device (2).
4. The plastic barrel injection molding production pressurizing equipment according to claim 3 is characterized by: The compensation part (7) is installed in the injection molding part (5), and the compensation part (7) includes a limit plate (71), the limit plate (71) is connected to the inner wall of the through hole (53), a slide rod (72) slides through the limit plate (71), one end of the slide rod (72) is connected to a piston head (73), the piston head (73) fits the inner wall of the through hole (53), the other end of the slide rod (72) is connected to a steel ball (74), a spring (75) is elastically connected between the steel ball (74) and the limit plate (71), and the steel ball (74) fits the inner wall of the through hole (53).
5. The plastic barrel injection molding production pressurizing equipment according to claim 4, characterized in that: The number of the compensating parts (7) is equal to the number of the second through holes (56), and each of the compensating parts (7) is respectively installed in the corresponding second through hole (56).
6. The plastic barrel injection molding production pressurizing equipment according to claim 5, characterized in that: The pressure-maintaining portion (8) is installed in the second through hole (56), and the pressure-maintaining portion (8) includes a second limiting plate (81), the second limiting plate (81) is connected to the inner wall of the second through hole (56), a second sliding rod (82) slides through the second limiting plate (81), one end of the second sliding rod (82) is connected to a first magnet (83) and is sleeved with a sealing sleeve, the other end of the second sliding rod (82) is connected to a second magnet (84), and a second spring (85) is elastically connected between the second magnet (84) and the second limiting plate (81).
7. The plastic barrel injection molding production pressurizing equipment according to claim 6, characterized in that: The outer wall of the second magnet (84) is connected with a number of telescopic rods (86) corresponding to the number of the inner grooves (55), and the inner rod of each telescopic rod (86) is connected with a slide column (87), and each slide column (87) is slidably connected in the corresponding through hole (53), and each slide column (87) is respectively abutted against the steel ball (74) adjacent to itself, and each slide column (87) is connected with a cross slider (88), and each cross slider (88) is slidably connected in the corresponding cross groove (54), and the inner wall of the slide groove (57) is connected with a magnet three (89), and the magnet three (89) and the magnet two (84) repel each other with the same polarity.
8. The plastic barrel injection molding production pressurizing equipment according to claim 7, characterized in that: The pressurizing part (9) comprises a nozzle shell (91), a plastic spraying port (92) is provided in the middle of the nozzle shell (91), the inner wall of the plastic spraying port (92) is connected with a support rod (93), the support rod (93) is connected with an electromagnet (94), the electromagnet (94) is connected with an electric wire (95), the electric wire (95) passes through the support rod (93) and the nozzle shell (91) and extends outward, the electromagnet (94) is plugged into the inner wall of the second through hole (56) and is attracted to the first magnet (83) by opposite charges.
9. The plastic barrel injection molding production pressurizing equipment according to claim 8, characterized in that: The electromagnet (94) is provided with an opening in the middle, the outer wall of the barrel (4) is provided with a heater (3), the nozzle shell (91) is installed at the end of the heater (3), the nozzle shell (91) is connected to the barrel (4) through a spray port (92), a hopper (10) is installed on the heater (3), the hopper (10) is connected to the barrel (4), and the nozzle shell (91) is installed on a mold clamping device of a horizontal injection molding machine (1).
10. A plastic barrel injection molding production pressurization process, characterized in that: The plastic barrel injection molding production pressurizing equipment according to claim 9 comprises the following steps: S1. High-pressure polyethylene and polypropylene raw materials are mixed and melted, and composite particles for making plastic barrels are prepared by vacuum drying, so that the water content of the composite particles is reduced to between 0.06% and 0.09%; S2, putting composite particles and additives from a hopper (10) into a barrel (4), using a screw conveying rod (6) to convey the raw materials, and using a heater (3) to heat the composite particles inside to plasticize them into a molten composite material melt, wherein the additives are plasticizers, antioxidants, antistatic agents, and lubricants; S3, the temperature of the starting section of the barrel (4) is between 145°C and 180°C, the temperature of the middle section of the barrel (4) is between 220°C and 285°C, and the temperature of the front section to the nozzle of the barrel (4) is between 235°C and 300°C. In the area from the front section to the nozzle of the barrel (4), the preload force of the spring 1 (75) in the compensation part (7) is used to drive the piston head (73) to extrude the composite material melt, thereby compensating for the loss pressure during the holding period. The pressure in the holding stage is between 10 and 20 MPa. S4. Using an electromagnet (94) to attract magnet one (83) causes the pressure-holding part (8) to drive the compensation part (7) to be forced to reset, thereby actively applying pressure during injection, and then allowing the composite material melt to be stably injected into the mold clamping device through the injection head (51) from the injection port (92) for cooling and molding. The mold clamping temperature is between 20°C and 60°C, the injection pressure is between 50 and 150 MPa, and the pressure is increased by 1 to 10 MPa based on the injection pressure.