Semiconductor structure deposition method, computer program product and computer device
By setting multiple stations in the reaction chamber and transferring wafers in sequence for nucleation and bulk deposition, the high cost and long process time-consuming problems of the existing tungsten metal deposition process are solved, and a more efficient tungsten metal deposition process is achieved. , reduces costs and improves output efficiency.
Patent Information
- Application Number
- CN202410912459.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-07-08
AI Technical Summary
The existing tungsten metal deposition process has problems of high cost and long process time-consuming, especially because the nucleation process is completed faster than the bulk deposition process, resulting in wait phenomena and process costs.
By setting up multiple stations isolated from each other in the reaction chamber, the wafer is transferred in sequence for nucleation and bulk deposition, ensuring that the same gas is always inflowing into each station, reducing the need for high-cost high-speed switching valves, and After the nucleation is completed, the body deposition is carried out uniformly to eliminate the waiting phenomenon.
It has achieved the reduction of process costs, shortened process time, and improved output efficiency. The current output of 80 pieces/hour is increased to 106 pieces/hour, and 8 high-speed switching valves are saved to achieve the effect of cost reduction and efficiency improvement.
Smart Images

Figure CN118880282A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing technology, and in particular to a semiconductor structure deposition method, a computer program product and a computer device. Background Art
[0002] In the contact window process, the contact hole is filled with tungsten, that is, the contact hole is filled with tungsten metal by tungsten metal deposition to form a tungsten plug. The tungsten metal deposition process mainly has two steps: the first step is nucleation, which mainly uses the atomic layer deposition (ALD) process to nucleate the inner wall of the contact hole; the second step is bulk deposition, which mainly uses the chemical vapor deposition (CVD) process with higher hole filling ability to fill the contact hole with tungsten to form a tungsten plug. In order to reduce the resistance value, the industry has done a lot of work on these two steps.
[0003] See also Figure 1, which is a schematic diagram of the working mode of the reaction chamber of the existing tungsten metal deposition process, and numbers 1 to 4 indicate stations 1 to 4 of the reaction chamber 10. The existing tungsten metal deposition process is divided into steps. The first step of the nucleation process is completed in four steps and multiple cycles in time sequence at stations 1 and 2 of the reaction chamber using a similar atomic layer deposition method; the second step of the bulk deposition process is completed at stations 3 and 4 of the reaction chamber using a chemical vapor deposition method. Specifically, taking the simultaneous operation of 4 wafers as an example, the flow of the existing tungsten metal deposition process is as follows: (1) Wafer 1 controls the flow of the first reaction gas of the first process time (extremely short) through the ALD high-speed switch valve (Valve) at station 1 of the reaction chamber, then flows the purge gas of the second process time, then controls the flow of the second reaction gas of the third process time (extremely short) through the ALD high-speed switch valve, and finally flows the purge gas of the fourth process time; after several such cycles, preliminary nucleation is formed. (2) Wafer 1 is transferred to station 2 of the reaction chamber, and wafer 2 is transferred to station 1. Stations 1 and 2 simultaneously perform the above step (1) ALD nucleation; thus, wafer 1 completes nucleation after re-nucleation, and wafer 2 undergoes preliminary nucleation. (3) Wafer 1 is transferred to station 3 of the reaction chamber, wafer 2 is transferred to station 2, wafer 3 is transferred to station 1, station 3 performs CVD film formation, and stations 1 / 2 simultaneously perform the above step (1) ALD nucleation; thereby, wafer 1 is initially film-formed, wafer 2 is nucleated again and nucleation is completed, and wafer 3 is initially nucleated; (4) Wafer 1 is transferred to station 4 of the reaction chamber, wafer 2 is transferred to station 3, wafer 3 is transferred to station 2, and wafer 4 is transferred to station 1, stations 3 and 4 simultaneously perform CVD film formation, and stations 1 and 2 simultaneously perform the above step (1) ALD nucleation; thereby, wafer 1 is film-formed again and film formation is completed (bulk deposition is completed), wafer 2 is initially film-formed, wafer 3 is nucleated again and nucleation is completed, and wafer 4 is initially nucleated.
[0004] Since workstation 1 / 2 is the same workstation and different reaction gases and purge gases are introduced into the ALD process in chronological order, an ALD high-speed switch valve needs to be set at the gas inlet to control the flow of reaction gases, which increases the process cost. At the same time, since the tungsten nucleation process is completed faster than the bulk deposition process, the above steps (3)-(4) all need to wait for the bulk deposition to be completed before proceeding to the next step, which makes the process time-consuming and affects the output.
[0005] Therefore, it is necessary to provide a method that can achieve a rapid tungsten metal deposition process. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a semiconductor structure deposition method, a computer program product and a computer device, which can achieve cost reduction and efficiency improvement of the metal deposition process by optimizing the metal deposition scheme.
[0007] In order to solve the above problems, the present invention provides a semiconductor structure deposition method, comprising: providing a reaction chamber, the reaction chamber at least comprising a first station, a second station and a purge station isolated from each other; performing a nucleation process, transferring multiple wafers to the first station, the purge station, the second station and the purge station in sequence, and cycling a preset number of times to complete the nucleation of the semiconductor structure, wherein the first station continuously introduces a first nucleation reaction gas, the second station continuously introduces a second nucleation reaction gas, and the purge station continuously introduces a purge gas; and performing a body deposition process, stopping the introduction of the first nucleation reaction gas, the second nucleation reaction gas and the purge gas, placing a wafer after nucleation on each station of the reaction chamber, and introducing a body deposition reaction gas and a preset deposition reaction time, respectively, to complete the body deposition of the semiconductor structure.
[0008] In order to solve the above problem, the present invention further provides a computer program product, including a computer program, and when the computer program is executed by a processor, the steps of the above method of the present invention are implemented.
[0009] In order to solve the above problem, the present invention further provides a computer device, including a memory for storing a computer program; a processor connected to the memory and used to execute the computer program to implement the steps of the above method of the present invention.
[0010] The above technical solution optimizes the semiconductor structure deposition solution. During the nucleation process, nucleation is achieved by sequentially transferring the wafer to different workstations. The same gas is always introduced into each workstation, so there is no need for high-cost high-speed switching valves, which effectively saves process costs. By quickly performing nucleation followed by one-step deposition, the waiting phenomenon is eliminated, which effectively saves process time, improves output, and achieves cost reduction and efficiency improvement.
[0011] It should be understood that the above general description and the detailed description below are exemplary and explanatory only and cannot limit the present invention. The techniques, methods and devices known to ordinary technicians in the relevant field may not be discussed in detail, but where appropriate, the techniques, methods and devices should be considered as part of the authorization specification. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments of the present invention are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0013] Figure 1 A schematic diagram of the working mode of a reaction chamber of an existing tungsten metal deposition process;
[0014] Figure 2 A flow chart of a semiconductor structure deposition method provided by one embodiment of the present invention;
[0015] Figure 3 A schematic diagram of the working mode of a reaction chamber of a tungsten metal deposition process provided by one embodiment of the present invention;
[0016] Figure 4 A cross-sectional view of a device structure formed by a tungsten metal deposition process provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0017] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0018] See also Figure 2 , which is a flow chart of a semiconductor structure deposition method provided by an embodiment of the present invention. Figure 2 As shown, the semiconductor structure deposition method described in this embodiment includes: step S1, providing a reaction chamber, the reaction chamber at least including a first station, a second station and a purge station isolated from each other; step S2, performing a nucleation process, transferring multiple wafers to the first station, the purge station, the second station and the purge station in sequence, and cycling a preset number of times to complete the nucleation of the semiconductor structure, wherein the first station continuously introduces the first nucleation reaction gas, the second station continuously introduces the second nucleation reaction gas, and the purge station continuously introduces the purge gas; and step S3, performing a body deposition process, stopping the introduction of the first nucleation reaction gas, the second nucleation reaction gas and the purge gas, placing a wafer after nucleation on each station of the reaction chamber, and introducing body deposition reaction gas and a preset deposition reaction time respectively to complete the body deposition of the semiconductor structure.
[0019] Regarding step S1 , a reaction chamber is provided, wherein the reaction chamber at least includes a first station, a second station, and a purge station that are isolated from each other.
[0020] In this embodiment, the purge station includes a first purge sub-station and a second purge sub-station. That is, the reaction chamber includes a first station, a first purge sub-station, a second station and a second purge sub-station that are isolated from each other; the first station, the first purge sub-station, the second station and the second purge sub-station are distributed circumferentially in the reaction chamber. With the above-mentioned station setting method, when the wafer is transferred, the wafer can be transferred to the first station, the first purge sub-station, the second station and the second purge sub-station in sequence by rotating the wafer in the same direction, so that the nucleation process of multiple wafers can be carried out simultaneously. Furthermore, the first station, the first purge sub-station, the second station and the second purge sub-station are evenly distributed circumferentially in the reaction chamber.
[0021] Regarding step S2, a nucleation process is performed, and multiple wafers are sequentially transferred to the first station, the purge station, the second station, and the purge station, and the cycle is repeated for a preset number of times to complete the nucleation of the semiconductor structure, wherein the first station continuously introduces the first nucleation reaction gas, the second station continuously introduces the second nucleation reaction gas, and the purge station continuously introduces the purge gas. In this step, during the nucleation process, since the wafers are sequentially transferred to the first station, the purge station, the second station, and the purge station, and the same gas is continuously introduced into each station, there is no need for a high-cost high-speed switch valve, which effectively saves process costs.
[0022] In this embodiment, when the nucleation process is performed, when a wafer is transferred to the first station, the first station starts and continuously introduces the first nucleation reaction gas; when a wafer is transferred to the second station, the second station starts and continuously introduces the second nucleation reaction gas; when a wafer is transferred to the purge station, the purge station starts and continuously introduces the purge gas.
[0023] The wafer is transferred in sequence through the first station, the purge station, the second station, and the purge station once to complete one cycle. In this embodiment, the preset number of cycles is 5 times. In other embodiments, the number of cycles can be adjusted according to the thickness requirements of the nucleation film layer, for example, it can be 2 times, 3 times, 4 times, 6 times, 7 times or more.
[0024] In some embodiments, the first nucleation reaction gas is SiH4, the second nucleation reaction gas is WF6, and the purge gas is Ar.
[0025] In some embodiments, the nucleation process uses an atomic layer deposition (ALD) process, which is a thin film deposition technology based on a surface self-limiting reaction.
[0026] Specifically, wafer 1 is transferred to the first station, and the first reaction gas (e.g., SiH4) is started and continuously introduced into the first station; then wafer 1 is transferred to the purge station, and the purge gas (e.g., Ar) is started and continuously introduced into the purge station; then wafer 1 is transferred to the second station, and the second reaction gas (e.g., WF6) is started and continuously introduced into the second station; then wafer 1 is transferred to the purge station for purging and cleaning; after one cycle is completed, wafer 1 is transferred to the first station again for the reaction of the first reaction gas. When wafer 1 is transferred from the first station to the purge station, wafer 2 is transferred to the first station for the reaction of the first reaction gas, and wafers 3 and 4 are transferred in the same manner. That is, in the nucleation process stage, all wafers are transferred in sequence to the first station, the purge station, the second station, and the purge station, and all stations in the reaction chamber participate in the nucleation process. After the cycle is executed for the number of times required for nucleation (e.g., 5 times), the nucleation of the semiconductor structure is completed. During the nucleation process, nucleation is achieved by transferring the wafer to different workstations in sequence. The same gas is always introduced into each workstation, so there is no need for high-cost high-speed switching valves, which effectively saves process costs.
[0027] In this embodiment, the process time for the wafer to react at the first station is substantially the same as the process time for the wafer to react at the second station, and is shorter than the process time for the wafer to be purged at the purging station. Since the nucleation process only requires deposition to form a thin film, the process time for the wafer to react at the first station and the process time for the wafer to react at the second station are both relatively short.
[0028] Regarding step S3, perform the bulk deposition process, stop introducing the first nucleation reaction gas, the second nucleation reaction gas and the purge gas, place a wafer that has completed nucleation on each station of the reaction chamber, introduce the bulk deposition reaction gas and the preset deposition reaction time, and complete the bulk deposition of the semiconductor structure. In this step, after all wafers have completed the nucleation process, turn off the introduction of the gas required for nucleation, and then place a wafer that has completed nucleation on each station of the reaction chamber, introduce the bulk deposition reaction gas, and perform bulk deposition at the same time. Since the nucleation process is completed faster than the bulk deposition process, this embodiment performs nucleation of all wafers first and then unified bulk deposition. Compared with the prior art that needs to wait for the completion of bulk deposition before proceeding to the next step of the process, which causes a long process time, this embodiment effectively saves the process time and improves output.
[0029] In this embodiment, the steps of executing the body deposition process specifically include: (1) stopping the introduction of the first nucleation reaction gas, the second nucleation reaction gas and the purge gas; (2) placing a wafer after nucleation at each station of the reaction chamber, and heating the base of each station; (3) introducing the body deposition reaction gas and the preset deposition reaction process time to complete the body deposition of the semiconductor structure. Specifically, the preset process time for executing the body deposition process is adjusted according to the body deposition film thickness requirement. Furthermore, the body deposition reaction process time of the corresponding station can be adjusted according to the body deposition film thickness requirement of each wafer.
[0030] In some embodiments, the bulk deposition reaction gas is a mixed gas of H2 and WF6, and the semiconductor structure is a tungsten plug.
[0031] In some embodiments, the bulk deposition process uses a chemical vapor deposition (CVD) process. Chemical vapor deposition is a process in which gaseous or vaporous substances react in a gas phase or at a gas-solid interface to generate solid deposits.
[0032] Please also read Figure 3-Figure 4 ,in, Figure 3 A schematic diagram of the working mode of a reaction chamber of a tungsten metal deposition process provided by an embodiment of the present invention, Figure 4 A cross-sectional view of a device structure formed by a tungsten metal deposition process provided by an embodiment of the present invention.
[0033] like Figure 3 As shown, the reaction chamber 30 includes four mutually isolated stations: station 1, station 2, station 3 and station 4; the four stations are distributed circumferentially in the reaction chamber 30. Specifically, station 1 can be the first station, station 2 is the first purge sub-station, station 3 is the second station, and station 4 is the second purge sub-station. When performing the nucleation process, the four wafers are sequentially transferred to station 1, station 2, station 3 and station 4 by rotating the wafers in the same direction.
[0034] In this embodiment, the wafer is pre-formed with a contact hole 401, such as Figure 4 As shown in part (a); the nucleation process is to deposit a first film layer 41 on the inner wall of the contact hole 401, such as Figure 4 As shown in part (b); the body deposition process is to deposit a second film layer 42 in the contact hole 401 to cover the first film layer 41 and fill the contact hole 401, as shown in FIG. Figure 4 As shown in part (c), the first film layer 41 and the second film layer 42 together form a contact structure as the semiconductor structure. For the tungsten metal deposition process, the contact structure is a tungsten plug.
[0035] The specific flow of the tungsten metal deposition process described in this embodiment can be: (1) Wafer 1 is transferred to station 1, and the first reaction gas (such as SiH4) is started and continuously introduced into station 1; then wafer 1 is transferred to station 2, and purge gas (such as Ar) is started and continuously introduced into station 2; then wafer 1 is transferred to station 3, and the second reaction gas (such as WF6) is started and continuously introduced into station 3; then wafer 1 is transferred to station 4, and purge gas (such as Ar) is started and continuously introduced into station 4; after one cycle is performed in this way, wafer 1 is transferred to station 1 again to react with the first reaction gas. When wafer 1 is transferred from station 1 to station 2, wafer 2 is transferred to station 1 to react with the first reaction gas, and wafers 3 and 4 are transferred in the same manner. After the cycle is executed for the number of times required for nucleation (for example, 5 times), tungsten nucleation is completed, such as Figure 4 (2) Turn off the gas required for the nucleation process, place wafers 1 to 4 on stations 1 to 4 respectively, heat the station base and start introducing tungsten body deposition reaction gas (such as H2 and WF6), and control the process time of the body deposition reaction according to the thickness of the body deposition film until the tungsten body deposition is completed on the four wafers at the same time, as shown in FIG. Figure 4 As shown in part (c).
[0036] In this embodiment, during the nucleation process, the nucleation is achieved by transferring the wafers to different stations in sequence, and the same gas is always introduced into each station, so there is no need for high-cost high-speed switching valves, which effectively saves process costs. After the nucleation of the same batch of wafers (for example, the 4 wafers mentioned above) is completed, the body deposition process is performed at the same time, which can eliminate the waiting phenomenon in the prior art that after the nucleation of some wafers is completed, it is necessary to wait for the body deposition of other wafers to be completed before continuing to perform its own body deposition. That is, the improved tungsten metal deposition process of this embodiment can eliminate the need to use high-cost high-speed switching valves and eliminate the waiting phenomenon, thereby reducing the tungsten metal deposition process time and reducing costs, and achieving cost reduction and efficiency improvement in the tungsten metal deposition process.
[0037] It has been verified experimentally that the tungsten metal deposition process provided in this embodiment can ensure higher output through rapid nucleation and subsequent bulk deposition, increasing the current output from 80 pieces / hour to 106 pieces / hour, while saving 8 high-speed switching valves, effectively achieving cost reduction and efficiency improvement in the tungsten metal deposition process.
[0038] The above-mentioned embodiment of the present invention optimizes the semiconductor structure deposition scheme. During the nucleation process stage, nucleation is achieved by sequentially transferring the wafer to different workstations. The same gas is always introduced into each workstation, so there is no need for high-cost high-speed switching valves, which effectively saves process costs. By quickly performing one-step deposition after nucleation, the waiting phenomenon is eliminated, which effectively saves process time, improves output, and achieves cost reduction and efficiency improvement.
[0039] Based on the same inventive concept, the present invention also provides a computer program product, including a computer program, which, when executed by a processor, implements the steps of the semiconductor structure deposition method described in the present invention: step S1, providing a reaction chamber, the reaction chamber at least including a first station, a second station and a purge station isolated from each other; step S2, executing a nucleation process, transferring multiple wafers to the first station, the purge station, the second station, and the purge station in sequence, and cycling a preset number of times to complete the nucleation of the semiconductor structure, wherein the first station continuously introduces a first nucleation reaction gas, the second station continuously introduces a second nucleation reaction gas, and the purge station continuously introduces a purge gas; and step S3, executing a body deposition process, stopping the introduction of the first nucleation reaction gas, the second nucleation reaction gas and the purge gas, placing a wafer after nucleation on each station of the reaction chamber, and introducing a body deposition reaction gas and a preset deposition reaction time respectively to complete the body deposition of the semiconductor structure.
[0040] Based on the same inventive concept, the present invention also provides a computer device, comprising: a memory for storing a computer program; a processor connected to the memory and for executing the computer program to implement the steps of the aforementioned method of the present invention.
[0041] Based on the same inventive concept, the present invention further provides a computer-readable storage medium on which a computer program is stored, and when the program is executed by a processor, the steps of the aforementioned method of the present invention are implemented.
[0042] Those skilled in the art can understand that all or part of the processes in the above-mentioned embodiments can be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to memory, storage, database or other media used in the embodiments provided by the present invention can include non-volatile and / or volatile memory. Non-volatile memory can include read-only memory (ROM), programmable ROM (PROM), electrically programmable ROM (EPROM), electrically erasable programmable ROM (EEPROM) or flash memory. Volatile memory can include random access memory (RAM) or external cache memory. As an illustration and not limitation, RAM is available in many forms, such as static RAM (SRAM), dynamic RAM (DRAM), synchronous DRAM (SDRAM), double data rate SDRAM (DDRSDRAM), enhanced SDRAM (ESDRAM), synchronous link (Synch Link) DRAM (SLDRAM), memory bus (Ram Bus) direct RAM (RDRAM), direct memory bus dynamic RAM (DRDRAM), and memory bus dynamic RAM (RDRAM).
[0043] It should be noted that the terms "including" and "having" and their variations involved in the document of the present invention are intended to cover non-exclusive inclusions. The terms "first", "second", etc. are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence, unless the context clearly indicates, and it should be understood that the data used in this way can be interchanged under appropriate circumstances. The term "one or more" depends at least in part on the context, and can be used to describe features, structures or characteristics in a singular sense, or can be used to describe features, structures or combinations of features in a plural sense. The term "based on" can be understood as not necessarily intended to express a set of exclusive factors, but can alternatively, also at least in part depending on the context, allow the presence of other factors that are not necessarily explicitly described. In addition, the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict. In addition, in the above description, the description of well-known components and technologies is omitted to avoid unnecessary confusion of the concept of the present invention. In the above embodiments, each embodiment focuses on the differences from other embodiments, and the same / similar parts between the embodiments can be referred to each other.
[0044] The above is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. It should be noted that a person skilled in the art can make several improvements and modifications without departing from the principle of the present invention, and these improvements and modifications should also be regarded as the protection scope of the present invention.
Claims
1. A semiconductor structure deposition method, characterized in that: include: Providing a reaction chamber, wherein the reaction chamber at least comprises a first station, a second station and a purge station that are isolated from each other; Performing a nucleation process, transferring a plurality of wafers to a first station, a purge station, a second station, and a purge station in sequence, and cycling a preset number of times to complete the nucleation of the semiconductor structure, wherein the first station continuously introduces a first nucleation reaction gas, the second station continuously introduces a second nucleation reaction gas, and the purge station continuously introduces a purge gas; and Perform a bulk deposition process, stop introducing the first nucleation reaction gas, the second nucleation reaction gas and the purge gas, place a wafer after nucleation on each workstation in the reaction chamber, and introduce bulk deposition reaction gas and a preset deposition reaction time to complete the bulk deposition of the semiconductor structure.
2. The method according to claim 1, characterized in that When performing the nucleation process, when a wafer is transferred to the first station, the first station starts and continuously introduces the first nucleation reaction gas; when a wafer is transferred to the second station, the second station starts and continuously introduces the second nucleation reaction gas; when a wafer is transferred to the purge station, the purge station starts and continuously introduces the purge gas.
3. The method according to claim 1, characterized in that The preset number of cycles is 5 times.
4. The method according to claim 1, characterized in that: The process time for the wafer to react at the first station is substantially the same as the process time for the wafer to react at the second station, and is shorter than the process time for the wafer to be purged at the purging station.
5. The method according to claim 1, characterized in that The steps of performing the body deposition process specifically include: Stopping the introduction of the first nucleation reaction gas, the second nucleation reaction gas and the purge gas; Placing a wafer after nucleation on each station of the reaction chamber, and heating the base of each station; The bulk deposition reaction gas is introduced and the deposition reaction is performed for a preset process time to complete the bulk deposition of the semiconductor structure.
6. The method according to claim 1, characterized in that The preset process time for performing the bulk deposition process is adjusted according to the bulk deposition film thickness requirement.
7. The method according to claim 1, characterized in that The purge station includes a first purge sub-station and a second purge sub-station, and the first station, the first purge sub-station, the second station and the second purge sub-station are distributed along the circumferential direction in the reaction chamber; When performing the nucleation process, the four wafers are sequentially transferred to the first station, the first purge sub-station, the second station and the second purge sub-station by rotating the wafers in the same direction.
8. The method according to claim 1, characterized in that The wafer is pre-formed with a contact hole; the nucleation process is to deposit a first film layer on the inner wall of the contact hole, and the body deposition process is to deposit a second film layer in the contact hole to cover the first film layer and fill the contact hole. The first film layer and the second film layer together constitute a contact structure as the semiconductor structure.
9. The method according to claim 1, characterized in that: The nucleation process adopts an atomic layer deposition process, and the bulk deposition process adopts a chemical vapor deposition process.
10. The method according to claim 1, characterized in that The first nucleation reaction gas is SiH4, the second nucleation reaction gas is WF6, the purge gas is Ar, the bulk deposition reaction gas is a mixed gas of H2 and WF6, and the semiconductor structure is a tungsten plug.
11. A computer program product, comprising a computer program, characterized in that When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 10 are implemented.
12. A computer device, characterized in that: include: Memory for storing computer programs; A processor, connected to the memory, is used to execute the computer program to implement the steps of the method according to any one of claims 1 to 10.
Citation Information
Patent Citations
Method for forming semiconductor structure
CN104157562A
Tungsten film forming method
CN114496781A
Metal tungsten film and preparation method thereof
CN115910917A
Semiconductor process method
CN116463613A
Method for fabricating semiconductor device by using PECYCLE-CVD process