Structure fatigue life evaluation method based on inverse difference residual stress intermittent correction
By determining the stress spectrum and residual stress eigenvalue of large-scale equipment structures in three-dimensional finite element analysis, the problem of failure to effectively evaluate the fatigue life of the structure in the prior art is solved, especially the impact of the counterdeficiency change in the intermittent working state, and achieve More accurate and efficient fatigue life prediction.
Patent Information
- Application Number
- CN202410917703.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-11-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The prior art is difficult to effectively evaluate the fatigue life of large-scale equipment structures, especially the impact of the change in residual stress counterdeficiency in the intermittent working state of the structure is not fully considered, resulting in insufficient prediction of fatigue life.
By determining the structural stress spectrum in the three-dimensional finite element analysis software, the residual stress value of the abnormal point of the stress distribution is obtained, the characteristic value of the residual stress counterdeficit change is calculated, and combined with the material fatigue characteristic parameters, specific mathematical formulas are used to correct the structural fatigue life. Evaluate.
The precise evaluation of the fatigue life of large-scale equipment structures is achieved, the accuracy and efficiency of online prediction are improved, and the disadvantage of not considering the change of residual stress counterdeficiency is avoided.
Smart Images

Figure CN118886256A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of parameter determination, and in particular to a structural fatigue life assessment method based on intermittent correction of reverse differential residual stress. Background Art
[0002] With the development and progress of society, large-scale equipment is developing in the direction of huge structure and intelligent operation. Under this background, the problem of structural reliability is becoming more and more serious, especially the accurate grasp of the fatigue residual life of the structure has become very critical. There are many methods for fatigue life assessment of large-scale equipment structures, but most of them are predictive assessment processes based on a small amount of stress data at a fixed measurement position. For actual engineering, in addition to the force of external loads, the structure itself will also have residual stress. And in actual engineering, the intermittent structural working state will cause the residual stress to interact at different time points, that is, the anti-deficit change phenomenon. Therefore, it is a common problem in this research field to evaluate the fatigue life of large structures from the perspective of the anti-deficit change characteristics within the residual stress. Summary of the invention
[0003] Purpose of the invention: The purpose of the present invention is to provide a structural fatigue life assessment method based on intermittent correction of reverse differential residual stress.
[0004] Technical solution: The present invention comprises the following steps:
[0005] (1) Determination of stress spectrum under structural load;
[0006] (2) Obtaining the structural residual stress value based on the abnormal points of stress distribution;
[0007] (3) Determination of the characteristic value of residual stress reverse difference change;
[0008] (4) Determination of fatigue life considering the intermittent phenomenon of reverse residual stress.
[0009] Furthermore, the step (1) comprises:
[0010] A 3D model of the structure to be analyzed is established in the 3D software PRO-E, and the 3D model is imported into the finite element analysis software ANSYS. The 3D model is meshed, and the mesh density is increased by local encryption at key stress concentration locations; then, fixed constraints and loads are applied to the structure to be analyzed under the ANSYS boundary module according to actual working conditions; finally, the post-processing module is used to solve the stress distribution of the structure under actual working conditions.
[0011] Furthermore, the three-dimensional model is meshed using a hexahedral mesh.
[0012] Furthermore, the step (2) comprises:
[0013] Based on the analysis in step (1), select the three locations with the largest stress values and mark their results as σ i , i = 1, 2, 3, select the three locations with the smallest stress values and mark their results as σ t , t=1, 2, 3, substitute the following formula to get the local adverse stress σ n To solve:
[0014]
[0015] Among them, σ n is the local stress deficit, σ i are the results of the three locations with the largest stress values, where t = 1, 2, 3, σ t The results of the three locations with the smallest stress values, i = 1, 2, 3, C (σ i ) max The results of the three locations with the largest stress values are σ i The maximum value in C(σ i ) min The results of the three locations with the largest stress values are σ i The minimum value among all the structural stresses analyzed in step (1) is greater than σ n The stress position points are marked with position numbers, marked as the qth point, q = 1, ... β, β is the number of all marked points, and the residual stress scanning test is performed on the β marked points, and the residual stress measurement results are marked as Y q , where q is the residual stress test position point number, q = 1,…β, β is the number of all marked points.
[0016] Furthermore, the residual stress scanning test on the β marking points adopts a surface scanning X-ray residual stress testing device.
[0017] Furthermore, the step (3) comprises:
[0018] Based on the analysis and test results in step (2), the residual stress reverse difference change characteristic value T is substituted into the following formula: q To solve:
[0019]
[0020] Among them, T q is the residual stress reverse difference variation characteristic value, σ n is the local stress deficit, n=1, 2, 3, σ i The results are for the three locations with the largest stress values, t = 1, 2, 3, σ tThe results for the three locations with the smallest stress values, i = 1, 2, 3, α q is the stress concentration factor corresponding to the qth marked point, β is the number of all marked points, Y q is the result of residual stress determination, C(Y q ) min is the minimum value of the residual stress measurement result, C(Y q ) max is the maximum value of the residual stress measurement result, q is the residual stress test point number, q=1,…β.
[0021] Furthermore, the α q is the stress concentration factor corresponding to the qth marked point, which is obtained through the photoelastic test.
[0022] Furthermore, the step (4) comprises:
[0023] Based on the analysis of steps (1) to (3), the relevant parameters are substituted into the following formula to solve the structural fatigue life L:
[0024]
[0025] Where L is the fatigue life of the structure, γ and m are parameters related to the fatigue properties of the material, which can be obtained through tensile fatigue tests, and C(T q ) max is the characteristic value T of all residual stress reverse difference changes q The maximum value in C(σ i ) max The results of all three locations with the largest stress values σ i The maximum value in .
[0026] Beneficial effects: Compared with the prior art, the present invention has the following significant advantages: it can realize accurate evaluation of structural fatigue life, and extract corresponding anti-deficit characteristics from the anti-deficit changes inside the residual stress under intermittent working conditions, and reversely correct the actual fatigue stress value on this basis, avoiding the traditional disadvantage of not considering the actual changes of residual stress anti-deficit, and effectively improving the accuracy and efficiency of online prediction and evaluation of fatigue life of large equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a flow chart of the present invention. DETAILED DESCRIPTION
[0028] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.
[0029] As shown in Figure 1, the present invention comprises the following steps:
[0030] (1) Determination of stress spectrum under structural load:
[0031] A 3D model of the structure to be analyzed is established in the 3D software PRO-E, and the 3D model is imported into the finite element analysis software ANSYS. The mesh is divided using a hexahedral mesh, and the mesh density is increased by local encryption at the key stress concentration location. Then, according to the actual working conditions, fixed constraints and loads are applied to the structure to be analyzed under the ANSYS boundary module. Finally, the post-processing module is used to solve the stress distribution of the structure under the actual working conditions.
[0032] (2) Obtaining the structural residual stress value based on the abnormal points of stress distribution:
[0033] Based on the analysis in step (1), select the three locations with the largest stress values and mark their results as σ i (i=1, 2, 3), select the three locations with the smallest stress values and mark their results as σ t (t=1,2,3), then substitute the following formula to calculate the local adverse stress σ n To solve:
[0034]
[0035] Among them, σ n is the local stress deficit, σ t are the results for the three locations with the largest stress values, (t=1, 2, 3), σ t are the results of the three locations with the smallest stress values, (i = 1, 2, 3), C (σ i ) max The results of the three locations with the largest stress values are σ i The maximum value in C(σ i ) min The results of the three locations with the largest stress values are σ i Then determine the minimum value of all structural stresses greater than σ in the analysis of S1. n The stress position points are marked with position numbers and labeled as the qth points (q=1,…β), where β is the number of all marked points.
[0036] Then, the residual stress of β marked points is scanned and tested using a surface scanning X-ray residual stress test device, and the residual stress measurement result is marked as Y. q (q is the number of the residual stress test position point, q=1,…β, β is the number of all marked points).
[0037] (3) Determination of the characteristic value of residual stress reverse difference change:
[0038] Based on the analysis and test results in step (2), the residual stress reverse difference change characteristic value T is substituted into the following formula: q To solve:
[0039]
[0040] Among them, T q is the residual stress reverse difference variation characteristic value, σ n is the local stress deficit, (n=1, 2, 3), σ i are the results for the three locations with the largest stress values, (t=1, 2, 3), σ t are the results of the three locations with the smallest stress values, (i = 1, 2, 3), α q is the stress concentration factor corresponding to the qth marking point, which can be obtained through photoelastic test, β is the number of all marking points, Y q is the result of residual stress determination, C(Y q ) min is the minimum value of the residual stress measurement result, C(Y q ) max is the maximum value of the residual stress measurement result, q is the residual stress test point number (q=1,…β).
[0041] (4) Determination of fatigue life considering the intermittent phenomenon of reverse residual stress:
[0042] Based on the analysis of steps (1) to (3), the relevant parameters are substituted into the following formula to solve the structural fatigue life L:
[0043]
[0044] Where L is the fatigue life of the structure, γ and m are parameters related to the fatigue properties of the material, which can be obtained through tensile fatigue tests, and C(T q ) max is the characteristic value T of all residual stress reverse difference changes q The maximum value in C(σ i ) max The results of all three locations with the largest stress values σ i The maximum value in .
Claims
1. A structural fatigue life assessment method based on intermittent correction of reverse differential residual stress, characterized in that: The steps include: (1) Determination of stress spectrum under structural load; (2) Obtaining the structural residual stress value based on the abnormal points of stress distribution; (3) Determination of the characteristic value of residual stress reverse difference change; (4) Determination of fatigue life considering the intermittent phenomenon of reverse residual stress.
2. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 1 is characterized in that: The step (1) comprises: A 3D model of the structure to be analyzed is established in the 3D software PRO-E, and the 3D model is imported into the finite element analysis software ANSYS. The 3D model is meshed, and the mesh density is increased by local encryption at key stress concentration locations. Then, fixed constraints and loads are applied to the structure to be analyzed under the ANSYS boundary module according to actual working conditions. Finally, the post-processing module is used to solve the stress distribution of the structure under actual working conditions.
3. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 2 is characterized in that: The three-dimensional model is meshed using a hexahedral mesh.
4. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 1 is characterized in that: The step (2) comprises: Based on the analysis in step (1), select the three locations with the largest stress values and mark their results as σ i , i = 1, 2, 3, select the three locations with the smallest stress values and mark their results as σ t , t=1, 2, 3, substitute the following formula to get the local adverse stress σ n To solve: Among them, σ n , is the local stress deficit, σ i are the results of the three locations with the largest stress values, where t = 1, 2, 3, σ t The results of the three locations with the smallest stress values, i = 1, 2, 3, C (σ i ) max The results of the three locations with the largest stress values are σ i The maximum value in C(σ i ) min The results of the three locations with the largest stress values are σ i The minimum value among all the structural stresses analyzed in step (1) is greater than σ n The stress position points are marked with position numbers, marked as the qth point, q = 1, ... β, β is the number of all marked points, and the residual stress scanning test is performed on the β marked points, and the residual stress measurement results are marked as Y q , where q is the residual stress test position point number, q = 1,…β, β is the number of all marked points.
5. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 4 is characterized in that: The residual stress scanning test on the β marking points adopts a surface scanning X-ray residual stress testing device.
6. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 1 is characterized in that: The step (3) comprises: Based on the analysis and test results in step (2), the residual stress reverse difference change characteristic value T is substituted into the following formula: q To solve: Among them, T q is the residual stress reverse difference variation characteristic value, σ n is the local stress deficit, n=1, 2, 3, σ i The results are for the three locations with the largest stress values, t = 1, 2, 3, σ t The results for the three locations with the smallest stress values, i = 1, 2, 3, α q is the stress concentration factor corresponding to the qth marked point, β is the number of all marked points, Y q is the result of residual stress determination, C(Y q ) min is the minimum value of the residual stress measurement result, C(Y q ) max is the maximum value of the residual stress measurement result, q is the residual stress test point number, q=1,…β.
7. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 6 is characterized in that: The α q is the stress concentration factor corresponding to the qth marked point, which is obtained through the photoelastic test.
8. The structural fatigue life assessment method based on intermittent correction of reverse differential residual stress according to claim 1 is characterized in that: The step (4) comprises: Based on the analysis of steps (1) to (3), the relevant parameters are substituted into the following formula to solve the structural fatigue life L: Where L is the fatigue life of the structure, γ and m are parameters related to the fatigue properties of the material, which can be obtained through tensile fatigue tests, and C(T q ) max is the characteristic value T of all residual stress reverse difference changes q The maximum value in C(σ i ) max The maximum value among the results v at the three locations where all stress values are the largest.