Electrochemical device and electronic apparatus

By setting a bonding area of ​​a specific area ratio in the insulating tape of the electrochemical device, the connection between the electrode assembly and the shell is optimized, and the problems of tear and poor bonding of the electrode assembly during drop are solved, and the safety and energy of the equipment are improved density.

CN118888941APending Publication Date: 2024-11-01NINGDE AMPEREX TECHNOLOGY LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410924864.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2021-01-29
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

When the battery of an electronic device falls, the insulating tape may cause the electrode assembly to tear, causing the risk of short circuit, and may cause the top seal to break when the bond is poor, affecting the safety and energy density of the device.

Method used

An electrochemical device is designed to reduce the peeling force per unit area by setting a specific area ratio (0.08≤B/A≤0.965) between the first bonding area and the second bonding area of ​​the insulating tape to improve the peeling force. The connection reliability of the electrode assembly and the insulating tape are improved by adjusting the shape and position of the bonding area, and the volume and weight of the insulating tape are optimized to improve the energy density.

Benefits of technology

It effectively reduces the risk of insulating tape tearing under external force, improves the safety of electrode assembly and the energy density of electrochemical devices, and ensures the reliability of the connection between the insulating tape and the shell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118888941A_ABST
    Figure CN118888941A_ABST
Patent Text Reader

Abstract

The invention discloses an electrochemical device and electronic equipment. The electrochemical device comprises a shell, an electrode assembly and an insulating tape, at least part of the electrode assembly is located in the shell; the insulated rubber tape is located between the shell and the electrode assembly, and the insulated rubber tape comprises a first surface bonded with the electrode assembly and a second surface bonded with the shell; the first surface comprises a first bonding area, and the second surface comprises a second bonding area; wherein the first bonding area is provided with a first outer edge, and the second bonding area is provided with a second outer edge; the distance between the orthographic projection of the second outer edge on the first surface and the first outer edge is h, and the width of the first surface is W2; wherein h is larger than or equal to 0.035 * W2 and smaller than or equal to 0.4 * W2. When the shell of the electrochemical device is subjected to external force, the external force can be sequentially transmitted to the second bonding area, the first bonding area and the electrode assembly from the shell, and the area of the first bonding area is larger than that of the second bonding area, so that the stripping force borne by the unit area between the first bonding area and the electrode assembly is reduced; therefore, the risk that the electrode assembly is torn by the insulating tape under the action of external force is reduced, and the safety of the electrode assembly is improved.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of a patent application with a filing date of January 29, 2021, application number 202180003680.0, and name “Electrochemical Devices and Electronic Devices”. Technical Field

[0002] The present application relates to the technical field of energy storage devices, and in particular to an electrochemical device and an electronic device. Background Art

[0003] With the development of electronic devices, the batteries of electronic devices are required to have larger capacity to meet the endurance requirements of electronic devices. The battery of an electronic device usually includes a shell and an electrode assembly located inside the shell, and the shell protects the electrode assembly. The shell and the electrode assembly can be bonded by an insulating tape. When the electronic device falls, the insulating tape may tear the electrode assembly, thereby causing the risk of internal short circuit of the electrode assembly. When the insulating tape is poorly bonded, there may be a risk of top seal breaking, affecting the safety of the electronic device. Summary of the invention

[0004] The present application provides an electrochemical device and an electronic device, wherein the electrochemical device can improve the connection reliability between an electrode assembly and a housing, enhance the drop resistance, and increase the energy density of the electrochemical device.

[0005] In a first aspect, the present application provides an electrochemical device, which includes: a housing, an electrode assembly and an insulating tape, wherein at least a portion of the electrode assembly is located in the housing; the insulating tape is located between the housing and the electrode assembly, and the insulating tape includes a first surface bonded to the electrode assembly and a second surface bonded to the housing; the first surface includes a first bonding area, and the second surface includes a second bonding area; wherein an area A of the first bonding area and an area B of the second bonding area satisfy: 0.08≤B / A≤0.965. In another possible design, 0.15≤B / A≤0.85.

[0006] In one possible design, the first bonding area has a first outer edge, and the second bonding area has a second outer edge; the distance between the orthographic projection of the second outer edge on the first surface and the first outer edge is h, and the width of the first surface is W2; wherein 0.035×W2≤h≤0.4×W2. In another possible design, 0.05×W2≤h≤0.35×W2.

[0007] In a possible design, the electrode assembly has a third surface bonded to the insulating tape, and the first bonding area covers the orthographic projection of the second bonding area on the third surface.

[0008] In one possible design, the electrode assembly has a third surface bonded to the insulating tape, and the length of the third surface is L1; along the width direction of the electrochemical device, the first bonding area has a first axis, the third surface has a second axis, and the distance between the orthographic projection of the first axis on the third surface and the second axis is D, D≤0.1×L1.

[0009] In a possible design, the width of the third surface is W1; along the length direction of the electrochemical device, the first bonding area has a third axis, the third surface has a fourth axis, and the distance between the orthographic projection of the third axis on the third surface and the fourth axis is E, E≤0.1×W1.

[0010] In one possible design, the orthographic projection of the geometric center of the second bonding area on the first surface coincides with the geometric center of the first bonding area; in one possible design, the ratio of the distance extending from the geometric centers of the first bonding area and the second bonding area along the same direction to the first outer edge and the distance extending to the second outer edge are the same.

[0011] In a possible design, the length of the first bonding area is L2, and the width of the first bonding area is W2; wherein, 0.4×L1≤L2≤0.8×L1, 0.4×W1≤W2≤0.8×W1.

[0012] In a possible design, the insulating tape includes a first adhesive material, a base material, and a second adhesive material that are stacked together. The first adhesive material is bonded to the electrode assembly, and the second adhesive material is bonded to the shell.

[0013] In a possible design, the shapes of the first bonding area and the second bonding area are selected from any one of square, rectangle, trapezoid, octagon, circle, and ellipse.

[0014] A second aspect of the present application provides an electronic device, which includes the electrochemical device described above.

[0015] When the shell of the electrochemical device is subjected to external force (for example, the shell is subjected to external force during a drop test), the external force can be transmitted from the shell to the second bonding area of ​​the insulating tape, from the second bonding area to the first bonding area, and from the first bonding area to the electrode assembly. Since the area of ​​the first bonding area is larger than the area of ​​the second bonding area, the peeling force per unit area between the first bonding area and the electrode assembly can be reduced, thereby reducing the risk of the insulating tape tearing the electrode assembly under the action of external force, improving the connection reliability between the electrode assembly and the insulating tape, and thus improving the safety of the electrode assembly. At the same time, when the area of ​​the second surface of the insulating tape connected to the shell is small, while ensuring the connection reliability between the insulating tape and the shell, the volume and weight of the insulating tape are also made smaller, thereby helping to improve the energy density of the electrochemical device.

[0016] It should be understood that the foregoing general description and the following detailed description are exemplary only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a schematic diagram of the connection structure of the housing, the electrode assembly, and the insulating tape in the first embodiment of the present application;

[0018] Figure 2 This is a schematic diagram of the connection structure of the housing, the electrode assembly, and the insulating tape in the second embodiment of the present application;

[0019] Figure 3 This is a schematic diagram of the connection structure of the housing, the electrode assembly, and the insulating tape in the third embodiment of the present application;

[0020] Figure 4 It is a schematic structural diagram of the insulating tape in the fourth embodiment of the present application projected onto the third surface of the electrode assembly;

[0021] Figure 5 It is a schematic structural diagram of the insulating tape in the fifth embodiment of the present application projected onto the third surface of the electrode assembly;

[0022] Figure 6 It is a schematic structural diagram of the insulating tape in the sixth embodiment of the present application projected onto the third surface of the electrode assembly;

[0023] Figure 7 A side view of an electrochemical device provided in one embodiment of the present application;

[0024] Figure 8 It is a schematic structural diagram of an electrochemical device provided in one embodiment of the present application.

[0025] Reference numerals:

[0026] 1- housing;

[0027] 2-Electrode assembly;

[0028] 21- third surface;

[0029] 211-second axis;

[0030] 212-the fourth axis;

[0031] 3-Insulation tape;

[0032] 31- first bonding area;

[0033] 311 - first outer edge;

[0034] 312- first axis;

[0035] 313-third axis;

[0036] 32- second bonding area;

[0037] 321 - second outer edge;

[0038] 33- first adhesive material;

[0039] 34- second adhesive material;

[0040] 35-substrate.

[0041] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present application and, together with the description, serve to explain the principles of the present application. DETAILED DESCRIPTION

[0042] In order to better understand the technical solution of the present application, the embodiments of the present application are described in detail below with reference to the accompanying drawings.

[0043] It should be clear that the described embodiments are only part of the embodiments of the present application, rather than all the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.

[0044] The terms used in the embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to limit the present application. The singular forms "a", "said" and "the" used in the embodiments of the present application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings.

[0045] It should be understood that the term "and / or" used in this article is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.

[0046] It should be noted that the directional words such as "upper", "lower", "left", and "right" described in the embodiments of the present application are described at the angles shown in the accompanying drawings and should not be understood as limiting the embodiments of the present application. In addition, in the context, it is also necessary to understand that when it is mentioned that an element is connected to another element "upper" or "lower", it can not only be directly connected to another element "upper" or "lower", but also indirectly connected to another element "upper" or "lower" through an intermediate element.

[0047] The present application provides an electrochemical device, such as Figures 1 to 3As shown, the electrochemical device includes a housing 1 and an electrode assembly 2, wherein the housing 1 has a housing cavity, and at least a portion of the electrode assembly 2 is located in the housing cavity, and the housing 1 is used to protect the electrode assembly 2. The electrode assembly 2 may include a first pole piece, a second pole piece, and a separator. One of the first pole piece and the second pole piece is a positive pole, and the other is a negative pole. The separator is used to separate the first pole piece and the second pole piece. The separator may be supported by a thermoplastic resin, such as polyethylene or polypropylene, and the separator is used to insulate the first pole piece from the second pole piece.

[0048] During the drop test, the electrochemical device is prone to the risk of top seal breaking, aluminum foil tearing of the electrode assembly 2, etc., which may cause a short circuit in the electrode assembly 2 and damage the electrochemical device. Figures 1 to 3 As shown, the electrochemical device also includes an insulating tape 3, which is located between the shell 1 and the electrode assembly 2, and the insulating tape 3 includes a first surface bonded to the electrode assembly 2 and a second surface bonded to the shell 1, the first surface includes a first bonding area 31, and the second surface includes a second bonding area 32, that is, the electrode assembly 2 is connected to the shell 1 through the insulating tape 3, so as to prevent the electrode assembly 2 from moving in the accommodating cavity of the shell 1 during the operation of the electrochemical device, and the insulating tape 3 can also prevent the electrode assembly 2 from short-circuiting with the shell 1, so that the electrochemical device can work normally. Among them, the bonding strength of the insulating tape 3 is related to factors such as the quality and size of the electrochemical device. Generally, the bonding strength of the insulating tape 3 ranges from 2MPa to 20MPa. At the same time, during the drop test, under the action of external force, there is also a risk that the insulating tape 3 will tear the aluminum foil of the electrode assembly 2.

[0049] In this embodiment, the area of ​​the first bonding area 31 is larger than the area of ​​the second bonding area 32 , that is, the area of ​​the surface of the insulating tape 3 bonding to the shell 1 is smaller than the area of ​​the surface bonding to the electrode assembly 2 .

[0050] When the shell 1 of the electrochemical device is subjected to external force (for example, the shell 1 is subjected to external force during the drop test), the external force can be transmitted from the shell 1 to the second bonding area 32 of the insulating tape 3, from the second bonding area 32 to the first bonding area 31, and from the first bonding area 31 to the electrode assembly 2. Since the area of ​​the first bonding area 31 is larger than the area of ​​the second bonding area 32, the peeling force per unit area between the first bonding area 31 and the electrode assembly 2 can be reduced, and the risk of the insulating tape 3 tearing the aluminum foil of the electrode assembly 2 is reduced, and the connection reliability between the electrode assembly 2 and the insulating tape 3 is improved, thereby improving the safety of the electrode assembly 2. At the same time, when the area of ​​the second bonding area 32 of the insulating tape 3 connected to the shell 1 is small, the volume and weight of the insulating tape 3 are also reduced while ensuring the connection reliability between the insulating tape 3 and the shell 1, thereby helping to improve the energy density of the electrochemical device.

[0051] Specifically, the area A of the first bonding area 31 and the area B of the second bonding area 32 satisfy: 0.08≤B / A≤0.965. In a specific embodiment, 0.1≤B / A≤0.6. For example, B / A can be: 0.1, 0.3, 0.4, 0.6, 0.8, 0.9, etc.

[0052] In this embodiment, when B / A is too large (for example, greater than 0.965), it means that the area A of the first bonding area 31 is close to the area B of the second bonding area 32, which makes it impossible to effectively reduce the peeling force per unit area between the edge of the first bonding area 31 and the electrode assembly 2, thereby causing the insulating tape 3 to tear the aluminum foil of the electrode assembly 2 at a high risk, reducing the safety of the electrode assembly 2; and causing the weight and volume of the insulating tape 3 to be too large, reducing the energy density of the electrochemical device. When B / A is too small (for example, less than 0.08), that is, the area B of the second bonding area 32 is too small, resulting in a large peeling force per unit area between the insulating tape 3 and the housing 1, and reducing the connection reliability.

[0053] More specifically, if Figures 1 to 6 As shown, the first bonding area 31 has a first outer edge 311, and the second bonding area 32 has a second outer edge 321. More specifically, as shown in FIG. Figure 4-6 As shown, the distance between the orthographic projection of the second outer edge 321 on the first surface and the first outer edge 311 is h, and the width of the first bonding area 31 is W2; wherein 0.035×W2≤h≤0.4×W2. In a specific embodiment, 0.05×W2≤h≤0.35×W2. For example, h can be 0.2×W2, 0.3×W2, etc. That is, the orthographic projection of the second outer edge 321 on the first surface is misaligned with the first outer edge 311. Among them, one of the four sides of the insulating tape 3 may have the above-mentioned misalignment (such as Figure 4 As shown), the above-mentioned misalignment may also exist on the opposite sides (as shown Figure 5 As shown), the above-mentioned misalignment may also exist on all four sides (as shown Figure 6 shown).

[0054] In this embodiment, when h is too large, it means that the difference between the area of ​​the second bonding area 32 and the area of ​​the first bonding area 31 is too large, that is, the area of ​​the bonding surface between the insulating tape 3 and the shell 1 is too small, resulting in excessive peeling force per unit area between the insulating tape 3 and the shell 1, thereby resulting in too low connection reliability between the insulating tape 3 and the shell 1; when h is too small, it means that the difference between the area of ​​the second bonding area 32 and the area of ​​the first bonding area 31 is too small, that is, the area of ​​the first bonding area 31 exceeding the edge of the second bonding area 32 is too small, resulting in too small stress action area transmitted from the edge of the second bonding area 32 to the edge of the first bonding area, that is, the peeling force per unit area between the edge of the first bonding area 31 of the insulating tape 3 and the electrode assembly 2 is too large, thereby resulting in the insulating tape 3 easily tearing the aluminum foil of the electrode assembly 2, and at the same time, the volume of the insulating tape 3 is too large, thereby reducing the energy density of the electrochemical device. Therefore, when 0.035×W2≤h≤0.4×W2, the areas of the first bonding area 31 and the second bonding area 32 are moderate, so that the insulating tape 3 has high connection reliability with the shell 1 and the electrode assembly 2, and the energy density of the electrochemical device can be improved.

[0055] Taking the lithium-ion battery with a rectangular maximum projection surface as an example, the drop test was carried out to compare the drop pass rates. Among them, Group 1 has Figure 4 The structure shown in FIG. 1 has the above-mentioned misalignment on one side of the width direction of the insulating tape 3; Group 2 has Figure 5 The structure shown in FIG. 1 has the above-mentioned misalignment on both sides of the width direction of the insulating tape 3; Group 3 has Figure 6 The structure shown has the above-mentioned misalignment around the insulating tape 3; the first bonding area 31 and the second bonding area 32 of the base group are the same in shape and size. The lithium-ion battery is tested 20 times at each position, and the pass rate is required to be not less than 80% (that is, at least 16 electrochemical devices do not fail when dropped) to be qualified. The drop conditions are: Group 1 is a single side drop, Group 2 is two opposite side drops, and Group 3 is six sides and four corners. The length L1 of the electrode assembly 2 of the selected rectangular lithium-ion battery is 87mm, the width W1 is 64mm, the length L2 of the first bonding area 31 is 60mm, and the width W2 is 42mm. The test results are shown in the following table:

[0056]

[0057] According to the test results in the above table, after setting the insulating tape 3 of the application so that the area A of the first bonding area and the area B of the second bonding area satisfy: 0.08≤B / A≤0.965, the electrochemical device has a higher pass rate in the drop test, and when 0.05×W2≤h≤0.35W2, the pass rate is even higher (≥90%).

[0058] In a specific embodiment, Figures 4 to 6 As shown, the electrode assembly 2 has a third surface 21 bonded to the insulating tape 3, that is, the third surface 21 of the electrode assembly 2 is bonded to the first bonding area 31 of the insulating tape 3, wherein the first bonding area 31 covers the positive projection of the second bonding area 32 on the third surface 21.

[0059] In this embodiment, when the first bonding area 31 covers the positive projection of the second bonding area 32 on the third surface 21, the external force transmitted from the second bonding area 32 can be completely transmitted to the first bonding area 31 through the insulating tape 3, and then transmitted to the third surface 21 of the electrode assembly 2, thereby reducing the risk of the insulating tape 3 breaking under the action of external force, improving the structural strength and service life of the insulating tape 3, and thus improving the connection reliability between the shell 1 and the electrode assembly 2.

[0060] Specifically, Figure 7 As shown, the length of the third surface 21 of the electrode assembly 2 is L1, and along the width direction of the electrochemical device, the first bonding area 31 has a first axis 312, and the third surface 21 has a second axis 211, and the first axis 312 and the second axis 211 are both axes extending along the width direction of the electrochemical device, and in the Figure 7 In the illustrated embodiment, along the length direction, the first bonding area 31 is symmetrical with respect to the first axis 312, and the third surface 21 is symmetrical with respect to the second axis 211. The distance between the orthographic projection of the first axis 312 on the third surface 21 and the second axis 211 is D, where D can be 0, or, according to actual conditions, L and L1 can also satisfy: D≤0.1×L1. For example, D can be 0.05L1, 0.06L1, etc. In addition, as Figure 7 As shown, along the length direction of the electrochemical device, the first bonding area 31 of the insulating tape 3 has a third axis 313, and the third surface 21 has a fourth axis 212, wherein the third axis 313 and the fourth axis 212 are axes extending along the length direction of the electrochemical device, and in the Figure 7In the illustrated embodiment, along the width direction of the electrochemical device, the first bonding area 31 is symmetrical with respect to the third axis 313, and the third surface 21 is symmetrical with respect to the fourth axis 212. In this embodiment, the distance between the orthographic projection of the third axis 313 on the third surface 21 and the fourth axis 212 is E, where E can be 0, or, according to actual conditions, E and W1 can also satisfy E≤0.15×W1.

[0061] Among them, the distance between D and L1, and the distance between E and W1 can be set according to actual conditions, as long as the connection reliability between the insulating tape 3 and the electrode assembly 2 can be improved and the risk of breakage between the two at the edges can be reduced.

[0062] In this embodiment, the weight of the electrode assembly 2 is not uniform in various places, and the connection reliability between the insulating tape 3 and the electrode assembly 2 is affected by the gravity of the electrode assembly 2. Therefore, when the weight of the electrode assembly 2 is uneven, the influence of the gravity of the electrode assembly 2 on the connection reliability between the insulating tape 3 and the electrode assembly 2 can be reduced by changing the position of the insulating tape 3 on the third surface 21.

[0063] In one possible design, Figures 4 to 7 As shown, the orthographic projection of the geometric center of the second bonding area 32 on the first surface coincides with the geometric center of the first bonding area 31. In another possible design, the ratio of the distance extending from the geometric centers of the first bonding area 31 and the second bonding area 32 along the same direction to the first outer edge 311 and the distance extending to the outer edge 321 is the same.

[0064] In this embodiment, since the orthographic projection of the geometric center of the second bonding area 32 on the first surface coincides with the geometric center of the first bonding area 31, the geometric center of the second bonding area 32 and the geometric center of the first bonding area 31 are located on the same straight line, so that after the insulating tape 3 is bonded to the shell 1 and the electrode assembly 2, the forces on the first bonding area 31 and the second bonding area 32 are relatively uniform, thereby improving the structural strength of the insulating tape 3. At the same time, since the ratio of the distance extending from the geometric centers of the first bonding area 31 and the second bonding area 32 to the first outer edge 311 and the distance extending to the outer edge 321 in the same direction is the same, the orthographic projection of the second bonding area 32 on the first surface is located in the middle of the first bonding area 31, thereby further improving the uniformity of the force transmitted from the second bonding area 32 to the first bonding area 31, improving the structural strength of the insulating tape 3 and the bonding strength between the insulating tape 3 and the electrode assembly 2.

[0065] In the above embodiments, Figure 7As shown, the electrode assembly 2 has a third surface 21 bonded to the insulating tape 3, the length of the third surface 21 is L1, and the width is W1; the length of the first bonding area 31 of the insulating tape 3 for bonding to the electrode assembly 2 is L2, and the width is W2; wherein, 0.4×L 1≤L2≤0.8×L 1, 0.4×W 1≤W2≤0.8×W 1. For example, L2 can be specifically 0.4×L 1, 0.5×L 1, 0.7×L 1, 0.8×L 1, etc., and W2 can be specifically 0.4×W 1, 0.6×W1, 0.7×W1, 0.8×W1, etc.

[0066] Among them, the relationship between L1 and L2, W1 and W2 is not limited to the above, and can also be set according to actual conditions, as long as it can improve the connection reliability between the insulating tape 3 and the electrode assembly 2 and prevent the electrode assembly 2 from being torn.

[0067] In a first specific embodiment, Figure 1 As shown, the insulating tape 3 may be an integrated structure, and the insulating tape 3 may be formed into a first bonding area 31 and a second bonding area 32 of different areas by cutting or other processing methods. In this embodiment, the integrated insulating tape 3 has the advantages of simple structure and high strength.

[0068] In the second specific embodiment, Figure 2 As shown, the insulating tape 3 can be a split structure, that is, it includes two tape monomers, and both tape monomers are double-sided adhesive, so that one surface of the two tape monomers is bonded, and the other surface is respectively used to bond with the shell 1 and the electrode assembly 2. In this embodiment, the insulating tape 3 of the split structure has the advantages of simple structure and convenient processing, and can facilitate the first bonding area 31 and the second bonding area 32 of the insulating tape 3 to have different bonding forces.

[0069] In the third specific embodiment, Figure 3 As shown, the insulating tape 3 includes a first adhesive material 33, a base material 35 and a second adhesive material 34 which are stacked, wherein the base material 35 is located between the first adhesive material 33 and the second adhesive material 34 and connected to the two. The first adhesive material 33 is used to bond with the electrode assembly 2, that is, the first bonding area 31 is arranged on the first adhesive material 33, and the second adhesive material 34 is used to bond with the shell 1, that is, the second bonding area 32 is arranged on the second adhesive material 34.

[0070] Among them, Figure 3 As shown, the area of ​​the first adhesive material 33 is larger than that of the second adhesive material 34 , the size of the substrate 35 is the same as that of the first adhesive material 33 with a larger area, the first adhesive material 33 and the substrate 35 can be bonded, and the second adhesive material 34 and the substrate 35 can also be bonded.

[0071] In this embodiment, the base material 35 of the insulating tape 3 can support the first adhesive material 33 and the second adhesive material 34, thereby improving the structural strength of the insulating tape 3, thereby reducing the risk of damage to the insulating tape 3 under the action of external force, and improving the connection reliability between the housing 1 and the electrode assembly 2. At the same time, the insulating tape 3 of the split structure has the advantages of simple structure and convenient processing, and can facilitate the first bonding area 31 and the second bonding area 32 of the insulating tape 3 to have different bonding forces.

[0072] In the above embodiments, Figure 8 As shown, in the insulating tape 3, the shapes of the first adhesive area 31 and the second adhesive area 32 are selected from any one of square, rectangle, trapezoid, octagon, circle and ellipse.

[0073] The electrochemical device in the embodiment of the present application can be used in a variety of fields, as long as the device can be powered by the electrochemical device, the electrochemical device in the embodiment of the present application can be used. For example, the electrochemical device can be used for the electrochemical device package and electronic devices of electric vehicles, and the electronic device can be a mobile phone, a tablet computer, a desktop computer, a laptop computer, a handheld computer, a notebook computer, an ultra-mobile personal computer (ultra-mobile personal computer, UMPC), a netbook, and a cellular phone, a personal digital assistant (personal digital assistant, PDA), an augmented reality (augmented reality, AR) device, a virtual reality (virtual reality, VR) device, an artificial intelligence (artificial intelligence, AI) device, a wearable device, a vehicle-mounted device, a smart home device and / or a smart city device, a power tool, an energy storage device, an electric tricycle, an electric vehicle, etc., and the specific type of the electronic device is not particularly limited in the embodiment of the present application.

[0074] Specifically, the electronic device may include components such as a housing, a screen, a circuit board, and an electrochemical device, wherein the screen, the circuit board, and the electrochemical device are all installed in the housing, and the electrochemical device is the electrochemical device described in any of the above embodiments.

[0075] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. An electrochemical device, It is characterized in that The electrochemical device comprises: case; an electrode assembly, at least a portion of which is located within the housing; and An insulating tape, the insulating tape is located between the housing and the electrode assembly, and the insulating tape includes a first surface bonded to the electrode assembly and a second surface bonded to the housing; the first surface includes a first bonding area, and the second surface includes a second bonding area; wherein the first bonding area has a first outer edge, and the second bonding area has a second outer edge; The distance between the orthographic projection of the second outer edge on the first surface and the first outer edge is h, and the width of the first surface is W2; Among them, 0.035×W2≤h≤0.4×W2.

2. The electrochemical device according to claim 1, It is characterized in that The area A of the first bonding area and the area B of the second bonding area satisfy: 0.08≤B / A≤0.

965.

3. The electrochemical device according to claim 2, It is characterized in that At least one of the following conditions is met: a) 0.15≤B / A≤0.85; b)0.05×W2≤h≤0.35×W2.

4. The electrochemical device according to claim 2, It is characterized in that The electrode assembly has a third surface bonded to the insulating tape, and the first bonding area covers the orthographic projection of the second bonding area on the third surface.

5. The electrochemical device according to claim 1, It is characterized in that The electrode assembly has a third surface bonded to the insulating tape, and the length of the third surface is L1; Along the width direction of the electrochemical device, the first bonding area has a first axis, the third surface has a second axis, and a distance D between an orthographic projection of the first axis on the third surface and the second axis is D, where D≤0.1×L1.

6. The electrochemical device according to claim 1, It is characterized in that The electrode assembly has a third surface bonded to the insulating tape, and the width of the third surface is W1; Along the length direction of the electrochemical device, the first bonding area has a third axis, the third surface has a fourth axis, and a distance between an orthographic projection of the third axis on the third surface and the fourth axis is E, where E≤0.1×W1.

7. The electrochemical device according to claim 2, It is characterized in that The orthographic projection of the geometric center of the second bonding area on the first surface coincides with the geometric center of the first bonding area.

8. The electrochemical device according to claim 1, It is characterized in that The insulating tape comprises a first adhesive material, a base material, and a second adhesive material which are stacked, wherein the first adhesive material is bonded to the electrode assembly, and the second adhesive material is bonded to the shell.

9. The electrochemical device according to claim 1, It is characterized in that The shapes of the first bonding area and the second bonding area are selected from any one of square, rectangle, trapezoid, octagon, circle and ellipse.

10. An electronic device, It is characterized in that The electronic device comprises the electrochemical device according to any one of claims 1 to 9.