Display panel and display device

By providing trenches on the partition structure of the OLED display panel and extending the sub-packaging portion to the trench side wall, the problem of easy peeling of the inorganic packaging layer is solved, and packaging performance and reliability of the display panel are improved.

CN118890923APending Publication Date: 2024-11-01BLACK COW FOOD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410950469.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-09-25
Filing Date
2024-07-16
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing OLED display panels have poor reliability, mainly because the inorganic packaging layer is easy to peel off, resulting in low packaging performance.

Method used

By providing grooves on the side where the partition structure is facing away from the substrate, and extending the sub-packaging part to the side wall and groove wall of the groove, the coverage area of ​​the packaging part is increased, the void between the packaging part and the partition structure is reduced, and the packaging is improved. performance.

Benefits of technology

It effectively reduces the risk of peeling off the sub-packaging part and partition structure, and improves packaging performance and reliability of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118890923A_ABST
    Figure CN118890923A_ABST
Patent Text Reader

Abstract

The invention relates to a display panel and a display device. The display panel includes: a substrate; the plurality of sub-pixels are arranged on the substrate at intervals; the partition structure is arranged between at least part of two adjacent sub-pixels; the plurality of sub-packaging parts are arranged on the sides, deviating from the substrate, of the corresponding sub-pixels; wherein the surface of one side, deviating from the substrate, of the partition structure is provided with at least one groove, and the groove is provided with a groove cavity close to the substrate and an opening end far away from the substrate; the orthographic projection of the opening end on the substrate falls into the orthographic projection range of the groove cavity on the substrate; the sub-packaging part corresponding to at least one sub-pixel adjacent to the groove further covers the side, close to the sub-pixel, of the partition structure, the side, away from the substrate, of the partition structure and at least part of the groove wall of the groove. The packaging performance of the sub-packaging parts can be improved, so that the reliability of the display panel is improved.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application claims priority to Chinese patent application number 2023112431657, filed on September 25, 2023, and entitled “Display Panel and Display Device,” the entire text of which is hereby incorporated by reference. Technical Field

[0002] The present application relates to the field of display technology, and in particular to a display panel and a display device. Background Art

[0003] Organic Light Emitting Diode (OLED) display technology is regarded as the most promising new flat panel display technology of the next generation. Compared with liquid crystal display technology, OLED display technology has the advantages of low energy consumption, low cost, self-luminescence, wide viewing angle and fast response speed. However, the current OLED display panel has the problem of poor reliability. Summary of the invention

[0004] Based on this, it is necessary to provide a display panel and a display device that can improve reliability.

[0005] In a first aspect, an embodiment of the present application provides a display panel, the display panel comprising:

[0006] substrate;

[0007] A plurality of sub-pixels are disposed on the substrate at intervals;

[0008] a partition structure, disposed between at least partially adjacent two of the sub-pixels; and

[0009] A plurality of sub-packaging parts are arranged on a side of the corresponding sub-pixel away from the substrate;

[0010] Wherein, at least one groove is provided on a surface of a side of the partition structure away from the substrate, and the groove has a groove cavity close to the substrate and an open end away from the substrate; the orthographic projection of the open end on the substrate falls within the orthographic projection range of the groove cavity on the substrate;

[0011] The sub-packaging portion corresponding to at least one of the sub-pixels adjacent to the groove further covers a side of the partition structure close to the sub-pixel, a side of the partition structure away from the substrate, and at least a portion of a groove wall of the groove.

[0012] The display panel provided by the embodiment of the present application is provided with a groove on the side of the partition structure away from the substrate, and the sub-encapsulation part is extended from the side wall of the partition structure to cover the side of the partition structure away from the substrate, and extends to cover at least part of the groove wall of the groove. In this way, on the one hand, the coverage area of ​​the sub-encapsulation part on the partition structure is increased, thereby extending the peeling path of the sub-encapsulation part and improving the packaging performance of the sub-encapsulation part; on the other hand, since the sub-encapsulation part extends to the groove wall of the groove, the void between the sub-encapsulation part and the surface of the side of the partition structure away from the substrate is eliminated, thereby reducing the risk of peeling between the sub-encapsulation part and the surface of the side of the partition structure away from the substrate, and improving the packaging performance of the sub-encapsulation part; on the other hand, since the sub-encapsulation part extends to the groove wall of the groove, even if peeling occurs, the groove wall of the groove can play a blocking role and "lock" the sub-encapsulation part, thereby reducing the risk of peeling between the sub-encapsulation part and the partition structure and improving the packaging performance of the sub-encapsulation part.

[0013] In a second aspect, an embodiment of the present application provides a display panel, including:

[0014] substrate;

[0015] A plurality of sub-pixels are disposed on the substrate at intervals;

[0016] a partition structure, disposed between at least partially adjacent two of the sub-pixels; and

[0017] A plurality of sub-packaging parts are arranged on a side of the corresponding sub-pixel away from the substrate;

[0018] Wherein, a side of the partition structure close to the sub-pixel is provided with a first concave portion and a second concave portion stacked and spaced apart in a direction away from the substrate;

[0019] The sub-encapsulation portion is configured as a continuous film layer structure covering the corresponding sub-pixel, the first concave portion, and the second concave portion.

[0020] The display panel provided by the embodiment of the present application is provided with a first recess and a second recess on the partition structure, and the sub-encapsulation part covers the corresponding sub-pixel, the first recess and the second recess. In this way, on the one hand, the coverage area of ​​the sub-encapsulation part on the partition structure is increased, thereby extending the peeling path of the sub-encapsulation part and improving the packaging performance of the sub-encapsulation part; on the other hand, since the sub-encapsulation part covers the second recess, even if peeling occurs, the second recess can play a blocking role, increasing the difficulty of peeling of the sub-encapsulation part, thereby reducing the risk of peeling between the sub-encapsulation part and the partition structure, and improving the packaging performance of the sub-encapsulation part.

[0021] In a third aspect, an embodiment of the present application provides a display panel, including:

[0022] substrate;

[0023] A plurality of sub-pixels are disposed on the substrate at intervals;

[0024] a partition structure, disposed on the substrate; the partition structure is disposed between at least two adjacent sub-pixels; and

[0025] A plurality of sub-packaging parts correspondingly covering a side of the sub-pixel away from the substrate;

[0026] Wherein, a first undercut portion is provided on a side of the partition structure close to the adjacent sub-pixel, so as to partition two adjacent sub-pixels;

[0027] The partition structure is further provided with a second undercut portion spaced apart from the first undercut portion;

[0028] The sub-encapsulation portion corresponding to the sub-pixel adjacent to the partition structure also extends to cover the wall surfaces of the first undercut portion and the second undercut portion to form a continuous film layer structure.

[0029] The display panel provided by the embodiment of the present application is provided with a first undercut portion and a second undercut portion on the partition structure, and the sub-encapsulation portion covers the corresponding sub-pixel, the first undercut portion and the second undercut portion. In this way, on the one hand, the coverage area of ​​the sub-encapsulation portion on the partition structure is increased, thereby extending the peeling path of the sub-encapsulation portion and improving the packaging performance of the sub-encapsulation portion; on the other hand, since the sub-encapsulation portion covers the second undercut portion, even if peeling occurs, the second undercut portion can play a blocking role, increasing the difficulty of peeling of the sub-encapsulation portion, thereby reducing the risk of peeling between the sub-encapsulation portion and the partition structure, and improving the packaging performance of the sub-encapsulation portion.

[0030] In a fourth aspect, an embodiment of the present application provides a display device, comprising the display panel in any of the above embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the technical solutions in the embodiments or exemplary embodiments of the present application, the drawings required for use in the description of the embodiments or exemplary embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0032] FIG. 1 is a schematic diagram of a cross-sectional structure of a display panel in the related art.

[0033] Figure 2AA schematic diagram of a partial cross-sectional structure of a display panel provided in one embodiment of the present application.

[0034] Figure 2B A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0035] Figure 2C A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0036] Figure 2D A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0037] Figure 3 for Figure 2A A schematic diagram of a partial cross-sectional structure of a partition structure of a display panel is shown.

[0038] Figure 4 for Figure 2A A schematic top view of a display panel is shown.

[0039] Figure 5A for Figure 2A Another schematic top view of the display panel is shown.

[0040] Figure 5B for Figure 2A Another schematic top view of the display panel is shown.

[0041] Figure 5C for Figure 5B A partial schematic diagram of .

[0042] Figure 6 A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0043] Figure 7 for Figure 6 A schematic diagram of a partial cross-sectional structure of a partition structure of a display panel is shown.

[0044] Figure 8 and Fig. 9 for Figure 2A The schematic diagram of the structure of the display panel during the manufacturing process is shown.

[0045] Fig.10 A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0046] Fig.11 for Fig.10 A schematic diagram of a partial cross-sectional structure of a partition structure of a display panel is shown.

[0047] Fig.12A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0048] Fig.13 for Fig.12 A schematic diagram of a partial cross-sectional structure of a partition structure of a display panel is shown.

[0049] Fig.14 A schematic diagram of a partial cross-sectional structure of another display panel provided in an embodiment of the present application.

[0050] Fig.15 for Fig.14 A schematic diagram of a partial cross-sectional structure of a partition structure of a display panel is shown.

[0051] Fig.16 A schematic diagram of the structure of a display device provided in one embodiment of the present application.

[0052] Description of reference numerals:

[0053] 10. Display panel; 11. Isolation structure; 12. Sub-pixel; 13. Inorganic encapsulation layer; 14. Cavity area;

[0054] 20. Display panel; 21. Substrate; 22. Sub-pixel; 221. First electrode; 222. Light-emitting functional unit; 223. Second electrode; 23. Partition structure; 23a. Partition opening; 23b. First recess; 23c. Second recess; 23d. First undercut; 23e. Second undercut; 231. Insulator; 2311. First metal layer; 2312. Second metal layer; 232. Blocking unit; 2321. Sub-blocking unit; 233. First insulator; 234. First blocking unit; 2341. First sub-blocking unit; 235. First Two insulators; 236, second blocking part; 2361, second sub-blocking part; 24, sub-packaging part; 25, groove; 25a, opening end; 25b, groove cavity; 25c, groove section; 251, sub-groove; 252, first sub-groove; 253, sub-opening; 254, second sub-groove; 26, pixel defining layer; 27, first packaging layer; 28, second packaging layer; 31, first metal material; 32, second metal material; 33, third metal material; 34, photoresist; 35, light-emitting material layer; 36, electrode material layer; 100, display device. DETAILED DESCRIPTION

[0055] In order to facilitate the understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present application more thorough and comprehensive.

[0056] It should be understood that although the terms "first", "second", etc. may be used herein to describe various elements, they do not represent any order, quantity or importance, but are only used to distinguish different components. These terms are only used to distinguish one element from another element. For example, without departing from the scope of the present application, the first element may be referred to as the second element, and similarly, the second element may be referred to as the first element. "Including" or "comprising" and similar words mean that the elements or objects appearing before the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects.

[0057] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0058] Organic Light Emitting Diode (OLED) display technology is regarded as the most promising new flat panel display technology of the next generation. Compared with liquid crystal display technology, OLED display technology has the advantages of low energy consumption, low cost, self-luminescence, wide viewing angle and fast response speed. As shown in Figure 1, in the relevant OLED display technology, the inorganic encapsulation layer 13 of the display panel 10 covers the sub-pixel 12 and the side wall of the isolation structure 11, and at the same time, a cavity area 14 is formed between the inorganic encapsulation layer 13 and the top surface of the isolation structure 11. However, due to the existence of the cavity area 14, the inorganic encapsulation layer 13 is prone to peeling from a position close to the cavity area 14 after being subjected to a force, resulting in the inorganic encapsulation layer 13 being peeled off from the isolation structure 11, thereby reducing the encapsulation performance of the inorganic encapsulation layer 13, making the reliability of the display panel 10 poor and prone to poor display.

[0059] In view of at least one of the above problems, embodiments of the present application provide a display panel and a display device, which can improve the packaging performance of the sub-packaging part, thereby improving the reliability of the display panel and the display device.

[0060] First, refer to Figure 2A , Figure 2B , Figure 2C , Figure 2D and Figure 3As shown, an embodiment of the present application provides a display panel 20, which may be an organic light emitting diode display panel 20 (Organic Light Emitting Diode, referred to as OLED) or a quantum dot electroluminescent display panel 20 (Quantum Dot Light Emitting Diodes, referred to as QLED).

[0061] The display panel 20 includes a substrate 21 , a plurality of sub-pixels 22 , a partition structure 23 , and a plurality of sub-packaging portions 24 .

[0062] Specifically, the substrate 21 may be an array substrate. A plurality of sub-pixels 22 are disposed at intervals on the substrate 21. The partition structure 23 is disposed between at least partially adjacent two sub-pixels 22. A plurality of sub-encapsulation portions 24 are disposed on a side of the corresponding sub-pixel 22 away from the substrate 21.

[0063] Among them, at least one groove 25 is provided on the surface of the side of the partition structure 23 facing away from the substrate 21, and the groove 25 has a groove cavity 25b close to the substrate 21 and an open end 25a away from the substrate 21. The orthographic projection of the open end 25a on the substrate 21 falls within the orthographic projection range of the groove cavity 25b on the substrate 21, that is, the groove 25 is a groove structure with a "small opening and a large cavity".

[0064] The sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers the side of the partition structure 23 close to the sub-pixel 22, the side of the partition structure 23 away from the substrate 21, and at least part of the groove wall of the groove 25, that is, the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 extends along the outer contour of the partition structure 23 from the side of the partition structure 23 close to the sub-pixel 22 into the groove 25, and passes through the top of the partition structure 23 (the side of the partition structure 23 away from the substrate 21).

[0065] Thus, on the one hand, compared with the related art, the embodiment of the present application increases the coverage area of ​​the sub-packaging portion 24 on the partition structure 23, thereby extending the termination coverage position of the sub-packaging portion 24 and the Peeling path of the sub-pixel 22 surface, thereby improving the packaging performance of the sub-packaging portion 24.

[0066] On the other hand, when evaporating the light-emitting material and the electrode material of the sub-pixel 22, the light-emitting material and the electrode material cannot cover the wall of the groove 25. However, since the sub-packaging portion 24 extends to the wall of the groove 25, that is, the sub-packaging portion 24 is in direct contact with the wall of the groove 25, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained to form a stacked light-emitting material layer 35 and an electrode material layer 36. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0067] On the other hand, since the sub-packaging portion 24 extends to the wall of the groove 25, even if peeling occurs, the wall of the groove 25 can act as a barrier to slow down the "lifting" of the sub-packaging portion 24 in the groove 25, thereby "locking" the sub-packaging portion 24, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0068] On the other hand, the sub-packaging portion 24 covers the side of the partition structure 23 close to the sub-pixel 22, that is, the sub-packaging portion 24 is in direct contact with the side of the partition structure 23 close to the sub-pixel 22, so that it can play a sealing role and improve the packaging reliability of the sub-packaging portion 24.

[0069] In one embodiment, the partition structure 23 includes an isolator 231 and a blocking portion 232 stacked on the substrate 21, and the blocking portion 232 extends toward the sub-pixel 22 to protrude from a side surface of the isolator 231 close to the sub-pixel 22. The isolator 231 and the blocking portion 232 define a groove 25.

[0070] It can be understood that by making the end of the blocking portion 232 close to the sub-pixel 22 protrude from the side wall of the insulator 231, the protruding part of the blocking portion 232 can form an "eave", so that the partition structure 23 has the function of isolating the light-emitting material and the electrode material.

[0071] It should be noted that the sub-packaging portion 24 covers a portion of the surface of the spacer 231 close to the sub-pixel 22, and covers the surface of the barrier 232 close to the substrate 21 (i.e., the lower surface of the protruding portion of the barrier 232). In this way, a sealing structure is formed between the sub-packaging portion 24 and the spacer 231, and a sealing structure is formed between the sub-packaging portion 24 and the lower surface of the protruding portion of the barrier 232, which can effectively prevent external water vapor from diffusing in the direction of the sub-pixel 22, and effectively prevent external defects from expanding in the direction of the sub-pixel 22, thereby improving the packaging reliability of the sub-packaging portion 24.

[0072] It should also be noted that, in one example, both opposite ends of the blocking portion 232 protrude from the sidewalls of the isolating body 231. The sub-packaging portions 24 corresponding to the sub-pixels 22 on both sides of the partition structure 23 respectively cover the lower surfaces of the protruding portions of the adjacent blocking portions 232, that is, the sub-packaging portions 24 corresponding to the sub-pixels 22 are in direct contact with the lower surfaces of the protruding portions of the adjacent blocking portions 232, thereby forming a sealing structure, which can effectively prevent external water vapor from diffusing along the surface of the partition structure 23 toward the sub-pixels 22, and effectively prevent external defects from extending toward the sub-pixels 22, thereby improving the packaging reliability of the sub-packaging portions 24.

[0073] In one embodiment, the opening end 25 a penetrates the blocking portion 232 along the thickness direction of the substrate 21 , and a sub-groove 251 is provided on a surface of the isolating body 231 facing away from the substrate 21 , and the sub-groove 251 defines a groove cavity 25 b .

[0074] In one embodiment, referring to Figure 3 As shown, the dimension L of the opening end 25a along the first direction X is smaller than the dimension W of the sub-groove 251 along the first direction X. The first direction X is perpendicular to the thickness direction of the substrate 21 and the extension direction of the groove 25. In the embodiment of the present application, the groove 25 extends in a direction perpendicular to the paper surface.

[0075] In one embodiment, referring to Figure 2B As shown, the sub-groove 251 penetrates the isolator 231 along the thickness direction of the substrate 21. In this way, the sub-packaging part 24 can cover a larger area, which is beneficial to improving the packaging reliability of the sub-packaging part 24.

[0076] In one embodiment, the sub-groove 251 is configured as a light-transmitting hole. In this way, light can pass through the partition structure 23, thereby improving the light transmittance of the display panel 20. In some embodiments, an under-screen functional module (such as an under-screen camera) is disposed on the back of the display panel 20. By configuring the sub-groove 251 as a light-transmitting hole, the working performance of the under-screen functional module can be improved.

[0077] In one embodiment, referring to Figure 2A As shown, a surface of the blocking portion 232 on one side away from the substrate 21 is provided with a light-emitting material layer 35 and an electrode material layer 36 stacked in sequence, and the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 is also covered on the top surface of the electrode material layer 36, the side surface of the electrode material layer 36, and the side surface of the light-emitting material layer 35.

[0078] In this way, the sub-encapsulation part 24 surrounds the light emitting material layer 35 and the electrode material layer 36. Compared with the related art, the embodiment of the present application eliminates the void between the sub-encapsulation part 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-encapsulation part 24 and the partition structure 23, and improving the packaging performance of the sub-encapsulation part 24.

[0079] In one embodiment, referring to Figure 2A and Figure 3 As shown, the partition structure 23 includes an isolator 231 and at least two sub-blocking portions 2321 stacked on the substrate 21. The at least two sub-blocking portions 2321 are arranged at intervals along the first direction X. That is, the at least two sub-blocking portions 2321 are arranged in parallel between two adjacent sub-pixels 12. The isolator 231 and the two adjacent sub-blocking portions 2321 define a groove 25.

[0080] It can be understood that when the partition structure 23 includes only two sub-blocking portions 2321, the two sub-blocking portions 2321 are spaced apart at both ends of the isolator 231 along the first direction X. At the same time, in the first direction X, the two sub-blocking portions 2321 extend in a direction away from the center of the isolator 231 to protrude from the side wall of the isolator 231. In this way, the partition structure 23 can achieve the effect of isolating the light-emitting materials of two adjacent sub-pixels 22.

[0081] In one embodiment, referring to Figure 3 As shown, a sub-groove 251 is provided on the surface of the isolator 231 facing away from the substrate 21, and the orthographic projections of two adjacent sub-blocking portions 2321 on the substrate 21 partially overlap with the orthographic projections of the corresponding sub-groove 251 on the substrate 21, that is, the two adjacent sub-blocking portions 2321 are spaced apart from each other, and the space between the two sub-blocking portions 2321 is the opening end 25a of the groove 25. Further, the groove cavity 25b is located in the sub-groove 251.

[0082] Here, it should be noted that the sub-groove 251 constitutes a part of the groove 25 , and the other part of the groove 25 is constituted by the space between the two sub-blocking portions 2321 .

[0083] In a preferred embodiment, the sub-packaging portion 24 extends to cover the groove wall of the sub-groove 251. On the one hand, there is no void between the sub-packaging portion 24 and the top of the partition structure 23, which can reduce the risk of peeling between the sub-packaging portion 24 and the partition structure 23; on the other hand, even if peeling occurs, the open end 25a of the groove 25 can play a blocking role, slowing down the "lifting" of the sub-packaging portion 24 located in the sub-groove 251 outward, thereby "locking" the sub-packaging portion 24, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0084] In one embodiment, the minimum distance L between two adjacent sub-blocking portions 2321 is smaller than a dimension W of an end of the sub-groove 251 away from the substrate 21 along the first direction X.

[0085] In this way, it is helpful to form a groove 25 with a "small opening and a large cavity". At the same time, when the light-emitting material and electrode material of the sub-pixel 22 are evaporated, the light-emitting material and the electrode material cannot cover the side surface of the sub-blocking part 2321 close to the sub-groove 251. However, since the sub-packaging part 24 extends to the groove wall of the sub-groove 251, that is, the sub-packaging part 24 is in direct contact with the side surface of the sub-blocking part 2321 close to the sub-groove 251, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained to form a stacked light-emitting material layer 35 and an electrode material layer 36. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging part 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging part 24 and the partition structure 23, and improving the packaging performance of the sub-packaging part 24.

[0086] In one embodiment, at least one groove 25 is disposed on the partition structure 23 between two adjacent sub-pixels 22 .

[0087] In one embodiment, referring to Figure 2A As shown, a groove 25 is provided on the partition structure 23 between two adjacent sub-pixels 22. The sub-packaging parts 24 corresponding to the two adjacent sub-pixels 22 extend and cover the same groove 25. In this way, one groove 25 can realize enhanced packaging of the sub-packaging parts 24 on both sides thereof, which is beneficial to improving the packaging reliability of the display panel 20.

[0088] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the groove 25 also covers a side of the blocking portion 232 adjacent to the sub-pixel 22 close to the groove 25 .

[0089] In a specific example, referring to Figure 2A As shown, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the groove 25 also covers a side of the sub-blocking portion 2321 adjacent to the sub-pixel 22 close to the groove 25 .

[0090] It can be understood that when evaporating the light-emitting material and the electrode material of the sub-pixel 22, the light-emitting material and the electrode material cannot cover the side surface of the sub-blocking portion 2321 close to the sub-groove 251. However, since the sub-packaging portion 24 extends to the groove wall of the sub-groove 251, that is, the sub-packaging portion 24 is in direct contact with the side surface of the sub-blocking portion 2321 close to the sub-groove 251, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained to form a stacked light-emitting material layer 35 and an electrode material layer 36. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0091] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the groove 25 also covers the groove wall of the sub-groove 251 adjacent to the sub-pixel 22. That is, the sub-encapsulation portion 24 covers the side wall of the sub-groove 251 adjacent to the sub-pixel 22.

[0092] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the trench 25 also covers at least a portion of the trench wall of the sub-trench 251 .

[0093] In a preferred embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the groove 25 also covers the sidewall of the sub-groove 251 adjacent to the sub-pixel 22 and a portion of the bottom wall of the sub-groove 251 .

[0094] Thus, for one sub-pixel 22, the sub-packaging portion 24 can form two "sealing rings", thereby improving the packaging performance of the sub-packaging portion 24. The sub-packaging portion 24 covering the side of the sub-blocking portion 2321 close to the sub-groove 251, the side wall of the sub-groove 251, and part of the bottom wall of the sub-groove 251 constitutes a "sealing ring", and the sub-packaging portion 24 covering the side of the partition structure 23 close to the sub-pixel 22 constitutes another "sealing ring".

[0095] In one embodiment, referring to Figure 2C As shown, part of the sub-encapsulation part 24 is located on the side of the bottom wall of the sub-groove 251 away from the substrate 21, and there is a gap between the part of the sub-encapsulation part 24 and the bottom wall of the sub-groove 251. This is because, during the manufacturing process, a light-emitting material layer 35 and an electrode material layer 36 are provided in the gap, and the part of the sub-encapsulation part 24 covers the light-emitting material layer 35 and the electrode material layer 36. In the subsequent wet etching process, the light-emitting material layer 35 and the electrode material layer 36 in the gap are removed, so that there is a gap between the part of the sub-encapsulation part 24 and the bottom wall of the sub-groove 251.

[0096] In one embodiment, the sub-encapsulation portion 24 is an inorganic film layer.

[0097] In one embodiment, referring to Figure 2D As shown, the display panel 20 further includes a first encapsulation layer 27 and a second encapsulation layer 28, wherein the first encapsulation layer 27 at least covers a side of the plurality of sub-encapsulation portions 24 away from the substrate 21, and the second encapsulation layer 28 covers a side of the first encapsulation layer 27 away from the substrate 21. The first encapsulation layer 27 is an organic film layer, and the second encapsulation layer 28 is an inorganic film layer. In this way, the encapsulation performance of the display panel 20 can be improved. It can be understood that the gap between the sub-encapsulation portion 24 and the bottom wall of the sub-groove 251 can also be filled with the first encapsulation layer 27.

[0098] In one embodiment, referring to Figure 4 , Figure 5A and Figure 5B As shown, the partition structure 23 defines a plurality of partition openings 23a, each of which corresponds to a sub-pixel 22. The groove 25 is disposed around at least a portion of the periphery of the partition opening 23a, that is, at least a portion of the periphery of the sub-pixel 22 is provided with the groove 25.

[0099] In one example, the partition structure 23 is a mesh structure, that is, the orthographic projection of the partition structure 23 on the substrate 21 is a mesh. It can be understood that the mesh partition structure 23 has mesh holes, and the mesh holes are the partition openings 23a.

[0100] In one embodiment, a groove 25 is disposed around at least a portion of the periphery of a partition opening 23 a.

[0101] In one embodiment, referring to Figure 5A and Figure 5B As shown, the grooves 25 are discontinuous grooves, that is, each groove 25 includes a plurality of groove segments 25c, and the plurality of groove segments 25c are arranged at intervals around the outer circumference of the partition opening 23a.

[0102] In one example, referring to Figure 5A As shown, four groove sections 25c are arranged on the outer periphery of one partition opening 23a, that is, the partition opening 23a has four sides, and one groove section 25c is arranged on each side.

[0103] In another example, referring to Figure 5B and Figure 5C As shown, a plurality of slot segments 25c are arranged on the periphery of a partition opening 23a. Specifically, the partition opening 23a has four sides, each of which is provided with a plurality of slot segments 25c. Thus, the plurality of slot segments 25c are arranged in an "island-like" manner on the periphery of the partition opening 23a.

[0104] It should be noted that Figure 5A and Figure 5B The difference between the groove 25 shown in FIG. 1 and FIG. 2 is that: Figure 5A The length of the middle groove section 25c is Figure 5B The length of the middle slot section 25c is longer. Figure 5A The number of the middle slot segments 25c is Figure 5B The number of middle slot segments 25c is even smaller.

[0105] It is understandable that the lengths of the slot segments 25c may be equal or unequal. The spacing between any two adjacent slot segments 25c may be equal or unequal. The specific arrangement of the slot segments 25c is not limited in the embodiment of the present application.

[0106] In a preferred embodiment, the plurality of groove segments 25c are evenly spaced around the periphery of the partition opening 23a, that is, the distance between any two adjacent groove segments 25c is equal. In this way, not only can the packaging reliability around the sub-pixel 22 be improved, but also the packaging reliability around the sub-pixel 22 can be made more uniform.

[0107] It can be understood that when the groove 25 is a discontinuous groove, the blocking portion 232 is an integrated structure.

[0108] It should be noted that when the groove 25 is a discontinuous groove, Figure 2B As shown, the groove 25 may penetrate the partition structure 23 along the thickness direction of the substrate 21 . At this time, the partition structure 23 is not divided into a plurality of independent structures by the groove 25 , that is, the partition structure 23 is still an integrated structure.

[0109] In one embodiment, referring to Figure 4 As shown, the groove 25 surrounds the entire periphery of the partition opening 23a, that is, the groove 25 is a continuous groove 25. In this way, at least two "sealing rings" can be formed around the sub-pixel 22, thereby further improving the packaging performance of the sub-packaging part 24.

[0110] It is understandable that, combined with Figure 2A and Figure 4 As shown, when the groove 25 is a continuous groove 25 and a groove 25 is provided on the periphery of a sub-pixel 22, the partition structure 23 includes two sub-blocking portions 2321, which are spaced apart on the isolation body 231, and the groove 25 is located between the two sub-blocking portions 2321.

[0111] In one embodiment, the orthographic projection of each groove 25 separating the outer periphery of the opening 23a on the substrate 21 is a closed ring, that is, the groove 25 is a ring structure. Exemplarily, the groove 25 can be a circular ring, a rectangular ring, a triangular ring, etc.

[0112] In one embodiment, the orthographic projections of all the grooves 25 on the partition structure 23 on the substrate 21 are in a grid shape. In this way, all the grooves 25 are connected to form a grid of grooves 25. In this way, the arrangement of the grooves 25 can be more regular and the arrangement density can be higher, which is conducive to further improving the packaging performance of the sub-packaging part 24.

[0113] In one embodiment, referring to Figure 6 and Figure 7 As shown, two trenches 25 arranged in parallel are disposed between two adjacent sub-pixels 22. The sub-encapsulation portions 24 corresponding to the two adjacent sub-pixels 22 extend to cover the trenches 25 adjacent to them.

[0114] In this way, two adjacent sub-packaging parts 24 can each “occupy” their own groove 25 , which is beneficial to increasing the coverage area of ​​each sub-packaging part 24 in the groove 25 , thereby improving the packaging performance of the sub-packaging part 24 .

[0115] In a specific embodiment, referring to Figure 6 and Figure 7 As shown, the partition structure 23 includes three sub-blocking portions 2321 arranged at intervals along the first direction X. The spacer 231 and the three sub-blocking portions 2321 together define two grooves 25. The two grooves 25 are arranged at intervals along the first direction X. The sub-encapsulation portions 24 corresponding to the two adjacent sub-pixels 22 extend and cover the grooves 25 adjacent to themselves.

[0116] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to each trench 25 also covers a side of the blocking portion 232 adjacent to the sub-pixel 22 close to the trench 25 .

[0117] In a specific embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to each groove 25 also covers a side of the sub-blocking portion 2321 adjacent to the sub-pixel 22 close to the groove 25 .

[0118] It can be understood that when evaporating the light-emitting material and the electrode material of the sub-pixel 22, the light-emitting material and the electrode material cannot cover the side surface of the sub-blocking portion 2321 close to the sub-groove 251. However, since the sub-packaging portion 24 extends to the groove wall of the sub-groove 251, that is, the sub-packaging portion 24 is in direct contact with the side surface of the sub-blocking portion 2321 close to the sub-groove 251, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained to form a stacked light-emitting material layer 35 and an electrode material layer 36. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0119] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to each trench 25 also covers the trench wall of the sub-trench 251 adjacent to the sub-pixel 22 . That is, the sub-encapsulation portion 24 also covers the sidewall of the sub-trench 251 adjacent to the sub-pixel 22 .

[0120] In this way, the packaging performance of the sub-packaging portion 24 can be further improved.

[0121] In one embodiment, the sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to each groove 25 also covers the entire groove wall of the sub-groove 251 adjacent to the sub-pixel 22. It can be understood that the side wall of the sub-blocking portion 2321 close to the sub-groove 251 is also a part of the groove wall.

[0122] Thus, for one sub-pixel 22, the sub-packaging portion 24 can form three "sealing rings", thereby improving the packaging performance of the sub-packaging portion 24. Among them, a "sealing ring" is formed on the sidewalls of the sub-groove 251 on both sides along the first direction X, and another "sealing ring" is formed on the side of the partition structure 23 close to the sub-pixel 22.

[0123] It should be noted that the light emitting material layer 35 and the electrode material layer 36 may be formed on the bottom wall of the sub-groove 251. When the light emitting material layer 35 and the electrode material layer 36 are formed on the bottom wall of the sub-groove 251, the sub-encapsulation part 24 may cover the light emitting material layer 35 and the electrode material layer 36.

[0124] In one embodiment, referring to Figure 6As shown, the sub-packaging portion 24 covers the entire groove wall of the groove 25 corresponding to itself, and extends outward from the groove 25 to the side of the sub-blocking portion 2321 in the middle away from the substrate 21, and forms a cavity between the sub-blocking portion 2321 and the top surface of the sub-blocking portion 2321. In this arrangement, even if a cavity is formed between the sub-blocking portion 2321 in the middle and the end of the sub-packaging portion 24, when the sub-packaging portion 24 peels, since the sub-packaging portion 24 forms three "sealing rings", compared with the related art, the embodiment of the present application can also improve the packaging performance of the sub-packaging portion 24.

[0125] In one embodiment, the sub-pixel 22 includes a first electrode 221 , a light emitting functional portion 222 , and a second electrode 223 stacked in a direction away from the substrate 21 . The second electrode 223 of the sub-pixel 22 is electrically connected to the partition structure 23 .

[0126] In this way, it is convenient to connect the second electrode 223 of the sub-pixel 22 with the pixel driving circuit through the partition structure 23, so that the wiring arrangement of the display area is more optimized.

[0127] It should be noted that the first electrode 221 may be an anode, and the second electrode 223 may be a cathode. The first electrode 221 and the second electrode 223 are both electrically connected to the pixel driving circuit. If the first electrode 221 is a cathode, the partition structure 23 transmits a VSS signal, and if the first electrode 221 is an anode, the partition structure 23 transmits a signal.

[0128] It is understood that the light-emitting functional part 222 includes at least a light-emitting layer (Emission layer, EML), and may also include one or more of a hole injection layer (HIL), a hole transport layer (HTL), an electron injection layer (EIL), an electron transport layer (ETL), a hole blocking layer (HBL) and an electron blocking layer (EBL). Alternatively, the light-emitting functional part 222 may also be a laminated light-emitting layer, that is, including at least two light-emitting layers and a charge generation layer (CGL) located between each adjacent light-emitting layer.

[0129] In one embodiment, the spacer 231 includes at least one metal layer, and the second electrode 223 of the sub-pixel 22 is electrically connected to the spacer 231. In one example, the spacer 231 includes a metal layer. Further, the material of the spacer 231 includes at least one of a metal and a metal oxide. Exemplarily, the metal may be silver, copper, titanium, aluminum, etc. The metal oxide may be tin oxide, zinc oxide, cadmium oxide, indium oxide, indium tin oxide, zinc indium oxide, zinc gallium oxide, zinc aluminum oxide, titanium tantalum oxide, etc.

[0130] In one embodiment, the spacer 231 includes a first metal layer 2311 and a second metal layer 2312 stacked in a direction away from the substrate 21. The resistivity of the second metal layer 2312 is less than that of the first metal layer 2311. The second electrode 223 of the sub-pixel 22 is in direct contact with the second metal layer 2312.

[0131] In this way, on the one hand, it is beneficial to reduce the electrical contact resistance between the partition structure 23 and the second electrode 223 , and on the other hand, it is beneficial to reduce the resistance of the partition structure 23 , thereby reducing the power consumption of the display panel 20 .

[0132] In one example, the material of the first metal layer 2311 may be Mo, the material of the second metal layer 2312 may be Al, and the material of the sub-blocking portion 2321 may be Ti.

[0133] In one embodiment, referring to Figure 8 and Fig. 9 As shown, the embodiment of the present application provides a Figure 2A The manufacturing method of the display panel 20 is shown as follows:

[0134] The specific steps are as follows:

[0135] S100 : forming a first electrode 221 and a pixel defining layer 26 on the substrate 21 in sequence.

[0136] S200 : forming a first metal material 31 , a second metal material 32 and a third metal material 33 which are sequentially stacked on the substrate 21 .

[0137] S300 : etching the third metal material 33 to form an opening end 25 a of the trench 25 .

[0138] S400 : etching the second metal material 32 to form a trench 25 .

[0139] S500 : forming a photoresist 34 on the third metal material 33 and exposing a portion of the surface of the third metal material 33 .

[0140] S600 : etching the third metal material 33 layer, the second metal material 32 layer and the first metal material 31 layer to form a partition structure 23 .

[0141] S700 : forming a sub-pixel 22 of a first color and a corresponding sub-packaging portion 24 on the substrate 21 .

[0142] S800 : forming a sub-pixel 22 of a second color and a corresponding sub-packaging portion 24 on the substrate 21 .

[0143] In one embodiment, after S800, the following steps are also included:

[0144] S900 : forming a sub-pixel 22 of a third color and a corresponding sub-packaging portion 24 on the substrate 21 .

[0145] Second, refer to Fig.10 and Fig.11 As shown, an embodiment of the present application provides a display panel 20, which may be an organic light emitting diode display panel 20 (Organic Light Emitting Diode, referred to as OLED) or a quantum dot electroluminescent display panel 20 (Quantum Dot Light Emitting Diodes, referred to as QLED).

[0146] The display panel 20 includes a substrate 21 , a plurality of sub-pixels 22 , a partition structure 23 , and a plurality of sub-packaging portions 24 .

[0147] Specifically, the substrate 21 may be an array substrate 21. A plurality of sub-pixels 22 are disposed at intervals on the substrate 21. The partition structure 23 is disposed between at least partially adjacent two sub-pixels 22. A plurality of sub-encapsulation portions 24 are disposed on a side of the corresponding sub-pixel 22 away from the substrate 21.

[0148] The partition structure 23 has a first recess 23b and a second recess 23c stacked and spaced apart in a direction away from the substrate 21 on one side thereof close to the sub-pixel 22. The sub-encapsulation portion 24 is configured as a continuous film layer structure covering the corresponding sub-pixel 22, the first recess 23b, and the second recess 23c.

[0149] It should be noted that in the embodiment of the present application, a pixel defining layer 26 is disposed on the substrate 21, and the partition structure 23 is disposed on a side of the pixel defining layer 26 away from the substrate 21. The partition structure 23 defines a plurality of partition openings 23a. The plurality of sub-pixels 22 are correspondingly disposed in the plurality of partition openings 23a.

[0150] Here, the “first recess 23 b ” and the “second recess 23 c ” may also be understood as grooves whose openings face toward the partition opening 23 a .

[0151] The display panel 20 provided in the embodiment of the present application is provided with a first recess 23b and a second recess 23c on the partition structure 23, and the sub-encapsulation part 24 covers the corresponding sub-pixel 22, the first recess 23b and the second recess 23c. In this way, on the one hand, the coverage area of ​​the sub-encapsulation part 24 on the partition structure 23 is increased, thereby extending the peeling path of the sub-encapsulation part 24 and improving the packaging performance of the sub-encapsulation part 24. On the other hand, since the sub-encapsulation part 24 covers the second recess 23c, even if peeling occurs, the second recess 23c can play a blocking role, increasing the difficulty of peeling of the sub-encapsulation part 24, thereby reducing the risk of peeling between the sub-encapsulation part 24 and the partition structure 23, and improving the packaging performance of the sub-encapsulation part 24.

[0152] In one embodiment, the partition structure 23 includes a first isolating body 233, a first blocking portion 234, a second isolating body 235, and a second blocking portion 236 stacked in a direction away from the substrate 21. The first blocking portion 234 extends in a direction close to the partition opening 23a to protrude from the wall surface of the first blocking portion 234. The second blocking portion 236 extends in a direction close to the partition opening 23a to protrude from the wall surface of the second isolating body 235. The first blocking portion 234, the first isolating body 233, and the substrate 21 define a first recess 23b, and the second blocking portion 236, the second isolating body 235, and the first blocking portion 234 define a second recess 23c.

[0153] That is, the substrate 21, the first insulator 233 and the first blocking portion 234 define a groove toward the isolated opening 23a. The first blocking portion 234, the second insulator 235 and the second blocking portion 236 define another groove toward the isolated opening 23a. In a specific embodiment, the pixel defining layer 26, the first insulator 233 and the first blocking portion 234 define a groove toward the isolated opening 23a.

[0154] The above arrangement makes it easier to arrange the first recess 23b and the second recess 23c on the partition structure 23, thereby reducing the difficulty of arranging the first recess 23b and the second recess 23c.

[0155] In one embodiment, referring to Fig.10 As shown, a surface of the first blocking portion 234 on one side away from the substrate 21 is provided with a light-emitting material layer 35 and an electrode material layer 36 stacked in sequence, and the sub-packaging portion 24 also covers the top surface of the electrode material layer 36 , the side surface of the electrode material layer 36 , and the side surface of the light-emitting material layer 35 .

[0156] In one example, after the sub-packaging portion 24 extends to cover the surfaces of the first recess 23 b and the second recess 23 c , it also extends to a side of the second blocking portion 236 away from the substrate 21 , and forms a cavity between the sub-packaging portion 24 and the top surface of the second blocking portion 236 .

[0157] In this way, on the one hand, the coverage area of ​​the sub-packaging part 24 on the partition structure 23 is increased, thereby extending the peeling path of the sub-packaging part 24 and improving the packaging performance of the sub-packaging part 24. On the other hand, even if the sub-packaging part 24 starts to peel from the top surface of the second blocking part 236, since the sub-packaging part 24 covers the second recess 23c, the second recess 23c can play a blocking role, increasing the difficulty of the sub-packaging part 24 peeling, thereby reducing the risk of peeling between the sub-packaging part 24 and the partition structure 23, and improving the packaging performance of the sub-packaging part 24.

[0158] In one embodiment, referring to Fig.12 As shown, at least one groove 25 is provided on the surface of the partition structure 23 facing away from the substrate 21, and the groove 25 has a groove cavity 25b close to the substrate 21 and an open end 25a away from the substrate 21. The orthographic projection of the open end 25a on the substrate 21 falls within the orthographic projection range of the groove cavity 25b on the substrate 21, that is, the groove 25 is a groove structure with a "small opening and a large cavity".

[0159] The sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers the side of the partition structure 23 close to the sub-pixel 22, the side of the partition structure 23 away from the substrate 21, and at least part of the groove wall of the groove 25, that is, the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 extends along the outer contour of the partition structure 23 from the side of the partition structure 23 close to the sub-pixel 22 toward the groove 25, and passes through the top of the partition structure 23 (the side of the partition structure 23 away from the substrate 21).

[0160] Thus, on one hand, the coverage area of ​​the sub-packaging portion 24 on the partition structure 23 is further increased, thereby extending the Peeling path between the termination coverage position of the sub-packaging portion 24 and the surface of the sub-pixel 22 , and improving the packaging performance of the sub-packaging portion 24 .

[0161] On the other hand, when evaporating the light-emitting material and the electrode material of the sub-pixel 22, the light-emitting material and the electrode material cannot cover the wall of the groove 25. However, since the sub-packaging portion 24 extends to the wall of the groove 25, that is, the sub-packaging portion 24 is in direct contact with the wall of the groove 25, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and further improves the packaging performance of the sub-packaging portion 24.

[0162] On the other hand, since the sub-packaging portion 24 extends to the wall of the groove 25, even if peeling occurs, the wall of the groove 25 can act as a barrier to slow down the "lifting" of the sub-packaging portion 24 in the groove 25, thereby "locking" the sub-packaging portion 24, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0163] On the other hand, the sub-packaging portion 24 covers the side of the partition structure 23 close to the sub-pixel 22, that is, the sub-packaging portion 24 is in direct contact with the side of the partition structure 23 close to the sub-pixel 22, so that it can play a sealing role and improve the packaging reliability of the sub-packaging portion 24.

[0164] It should be noted that the structure of the groove 25 in the embodiment of the second aspect may be the same as that of the groove 25 in the embodiment of the first aspect, and the structure of the groove 25 will not be described in detail in the embodiment of the present application.

[0165] In one embodiment, a side surface of the second blocking portion 236 away from the substrate 21 is provided with a light-emitting material layer 35 and an electrode material layer 36 stacked in sequence, and the sub-packaging portion 24 also covers the top surface of the electrode material layer 36, the side surface of the electrode material layer 36, and the side surface of the light-emitting material layer 35.

[0166] In this way, the void between the sub-packaging portion 24 and the top of the partition structure 23 is eliminated, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23 , and further improving the packaging performance of the sub-packaging portion 24 .

[0167] In one embodiment, referring to Fig.12 and Fig.13 As shown, the groove 25 penetrates the second blocking portion 236 and at least a portion of the second isolating body 235 along the thickness direction of the substrate 21. In this way, the groove 25 can have enough space, which is conducive to the attachment of the sub-packaging portion 24.

[0168] In one embodiment, the groove 25 penetrates the entire second spacer 235 along the thickness direction of the substrate 21. In this way, the groove 25 can be made deeper, so that the space for the sub-package 24 to be attached is larger, which is beneficial to improving the packaging reliability of the sub-package 24.

[0169] In one embodiment, the groove 25 is configured as a light-transmitting hole. In this way, light can pass through the partition structure 23, thereby improving the light transmittance of the display panel 20. In some embodiments, an under-screen functional module (such as an under-screen camera) is disposed on the back of the display panel 20. By configuring the groove 25 as a light-transmitting hole, the working performance of the under-screen functional module can be improved.

[0170] In one embodiment, the opening end 25a penetrates the second blocking portion 236 along the thickness direction of the substrate 21, and the groove 25 includes a first sub-groove 252, and the first sub-groove 252 penetrates the entire second isolation body 235 along the thickness direction of the substrate 21. That is, the bottom wall of the first sub-groove 252 is arranged on the surface of the first blocking portion 234. In this way, it is beneficial to increase the coverage area of ​​the sub-encapsulation portion 24 in the first sub-groove 252.

[0171] In one embodiment, the first blocking portion 234 , the second isolating body 235 , and the second blocking portion 236 define a groove 25 , and the first sub-groove 252 defines a groove cavity 25 b.

[0172] In a specific embodiment, the second blocking portion 236 includes two second sub-blocking portions 2361 arranged at intervals along the first direction X. The first blocking portion 234 , the second isolation body 235 and the two second sub-blocking portions 2361 define a groove 25 .

[0173] In one embodiment, a first sub-groove 252 is disposed on a side of the second isolator 235 away from the substrate 21, and the orthographic projections of the two second sub-blocking portions 2361 on the substrate 21 partially overlap with the orthographic projections of the first sub-groove 252 on the substrate 21 to define an open end 25a of the groove 25. The groove cavity 25b is located in the first sub-groove 252.

[0174] Here, it should be noted that the sub-groove 25 constitutes a part of the groove 25 , and the other part of the groove 25 is constituted by the space between the two second sub-blocking portions 2361 .

[0175] In one embodiment, the dimension of the opening end 25 a along the first direction X is smaller than the dimension of the first sub-groove 252 along the first direction X. The first direction X is perpendicular to the thickness direction of the substrate 21 and the extension direction of the groove 25 .

[0176] In a specific embodiment, the minimum distance between two adjacent second sub-blocking portions 2361 is smaller than the dimension of the first sub-groove 252 along the first direction X at one end away from the substrate 21 .

[0177] In this way, it is helpful to form a groove 25 with a "small opening and a large cavity". At the same time, when the light-emitting material and the electrode material of the sub-pixel 22 are evaporated, the light-emitting material and the electrode material cannot cover the side surface of the second sub-blocking portion 2361 close to the first sub-groove 252. However, since the sub-packaging portion 24 extends to the groove wall of the first sub-groove 252, that is, the sub-packaging portion 24 is in direct contact with the side surface of the second sub-blocking portion 2361 close to the first sub-groove 252, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and the electrode material on the top of the partition structure 23 are retained. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0178] In one embodiment, the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers a side of the second blocking portion 236 adjacent to the sub-pixel 22 close to the groove 25 and at least a portion of the groove wall of the first sub-groove 252 .

[0179] In a preferred embodiment, the sub-encapsulation portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers the sidewall of the first sub-groove 252 adjacent to the sub-pixel 22 and a portion of the bottom wall of the first sub-groove 252 .

[0180] Thus, for one sub-pixel 22, the sub-packaging portion 24 can form three "sealing rings", thereby improving the packaging performance of the sub-packaging portion 24. Among them, a "sealing ring" is formed in the first sub-groove 252, a "sealing ring" is formed on the first concave portion 23b, and another "sealing ring" is formed on the second concave portion 23c.

[0181] In one embodiment, the sub-packaging parts 24 on both sides of the groove 25 extend to cover the same groove 25. In this way, a groove 25 can achieve enhanced packaging for the sub-packaging parts 24 on both sides thereof, which is beneficial to improving the packaging reliability of the display panel 20.

[0182] In one embodiment, referring to Fig.14 and Fig.15 As shown, the groove 25 also penetrates the first blocking portion 234 along the thickness direction of the substrate 21 .

[0183] In a preferred embodiment, the groove 25 also penetrates at least a portion of the first isolator 233 along the thickness direction of the substrate 21. In this way, the groove 25 can be made deeper, so that the sub-package 24 can be attached to a larger space, which is conducive to improving the packaging reliability of the sub-package 24.

[0184] In one embodiment, the groove 25 further includes a sub-opening 253 and a second sub-groove 254, the sub-opening 253 penetrates the first blocking portion 234 along the thickness direction of the substrate 21, and the second sub-groove 254 is provided on the surface of the first isolating body 233 away from the substrate 21. The first isolating body 233, the first blocking portion 234, the second isolating body 235 and the second blocking portion 236 define the groove 25. The first sub-groove 252, the sub-opening 253 and the second sub-groove 254 define a groove cavity 25b.

[0185] This is beneficial to increasing the attachment area of ​​the sub-packaging portion 24 in the groove 25 , thereby improving the packaging reliability of the sub-packaging portion 24 .

[0186] In one embodiment, a dimension of the sub-opening 253 along the first direction X is smaller than a dimension of the second sub-trench 254 along the first direction X.

[0187] This is beneficial for the sub-packaging portion 24 to form a plurality of “sealing rings” in the groove 25 , thereby further improving the packaging reliability of the sub-packaging portion 24 .

[0188] In one embodiment, the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers the side of the second blocking portion 236 adjacent to the sub-pixel 22 close to the groove 25, the groove wall of the first sub-groove 252 adjacent to the sub-pixel 22, the side of the first blocking portion 234 adjacent to the sub-pixel 22 close to the groove 25, and at least part of the groove wall of the second sub-groove 254.

[0189] In this way, for one sub-pixel 22, the sub-packaging portion 24 can form four "sealing rings", thereby improving the packaging performance of the sub-packaging portion 24. Among them, a "sealing ring" is formed in the second sub-groove 254, a "sealing ring" is formed in the first sub-groove 252, a "sealing ring" is formed on the first recess 23b, and another "sealing ring" is formed on the second recess 23c. Furthermore, in the embodiment, the void between the top of the partition structure 23 and the sub-packaging portion 24 can also be eliminated, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0190] In a specific embodiment, the first blocking portion 234 includes two first sub-blocking portions 2341 arranged at intervals along the first direction X. A sub-opening 253 is formed between the two first sub-blocking portions 2341. The first isolating body 233, the second isolating body 235, the two first sub-blocking portions 2341 and the two second sub-blocking portions 2361 define the groove 25.

[0191] In one example, the sub-packaging portion 24 corresponding to at least one sub-pixel 22 adjacent to the groove 25 also covers a side of the second sub-blocking portion 2361 close to the groove 25, a groove wall of the first sub-groove 252, a side of the first sub-blocking portion 2341 close to the groove 25, and at least a portion of the groove wall of the second sub-groove 254.

[0192] In one example, the second sub-groove 254 does not penetrate the first isolator 233 along the thickness direction of the substrate 21. In this way, the first isolator 233 is not interrupted, so that the first isolator 233 can have the function of transmitting current.

[0193] In one embodiment, the sub-pixel 22 includes a first electrode 221 , a light emitting functional portion 222 , and a second electrode 223 stacked in a direction away from the substrate 21 . The second electrode 223 of the sub-pixel 22 is electrically connected to the partition structure 23 .

[0194] In this way, it is convenient to connect the second electrode 223 of the sub-pixel 22 with the pixel driving circuit through the partition structure 23, so that the wiring arrangement of the display area is more optimized.

[0195] It should be noted that the first electrode 221 may be an anode, and the second electrode 223 may be a cathode. The first electrode 221 and the second electrode 223 are both electrically connected to the pixel driving circuit. If the first electrode 221 is a cathode, the partition structure 23 transmits a VSS signal, and if the first electrode 221 is an anode, the partition structure 23 transmits a signal.

[0196] It is understood that the light-emitting functional part 222 includes at least a light-emitting layer (Emission layer, EML), and may also include one or more of a hole injection layer (HIL), a hole transport layer (HTL), an electron injection layer (EIL), an electron transport layer (ETL), a hole blocking layer (HBL) and an electron blocking layer (EBL). Alternatively, the light-emitting functional part 222 may also be a laminated light-emitting layer, that is, including at least two light-emitting layers and a charge generation layer (CGL) located between each adjacent light-emitting layer.

[0197] In one embodiment, the first spacer 233 includes at least one metal layer. The second electrode 223 of the sub-pixel 22 is electrically connected to the first spacer 233. In one example, the spacer 231 includes a metal layer. Further, the material of the spacer 231 includes at least one of a metal and a metal oxide. Exemplarily, the metal may be silver, copper, titanium, aluminum, etc. The metal oxide may be tin oxide, zinc oxide, cadmium oxide, indium oxide, indium tin oxide, zinc indium oxide, zinc gallium oxide, zinc aluminum oxide, titanium tantalum oxide, etc.

[0198] In one embodiment, the first spacer 233 includes a first metal layer 2311 and a second metal layer 2312 stacked in a direction away from the substrate 21. The resistivity of the second metal layer 2312 is less than that of the first metal layer 2311. The second electrode 223 of the sub-pixel 22 is in direct contact with the second metal layer 2312.

[0199] In this way, on the one hand, it is beneficial to reduce the electrical contact resistance between the partition structure 23 and the second electrode 223 , and on the other hand, it is beneficial to reduce the resistance of the partition structure 23 , thereby reducing the power consumption of the display panel 20 .

[0200] In one example, the material of the first metal layer 2311 may be Mo, the material of the second metal layer 2312 may be Al, and the material of the first sub-blocking portion 2341 may be Ti.

[0201] In one embodiment, the material of the second isolating body 235 is the same as the material of the first isolating body 233. The material of the second sub-blocking portion 2361 can be the same as the material of the first sub-blocking portion 2341.

[0202] In one embodiment, the second isolator 235 and the second blocking portion 236 are an integrated structure, and the second isolator 235 and the second blocking portion 236 are made of organic material or inorganic material. In this way, the difficulty of manufacturing the second isolator 235 and the second blocking portion 236 can be reduced.

[0203] In one embodiment, the display panel 20 further includes a first encapsulation layer 27 and a second encapsulation layer 28, wherein the first encapsulation layer 27 at least covers a side of the plurality of sub-encapsulation portions 24 away from the substrate 21, and the second encapsulation layer 28 covers a side of the first encapsulation layer 27 away from the substrate 21. The first encapsulation layer 27 is an organic film layer, and the second encapsulation layer 28 is an inorganic film layer. In this way, the encapsulation performance of the display panel 20 can be improved.

[0204] In one embodiment, Fig.13 The second isolating body 235 and the second blocking portion 236 in the embodiment can be manufactured by the following steps:

[0205] S100 : forming a negative adhesive on the second blocking portion 236 .

[0206] S200: Hardening the local area of ​​the negative photoresist. Specifically, a chemical may be used to harden the local area of ​​the negative photoresist, making it difficult to be developed and etched.

[0207] S200: Etching the negative photoresist to form the second spacer 235 and the second barrier 236. Since the etching speed of the treated negative photoresist is lower than that of the untreated negative photoresist, the second spacer 235 and the second barrier 236 can be formed. Fig.13 The structure shown in .

[0208] Thirdly, refer to Figure 2A and Fig.10 As shown, an embodiment of the present application provides a display panel 20, which may be an organic light emitting diode display panel 20 (Organic Light Emitting Diode, referred to as OLED) or a quantum dot electroluminescent display panel 20 (Quantum Dot Light Emitting Diodes, referred to as QLED).

[0209] The display panel 20 includes a substrate 21 , a plurality of sub-pixels 22 , a partition structure 23 , and a plurality of sub-packaging portions 24 .

[0210] Specifically, the substrate 21 may be an array substrate 21. A plurality of sub-pixels 22 are disposed on the substrate 21 at intervals. A partition structure 23 is disposed on the substrate 21. A partition structure 23 is disposed between at least two adjacent sub-pixels 22. A plurality of sub-encapsulation portions 24 cover the side of the sub-pixel 22 facing away from the substrate 21.

[0211] Among them, a first undercut portion 23d is provided on one side of the partition structure 23 close to the adjacent sub-pixel 22, so as to separate two adjacent sub-pixels 22. The partition structure 23 is also provided with a second undercut portion 23e spaced apart from the first undercut portion 23d. The sub-encapsulation portion 24 corresponding to the sub-pixel 22 adjacent to the partition structure 23 also extends to cover the wall surfaces of the first undercut portion 23d and the second undercut portion 23e, so as to form a continuous film layer structure.

[0212] The display panel 20 provided in the embodiment of the present application is provided with a first undercut portion 23d and a second undercut portion 23e on the partition structure 23, and the sub-encapsulation portion 24 covers the corresponding sub-pixel 22, the first undercut portion 23d and the second undercut portion 23e. In this way, on the one hand, the coverage area of ​​the sub-encapsulation portion 24 on the partition structure 23 is increased, thereby extending the peeling path of the sub-encapsulation portion 24 and improving the packaging performance of the sub-encapsulation portion 24. On the other hand, since the sub-encapsulation portion 24 covers the second undercut portion 23e, even if peeling occurs, the second undercut portion 23e can play a blocking role, increasing the difficulty of peeling of the sub-encapsulation portion 24, thereby reducing the risk of peeling between the sub-encapsulation portion 24 and the partition structure 23, and improving the packaging performance of the sub-encapsulation portion 24.

[0213] In one embodiment, the end of the first bottom cut portion 23d close to the substrate 21 is defined as the first bottom, the end of the first bottom cut portion 23d away from the substrate 21 is defined as the first top, and the outer contour of the orthographic projection of the first top on the substrate 21 is located outside the outer contour of the orthographic projection of the first bottom on the substrate 21.

[0214] The end of the second bottom cut portion 23e close to the substrate 21 is defined as the second bottom, the end of the second bottom cut portion 23e away from the substrate 21 is defined as the second top, and the outer contour of the orthographic projection of the second top on the substrate 21 is located outside the outer contour of the orthographic projection of the second bottom on the substrate 21.

[0215] It should be noted that the “undercut portion” in the embodiments of the present application is an undercut structure well known to those skilled in the art.

[0216] In one embodiment, referring to Figure 2A As shown, the first undercut portion 23d and the second undercut portion 23e are arranged in parallel between two adjacent sub-pixels 22. In one example, in two adjacent sub-pixels 22, one first undercut portion 23d and one second undercut portion 23e are arranged, and the one first undercut portion 23d and the one second undercut portion 23e both correspond to the same sub-pixel 22. In this way, only the sub-encapsulation portion 24 corresponding to the one sub-pixel 22 can extend to cover the wall surfaces of the first undercut portion 23d and the second undercut portion 23e.

[0217] In a preferred embodiment, two first undercut portions 23d and at least one second undercut portion 23e are disposed between two adjacent sub-pixels 22, and the at least one second undercut portion 23e is disposed between the two first undercut portions 23d. In this way, the sub-encapsulation portions 24 corresponding to the two sub-pixels 22 can extend to cover the wall surfaces of the corresponding first undercut portion 23d and the second undercut portion 23e.

[0218] In one example, a first concave portion 23b is provided on a side of the partition structure 23 close to the adjacent sub-pixel 22, and the first concave portion 23b defines a first undercut portion 23d. A surface of the partition structure 23 facing away from the substrate 21 is provided with at least one groove 25, and the groove 25 has a groove cavity 25b close to the substrate 21 and an open end 25a away from the substrate 21. The orthographic projection of the open end 25a on the substrate 21 falls within the orthographic projection range of the groove cavity 25b on the substrate 21. The groove 25 defines a second undercut portion 23e.

[0219] Thus, on the one hand, compared with the related art, the embodiment of the present application increases the coverage area of ​​the sub-packaging portion 24 on the partition structure 23, thereby extending the Peeling path from the termination coverage position of the sub-packaging portion 24 to the surface of the sub-pixel 22, thereby improving the packaging performance of the sub-packaging portion 24.

[0220] On the other hand, when evaporating the light-emitting material and electrode material of the sub-pixel 22, the light-emitting material and electrode material 36 cannot cover the wall of the groove 25. However, since the sub-packaging portion 24 extends to the wall of the groove 25, that is, the sub-packaging portion 24 is in direct contact with the wall of the groove 25, the top of the partition structure 23 is completely encapsulated. In the subsequent etching process, the light-emitting material and electrode material on the top of the partition structure 23 are retained. Therefore, compared with the related art, the embodiment of the present application eliminates the void between the sub-packaging portion 24 and the top of the partition structure 23, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0221] On the other hand, since the sub-packaging portion 24 extends to the wall of the groove 25, even if peeling occurs, the wall of the groove 25 can act as a barrier to slow down the "lifting" of the sub-packaging portion 24 in the groove 25, thereby "locking" the sub-packaging portion 24, thereby reducing the risk of peeling between the sub-packaging portion 24 and the partition structure 23, and improving the packaging performance of the sub-packaging portion 24.

[0222] On the other hand, for one sub-pixel 22, the sub-encapsulation portion 24 can form two "sealing rings", thereby improving the encapsulation performance of the sub-encapsulation portion 24. Among them, a "sealing ring" is formed at the first undercut portion 23d, and another "sealing ring" is formed at the second undercut portion 23e.

[0223] On the other hand, the sub-packaging portion 24 covers the side of the partition structure 23 close to the sub-pixel 22, that is, the sub-packaging portion 24 is in direct contact with the side of the partition structure 23 close to the sub-pixel 22, so that it can play a sealing role and improve the packaging reliability of the sub-packaging portion 24.

[0224] It should be noted that the arrangement of the grooves 25 in this embodiment may be the same as the arrangement of the grooves 25 of the display panel 20 in the first aspect, and will not be described in detail herein.

[0225] In one embodiment, referring to Fig.10 As shown, the first undercut portion 23 d and the second undercut portion 23 e are stacked in a direction away from the substrate 21 .

[0226] Specifically, the partition structure 23 defines a plurality of partition openings 23a. A plurality of sub-pixels 22 are correspondingly arranged in the plurality of partition openings 23a. The partition structure 23 includes a first insulator 233, a first blocking portion 234, a second insulator 235, and a second blocking portion 236 stacked in a direction away from the substrate 21. The first blocking portion 234 extends in a direction close to the partition opening 23a to protrude from the wall surface of the first blocking portion 234. The second blocking portion 236 extends in a direction close to the partition opening 23a to protrude from the wall surface of the second insulator 235. The first blocking portion 234 and the first insulator 233 define a first undercut portion 23d, and the second blocking portion 236 and the second insulator 235 define a second undercut portion 23e. That is, the first recess 23b is the first undercut portion 23d, and the second recess 23c is the second undercut portion 23e.

[0227] It should be noted that the partition structure 23 in this embodiment may also be provided with a groove 25 , and the arrangement of the groove 25 may be the same as the arrangement of the display panel 20 in the second aspect, which will not be described in detail herein.

[0228] In one embodiment, the display panel 20 further includes a first encapsulation layer 27 and a second encapsulation layer 28, wherein the first encapsulation layer 27 at least covers a side of the plurality of sub-encapsulation portions 24 away from the substrate 21, and the second encapsulation layer 28 covers a side of the first encapsulation layer 27 away from the substrate 21. The first encapsulation layer 27 is an organic film layer, and the second encapsulation layer 28 is an inorganic film layer. In this way, the encapsulation performance of the display panel 20 can be improved.

[0229] Fourthly, refer to Fig.16 As shown, an embodiment of the present application provides a display device 100, which includes the display panel 20 described in any embodiment of the first aspect, the second aspect or the third aspect.

[0230] The display device 100 can be a laptop computer, a mobile phone, a wireless device, a personal digital assistant (PDA), a handheld or portable computer, a GPS receiver / navigator, a camera, an MP4 video player, a camcorder, a game console, a watch, a clock, a calculator, a television monitor, a flat-panel display, a computer monitor, a car display (e.g., an odometer display, etc.), a navigator, a cockpit controller and / or display, a display of a camera view (e.g., a display of a rearview camera in a vehicle), an electronic photo, an electronic billboard or sign, a projector, etc.

[0231] The display device 100 provided in the embodiment of the present application can improve the packaging performance of the sub-packaging portion 24 , thereby improving the reliability of the display device 100 .

[0232] In the case of using “including”, “having”, and “comprising” described herein, another component may be added unless a clear limiting term such as “only”, “consisting of”, etc. is used. Unless mentioned otherwise, a term in the singular form may include a plural form and should not be understood as being one in number.

[0233] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0234] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.

Claims

1. A display panel, characterized in that: include: substrate; A plurality of sub-pixels are disposed on the substrate at intervals; A partition structure is provided between at least partially adjacent two of the sub-pixels; as well as A plurality of sub-packaging parts are arranged on a side of the corresponding sub-pixel away from the substrate; Wherein, at least one groove is provided on a surface of a side of the partition structure away from the substrate, and the groove has a groove cavity close to the substrate and an open end away from the substrate; the orthographic projection of the open end on the substrate falls within the orthographic projection range of the groove cavity on the substrate; The sub-packaging portion corresponding to at least one of the sub-pixels adjacent to the groove further covers a side of the partition structure close to the sub-pixel, a side of the partition structure away from the substrate, and at least a portion of a groove wall of the groove.

2. The display panel according to claim 1, characterized in that: The partition structure includes an isolator and a blocking portion stacked on the substrate, the blocking portion extending toward the direction close to the sub-pixel to protrude from a side surface of the isolator close to the sub-pixel; the isolator and the blocking portion define the groove; Optionally, the opening end penetrates the blocking portion along the thickness direction of the substrate, and a sub-groove is provided on a surface of the isolating body facing away from the substrate, and the sub-groove defines the groove cavity; Optionally, a dimension of the opening end along the first direction is smaller than a dimension of the sub-groove along the first direction; The first direction is perpendicular to the thickness direction of the substrate and the extending direction of the groove; Optionally, the sub-groove penetrates the isolator along the thickness direction of the substrate; Optionally, the sub-groove is configured as a light-transmitting hole; Optionally, at least one groove is provided on the partition structure between two adjacent sub-pixels; Optionally, a surface of the blocking portion on one side away from the substrate is provided with a light-emitting material layer and an electrode material layer stacked in sequence, and the sub-packaging portion corresponding to at least one of the sub-pixels adjacent to the groove also covers the top surface of the electrode material layer, the side surface of the electrode material layer, and the side surface of the light-emitting material layer.

3. The display panel according to claim 2, characterized in that: A groove is provided between two adjacent sub-pixels; the sub-encapsulation parts corresponding to the two adjacent sub-pixels extend and cover the same groove; Optionally, the sub-encapsulation portion corresponding to the sub-pixel adjacent to the groove further covers a side of the blocking portion adjacent to the sub-pixel close to the groove; Optionally, the sub-encapsulation portion corresponding to the sub-pixel adjacent to the groove further covers the groove wall of the sub-groove adjacent to the sub-pixel.

4. The display panel according to claim 2, characterized in that: Two grooves arranged in parallel are arranged between two adjacent sub-pixels; The sub-packaging parts corresponding to the two adjacent sub-pixels respectively extend to cover the grooves adjacent to themselves; Optionally, the sub-encapsulation portion corresponding to the sub-pixel adjacent to each of the grooves further covers a side of the blocking portion adjacent to the sub-pixel close to the groove; Optionally, the sub-encapsulation portion corresponding to the sub-pixel adjacent to each of the grooves further covers the groove wall adjacent to the sub-pixel among the groove walls of the sub-grooves; Optionally, the sub-encapsulation portion corresponding to the sub-pixel adjacent to each of the trenches also covers the entire trench wall of the sub-trench.

5. The display panel according to claim 2, characterized in that: The sub-pixel comprises a first electrode, a light-emitting functional portion, and a second electrode stacked in a direction away from the substrate; the second electrode of the sub-pixel is electrically connected to the partition structure; Optionally, the isolator includes at least one metal layer, and the second electrode of the sub-pixel is electrically connected to the isolator; Optionally, the insulator includes a first metal layer and a second metal layer stacked in a direction away from the substrate; the resistivity of the second metal layer is smaller than the resistivity of the first metal layer, and the second electrode of the sub-pixel is in direct contact with the second metal layer.

6. The display panel according to claim 1, characterized in that: The partition structure defines a plurality of partition openings, each of which has a corresponding sub-pixel disposed therein; the groove is disposed around at least a portion of the periphery of the partition opening; Optionally, one of the grooves is disposed around at least a portion of the periphery of one of the partition openings; Optionally, the groove comprises a plurality of groove segments, and the plurality of groove segments are arranged at intervals around the periphery of the partition opening; Optionally, the plurality of slot segments are evenly spaced around the periphery of the partition opening; Optionally, the groove is arranged around the entire periphery of the partition opening; Optionally, the orthographic projection of each of the grooves at the periphery of the partition opening on the substrate is a closed ring; Optionally, the sub-packaging portion is an inorganic film layer; Optionally, the display panel further includes a first encapsulation layer and a second encapsulation layer, the first encapsulation layer at least covers a side of the multiple sub-encapsulation parts away from the substrate, and the second encapsulation layer covers a side of the first encapsulation layer away from the substrate; the first encapsulation layer is an organic film layer, and the second encapsulation layer is an inorganic film layer.

7. A display panel, characterized in that: include: substrate; A plurality of sub-pixels are disposed on the substrate at intervals; A partition structure is provided between at least partially adjacent two of the sub-pixels; as well as A plurality of sub-packaging parts are arranged on a side of the corresponding sub-pixel away from the substrate; Wherein, a side of the partition structure close to the sub-pixel is provided with a first concave portion and a second concave portion stacked and spaced apart in a direction away from the substrate; The sub-encapsulation portion is configured as a continuous film layer structure covering the corresponding sub-pixel, the first concave portion, and the second concave portion.

8. The display panel according to claim 7, characterized in that: The partition structure defines a plurality of partition openings; the plurality of sub-pixels are correspondingly arranged in the plurality of partition openings; The partition structure comprises a first isolator, a first blocking portion, a second isolator and a second blocking portion stacked in a direction away from the substrate; the first blocking portion extends in a direction close to the partition opening to protrude from a wall surface of the first blocking portion; The second blocking portion extends toward the direction close to the partition opening so as to protrude from the wall surface of the second isolating body; The first blocking portion, the first isolating body and the substrate define the first recessed portion, and the second blocking portion, the second isolating body and the first blocking portion define the second recessed portion; Optionally, a surface of the first blocking portion on one side away from the substrate is provided with a light-emitting material layer and an electrode material layer stacked in sequence, and the sub-packaging portion also covers the top surface of the electrode material layer, the side surface of the electrode material layer, and the side surface of the light-emitting material layer.

9. The display panel according to claim 8, characterized in that: At least one groove is provided on a surface of the partition structure on one side away from the substrate, wherein the groove has a groove cavity close to the substrate and an open end away from the substrate; the orthographic projection of the open end on the substrate falls within the orthographic projection range of the groove cavity on the substrate; The sub-encapsulation portion corresponding to at least one of the sub-pixels adjacent to the groove also covers a side of the partition structure close to the sub-pixel, a side of the partition structure away from the substrate, and at least a portion of the groove wall of the groove; Optionally, a surface of the second blocking portion on one side away from the substrate is provided with a light-emitting material layer and an electrode material layer stacked in sequence, and the sub-packaging portion also covers the top surface of the electrode material layer, the side surface of the electrode material layer, and the side surface of the light-emitting material layer.

10. The display panel according to claim 9, characterized in that: The groove penetrates the second blocking portion and at least a portion of the second isolating body along the thickness direction of the substrate; Optionally, the groove runs through the entire second isolator along the thickness direction of the substrate; Optionally, the groove is configured as a light-transmitting hole; Optionally, the open end penetrates the second blocking portion along the thickness direction of the substrate, the groove includes a first sub-groove, and the first sub-groove penetrates the entire second isolator along the thickness direction of the substrate; Optionally, the first blocking portion, the second isolating body and the second blocking portion define the groove, and the first sub-groove defines the groove cavity; Optionally, a dimension of the opening end along a first direction is smaller than a dimension of the first sub-groove along the first direction, and the first direction is perpendicular to a thickness direction of the substrate and an extending direction of the groove; Optionally, the sub-encapsulation portion corresponding to at least one of the sub-pixels adjacent to the groove further covers a side of the second blocking portion adjacent to the sub-pixel close to the groove, and at least a portion of a groove wall of the first sub-groove; Optionally, at least one groove is provided on the partition structure between two adjacent sub-pixels.

11. The display panel according to claim 10, characterized in that: The groove also penetrates the first blocking portion along the thickness direction of the substrate; Optionally, the groove also penetrates at least a portion of the first isolator along the thickness direction of the substrate; Optionally, the groove further includes a sub-opening and a second sub-groove, the sub-opening passes through the first blocking portion along the thickness direction of the substrate, and the second sub-groove is provided on a surface of the first isolator on one side away from the substrate; The first isolating body, the first blocking portion, the second isolating body and the second blocking portion define the groove; the first sub-groove, the sub-opening and the second sub-groove define the groove cavity; Optionally, a size of the sub-opening along the first direction is smaller than a size of the second sub-groove along the first direction; Optionally, the sub-packaging portion corresponding to at least one of the sub-pixels adjacent to the groove also covers the side of the second blocking portion adjacent to the sub-pixel close to the groove, the groove wall of the first sub-groove adjacent to the sub-pixel, the side of the first blocking portion adjacent to the sub-pixel close to the groove, and at least part of the groove wall of the second sub-groove.

12. The display panel according to claim 8, characterized in that: The sub-pixel comprises a first electrode, a light-emitting functional portion, and a second electrode stacked in a direction away from the substrate; the second electrode of the sub-pixel is electrically connected to the partition structure; Optionally, the first isolator includes at least one metal layer; the second electrode of the sub-pixel is electrically connected to the first isolator; Optionally, the first insulator comprises a first metal layer and a second metal layer stacked in a direction away from the substrate; the resistivity of the second metal layer is smaller than the resistivity of the first metal layer, and the second electrode of the sub-pixel is in direct contact with the second metal layer; Optionally, the second isolating body and the second blocking portion are an integrated structure, and the second isolating body and the second blocking portion are made of an organic material or an inorganic material; Optionally, the sub-packaging portion is an inorganic film layer; Optionally, the display panel further includes a first encapsulation layer and a second encapsulation layer, the first encapsulation layer at least covers a side of the multiple sub-encapsulation parts away from the substrate, and the second encapsulation layer covers a side of the first encapsulation layer away from the substrate; the first encapsulation layer is an organic film layer, and the second encapsulation layer is an inorganic film layer.

13. A display panel, characterized in that: include: substrate; A plurality of sub-pixels are disposed on the substrate at intervals; A partition structure is disposed on the substrate; The partition structure is disposed between at least two adjacent sub-pixels; and A plurality of sub-packaging parts correspondingly covering a side of the sub-pixel away from the substrate; Wherein, a first undercut portion is provided on a side of the partition structure close to the adjacent sub-pixel, so as to partition two adjacent sub-pixels; The partition structure is further provided with a second undercut portion spaced apart from the first undercut portion; The sub-encapsulation portion corresponding to the sub-pixel adjacent to the partition structure also extends to cover the wall surfaces of the first undercut portion and the second undercut portion to form a continuous film layer structure.

14. The display panel according to claim 13, characterized in that: Define an end of the first undercut portion close to the substrate as a first bottom portion, an end of the first undercut portion away from the substrate as a first top portion, and an outer contour of an orthographic projection of the first top portion on the substrate is located outside an outer contour of an orthographic projection of the first bottom portion on the substrate; The end of the second undercut portion close to the substrate is defined as a second bottom, the end of the second undercut portion away from the substrate is defined as a second top, and the outer contour of the orthographic projection of the second top on the substrate is located outside the outer contour of the orthographic projection of the second bottom on the substrate.

15. The display panel according to claim 13, characterized in that: The first undercut portion and the second undercut portion are stacked in a direction away from the substrate; Optionally, the partition structure defines a plurality of partition openings; the plurality of sub-pixels are correspondingly arranged in the plurality of partition openings; The partition structure comprises a first isolator, a first blocking portion, a second isolator and a second blocking portion stacked in a direction away from the substrate; the first blocking portion extends in a direction close to the partition opening to protrude from a wall surface of the first blocking portion; the second blocking portion extends in a direction close to the partition opening to protrude from a wall surface of the second isolator; The first blocking portion and the first isolating body define the first undercut portion, and the second blocking portion and the second isolating body define the second undercut portion.

16. The display panel according to claim 13, characterized in that: The first undercut portion and the second undercut portion are arranged in parallel between two adjacent sub-pixels; Optionally, two first undercut portions and at least one second undercut portion are arranged between two adjacent sub-pixels, and the at least one second undercut portion is arranged between the two first undercut portions; Optionally, a first concave portion is provided on a side of the partition structure close to the adjacent sub-pixel, and the first concave portion defines a first undercut portion; At least one groove is provided on a surface of a side of the partition structure away from the substrate, wherein the groove has a groove cavity close to the substrate and an open end away from the substrate; the orthographic projection of the open end on the substrate falls within the orthographic projection range of the groove cavity on the substrate; the groove defines the second undercut portion; Optionally, the sub-packaging portion is an inorganic film layer; Optionally, the display panel further includes a first encapsulation layer and a second encapsulation layer, the first encapsulation layer at least covers a side of the multiple sub-encapsulation parts away from the substrate, and the second encapsulation layer covers a side of the first encapsulation layer away from the substrate; the first encapsulation layer is an organic film layer, and the second encapsulation layer is an inorganic film layer.

17. A display device, characterized in that: Comprising the display panel as claimed in any one of claims 1 to 16.