Composite steel opening edge sealing process and structure

By dividing the composite steel pot into multiple areas and clamping and fixing with positioning and calibration mechanisms, the external surface damage caused by tool vibration is solved, and the quality and accuracy of the edge sealing process are improved.

CN118893461APending Publication Date: 2024-11-05JIANGMEN ANNUOTE COOKING UTENSILS MFG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411098757.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

During the edge sealing process, the composite steel pot has indentation, scratches and other damages on the outer surface due to tool vibration, which affects the product quality.

Method used

The composite steel pot is divided into several areas, and the positioning mechanism is used to clamp and fix the two sides of the first sliding area and the second sliding area respectively, and the deformation caused by molding is calibrated by the calibration mechanism to ensure the stability of clamping and Accuracy to avoid damage caused by vibration transmission.

Benefits of technology

It effectively reduces the external surface damage of the composite steel pot during the edge sealing process, and improves the quality of the product and edge sealing accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118893461A_ABST
    Figure CN118893461A_ABST
Patent Text Reader

Abstract

The invention relates to a composite steel opening edge sealing process and structure, and belongs to the technical field of composite steel opening edge sealing, a pot body part is divided into a plurality of areas through the characteristics of a composite steel pot, and the arc length L at the joint of a pot bottom part and the pot body part is delimited as a first sliding area with the arc length L as the length; delimiting a deformation area with the arc length M as the length along the direction of the pan body by taking the first sliding area as a starting point; the deformation area serves as a starting point, a second sliding area with the arc length S as the length is defined in the direction of the pot body, finally, the remaining part from the second sliding area to the top of the pot body is defined as an edge sealing area, the two sides of the first sliding area and the two sides of the second sliding area are clamped and fixed through a positioning mechanism, and meanwhile one side of the deformation area is fixed; the positioning mechanism is also used for limiting and fixing a third sliding area of the pot bottom; the problem that the outer surface of the composite steel pot is prone to being impressed, scratched and the like due to vibration is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of composite steel mouth edge sealing, and in particular relates to a composite steel mouth edge sealing process and structure. Background Art

[0002] Composite steel is a type of steel made by combining two or more different materials through a specific process. It usually combines materials with different performance characteristics to obtain products with better overall performance. Products made of composite steel have high hardness to ensure wear resistance, cutting resistance and other properties, and good toughness, and can also prevent easy breakage during use. Therefore, in practical applications, composite steel is widely used in the manufacture of knives, kitchen utensils, mechanical parts, etc. For example, some high-quality composite steel pots have high strength and can withstand certain impact and vibration.

[0003] At present, when the composite steel pot is undergoing the edge sealing process, it is necessary to ensure that the middle aluminum substrate is not exposed and that there is no risk of corrosion at the mouth of the product after its use. During this process, due to the work hardening and forming force of the composite steel pot material itself, the product will change in shape, resulting in poor concentricity. At the same time, the fit between the product and the mold is poor, and the deformation of the product is inconsistent, resulting in poor fit between the composite steel pot and the mold. In order to solve the above problems, most of them use a clamping device to clamp the composite steel pot as a whole on the mold along the outside of the composite steel pot, exposing the mouth of the composite steel pot, and then perform edge sealing processes such as curling and pressing on the mouth of the composite steel pot.

[0004] However, the current composite steel mouth edge sealing process still has some problems: when sealing the composite steel pot with a flat bottom, due to the irregular structure of the composite steel pot itself, when performing edge sealing processes such as curling and pressing, the tools used will generate vibrations, and the vibrations are transmitted to the composite steel pot, and the composite steel pot will tend to vibrate. However, since the clamping device will clamp the entire composite steel pot along the outer side of the composite steel pot and fix it on the mold, the vibration at this time will easily cause indentations, scratches and other damages to the outer surface of the composite steel pot. Therefore, a composite steel mouth edge sealing process and structure are proposed to reduce the occurrence of indentations, scratches and other damages on the outer surface of the composite steel pot during edge sealing. Summary of the invention

[0005] In order to solve the above-mentioned problems existing in the prior art, the present invention provides a composite steel mouth edge sealing process and structure, which solves the problem that when performing edge sealing processes such as curling and pressing in the prior art, the tools used will generate vibrations. After the vibrations are transmitted to the composite steel pot, the vibrations at this time will easily cause indentations, scratches and other damages on the outer surface of the composite steel pot.

[0006] The purpose of the present invention can be achieved through the following technical solutions:

[0007] A composite steel mouth edge sealing process comprises the following steps:

[0008] S1: Divide the composite steel pot into a pot bottom part and a pot body part;

[0009] S2: The pot body is divided into several areas. First, the arc length L is used as the length to define the arc length L at the connection between the pot bottom and the pot body as the first sliding area; then, starting from the first sliding area, along the direction of the pot body, a deformation area with an arc length M is defined; then, starting from the deformation area, along the direction of the pot body, a second sliding area with an arc length S is defined; finally, the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area;

[0010] S3: using a positioning mechanism to clamp and fix both sides of the first sliding area and the second sliding area respectively, and fix one side of the deformation area at the same time;

[0011] S4: Carry out edge turning, curling and pressing operations on the edge banding area.

[0012] As a further solution of the present invention, the arc length L in step S2 is greater than the arc length S.

[0013] As a further solution of the present invention, when the two sides of the first sliding area and the second sliding area are clamped and fixed in step S3, the deformation of the product caused by molding is calibrated by a calibration mechanism.

[0014] As a further solution of the present invention, the cutting operation in S4 is to perform cutting and level cutting processes on the product by using a CNC turning tool according to CNC programming.

[0015] A composite steel mouth edge sealing structure comprises a positioning mechanism, a calibration mechanism connected to the positioning mechanism, and a pressing and curling mechanism. The positioning mechanism is used to clamp and fix the composite steel pot. The composite steel pot is clamped and fixed by the positioning mechanism. The pressing and curling mechanism is used to press and curl the pot mouth of the composite steel pot.

[0016] As a further solution of the present invention, the curling mechanism includes a curling machine, a curling wheel and a pressing wheel. The curling wheel and the pressing wheel are both arranged on the curling machine, and the curling machine drives the curling wheel and the pressing wheel to move.

[0017] As a further solution of the present invention, the positioning mechanism includes a support frame, an upper mold, a positioning piece and a lower mold. The upper mold, the positioning piece and the lower mold are all arranged on the support frame, and the upper mold, the positioning piece and the lower mold are arranged in sequence from top to bottom. The pot body of the composite steel pot is clamped by the lower mold and the upper mold and the positioning piece and the upper mold respectively.

[0018] As a further solution of the present invention, the upper mold is connected to the support frame through an upper cylinder connecting rod, the calibration mechanism is arranged on the support frame, the lower mold is arranged on the calibration mechanism, and the bottom part of the composite steel pot is detachably located on the positioning piece.

[0019] As a further solution of the present invention, flexible gaskets are provided at the positions where the upper mold, the positioning member and the lower mold contact the composite steel pot.

[0020] As a further solution of the present invention, the calibration mechanism includes a calibration platform, two first hydraulic cylinders and two second hydraulic cylinders arranged on a support frame, the two first hydraulic cylinders having two ends connected to the lower mold and the calibration platform respectively, and the two second hydraulic cylinders having two ends connected to the positioning member and the calibration platform respectively.

[0021] The beneficial effects of the present invention are:

[0022] According to the characteristics of the composite steel pot, the pot body is divided into several areas. First, the arc length L is used as the length to define the arc length L at the connection between the pot bottom and the pot body as the first sliding area; then, starting from the first sliding area, a deformation area with an arc length M is defined along the direction of the pot body; then, starting from the deformation area, a second sliding area with an arc length S is defined along the direction of the pot body; finally, the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area, and a positioning mechanism is used to clamp and fix both sides of the first sliding area and the second sliding area respectively, and at the same time, the deformation area is fixed. One side of the area is fixed, and the positioning mechanism also limits and fixes the third sliding area of ​​the bottom of the pot; finally, the edge sealing area is turned, curled and pressed to complete the edge sealing process, which solves the problem that the tools used in edge sealing processes such as curling and pressing will generate vibrations, and the vibrations are transmitted to the composite steel pot. The composite steel pot has a tendency to vibrate, but because the clamping device will clamp and fix the entire composite steel pot on the mold along the outer side of the composite steel pot, the vibration at this time will easily cause damages such as indentations and scratches on the outer surface of the composite steel pot, which will ultimately affect the quality of the composite steel pot. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings.

[0024] Figure 1 A schematic diagram of several areas of the pot body of the present invention;

[0025] Figure 2 It is a schematic diagram of the overall structure of the present invention;

[0026] Description of main component symbols:

[0027] In the figure: 1. upper die; 2. positioning member; 3. lower die; 4. calibration mechanism; 5. CNC turning tool; 6. curling wheel; 7. pressing wheel; 8. support frame; 9. upper cylinder connecting rod; 10. first hydraulic cylinder; 11. second hydraulic cylinder. DETAILED DESCRIPTION

[0028] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in conjunction with the accompanying drawings and preferred embodiments.

[0029] See also Figure 1-2 This embodiment provides a composite steel mouth edge sealing process, comprising the following steps:

[0030] S1: Divide the composite steel pot into a pot bottom part and a pot body part;

[0031] S2: Since the composite steel pot itself is an irregularly shaped object, and the surface of the composite steel pot is easily damaged when it is fixed and clamped by the clamping device, scratches or indentations are easily caused. Therefore, intermittent point clamping is used when the composite steel pot is clamped by the clamping device to avoid surface damage, scratches or indentations. However, it is also necessary to ensure good clamping stability. Therefore, the pot body is divided into several areas. First, the arc length L is used as the length, and the arc length L at the connection between the pot bottom part and the pot body part is defined as the first sliding area; then, starting from the first sliding area, along the direction of the pot body, a deformation area with an arc length M is defined; and then starting from the deformation area, along the direction of the pot body, a deformation area with an arc length M is defined. The second sliding area with arc length S is determined, and finally the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area. In addition, if you want to use intermittent point clamping to ensure good clamping stability, the position of the intermittent clamping point needs special design. According to the characteristics of the composite steel pot and the force analysis of the composite steel pot, when the pot is clamped, the following parts are relatively easy to slide. The first is the connection between the bottom of the pot and the pot body. This part is usually an area of ​​stress concentration, and there may be a situation where the connection is not stable enough. When the clamping force is not applied properly, it is easy to slide here. The second is the edge of the pot body, especially the thinner or uneven edge of the pot. Because the edge part is relatively fragile, it may not provide enough friction to prevent sliding when clamping. The third is the bottom of the pot. If the bottom of the pot is uneven or has oil stains, water stains, etc., it is also easy to slide when clamping. Therefore, according to this situation, the first sliding area and the second sliding area are defined, and the bottom of the pot can also be defined as the third sliding area;

[0032] S3: using a positioning mechanism to clamp and fix both sides of the first sliding area and the second sliding area respectively, and fix one side of the deformation area at the same time, and the positioning mechanism also limits and fixes the third sliding area of ​​the pot bottom;

[0033] S4: Carry out edge turning, curling and pressing operations on the edge banding area.

[0034] At present, when the composite steel pot is undergoing the edge sealing process, in order to ensure the quality, it is necessary to ensure that the middle aluminum substrate is not exposed, and the mouth of the product does not have the risk of corrosion after its use. During this process, due to the work hardening and forming force of the composite steel pot itself, the product will change in shape, resulting in poor concentricity. At the same time, the fit between the product and the mold is poor, and the deformation of the product is inconsistent, resulting in poor fit between the composite steel pot and the mold. In order to solve the above problems, most of them currently use a clamping device to clamp the composite steel pot as a whole on the mold along the outer side of the composite steel pot, exposing the mouth of the composite steel pot, and then The composite steel pot is subjected to edge sealing processes such as curling and pressing, but the current composite steel pot edge sealing process still has some problems. For example, when a composite steel pot with a flat bottom is edge sealed, due to the irregular structure of the composite steel pot itself, the tools used will vibrate when edge sealing processes such as curling and pressing are performed. The vibration is transmitted to the composite steel pot, and the composite steel pot tends to vibrate. However, the clamping device will clamp the entire composite steel pot on the mold along the outer side of the composite steel pot. The vibration at this time will easily cause damage such as indentations and scratches on the outer surface of the composite steel pot, which will ultimately affect the quality of the composite steel pot.

[0035] In order to solve the above problems, in this embodiment, the pot body is divided into several areas according to the characteristics of the composite steel pot. First, the arc length L is used as the length to define the arc length L at the connection between the pot bottom part and the pot body part as the first sliding area; then, starting from the first sliding area, a deformation area with an arc length M as the length is defined along the direction of the pot body; then, starting from the deformation area, a second sliding area with an arc length S as the length is defined along the direction of the pot body; finally, the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area, and a positioning mechanism is used to clamp both sides of the first sliding area and the second sliding area respectively. The positioning mechanism also limits and fixes the third sliding area of ​​the pot bottom; finally, the edge sealing area is turned, curled and pressed to complete the edge sealing process, which solves the problem that the tools used in edge sealing processes such as curling and pressing will generate vibration, and the vibration is transmitted to the composite steel pot. The composite steel pot has a tendency to vibrate, but because the clamping device will clamp and fix the entire composite steel pot on the mold along the outer side of the composite steel pot, the vibration at this time will easily cause damages such as indentations and scratches on the outer surface of the composite steel pot, which will ultimately affect the quality of the composite steel pot.

[0036] In addition, in order to ensure that the composite steel pot is clamped and fixed with better stability, in one embodiment, the arc length L in step S2 is greater than the arc length S, because the bending conditions of the first sliding area and the second sliding area are different, and the first sliding area is more likely to slide than the second sliding area. Therefore, the positioning mechanism used is used to clamp and fix the two sides of the first sliding area and the second sliding area respectively. Since the first sliding area is an area with a larger arc angle, it is more likely to slide. Therefore, it is necessary to ensure that the arc length L in step S2 is greater than the arc length S. In addition,

[0037] The longer the arc length M is, the smaller the area where the composite steel pot may deform will be. However, the overall arc length of the composite steel pot is limited. Therefore, the specific length of the arc length M needs to be determined again based on the arc length L and arc length S, because first of all, it is necessary to ensure that the composite steel pot is firmly fixed and consider the area that may deform.

[0038] Furthermore, after the composite steel pot is clamped and fixed, the tools used will inevitably vibrate during the edge turning, curling and pressing operations, and part of the vibration force will be transmitted to the composite steel pot. The composite steel pot may still move slightly under this vibration force. Once it moves slightly, it will affect the concentricity of the composite steel pot. In order to avoid this problem, in one embodiment, when the two sides of the first sliding area and the second sliding area are clamped and fixed in step S3, the deformation of the product caused by forming is calibrated by the calibration mechanism 4. Through the design of the calibration mechanism 4, when the composite steel pot moves slightly, the calibration mechanism 4 can be used to adjust and reset the composite steel pot in time, thereby avoiding affecting the concentricity of the composite steel pot.

[0039] Furthermore, in order to ensure the accuracy of the composite steel pot sealing process, in one embodiment, the edge turning operation in S4 is to perform edge turning and grade edge turning on the product through the CNC turning tool 5 according to the CNC programming. The CNC turning tool 5 is used to perform edge turning and grade edge turning on the product according to the CNC programming system. The program on the CNC machine tool is used to improve the accuracy of the composite steel pot sealing process.

[0040] A composite steel mouth edge sealing structure includes a positioning mechanism, a calibration mechanism 4 connected to the positioning mechanism, and a crimping mechanism. The positioning mechanism is used to clamp and fix the composite steel pot. The composite steel pot is clamped and fixed by the positioning mechanism. The crimping mechanism is used to crimp and curl the pot mouth of the composite steel pot. The composite steel pot is first fixed and clamped by the positioning mechanism, and then the composite steel pot is positioned by the calibration mechanism 4 to ensure the accuracy of the positioning mechanism for the composite steel pot. Finally, the pot mouth is crimped by the crimping mechanism. The crimping mechanism includes a crimping machine, a crimping wheel 6 and a crimping wheel 7. The crimping wheel 6 and the crimping wheel 7 are both arranged on the crimping machine. The crimping machine drives the crimping wheel 6 and the crimping wheel 7 to move. Figure 2 In order to facilitate the observation of the positioning mechanism, a cross-sectional view of the positioning mechanism is drawn. The curling wheel 6 and the pressing wheel 7 are both arranged on an integrated curling and pressing machine. The integrated curling and pressing machine, the curling wheel 6 and the pressing wheel 7 are all commercially available machines. The curling wheel 6 and the pressing wheel 7 are simply drawn in the figure to facilitate the understanding of the positional relationship between the curling wheel 6 and the pressing wheel 7 and the pot mouth of the composite steel pot.

[0041] It is worth mentioning that the first sliding area, the second sliding area, the third sliding area and the deformation area need to be clamped by the positioning mechanism, and it is necessary to ensure that the composite steel pot is firmly clamped while avoiding damage such as indentations and scratches on the outer surface of the composite steel pot. In order to cope with this problem, the positioning mechanism needs to have a special design. In one embodiment, the positioning mechanism includes a support frame 8, an upper mold 1, a positioning member 2 and a lower mold 3. The upper mold 1, the positioning member 2 and the lower mold 3 are all arranged on the support frame 8, and the upper mold 1, the positioning member 2 and the lower mold 3 are arranged in sequence from top to bottom. The pot body of the composite steel pot is respectively connected to the upper mold 3 and the lower mold 3 through the lower mold 3. The mold 1 and the positioning member 2 are clamped with the upper mold 1. The part of the inner wall of the upper mold 1 that contacts the bottom of the pot is flat, so that the third sliding area can be fitted, and the bottom of the pot can be limited by the upper positioning member 2. The positioning member 2 and the upper mold 1 are used to limit and fix the first sliding area, and the lower mold 3 and the upper mold 1 are used to limit and fix the second sliding area. In addition, the two ends of the positioning member 2 are protruding outward and the middle is concave inward. This structure can not only enable the positioning member 2 and the upper mold 1 to limit and fix the first sliding area and the third sliding area, but also avoid indentations or deformation of the bottom of the pot at the third sliding area.

[0042] The upper mold 1 is connected to the support frame 8 through the upper cylinder connecting rod 9, and the upper cylinder connecting rod 9 is also connected to the numerical control programming system for communication, so as to better ensure the accuracy of the movement of the upper mold 1. The calibration mechanism 4 is arranged on the support frame 8, and the lower mold 3 is arranged on the calibration mechanism 4. The bottom part of the composite steel pot is detachably located on the positioning piece 2. In order to further avoid damage such as indentation and scratches on the composite steel pot when it is clamped, flexible gaskets are arranged at the positions where the upper mold 1, the positioning piece 2 and the lower mold 3 are in contact with the composite steel pot.

[0043] In addition, how the calibration mechanism 4 calibrates the fixed composite steel pot, in this regard, in one embodiment, the calibration mechanism 4 includes a calibration platform, two first hydraulic cylinders 10 and two second hydraulic cylinders 11 arranged on the support frame 8, the two ends of the two first hydraulic cylinders 10 are respectively connected to the lower mold 3 and the calibration platform, the two ends of the two second hydraulic cylinders 11 are respectively connected to the positioning member 2 and the calibration platform, the two first hydraulic cylinders 10 and the two second hydraulic cylinders 11 are both connected to the numerical control programming system for communication, and a leveling instrument for measuring the level of the composite steel pot mouth is arranged on the calibration platform After the composite steel pot is fixed and limited by the upper mold 1, the positioning piece 2 and the lower mold 3, the flatness of the composite steel pot mouth can be measured by a horizontal level meter, and the measured data is fed back to the control terminal of the numerical control programming system. Then, the control terminal in the numerical control programming system analyzes the feedback data and drives the two first hydraulic cylinders 10 and the two second hydraulic cylinders 11 to adjust their positions until the composite steel pot mouth is placed horizontally. In addition, during the edge sealing process of the composite steel pot mouth, as long as there is an uneven situation, this calibration mechanism 4 can automatically adjust the horizontal position of the composite steel pot mouth.

[0044] The working principle and use process of the present invention:

[0045] According to the characteristics of the composite steel pot, the pot body is divided into several areas. First, the arc length L is used as the length to define the arc length L at the connection between the pot bottom and the pot body as the first sliding area; then, starting from the first sliding area, a deformation area with an arc length M is defined along the direction of the pot body; starting from the deformation area, a second sliding area with an arc length S is defined along the direction of the pot body; finally, the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area, and a positioning mechanism is used to clamp and fix both sides of the first sliding area and the second sliding area respectively, and to fix one side of the deformation area at the same time. The positioning mechanism also limits and fixes the third sliding area of ​​the pot bottom; finally, the edge sealing area is machined, curled, and pressed to complete the edge sealing process.

[0046] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A composite steel mouth edge sealing process, characterized in that: The following steps are involved: S1: Divide the composite steel pot into a pot bottom part and a pot body part; S2: Divide the pot body into several areas. First, take the arc length L as the length, and define the arc length L at the connection between the pot bottom and the pot body as the first sliding area; then take the first sliding area as the starting point, Along the direction of the pot body, a deformation area with an arc length M is delineated; Then, starting from the deformation area, a second sliding area with an arc length S is defined along the direction of the pot body, and finally the remaining part from the second sliding area to the top of the pot body is defined as the edge sealing area; S3: using a positioning mechanism to clamp and fix both sides of the first sliding area and the second sliding area respectively, and fix one side of the deformation area at the same time; S4: Carry out edge turning, curling and pressing operations on the edge banding area.

2. A composite steel mouth edge sealing process according to claim 1, characterized in that: The arc length L in step S2 is greater than the arc length S.

3. A composite steel mouth edge sealing process according to claim 1, characterized in that: When the two sides of the first sliding area and the second sliding area are clamped and fixed in step S3, the deformation of the product caused by molding is calibrated by the calibration mechanism.

4. A composite steel mouth edge sealing process according to claim 1, characterized in that: The machining operation in S4 is to perform machining and level machining on the product by using a CNC turning tool according to CNC programming.

5. A composite steel mouth edge sealing structure, according to a composite steel mouth edge sealing process according to any one of claims 1 to 4, characterized in that: It includes a positioning mechanism, a calibration mechanism connected to the positioning mechanism, and a pressing and curling mechanism. The positioning mechanism is used to clamp and fix the composite steel pot. The composite steel pot is clamped and fixed by the positioning mechanism. The pressing and curling mechanism is used to press and curl the pot mouth of the composite steel pot.

6. A composite steel mouth edge sealing structure according to claim 5, characterized in that: The crimping mechanism comprises a crimping machine, a crimping wheel and a pressing wheel. The crimping wheel and the pressing wheel are both arranged on the crimping machine, and the crimping machine drives the crimping wheel and the pressing wheel to move.

7. The composite steel mouth edge sealing structure according to claim 5, characterized in that: The positioning mechanism includes a support frame, an upper mold, a positioning piece and a lower mold. The upper mold, the positioning piece and the lower mold are all arranged on the support frame, and the upper mold, the positioning piece and the lower mold are arranged in sequence from top to bottom. The pot body of the composite steel pot is clamped by the lower mold and the upper mold and the positioning piece and the upper mold respectively.

8. The composite steel mouth edge sealing structure according to claim 7, characterized in that: The upper die is connected to the support frame through an upper cylinder connecting rod, the calibration mechanism is arranged on the support frame, the lower die is arranged on the calibration mechanism, and the bottom part of the composite steel pot is detachably located on the positioning piece.

9. A composite steel mouth edge sealing structure according to claim 8, characterized in that: Flexible gaskets are arranged at the positions where the upper die, the positioning piece and the lower die contact with the composite steel pot.

10. The composite steel mouth edge sealing structure according to claim 8, characterized in that: The calibration mechanism includes a calibration platform, two first hydraulic cylinders and two second hydraulic cylinders arranged on a support frame, the two first hydraulic cylinders have two ends connected to the lower mold and the calibration platform respectively, and the two second hydraulic cylinders have two ends connected to the positioning member and the calibration platform respectively.