Method of manufacturing display device

Through inkjet printing technology, the protective layer with different peeling forces is formed and the acid-resistant film is used, which solves the problem of removing the protective film and the acid-resistant film during the etching of the substrate, improves the thinning and lightweighting and stability of the display device, and ensures the manufacturing process stability.

CN118900608APending Publication Date: 2024-11-05SAMSUNG DISPLAY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410388225.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-03
Filing Date
2024-04-01
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The prior art is difficult to prevent the protective film from being removed together with the acid-resistant film during the etching of the substrate, resulting in damage to the outer part of the substrate and foreign matter entering, affecting the thinning and stability of the display device.

Method used

Inkjet printing technology is used to form the first and second protective layers with different peeling forces, cure the resin material by ultraviolet light, and use an acid-resistant film and adhesive to protect the substrate during the etching process to ensure the smooth removal of the protective layer and the substrate. Safety.

Benefits of technology

It effectively prevents the protective layer from being removed together with the acid-resistant film, protects the substrate from damage, improves the thinning and stability of the display device, and ensures the stability of the manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900608A_ABST
    Figure CN118900608A_ABST
Patent Text Reader

Abstract

Disclosed is a method of manufacturing a display device, the method comprising the steps of: sequentially forming a display panel and an encapsulation layer on a first surface of a substrate; forming a first protection layer covering the packaging layer; forming a second protective layer covering the first protective layer; forming a first film on the first surface of the substrate; removing a second surface of the substrate facing the first surface; removing the first film and the second protective layer; and removing the first protective layer after the step of removing the first film and the second protective layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a method of manufacturing a display device. Background Art

[0002] As the information society develops, the demand for display devices for displaying images in various forms increases. For example, display devices are applied to various electronic devices such as smart phones, digital cameras, notebook computers, navigation devices, and smart TVs.

[0003] In addition, in order to enhance the portability of display devices, there is a trend toward thinner and lighter devices. Therefore, technology development for making display device components thinner and lighter is being actively carried out. Summary of the invention

[0004] Embodiments of the present disclosure may provide a method of manufacturing a display device which prevents a protective film disposed on a substrate from being removed together with the acid-resistant film in a process of stripping the acid-resistant film after etching the substrate.

[0005] Furthermore, the embodiments of the present disclosure may provide a method of manufacturing a display device that prevents foreign matter from entering an outer portion of a substrate and prevents the substrate from being damaged by scratches or the like.

[0006] An embodiment of a method for manufacturing a display device may include the following steps: sequentially forming a display panel and an encapsulation layer on a first surface of a substrate; forming a first protective layer covering the encapsulation layer; forming a second protective layer covering the first protective layer; forming a first film on the first surface of the substrate; removing the second surface of the substrate facing the first surface; removing the first film and the second protective layer; and after the steps of removing the first film and the second protective layer, removing the first protective layer.

[0007] In an embodiment, the step of forming the first protective layer may include: spraying a first resin material through a nozzle of an inkjet printing device; curing the first resin material with ultraviolet light; and supplying plasma to the first resin material.

[0008] In an embodiment, the step of forming the second protective layer may include: spraying the second resin material through a nozzle of an inkjet printing device; and curing the second resin material with ultraviolet light.

[0009] In an embodiment, the first protective layer may have a first peeling force, and the second protective layer may have a second peeling force different from the first peeling force. The first peeling force may be greater than the second peeling force.

[0010] In an embodiment, the first film may have a third peel force that is smaller than the second peel force.

[0011] In an embodiment, the first resin material and the second resin material may include the same UV-curable resin material, and in the step of curing the first resin material with UV light, the first resin material can be cured with UV light for a first time period, and in the step of curing the second resin material with UV light, the second resin material can be cured with UV light for a second time period shorter than the first time period.

[0012] In an embodiment, the first resin material and the second resin material may include an ultraviolet curable resin, the ultraviolet curable resin may include a plurality of monomers and oligomers, and the number of oligomers included in the first resin material may be greater than the number of oligomers included in the second resin material.

[0013] In an embodiment, the step of forming the second protective layer may further include supplying plasma to the second resin material.

[0014] In an embodiment, the ejection angle of the nozzle of the inkjet printing device may be about 45° to 135°.

[0015] In an embodiment, the steps of ejecting the first resin material and curing the first resin material with ultraviolet light may be performed simultaneously, and the steps of ejecting the second resin material and curing the second resin material with ultraviolet light may be performed simultaneously.

[0016] In an embodiment, in the step of removing the second surface of the substrate, the substrate may be etched using an etchant.

[0017] In an embodiment, the thickness of the substrate including the first surface and the second surface may be about 500 μm, and the thickness of the substrate from which the second surface is removed may be about 200 μm.

[0018] In an embodiment, the first film may be an acid-resistant film.

[0019] In an embodiment, the first film may include a PET (polyethylene terephthalate) film.

[0020] In an embodiment, the first protective layer may have a thickness of about 100 μm, and the second protective layer may have a thickness of about 10 μm to 30 μm.

[0021] In an embodiment, the method of manufacturing a display device may further include providing an adhesive layer covering the first surface of the substrate and the second protective layer, and in the step of forming the first film, the first film may be formed on the adhesive layer.

[0022] In an embodiment, the method of manufacturing a display device may further include removing the second protective layer, and the second protective layer may be removed simultaneously with the first film.

[0023] In an embodiment, the method of manufacturing a display device may further include: removing the first protective layer; and disposing a polarizing plate on the encapsulation layer, and the first protective layer may be removed before disposing the polarizing plate.

[0024] In an embodiment, the first surface of the substrate may include a display area and a peripheral area located at least one side of the display area, and at least a portion of the peripheral area may not be covered by the first protective layer.

[0025] In an embodiment, the second protection layer may completely cover the display area and the peripheral area. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The accompanying drawings, which are included to provide a further understanding of the inventive concept and are incorporated in and constitute a part of this specification, illustrate exemplary embodiments of the inventive concept and together with the description serve to explain the principles of the inventive concept.

[0027] Figure 1 is a plan view showing a mother substrate for a display substrate according to an embodiment of the present disclosure.

[0028] Figure 2A It is shown Figure 1 A plan view of an embodiment of a display substrate.

[0029] Figure 2B It is shown Figure 1 A plan view of another embodiment of a display substrate.

[0030] Figure 3 It is schematically shown Figure 2A and Figure 2B Circuit diagram of a pixel.

[0031] Figure 4 It is schematically shown that includes Figure 3 A cross-sectional view of a display substrate of a light-emitting element.

[0032] Figure 5A , Figure 5B , Fig. 6A , Figure 6B , Figure 7 , Fig. 8A , Figure 8B , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 and Fig.14 is a cross-sectional view schematically illustrating a method of manufacturing a display device according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0033] Hereinafter, preferred embodiments will be described in more detail with reference to the accompanying drawings. In the accompanying drawings, the same reference numerals are used for the same elements, and repeated description of the same elements is omitted.

[0034] Figure 1 is a plan view showing a mother substrate for a display substrate according to an embodiment.

[0035] Reference Figure 1 The base substrate 11 of the mother substrate 10 for the display substrate may include a plurality of array areas AA and an outer area SA between adjacent array areas AA. Each array area AA may include a display area DA for displaying an image and a peripheral area PA located at one side of the display area DA.

[0036] Each array area AA of the base substrate 11 may be formed into one display substrate DP by a cutting process of cutting the base substrate 11 into the unit array areas AA. In the base substrate 11, a cutting line extending in a first direction DR1 may be defined as a first cutting line CL1, and a cutting line extending in a second direction DR2 crossing the first direction DR1 may be defined as a second cutting line CL2. The first cutting line CL1 and the second cutting line CL2 may correspond to virtual lines for cutting the mother substrate 10 for the display substrate in the cutting process.

[0037] Alignment marks (not shown) may be formed in the outer area SA of the base substrate 11. The alignment marks may be used to monitor each layer stacked on the display substrate DP. The alignment marks may be formed one by one per unit in the outer area SA of the base substrate 11, but the alignment marks are not limited thereto. The number of alignment marks may be appropriately changed according to the size of the base substrate 11 and the size and number of the units to be formed.

[0038] Figure 2A It is shown Figure 1 A plan view of an embodiment of a display substrate. Figure 2B It is shown Figure 1 A plan view of another embodiment of a display substrate.

[0039] Reference Figure 1 , Figure 2A and Figure 2B , the display substrate DP may be one region of the base substrate 11 corresponding to each array area AA.

[0040] Reference Figure 2A and Figure 2B, the display device DD may include a display substrate DP. The display substrate DP may be provided in various shapes. As an example, the display substrate DP may be provided in the shape of a rectangular plate having two pairs of sides parallel to each other, but the display substrate DP is not limited thereto. When the display substrate DP is provided in the shape of a rectangular plate, one of the two pairs of sides may be provided to be longer than the other pair of sides.

[0041] The display substrate DP may have various shapes. As an example, the display substrate DP may be provided in a rectangular shape, but the display substrate DP is not limited thereto. For example, the display substrate DP may have a circular shape or an elliptical shape. In addition, the display substrate DP may include angled corners or curved corners. For ease of description, Figure 2A and Figure 2B An embodiment is shown in which the display substrate DP has a rectangular plate shape. Figure 2A and Figure 2B , a direction along which the short sides of the display substrate DP extend (eg, a horizontal direction) is represented as a first direction DR1, and a direction along which the long sides extend (eg, a vertical direction) is represented as a second direction DR2.

[0042] The display substrate DP may include a display panel (eg, Figure 4 In one example, as the display panel, a display panel capable of self-luminescence (such as an organic light-emitting display panel (OLED panel) using an organic light-emitting diode as a light-emitting element, a micro-LED (or nano-LED) panel using a micro-light-emitting diode as a light-emitting element, and a quantum dot organic light-emitting display panel (QD OLED panel) using quantum dots and organic light-emitting diodes) can be used. In addition, as the display panel, a non-luminous display panel (such as a liquid crystal display panel (LCD panel), an electrophoretic display panel (EPD panel), and an electrowetting display panel (EWD panel)) can be used. Hereinafter, a case in which the display substrate DP includes an organic light-emitting display panel will be described as an example.

[0043] The display substrate DP may include a substrate SUB and a plurality of pixels PX disposed on the substrate SUB.

[0044] The substrate SUB may include a transparent insulating material to transmit light. The substrate SUB may be a rigid substrate or a flexible substrate.

[0045] The rigid substrate may be, for example, one of a glass substrate, a quartz substrate, a glass ceramic substrate, and a crystallized glass substrate.

[0046] The flexible substrate may be one of a film substrate and a plastic substrate including a polymer organic material. For example, the flexible substrate may include at least one of polystyrene, polyvinyl alcohol, polymethyl methacrylate, polyether sulfone, polyacrylate, polyetherimide, polyethylene naphthalate, polyethylene terephthalate, polyphenylene sulfide, polyarylate, polyimide, polycarbonate, cellulose triacetate, and cellulose acetate propionate.

[0047] The display substrate DP may include a display area DA and a peripheral area PA. The display area DA may be an area in which a plurality of pixels PX are formed to display an image. Each pixel PX may include a pixel circuit connected to a plurality of signal lines and an organic light emitting element whose light emission is controlled by the pixel circuit. The peripheral area PA may be an area other than the display area DA, and may be a non-display area. The peripheral area PA may have a structure for protecting components included in the pixels PX disposed in the display area DA, but the peripheral area PA is not limited thereto. For example, a wiring unit connected to each pixel PX and a driving unit connected to the wiring unit to drive the pixel PX may be disposed in the peripheral area PA.

[0048] Reference Figure 2A , the peripheral area PA may surround the periphery (or edge) of the display area DA. Figure 2B , the peripheral area PA may be disposed on at least one side of the display area DA.

[0049] Reference Figure 2B When the display substrate DP is applied to a rollable display device, the display substrate DP may include a flexible material that can be easily bent, folded, or rolled. In this case, at least one of the display area DA and the peripheral area PA may include a bending area.

[0050] Figure 3 It is schematically shown Figure 2A and Figure 2B Circuit diagram of a pixel.

[0051] exist Figure 3 In the figure, for the convenience of description, the pixel PX located in the j-th pixel column of the i-th pixel row (or the i-th horizontal line) is shown as an example, where i and j may be positive integers.

[0052] Reference Figure 3 The pixel PX may include an emission unit EMU that generates light having brightness corresponding to the data signal. In addition, the pixel PX may further include a pixel circuit PXC for driving the emission unit EMU.

[0053] The emission unit EMU may include a light emitting element LD connected between a first power line PL1 receiving a voltage of a first driving power source VDD (or a first power source) and a second power line PL2 receiving a voltage of a second driving power source VSS (or a second power source). As an example, the emission unit EMU may include a light emitting element LD including a first electrode AE ​​connected to the first driving power source VDD via the first power line PL1 and the pixel circuit PXC and a second electrode CE connected to the second driving power source VSS via the second power line PL2. The first electrode AE ​​may be an anode, and the second electrode CE may be a cathode. The first driving power source VDD and the second driving power source VSS may have different potentials. In this case, during the emission period of the pixel PX, the potential difference between the first driving power source VDD and the second driving power source VSS may be set to be higher than or equal to the threshold voltage of the light emitting element LD.

[0054] When the pixel PX is located in the i-th pixel row and the j-th pixel column in the display area DA, the pixel circuit PXC of the pixel PX (or sub-pixel) can be electrically connected to the i-th scan line Si and the j-th data line Dj. In addition, the pixel circuit PXC can be electrically connected to the i-th control line CLi and the j-th sensing line SENj.

[0055] The pixel circuit PXC may include first, second and third transistors T1, T2 and T3 and a storage capacitor Cst.

[0056] The first transistor T1 may be a driving transistor for controlling a driving current applied to the light emitting element LD, and may be electrically connected between the first driving power source VDD and the light emitting element LD. Specifically, the first terminal of the first transistor T1 may be electrically connected to the first driving power source VDD through the first power line PL1, the second terminal of the first transistor T1 may be electrically connected to the second node N2, and the gate electrode of the first transistor T1 may be electrically connected to the first node N1. The first transistor T1 may control the amount of driving current applied to the light emitting element LD from the first driving power source VDD through the second node N2 according to the voltage applied to the first node N1. In an embodiment, the first terminal of the first transistor T1 may be a drain electrode, and the second terminal of the first transistor T1 may be a source electrode, but the first transistor T1 is not limited thereto. According to an embodiment, the first terminal may be a source electrode, and the second terminal may be a drain electrode.

[0057] The second transistor T2 may be a switching transistor that selects the pixel PX in response to the scan signal and activates the pixel PX, and may be electrically connected between the data line (e.g., the jth data line) Dj and the first node N1. The first terminal of the second transistor T2 may be electrically connected to the data line Dj, the second terminal of the second transistor T2 may be electrically connected to the first node N1 (or the gate electrode of the first transistor T1), and the gate electrode of the second transistor T2 may be electrically connected to the scan line (or the i-th scan line) Si. The first terminal and the second terminal of the second transistor T2 may be different terminals. For example, when the first terminal is a drain electrode, the second terminal may be a source electrode.

[0058] The second transistor T2 may be turned on to electrically connect the data line Dj to the first node N1 when a scan signal having a gate-on voltage (e.g., a high-level voltage) is supplied from the scan line Si. The first node N1 may be a point at which the second terminal of the second transistor T2 is connected to the gate electrode of the first transistor T1, and the second transistor T2 may transmit a data signal to the gate electrode of the first transistor T1.

[0059] The third transistor T3 can obtain a sensing signal through the sensing line SENj by electrically connecting the first transistor T1 to the sensing line (e.g., the jth sensing line) SENj, and can detect the characteristics of the pixel PX (such as the threshold voltage of the first transistor T1) by using the sensing signal. Information about the characteristics of the pixel PX can be used to convert image data so that the characteristic deviation between the pixels PX can be compensated. The second terminal of the third transistor T3 can be electrically connected to the second terminal of the first transistor T1, the first terminal of the third transistor T3 can be electrically connected to the sensing line SENj, and the gate electrode of the third transistor T3 can be electrically connected to the control line (e.g., the i-th control line) CLi. The first terminal can be a drain electrode, and the second terminal can be a source electrode.

[0060] The third transistor T3 may be an initialization transistor capable of initializing the second node N2 and may be turned on when a sensing control signal is supplied from the control line CLi to transfer a voltage of an initialization power source to the second node N2. Thus, the storage capacitor Cst electrically connected to the second node N2 may be initialized.

[0061] The storage capacitor Cst may include a lower electrode (or first storage electrode) LE and an upper electrode (or second storage electrode) UE. The lower electrode LE may be electrically connected to the first node N1, and the upper electrode UE may be electrically connected to the second node N2. The storage capacitor Cst may be charged with a data voltage corresponding to a data signal supplied to the first node N1 during one frame period. Therefore, the storage capacitor Cst may store a voltage corresponding to a difference between a voltage of the gate electrode of the first transistor T1 and a voltage of the second node N2.

[0062] Figure 3 An embodiment in which all transistors of the first transistor T1 to the third transistor T3 are N-type transistors is shown, but the first transistor T1 to the third transistor T3 are not limited thereto. For example, at least one of the first transistor T1, the second transistor T2, and the third transistor T3 may be changed to a P-type transistor. The structure of the pixel circuit PXC may be variously changed and implemented.

[0063] Figure 4 It is schematically shown that includes Figure 3 A cross-sectional view of a display substrate of a light-emitting element.

[0064] The display substrate DP (or the display device) may include a substrate SUB, a display panel PNL disposed on the substrate SUB, and an encapsulation layer TFE.

[0065] The substrate SUB may be a base substrate (eg, Figure 1 A base substrate 11) is a substrate disposed in a display device after undergoing chemical / physical treatment.

[0066] The display panel PNL may include a pixel circuit layer PCL and a display element layer DPL.

[0067] The pixel circuit layer PCL may be disposed on a substrate SUB and may include a plurality of transistors and signal lines connected to the transistors. For example, each transistor may have a form in which a semiconductor pattern, a gate electrode, a source electrode, and a drain electrode are sequentially stacked and an insulating layer is placed therebetween. The semiconductor pattern may include amorphous silicon, polycrystalline silicon, low-temperature polycrystalline silicon, an organic semiconductor, or an oxide semiconductor. The gate electrode, the source electrode, and the drain electrode may include one of aluminum (Al), copper (Cu), titanium (Ti), and molybdenum (Mo), but they are not limited thereto. In addition, the pixel circuit layer PCL may include one or more insulating layers.

[0068] The display element layer DPL may be disposed on the pixel circuit layer PCL. The display element layer DPL may include a light emitting element that emits light. The light emitting element may be, for example, an organic light emitting diode, but the light emitting element is not limited thereto. According to an embodiment, the light emitting element may be an inorganic light emitting device including an inorganic light emitting material or a light emitting element that emits light by changing the wavelength of the emitted light using quantum dots. In this specification, for ease of description, an embodiment in which the light emitting element LD is an organic light emitting diode (OLED) will be described as an example.

[0069] The encapsulation layer TFE may be disposed on the display element layer DPL. The encapsulation layer TFE may be an encapsulation substrate or may have the form of an encapsulation film made of a multilayer film. When the encapsulation layer TFE has the form of an encapsulation film, the encapsulation layer TFE may include an inorganic film or an organic film. For example, the encapsulation layer TFE may have a form in which an inorganic film, an organic film, and an inorganic film are sequentially stacked. The encapsulation layer TFE may prevent air and moisture from penetrating into the display element layer DPL and the pixel circuit layer PCL from the outside.

[0070] The light emitting element LD may be disposed on the pixel circuit layer PCL. According to an embodiment, the light emitting element LD may include a first electrode AE, a light emitting layer EML, and a second electrode CE. According to an embodiment, the light emitting layer EML may be disposed in a region defined by the pixel defining layer PDL. One surface of the light emitting layer EML may be electrically connected to the first electrode AE, and the other surface of the light emitting layer EML may be electrically connected to the second electrode CE.

[0071] The first electrode AE ​​may be an anode electrode for the light emitting layer EML, and the second electrode CE may be a common electrode (or cathode electrode) for the light emitting layer EML. According to an embodiment, the first electrode AE ​​and the second electrode CE may include a conductive material. For example, the first electrode AE ​​may include a conductive material having a reflective property, and the second electrode CE may include a transparent conductive material, but the disclosure is not necessarily limited thereto.

[0072] The light emitting layer EML may have a multilayer thin film structure including a light generating layer. The light emitting layer EML may include a hole injection layer for injecting holes, a hole transport layer having excellent hole transport properties and suppressing the movement of electrons that are not recombined in the light generating layer to increase the chance of recombination between holes and electrons, a light generating layer that emits light by recombination of injected electrons and holes, a hole blocking layer for suppressing the movement of holes that are not recombined in the light generating layer, an electron transport layer for smoothly transporting electrons to the light generating layer, and an electron injection layer for injecting electrons. The light emitting layer EML may emit light based on an electrical signal provided from the first electrode AE ​​and the second electrode CE.

[0073] The pixel defining layer PDL may be disposed on the pixel circuit layer PCL to define a position where the light emitting layer EML is disposed. The pixel defining layer PDL may include an organic material. According to an embodiment, the pixel defining layer PDL may include at least one selected from the group consisting of acrylic resin, epoxy resin, phenolic resin, polyamide resin, and polyimide resin. However, the disclosure is not limited thereto.

[0074] The encapsulation layer TFE may be disposed on the light emitting element LD (e.g., the second electrode CE). The encapsulation layer TFE may offset the step difference generated by the light emitting element LD and the pixel defining layer PDL. The encapsulation layer TFE may include a plurality of insulating films covering the light emitting element LD. A polarizing film (or color filter) (not shown) may be further disposed on the encapsulation layer TFE.

[0075] FIG. 5A to FIG. 14 is a cross-sectional view schematically illustrating a method of manufacturing a display device according to an embodiment.

[0076] Will refer to FIG. 5A to FIG. 14 Description can be used for the mother substrate MSUB for display substrate to manufacture display device (or display substrate). However, for ease of description, will focus on the base substrate SUB for the mother substrate MSUB for display substrate a unit (eg, a display substrate DP) on the base substrate to describe the method of manufacturing the display device.

[0077] Reference FIG. 5A to FIG. 14 The method for manufacturing a display device may include: sequentially forming a display panel PNL and an encapsulation layer TFE on a substrate MSUB (refer to Figure 5A and Figure 5B ); forming a first protective layer RF1 on the encapsulation layer TFE and the first protective layer RF1 covers the encapsulation layer TFE (refer to FIG. 6A to FIG. 7 ); forming a second protective layer RF2 on the first protective layer RF1 and the second protective layer RF2 covers the first protective layer RF1 (refer to FIG. 8A to FIG. 10 ); forming a first film ARF on the first surface SF1 of the substrate MSUB (refer to Fig.11 ); remove the second surface SF2 of the substrate MSUB (refer to Fig.12 ); and removing the first film ARF after removing the second surface SF2 of the substrate MSUB (reference Fig.13 ). In addition, the method for manufacturing a display device may further include removing the first protective layer RF1 (refer to Fig.14 ).

[0078] like Figure 5A and Figure 5B As shown in FIG. 1 , the display panel PNL and the encapsulation layer TFE may be sequentially formed on the first surface SF1 of the substrate MSUB (or mother substrate) in the third direction DR3 .

[0079] The substrate MSUB may be a mother substrate (e.g., Figure 1 The substrate MSUB may include a first surface SF1 and a second surface SF2 facing the first surface SF1.

[0080] In an embodiment, the first surface SF1 of the substrate MSUB may be a layer on which the display panel PNL and the encapsulation layer TFE are formed. The second surface SF2 of the substrate MSUB may include one surface of the substrate MSUB polished (etched) by a thinning process.

[0081] Reference Figure 5A , the display panel PNL and the encapsulation layer TFE may be disposed in the display area DA and the peripheral area PA. Some components of the encapsulation layer TFE and the display panel PNL disposed in the display area DA may extend to and be disposed in the peripheral area PA. Figure 5B , the encapsulation layer TFE may be disposed only on the display panel PNL disposed in the display area DA. The display panel PNL disposed in the peripheral area PA may be exposed to the outside.

[0082] Reference Fig. 6A and Figure 6B , a first protection layer RF1 covering the encapsulation layer TFE may be formed on the encapsulation layer TFE.

[0083] In an embodiment, the first protection layer RF1 may be formed by an inkjet printing method by spraying the first resin material R1 on the encapsulation layer TFE and curing the first resin material R1 with ultraviolet (or ultraviolet) (UV) light.

[0084] The first resin material R1 may be discharged onto the encapsulation layer TFE through the nozzle 201 of the inkjet printing device 200. The first resin material R1 may be cured or dried by irradiating the first resin material R1 discharged onto the encapsulation layer TFE with UV light using the UV lamp 300.

[0085] In an embodiment, the ejection angle of the nozzle 201 of the inkjet printing device 200 may be about 45° to about 135°.

[0086] The thickness of the first protection layer RF1 may be about 100 μm, but the thickness is not limited thereto.

[0087] The process of spraying the first resin material R1 on the encapsulation layer TFE and the process of curing the first resin material R1 with UV light may be performed simultaneously. Alternatively, the process of curing the first resin material R1 with UV light may be performed after the process of spraying the first resin material R1 on the encapsulation layer TFE is completed.

[0088] The first protective layer RF1 may have a first peeling force. The first peeling force of the first protective layer RF1 may be a physical property value indicating an amount of force required when the first protective layer RF1 is peeled from the adhesive.

[0089] The peeling force may vary depending on the type of resin material and the degree of curing of the resin material. The degree of curing by irradiation of UV light may vary depending on the number of monomers constituting the resin material. For example, the more the number of monomers constituting the resin material, the higher the peeling force. In addition, the higher the degree of curing of the resin material, the higher the peeling force.

[0090] That is, the first peeling force of the first protection layer RF1 may vary according to the type of the first resin material R1, the curing degree of the first resin material R1, or a combination thereof.

[0091] Fig. 6A A case is shown in which the first protection layer RF1 completely covers the display panel PNL and the encapsulation layer TFE.

[0092] Figure 6B 1 shows a state in which the first protective layer RF1 completely covers the encapsulation layer TFE and the display panel PNL disposed in the display area DA, but the display panel PNL disposed in the peripheral area PA is exposed. In this case, foreign matter may be introduced through the display panel PNL exposed to the peripheral area PA, and the display panel PNL may be damaged due to scratches.

[0093] Reference Figure 7 , plasma can be supplied to the first protective layer RF1. The thin film properties of the first protective layer RF1 can be improved by exposing the first protective layer RF1 to plasma using a plasma treatment device 400. Through plasma surface treatment, the adhesion between the first protective layer RF1 and the encapsulation layer TFE (and the second protective layer RF2 to be described later) can be improved. In one example, the surface properties of the first protective layer RF1 can be changed by plasma surface treatment. For example, through plasma surface treatment, the contact angle of the first protective layer RF1 can be about 10° to about 15°.

[0094] Reference Fig. 8A and Figure 8B , a second protection layer RF2 covering the first protection layer RF1 may be formed on the first protection layer RF1.

[0095] In an embodiment, the second protective layer RF2 may be disposed on the entire surface of the display substrate DP. In one example, the second protective layer RF2 may be disposed on the entire surface of the display area DA and the peripheral area PA. In one example, the second protective layer RF2 may be disposed on the entire surface of the base substrate (eg, Figure 1 The second protective layer RF2 is disposed on the entire surface of the base substrate 11. The second protective layer RF2 may be formed to cover the array region of the base substrate 11 (eg, Figure 1 array area AA) and the outer area (e.g., Figure 1In another example, the second protective layer RF2 may be formed on each display substrate DP of the base substrate 11.

[0096] In an embodiment, the second protection layer RF2 may be formed by spraying the second resin material R2 on the first protection layer RF1 through an inkjet printing method and curing the second resin material R2 with UV light.

[0097] The second resin material R2 may be discharged onto the first protective layer RF1 through the nozzle 202 of the inkjet printing device 200. The second resin material R2 may be cured or dried by irradiating the second resin material R2 discharged onto the first protective layer RF1 with UV light using the UV lamp 300. In one example, the second resin material R2 may be exposed to UV light for a second period of time.

[0098] The second protection layer RF2 may include a UV curable resin material that may be cured by a chemical reaction when exposed to UV light.

[0099] In an embodiment, the ejection angle of the nozzle 202 of the inkjet printing device 200 may be about 45° to about 135°.

[0100] The second protective layer RF2 may have a thickness of about 10 μm to about 30 μm, but the thickness is not limited thereto.

[0101] The process of spraying the second resin material R2 on the first protective layer RF1 and the process of curing the second resin material R2 with UV light may be performed simultaneously. Alternatively, the process of curing the second resin material R2 with UV light may be performed after the process of spraying the second resin material R2 on the first protective layer RF1 is completed.

[0102] The second protective layer RF2 may have a second peeling force that is different from the first peeling force of the first protective layer RF1. That is, the second peeling force of the second protective layer RF2 may be a physical property value indicating the amount of force required when the second protective layer RF2 is peeled off from the adhesive. In one example, the second peeling force may be less than the first peeling force. In this case, since the first peeling force of the first protective layer RF1 is greater than the second peeling force of the second protective layer RF2, the amount of force required to peel the first protective layer RF1 from the adhesive may be greater than the amount of force required to peel the second protective layer RF2 from the adhesive.

[0103] In an embodiment, the first protection layer RF1 and the second protection layer RF2 may include a UV curable resin material. In one example, the UV curable resin material may include a compound that may be cured by UV light.

[0104] Reference Fig. 6A , Figure 6B, Fig. 8A and Figure 8B , the first protection layer RF1 and the second protection layer RF2 may include the same UV curable resin material.

[0105] In an embodiment, the first protective layer RF1 may have a first peeling force, and the second protective layer RF2 may have a second peeling force different from the first peeling force.

[0106] The first resin material R1 constituting the first protective layer RF1 may be exposed to UV light for a first period of time, and the second resin material R2 constituting the second protective layer RF2 may be exposed to UV light for a second period of time shorter than the first period of time. Since the first resin material R1 is exposed to UV light for a longer period of time than the second resin material R2, the degree of curing may be greater. In this case, the first peeling force of the first protective layer RF1 may be greater than the second peeling force of the second protective layer RF2.

[0107] Reference Fig. 6A , Figure 6B , Fig. 8A and Figure 8B , the first protection layer RF1 and the second protection layer RF2 may include different UV curable resin materials.

[0108] The UV curable resin material may include a monomer, an oligomer, or a combination thereof. The first protective layer RF1 may have a weight average molecular weight higher than that of the second protective layer RF2. For example, the first protective layer RF1 may include more oligomers than the second protective layer RF2. The smaller the weight average molecular weight, the lower the density after UV curing, and thus the peeling force may be reduced. Therefore, since the weight average molecular weight of the first protective layer RF1 is greater than the weight average molecular weight of the second protective layer RF2, the peeling force of the first protective layer RF1 may be greater than the peeling force of the second protective layer RF2.

[0109] Reference Figure 8B , the second protective layer RF2 may completely cover the first protective layer RF1 and the display panel PNL. In one example, the second protective layer RF2 may completely cover the display panel PNL and the first protective layer RF1 disposed in the peripheral area PA. Therefore, the second protective layer RF2 may prevent foreign matter from entering through the display panel PNL exposed to the peripheral area PA, and prevent the display panel PNL from being damaged by external force.

[0110] Reference Fig. 9 , plasma may be supplied to the second protective layer RF2. The plasma processing apparatus 400 may be used to improve the film characteristics of the second protective layer RF2 by exposing the second protective layer RF2 to plasma.

[0111] Reference Fig.10, heat may be supplied to the second protective layer RF2. The second protective layer RF2 may be cured by exposing the second protective layer RF2 to heat using the heating device 500.

[0112] Reference Fig. 9 and Fig.10 In the range where the second protective layer RF2 has a second peeling force smaller than the first peeling force of the first protective layer RF1, the surface of the second protective layer RF2 may be optionally subjected to plasma treatment, heat treatment, or a combination thereof. Fig. 9 The plasma treatment process shown in Fig.10 The heat treatment process shown in .

[0113] In an embodiment, the first protection layer RF1 and the second protection layer RF2 may protect the encapsulation layer TFE and the display panel PNL.

[0114] Reference Fig.11 , the first film ARF may be formed on the first surface SF1 of the substrate MSUB. The first film ARF may be completely coated on the first surface SF1 of the substrate MSUB.

[0115] In an embodiment, the first film ARF may be provided on the entire surface of the substrate MSUB by an adhesive ADL. The adhesive ADL may be formed to completely cover the first surface SF1 of the substrate MSUB. In one example, the adhesive ADL may be formed on the second protective layer RF2 to completely surround the second protective layer RF2. The adhesive ADL may include at least one of an optically clear adhesive (OCA), a pressure sensitive adhesive (PSA), a heat reactive adhesive, a general adhesive, and a double-sided tape.

[0116] In an embodiment, the first film ARF may be formed directly on the adhesive ADL. In one example, the first film ARF may completely cover the first surface SF1 of the substrate MSUB.

[0117] In an embodiment, the first film ARF may include an acid-resistant film. The first film ARF may be formed of an acid-resistant material that does not react with an etchant described later. That is, the first film ARF may prevent the etchant from contacting the first surface SF1 of the substrate MSUB. That is, the first film ARF may prevent the etchant from contacting the first protective layer RF1 and the second protective layer RF2 disposed on the first surface SF1 and the display element (e.g., the encapsulation layer TFE and the display panel PNL). In one example, the first film ARF may include a polyethylene terephthalate (PET) film.

[0118] In an embodiment, the first film ARF may have a third peeling force. The third peeling force may be smaller than the second peeling force of the second protective layer RF2. That is, the force used to peel off the first film ARF may be smaller than the force used to peel off the second protective layer RF2.

[0119] Reference Fig.12 , the second surface SF2 of the substrate MSUB can be removed. In a state where the first film ARF is attached to the first surface SF1 of the substrate MSUB, a thinning process can be performed on the substrate MSUB by a physical / chemical process such as etching. The thinning process may include a wet etching process using an etchant. The etchant may include hydrofluoric acid or a hydrofluoric acid-based material. For example, the wet etching process may include an immersion method, a spray method, or a top-down glass etching method. The immersion method may be a method of vertically immersing the substrate MSUB in a bath and etching the substrate MSUB. The spray method may be a method of etching the second surface SF2 of the substrate MSUB by spraying the etchant to one side of the vertically placed substrate MSUB at a predetermined spray pressure using multiple spray nozzles. The top-down glass etching method may be a method of etching the second surface SF2 of the substrate MSUB by causing the etchant to flow downward from the upper side of the vertically placed substrate MSUB.

[0120] Reference Figure 5A , Figure 5B and Fig.12 , the second surface SF2 of the substrate MSUB may be removed by a thinning process. The substrate SUB may include a substrate from which the second surface SF2 of the substrate MSUB is removed. The thickness H of the substrate MSUB may be reduced to a thickness H' of the substrate SUB. For example, the thickness H of the substrate MSUB may be about 500 μm, and the thickness H' of the substrate SUB according to the thinning process may be about 200 μm.

[0121] Reference Fig.13 , after completing the thinning process, the second protection layer RF2 and the first film ARF may be removed.

[0122] In an embodiment, the second protective layer RF2 and the first film ARF may be removed simultaneously. Since the second protective layer RF2 is formed between the first film ARF and the first protective layer RF1, the first film ARF may be removed together with the second protective layer RF2 in the process of removing the first film ARF. Therefore, the first protective layer RF1 may be prevented from being removed together with the first film ARF. That is, in the process of removing the first film ARF, the function of the first protective layer RF1 may be maintained so that the encapsulation layer TFE and the display panel PNL may be protected.

[0123] Reference Figure 5A and Fig.13The substrate SUB may include a first surface SF1 and a second surface SF2'. In an example, a thickness between the first surface SF1 and the second surface SF2' of the substrate SUB may be smaller than a thickness between the first surface SF1 and the second surface SF2 of the substrate MSUB.

[0124] The first protective layer RF1 may protect the encapsulation layer TFE and the display panel PNL on the substrate SUB from the manufacturing process performed after the first film ARF is removed. In one example, after the process of removing the first film ARF, a process of washing and drying the substrate SUB may be performed to remove the remaining etchant. In addition, after the process of removing the first film ARF, the base substrate (e.g., Figure 1 The process of forming one display substrate DP is performed by a cutting process of the base substrate 11).

[0125] Reference Fig.14 , the first protective layer RF1 may be removed before the module process of the display substrate DP may be performed. After removing the first protective layer RF1, a polarizer POL may be formed on the encapsulation layer TFE. In one example, the polarizer POL may include a polarizing film. In another example, the display substrate DP may include a color filter (not shown) instead of the polarizer POL. The color filter may have the same or similar function as the polarizer POL. In an embodiment, a window layer (not shown) may be additionally provided on the polarizer POL.

[0126] According to the method of manufacturing the display device according to the embodiment, a second protective layer RF2 having a peeling force different from that of the first protective layer RF1 may be provided between the first protective layer RF1 provided on the display element (e.g., the encapsulation layer TFE and the display panel PNL) of the display device and the acid-resistant film (e.g., the first film ARF) provided on the entire surface of the substrate SUB. Therefore, the first protective layer RF1 can be prevented from being removed together with the acid-resistant film in the process of peeling the acid-resistant film.

[0127] In addition, since the second protection layer RF2 covers the outer region (eg, the peripheral area PA) of the display device, damage to the outer region of the display device may be prevented during a manufacturing process of the display device.

[0128] In a process of manufacturing a display device, stability of the process of manufacturing the display device can be ensured by ensuring durability of a film for protecting a display element in a process of etching a substrate.

[0129] Although the embodiments of the inventive concept have been described, various modifications and similar arrangements of these embodiments will be apparent to those skilled in the art. Therefore, the inventive concept is not limited to these embodiments, but is limited to the scope and spirit of the appended claims.

Claims

1. A method for manufacturing a display device, the method comprising: The following steps are involved: sequentially forming a display panel and an encapsulation layer on a first surface of the substrate; forming a first protective layer covering the encapsulation layer; forming a second protective layer covering the first protective layer; forming a first film on the first surface of the substrate; removing a second surface of the substrate facing the first surface; removing the first film and the second protective layer; as well as After the steps of removing the first film and the second protective layer, the first protective layer is removed.

2. The method according to claim 1, in, The step of forming the first protective layer comprises: ejecting a first resin material through a nozzle of an inkjet printing device; curing the first resin material with ultraviolet light; and supplying plasma to the first resin material, and The step of forming the second protective layer includes: ejecting a second resin material through the nozzles of the inkjet printing device; and The second resin material is cured by using the ultraviolet light.

3. The method according to claim 2, in, The first protective layer has a first peeling force, and the second protective layer has a second peeling force different from the first peeling force, wherein the first peeling force is greater than the second peeling force, and The first film has a third peeling force that is smaller than the second peeling force.

4. The method according to claim 3, in, The first resin material and the second resin material include the same ultraviolet curable resin material, wherein, in the step of curing the first resin material with the ultraviolet light, the first resin material is cured with the ultraviolet light for a first period of time, and Wherein, in the step of curing the second resin material with the ultraviolet light, the second resin material is cured with the ultraviolet light for a second time period that is shorter than the first time period.

5. The method according to claim 3, in, The first resin material and the second resin material include ultraviolet curable resins, Wherein, the UV curable resin comprises a plurality of monomers and oligomers, and The amount of the oligomers included in the first resin material is greater than the amount of the oligomers included in the second resin material.

6. The method according to claim 2, in, The step of forming the second protective layer further includes: supplying plasma to the second resin material, Wherein, the spraying angle of the nozzle of the inkjet printing device is 45° to 135°, wherein the step of spraying the first resin material and the step of curing the first resin material with the ultraviolet light are performed simultaneously, and The step of spraying the second resin material and the step of curing the second resin material with the ultraviolet light are performed simultaneously.

7. The method according to claim 1, in, In the step of removing the second surface of the substrate, the substrate is etched using an etchant.

8. The method according to claim 1, in, The first film is an acid-resistant film, and Wherein, the second protective layer and the first film are removed simultaneously.

9. The method according to claim 8, in, The first film comprises a polyethylene terephthalate film, Wherein, the thickness of the first protective layer is 100 μm, and Wherein, the thickness of the second protective layer is 10 μm to 30 μm.

10. The method according to claim 1, in, The first surface of the substrate includes a display area and a peripheral area located on at least one side of the display area, wherein at least a portion of the peripheral area is not covered by the first protective layer, and Wherein, the second protective layer completely covers the display area and the peripheral area.