Composite material structural member and electronic device

By using a combined structure of substrate, transition layer and appearance layer in electronic equipment components, the problem of structural strength and lightness is solved, impact resistance and aesthetics are improved, and processing costs and complexity are reduced.

CN118906567AActive Publication Date: 2024-11-08HONOR DEVICE CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202410856629.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-11-08
Estimated Expiration
2044-06-27

AI Technical Summary

Technical Problem

It is difficult for existing electronic equipment components to take into account the requirements of structural strength and lightness, resulting in poor protection effect during drop or collision, and the appearance layer is difficult to adhere to the substrate, resulting in uneven color and poor aesthetics.

Method used

Composite material structural parts are adopted, including substrate, transition layer and appearance layer. The substrate is composed of multi-layer fiber cloth and resin matrix. The transition layer covers the surface of the substrate through fillers and resin matrix. The appearance is laminated on the transition layer, and the color of the transition layer is relatively large. Lightly cover the color of the substrate to improve the flatness and aesthetics of the appearance layer.

Benefits of technology

The structural strength and impact resistance of composite structural parts are improved, uneven problems caused by the contact between the appearance layer and the substrate are avoided, aesthetics and user experience are enhanced, and processing costs and complexity are reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118906567A_ABST
    Figure CN118906567A_ABST
Patent Text Reader

Abstract

The invention discloses a composite material structural part and electronic equipment, relates to the technical field of electronic equipment, and aims to solve the problem that parts are difficult to meet the requirements of structural strength and lightness and thinness at the same time. The composite material structural part comprises a base plate, a transition layer and an appearance layer. The base plate comprises multiple layers of first fiber cloth and a first resin matrix, the multiple layers of first fiber cloth are arranged in a stacked mode and embedded in the first resin matrix, the base plate comprises a first surface, the base plate is in a first preset color, and the corresponding L value of the first preset color in the Lab color space is L1. The transition layer is arranged on the first surface in a stacked mode, the transition layer comprises a second surface back to the first surface, the transition layer is in a second preset color, the L value corresponding to the second preset color in the Lab color space is L2, and L2 is larger than L1. The appearance layer is arranged on the second surface in a stacked mode, the transition layer is in a third preset color, the L value corresponding to the third preset color in the Lab color space is L3, and L3 is larger than L1.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of electronic equipment, and in particular to a composite material structure and electronic equipment. Background Art

[0002] In electronic devices such as mobile phones, tablet computers and electronic devices, there are usually components to protect the circuit components inside the electronic devices, for example, the middle frame in the mobile phone, the C shell and D shell in the notebook computer, etc. It is difficult for the components in the related art to meet the requirements of structural strength and lightness, and further improvement is needed. Summary of the invention

[0003] The embodiments of the present application provide a composite material structural component and an electronic device, wherein the composite material structural component is used to solve the problem that it is difficult for components to have both structural strength and lightness.

[0004] To achieve the above objectives, the embodiments of the present application adopt the following technical solutions:

[0005] In the first aspect, the composite material structural member provided by the embodiment of the present application comprises a substrate, a transition layer and an appearance layer. The substrate comprises a plurality of first fiber cloths and a first resin matrix, the plurality of first fiber cloths are stacked, and the plurality of first fiber cloths are embedded in the first resin matrix, the substrate comprises a first surface, the substrate is in a first preset color, and the L value corresponding to the first preset color in the Lab color space is L1. The substrate has the characteristics of high strength and light weight.

[0006] The transition layer is stacked on the first surface, the transition layer includes a second surface facing away from the first surface, the transition layer is a second preset color, the second preset color corresponds to an L value of L2 in the Lab color space, and L2 is greater than L1. The appearance layer is stacked on the second surface, the transition layer is a third preset color, the third preset color corresponds to an L value of L3 in the Lab color space, and L3 is greater than L1.

[0007] L2 is greater than L1, which means that the second preset color is lighter than the first preset color, that is, the color of the transition layer is lighter than the color of the substrate. L3 is greater than L1, which means that the third preset color is lighter than the first preset color, that is, the color of the appearance layer is lighter than the color of the substrate. In this way, the transition layer can be used as an intermediate layer, and the transition layer can better cover the dark-colored substrate, so that the light-colored appearance layer can also more easily cover the dark-colored substrate. The appearance layer presents a uniform color, avoiding the problem of uneven color of the composite material structural parts. This improves the aesthetics of the appearance of the composite material structural parts, presents a good visual effect to the user, and enhances the user experience.

[0008] In addition, the transition layer is arranged on the first surface, and the surface unevenness problems such as resin enrichment, resin deficiency, black particles, etc. on the first surface can be covered with the help of the transition layer, avoiding the problem that the appearance layer is difficult to adhere to the substrate due to the uneven first surface.

[0009] In a possible implementation of the first aspect, the hardness of the substrate is greater than the hardness of the transition layer. It is easier to polish the second surface of the transition layer, and thus the processing technology of the composite material structure is simpler, which is conducive to improving the yield rate of the composite material structure and reducing the processing cost of the composite material structure.

[0010] In a possible implementation of the first aspect, the material of the first fiber cloth includes at least one of carbon fiber, glass fiber, graphite fiber, carbon nanotube fiber, graphene fiber, aluminum oxide fiber, silicon carbide fiber, silicon nitride fiber and boron nitride fiber. The tensile strength of these materials is greater than 1000 MPa, and the bending strength is also greater than 1000 MPa, so these materials have high structural strength.

[0011] As a result, when the first fiber cloth is the above-mentioned type of fiber cloth, the first fiber cloth has a higher structural strength and hardness, thereby improving the structural strength and hardness of the substrate. When the electronic device falls or collides, the composite material structure is subjected to stress impact, and the composite material structure relies on higher structural strength and hardness to resist the stress impact and avoid deformation.

[0012] In a possible implementation of the first aspect, the transition layer includes a second resin matrix and a filler, the filler is distributed in the second resin matrix, the filler is a fourth preset color, the fourth preset color corresponds to an L value L4 in the Lab color space, and L4 is greater than or equal to L2.

[0013] In this way, the matrix of the transition layer is a resin material, and the second resin matrix covers the first surface of the substrate. Specifically, the second resin matrix can fill the pits on the first surface and cover the protrusions on the first surface, thereby avoiding the problem of uneven appearance caused by the appearance layer directly contacting the first surface. In addition, the material of the second resin matrix is ​​resin, and the hardness of the second resin matrix is ​​lower than that of the substrate. The second resin matrix is ​​also easier to grind than the substrate to obtain a flat second surface, thereby improving the flatness of the appearance layer after it is set on the second surface.

[0014] The transition layer is arranged with fillers in the second resin matrix so that its color matches the light color in the above embodiment. When the appearance layer is stacked on the second surface, the light-colored transition layer will not be visible through the appearance layer, thereby improving the color uniformity of the appearance layer and further improving the aesthetics of the composite material structure.

[0015] In a possible implementation of the first aspect, both the first resin matrix and the second resin matrix are thermosetting materials, and the surface of the transition layer facing the substrate is bonded to the substrate to be connected to the substrate as an integral structure. In this way, the first resin matrix and the second resin matrix are directly cured into an integral structure, and no additional connecting member, such as glue, is required between the substrate and the transition layer to connect the two. This reduces the overall thickness of the composite material structure.

[0016] In a possible implementation of the first aspect, the interlayer bonding force between the second resin matrix and the first resin matrix is ​​greater than or equal to 1.5 MPa. When the interlayer bonding force between the second resin matrix and the first resin matrix is ​​within the above range, the bonding force between the substrate and the transition layer is relatively high, which can enhance the overall strength and stiffness of the composite structural member, so that the composite structural member can maintain structural integrity when subjected to external loads, and especially avoid the problem of misalignment between the substrate and the transition layer when the composite structural member is subjected to shear force. This ensures that the composite structural member remains stable when subjected to force or environmental changes, avoiding the risk of structural deformation and damage. The durability of the composite structural member is improved, and the maintenance and repair costs caused by structural damage are reduced.

[0017] Furthermore, when the interlayer bonding force between the second resin matrix and the first resin matrix is ​​within the above range, the flatness of the interface between the substrate and the transition layer can be ensured, defects such as unevenness or delamination can be reduced, and the aesthetics of the composite material structure can be improved.

[0018] Furthermore, when the bonding force between the first resin matrix and the second resin matrix is ​​within the above range, dust, moisture and other fine particles can be prevented from entering between the substrate and the transition layer, thereby ensuring the tight bonding between the substrate and the transition layer, and avoiding the performance degradation of the composite material structure due to environmental factors (such as temperature changes, humidity, chemical corrosion, etc.) during use.

[0019] In a possible implementation of the first aspect, the material of the first resin matrix is ​​the same as the material of the second resin matrix. In this way, the bonding force between the first resin matrix and the second resin matrix is ​​relatively high, and the bonding force between the substrate and the transition layer is also relatively high. The overall structural strength of the composite material structure is improved. When the composite material structure falls or collides, the stress and load can be better transferred between the substrate and the transition layer, so that the substrate and the transition layer can jointly resist the impact of external forces, thereby improving the impact resistance of the composite material structure.

[0020] In a possible implementation of the first aspect, the first resin matrix is ​​at least one of epoxy resin, unsaturated polyester resin, phenolic resin, polyurethane and bismaleimide resin. These types of thermosetting resin materials have high strength performance, and these thermosetting resin materials have low cost and mature processing technology, which facilitates the processing of the substrate and the transition layer, thereby improving the processing efficiency of the composite material structure.

[0021] In a possible implementation of the first aspect, the second resin matrix is ​​a thermoplastic material, the composite material structure also includes a bonding portion, and the transition layer is bonded to the substrate through the bonding portion. In this way, the material selection of the second resin matrix is ​​more diverse, the selection of the processing technology of the transition layer is also more diverse, and the composite material structure can select a transition layer material that is compatible with the material of the substrate. The bonding portion is set between the transition layer and the substrate, and the bonding portion can improve the bonding strength between the substrate and the transition layer, thereby improving the stability of the overall structure of the composite material structure.

[0022] In a possible implementation of the first aspect, the second resin matrix includes at least one of polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyamide, polyoxymethylene, polycarbonate, polyphenylene oxide, polysulfone, polyetherimide, polyethersulfone, polyphenylene sulfone resin and polyphthalamide. These types of thermoplastic resin materials have high strength performance, and these thermoplastic resin materials have low cost and mature processing technology, which facilitates the molding of the transition layer, thereby improving the processing efficiency of the composite material structure.

[0023] In a possible implementation of the first aspect, the filler includes at least one of titanium dioxide, white carbon black, calcium carbonate, kaolin, talc, and mica. In this way, the transition layer presents a white appearance by adding the filler, and since white is the lightest color among colors, when the light-colored appearance layer is disposed on the transition layer, the appearance layer can cover the transition layer. The white transition layer will not interfere with the color of the appearance layer, so that the appearance layer presents a uniform color, thereby improving the aesthetics of the composite material structure.

[0024] In a possible implementation of the first aspect, the filler is a surface-modified filler to increase the compatibility of the filler with the second resin matrix. Thus, by surface-modifying the filler, the surface energy of the filler can be adjusted to better match the surface energy of the second resin matrix, and the filler is better dispersed in the second resin matrix, the gap and interfacial tension between the filler and the second resin matrix are reduced, the interfacial adhesion between the filler and the second resin matrix is ​​enhanced, and the compatibility of the filler with the second resin matrix is ​​improved.

[0025] In a possible implementation of the first aspect, the transition layer includes multiple layers of second fiber cloth and a second resin matrix, wherein the multiple layers of second fiber cloth are stacked and embedded in the second resin matrix. As a result, the transition layer is a light-colored fiberboard, and the transition layer can better cover the dark-colored substrate, so that the light-colored appearance layer can also more easily cover the dark-colored substrate, and the appearance layer presents a uniform color, avoiding the problem of uneven color of the composite material structural part. This improves the aesthetics of the appearance of the composite material structural part, presents a good visual effect to the user, and enhances the user's experience.

[0026] Moreover, the hardness of the second fiber cloth is lower than that of the first fiber cloth. Compared with directly polishing the first surface of the substrate, the transition layer composed of the second fiber cloth and the second resin matrix is ​​easier to polish, which is beneficial to improving the processing efficiency of the composite material structure.

[0027] In a possible implementation of the first aspect, the material of the second fiber cloth includes at least one of glass, ceramic, aramid, and polyethylene. The colors of glass fiber, ceramic fiber, aramid fiber, and polyethylene fiber are close to white, and the transition layer composed of the second fiber cloth also appears white. In this way, after the appearance layer is arranged on the transition layer, the color of the transition layer will not be observed through the appearance layer, and the appearance layer presents a uniform color, which is conducive to improving the aesthetics of the composite material structure.

[0028] In a possible implementation manner of the first aspect, a material of the first fiber cloth is different from a material of the second fiber cloth.

[0029] In a possible implementation of the first aspect, the roughness of the second surface is greater than or equal to 0.2 micrometers and less than or equal to 10 micrometers, providing a smooth surface for the subsequent setting of the appearance layer, thereby improving the aesthetics of the appearance layer, and improving the flatness of the appearance layer of the composite material structure after being set on the transition layer.

[0030] In a possible implementation of the first aspect, L1 is greater than or equal to 0 and less than or equal to 30. The color of the first fiber cloth is related to the structural strength and material of the first fiber cloth, and thus, when the L1 value of the first fiber cloth is within the above range, it is configured to be compatible with the structural strength and material of the first fiber cloth, so that the first fiber cloth meets the requirements of structural strength and hardness.

[0031] In a possible implementation of the first aspect, L2 is greater than or equal to 90 and less than or equal to 100. In this way, when the L2 value is within the above range, the color of the transition layer is lighter, and the appearance layer is disposed on the second surface of the transition layer. When the appearance layer is light-colored, the appearance layer can also cover the light-colored transition layer. The color of the transition layer is lighter and cannot be observed through the appearance layer. Therefore, the appearance layer can present a good color, thereby improving the aesthetics of the composite material structure.

[0032] In a possible implementation of the first aspect, the a value corresponding to the first preset color in the Lab color space is a1, the b value corresponding to the first preset color in the Lab color space is b1, a1 is greater than or equal to -30 and less than or equal to 30, and b1 is greater than or equal to -30 and less than or equal to 30. As a result, when the a1 value and the b1 value of the first fiber cloth are within the above range, they are configured in accordance with the structural strength and material of the first fiber cloth, so that the first fiber cloth meets the requirements of structural strength and hardness.

[0033] In a possible implementation of the first aspect, the a value corresponding to the second preset color in the Lab color space is a2, the b value corresponding to the second preset color in the Lab color space is b2, a2 ​​is greater than or equal to -30 and less than or equal to 30, and b2 is greater than or equal to -30 and less than or equal to 30. In this way, when the L2 value is within the above range, the color of the transition layer is lighter, the appearance layer is arranged on the second surface of the transition layer, and when the appearance layer is light-colored, the appearance layer can also cover the light-colored transition layer, and the color of the transition layer is lighter and will not be observed through the appearance layer. Therefore, the appearance layer can present a good color, thereby improving the aesthetics of the composite material structure.

[0034] In a second aspect, an embodiment of the present application further provides a housing of an electronic device, at least a portion of which is a composite material structural member as described above.

[0035] In a third aspect, an embodiment of the present application further provides an electronic device, which includes a housing, a display and a host, wherein the housing is the housing described above, and includes a first housing and a second housing. The first housing is the housing of the display, and the second housing is the housing of the host.

[0036] In a fourth aspect, an embodiment of the present application further provides a method for processing a composite material structural member, the method comprising the following steps:

[0037] Providing a first fiber prepreg; the first fiber prepreg is in a first preset color, the L value corresponding to the first preset color in the Lab color space is L1, and the first fiber prepreg includes a first surface;

[0038] Providing a transition layer, which is a second preset color, wherein the second preset color corresponds to an L value of L2 in the Lab color space, L2 is greater than L1, and the transition layer is stacked on the first surface, and the transition layer includes a second surface facing away from the first surface;

[0039] An appearance layer is provided, and the appearance layer is stacked on the second surface.

[0040] In a possible implementation of the fourth aspect, the transition layer includes a second resin matrix and a filler, the filler is distributed in the second resin matrix, and the interlayer bonding force between the second resin matrix and the first resin matrix is ​​greater than or equal to 1.5 MPa.

[0041] In a possible implementation manner of the fourth aspect, the second resin matrix is ​​a thermosetting material, and the transition layer and the substrate are an integral structural component.

[0042] In a possible implementation manner of the fourth aspect, the second resin matrix is ​​a thermoplastic material, and after curing the first fiber prepreg and before providing the transition layer, the processing method further includes:

[0043] An adhesive portion is provided, the adhesive portion is arranged on the first surface, and the transition layer is arranged on a side of the adhesive portion facing away from the first surface.

[0044] In a possible implementation of the fourth aspect, the transition layer includes a second resin matrix and a second fiber cloth, the second fiber cloth is distributed in the second resin matrix, and the interlayer bonding force between the material of the second resin matrix and the material of the first resin matrix is ​​greater than or equal to 1.5 MPa.

[0045] In a possible implementation manner of the fourth aspect, after providing the transition layer and before providing the appearance layer, the processing method further includes:

[0046] Cleaning the second surface to remove impurities, grease and dust on the second surface;

[0047] The second surface is polished to remove scratches, pits and surface unevenness of the second surface.

[0048] Among them, the technical effects brought about by the second aspect, the third aspect and any one of the design methods in the third aspect can refer to the technical effects brought about by the different design methods in the first aspect, and will not be repeated here. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Figure 1 A schematic diagram of the structure of an electronic device provided in some embodiments of the present application;

[0050] Figure 2 for Figure 1 An exploded view of the electronic device shown in;

[0051] Figure 3 A schematic diagram of the structure of a composite material structural member provided in some embodiments of the present application;

[0052] Figure 4 for Figure 3 A schematic structural diagram of a substrate in the composite material structural member shown;

[0053] Figure 5A schematic diagram of a composite material structure is provided for some other embodiments of the present application;

[0054] Figure 6 A structural diagram of a substrate in a composite material structural member provided in some embodiments of the present application;

[0055] Figure 7 A schematic diagram of the structure of a composite material structural member provided in some embodiments of the present application;

[0056] Figure 8 A coordinate diagram of color and L value in the Lab color space referenced by the composite material structural member provided in some embodiments of the present application;

[0057] Fig. 9 A coordinate diagram of color and a value in a Lab color space referenced by a composite material structural member provided in some embodiments of the present application;

[0058] Fig.10 A coordinate diagram of color and b value in a Lab color space referenced by a composite material structural member provided in some embodiments of the present application;

[0059] Fig.11 A schematic diagram of the structure of a transition layer provided in some embodiments of the present application;

[0060] Fig.12 A diagram of the processing process of a composite material structural member provided in some embodiments of the present application;

[0061] Fig.13 A schematic diagram of the structure of a composite material structural member provided in some embodiments of the present application;

[0062] Fig.14 A diagram of the processing of composite material structural parts provided in some other embodiments of the present application;

[0063] Fig.15 A diagram of the processing process of composite material structural parts provided in some other embodiments of the present application;

[0064] Fig.16 Schematic diagram of the structure of composite material structural parts provided in some further embodiments of the present application.

[0065] Reference numerals:

[0066] 100. Electronic equipment;

[0067] 10. display; 11. display screen; 12. first housing;

[0068] 20. Host; 21. Host body; 211. Second housing; 211a. C housing; 211b. D housing; 22. Keyboard; 23. Touchpad;

[0069] 30. Composite material structural member; 31. Base plate; 311. First fiber cloth; 312. First resin matrix; 31a. First surface;

[0070] 32. Appearance layer; 321. Primer; 322. Intermediate paint; 323. Topcoat;

[0071] 33, transition layer; 33a, second surface; 331, second resin matrix; 332, filler;

[0072] 34. first fiber prepreg; 36. bonding portion;

[0073] 37. Second fiber prepreg; 371. Second fiber cloth; 38. First blank. DETAILED DESCRIPTION

[0074] In the embodiments of the present application, the terms "first", "second", and "third" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or more of the features.

[0075] In the embodiments of the present application, the terms "include", "comprises" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element.

[0076] The present application provides an electronic device, which includes but is not limited to mobile phones, electronic devices, laptop computers, personal digital assistants (PDAs), personal computers, vehicle-mounted devices and other electronic devices and accessories of these electronic devices (such as tablet computer stands, protective cases, etc.).

[0077] See also Figure 1 and Figure 2 , Figure 1 A schematic diagram of the structure of an electronic device 100 provided in some embodiments of the present application; Figure 2 for Figure 1 The exploded view of the electronic device 100 is shown. In this embodiment, the electronic device 100 is a notebook computer. In this embodiment, the electronic device 100 includes a display 10 and a host 20.

[0078] The display 10 includes a display screen 11 and a first housing 12. The display screen 11 is used to display images, videos, etc. The display screen 11 can be a flexible display screen or a rigid display screen. The first housing 12 is used to protect the display screen 11. The first housing 12 can cover the edge of the display screen 11 and the back of the display screen 11.

[0079] The host 20 includes a host body 21, a keyboard 22 and a touchpad 23. The keyboard 22 and the touchpad 23 are arranged on the host body 21. The keyboard 22 is used to input instructions or data. The touchpad 23 can be used as a mouse, and the touch action of the user's finger (including swiping, clicking, etc.) is used to control the action of the cursor on the display 10 to perform the mouse operations such as "cursor navigation", "selection", and "confirmation".

[0080] The host body 21 includes a second shell 211 and electronic components. The second shell 211 includes a C shell 211a and a D shell 211b. The C shell 211a and the D shell 211b cooperate to form a storage space. The electronic components are accommodated in the storage space, and the electronic components include but are not limited to a processor, a memory, etc. The host body 21 is used to control the display 10 to display images and videos according to the instructions or data input by the keyboard 22, and is also used to control the cursor action on the display 10 according to the touch action input by the touch pad 23.

[0081] The host body 21 is hinged to the display 10. In some embodiments, the host body 21 is hinged to the first shell 12 of the display 10 through the second shell 211. In other embodiments, the host body 21 can also be hinged to other parts of the display 10 through other parts.

[0082] The electronic device 100 can be switched between an open state and a closed state. When the electronic device 100 is in the open state, the display 10 and the host 20 form an angle greater than 0° and less than 180°. When the electronic device 100 is in the closed state, the display 10 covers the host 20, and the display surface of the display 10 faces the keyboard surface of the host 20.

[0083] In order to facilitate the description of the following embodiments, an XYZ coordinate system is established for the electronic device 100. Specifically, the extension direction of the rotation axis of the host 20 and the display 10 is defined as the X-axis direction, the thickness direction of the display 10 is defined as the Z-axis direction, and the direction perpendicular to both the X-axis direction and the Z-axis direction is defined as the Y-axis direction. It is understandable that the coordinate system setting of the display 10 can be flexibly set according to actual needs and is not specifically limited here.

[0084] As can be seen from the above, the first housing 12 serves as the top cover of the electronic device 100. The first housing 12 covers the display screen 11, and in the closed state, the first housing 12 covers the keyboard 22 and the touchpad 23. The first housing 12 protects the display screen 11, and in the closed state, protects the keyboard 22, the touchpad 23 and the host body.

[0085] The second housing 211 serves as the bottom shell of the electronic device 100. The second housing 211 covers the main body, and in the closed state, the second housing 211 covers the display screen 11, the keyboard 22, and the touch pad 23. The second housing 211 protects the main body, and in the closed state, protects the keyboard 22, the touch pad 23, and the display screen 11. Further, when the electronic device 100 is in use, the second housing 211 is located at the bottom of the electronic device 100, and the second housing 211 also plays a supporting role to ensure the stability of the electronic device 100 when in use.

[0086] Therefore, the first housing 12 and the second housing 211 are protective parts of the electronic device 100, and the first housing 12 and the second housing 211 have high structural strength requirements to protect the internal structural parts of the electronic device 100. The material of the first housing 12 and the material of the second housing 211 are mostly metals, which have sufficient structural strength to improve the stress resistance of the electronic device 100.

[0087] However, metal is heavy, which increases the overall weight of the electronic device 100 and makes it inconvenient to carry. Therefore, in order to meet the requirements of the electronic device 100 being thin and light, and having a high structural strength, some embodiments of the present application provide a composite material structure 30, which is used to form at least one of the first shell 12 and the second shell 211 in the above content. In some embodiments, only the first shell 12 is formed by the composite material structure 30; in other embodiments, only the second shell 211 is formed by the composite material structure 30; in still other embodiments, both the first shell 12 and the second shell 211 are formed by the composite material structure 30.

[0088] In the following text, the material of the first shell 12 and the material of the second shell 211 are both formed by the composite material structural member 30, and the material of the first shell 12 is consistent with the material of the second shell 211. In the following text, the first shell 12 is used as an example for explanation.

[0089] See also Figure 3 , Figure 3A schematic diagram of the structure of a composite material structure 30 provided in some embodiments of the present application. The composite material structure 30 includes a substrate 31 and an appearance layer 32, wherein the appearance layer 32 is laminated on a first surface 31a of the substrate 31, the substrate 31 supports and protects the electronic device 100, and the appearance layer 32 provides the electronic device 100 with an aesthetic appearance.

[0090] See also Figure 4 , Figure 4 for Figure 3 The schematic diagram of the structure of the substrate 31 in the composite material structural member 30 is shown. The substrate 31 includes multiple layers of first fiber cloth 311 and a first resin matrix 312 , wherein the multiple layers of first fiber cloth 311 are stacked and embedded in the first resin matrix 312 .

[0091] The material of the substrate 31 is a fiberboard, that is, a fiberboard composed of multiple layers of first fiber cloth 311 and first resin matrix 312. The fiberboard is formed by curing fiber prepreg, which is a material used in the production of composite materials. It is a composite material in a semi-cured state formed by pre-impregnating continuous fibers or cloth with resin.

[0092] Fiberboard is generally lighter than metal or plastic housings, which helps reduce the overall weight of the electronic device 100 and improve portability. The continuous fibers in the fiberboard have higher strength and stiffness and can withstand higher impact and pressure. The durability of fiber prepreg is also generally better than metal or plastic, and can resist wear and tear and the impact of long-term use.

[0093] Due to the high strength and stiffness of the fiber prepreg, the composite material structural member 30 made of the prepreg also has high structural strength and stiffness. The first shell 12 and the second shell 211 formed by the composite material structural member 30 have good impact resistance. When the electronic device 100 falls or collides, the first shell 12 and the second shell 211 provide good protection for the electronic components inside the electronic device 100, thereby avoiding the risk of damage to the electronic device 100.

[0094] The substrate 31 includes a first surface 31a, and the appearance layer 32 is stacked on the first surface 31a. The appearance layer 32 can provide different colors and glossiness according to design requirements, thereby increasing the aesthetics and attractiveness of the composite material structure 30. For example, the appearance layer 32 can be black, gray, dark gray, pure white, off-white, pink, light blue, etc.

[0095] Most fiber prepregs are dark in color, for example, carbon fiber prepregs are usually black or dark gray, and silicon carbide fiber prepregs and basalt fiber prepregs are usually dark gray. When the appearance layer 32 needs to present a dark color appearance, for example, black, dark gray, etc. Since the color of the appearance layer 32 is similar to that of the substrate 31, the appearance layer 32 can easily cover the color of the substrate 31, so that the composite structure 30 presents a color that meets the design requirements.

[0096] See also Figure 5 , Figure 5 A schematic diagram of a composite material structure 30 is provided for some other embodiments of the present application, wherein the appearance layer 32 is light-colored. When the color of the composite material structure 30 needs to be light-colored, that is, the appearance layer 32 needs to be light-colored, for example, pure white, off-white, pink, light blue, etc.

[0097] In this way, the light color of the appearance layer 32 is difficult to cover the dark color of the substrate 31, and the dark color of the substrate 31 may be transmitted through the appearance layer 32. Especially under light irradiation, the composite material structural component 30 presents an uneven color problem, thereby reducing the aesthetics of the composite material structural component 30 and further reducing the user experience.

[0098] See also Figure 6 , Figure 6 The structure diagram of the substrate 31 in the composite material structural member 30 provided in some embodiments of the present application. In addition, since the substrate 31 is composed of the first fiber cloth 311 and the first resin matrix 312, in order to meet the requirement of higher structural strength, the fibers in the first fiber cloth 311 are closely arranged in a woven manner, and the staggered arrangement of the fibers makes the first resin matrix 312 coated outside the first fiber cloth 311 uneven, thereby making the flatness of the first surface 31a poor.

[0099] Therefore, the substrate 31 includes but is not limited to the following problems. First, there may be pits, scratches or other irregular shapes on the surface of the substrate 31, which will affect the flatness of the substrate 31. Second, during the processing of the composite structural part 30, the resin may accumulate excessively in certain areas, especially on the surface or edge of the substrate 31, which will lead to the problem of resin enrichment. Third, during the processing of the composite structural part 30, some areas may not be fully filled with resin, resulting in resin loss. Fourth, due to the presence of impurities on the surface or inside of the substrate 31, such as dust, fiber debris, etc., these impurities are wrapped by the resin during the curing process, resulting in black particle spots.

[0100] The technical problem of this embodiment is explained below from the perspective of a processing method of the composite material structural member 30 .

[0101] In order to improve the flatness of the surface of the substrate 31 , before the appearance layer 32 is disposed on the substrate 31 , the first surface 31 a of the substrate 31 needs to be polished to obtain a flat first surface 31 a for facilitating the disposition of the appearance layer 32 .

[0102] Specifically, the first surface 31a is wiped to remove dust, oil and other impurities on the first surface 31a in preparation for grinding. Check whether the first surface 31a has defects such as pits, scratches, resin enrichment or resin loss. Grind the first surface 31a to remove pits, scratches, resin enrichment and resin loss on the first surface 31a and improve the flatness of the first surface 31a. The first surface 31a can be grinded with sandpaper of different coarseness or fineness, or with a polishing wheel or a grinder. After the first surface 31a is grinded, remove the dust and debris generated by the first surface 31a during the grinding process in preparation for subsequent processes.

[0103] Through the above steps, the flatness of the first surface 31 a can be effectively improved, providing a good foundation for the subsequent setting of the appearance layer 32 by coating and painting.

[0104] However, due to the high hardness of the substrate 31, the grinding time of the substrate 31 is long, which leads to low production efficiency of the composite material structure 30. In addition, due to the high hardness of the substrate 31, it is difficult to grind the substrate 31, and the surface of the substrate 31 is difficult to achieve the flatness and smoothness required by the design, and the yield rate is only 60%-70%, which increases the processing cost of the composite material structure 30.

[0105] In summary, due to the dark color of the substrate 31 itself and the uneven surface of the substrate 31 , the appearance of the composite material structural component 30 is not good after the appearance layer 32 is disposed on the first surface 31 a .

[0106] See also Figure 7 , Figure 7 This is a schematic diagram of the structure of a composite material structure 30 provided in some embodiments of the present application. In order to solve the problem that the appearance effect presented by the appearance layer 32 in the composite material structure 30 is not good after being arranged on the first surface 31a, on the basis of the above embodiments, some embodiments of the present application further provide a composite material structure 30, the composite material structure 30 includes a substrate 31, a transition layer 33 and an appearance layer 32. Compared with the above embodiments, the present embodiment adds a transition layer 33. The material and structure of the substrate 31 are consistent with the above contents and will not be repeated here.

[0107] The substrate 31 includes multiple layers of first fiber cloth 311 and a first resin matrix 312. The multiple layers of first fiber cloth 311 are stacked and embedded in the first resin matrix 312. The substrate 31 includes a first surface 31a. The substrate 31 is in a first preset color. The L value corresponding to the first preset color in the Lab color space is L1.

[0108] The transition layer 33 is stacked on the first surface 31a, and includes a second surface 33a facing away from the first surface 31a. The transition layer 33 is a second preset color, and the L value corresponding to the second preset color in the Lab color space is L2, and L2 is greater than L1. The appearance layer 32 is stacked on the second surface 33a, and the transition layer 33 is a third preset color, and the L value corresponding to the third preset color in the Lab color space is L3, and L3 is greater than L1.

[0109] The Lab color space is a color model defined by the International Commission on Illumination (CIE) for representing colors. It consists of three channels. First, the L channel represents luminance, which is the brightness or lightness of the color. Second, the a channel represents the red and green components. Positive values ​​indicate that the color is reddish, and negative values ​​indicate that the color is greenish. Third, the b channel represents the yellow and blue components. Positive values ​​indicate that the color is yellowish, and negative values ​​indicate that the color is bluish.

[0110] The following is an expanded discussion of the L value. Figure 8 , Figure 8 A coordinate diagram of color and L value in the Lab color space referenced by the composite material structural member 30 provided in some embodiments of the present application. In the Lab color space, the L value (Luminance) can be used to represent the lightness or brightness parameter of a color. The range of the L value is 0 (black) to 100 (white), and the L value determines the depth of the color. The higher the L value, the brighter the color, and the lighter the color; the lower the L value, the darker the color, and the darker the color.

[0111] Therefore, L2 being greater than L1 means that the second preset color is lighter than the first preset color, that is, the color of the transition layer 33 is lighter than the color of the substrate 31. For example, when the substrate 31 is black, the transition layer 33 is white; when the substrate 31 is black, the transition layer 33 is gray; when the substrate 31 is gray, the transition layer 33 is white, and so on.

[0112] L3 being greater than L1 means that the third preset color is lighter than the first preset color, that is, the color of the appearance layer 32 is lighter than the color of the substrate 31. For example, when the substrate 31 is black, the appearance layer 32 is white; when the substrate 31 is black, the appearance layer 32 is gray; when the substrate 31 is gray, the appearance layer 32 is white, and so on.

[0113] In this way, the transition layer 33 can be used as an intermediate layer, and the transition layer 33 can better cover the dark substrate 31, so that the light-colored appearance layer 32 can also more easily cover the dark substrate 31, and the appearance layer 32 presents a uniform color, avoiding the problem of uneven color of the composite material structure 30. In this way, the appearance of the composite material structure 30 is improved, presenting a good visual effect to the user, and enhancing the user's use experience.

[0114] In addition, the transition layer 33 is arranged on the first surface 31a. The surface unevenness problems such as resin enrichment, resin deficiency, black particles, etc. on the first surface 31a can also be covered with the help of the transition layer 33, avoiding the problem that the appearance layer 32 is difficult to adhere to the substrate 31 due to the unevenness of the first surface 31a.

[0115] In order to improve the flatness of the appearance of the composite material structural component 30, before the appearance layer 32 is disposed on the second surface 33a, the second surface 33a of the transition layer 33 is polished, and the hardness of the transition layer 33 is less than the hardness of the substrate 31. Therefore, compared with polishing the first surface 31a of the substrate 31, it is easier to polish the second surface 33a of the transition layer 33, and thus the processing technology of the composite material structural component 30 is simpler, which is conducive to improving the yield rate of the composite material structural component 30 and reducing the processing cost of the composite material structural component 30.

[0116] The material and structure of the substrate 31 are described in detail below.

[0117] The substrate 31 includes a first fiber cloth 311 and a first resin matrix 312, wherein the material of the first fiber cloth 311 includes at least one of carbon fiber, graphite fiber, carbon nanotube fiber, graphene fiber, alumina fiber, silicon carbide fiber and silicon nitride fiber. The tensile strength of these materials is greater than 1000 MPa, and the bending strength is also greater than 1000 MPa, so these materials have high structural strength.

[0118] As a result, when the first fiber cloth 311 is the above-mentioned type of fiber cloth, the first fiber cloth 311 has a high structural strength and hardness, thereby improving the structural strength and hardness of the substrate 31. When the electronic device 100 falls or collides, the first shell 12 and the second shell 211 formed by the composite material structure 30 are subjected to stress impact, and the first shell 12 and the second shell 211 rely on high structural strength and hardness to resist the stress impact and avoid deformation, thereby the first shell 12 and the second shell 211 provide good protection for the internal structural parts and electronic components of the electronic device 100, thereby improving the stability of the electronic device 100.

[0119] This application takes the material of the first fiber cloth 311 as carbon fiber as an example for introduction. Carbon fiber is a fiber material with high strength, high modulus, light weight and corrosion resistance, mainly composed of carbon elements, and is made by chemically treating and heating (carbonizing) precursors such as polyacrylonitrile (PAN), petroleum asphalt or viscose. Carbon fiber is usually dark black or gray.

[0120] The tensile strength of carbon fiber is greater than or equal to 1000 MPa and less than or equal to 7000 MPa; the flexural strength of carbon fiber is greater than or equal to 1000 MPa and less than or equal to 6000 MPa; the Brinell hardness of carbon fiber is greater than or equal to 50 and less than or equal to 80; the density of carbon fiber is greater than or equal to 1.5 grams per cubic centimeter and less than or equal to 2 grams per cubic centimeter.

[0121] Therefore, carbon fiber has very high structural strength and hardness, and carbon fiber has very light weight, and carbon fiber has a low thermal expansion coefficient and good thermal stability. As a result, the structural strength and hardness of the composite material structure 30 are also high. When the electronic device 100 falls or collides, the composite material structure 30 is subjected to stress impact. The composite material structure 30 relies on high structural strength and hardness to resist stress impact and avoid deformation. In addition, the composite material structure 30 provides good protection for the internal structural parts and electronic components of the electronic device 100, thereby improving the stability of the electronic device 100.

[0122] The materials of the first fiber cloth 311, especially the carbon fiber, all have darker colors. For example, the color of the carbon fiber is black or dark gray, the color of the graphite fiber is black, the color of the carbon nanotube fiber is black, the color of the graphene fiber is black, the color of the silicon carbide fiber is black or dark gray, the color of the silicon nitride is grayish white, and the color of the boron nitride is grayish white.

[0123] Furthermore, the higher the structural strength of the first fiber cloth 311 is, the denser the fibers in the first fiber cloth 311 are arranged, so that the color of the first fiber cloth 311 is darker, and thus the color of the substrate 31 is also darker.

[0124] Therefore, when the material of the first fiber cloth 311 is the above material, the color of the substrate 31 is darker. Figure 7Specifically, L1 is greater than or equal to 0 and less than or equal to 30. The substrate 31 as a whole presents a black, dark gray, or medium gray appearance. For example, when L1 is equal to 0, the substrate 31 presents pure black; when L1 is equal to 10, the substrate 31 presents a very dark black, which is slightly lighter than pure black; when the L value is equal to 20, the substrate 31 presents a darker black, which is lighter than when the L value is 10, but still very dark; when the L value is equal to 30, the substrate 31 presents a dark black, which is lighter than when the L value is 20, but still a very dark tone.

[0125] The color of the first fiber cloth 311 is related to the structural strength and material of the first fiber cloth 311. Therefore, when the L1 value of the first fiber cloth 311 is within the above range, it is set in accordance with the structural strength and material of the first fiber cloth 311 so that the first fiber cloth 311 meets the requirements of structural strength and hardness.

[0126] Please continue reading Figure 8 , further, based on the above embodiment, L2 is greater than or equal to 90 and less than or equal to 100. For example, L2 is 90, 91, 92, 93, 94, 95, 96, 97, 98, 99, 100. When the L2 value is 100, the color of the transition layer 33 is pure white, and when the L2 value is 90, the color of the transition layer 33 is off-white.

[0127] In this way, when the L2 value is within the above range, the color of the transition layer 33 is lighter, and the appearance layer 32 is disposed on the second surface 33a of the transition layer 33. When the appearance layer 32 is light-colored, the appearance layer 32 can also cover the light-colored transition layer 33. The color of the transition layer 33 is lighter and cannot be observed through the appearance layer 32. Therefore, the appearance layer 32 can present a good color, thereby improving the aesthetics of the composite material structural component 30.

[0128] Please also read Fig. 9 and Fig.10 , Fig. 9 A coordinate diagram of color and a value in a Lab color space referenced by a composite material structural member 30 provided in some embodiments of the present application; Fig.10 A coordinate diagram of color and b value in the Lab color space referenced by the composite material structural member 30 provided in some embodiments of the present application.

[0129] The a value corresponding to the first preset color in the Lab color space is a1, the b value corresponding to the first preset color in the Lab color space is b1, the a value corresponding to the second preset color in the Lab color space is a2, and the b value corresponding to the second preset color in the Lab color space is b2.

[0130] The corresponding a value in the Lab color space refers to the red-green hue of the color. Specifically, the a value is the red-green difference between the color and white. The a value ranges from -128 to +127, where a positive value indicates that the color is biased towards red, and a negative value indicates that the color is biased towards green. When the a value is larger, the color is closer to red; when the a value is smaller, the color is closer to green. When the a value is 0, it means that the color is neutral in red-green hue, that is, the color has no obvious red-green tendency.

[0131] The corresponding b value in the Lab color space refers to the b value, which is a parameter that describes the color, and it represents the yellow-blue tone of the color. Specifically, the b value is the yellow-blue difference between the color and white. The b value ranges from -128 to +127, where a positive value indicates that the color is biased toward yellow, and a negative value indicates that the color is biased toward blue. When the b value is larger, the color is closer to yellow; when the b value is smaller, the color is closer to blue. When the b value is 0, it means that the color is neutral in yellow-blue tone, that is, the color has no obvious yellow-blue tendency.

[0132] Based on the above embodiment, a1 is greater than or equal to -30 and less than or equal to 30, and b1 is greater than or equal to -30 and less than or equal to 30. According to the structural strength and material of the above first fiber cloth 311, the color of the first fiber cloth 311 is mostly black and dark gray, and the first fiber cloth 311 has no obvious deviation in red-green and yellow-blue hues, which is close to a neutral tone, and the substrate 31 also appears black and dark gray.

[0133] As a result, when the a1 value and the b1 value of the first fiber cloth 311 are within the above range, they are configured in accordance with the structural strength and material of the first fiber cloth 311 so that the first fiber cloth 311 meets the requirements of structural strength and hardness.

[0134] a2 is greater than or equal to -30 and less than or equal to 30, and b2 is greater than or equal to -30 and less than or equal to 30. The transition layer 33 has no obvious deviation in red-green and yellow-blue hues, and is close to a neutral tone. In this way, when the L2 value is within the above range, the color of the transition layer 33 is lighter, and the appearance layer 32 is disposed on the second surface 33a of the transition layer 33. When the appearance layer 32 is light-colored, the appearance layer 32 can also cover the light-colored transition layer 33. The color of the transition layer 33 is lighter and will not be observed through the appearance layer 32. Therefore, the appearance layer 32 can present a good color, thereby improving the aesthetics of the composite material structural component 30.

[0135] The structure and materials of the transition layer 33 are described below.

[0136] See also Fig.11 , Fig.11The schematic diagram of the structure of the transition layer 33 provided in some embodiments of the present application. The transition layer 33 includes a second resin matrix 331 and a filler 332. The second resin matrix 331 can be a transparent resin or a translucent resin. The filler 332 is distributed in the second resin matrix 331. The filler 332 is used to change the color of the transition layer 33. The filler 332 is a fourth preset color. The L value corresponding to the fourth preset color in the Lab color space is L4, and L4 is greater than or equal to L2.

[0137] In this way, the matrix of the transition layer 33 is a resin material, and the second resin matrix 331 covers the first surface 31a of the substrate 31. Specifically, the second resin matrix 331 can fill the pits of the first surface 31a and cover the protrusions of the first surface 31a, thereby avoiding the problem of uneven appearance caused by the direct contact between the appearance layer 32 and the first surface 31a. In addition, the material of the second resin matrix 331 is resin, and the hardness of the second resin matrix 331 is lower than that of the substrate 31. The second resin matrix 331 is also easier to grind than the substrate 31 to obtain a flat second surface 33a, thereby improving the flatness of the appearance layer 32 after being set on the second surface 33a.

[0138] The transition layer 33 is provided with fillers 332 in the second resin matrix 331 so that its color conforms to the light color in the above embodiment. When the appearance layer 32 is stacked and arranged on the second surface 33a, the light-colored transition layer 33 will not be visible through the appearance layer 32, thereby improving the uniformity of the color of the appearance layer 32 and further improving the aesthetics of the composite material structural component 30.

[0139] In some embodiments, the filler 332 includes at least one of titanium dioxide, white carbon black, calcium carbonate, kaolin, talc, and mica. The colors of these types of fillers 332 are all white. After these fillers 332 are added to the second resin matrix 331, the transition layer 33 appears white.

[0140] In this way, the transition layer 33 presents a white appearance by adding filler 332. Since white is the lightest color among colors, when the light-colored appearance layer 32 is disposed on the transition layer 33, the appearance layer 32 can cover the transition layer 33. The white transition layer 33 does not interfere with the color of the appearance layer 32, so that the appearance layer 32 presents a uniform color, thereby improving the aesthetics of the composite material structural component 30.

[0141] The filler 332 is usually a non-polar or less polar particle, while the second resin matrix 331 may be polar. This polarity difference will lead to poor dispersion of the filler 332 in the resin, thereby affecting the compatibility of the filler 332 with the second resin matrix 331. In order to improve the compatibility of the filler 332 with the second resin matrix 331, the filler 332 is a surface-modified filler 332 to increase the compatibility of the filler 332 with the second resin matrix 331.

[0142] Surface modification of filler 332 is a technology in materials science and chemical engineering, which is used to improve the interface interaction between filler 332 and second resin matrix 331. The purpose of surface modification is to increase the hydrophilicity or lipophilicity of filler 332 by introducing specific functional groups on the surface of filler 332, improve the bonding force between filler 332 and second resin matrix 331, and improve the dispersibility of filler 332 in second resin matrix 331.

[0143] The surface modification of the filler 332 may include but is not limited to the following methods. First, acid-base modification, by treating the filler 332 with an acid or a base, functional groups may be introduced or removed from the surface of the filler 332 to change the surface properties of the filler 332 .

[0144] Second, active groups are added by introducing specific functional groups such as hydroxyl, carboxyl, amino, etc. on the surface of filler 332 through chemical reactions. These functional groups can form chemical bonds with the groups in the resin, thereby improving the bonding force between filler 332 and the resin.

[0145] As a result, by performing surface modification on the filler 332, the surface energy of the filler 332 can be adjusted to better match the surface energy of the second resin matrix 331, and it helps to better disperse the filler 332 in the second resin matrix 331, reduce the gap and interfacial tension between the filler 332 and the second resin matrix 331, enhance the interfacial adhesion between the filler 332 and the second resin matrix 331, and improve the compatibility of the filler 332 with the second resin matrix 331.

[0146] In some embodiments, the first resin matrix 312 and the second resin matrix 331 are both thermosetting materials, and the surface of the transition layer 33 facing the substrate 31 is in contact with the substrate 31 to form an integral structure with the substrate 31. In this way, the first resin matrix 312 and the second resin matrix 331 are directly cured into an integral structure, and no additional connecting member, such as glue, is required between the substrate 31 and the transition layer 33 to connect the two. This reduces the overall thickness of the composite material structure 30.

[0147] Furthermore, the interlayer bonding force between the second resin matrix 331 and the first resin matrix 312 is greater than or equal to 1.5 MPa. The interlayer bonding force refers to the bonding force between two adjacent layers or stacked structures, which determines the interaction and load transfer capacity between layers.

[0148] In this way, when the interlayer bonding force between the second resin matrix 331 and the first resin matrix 312 is within the above range, the bonding force between the substrate 31 and the transition layer 33 is relatively high, which can enhance the overall strength and rigidity of the composite structural member 30, so that the composite structural member 30 can maintain the structural integrity when subjected to external loads, especially avoiding the problem of misalignment between the substrate 31 and the transition layer 33 when the composite structural member 30 is subjected to shear force. This ensures that the composite structural member 30 remains stable when subjected to force or environmental changes, avoiding the risk of structural deformation and damage. The durability of the composite structural member 30 is improved, and the maintenance and repair costs caused by structural damage are reduced.

[0149] Furthermore, when the interlayer bonding force between the second resin matrix 331 and the first resin matrix 312 is within the above range, the flatness of the interface between the substrate 31 and the transition layer 33 can be ensured, defects such as unevenness or delamination can be reduced, and the aesthetics of the composite material structure 30 can be improved.

[0150] Furthermore, when the bonding force between the first resin matrix 312 and the second resin matrix 331 is within the above range, dust, moisture and other fine particles can be prevented from entering between the substrate 31 and the transition layer 33, thereby ensuring the tight bonding between the substrate 31 and the transition layer 33, and avoiding the performance degradation of the composite material structure 30 due to environmental factors (such as temperature changes, humidity, chemical corrosion, etc.) during use.

[0151] In some embodiments, the material of the first resin matrix 312 is the same as the material of the second resin matrix 331. In this way, the bonding force between the first resin matrix 312 and the second resin matrix 331 is relatively high, and the bonding force between the substrate 31 and the transition layer 33 is also relatively high. The overall structural strength of the composite structural member 30 is improved. When the composite structural member 30 falls or collides, the stress and load can be better transferred between the substrate 31 and the transition layer 33, so that the substrate 31 and the transition layer 33 can jointly resist the impact of external forces, thereby improving the impact resistance of the composite structural member 30.

[0152] In some embodiments, the first resin matrix 312 is at least one of epoxy resin, unsaturated polyester resin, phenolic resin, polyurethane and bismaleimide resin. These types of thermosetting resin materials have high strength performance, and these thermosetting resin materials have low cost and mature processing technology, which facilitates the processing of the substrate 31 and the transition layer 33, thereby improving the processing efficiency of the composite material structure 30.

[0153] See also Fig.12 , Fig.12 The processing diagram of the composite material structure 30 provided in some embodiments of the present application. For the embodiment in which the second resin matrix 331 is a thermosetting material, the processing process of the composite material structure 30 in this embodiment is described in detail.

[0154] A first fiber prepreg 34 is provided. The first fiber prepreg 34 includes multiple layers of first fiber cloth 311 and a first resin matrix 312. The multiple layers of first fiber cloth 311 are embedded in the first resin matrix 312. The first fiber prepreg 34 is in a semi-solid state. The processing of the first fiber prepreg 34 includes:

[0155] The multi-layer first fiber cloth 311 is pretreated to clean the fibers to remove surface oil, dust and impurities. In some embodiments, the processing method of the first fiber prepreg 34 also includes heat treatment or other surface treatment steps for the multi-layer first fiber cloth 311 to improve the adhesion between the fibers and the resin.

[0156] The first resin matrix 312 and the curing agent are mixed in a certain proportion and heated to a designed temperature to improve the fluidity of the resin. The pretreated multi-layer first fiber cloth 311 is impregnated in the first resin matrix 312 so that the multi-layer first fiber cloth 311 fully absorbs the resin. The fiber impregnation process can be completed using equipment such as a roller, a sprayer, and an impregnation tank. The above processing process obtains a semi-solid first fiber prepreg 34.

[0157] The processing of the transition layer 33 includes adding a filler 332 to the second resin matrix 331, and chemically reacting the second resin matrix 331 with the filler 332 to improve the compatibility between the second resin matrix 331 and the filler 332. When the second resin matrix 331 and the filler 332 reach a certain degree of cross-linking, the viscosity of the second resin matrix 331 and the filler 332 increases, and the fluidity decreases, and the second resin matrix 331 and the filler 332 are transformed into a semi-solid state to form a transition layer blank 35.

[0158] The semi-solid transition layer blank 35 is stacked on the surface of the first fiber prepreg 34 to form a first blank 38, and the first blank 38 is placed in a mold and laid into a desired shape, and pressure and temperature are applied to cure the first fiber prepreg 34 and the transition layer blank 35 to form a blank of the composite material structure 30. The curing process can be thermal curing or light curing, depending on the type of resin used.

[0159] After curing is completed, the composite material structure blank is taken out from the mold. According to the design requirements, the composite material structure blank is cut and formed to obtain the composite material structure 30. The cutting and forming of the composite material structure blank can be performed by laser cutting, mechanical cutting or thermal cutting.

[0160] Through the above processing method, the substrate 31 and the transition layer 33 are cured and formed in the same process, and no additional connector is required between the substrate 31 and the transition layer 33, which is conducive to the thinning of the composite material structure 30. In addition, the processing of the composite material structure 30 is simpler, which is conducive to improving the processing efficiency of the composite material structure 30. The substrate 31 and the transition layer 33 are cured and formed in the same process to ensure better combination between the two, forming an integral structure, and improving the structural integrity and strength of the composite material structure 30.

[0161] The exterior layer 32 is disposed on the second surface 33 a of the transition layer 33 .

[0162] See also Fig.13 , Fig.13 Schematic diagram of the structure of the composite material structural member 30 provided in some embodiments of the present application. In some other embodiments, the second resin matrix 331 is a thermoplastic material, so that the second resin matrix 331 and the filler 332 can be connected to the substrate 31 after being separately molded, that is, after the transition layer 33 is separately processed into a shape adapted to the substrate 31, the transition layer 33 is connected to the first surface 31a of the substrate 31 by means of the adhesive portion 36.

[0163] In this way, the material selection of the second resin matrix 331 is more diverse, the selection of the processing technology of the transition layer 33 is also more diverse, and the composite material structure 30 can select the transition layer 33 material that is compatible with the material of the substrate 31. An adhesive portion 36 is provided between the transition layer 33 and the substrate 31, and the adhesive portion 36 can improve the bonding strength between the substrate 31 and the transition layer 33, thereby improving the overall structural stability of the composite material structure 30.

[0164] Further, the second resin matrix 331 includes at least one of polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyamide, polyoxymethylene, polycarbonate, polyphenylene oxide, polysulfone, polyetherimide, polyethersulfone, polyphenylene sulfone resin and polyphthalamide. These types of thermoplastic resin materials have high strength performance, and these thermoplastic resin materials have low cost and mature processing technology, which is convenient for forming the transition layer 33, thereby improving the processing efficiency of the composite material structure 30.

[0165] See also Fig.14 , Fig.14 The processing diagram of the composite material structure 30 provided in some other embodiments of the present application. For the above embodiment in which the second resin matrix 331 is a thermoplastic material, the processing process of the composite material structure 30 in this embodiment is introduced in detail.

[0166] A first fiber prepreg 34 is provided. The first fiber prepreg 34 includes multiple layers of first fiber cloth 311 and a first resin matrix 312, wherein the multiple layers of first fiber cloth 311 are embedded in the first resin matrix 312, and the first fiber prepreg 34 is in a semi-solid state. It is worth noting that the difference between this embodiment and the processing process in which the second resin matrix 331 is a thermosetting material is that the first fiber prepreg 34 is cured and formed separately after preparation to obtain the substrate 31.

[0167] A second resin matrix 331 and a filler 332 are provided, and the second resin matrix 331 and the filler 332 are fixedly formed to obtain a transition layer 33 .

[0168] An adhesive portion 36 is disposed on the first surface 31 a of the substrate 31 , and the transition layer 33 is connected to the substrate 31 via the adhesive portion 36 .

[0169] In the above processing method, the substrate 31 and the transition layer 33 are connected by means of the adhesive portion 36 after being formed separately. The transition layer 33 is formed separately, which can improve the surface flatness of the transition layer 33 and facilitate the arrangement of the appearance layer 32 on the second surface 33a of the transition layer 33.

[0170] In some other embodiments, the transition layer 33 includes multiple layers of second fiber cloth 371 and a second resin matrix 331, wherein the multiple layers of second fiber cloth 371 are stacked and embedded in the second resin matrix 331. Thus, the transition layer 33 is a light-colored fiberboard, and the material of the transition layer 33 is similar to that of the substrate 31, which is conducive to the bonding between the substrate 31 and the transition layer 33, thereby improving the overall structural strength of the composite material structural component 30, and the composite material structural component 30 can withstand greater stress and load, thereby improving the impact resistance of the composite material structural component 30.

[0171] Furthermore, the material of the second fiber cloth 371 includes at least one of glass, ceramic, aramid, and polyethylene. The colors of glass fiber, ceramic fiber, aramid fiber, and polyethylene fiber are close to white, and the transition layer 33 composed of the second fiber cloth 371 also appears white. In this way, after the appearance layer 32 is set on the transition layer 33, the color of the transition layer 33 will not be observed through the appearance layer 32, and the appearance layer 32 presents a uniform color, which is conducive to improving the aesthetics of the composite material structure 30.

[0172] See also Fig.15 , Fig.15 The processing diagram of the composite material structural member 30 provided in some embodiments of the present application. For the processing method of the transition layer 33 including multiple layers of second fiber cloth 371 and second resin matrix 331, reference can be made to the processing method of the second resin matrix 331 of the transition layer 33 as a thermosetting material in the above content. Specifically, the processing method includes:

[0173] A first fiber prepreg 34 is provided. The first fiber prepreg 34 includes multiple layers of first fiber cloth 311 and a first resin matrix 312. The multiple layers of first fiber cloth 311 are embedded in the first resin matrix 312. The first fiber prepreg 34 is in a semi-solid state.

[0174] A second fiber prepreg 37 is provided. The second fiber prepreg 37 includes multiple layers of second fiber cloth 371 and a second resin matrix 331. The multiple layers of second fiber cloth 371 are embedded in the second resin matrix 331. The second fiber prepreg 37 is in a semi-solid state.

[0175] The semi-solid second fiber prepreg 37 is stacked on the surface of the first fiber prepreg 34 to form a first blank, the first blank is placed in a mold and laid into a desired shape, and pressure and temperature are applied to cure the first fiber prepreg 34 and the second fiber prepreg 37 to form a composite material structural blank. The curing process can be thermal curing or light curing, depending on the type of resin used.

[0176] After curing is completed, the composite material structural component blank is taken out from the mold. According to the design requirements, the composite material structural component blank is cut and formed to obtain a composite material structural component 30, in which the substrate 31 is formed by curing the first fiber prepreg 34, and the transition layer 33 is formed by curing the second fiber prepreg 37.

[0177] Through the above processing method, the substrate 31 and the transition layer 33 are cured and formed in the same process, and no additional connector is required between the substrate 31 and the transition layer 33, which is conducive to the thinning of the composite material structure 30. In addition, the processing of the composite material structure 30 is simpler, which is conducive to improving the processing efficiency of the composite material structure 30. The substrate 31 and the transition layer 33 are cured and formed in the same process to ensure better combination between the two, forming an integral structure, and improving the structural integrity and strength of the composite material structure 30.

[0178] On the basis of any of the above processing methods, after the substrate 31 is connected to the transition layer 33 , the processing method of the composite material structural component 30 further includes the following steps.

[0179] The second surface 33a of the transition layer 33 is polished to make the roughness of the second surface 33a greater than or equal to 0.2 microns and less than or equal to 10 microns, so as to provide a flat surface for the subsequent arrangement of the appearance layer 32, thereby improving the aesthetics of the appearance layer 32, and improving the flatness of the appearance layer 32 of the composite material structural component 30 after being arranged on the transition layer 33.

[0180] In any of the above embodiments, the thickness of the transition layer 33 is greater than or equal to 80 microns and less than or equal to 120 microns. When the thickness of the transition layer 33 is within this range, the transition layer 33 can better cover the unevenness on the substrate 31, and has little effect on the thickness of the composite material structure 30, thereby ensuring the lightness and thinness of the composite material structure 30.

[0181] See also Fig.16 , Fig.16 Schematic diagram of the structure of a composite material structural member 30 provided in some embodiments of the present application. The appearance layer 32 is applied to the second surface 33a. The appearance layer 32 includes a primer 321, a midcoat 322 and a topcoat 323. The primer 321 is applied to the second surface 33a, the midcoat 322 is applied to the surface of the primer 321 away from the second surface 33a, and the topcoat 323 is applied to the surface of the midcoat 322 away from the primer 321. The primer 321 and the topcoat 323 are transparent materials, and the midcoat 322 presents the color of the composite material structural member 30.

[0182] The arrangement direction of the substrate 31 and the transition layer 33 is a first direction, the thickness of the primer 321 in the first direction is greater than or equal to 5 microns and less than or equal to 10 microns, the thickness of the intermediate paint 322 in the first direction is greater than or equal to 30 microns, and the thickness of the topcoat 323 in the first direction is greater than or equal to 15 microns and less than or equal to 30 microns.

[0183] Among them, the primer 321 is used to enhance the adhesion between the transition layer 33 and the intermediate paint 322 and the topcoat 323. The primer 321 fills the small defects on the second surface 33a, improves the flatness of the second surface 33a, and provides a good adhesion foundation for the subsequent paint layer. The intermediate paint 322 can enhance the wear resistance, chemical resistance, heat resistance, etc. of the primer 321, fill the defects in the intermediate coating, and provide a better appearance effect. The topcoat 323 enhances the weather resistance, pollution resistance, scratch resistance, etc. of the intermediate paint 322, and provides a good appearance and protection.

[0184] The appearance layer 32 can form a multi-layer coating system by setting the primer 321, the intermediate paint 322 and the topcoat 323, and the composite material structure 30 has comprehensive, durable and beautiful protection. After the appearance layer 32 is sprayed, it is cured.

[0185] Finally, the exterior layer 32 is polished and finished, and the cured exterior layer 32 is polished to further improve the surface flatness and smoothness of the composite material structural component 30 .

[0186] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.

[0187] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.

Claims

1. A composite material structural part, characterized in that: include: A substrate, comprising a plurality of first fiber cloths and a first resin matrix, wherein the plurality of first fiber cloths are stacked and embedded in the first resin matrix, the substrate comprising a first surface, the substrate being in a first preset color, and the L value corresponding to the first preset color in the Lab color space is L1; A transition layer is stacked on the first surface, the transition layer includes a second surface facing away from the first surface, the transition layer is in a second preset color, the second preset color corresponds to an L value of L2 in the Lab color space, and L2 is greater than L1; The appearance layer is stacked on the second surface, the transition layer is in a third preset color, the L value corresponding to the third preset color in the Lab color space is L3, and the L3 is greater than the L1.

2. The composite material structural member according to claim 1, characterized in that: The hardness of the substrate is greater than the hardness of the transition layer.

3. The composite material structural member according to claim 2, characterized in that: The material of the first fiber cloth includes at least one of carbon fiber, glass fiber, graphite fiber, carbon nanotube fiber, graphene fiber, aluminum oxide fiber, silicon carbide fiber, silicon nitride fiber and boron nitride fiber.

4. The composite material structural member according to any one of claims 1 to 3, characterized in that: The transition layer includes a second resin matrix and a filler, wherein the filler is distributed in the second resin matrix and presents a fourth preset color. The L value corresponding to the fourth preset color in the Lab color space is L4, and L4 is greater than or equal to L2.

5. The composite material structural member according to claim 4, characterized in that: The first resin matrix and the second resin matrix are both thermosetting materials, and the surface of the transition layer facing the substrate is in contact with the substrate so as to be connected with the substrate to form an integral structural component.

6. The composite material structural member according to claim 4 or 5, characterized in that: The interlayer bonding force between the second resin matrix and the first resin matrix is ​​greater than or equal to 1.5 MPa.

7. The composite material structural member according to claim 5 or 6, characterized in that: The material of the first resin matrix is ​​the same as the material of the second resin matrix; and / or, The first resin matrix is ​​at least one of epoxy resin, unsaturated polyester resin, phenolic resin, polyurethane and bismaleimide resin.

8. The composite material structural member according to claim 4, characterized in that: The second resin matrix is ​​a thermoplastic material, and the composite material structural component further includes a bonding portion, through which the transition layer is bonded to the substrate.

9. The composite material structural member according to claim 8, characterized in that: The second resin matrix includes at least one of polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyamide, polyoxymethylene, polycarbonate, polyphenylene oxide, polysulfone, polyetherimide, polyethersulfone, polyphenylene sulfone resin and polyphthalamide.

10. The composite material structural member according to any one of claims 4 to 9, characterized in that: The filler includes at least one of titanium dioxide, white carbon black, calcium carbonate, kaolin, talc and mica.

11. The composite material structural member according to any one of claims 4 to 10, characterized in that: The filler is a surface-modified filler to increase the compatibility of the filler with the second resin matrix.

12. The composite material structural member according to claim 2 or 3, characterized in that: The transition layer includes multiple layers of second fiber cloth and a second resin matrix, wherein the multiple layers of the second fiber cloth are stacked and embedded in the second resin matrix.

13. The composite material structural member according to claim 12, characterized in that: The material of the second fiber cloth includes at least one of glass, ceramic, aramid and polyethylene.

14. The composite material structural member according to claim 12 or 13, characterized in that: The material of the first fiber cloth is different from the material of the second fiber cloth.

15. The composite material structural member according to any one of claims 1 to 14, characterized in that: The roughness of the second surface is greater than or equal to 0.2 micrometers and less than or equal to 10 micrometers.

16. The composite material structural member according to any one of claims 1 to 15, characterized in that: The L1 is greater than or equal to 0 and less than or equal to 30.

17. The composite material structural member according to any one of claims 1 to 16, characterized in that: The L2 is greater than or equal to 90 and less than or equal to 100.

18. The composite material structural member according to any one of claims 1 to 17, characterized in that: The a value corresponding to the first preset color in the Lab color space is a1, the b value corresponding to the first preset color in the Lab color space is b1, a1 is greater than or equal to -30 and less than or equal to 30, and b1 is greater than or equal to -30 and less than or equal to 30.

19. The composite material structural member according to any one of claims 1 to 18, characterized in that: The a value corresponding to the second preset color in the Lab color space is a2, the b value corresponding to the second preset color in the Lab color space is b2, a2 ​​is greater than or equal to -30 and less than or equal to 30, and b2 is greater than or equal to -30 and less than or equal to 30.

20. A housing of an electronic device, characterized in that: At least a portion of the shell is a composite material structure according to any one of claims 1 to 19.

21. An electronic device, characterized in that: include: The housing is the housing according to claim 20, wherein the housing comprises a first housing and a second housing; A display, wherein the first housing is a housing of the display; Host, the second shell is the shell of the host.

Citation Information

Patent Citations

  • Protective cover plate and electronic device applying same

    CN108323056A

  • Decoration member and method for manufacturing same

    CN111757808A

  • Shell, electronic equipment and shell manufacturing method

    CN114554739A

  • Shell assembly, preparation method thereof and terminal

    CN115967759A

  • Article of footwear with masking layer with structural color

    CN116113341A