Method for recycling and treating lithium battery disassembling and recycling wastewater

Through the combination of lithium-rich positive electrode and degraded negative electrode, the lithium electrolyte and organic matter in the dismantling wastewater by using the electrolysis process, the problems of low resource utilization and high treatment cost in the wastewater recycling of lithium batteries are solved. Efficient lithium ion recovery and organic pollutant removal are achieved.

CN118908352AInactive Publication Date: 2024-11-08GUANGZHOU HKUST FOK YING TUNG RES INST
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410997253.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The prior art has a potential threat to human health in the dismantling and recycling of lithium batteries, and it is difficult to effectively recover lithium ions.

Method used

Using a combination of lithium-rich positive electrode and degraded negative electrode, the lithium electrolyte and organic matter in wastewater are removed and recovered through the electrolysis process, and the lithium-manganese oxide composite electrode and boron-doped diamond electrode are used for electrolysis to generate efficient lithium ion recovery solution and degrade it. Organic pollutants.

Benefits of technology

It realizes efficient recovery of lithium ions and efficient removal of organic pollutants, reduces the difficulty of subsequent biological treatment, improves resource utilization, and reduces processing costs. It is simple to operate and has conventional equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908352A_ABST
    Figure CN118908352A_ABST
Patent Text Reader

Abstract

The invention relates to a method for recycling and treating lithium battery disassembling and recycling wastewater, and belongs to the field of lithium battery disassembling and recycling wastewater and reuse. The method comprises: preparing a lithium-rich positive electrode; adjusting the pH value of the lithium-containing wastewater, standing, transferring to an electrode recovery pool, placing a lithium-rich positive electrode and a degradation negative electrode, applying constant current to flow from the positive electrode to the negative electrode to obtain a lithium manganese oxide composite electrode, and degrading organic matters by the degradation negative electrode; the lithium manganese oxide composite electrode is placed in an electrode release pool, a lithium-based phosphate buffer solution is poured, a stainless steel negative electrode is placed, constant current is applied, the current flows from the negative electrode to the positive electrode, and a lithium-rich positive electrode and a lithium-rich solution are obtained. According to the method, organic matters are decomposed while lithium is efficiently recycled, the resource utilization rate is high, operation is simple, equipment is conventional, the treatment difficulty is small, and the cost is low. The method has high lithium extraction rate and organic pollutant removal rate, solves the problem that organic pollutants in waste water need to be removed in advance in a traditional recovery process, and provides a new scheme for improving lithium ions in waste water recovered in the waste lithium battery recovery industry.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of lithium battery disassembly and recycling of waste water, and in particular relates to a method for recycling and treating lithium battery disassembly and recycling waste water. Background Art

[0002] Lithium-ion batteries are widely used as electrochemical power sources due to their advantages such as high battery voltage, high energy density, low self-discharge rate and long storage life.

[0003] In recent years, research on the recycling of lithium-ion batteries has attracted great interest, and the hydrometallurgical process is a commercial method for recovering metals from waste lithium-ion batteries. In this method, the disassembled electrodes are dissolved in concentrated acid, and the dissolved metals are then recovered by extraction, precipitation, or electrodeposition. Traditional pyrometallurgical methods burn off all organic electrolytes and binders, making it easier to recover valuable metals. However, these processes can only effectively recover cobalt, and hydrometallurgical and pyrometallurgical processes are not suitable for lithium recovery. In addition, the lithium ions produced in these processes are usually discharged as waste, resulting in a waste of lithium resources. In terms of human health, exposure to lithium ions may cause damage to the nervous system, kidneys, liver, brain, cardiovascular and endocrine systems.

[0004] Although the recovery of lithium from spent batteries has recently begun via solvent extraction. However, these methods are not suitable for use at an industrial level because they are time-consuming and costly, and the use of organic solvents in solvent extraction can cause environmental issues. In addition, there are few reports on the recovery of lithium from battery plant wastewater via adsorption processes, but the interference of organic pollutants in the wastewater and the use of acid in the desorption step limit the practical application of this method. This results in most of the lithium ions in spent batteries being discarded without a proper recovery step, so it is very important to remove and recover lithium ions from industrial wastewater generated by spent lithium battery operations. Summary of the invention

[0005] The purpose of the present invention is to solve the problems of great difficulty in treating industrial wastewater generated by the operation of existing waste lithium batteries, low resource utilization rate and high treatment cost, and to provide a method for recycling and treating lithium battery disassembly and recycling wastewater.

[0006] A method for recycling and treating lithium battery disassembly and recycling wastewater, which is carried out according to the following steps:

[0007] 1. Preparation of lithium-rich cathode:

[0008] The lithium manganese oxide powder, carbon black and polytetrafluoroethylene are mixed and calcined to obtain a lithium manganese oxide composite electrode, which is then placed in a lithium-based phosphate buffer solution and a stainless steel negative electrode, and a constant current is applied until the potential reaches 2.5V to obtain a λ-MnO2 positive electrode, which is a lithium-rich positive electrode;

[0009] 2. The lithium-containing wastewater enters the pH adjustment tank, and 1M NaOH is added to adjust the pH value to 6.6-6.7. After stirring for 2 hours, it is allowed to stand for 3 hours. The resulting supernatant is the wastewater solution, which is then transferred to the electrode recovery tank, and the lithium-rich positive electrode and degraded negative electrode prepared in step 1 are placed, and then 100 mA·h·g –1 A constant current is generated and the current flows from the positive electrode to the negative electrode until the potential of the lithium-rich positive electrode reaches 1.5V, thereby obtaining a lithium manganese oxide composite electrode, and degrading the negative electrode to produce hydroxyl radicals to degrade organic matter in the wastewater solution, and the generated wastewater enters the existing biological treatment section;

[0010] 3. The lithium manganese oxide composite electrode obtained in step 2 is placed in an electrode release cell, a lithium-based phosphate buffer solution is poured in, a stainless steel negative electrode is placed, and then 100 mA·h·g –1 A constant current is supplied from the negative electrode to the positive electrode until the potential of the lithium manganese oxide composite electrode reaches 1.5 V, thereby obtaining a lithium-rich positive electrode and a lithium-rich solution, thereby completing the method for recycling and treating lithium battery disassembly and recycling wastewater.

[0011] Furthermore, in step 1, the volume percentage of the lithium manganese oxide powder, carbon black and polytetrafluoroethylene is 80:10:10.

[0012] Furthermore, the calcination in step 1 is performed at 400° C. for 8 h.

[0013] Furthermore, the lithium-rich positive electrode in step 1 is rectangular in shape, with a specification of 20 cm per 2 The active area contains 1000 mg of active material.

[0014] Furthermore, the concentration of the lithium-based phosphate buffer solution in step 1 is 100 mM, and the pH value is 7.2; preparation of the lithium-based phosphate buffer solution: add 1 mol of methyl methacrylate (PMMA), 1 mmol of lithium phosphate (Li3PO4) and 1 mol of lithium fluorophosphate (liPF6) salt to 500 ml of aqueous phosphoric acid solution (MAP), then heat to 90°C and stir for 10 minutes.

[0015] Furthermore, the indicator of the lithium-containing wastewater in step 2 is: the oxidation-reduction potential ORP is +100mV; it is detected by an Ag / AgCl reference electrode installed in a pH adjustment tank.

[0016] Furthermore, the degradation negative electrode in step 2 is a rectangular boron-doped diamond electrode with a specification of 5 cm 2 The active area contains 20 mg of active material.

[0017] Furthermore, the lithium-rich positive electrode obtained in step three is continuously reused in the electrode recovery pool, and steps two and three are cycled 5 to 10 times to complete the reuse of the lithium-rich positive electrode.

[0018] Furthermore, the lithium-rich solution obtained in step three is the recovered lithium ions.

[0019] Advantages of the present invention:

[0020] 1. The present invention proposes a method for removing and recovering high-value lithium electrolytes and difficult-to-remove organic matter in wastewater from the dismantling and recovery of waste lithium batteries by using lithium-rich electrodes and degradable electrodes. The method can efficiently recover lithium while decomposing organic matter, with a high resource utilization rate, simple operation, conventional equipment, low processing difficulty and low processing cost.

[0021] 2. The present invention has a high lithium extraction rate and organic pollutant removal rate, which solves the problem of the need to remove organic pollutants in wastewater in advance in the traditional recycling process, and provides a new feasible solution for improving the recovery of lithium ions in wastewater in the waste lithium battery recycling industry.

[0022] 3. The degradation electrode used in the present invention is a boron-doped diamond electrode, which has the advantages of high efficiency, environmental protection, and no need to add chemical reagents. During the electrolysis process, the boron-doped diamond electrode can directly or indirectly oxidize the organic matter in the wastewater solution into non-toxic and harmless inorganic matter (such as carbon dioxide and water), thereby reducing the content of organic pollutants in the water, or directly mineralizing them, greatly reducing the difficulty of subsequent biological treatment.

[0023] The present invention is suitable for recycling and treating lithium battery disassembly and recycling wastewater. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A bar graph showing the increased concentration of lithium ions in the electrode recovery pool in the embodiment;

[0025] Figure 2 is the ratio of organic carbon in the example to initial organic carbon. DETAILED DESCRIPTION

[0026] The technical solution of the present invention is not limited to the specific implementation modes listed below, but also includes any combination of the specific implementation modes.

[0027] Specific implementation method 1: This implementation method is a method for recycling and treating lithium battery disassembly and recycling wastewater, which is carried out in the following steps:

[0028] 1. Preparation of lithium-rich cathode:

[0029] The lithium manganese oxide powder, carbon black and polytetrafluoroethylene are mixed and calcined to obtain a lithium manganese oxide composite electrode, which is then placed in a lithium-based phosphate buffer solution and a stainless steel negative electrode, and a constant current is applied until the potential reaches 2.5V to obtain a λ-MnO2 positive electrode, which is a lithium-rich positive electrode;

[0030] 2. The lithium-containing wastewater enters the pH adjustment tank, and 1M NaOH is added to adjust the pH value to 6.6-6.7. After stirring for 2 hours, it is allowed to stand for 3 hours. The resulting supernatant is the wastewater solution, which is then transferred to the electrode recovery tank, and the lithium-rich positive electrode and degraded negative electrode prepared in step 1 are placed, and then 100 mA·h·g –1 A constant current is generated and the current flows from the positive electrode to the negative electrode until the potential of the lithium-rich positive electrode reaches 1.5V, thereby obtaining a lithium manganese oxide composite electrode, and degrading the negative electrode to produce hydroxyl radicals to degrade organic matter in the wastewater solution, and the generated wastewater enters the existing biological treatment section;

[0031] 3. The lithium manganese oxide composite electrode obtained in step 2 is placed in an electrode release cell, a lithium-based phosphate buffer solution is poured in, a stainless steel negative electrode is placed, and then 100 mA·h·g –1 A constant current is supplied from the negative electrode to the positive electrode until the potential of the lithium manganese oxide composite electrode reaches 1.5 V, thereby obtaining a lithium-rich positive electrode and a lithium-rich solution, thereby completing the method for recycling and treating lithium battery disassembly and recycling wastewater.

[0032] In the electrode recovery pool described in step 2 of this embodiment, a measuring electrode is installed to detect whether the redox point of the wastewater in the recovery pool meets the lithium ion recovery requirements of step 3.

[0033] In step three of this embodiment, a measuring electrode is installed in the electrode release pool to detect the redox point of the wastewater in the electrode release pool to prevent excessive electrode release.

[0034] The lithium-containing wastewater described in step 2 of this embodiment is the lithium-containing wastewater generated during the dismantling of waste lithium batteries and the acid leaching of lithium batteries to recover positive electrode materials. The wastewater contains a large amount of lithium ions, sulfate ions used in the acid leaching process, organic matter in the electrolyte, etc.

[0035] After the current is applied in step 2 of this embodiment, the lithium ions in the wastewater will be captured on the lithium-rich positive electrode, and the lithium-rich positive electrode is converted into a lithium-manganese oxide composite electrode.

[0036] After the current is applied in step 2 of this embodiment, the degradation negative electrode produces hydroxyl radicals during the electrolysis process, which can degrade the organic matter in the wastewater solution into inorganic matter and water, so that the content of organic pollutants in the wastewater solution is reduced or directly mineralized. The generated wastewater enters the existing biological treatment section for treatment, and then it can meet the emission standards, which greatly reduces the difficulty of subsequent treatment.

[0037] After the current is applied in step three of this embodiment, the lithium ions in the lithium manganese oxide composite electrode are released into the lithium-based phosphate buffer solution, thereby obtaining a lithium-rich solution, and also converting the lithium manganese oxide composite electrode into a lithium-rich positive electrode.

[0038] Specific embodiment 2: This embodiment is different from specific embodiment 1 in that the volume percentage of lithium manganese oxide powder, carbon black and polytetrafluoroethylene in step 1 is 80:10:10. Other steps and parameters are the same as those in specific embodiment 1.

[0039] Specific implementation method 3: This implementation method is different from specific implementation method 1 in that the calcination in step 1 is carried out at 400° C. for 8 h. The other steps and parameters are the same as those in specific implementation method 1.

[0040] Specific embodiment 4: This embodiment is different from the specific embodiment 1 in that the lithium-rich positive electrode in step 1 is rectangular in shape, with a specification of 20 cm per 2 The active area contains 1000 mg of active material. Other steps and parameters are the same as those in the first embodiment.

[0041] Specific embodiment 5: This embodiment differs from specific embodiment 1 in that the concentration of the lithium-based phosphate buffer solution in step 1 is 100 mM and the pH value is 7.2; preparation of the lithium-based phosphate buffer solution: add 1 mol of methyl methacrylate, 1 mmol of lithium phosphate and 1 mol of lithium fluorophosphate salt to 500 ml of phosphoric acid aqueous solution, then heat to 90°C and stir for 10 minutes. Other steps and parameters are the same as those in specific embodiment 1.

[0042] Specific implementation method 6: This implementation method is different from specific implementation method 1 in that the indicator of lithium-containing wastewater in step 2 is: the oxidation-reduction potential ORP is +100mV; it is detected by an Ag / AgCl reference electrode installed in a pH adjustment tank. Other steps and parameters are the same as those in specific implementation method 1.

[0043] In this embodiment, the Ag / AgCl reference electrode is filled with a 0.1 M saturated potassium chloride solution.

[0044] Specific embodiment 7: This embodiment is different from the specific embodiment 1 in that the degradation negative electrode in step 2 is a rectangular boron-doped diamond electrode with a specification of 5 cm per 2 The active area contains 20 mg of active material. Other steps and parameters are the same as those in the first embodiment.

[0045] Specific embodiment eight: This embodiment differs from specific embodiment one in that the lithium-rich positive electrode obtained in step three is continuously reused in the electrode recovery pool, and steps two and three are cycled 5 to 10 times to complete the reuse of the lithium-rich positive electrode. The other steps and parameters are the same as those in specific embodiment one.

[0046] Specific embodiment 9: This embodiment differs from specific embodiment 1 in that the lithium-rich solution obtained in step 3 is the recovered lithium ions. The other steps and parameters are the same as those in specific embodiment 1.

[0047] The beneficial effects of the present invention are verified by the following examples:

[0048] Example:

[0049] A method for recycling and treating lithium battery disassembly and recycling wastewater, which is carried out according to the following steps:

[0050] 1. Preparation of lithium-rich cathode:

[0051] The lithium manganese oxide powder, carbon black and polytetrafluoroethylene are mixed and calcined to obtain a lithium manganese oxide composite electrode, which is then placed in a lithium-based phosphate buffer solution and a stainless steel negative electrode, and a constant current is applied until the potential reaches 2.5V to obtain a λ-MnO2 positive electrode, which is a lithium-rich positive electrode;

[0052] 2. The lithium-containing wastewater enters the pH adjustment tank, and 1M NaOH is added to adjust the pH value to 6.6-6.7. After stirring for 2 hours, it is allowed to stand for 3 hours. The resulting supernatant is the wastewater solution, which is then transferred to the electrode recovery tank, and the lithium-rich positive electrode and degraded negative electrode prepared in step 1 are placed, and then 100 mA·h·g –1 A constant current is generated and the current flows from the positive electrode to the negative electrode until the potential of the lithium-rich positive electrode reaches 1.5V, thereby obtaining a lithium manganese oxide composite electrode, and degrading the negative electrode to produce hydroxyl radicals to degrade organic matter in the wastewater solution, and the generated wastewater enters the existing biological treatment section;

[0053] 3. The lithium manganese oxide composite electrode obtained in step 2 is placed in an electrode release cell, a lithium-based phosphate buffer solution is poured in, a stainless steel negative electrode is placed, and then 100 mA·h·g –1 A constant current is supplied from the negative electrode to the positive electrode until the potential of the lithium manganese oxide composite electrode reaches 1.5 V, thereby obtaining a lithium-rich positive electrode and a lithium-rich solution, thereby completing the method for recycling and treating lithium battery disassembly and recycling wastewater.

[0054] In step 1 of this embodiment, the volume percentage of lithium manganese oxide powder, carbon black and polytetrafluoroethylene is 80:10:10.

[0055] Calcination in step 1 of this embodiment: calcination at 400°C for 8h.

[0056] The lithium-rich positive electrode in step 1 of this embodiment is rectangular in shape and has a size of 20 cm 2 The active area contains 1000 mg of active material.

[0057] The concentration of the lithium-based phosphate buffer solution in step 1 of this embodiment is 100 mM, and the pH value is 7.2; the lithium-based phosphate buffer solution is prepared by adding 1 mol of methyl methacrylate, 1 mmol of lithium phosphate and 1 mol of lithium fluorophosphate to 500 ml of phosphoric acid aqueous solution, then heating to 90° C. and stirring for 10 min.

[0058] The degradation negative electrode in step 2 of this embodiment is a rectangular boron-doped diamond electrode with a specification of 5 cm 2 The active area contains 20 mg of active material.

[0059] The lithium-rich solution obtained in step 3 of this embodiment is the recovered lithium ions.

[0060] The lithium-containing wastewater in step 2 of this embodiment comes from Shenzhen, Guangdong. The company mainly performs acid leaching on the negative electrode of waste batteries and then collects the metal ions therein by solvent extraction. The water quality of the lithium-containing wastewater is shown in Table 1

[0061] Table 1 Water quality of lithium-containing wastewater

[0062] Li+ <![CDATA[Na + ]]> <![CDATA[Ni + ]]> DOC concentration 2015mg / L 32518mg / L 512mg / L 289mg / L

[0063] The lithium-rich positive electrode obtained in step 3 of this embodiment is continuously reused in the electrode recovery pool, and steps 2 and 3 are cycled for 5 times (i.e., five recovery cycles), completing the reuse of the lithium-rich positive electrode; after completing these five recovery cycles, an ion detector and a total organic carbon analyzer are used to measure the changes in the ion concentration recovered by the electrode and the ratio of organic matter in the wastewater to the initial organic matter concentration in these five cycles. The increase in the lithium ion concentration in the electrode recovery pool is as follows: Figure 1 As shown, from Figure 1 It can be clearly seen that the concentration of lithium ions in the recovery pool increases after each cycle, but the increase in ions in the first cycle is the highest. Despite multiple cycles, the electrode still has a high lithium ion recovery rate, which shows that the present invention has the advantages of high sustainability and high recovery rate.

[0064] Figure 2 As shown, the DOC in the lithium-containing wastewater gradually decreased and decreased by 65% ​​after five operation cycles, although there was a large deviation between the measured values, which was caused by the organic impact and complexity of the actual wastewater. This result shows that the present invention is very effective for the simultaneous recovery of lithium and removal of organic pollutants.

[0065] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for recycling and treating lithium battery disassembly and recycling wastewater, characterized in that It is implemented as follows:

1. Preparation of lithium-rich cathode: The lithium manganese oxide powder, carbon black and polytetrafluoroethylene are mixed and calcined to obtain a lithium manganese oxide composite electrode, which is then placed in a lithium-based phosphate buffer solution and a stainless steel negative electrode, and a constant current is applied until the potential reaches 2.5V to obtain a λ-MnO2 positive electrode, which is a lithium-rich positive electrode; 2. The lithium-containing wastewater enters the pH adjustment tank, and 1M NaOH is added to adjust the pH value to 6.6-6.

7. After stirring for 2 hours, it is allowed to stand for 3 hours. The resulting supernatant is the wastewater solution, which is then transferred to the electrode recovery tank, and the lithium-rich positive electrode and degraded negative electrode prepared in step 1 are placed, and then 100 mA·h·g –1 A constant current is generated and the current flows from the positive electrode to the negative electrode until the potential of the lithium-rich positive electrode reaches 1.5V, thereby obtaining a lithium manganese oxide composite electrode, and degrading the negative electrode to produce hydroxyl radicals to degrade organic matter in the wastewater solution, and the generated wastewater enters the existing biological treatment section; 3. The lithium manganese oxide composite electrode obtained in step 2 is placed in an electrode release cell, a lithium-based phosphate buffer solution is poured in, a stainless steel negative electrode is placed, and then 100 mA·h·g –1 A constant current is supplied from the negative electrode to the positive electrode until the potential of the lithium manganese oxide composite electrode reaches 1.5 V, thereby obtaining a lithium-rich positive electrode and a lithium-rich solution, thereby completing the method for recycling and treating lithium battery disassembly and recycling wastewater.

2. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that The volume percentage of the lithium manganese oxide powder, carbon black and polytetrafluoroethylene in step 1 is 80:10:

10.

3. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that Calcination in step 1: calcination at 400°C for 8h.

4. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that The lithium-rich positive electrode in step 1 is rectangular in shape, with a specification of 20 cm per 2 The active area contains 1000 mg of active material.

5. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that Step 1: The concentration of the lithium-based phosphate buffer solution is 100 mM, and the pH value is 7.2; Preparation of the lithium-based phosphate buffer solution: add 1 mol of methyl methacrylate, 1 mmol of lithium phosphate and 1 mol of lithium fluorophosphate to 500 ml of phosphoric acid aqueous solution, then heat to 90°C and stir for 10 minutes.

6. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that Indicators of lithium-containing wastewater in step 2: Redox potential ORP is +100mV, which is detected by an Ag / AgCl reference electrode installed in a pH adjustment tank.

7. A method for recycling and treating lithium battery disassembly and recycling wastewater according to claim 1, characterized in that The degradation negative electrode in step 2 is a rectangular boron-doped diamond electrode with a specification of 5 cm per 2 The active area contains 20 mg of active material.

8. The method for recycling and treating lithium battery disassembly wastewater according to claim 1, characterized in that The lithium-rich positive electrode obtained in step three is continuously reused in the electrode recovery pool, and steps two and three are cycled 5 to 10 times to complete the reuse of the lithium-rich positive electrode.

9. The method for recycling and treating lithium battery disassembly wastewater according to claim 1, characterized in that The lithium-rich solution obtained in step 3 is the recovered lithium ions.

Citation Information

Patent Citations

  • Lithium battery electrolyte production wastewater treatment and resource recovery method

    CN115259485A

  • Pretreatment method for improving performance of positive electrode material in regeneration process of battery material

    CN117374443A

  • Method for treating wastewater of waste lithium ion battery

    WO2021125633A2