Diffusion film and manufacturing method thereof
By adopting a diffusion particle design with a combination of multi-layer structure and a specific particle size in the diffusion film, the problem of flashing in high-definition display is solved, and the combination of high brightness and high shading is achieved, which improves the purity of the display effect and clarity.
Patent Information
- Application Number
- CN202411014353.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-08
AI Technical Summary
Under high-definition display, traditional diffusion films often flash on green pictures, making it difficult to significantly improve shielding while ensuring high brightness. The production process requirements are high, which can easily lead to performance failure.
A diffusion film design adopts a multi-layer structure, in which a first diffusion layer with monodispersed particle size and a second diffusion layer with dispersed particle size are formed on the substrate layer. Combined with diffusion particles of different particle sizes, the particle size and concentration are precisely controlled. , optimize light scattering and reflection to eliminate flashing phenomenon.
It has achieved significant improvement in shading while maintaining high brightness, eliminated flashing, improved the purity and clarity of the display effect, reduced production costs, and enhanced product consistency and stability.
Smart Images

Figure CN118915210A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of display technology, and in particular to a diffusion film and a method for manufacturing the same. Background Art
[0002] With the rapid development of display technology, especially with the widespread application of smart terminal products such as smart phones, iPads, Mini computers and MNT (Monitor, Notebook, Tablet), the requirements for display quality are increasing. Among them, the diffusion film, as a key component of the backlight source of the LCD module, plays a vital role in improving the display effect. However, in the current display technology, especially for high-definition (such as 4K) mirror LCM (Liquid Crystal Module) driving, the sparkling phenomenon that often appears on the green screen has become a technical problem that needs to be solved urgently. The traditional diffusion film structure usually includes a substrate layer (such as PET, with a thickness of 50um~250um) and an optical coating coated on its surface. In order to improve the wear and scratch resistance, many products also introduce additional protective coatings. The design of the diffusion film on the double-sided particles, that is, the upper diffusion film includes the front coating, PET substrate layer, and back coating from bottom to top, is the product of this trend. This design aims to improve optical performance and physical durability through the optimization of the multi-layer structure.
[0003] Although the double-sided particle diffuser film performs well in improving wear resistance and scratch resistance, it still faces many challenges in dealing with the flash phenomenon under high-definition display: the flash phenomenon is mainly caused by excessive product brightness and poor shielding. Although improving the shielding of the diffuser film can effectively reduce the scattering and reflection of light, it is often accompanied by a significant reduction in brightness, thus affecting the overall display effect. On the contrary, if high brightness is pursued, it is difficult to effectively eliminate the flash phenomenon. In order to eliminate the flash phenomenon of the green screen under the 4K mirror LCM drive, the positive coating of the upper diffuser film needs to accurately control the mixing ratio and distribution of multiple particles. This process has extremely high requirements for the production process. Any slight deviation may cause the product performance to fail to meet the standards.
[0004] The main bottleneck faced by front diffuser products in solving the flash phenomenon is how to significantly improve the shielding while ensuring high brightness, and taking into account physical properties such as wear resistance and scratch resistance. In addition, how to optimize the process of particle mixing, reduce production costs, and improve product consistency and stability are also technical issues that need to be solved urgently. Summary of the invention
[0005] The purpose of the present application is to provide a diffusion film that can eliminate the flash phenomenon so that the product can meet both the brightness requirements and the shielding requirements. The diffusion film of the present application includes: A substrate layer, a first diffusion layer on the front side of the substrate layer, and a second diffusion layer on the first diffusion layer; The first diffusion layer includes first diffusion particles with monodispersed particle sizes, and the second diffusion layer includes second diffusion particles with medium particle sizes and third diffusion particles with monodispersed particle sizes; The particle size of the first diffusion particles is smaller than the particle sizes of the second diffusion particles and the third diffusion particles.
[0006] In one embodiment, the particle size of the first diffusion particles is in the range of 2-2.5 μm, the particle size of the second diffusion particles is in the range of 4-6 μm, and the particle size of the third diffusion particles is in the range of 5-5.5 μm.
[0007] In one embodiment, the average particle size of the second diffusion particles is 5 μm.
[0008] In one of the embodiments, it further comprises an anti-scratch layer, wherein the anti-scratch layer is disposed on a side of the substrate layer opposite to the first diffusion layer.
[0009] In one embodiment, the anti-scratch layer includes soft particles, and the particle size of the soft particles is in the range of 5-8 μm.
[0010] In one embodiment, the soft particles are PU particles or PBMA particles.
[0011] In one embodiment, the diffusion particle material is selected from one or more of the following materials: PMMA, PBMA, PU, barium sulfate, calcium carbonate, silicon dioxide or titanium dioxide.
[0012] In one embodiment, the second diffusion particles are high refractive index particles, and the refractive index is in the range of 1.61-1.67.
[0013] In one embodiment, the concentration of the first diffusion particles is 0.3-0.45 g / m 2 In the range of 0.3-0.45 g / m 2 In the range of 0.45-0.7 g / m 2 within the range.
[0014] In addition, the present application also provides a method for manufacturing a diffusion film, comprising: Prepare a first coating material including first diffusion particles with monodispersed particle sizes, and apply the first coating material on the substrate layer to form a first diffusion layer; preparing a second coating material including second diffusion particles dispersed in medium particle sizes and third diffusion particles monodispersed in particle sizes, and coating the second coating material on the first diffusion layer to form a second diffusion layer; The particle size of the first diffusion particles is smaller than the particle sizes of the second diffusion particles and the third diffusion particles.
[0015] Compared with the prior art, the present application has the following beneficial effects: the multi-layer structure diffusion film proposed in the present application, through a combination of multiple diffusion layers and diffusion particles of specific particle size and concentration, the diffusion film introduces two diffusion layers, wherein the first diffusion layer adopts small-size first diffusion particles with monodisperse particle size, which can evenly scatter light and reduce bright spots caused by direct penetration of light; the second diffusion layer combines second diffusion particles dispersed in the particle size and third diffusion particles with monodisperse particle size, and through the difference in particle size and distribution optimization, further refines and homogenizes the light distribution, effectively suppresses the scattering and reflection of light on the interface, thereby completely eliminating the flash phenomenon on the green screen and ensuring the purity and clarity of the picture. By precisely controlling the particle size, concentration and distribution of each layer of diffusion particles, the present application significantly enhances the shielding property while maintaining a high brightness. The small-size particles in the first diffusion layer reduce scattering losses while ensuring light transmission; and the combination of medium-dispersed and monodispersed particles in the second diffusion layer further refines the light distribution through a multiple scattering mechanism, making the light softer and more uniform, which not only retains sufficient brightness but also effectively shields unnecessary scattered light. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 is a schematic diagram of the structure of a diffusion membrane in one embodiment of the present application; Figure 2 It is a schematic diagram of the structure of a diffusion membrane in another embodiment of the present application.
[0017] Explanation of reference numerals: 100, substrate layer; 210, first diffusion layer; 220, second diffusion layer; 310, first diffusion particles; 320, second diffusion particles; 330, third diffusion particles; 400, anti-scratch layer. DETAILED DESCRIPTION
[0018] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. It is to be understood that the specific embodiments described herein are only used to explain the present application, rather than to limit the present application. It should also be noted that, for ease of description, only some structures related to the present application are shown in the accompanying drawings, rather than all structures. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0019] The terms "including" and "having" and any variations thereof in this application are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device comprising a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products or devices.
[0020] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0021] See also Figure 1 to Figure 2 As shown, a diffusion film in a preferred embodiment of the present application is suitable for enhancing shielding properties while maintaining a high brightness, and can avoid flashing. The diffusion film includes: A substrate layer 100, a first diffusion layer 210 on the front side of the substrate layer 100, and a second diffusion layer 220 on the first diffusion layer 210; The first diffusion layer 210 includes first diffusion particles 310 with monodisperse particle sizes, and the second diffusion layer 220 includes second diffusion particles 320 with medium particle sizes and third diffusion particles 330 with monodisperse particle sizes. Monodisperse particle sizes in the present application refer to particles having the same particle sizes, and medium particle sizes refer to particles having particle sizes distributed within a range, and the particle sizes have a distribution interval.
[0022] The particle size of the first diffusion particles 310 is smaller than the particle sizes of the second diffusion particles 320 and the third diffusion particles 330 .
[0023] The diffusion film structure of the present application is constructed by multiple layers, including a stable substrate layer 100, which serves as the support foundation of the entire film structure. On the front of the substrate layer 100, a first diffusion layer 210 is first covered, in which tiny first diffusion particles 310 with uniform particle size are evenly distributed. These particles preliminarily achieve the initial scattering and homogenization of light when entering the film layer. On top of the first diffusion layer 210, a second diffusion layer 220 is formed, which combines the second diffusion particles 320 dispersed in the particle size and the third diffusion particles 330 with uniform particle size. The particle sizes of both are larger than the first diffusion particles 310, which further enhances the scattering effect of light, optimizes the uniformity of light distribution, reduces the flash phenomenon, and improves the visual experience.
[0024] By introducing diffusion particles of different sizes and arranging them in layers, the scattering frequency and range of light passing through the diffusion film are effectively improved, so that the light can be more evenly distributed on the entire light-emitting surface, avoiding glare or dark area problems caused by light concentration, thereby significantly improving the display effect of the display or lighting equipment. The combined use of the monodisperse first diffusion particles 310 and the second and third diffusion particles 330, especially the monodisperse and medium-dispersed characteristics, can effectively reduce the defects caused by light interference and improve the clarity and fineness of the image. By precisely controlling the distribution and particle size of the diffusion particles, it is possible to reduce unnecessary energy losses while ensuring the light scattering effect, thereby improving the energy efficiency of the entire optical system.
[0025] Specifically, the particle size of the first diffusion particles 310 is in the range of 2-2.5 μm, the particle size of the second diffusion particles 320 is in the range of 4-6 μm, and the particle size of the third diffusion particles 330 is in the range of 5-5.5 μm. The first diffusion particles 310 are prepared by a particle size control process, and their particle size is controlled in the range of 2-2.5 μm. The particle size of the above size can effectively reduce the non-uniformity in light scattering and improve the light transmission efficiency and directionality. The second diffusion particles 320 have a particle size distribution in the range of 4-6 μm, and the light scattering effect is enhanced by the particle size gradient. The product brightness can be further improved by the dispersed particles, so that the product brightness meets the requirements.
[0026] Specifically, the average particle size of the second diffusion particles 320 is 5 μm. The average particle size is selected to be 5 μm. This selection not only takes into account the interaction between particles and its influence on the light scattering effect, but also takes into account the uniformity, light transmittance and cost-effectiveness of the entire material.
[0027] Specifically, it also includes an anti-scratch layer 400, which is arranged on the side of the substrate layer 100 opposite to the first diffusion layer 210. In addition to the multi-layer diffusion particle layer, the anti-scratch layer 400 is introduced as a key component, and the anti-scratch layer 400 is arranged on the other side of the substrate layer 100 opposite to the first diffusion layer 210, that is, the side facing the external environment. This setting not only enhances the physical protection ability of the diffusion membrane, but also prolongs its service life.
[0028] Specifically, the anti-scratch layer 400 includes soft particles, and the particle size of the soft particles is in the range of 5-8 μm. In the composition of the anti-scratch layer 400, uniformly distributed soft particles are introduced. These particles serve as key buffering and lubricating elements, and their particle size is precisely controlled in the range of 5-8 μm. This particle size selection is based on the comprehensive consideration of the material surface hardness, wear resistance, transparency and processing performance.
[0029] Specifically, the soft particles are PU particles or PBMA particles. In the anti-scratch layer 400, high-performance PU (polyurethane) particles or PBMA (polybutyl methacrylate) particles are selected as soft components. These particles, with their unique physical and chemical properties, provide the coating with excellent scratch resistance, flexibility and transparency under the precise control of particle size of 5-8μm.
[0030] Specifically, the material forming the diffusion particles is selected from one or more of the following materials: PMMA, PBMA, PU, barium sulfate, calcium carbonate, silicon dioxide or titanium dioxide.
[0031] Specifically, the second diffusion particles 320 are high refractive index particles with a refractive index in the range of 1.61-1.67. By increasing the refractive index of the particles, the scattering effect and optical performance of the coating are further enhanced, while ensuring the visual uniformity and clarity of the coating. The high refractive index particles can scatter light more effectively, causing the light to be reflected and refracted more times inside the coating, which helps to improve the brightness, contrast and color saturation of the product, ensuring that the coating achieves a more uniform light distribution while maintaining a high light transmittance. By reasonably matching the high refractive index particles with other particles, the overall structure of the coating can be further optimized and the overall performance of the coating can be improved.
[0032] Specifically, the concentration of the first diffusion particles 310 is 0.3-0.45 g / m 2 In the range of 0.3-0.45 g / m 2 In the range of 0.45-0.7 g / m 2 The concentration of the first diffusion particles 310 is set between 0.3 and 0.45 grams per square meter (g / m²), the concentration of the second diffusion particles 320 (high refractive index particles) is also controlled in the range of 0.3 to 0.45 g / m², and the concentration of the third diffusion particles 330 is slightly higher, between 0.45 and 0.7 g / m². This concentration ratio is designed to achieve the best balance of coating performance, including light scattering effect, light transmittance, color performance, and overall aesthetics and durability. Reasonable particle concentration distribution helps reduce visual defects on the coating surface. By setting the concentration range of different diffusion particles, we provide greater flexibility for the customized design of the coating. According to different application requirements and performance goals, the concentration ratio of each particle can be flexibly adjusted to achieve the best overall performance.
[0033] In addition, the present application also provides a method for manufacturing a diffusion film, comprising: Prepare a first coating material including first diffusion particles 310 with monodispersed particle sizes, and apply the first coating material on the substrate layer 100 to form a first diffusion layer 210; Prepare a second coating material including second diffusion particles 320 dispersed in medium particle sizes and third diffusion particles 330 with monodispersed particle sizes, and apply the second coating material on the first diffusion layer 210 to form a second diffusion layer 220; The particle size of the first diffusion particle 310 is smaller than that of the second diffusion particle 320 and the third diffusion particle 330. The particle size, material, concentration and other distributions of each particle are consistent with the above-mentioned setting method, so they are not repeated in the introduction of the method-related content. Specific embodiments In embodiment 1, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PU particles with a particle size of 2 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer includes PU particles with a particle size distribution of 4-6 μm, wherein the average particle size is 5 μm, and PBMA particles with a particle size of 5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PU particles with a particle size of 5 μm.
[0035] In embodiment 2, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PU particles with a particle size of 2.5 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer includes PU particles with a particle size distribution of 4-6 μm, wherein the average particle size is 4.5 μm, and PBMA particles with a particle size of 5.5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PU particles with a particle size of 8 μm.
[0036] In embodiment three, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PBMA particles with a particle size of 2 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer includes PBMA particles with a particle size distribution of 6 μm, wherein the average particle size is 5 μm, and PU particles with a particle size of 5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PBMA particles with a particle size of 5 μm.
[0037] In embodiment 4, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PBMA particles with a particle size of 2.5 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer includes PBMA particles with a particle size distribution of 4-6 μm, wherein the average particle size is 5.5 μm, and PU particles with a particle size of 5.5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PBMA particles with a particle size of 8 μm.
[0038] In Example 5, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PU particles with a particle size of 2 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer includes PBMA particles with a particle size distribution of 4-6 μm, wherein the average particle size is 5 μm, and PU particles with a particle size of 5.5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PBMA particles with a particle size of 7 μm.
[0039] In comparative example 1, only a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PU particles with a particle size of 2 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PU particles with a particle size of 5 μm.
[0040] In comparative example 2, only a second diffusion layer is formed on the surface of the PET substrate layer, the second diffusion layer includes PU particles with a particle size distribution of 4-6 μm, wherein the average particle size is 5 μm, and the third PBMA particles with a particle size of 5 μm. An anti-scratch layer is formed on the back of the PET substrate layer, and the anti-scratch layer contains PBMA particles with a particle size of 8 μm.
[0041] In comparative example three, a first diffusion layer is formed on the surface of the PET substrate layer, the first diffusion layer includes PU particles with a particle size of 2.5 μm, a second diffusion layer is formed on the first diffusion layer, the second diffusion layer only includes PU particles with a particle size distribution of 4-6 μm, wherein the average particle size is 5 μm, and an anti-scratch layer is formed on the back of the PET substrate layer, the anti-scratch layer contains PU particles or PBMA particles with a particle size of 5-8 μm.
[0042] Table 1 Statistical table of test results of embodiments and comparative examples From the above content, it can be seen that the flash phenomenon cannot be avoided by forming the first diffusion layer or the second diffusion layer alone. When the second diffusion layer only includes medium-dispersed diffusion particles, the brightness is lower than that of the embodiment including both medium-dispersed and monodispersed diffusion particles. Therefore, it can be seen that the two diffusion layers of the present application and the technical solution of simultaneously including medium-dispersed and monodispersed diffusion particles in the second diffusion layer can reduce the flash phenomenon while maintaining a high brightness.
[0043] From the foregoing, it can be seen that the present application proposes an innovatively designed multi-layer structure diffusion membrane, which achieves a delicate balance between light scattering and transmission through a carefully constructed multi-layer diffusion layer system and a combination of diffusion particles of specific particle size and concentration, thereby significantly improving the purity, clarity and brightness of the display image.
[0044] Specifically, the diffusion film introduces two diffusion layers, each of which carries different optical roles and functional optimizations. The first diffusion layer uses small-sized first diffusion particles with monodispersed particle size. These tiny and uniform particles can serve as the pre-scattering center of light, effectively disperse the incident light, and reduce the bright spot phenomenon caused by the light directly penetrating the coating. At the same time, the small-sized particles minimize the scattering loss while ensuring the light transmission, ensuring the brightness of the picture. The second diffusion layer adopts a particle size combination strategy, combining the second diffusion particles with medium particle size and the third diffusion particles with monodispersed particle size. Through the carefully designed particle size difference and distribution optimization, the light scattering is further refined and uniformed. The synergistic effect of the medium-dispersed particles and the monodispersed particles constructs a multi-level light scattering network, which effectively suppresses the irregular scattering and reflection of light on the interface, completely eliminates the flash phenomenon commonly seen on the green screen, and ensures the purity of the picture. In addition, this multiple scattering mechanism also makes the light distribution softer and more uniform, which not only retains sufficient brightness, but also effectively shields unnecessary scattered light, improving the overall visual effect of the picture.
[0045] The above is only a specific implementation of the present application, and any other improvements made based on the concept of the present application are deemed to be within the protection scope of the present application.
Claims
1. A diffusion film, It is characterized in that include: A substrate layer (100), a first diffusion layer (210) on the front side of the substrate layer (100), and a second diffusion layer (220) on the first diffusion layer (210); The first diffusion layer (210) includes first diffusion particles (310) with a monodisperse particle size, and the second diffusion layer (220) includes second diffusion particles (320) dispersed in a medium particle size and third diffusion particles (330) with a monodisperse particle size; The particle size of the first diffusion particles (310) is smaller than the particle sizes of the second diffusion particles (320) and the third diffusion particles (330).
2. The diffusion membrane according to claim 1, It is characterized in that The particle size of the first diffusion particles (310) is within the range of 2-2.5 μm, the particle size of the second diffusion particles (320) is within the range of 4-6 μm, and the particle size of the third diffusion particles (330) is within the range of 5-5.5 μm.
3. The diffusion membrane according to claim 2, It is characterized in that The average particle size of the second diffusion particles (320) is 5 μm.
4. The diffusion membrane according to claim 1, It is characterized in that It also includes an anti-scratch layer (400), wherein the anti-scratch layer (400) is arranged on a surface of the substrate layer (100) opposite to the first diffusion layer (210).
5. The diffusion membrane according to claim 4, It is characterized in that The anti-scratch layer (400) comprises soft particles, and the particle size of the soft particles is in the range of 5-8 μm.
6. The diffusion membrane according to claim 5, It is characterized in that The soft particles are PU particles or PBMA particles.
7. The diffusion membrane according to claim 1, It is characterized in that The material forming the diffusion particles is selected from one or more of the following materials: PMMA, PBMA, PU, barium sulfate, calcium carbonate, silicon dioxide or titanium dioxide.
8. The diffusion membrane according to claim 1, It is characterized in that The second diffusion particles (320) are high refractive index particles, and the refractive index is in the range of 1.61-1.
67.
9. The diffusion membrane according to claim 1, It is characterized in that The concentration of the first diffusion particles (310) is between 0.3 and 0.45 g / m 2 In the range of 0.3-0.45 g / m 2 In the range of 0.45-0.7 g / m 2 within the range.
10. A method for manufacturing a diffusion film, It is characterized in that include: Prepare a first coating material including first diffusion particles (310) with monodispersed particle sizes, and apply the first coating material on a substrate layer (100) to form a first diffusion layer (210); preparing a second coating material comprising second diffusion particles (320) dispersed in medium particle sizes and third diffusion particles (330) with monodispersed particle sizes, and coating the second coating material on the first diffusion layer (210) to form a second diffusion layer (220); The particle size of the first diffusion particles (310) is smaller than the particle sizes of the second diffusion particles (320) and the third diffusion particles (330).