Battery pack

By designing a sealing structure with prone to cracking in the battery pack, the abnormal chain problem caused by short circuit in the laminated unit is solved, the smooth discharge of gas and stable isolation of the unit is achieved, and the safety and reliability of the battery pack are improved.

CN118920002APending Publication Date: 2024-11-08PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411011589.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2021-02-18
Filing Date
2022-02-17
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

When the existing laminated unit is short-circuited internally, the sealing portion may crack, causing gas to eject, which may cause abnormal chaining of adjacent units, causing heat accumulation and further failure.

Method used

A battery pack is designed in which the sealing portion of each unit is divided into three regions, the second region has a crack-prone portion for first cracking when the temperature and internal pressure rise, thereby preventing gas accumulation and propagation and reducing abnormalities. Possibility of chain. The cracking part can be achieved by using a low melting point resin or a rough surface, and the cracking part can be arranged in the exhaust pipe to facilitate gas discharge.

Benefits of technology

The abnormal chaining of units is effectively prevented. By controlling the position and direction of gas ejection, the heating risk of adjacent units is reduced, and the stability and safety of the battery pack are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118920002A_ABST
    Figure CN118920002A_ABST
Patent Text Reader

Abstract

The purpose of the present invention is to provide a battery pack in which cell abnormalities are difficult to interlock. The battery pack includes modules. The module comprises more than one unit pair. The cell pair includes a first cell and a second cell. The first unit includes an exterior body, an electrode body, and an electrode terminal. The electrode terminal includes a first main surface and a second main surface. The first main surface faces the direction of the second unit. A sealing part is formed on the periphery of the exterior body. The sealing portion includes a first region, a second region, and a third region. The first region is formed between the first main surface and the resin layer. The second region is formed between the second main surface and the resin layer. The third region is formed between the resin layers. The second region includes an easy-to-crack portion.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of the invention patent application named "Battery Pack", filed on February 17, 2022, and with application number 202210143887.4. Technical Field

[0002] The present technology relates to a battery pack. Background Art

[0003] Japanese Patent Application Laid-Open No. 2003-346768 discloses a lamination unit.

[0004] As the outer casing of a single cell (unit), a laminate film is used. The laminate film includes a resin layer and a metal layer. The resin layer covers the metal layer. The laminate film is processed into a bag, for example. A sealing portion is formed at the periphery of the bag by welding the resin layer. The outer casing is sealed by forming the sealing portion. A unit including an outer casing made of a laminate film is also called a "laminated unit".

[0005] A module is formed by electrically connecting two or more cells. In a module, two or more cells can form a series circuit or a parallel circuit. A battery pack is formed using one or more modules.

[0006] In the module, it is assumed that an abnormality occurs in one unit. For example, it is assumed that an internal short circuit occurs in one unit. Due to the internal short circuit, the temperature of the unit may rise. In addition, gas may be generated inside the unit. Due to at least one of the temperature rise and the internal pressure rise, the sealing portion of the outer body may rupture. Due to the rupture of the sealing portion, gas may be ejected from the outer body.

[0007] In the conventional laminated units, the cracking position of the seal may be random. For example, between adjacent units, gas may be ejected to a position where gas is easily gathered. The gas may be high temperature. Due to the gathering of high temperature gas, the adjacent unit may be heated. Due to the heating of adjacent units, abnormal chain reactions may occur. Summary of the invention

[0008] Problems to be solved by the invention

[0009] An object of the present invention is to provide a battery pack in which abnormalities of cells are unlikely to be interlocked.

[0010] The structure and effects of the present technology are described below. However, the mechanism of action in this specification includes assumptions. The mechanism of action does not limit the scope of the present technology.

[0011] [1] A battery pack includes a module. The module includes one or more cell pairs. The cell pairs include a first cell and a second cell. The second cell is adjacent to the first cell. The second cell is electrically connected to the first cell.

[0012] The first unit includes an outer casing, an electrode body, and an electrode terminal. The outer casing includes a laminate film. The laminate film includes a resin layer and a metal layer. The resin layer covers the metal layer. The resin layer includes a first thermoplastic resin. The outer casing accommodates the electrode body. A sealing portion is formed at the periphery of the outer casing. The electrode terminal is connected to the electrode body. The electrode terminal passes through the sealing portion and is led out from the inside of the outer casing to the outside.

[0013] The electrode terminal is in the shape of a plate. The electrode terminal includes a first main surface and a second main surface. The first main surface faces the direction of the second unit. The second main surface is the opposite surface of the first main surface.

[0014] The sealing portion includes a first region, a second region, and a third region. The first region is formed between the first main surface and the resin layer. The second region is formed between the second main surface and the resin layer. The third region is formed between the resin layers.

[0015] The second region includes an easily breakable portion. The easily breakable portion is configured to break more easily than the first region and the third region when at least one of the temperature and the internal pressure of the first unit increases.

[0016] The module of the present technology includes two or more laminated units. Two laminated units constitute a unit pair. The unit pair includes a first unit (also simply referred to as a "unit") and a second unit (also referred to as an "adjacent unit"). The unit pair forms a series circuit or a parallel circuit.

[0017] The sealing portion of the unit can be divided into a first area, a second area, and a third area according to the relationship with the electrode terminal. The second area includes an easily cracked portion. The easily cracked portion functions as an explosion-proof valve. That is, the easily cracked portion is easier to crack than the first area and the third area in an abnormality. Gas is ejected from the easily cracked portion by the cracking of the easily cracked portion. Since the ejection position of the gas is in the second area, it can be expected that the abnormality of the unit is difficult to be chained.

[0018] Figure 1 This is a schematic diagram showing the flow of gas when the gas is ejected from the first region.

[0019] The electrode terminal 30a of the first unit 100a is electrically connected to the electrode terminal 30b of the second unit 100b (adjacent unit). The electrode terminal 30a may also be directly connected to the electrode terminal 30b. The bus bar 150 may also connect the electrode terminal 30a to the electrode terminal 30b. By connecting the electrode terminal 30a to the electrode terminal 30b, a partially closed space can be formed. The first region 13a faces the adjacent unit. It is considered that if gas is ejected from the first region 13a during an abnormality, the gas is likely to flow in the direction of the adjacent unit. Moreover, it is considered that the gas is likely to gather in a closed space. Since the adjacent unit is heated, the abnormality may be chained in the adjacent unit.

[0020] Figure 2 This is a schematic diagram showing the flow of gas when the gas is ejected from the third region.

[0021] The gas ejected from the third region 13c is likely to diffuse in multiple directions. Since the gas diffuses in multiple directions, it is possible to heat multiple units. Moreover, it is considered that the gas ejected from the third region 13c is likely to flow toward the storage portion of the electrode body. As a result, the abnormality may be chained in multiple units.

[0022] Figure 3 It is a schematic diagram showing the flow of gas when the gas is ejected from the second region.

[0023] The second region 13b is located on the opposite side of the first region 13a. By connecting the electrode terminal 30a and the electrode terminal 30b, a partially enclosed space is formed on the first region 13a side. On the other hand, on the second region 13b side, the space is not enclosed. It can be considered that the gas ejected from the second region 13b tends to flow in one direction. It can be considered that this is because the first region 13a side is enclosed. Moreover, since the space on the second region 13b side is not enclosed, it can be considered that the gas is difficult to gather. In addition, it can be considered that the gas ejected from the second region 13b tends to flow in a direction away from the storage portion of the electrode body 20. Therefore, since the gas is ejected from the second region 13b, it can be expected that the abnormality of the unit is difficult to be chained.

[0024] [2] In the battery pack described in [1] above, for example, the first main surface may include a rough surface portion.

[0025] In the rough surface, an anchoring effect can be generated. The anchoring effect can increase the bonding strength. Since the first region includes the rough surface, the first region can have a higher bonding strength than the second region. That is, the second region has a relatively low bonding strength. Since the second region has a relatively low bonding strength, an easy-to-crack portion can be formed in the second region. It can be expected that the easy-to-crack portion will crack when the internal pressure rises, for example.

[0026] [3] In the battery pack described in [1] or [2] above, the easily breakable portion may include a second thermoplastic resin. The second thermoplastic resin may have a lower melting point than the first thermoplastic resin.

[0027] When the temperature rises, the second thermoplastic resin can soften earlier than the first thermoplastic resin. For example, the easily cleavable portion including the second thermoplastic resin can be expected to cleave when the temperature rises.

[0028] [4] In the battery pack described in any one of [1] to [3] above, for example, it may further include a container. The container accommodates the module. An exhaust duct is formed inside the container. An easy-to-break portion is arranged inside the exhaust duct.

[0029] In the present technology, it is assumed that gas will be ejected from the easily ruptured portion in an abnormal situation. By arranging the easily ruptured portion inside the exhaust duct, the gas ejected from the easily ruptured portion can be smoothly discharged to the outside of the container.

[0030] [5] The module may include, for example, two or more unit pairs. In each of the two or more unit pairs, the easily breakable portion may be disposed inside the exhaust duct.

[0031] When the battery pack includes a plurality of easy-break portions, the exhaust duct may be arranged so that each easy-break portion is arranged inside the exhaust duct.

[0032] The foregoing and other objects, features, aspects and advantages of the present technology will become more apparent from the following detailed description of the present technology when read in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 This is a schematic diagram showing the flow of gas when the gas is ejected from the first region.

[0034] Figure 2 This is a schematic diagram showing the flow of gas when the gas is ejected from the third region.

[0035] Figure 3 It is a schematic diagram showing the flow of gas when the gas is ejected from the second region.

[0036] Figure 4 This is a schematic diagram of a battery pack in this embodiment.

[0037] Figure 5 It is a schematic cross-sectional view of the battery pack in this embodiment.

[0038] Figure 6 yes Figure 5 Magnified view of region VI in FIG.

[0039] Figure 7 It is a first top view of the unit in this embodiment.

[0040] Figure 8 It is a second top view of the unit in this embodiment.

[0041] Fig. 9 1 is a schematic cross-sectional view showing a first example of an easy-to-break portion.

[0042] Fig.10 1 is a schematic cross-sectional view showing a second example of the easy-to-break portion.

[0043] Fig.11 1 is a schematic cross-sectional view showing a third example of the easy-to-break portion.

[0044] Fig.12This is a conceptual diagram showing a first example of the arrangement of easy-to-break portions.

[0045] Fig.13 This is a conceptual diagram showing a second example of the arrangement of the easy-to-break portions.

[0046] Fig.14 1 is a conceptual diagram showing a third example of the arrangement of the easy-to-break portions.

[0047] Fig.15 It is a schematic cross-sectional view showing a test product.

[0048] Fig.16 Shows the structure of the test sample and the results of the nail penetration test. DETAILED DESCRIPTION

[0049] The following describes an embodiment of the present technology (also referred to as "the present embodiment" in this specification). However, the following description does not limit the scope of the present technology. For example, the content of the effects mentioned in this specification does not limit the scope of the present technology within the scope of all the effects.

[0050] In this specification, the records of "comprise, include", "have" and their variations [such as "be composed of", "encompass, involve", "contain", "carry, support", "hold", etc.] are open forms. The open form may further include additional elements in addition to the essential elements, or may not include additional elements. The record of "consist of" is a closed form. The record of "consist essentially of" is a semi-closed form. Within the scope of not hindering the purpose of the present technology, the semi-closed form may also include additional elements in addition to the essential elements. For example, elements that are generally envisioned in the field to which the present technology belongs (such as unavoidable impurities, etc.) may also be included as additional elements.

[0051] In this specification, expressions such as “may…, can…” are not used in an obligatory sense, such as “must…”, but are used in a permissive sense, such as “having the possibility of…”. In this specification, unless otherwise specified, the singular (a, an, the) also includes the plural form.

[0052] The geometric terms (such as "parallel" etc.) in this specification should not be understood as strict meanings. For example, "parallel" may also slightly deviate from the strict meaning of "parallel". The geometric terms in this specification can include tolerances, errors, etc. in design, operation, and manufacturing. The dimensional relationship in each figure is sometimes inconsistent with the actual dimensional relationship. In order to facilitate the understanding of this technology, the dimensional relationship (length, width, thickness, etc.) in each figure may be changed sometimes. In addition, a part of the structure may be omitted sometimes.

[0053] In each figure, the "stacking direction" corresponds to the Z-axis direction. In addition, the relationship between the stacking direction and the vertical direction is arbitrary. For example, the stacking direction may be parallel to the vertical direction. For example, the stacking direction may also be orthogonal to the vertical direction.

[0054] In this specification, unless otherwise specified, numerical ranges such as "95°C to 140°C" and "95~140°C" include upper and lower limits. That is, "95°C to 140°C" and "95~140°C" represent numerical ranges of "95°C or more and 140°C or less". In addition, any numerical value selected from the numerical range may be set as a new upper and lower limit. For example, a new numerical range may be set by arbitrarily combining numerical values ​​within the numerical range with numerical values ​​described elsewhere in this specification.

[0055] In this specification, "abnormal" means at least one of temperature rise and internal pressure rise. "Temperature rise" means that the surface temperature of the unit becomes 90°C or higher. The surface temperature of the unit can be measured, for example, by a thermocouple. "Internal pressure rises" means that the difference between the internal pressure and the external pressure of the unit becomes 0.1 MPa or higher. The internal pressure can be measured by an internal pressure measuring instrument.

[0056] In this specification, the "first unit" and the "second unit" can be collectively referred to as "unit".

[0057] <Battery Pack>

[0058] Figure 4 This is a schematic diagram of a battery pack in this embodiment.

[0059] The battery pack 1000 can be used for any purpose. The battery pack 1000 can also be used as a main power source or a power auxiliary power source in an electric vehicle, etc., for example. The battery pack 1000 includes a module 500. The battery pack 1000 can include a single module 500. The battery pack 1000 can also include two or more modules 500. As long as the battery pack 1000 includes the module 500, it can further include any structure. The battery pack 1000 can also include, for example, a protection circuit, a protection device, a monitoring circuit, a cooling device, etc.

[0060] "container"

[0061] The battery pack 1000 may further include, for example, a container 600 . The container 600 may also be referred to as a “frame” or the like. The container 600 stores the module 500 . The container 600 may store one module 500 . The container 600 may also store two or more modules 500 .

[0062] The container 600 can have any shape. The container 600 can be, for example, square. The container 600 can be, for example, made of metal or resin. An exhaust duct 610 can be formed inside the container 600. The exhaust duct 610 is connected to the outside of the container 600. The exhaust duct 610 can include, for example, a straight pipe. The exhaust duct 610 can also include, for example, a bent pipe. The exhaust duct 610 guides the gas ejected from the module 500 to the outside of the container 600. In order to promote the exhaust of the gas, the container 600 can also include a fan, a suction blower, etc.

[0063] Module

[0064] Figure 5 It is a schematic cross-sectional view of the battery pack according to this embodiment.

[0065] Figure 5 Shown with Figure 4 The YZ plane is parallel to the cross section. Figure 5 The cross section is parallel to the stacking direction (Z-axis direction).

[0066] The battery pack 1000 includes a module 500. The module 500 is formed by stacking two or more units 100 (single cells) in the Z-axis direction. As long as there are two or more units 100, the number of units 100 is arbitrary. The module 500 may include, for example, 2 to 100 units 100. The module 500 may also include, for example, 4 to 50 units 100. The module 500 may also include, for example, 6 to 10 units 100.

[0067] Unit Pair

[0068] Figure 6 yes Figure 5 Magnified view of region VI in FIG.

[0069] The module 500 includes more than one unit pair 200. The unit pair 200 includes a first unit 100a and a second unit 100b. The second unit 100b is adjacent to the first unit 100a. The second unit 100b can be directly connected to the first unit 100a. The unit pair 200 can include, for example, a bus bar 150. The bus bar 150 has conductivity. The bus bar 150 can connect the first unit 100a to the second unit 100b.

[0070] The electrode terminal 30b may have the same polarity as the electrode terminal 30a. That is, the second unit 100b may be connected in parallel with the first unit 100a. The electrode terminal 30b may also have a polarity different from that of the electrode terminal 30a. That is, the second unit 100b may also be connected in series with the first unit 100a. When the unit pair 200 forms a series circuit, there is a tendency for abnormalities to be easily chained compared to when the unit pair 200 forms a parallel circuit. In the present embodiment, when the unit pair 200 forms a series circuit, it is also expected that abnormalities are unlikely to be chained.

[0071] As long as there is one or more unit pairs 200, the number of unit pairs 200 is arbitrary. The module 500 may include, for example, 1 to 50 unit pairs 200. The module 500 may include, for example, 2 to 25 unit pairs 200. The module 500 may include, for example, 3 to 5 unit pairs 200.

[0072] "unit"

[0073] The first unit 100a and the second unit 100b can each independently be any battery system. The first unit 100a can be, for example, a liquid lithium-ion battery, a lithium-ion polymer battery, or an all-solid lithium-ion battery. The first unit 100a can have any shape. The first unit 100a can be, for example, flat. The first unit 100a includes an outer body 10, an electrode body 20, and an electrode terminal 30a. The second unit 100b can have, for example, substantially the same structure as the first unit 100a.

[0074] (outer body)

[0075] The outer casing 10 accommodates the electrode body 20. The outer casing 10 may be in a bag shape. The outer casing 10 is sealed. The outer casing 10 includes a laminate film. The outer casing 10 may be substantially composed of a laminate film, for example. The laminate film includes a resin layer 11 and a metal layer 12. The resin layer 11 covers the metal layer 12. For example, the resin layer 11 may be welded to the metal layer 12. The resin layer 11 may cover only one side of the metal layer 12. The resin layer 11 may also cover both sides of the metal layer 12. That is, the laminate film may have a two-layer structure (resin layer 11 / metal layer 12) or a three-layer structure (resin layer 11 / metal layer 12 / resin layer 11).

[0076] The resin layer 11 may have a thickness of, for example, 1 μm to 100 μm. The resin layer 11 includes a first thermoplastic resin. The resin layer 11 may be substantially composed of a first thermoplastic resin. The first thermoplastic resin may include any component as long as it exhibits thermoplasticity. The first thermoplastic resin may include, for example, at least one selected from the group consisting of polyamide (nylon), polyethylene terephthalate, polyethylene naphthalate, polyphenylene sulfide, phenolic resin, polyvinyl alcohol, ethylene vinyl acetate copolymer, polyethylene, polypropylene, polyvinyl chloride, and ionomer. In the case where the laminate film has a three-layer structure, the two resin layers 11 may include the same thermoplastic resin or different thermoplastic resins.

[0077] The metal layer 12 may have a thickness of, for example, 10 μm to 500 μm. The metal layer 12 includes a metal. The metal layer 12 may be substantially composed of a metal. The metal layer 12 may also be substantially composed of a metal foil. The metal layer 12 may also be, for example, a metal vapor-deposited layer. The metal vapor-deposited layer may be formed by vapor-depositing a metal on the surface of the resin layer 11. The metal layer 12 may include, for example, aluminum (Al), an Al alloy, or the like.

[0078] (Electrode body)

[0079] The electrode body 20 includes a positive electrode and a negative electrode. The positive electrode includes a positive electrode active material. The negative electrode includes a negative electrode active material. Each of the positive electrode and the negative electrode can be, for example, in a sheet shape. The electrode body 20 can be, for example, a stacked type. That is, the electrode body 20 can be formed by alternately stacking the positive electrode and the negative electrode. The electrode body 20 can also be, for example, a wound type. That is, the electrode body 20 can also be formed by winding a stack including the positive electrode and the negative electrode into a spiral shape.

[0080] The electrode body 20 may further include a separator. The separator has electrical insulation properties. The separator separates the positive electrode from the negative electrode. The separator may include, for example, a porous film. The electrode body 20 may further include an electrolyte. The electrolyte may be a liquid, a gel, or a solid. For example, a liquid electrolyte (electrolyte) may be impregnated in the electrode body 20.

[0081] (Electrode terminal)

[0082] The first unit 100a includes two electrode terminals 30a. One is a positive terminal. The other is a negative terminal. The electrode terminal 30a is connected to the electrode body 20. The electrode terminal 30a can be welded to the electrode body 20. The electrode terminal 30a is in the shape of a flat plate. The electrode terminal 30a can include, for example, a metal plate. The electrode terminal 30a can have a thickness of, for example, 0.1 mm to 5 mm. The positive terminal can include, for example, an Al plate, etc. The negative terminal can include, for example, a copper (Cu) plate, etc.

[0083] (Seal part)

[0084] Figure 7 It is a first top view of the unit in this embodiment.

[0085] The outer casing 10 can have any planar shape. For example, the outer casing 10 can be rectangular. A sealing portion 13 is formed at the periphery of the outer casing 10. The sealing portion 13 is formed by heat welding. The sealing portion 13 can surround the housing portion 15. The housing portion 15 houses the electrode body 20.

[0086] The sealing portion 13 includes a first region 13a, a second region 13b, and a third region 13c. The third region 13c is formed between the resin layers 11 (see Figure 6 ). In the third region 13c, the resin layers 11 are welded to each other.

[0087] The electrode terminal 30 passes through the sealing portion 13 and is led out from the inside of the outer casing 10 to the outside. A first region 13a and a second region 13b are formed at a position where the electrode terminal 30 passes through the sealing portion 13. Figure 7 In the figure, the first region 13a and the second region 13b are in a positive and negative positional relationship.

[0088] The outline of the outer casing 10 may be composed of four sides, for example. The electrode terminals 30 (positive electrode terminals or negative electrode terminals) may be disposed on two sides facing each other among the four sides.

[0089] Figure 8 It is a second top view of the unit in this embodiment.

[0090] The outline of the exterior body 10 may be composed of four sides, for example. Two electrode terminals 30 (a positive electrode terminal and a negative electrode terminal) may be arranged on one of the four sides.

[0091] 《Easy to crack》

[0092] The electrode terminal 30a includes a first main surface 31 and a second main surface 32 (see Figure 6 ). The second main surface 32 is the opposite surface of the first main surface 31. The first main surface 31 faces the direction of the adjacent unit (the second unit 100b).

[0093] The first region 13a is formed between the first main surface 31 and the resin layer 11. In the first region 13a, the resin layer 11 is welded to the first main surface 31. The second region 13b is formed between the second main surface 32 and the resin layer 11. In the second region 13b, the resin layer 11 is welded to the second main surface 32.

[0094] The second region 13b includes an easily breakable portion. The easily breakable portion is configured to break more easily than the first region 13a and the third region 13c in an abnormal situation. The easily breakable portion may be formed in one of the first unit 100a and the second unit 100b in the unit pair 200, or may be formed in both the first unit 100a and the second unit 100b. That is, in the unit pair 200, at least one of the first unit 100a and the second unit 100b may include an easily breakable portion.

[0095] The easy-to-break portion may be arranged over the entire second region 13b. The easy-to-break portion may be arranged in a portion of the second region 13b. That is, the easy-to-break portion may be formed in at least a portion of the second region 13b.

[0096] The easily breakable portion may extend so as to connect the inside and the outside of the outer body 10. By connecting the inside and the outside of the outer body 10 through the easily breakable portion, it is expected that a gas flow path will be smoothly formed.

[0097] (Rough face)

[0098] Fig. 9 1 is a schematic cross-sectional view showing a first example of an easy-to-break portion.

[0099] The easy-to-break portion can have any structure. For example, the first main surface 31 can include a rough surface rp. For example, the first main surface 31 can be substantially composed of a rough surface rp. By including the rough surface rp in the first main surface 31, the bonding strength of the first region 13a can be increased. That is, the second region 13b has a relatively low bonding strength. As a result, an easy-to-break portion can be formed in the second region 13b. The easy-to-break portion can, for example, break when pressure increases.

[0100] The rough surface rp includes bumps and depressions on the surface. The rough surface rp can be formed, for example, by sandblasting. The rough surface rp can have, for example, an Ra of 0.1 μm or more. The rough surface rp can also have, for example, an Ra of 0.5 μm or more. The rough surface rp can also have, for example, an Ra of 10 μm or less. "Ra" in this specification represents the "arithmetic mean roughness" defined in "JIS B 0601". Ra can be measured by a laser microscope.

[0101] For example, the second main surface 32 may include a smooth surface. For example, the second main surface 32 may be substantially composed of a smooth surface. The smooth surface may have an Ra of less than 0.1 μm, for example. The smooth surface may have an Ra of 0.01 μm to 0.05 μm, for example.

[0102] For example, both the first main surface 31 and the second main surface 32 may include a rough surface rp. When both the first main surface 31 and the second main surface 32 include a rough surface rp, for example, the relationship of "Ra of the first main surface>Ra of the second main surface" may be satisfied. For example, the first main surface 31 may have Ra 2 to 100 times that of the second main surface 32. For example, the first main surface 31 may have Ra 5 to 50 times that of the second main surface 32.

[0103] (Adhesion strength)

[0104] The second region 13b may have a lower adhesive strength than the first region 13a and the third region 13c, for example. The second region 13b has a relatively low adhesive strength, so that an easily cracked portion can be formed in the second region 13b. The easily cracked portion with low adhesive strength can be cracked, for example, when pressure rises.

[0105] For example, the first region 13a and the third region 13c may each independently have an adhesive strength of 5 to 10 kgf / 15 mm. For example, the second region 13b may have an adhesive strength of less than 5 kgf / 15 mm. For example, the second region 13b may have an adhesive strength of 1 kgf / 15 mm or more. The "adhesive strength" in this specification means "peel adhesive strength". The "peel adhesive strength" is measured by the "peel adhesive strength test (180° peeling)" according to "JIS K 6854-2". The peel adhesive strength test can be implemented, for example, by "Autograph (registered trademark)" manufactured by Shimadzu Corporation. A tensile testing machine having the same function as the device can also be used. Prepare a test piece. The test piece is cut out from each region. For example, the test piece cut out from the first region 13a includes a portion of the electrode terminal 30a and a portion of the outer body 10 (laminated film). A portion of the outer body 10 is welded to a portion of the electrode terminal 30a. The ends of the electrode terminal 30a and the ends of the outer casing 10 are fixed to the clamp of the tensile tester, respectively. The outer casing 10 is peeled off from the electrode terminal 30a at an angle of 180°. The moving speed of the clamp is 100 mm / min. The average peeling force (kgf) is calculated from the force-clamp moving distance curve. "kgf / 15mm" represents the average peeling force when the width of the test piece is 15mm.

[0106] (Low melting point resin)

[0107] For example, the easily cracked portion may include a second thermoplastic resin. For example, in the second region 13b, the resin layer 11 may include a second thermoplastic resin. The second thermoplastic resin has a lower melting point than the first thermoplastic resin. It is expected that the easily cracked portion including the second thermoplastic resin will crack, for example, when the temperature rises. By releasing the internal pressure at an earlier stage during an abnormality, for example, the exothermic reaction becomes slow, and the amount of gas generated may also be reduced. Moreover, the heating of the electrode body 20 may also become slow.

[0108] In the second region 13b, the resin layer 11 may include, for example, a mixture of a first thermoplastic resin and a second thermoplastic resin. The mixture may, for example, form a homogeneous phase. The mixture may, for example, have an island structure. For example, the first thermoplastic resin may form a sea phase, and the second thermoplastic resin may form an island phase. For example, the second thermoplastic resin may form a sea phase, and the first thermoplastic resin may form an island phase.

[0109] Fig.10 1 is a schematic cross-sectional view showing a second example of the easy-to-break portion.

[0110] For example, in the second region 13b, the resin layer 11 may have a multilayer structure. That is, the resin layer 11 may include a first layer 11a and a second layer 11b. The second layer 11b is between the second main surface 32 and the first layer 11a. The second layer 11b may extend in a manner that connects the inside of the outer body 10 to the outside. For example, the first layer 11a may include a first thermoplastic resin. The first layer 11a may be substantially composed of a first thermoplastic resin. For example, the second layer 11b may include a second thermoplastic resin. The second layer 11b may be substantially composed of a second thermoplastic resin.

[0111] The second thermoplastic resin may include any component as long as it has a lower melting point than the first thermoplastic resin. The second thermoplastic resin may include, for example, at least one selected from the group consisting of polyethylene (melting point: 95-140°C), polypropylene (melting point: 160-170°C) and polyvinyl chloride (melting point: 180°C). In this specification, the "melting point" of a thermoplastic resin refers to the peak top temperature of a melting peak (endothermic peak) in a DSC (Differential Scanning Calorimetry) curve. The DSC curve can be measured in accordance with "JIS K 7121".

[0112] Fig.11 1 is a schematic cross-sectional view showing a third example of the easy-to-break portion.

[0113] For example, the easy-to-break portion may be formed by using one of the rough surface portion rp and the low-melting-point resin (second thermoplastic resin). For example, the easy-to-break portion may be formed by combining the rough surface portion rp and the low-melting-point resin. For example, the first main surface 31 may include the rough surface portion rp. In addition, the resin layer 11 disposed on the second main surface 32 side may include a first layer 11a and a second layer 11b. The second layer 11b may contain a second thermoplastic resin.

[0114] 《Arrangement of the crack-prone parts》

[0115] Fig.12 This is a conceptual diagram showing a first example of the arrangement of easy-to-break portions.

[0116] In each unit 100, the two electrode terminals 30 can be led out on different sides in a direction (Y-axis direction) intersecting the stacking direction (Z-axis direction). For example, all the easily breakable portions 40 can be gathered on one side in the Y-axis direction. By gathering all the easily breakable portions 40 on one side, all the easily breakable portions 40 can be easily arranged inside the exhaust duct 610. That is, the exhaust duct 610 can have a simple structure.

[0117] Fig.13 This is a conceptual diagram showing a second example of the arrangement of the easy-to-break portions.

[0118] The easily breakable portion 40 may be disposed on both sides of the Y-axis direction. The exhaust duct 610 may be disposed on only one side of the Y-axis direction or on both sides of the Y-axis direction. All of the easily breakable portions 40 may be disposed inside the exhaust duct 610. A portion of the easily breakable portions 40 may be disposed outside the exhaust duct 610.

[0119] Fig.14 1 is a conceptual diagram showing a third example of the arrangement of the easy-to-break portions.

[0120] For example, the easily breakable portion 40 may be disposed between all the electrode terminals 30 and the laminate film.

[0121] In addition, the electrode terminal 30x located at the end of the stacking direction has no object (unit) to be connected. At the end of the stacking direction, the easy-to-break portion 40 may be arranged, for example, on the side where there is no adjacent unit. At the end of the stacking direction, the easy-to-break portion 40 may be arranged, for example, on the side where there is an adjacent unit. At the end of the stacking direction, the easy-to-break portion 40 may not be arranged.

[0122] [Example]

[0123] Hereinafter, an embodiment of the present technology (also referred to as “the present embodiment” in this specification) will be described. However, the following description does not limit the scope of the present technology.

[0124] <Preparation of test samples>

[0125] Fig.15 It is a schematic cross-sectional view showing a test product.

[0126] The battery pack 1000 for trial use includes a container 600. The container 600 is made of Al. An exhaust duct 610 is provided inside the container 600. An insertion hole 620 is formed in the container 600. The insertion hole 620 has a diameter of 1.2 mm.

[0127] A module is arranged in the container 600. The module is composed of a unit pair 200. The unit pair 200 includes a first unit 100a, a second unit 100b and a bus bar 150. The unit pair 200 forms a series circuit. The bus bar 150 connects the first unit 100a and the second unit 100b in series. The first unit 100a and the second unit 100b are both liquid-based lithium-ion batteries. The outer body is made of an Al laminated film. The outer body is sealed by thermal welding. The outer body accommodates an electrode body. The electrode body is a stacked type. The positive terminal is an Al plate. The negative terminal is a Cu plate. A rough surface is formed on at least one of the positive terminal and the negative terminal by sandblasting.

[0128] <Test method>

[0129] Prepare the nail 300. The nail 300 is a round nail (tube diameter: 1.0 mm). The nail 300 is inserted from the insertion hole 620. Then, the nail 300 is inserted into the first unit 100a. Due to the insertion of the nail 300, an internal short circuit occurs in the first unit 100a. After the gas is ejected from the first unit 100a, the surface temperature of the second unit 100b is measured within 30 minutes.

[0130] No.1

[0131] Fig.16 Shows the structure of the test sample and the results of the nail penetration test.

[0132] In the battery pack 1000 of No. 1, the rough surface portion rp of the electrode terminal 30a and the rough surface portion rp of the electrode terminal 30b are arranged to face each other. That is, in the battery pack 1000 of No. 1, the second region 13b includes the easily breakable portion 40 .

[0133] No.2

[0134] In the battery pack 1000 of No. 2, the rough surface portion rp is not formed on both the electrode terminal 30a and the electrode terminal 30b. That is, the battery pack 1000 of No. 2 does not include the easily breakable portion 40. This is because the bonding strength does not substantially differ across all surfaces.

[0135] No.3

[0136] In the battery pack 1000 of No. 3, the rough surface portion rp of the electrode terminal 30a and the rough surface portion rp of the electrode terminal 30b are arranged to face opposite directions to each other. That is, in the battery pack 1000 of No. 3, the first region 13a includes the easy-to-break portion 40 .

[0137] No.4

[0138] In the battery pack 1000 of No. 4, the rough surface portion rp is formed on all the surfaces of the electrode terminal 30a and the electrode terminal 30b. Therefore, the battery pack 1000 of No. 4 does not include the easily breakable portion 40. This is because the bonding strength does not substantially differ on all the surfaces.

[0139] <Results>

[0140] exist Fig.16 In the item of "heat generation linkage", "yes" means that the surface temperature of the second unit 100b rises to 90°C or higher after the gas is ejected from the first unit 100a. "no" means that the surface temperature of the second unit 100b is less than 90°C within 30 minutes after the gas is ejected from the first unit 100a.

[0141] exist Fig.16 In the embodiment, since the second region 13b includes the easy-to-break portion 40, a tendency that the second unit 100b is unusually difficult to interlock is observed.

[0142] The present embodiment and the present example are illustrative in all respects. The present embodiment and the present example are not restrictive. The scope of the present technology includes all changes within the meaning and scope equivalent to the claims. For example, it is initially intended that any structure can be extracted from the present embodiment and the present example and they can be combined arbitrarily.

Claims

1. A battery pack, wherein: The battery pack includes a module, The unit pair includes a first unit and a second unit, The second unit is adjacent to the first unit, The first unit includes an outer casing, an electrode body and an electrode terminal. The outer body includes a laminate film, The laminated film comprises a resin layer and a metal layer, The outer casing includes a housing portion for housing the electrode body. A sealing portion is formed on the outer casing, The electrode terminal is connected to the electrode body, The electrode terminal passes through the sealing portion and is led out from the inside of the outer casing to the outside. The portion of the electrode terminal that passes through the sealing portion is in the shape of a flat plate. The electrode terminal includes a first main surface and a second main surface, The first main surface faces the direction of the second unit, The second main surface is the opposite surface of the first main surface, The area of ​​the sealing portion that contacts the second main surface includes an easy-to-break portion, The easily ruptured portion is configured to be more easily ruptured than a region other than the easily ruptured portion in the sealing portion when at least one of the temperature and the internal pressure of the first unit increases. The electrode terminal of the first unit is connected to the electrode terminal of the second unit, The battery pack further includes a container, The container accommodates the module. An exhaust duct is formed inside the container. The storage portion is arranged outside the exhaust duct. The easily breakable portion is disposed inside the exhaust duct.

2. A battery pack, wherein: The battery pack includes a module, The unit pair includes a first unit and a second unit, The second unit is adjacent to the first unit, The first unit includes an outer casing, an electrode body and an electrode terminal. The outer body includes a laminate film, The laminated film comprises a resin layer and a metal layer, The outer casing includes a housing portion for housing the electrode body. A sealing portion is formed on the outer casing, The electrode terminal is connected to the electrode body, The electrode terminal passes through the sealing portion and is led out from the inside of the outer casing to the outside. The portion of the electrode terminal that passes through the sealing portion is in the shape of a flat plate. The electrode terminal includes a first main surface and a second main surface, The first main surface faces the direction of the second unit, The second main surface is the opposite surface of the first main surface, The area of ​​the sealing portion that contacts the second main surface includes an easy-to-break portion, The easily ruptured portion is configured to be more easily ruptured than a region other than the easily ruptured portion in the sealing portion when at least one of the temperature and the internal pressure of the first unit increases. A partially closed space is formed on the first region side by connecting the electrode terminal of the first cell and the electrode terminal of the second cell.

3. The battery pack according to claim 1 or 2, wherein: When the module further includes a third cell and the third cell is adjacent to the first cell and arranged on the opposite side of the second cell, the electrode terminal of the first cell connected to the electrode terminal of the second cell is not connected to the electrode terminal of the third cell.

4. The battery pack according to claim 1 or 2, wherein: The first main surface includes a rough surface.

5. The battery pack according to claim 1 or 2, wherein: At the sealing portion, the easy-to-break portion has a lower melting point than other portions.

6. The battery pack according to claim 1 or 2, wherein: The module includes more than two unit pairs, two or more of the unit pairs each include the first unit and the second unit, In each of the two or more unit pairs, the easy-to-break portion is disposed inside the exhaust duct.