In-vehicle air treatment method based on macromolecule nanometer resonance spraying material
Through polymer nanoresonance spraying materials and intelligent sensor systems, real-time monitoring and dynamic management of in-vehicle air quality is solved, and the shortcomings of traditional in-vehicle air treatment methods are achieved, and efficient and long-term air purification and environmentally friendly reuse are achieved.
Patent Information
- Application Number
- CN202411081402.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-12
Smart Images

Figure CN118927957A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of air treatment, and specifically is a method for treating air in a vehicle based on a polymer nano resonance spray material. Background Art
[0002] At present, with the continuous increase in the number of cars, the air quality inside the car has become an important factor affecting the health of drivers and passengers. The air quality inside new cars or vehicles that have been used for a long time has declined due to harmful gases released by materials, passenger activities, and dust and bacterial pollutants accumulated during long-term use. This not only affects the health of drivers and passengers, but may also cause respiratory diseases and allergic reactions.
[0003] Traditional methods of in-car air treatment mainly include ventilation, activated carbon adsorption, and spraying chemical deodorizers. However, these methods have many shortcomings: although ventilation can temporarily improve air quality, it cannot fundamentally solve the pollution source problem; activated carbon adsorption is easily saturated, needs to be replaced regularly and has limited effect; chemical deodorizers may cause secondary pollution and pose a potential threat to human health.
[0004] For example, the patent with the authorization announcement number CN101433731B discloses a method for indoor air pollution control, including: pre-coating a layer of photocatalyst material on the inner surface of one or more surfaces of the product packaging box, and when the product is taken out for use, disassembling the packaging box to expose the photocatalyst material coated on the inner surface to the indoor air, so that the photocatalyst participates in the oxidation-reduction catalytic reaction of organic pollutants in the air. This method provides an environmentally friendly utilization method for the packaging box, and is particularly suitable for use on the outer packaging boxes of household electrical appliances, especially large household appliances such as refrigerators, air conditioners, color TVs, and washing machines. Most of their outer packaging boxes are cardboard boxes, which are easy to operate and have a considerable total surface area. Not only does it turn the packaging box into "waste into treasure" and improve the environmentally friendly utilization surplus value, but it also greatly simplifies the existing indoor air pollution control application photocatalyst operation procedures, making it convenient for users to use it by themselves.
[0005] For example, the patent with the authorization announcement number CN101081307B discloses a method for improving the photocatalytic air purification effect, including: utilizing the good adsorption effect of cyclodextrin substances on pollutants in the air, coating or impregnating and adsorbing the load on the surface of the photocatalyst, forming a thin layer containing cyclodextrin or its derivatives, thereby improving the adsorption and purification effect of air pollutants, especially aromatic and toxic compounds, and especially improving the adsorption photocatalytic purification effect of low-concentration pollutants. The effect and benefit of this technical solution is that the prepared photocatalytic material composited with cyclodextrin compounds is more stable, not easy to deactivate, and has higher activity and efficiency in removing pollutants. It has broad application prospects in the fields of indoor air pollution control, automobile and other atmospheric pollution control.
[0006] The above existing technologies all have the following problems: CN101433731B mainly relies on the photocatalyst material on the inner surface of the packaging box to treat indoor air, but the total surface area of the packaging box is still limited relative to the entire indoor space, so its purification effect may be limited to the local area near the packaging box, and it is difficult to have a significant impact on the entire indoor environment, and it lacks intelligent and automated elements; CN101081307B mainly relies on the combination of photocatalysts and cyclodextrin substances to improve the purification effect, but this method lacks real-time air quality monitoring and dynamic adjustment mechanisms. Summary of the invention
[0007] In view of the shortcomings of the prior art, the present invention proposes a method for in-vehicle air treatment based on polymer nano-resonance spraying materials. The method monitors the in-vehicle air quality in real time by integrating on-board intelligent sensors, and automatically starts a deep cleaning program based on the evaluation results. Adaptive spraying equipment is used to evenly cover the key surfaces in the vehicle with polymer nano-resonance spraying materials to form a nano-coating. In combination with environmental perception data, a dynamic curing strategy is implemented to enhance the function of the coating. The nano-coating utilizes the resonance effect to effectively decompose harmful gas molecules, oxidize pollutants, and inhibit the growth of microorganisms, converting them into harmless substances. Based on the coating wear model and air quality data, maintenance needs are automatically warned, and after the coating life ends, a stripping-purification process is used to achieve environmentally friendly recycling and reuse, thereby improving the in-vehicle air quality, maintaining the purification effect for a long time, and reducing recurrence after treatment.
[0008] To achieve the above object, the present invention provides the following technical solutions:
[0009] The in-vehicle air treatment method based on polymer nano resonance spraying material includes:
[0010] Step S1: Use the vehicle-mounted intelligent sensor system to monitor and evaluate the air quality in the vehicle in real time. According to the evaluation results, deep cleaning is performed in the vehicle, and the polymer nano resonance spray material is evenly sprayed on the surface of the vehicle ceiling, seats, and interior panels using an adaptive spraying device to form a nano coating;
[0011] Step S2: In combination with the in-vehicle environment perception data, a dynamic curing strategy is used to cure the nano coating to generate a functional layer;
[0012] Step S3: When harmful gas molecules or microbial pollutants in the air inside the vehicle contact the functional layer through air flow, the resonance effect of the polymer nanomaterial is used to resonate and generate hole pairs, which react with the harmful gas molecules or microbial pollutants to oxidize them into harmless carbon dioxide and water products, or destroy the cell structure of the microorganisms to inhibit the growth of the microorganisms;
[0013] Step S4: Combine the coating wear model and air quality monitoring data to achieve predictive maintenance. When the functional layer is worn or the air quality in the car decreases, the user is automatically reminded to perform maintenance or repaint. At the same time, after the functional layer reaches the end of its service life, it is recycled and reused through a stripping-purification process.
[0014] Specifically, the specific steps of the dynamic solidification strategy in step S2 include:
[0015] S2.1: Use the vehicle-mounted sensor system to collect real-time in-vehicle environmental perception data, and set the curing condition range according to the material properties and curing requirements of the nano-coating. The formula is:
[0016]
[0017] Among them, T arg Indicates the curing temperature range, S arg Indicates the relative humidity range of curing, t cure Indicates the curing time, T min , T max Respectively represent the minimum and maximum curing temperatures, S min , S max represent the minimum relative humidity and the maximum relative humidity of curing, respectively, T represents the curing temperature, S represents the curing relative humidity, A represents the polymer nano resonance spraying material formula, and F(·) represents a multivariable function;
[0018] S2.2: Compare and match the real-time in-vehicle environment perception data with the preset curing condition range to determine whether the current in-vehicle environment meets the curing requirements.
[0019] Specifically, the specific steps of the dynamic solidification strategy in step S2 also include:
[0020] S2.3: If the current environment meets the curing conditions, a preliminary curing strategy is formulated based on the material properties and application requirements, and the parameters in the curing strategy are dynamically adjusted according to the changes in the real-time in-vehicle environment perception data;
[0021] S2.4: transmitting the adjusted curing strategy to the curing equipment, executing the curing operation, and continuously monitoring the environmental parameters and the operating status of the curing equipment during the curing process;
[0022] S2.5: After curing, the formation of the functional layer is verified by adhesion test and infrared spectroscopy analysis.
[0023] Specifically, the specific steps of S2.5 include:
[0024] S2.51: Obtain the cured nanocoating sample and perform preliminary cleaning;
[0025] S2.52: Set the maximum shedding area threshold to h1, use the cross-hatch method to draw grids with a spacing of b on the nano-coating, stick them with tape and quickly tear them off, and observe whether the nano-coating falls off from the substrate.
[0026] If β≤h1, the adhesion is qualified;
[0027] If β>h1, the adhesion is unqualified, that is, the nano coating is unqualified or has reached the end of its service life, where β represents the shedding area of the nano coating.
[0028] Specifically, the specific steps of S2.5 also include:
[0029] S2.53: Slicing the cured nano-coating sample to obtain the sliced nano-coating sample, and performing infrared spectrum analysis on the sliced nano-coating sample using a Fourier transform infrared spectrometer to generate an infrared spectrum graph of the nano-coating sample;
[0030] S2.54: Obtain a plurality of standard infrared spectra, and compare the infrared spectrum of the nanocoating sample with the standard infrared spectrum. If the absorption peak position on the infrared spectrum of the nanocoating sample coincides with the absorption peak positions of the plurality of standard infrared spectra, a functional layer is present.
[0031] Specifically, the specific steps of step S4 include:
[0032] S4.1: Collect the wear data of the functional layer under different use conditions and perform preprocessing to obtain the coating wear data X = {x1,...,x N}, based on the coating wear data, a coating wear prediction model is established using machine learning methods, where x N represents the Nth coating wear data, where N represents the number of coating wear data;
[0033] S4.2: Collect the in-vehicle air quality data through the vehicle-mounted intelligent sensor system and perform preprocessing to obtain the air quality monitoring data Y = {y1,...,y M}, based on the air quality monitoring data, an air quality change trend prediction model is established, where y M Represents the Mth air quality monitoring data, and M represents the number of air quality monitoring data.
[0034] Specifically, the specific steps of step S4 also include:
[0035] S4.3: Set the functional layer wear warning threshold h2 and the air quality qualified threshold h3, and integrate the coating wear prediction model and the air quality change trend prediction model into the predictive maintenance system;
[0036] S4.4: If δ≥h2, or μ≤h3, a warning signal is automatically issued, where δ represents the degree of coating wear and μ represents the real-time in-vehicle air quality;
[0037] S4.5: After receiving the warning signal, the user shall perform maintenance or re-spray according to the system recommendations.
[0038] Specifically, the specific steps of step S4 also include:
[0039] S4.6: If δ ≥ h2, or μ ≤ h3, or β > h1, it means that the functional layer has reached the end of its service life, and a physical stripping method is used to perform a stripping operation under controlled conditions according to the substrate and coating type of the functional layer;
[0040] S4.7: Preliminary treatment is performed on the peeled functional layer material to remove dirt and residues on the surface, and impurities in the functional layer are separated by a separation method;
[0041] S4.8: Purify using an ion exchange purification treatment method according to the specific composition and properties of the functional layer;
[0042] S4.9: Perform performance testing on the purified functional layer, and adjust the formula of the nanocoating based on the performance test results of the functional layer.
[0043] Specifically, the curing strategy in S2.3 includes target temperature, target humidity, heating rate, cooling rate and control method during the curing process.
[0044] Compared with the prior art, the present invention has the following beneficial effects:
[0045] 1. The present invention proposes an in-vehicle air treatment method based on polymer nano-resonance spraying materials, which improves the in-vehicle air quality and can maintain the purification effect for a long time through real-time monitoring, comprehensive cleaning, efficient purification, dynamic curing, predictive maintenance and intelligent management.
[0046] 2. The present invention proposes an in-vehicle air treatment method based on polymer nano resonance spraying materials, which realizes comprehensive control and efficient treatment of in-vehicle air quality through intelligent monitoring and instant response mechanism; from real-time monitoring to deep cleaning, and then to dynamic curing of nano coating and generation of functional layer, each step is closely linked to form a closed-loop treatment system, which effectively ensures the freshness and health of in-vehicle air; while improving purification efficiency, it also pays attention to environmental protection and sustainability, the resonance effect of polymer nano materials can efficiently convert harmful gases and inhibit the growth of microorganisms, while the predictive maintenance and recycling and reuse mechanism reduces the user's maintenance cost and reduces resource waste. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figure 1This is a process framework diagram of the in-vehicle air treatment method based on the polymer nano resonance spray material of the present invention;
[0048] Figure 2 This is a principle flow chart of the in-vehicle air treatment method based on polymer nano resonance spraying material of the present invention;
[0049] Figure 3 This is a flow chart of the functional layer of the in-vehicle air treatment method based on the polymer nano resonance spray material of the present invention;
[0050] Figure 4 The present invention is a flow chart for predictive maintenance and reuse of the in-vehicle air treatment method based on polymer nano resonance spraying materials. DETAILED DESCRIPTION
[0051] Example 1
[0052] See also Figure 1-Figure 2 The present invention provides an embodiment: a method for treating in-vehicle air based on a polymer nano-resonance spraying material, comprising the following steps:
[0053] Step S1: Use the vehicle-mounted intelligent sensor system to monitor and evaluate the air quality in the vehicle in real time. According to the evaluation results, deep cleaning is performed in the vehicle, and the polymer nano resonance spray material is evenly sprayed on the surface of the vehicle ceiling, seats, and interior panels using an adaptive spraying device to form a nano coating;
[0054] Furthermore, the specific steps of step S1 include:
[0055] (1) Install multiple sensors inside the vehicle, including PM2.5 sensors, TVOC sensors, and temperature and humidity sensors, to monitor the air quality inside the vehicle in real time. The sensors are wirelessly connected to the vehicle control system to transmit monitoring data in real time;
[0056] (2) The vehicle control system receives the data transmitted by the sensor, processes and analyzes it, and evaluates the air quality in the vehicle based on the preset air quality standards to determine whether deep cleaning is needed;
[0057] (3) When the assessment results show that the in-vehicle air quality does not meet the standards, initiate a deep cleaning procedure and use professional in-vehicle cleaning equipment and cleaning agents to thoroughly clean the interior of the vehicle, including seats, carpets, interior panels, and air conditioning systems;
[0058] (4) After deep cleaning is completed, prepare the adaptive spraying equipment and polymer nano resonance spraying materials. Ensure that the spraying equipment is in good working condition and adjust the spraying parameters according to the structure and materials inside the vehicle;
[0059] (5) Use adaptive spraying equipment to evenly spray the polymer nano-resonance spray material onto the surface of the vehicle ceiling, seats, and interior panels. During the spraying process, pay attention to controlling the spraying thickness and uniformity to ensure the coating quality.
[0060] Step S2: In combination with the in-vehicle environment perception data, a dynamic curing strategy is used to cure the nano coating to generate a functional layer;
[0061] Step S3: When harmful gas molecules or microbial pollutants in the air inside the vehicle contact the functional layer through air flow, the resonance effect of the polymer nanomaterial is used to resonate and generate hole pairs, which react with the harmful gas molecules or microbial pollutants to oxidize them into harmless carbon dioxide and water products, or destroy the cell structure of the microorganisms to inhibit the growth of the microorganisms;
[0062] Furthermore, the specific steps of generating hole pairs include:
[0063] (1) When the nano-coating is exposed to light, especially ultraviolet light, the polymer nano-materials in the coating, such as nano-titanium dioxide TiO2, will absorb light energy. The absorption of light energy is the first step to trigger the subsequent photocatalytic reaction;
[0064] (2) The absorbed light energy causes the electrons in the nanomaterial to jump from the valence band to the conduction band, that is, from a low energy level to a high energy level, forming an excited state. In this process, corresponding holes, i.e., positive charge centers, will be left on the valence band, forming electron-hole pairs;
[0065] (3) After the electron transition, the hole left in the valence band and the electron that transitioned to the conduction band together form an electron-hole pair.
[0066] At the same time, it can be simplified to understand that under light conditions, the photocatalyst in the nanocoating absorbs light energy and generates electron-hole pairs, which then react with the pollutant molecules adsorbed on the surface of the coating. There are multiple intermediate steps and products involved in the reaction process, but the final result is to convert harmful gas molecules into harmless carbon dioxide and water products, or to kill microbial pollutants or inhibit their growth. The chemical equation is: hole (h + )+harmful gas molecules (RH)→intermediate products→CO2+H2O.
[0067] Step S4: Combine the coating wear model and air quality monitoring data to achieve predictive maintenance. When the functional layer is worn or the air quality in the car decreases, the user is automatically reminded to perform maintenance or repaint. At the same time, after the functional layer reaches the end of its service life, it is recycled and reused through a stripping-purification process.
[0068] Example 2
[0069] See also Figure 3 In this embodiment, the specific steps of the dynamic solidification strategy in step S2 include:
[0070] S2.1: Use the vehicle-mounted sensor system to collect real-time in-vehicle environmental perception data, and set the curing condition range according to the material properties and curing requirements of the nano-coating. The formula is:
[0071]
[0072] Among them, T arg Indicates the curing temperature range, S arg Indicates the relative humidity range of curing, t cure Indicates the curing time, T min 、T max Respectively represent the minimum and maximum curing temperatures, S min , S max They represent the minimum relative humidity and the maximum relative humidity of curing, respectively, T represents the curing temperature, S represents the curing relative humidity, A represents the polymer nano resonance spraying material formula, and F(·) represents a multivariable function;
[0073] S2.2: Compare and match the real-time in-vehicle environment perception data with the preset curing condition range to determine whether the current in-vehicle environment meets the curing requirements;
[0074] S2.3: If the current environment meets the curing conditions, a preliminary curing strategy is formulated based on the material properties and application requirements, and the parameters in the curing strategy are dynamically adjusted according to the changes in the real-time in-vehicle environment perception data;
[0075] Among them, in the process of adjusting the curing strategy, the adjustments include curing temperature, curing time, and curing rate.
[0076] Furthermore, the curing strategy in S2.3 includes target temperature, target humidity, heating rate, cooling rate and control method during the curing process.
[0077] The target temperature refers to the specific temperature value that needs to be reached and maintained during the curing process. It is usually provided by the material supplier and is determined based on the curing characteristics of the material and the application requirements. For example, for the curing of a certain resin material, the target temperature may be set to 150°C.
[0078] Target humidity refers to the specific humidity level that needs to be achieved and maintained during the curing process. The humidity setting depends on the characteristics of the material and the requirements of the curing process, and the relative humidity is usually set at 50% RH.
[0079] Heating rate R hotIt refers to the speed at which the material temperature rises from the initial value to the target temperature, which affects the temperature distribution inside the material and the speed of the curing reaction. It is usually expressed by dividing the temperature change ΔT by the time Δt, that is,
[0080] Cooling rate R cold It refers to the speed at which the material temperature drops from the target temperature to the temperature required for safety or subsequent processing. The formula is also:
[0081] The control method is to use a PID control algorithm to adjust the output power of the heating device to maintain a set temperature value. However, the PID control algorithm is a prior art in this field and is not an inventive solution of the present application, and will not be described in detail here.
[0082] S2.4: transmitting the adjusted curing strategy to the curing equipment, executing the curing operation, and continuously monitoring the environmental parameters and the operating status of the curing equipment during the curing process;
[0083] S2.5: After curing, the formation of the functional layer is verified by adhesion test and infrared spectroscopy analysis.
[0084] Specifically, the specific steps of S2.5 include:
[0085] S2.51: Obtain the cured nanocoating sample and perform preliminary cleaning;
[0086] S2.52: Set the maximum shedding area threshold to h1, use the cross-hatch method to draw grids with a spacing of b on the nano-coating, stick them with tape and quickly tear them off, and observe whether the nano-coating falls off from the substrate.
[0087] If β≤h1, the adhesion is qualified;
[0088] If β>h1, the adhesion is unqualified, that is, the nano coating is unqualified or has reached the end of its service life, where β represents the shedding area of the nano coating;
[0089] S2.53: Slice the cured nanocoating sample to obtain the sliced nanocoating sample, and use a Fourier transform infrared spectrometer to perform infrared spectrum analysis on the sliced nanocoating sample to generate an infrared spectrum graph of the nanocoating sample, wherein the process of performing infrared spectrum analysis with a Fourier transform infrared spectrometer is the prior art content in this field, and is not an inventive solution of the present application, and is not described in detail here;
[0090] S2.54: Obtain a plurality of standard infrared spectra, and compare the infrared spectrum of the nanocoating sample with the standard infrared spectrum. If the absorption peak position on the infrared spectrum of the nanocoating sample coincides with the absorption peak positions of the plurality of standard infrared spectra, a functional layer is present.
[0091] Example 3
[0092] See also Figure 4 In this embodiment, the specific steps of step S4 include:
[0093] S4.1: Collect the wear data of the functional layer under different use conditions and perform preprocessing to obtain the coating wear data X = {x1,...,x N}, based on the coating wear data, a coating wear prediction model is established using machine learning methods, where x N represents the Nth coating wear data, N represents the number of coating wear data, and at the same time, the implementation process of establishing a prediction model using a machine learning method is the prior art content in this field, which is not the inventive solution of the present application and will not be described in detail here;
[0094] S4.2: Collect the in-vehicle air quality data through the vehicle intelligent sensor system and perform preprocessing to obtain the air quality monitoring data Y = {y1,…,y M}, based on the air quality monitoring data, an air quality change trend prediction model is established, where y M represents the Mth air quality monitoring data, where M represents the number of air quality monitoring data;
[0095] S4.3: Set the functional layer wear warning threshold h2 and the air quality qualified threshold h3, and integrate the coating wear prediction model and the air quality change trend prediction model into the predictive maintenance system;
[0096] S4.4: If δ≥h2, or μ≤h3, a warning signal is automatically issued, where δ represents the degree of coating wear and μ represents the real-time in-vehicle air quality;
[0097] S4.5: After receiving the warning signal, the user performs maintenance or re-spraying according to the system's recommendations;
[0098] S4.6: If δ ≥ h2, or μ ≤ h3, or β > h1, it means that the functional layer has reached the end of its service life, and a physical stripping method is used to perform a stripping operation under controlled conditions according to the substrate and coating type of the functional layer;
[0099] S4.7: Preliminary treatment is performed on the peeled functional layer material to remove dirt and residues on the surface, and impurities in the functional layer are separated by a separation method;
[0100] The impurities in the functional layer include: unreacted raw materials, by-products, and solvent residues.
[0101] Furthermore, the specific steps of S4.7 include:
[0102] (1) The peeled functional layer material is first cleaned to remove dirt and residues on the surface, wherein anhydrous ethanol or deionized water solvent is used to assist ultrasonic cleaning in a high-frequency numerically controlled ultrasonic cleaning device to remove tiny particles on the surface and pollutants that are easily soluble in the solvent. At the same time, for some stubborn impurities, such as oily compounds, a specific degreasing liquid needs to be prepared, the material is immersed in it, and decomposed through a chemical reaction, such as a saponification reaction, and then ultrasonic cleaning is performed with deionized water and anhydrous ethanol;
[0103] (2) After cleaning, in order to avoid the influence of residual solvent on the surface of the material on the subsequent processing process, the material needs to be placed in a vacuum drying oven for constant temperature treatment to completely remove the residual solvent on the surface;
[0104] (3) Before impurity separation, it is necessary to first determine the type and nature of the impurities in the functional layer in order to select a suitable separation method. In the present invention, the ion exchange method is selected;
[0105] (4) Based on the selected separation method, perform experimental operations to achieve effective separation of impurities.
[0106] S4.8: Purify using an ion exchange purification treatment method according to the specific composition and properties of the functional layer;
[0107] S4.9: Perform performance testing on the purified functional layer, and adjust the formula of the nanocoating based on the performance test results of the functional layer.
[0108] Those skilled in the art will appreciate that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.
[0109] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1A device that provides the functions specified in a block or multiple blocks.
[0110] The embodiments of the present invention are described above in conjunction with the accompanying drawings, but the present invention is not limited to the above-mentioned specific implementation modes, which are merely illustrative rather than restrictive. Under the guidance of the present invention, ordinary technicians in the field may also change, modify, replace and modify the above-mentioned embodiments without departing from the purpose and scope of protection of the present invention, and all of these are within the protection of the present invention.
Claims
1. A method for treating in-vehicle air based on polymer nano-resonance spraying materials, characterized in that: include: Step S1: Use the vehicle-mounted intelligent sensor system to monitor and evaluate the air quality in the vehicle in real time. According to the evaluation results, deep cleaning is performed in the vehicle, and the polymer nano resonance spray material is evenly sprayed on the surface of the vehicle ceiling, seats, and interior panels using an adaptive spraying device to form a nano coating; Step S2: In combination with the in-vehicle environment perception data, a dynamic curing strategy is used to cure the nano coating to generate a functional layer; Step S3: When harmful gas molecules or microbial pollutants in the air inside the vehicle contact the functional layer through air flow, the resonance effect of the polymer nanomaterial is used to resonate and generate hole pairs, which react with the harmful gas molecules or microbial pollutants to oxidize them into harmless carbon dioxide and water products, or destroy the cell structure of the microorganisms to inhibit the growth of the microorganisms; Step S4: Combine the coating wear model and air quality monitoring data to achieve predictive maintenance. When the functional layer is worn or the air quality in the car decreases, the user is automatically reminded to perform maintenance or repaint. At the same time, after the functional layer reaches the end of its service life, it is recycled and reused through a stripping-purification process.
2. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 1, characterized in that: The specific steps of the dynamic curing strategy in step S2 include: S2.1: Use the vehicle-mounted sensor system to collect real-time in-vehicle environmental perception data, and set the curing condition range according to the material properties and curing requirements of the nano-coating. The formula is: Among them, T arg Indicates the curing temperature range, S arg Indicates the relative humidity range of curing, t cure Indicates the curing time, T min 、T max Respectively represent the minimum and maximum curing temperatures, S min , S max represent the minimum relative humidity and the maximum relative humidity of curing, respectively, T represents the curing temperature, S represents the curing relative humidity, A represents the polymer nano resonance spraying material formula, and F(·) represents a multivariable function; S2.2: Compare and match the real-time in-vehicle environment perception data with the preset curing condition range to determine whether the current in-vehicle environment meets the curing requirements.
3. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 2, characterized in that: The specific steps of the dynamic solidification strategy in step S2 also include: S2.3: If the current environment meets the curing conditions, a preliminary curing strategy is formulated based on the material properties and application requirements, and the parameters in the curing strategy are dynamically adjusted according to the changes in the real-time in-vehicle environment perception data; S2.4: transmitting the adjusted curing strategy to the curing equipment, executing the curing operation, and continuously monitoring the environmental parameters and the operating status of the curing equipment during the curing process; S2.5: After curing, the formation of the functional layer is verified by adhesion test and infrared spectroscopy analysis.
4. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 3, characterized in that: The specific steps of S2.5 include: S2.51: Obtain the cured nanocoating sample and perform preliminary cleaning; S2.52: Set the maximum shedding area threshold to h1, use the cross-hatch method to draw grids with a spacing of b on the nano-coating, stick them with tape and quickly tear them off, and observe whether the nano-coating falls off from the substrate. If β≤h1, the adhesion is qualified; If β>h1, the adhesion is unqualified, that is, the nano coating is unqualified or has reached the end of its service life, where β represents the shedding area of the nano coating.
5. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 4, characterized in that: The specific steps of S2.5 also include: S2.53: Slicing the cured nano-coating sample to obtain the sliced nano-coating sample, and performing infrared spectrum analysis on the sliced nano-coating sample using a Fourier transform infrared spectrometer to generate an infrared spectrum graph of the nano-coating sample; S2.54: Obtain a plurality of standard infrared spectra, and compare the infrared spectrum of the nanocoating sample with the standard infrared spectrum. If the absorption peak position on the infrared spectrum of the nanocoating sample coincides with the absorption peak positions of the plurality of standard infrared spectra, a functional layer is present.
6. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 5, characterized in that: The specific steps of step S4 include: S4.1: Collect the wear data of the functional layer under different use conditions and perform preprocessing to obtain the coating wear data X = {x1,...,x N }, based on the coating wear data, a coating wear prediction model is established using machine learning methods, where x N represents the Nth coating wear data, where N represents the number of coating wear data; S4.2: Collect the in-vehicle air quality data through the vehicle-mounted intelligent sensor system and perform preprocessing to obtain the air quality monitoring data Y = {y1,...,y M }, based on the air quality monitoring data, an air quality change trend prediction model is established, where y M Represents the Mth air quality monitoring data, and M represents the number of air quality monitoring data.
7. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 6, characterized in that: The specific steps of step S4 also include: S4.3: Set the functional layer wear warning threshold h2 and the air quality qualified threshold h3, and integrate the coating wear prediction model and the air quality change trend prediction model into the predictive maintenance system; S4.4: If δ≥h2, or μ≤h3, a warning signal is automatically issued, where δ represents the degree of coating wear and μ represents the real-time in-vehicle air quality; S4.5: After receiving the warning signal, the user shall perform maintenance or re-spray according to the system recommendations.
8. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 7, characterized in that: The specific steps of step S4 also include: S4.6: If δ ≥ h2, or μ ≤ h3, or β > h1, it means that the functional layer has reached the end of its service life, and a physical stripping method is used to perform a stripping operation under controlled conditions according to the substrate and coating type of the functional layer; S4.7: Preliminary treatment is performed on the peeled functional layer material to remove dirt and residues on the surface, and impurities in the functional layer are separated by a separation method; S4.8: Purify using an ion exchange purification treatment method according to the specific composition and properties of the functional layer; S4.9: Perform performance testing on the purified functional layer, and adjust the formula of the nanocoating based on the performance test results of the functional layer.
9. The method for treating in-vehicle air based on polymer nano resonance spraying material according to claim 8, characterized in that: The curing strategy in S2.3 includes target temperature, target humidity, heating rate, cooling rate and control method during the curing process.
Citation Information
Cited By
Solidification degree analysis-based magnesium oxide coating performance detection system and method
CN120890972A