Shading fine silver paint coating for mini-character base material and preparation method of shading fine silver paint coating

By using the two-component structure of the mini-font substrate with a fine silver paint coating, the number of spraying is simplified, the problems of high cost and complex operations in the existing technology are solved, and the efficient and environmentally friendly light-shielding effect is achieved.

CN118931281AInactive Publication Date: 2024-11-12RIZHAO BANGNI PAINT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411158801.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing mini-word shade coating process requires three spraying, which is costly, complex operation process and is not environmentally friendly, and cannot meet the energy-saving and environmental protection requirements.

Method used

A thin silver paint coating for a mini-font substrate with a two-component structure includes phase A and phase B. Phase A is composed of acrylic resin, dispersant, butyl ether, butyl ester, CAB, and Phase B is composed of 5μm silver paste and poly The amide wax is composed of a uniform continuous phase by stirring and blending, reducing the number of spraying times and eliminating the gray spraying process.

Benefits of technology

It realizes that only two sprays can achieve a light-shielding effect, reduces operating procedures and costs, improves work efficiency, and meets the requirements of energy conservation and environmental protection.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a shading fine silver paint coating for a mini-character substrate and a preparation method thereof, the shading fine silver paint coating comprises a phase A and a phase B. The phase A comprises the following components by weight: 50-60% of acrylic resin, 1-5% of a dispersant, 1-5% of butyl ether, 10-15% of butyl ester, and 1-5% of CAB; the phase B comprises the following components in percentage by weight: 20-30% of 5-micron silver paste and 1-5% of polyamide wax; when the preparation method is applied, a fine silver shading product can be obtained only by spraying paint twice, firstly performing bottoming and brightening on white paint once and directly spraying the paint of the product in the next step, so that a gray spraying process is omitted, the operation process and cost are reduced, the working efficiency is improved, and the requirements of energy conservation and environmental protection are met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of coatings, and in particular relates to a light-shielding fine silver paint coating for a mini-character substrate and a preparation method thereof. Background Art

[0002] Mini fonts are a typeface logo that has emerged in recent years. They are small in size, exquisite in design, and made of polymer materials. They have a variety of materials and production processes and can be widely used in commercial stores, exhibitions and other fields to enhance brand image and space quality.

[0003] Mini letters are made of a variety of materials, each of which has its own unique charm and advantages. Among them, metal mini letters are popular in outdoor environments because of their stability, durability and resistance to damage. Metal materials such as stainless steel, brass, and aluminum not only have excellent weathering and corrosion resistance, but can also show a variety of decorative effects through frosting, gold plating, spraying and other treatment methods.

[0004] Acrylic mini letters are an ideal choice for interior signage design with their smooth, delicate appearance and rich colors and textures. Acrylic sheets are available in a variety of colors and textures, such as transparent, white, and colorful, to meet different decorative needs. At the same time, acrylic mini letters can also be made into a variety of complex three-dimensional shapes, adding a unique artistic atmosphere to the space.

[0005] Wood mini letters bring a warm and natural atmosphere to the space with their natural texture and grain. Natural wood or artificial board can be used as the production material, and different colors and textures can be customized according to needs, so that the mini letters can be integrated with the space environment and create a harmonious and comfortable atmosphere.

[0006] The mini letters made of the above materials are light-transmitting after use, while some merchants choose opaque mini letters, that is, mini letters with shading properties. When producing such light-shielding mini letters, the process is generally a process of spraying three coats of paint. First, white is used for base brightening, then gray is used for shading, and finally colored topcoat is sprayed to obtain a light-shielding product. This three-layer molding process has a relatively high cost expenditure, and at the same time, the operation process is increased, and work efficiency is reduced. Due to the large number of spray layers, it does not meet environmental protection requirements and is not energy-saving and environmentally friendly. Summary of the invention

[0007] The purpose of the present invention is to overcome the above-mentioned deficiencies of the prior art and provide a light-shielding fine silver paint coating for a mini-letter substrate and a preparation method thereof to solve the above-mentioned problems.

[0008] To achieve the above object, the present invention adopts the following technical scheme: a light-shielding fine silver paint coating for a mini-letter substrate, comprising a phase A and a phase B, wherein the components of the phase A are as follows by weight: 50-60% acrylic resin, 1-5% dispersant, 1-5% butyl ether, 10-15% butyl ester, and 1-5% CAB; The weight ratio of the components of the B phase is: 20-30% of 5 μm silver paste and 1-5% of polyamide wax.

[0009] Preferably, the components of phase A are as follows by weight: acrylic resin 54.3%, dispersant 2%, butyl ether 3%, butyl ester 12.2%, CAB 2%; The weight ratio of the components of the B phase is: 25% of 5 μm silver paste and 1.5% of polyamide wax.

[0010] Preferably, the components of phase A are as follows by weight: acrylic resin 52%, dispersant 3%, butyl ether 2%, butyl ester 12%, CAB 2%; The weight ratio of the components of the B phase is: 27% of 5 μm silver paste and 2% of polyamide wax.

[0011] Preferably, the components of phase A are as follows by weight: 55% acrylic resin, 3% dispersant, 3% butyl ether, 13.5% butyl ester, and 1.5% CAB; The weight ratio of the components of the phase B is: 23% of 5 μm silver paste and 1% of polyamide wax.

[0012] Preferably, the weight ratio of the components of phase A and phase B is (0.7-0.8): (0.2-0.3).

[0013] A method for preparing a light-shielding fine silver paint coating for a mini-letter substrate comprises the following steps: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 700-800 rpm for 3 minutes to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 300-400 rpm for 2 min; (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product.

[0014] The beneficial effects of the present invention are: 1. The mini-letter shading fine silver paint coating of the present invention has a two-component structure, wherein phase A is a blend formed by resin, powder, solvent, etc., and phase B is silver paste and additives. The two are blended and dispersed to form a uniform continuous phase, so that the paint forms a fine silver shading coating with good film-forming properties on the surface of the substrate.

[0015] 2. When the preparation of the present invention is used, only two coats of paint need to be sprayed, firstly, white is used for base brightening, and then the paint of the product is directly sprayed to obtain a fine silver shading product, thereby eliminating the gray spraying process. The traditional second step and the third step are combined to form a fine silver paint product with both shading and topcoat, thereby reducing the operation process and cost, improving work efficiency, and meeting the requirements of energy saving and environmental protection. DETAILED DESCRIPTION

[0016] In order to better understand the present invention, the technical solution of the present invention is described in detail with specific examples below. Example

[0017] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of the phase A are as follows by weight: 54.3% acrylic resin, 2% dispersant, 3% butyl ether, 12.2% butyl ester, and 2% CAB; The weight ratio of the components of the B phase is: 25% of 5 μm silver paste and 1.5% of polyamide wax.

[0018] The weight ratio of phase A to phase B is 0.735:0.265.

[0019] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 700 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B evenly at 300 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product. Example

[0020] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of the phase A are as follows by weight: 52% acrylic resin, 3% dispersant, 2% butyl ether, 12% butyl ester, and 2% CAB; The weight ratio of the components of the B phase is: 27% of 5 μm silver paste and 2% of polyamide wax.

[0021] The weight ratio of phase A to phase B is 0.71:0.29.

[0022] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 750 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 400 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product. Example

[0023] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of phase A are as follows by weight: 55% acrylic resin, 3% dispersant, 3% butyl ether, 13.5% butyl ester, and 1.5% CAB; The weight ratio of the components of the phase B is: 23% of 5 μm silver paste and 1% of polyamide wax.

[0024] The weight ratio of phase A to phase B is 0.76:0.24.

[0025] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 800 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 350 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product. Example

[0026] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of the phase A are as follows by weight: 53% acrylic resin, 2% dispersant, 2% butyl ether, 11% butyl ester, and 2% CAB; The weight ratio of the components of the B phase is: 29.5% of 5 μm silver paste and 1.5% of polyamide wax.

[0027] The weight ratio of phase A to phase B is 0.7:0.3.

[0028] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 800 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 350 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product. Example

[0029] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of the phase A are as follows by weight: 56% acrylic resin, 2% dispersant, 2% butyl ether, 12% butyl ester, and 2% CAB; The weight ratio of the components of the B phase is: 25% of 5 μm silver paste and 1% of polyamide wax.

[0030] The weight ratio of phase A to phase B is 0.74:0.26.

[0031] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 800 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 350 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product. Example

[0032] A light-shielding fine silver paint for a mini-letter substrate, wherein the components of the phase A are as follows by weight: 57% acrylic resin, 2% dispersant, 3% butyl ether, 12% butyl ester, and 2% CAB; The weight ratio of the components of the phase B is: 23% of 5 μm silver paste and 1% of polyamide wax.

[0033] The weight ratio of phase A to phase B is 0.76:0.24.

[0034] The preparation method of the above-mentioned mini-letter light-shielding fine silver paint coating is as follows: (1) Putting the A phase components consisting of acrylic resin, dispersant, butyl ether, butyl ester and CAB into a stirring tank in an inert environment and stirring at a speed of 800 rpm for 3 min to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 350 rpm for 2 min. (3) Blending the phase A and the phase B, stirring evenly to obtain a product, and discharging the product.

[0035] Test Example 1 The coating was tested using the following methods: The coatings obtained in the multiple embodiments are uniformly and single-sidedly applied on a plurality of transparent substrates of the same area; Light blocking test: judge by visual inspection, turn on the flashlight device on the mobile phone, and then stick the transparent substrate to the light source at zero distance to see its light transmittance. The substrate selected is PMMA transparent substrate with a thickness of 1.8mm.

[0036] Test results: Test conclusion: The coating dry film thickness of Examples 1 to 6 can achieve a certain light-shielding effect, or even a complete light-shielding effect, when it is between 50-80um. Within a certain range, it can be achieved that when the dry film thickness is 40um, basically complete light-shielding can be achieved, and when the dry film thickness is 50um, complete light-shielding can be achieved. When the B phase composed of 5μm silver paste accounts for between 0.2 and 0.3 of the total proportion, the light-shielding phenomenon can be achieved. This shows that the technical solution of the present invention has excellent light-shielding performance.

[0037] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A light-shielding fine silver paint for a mini-letter substrate, characterized in that: The invention comprises a phase A and a phase B, wherein the components of the phase A are as follows by weight: 50-60% acrylic resin, 1-5% dispersant, 1-5% butyl ether, 10-15% butyl ester, and 1-5% CAB; and the components of the phase B are as follows by weight: 20-30% 5μm silver paste and 1-5% polyamide wax.

2. The light-shielding fine silver paint for mini-letter substrate according to claim 1, characterized in that: The components of phase A are as follows by weight: 54.3% acrylic resin, 2% dispersant, 3% butyl ether, 12.2% butyl ester, and 2% CAB; the components of phase B are as follows by weight: 25% 5μm silver paste and 1.5% polyamide wax.

3. The light-shielding fine silver paint for mini-letter substrate according to claim 1, characterized in that: The components of phase A are as follows by weight: 52% acrylic resin, 3% dispersant, 2% butyl ether, 12% butyl ester, and 2% CAB; the components of phase B are as follows by weight: 27% 5μm silver paste and 2% polyamide wax.

4. The light-shielding fine silver paint for mini-letter substrate according to claim 1, characterized in that: The components of phase A are as follows by weight: 55% acrylic resin, 3% dispersant, 3% butyl ether, 13.5% butyl ester, and 1.5% CAB; the components of phase B are as follows by weight: 23% 5μm silver paste and 1% polyamide wax.

5. The light-shielding fine silver paint for mini-letter substrate according to claim 1, characterized in that: The weight ratio of the components of phase A and phase B is (0.7-0.8): (0.2-0.3).

6. A method for preparing a light-shielding fine silver paint for a mini-letter substrate, which is used to prepare the light-shielding fine silver paint for mini-letter substrates according to any one of claims 1 to 5, characterized in that: The following steps are involved: (1) The components of phase A, consisting of acrylic resin, dispersant, butyl ether, butyl ester, and CAB, are placed in a stirring tank in an inert environment and stirred at a speed of 700-800 rpm for 3 minutes to obtain a co-polymer resin; (2) Mix the ingredients of phase B uniformly at 300-400 rpm for 2 min; (3) Blending the phase A and the phase B, stirring evenly to obtain the product, and discharging the product.