Method and equipment for improving low-concentration TMAH corrosion uniformity
By optimizing the circulation system and heating efficiency of low-concentration TMAH corrosion liquid, combined with the timed lifting device and double-layer corrosion tank design, the toxicity and bubble accumulation problems of high-concentration TMAH are solved, and the uniformity and stability of the TMAH corrosion process are achieved. Protect the health of the operator and improve the quality of the silicon needle.
Patent Information
- Application Number
- CN202410990350.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-12
AI Technical Summary
In the TMAH corrosion process, high concentration of drug solution is easy to volatilize and has high neurotoxicity. The accumulation of hydrogen bubbles in low concentration solutions affects uniformity and surface roughness, and temperature and flow control are difficult to ensure corrosion efficiency and stability.
Using a low concentration of 2.38% TMAH corrosion liquid, the flow rate of 2-4 liters/min and the temperature of 78-82 ℃ is controlled through the circulation system, and the wafer is lifted regularly to release bubbles, combining the double-layer structure of the outer and inner grooves and The circulating flow design ensures uniform distribution of corrosion liquid and stable temperature.
It significantly reduces the risk of operator exposure to harmful substances, improves corrosion uniformity and stability, reduces the adverse effects of bubbles on the surface, and ensures consistency of silicon needle length and overall quality.
Smart Images

Figure CN118943048A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductors, and in particular relates to a method and a device for improving the uniformity of low-concentration TMAH corrosion. Background Art
[0002] TMAH (tetramethylammonium hydroxide), with the chemical formula (CH3)4NOH, is a strongly alkaline organic compound widely used in the micro-processing of silicon wafers. It exhibits different corrosion rates on different crystal planes of silicon, especially on the (111) crystal plane, which has a very low corrosion rate. This property makes TMAH an ideal etchant for silicon materials. After etching the silicon wafer with TMAH, a slope of 54.74° will be formed on its surface. This property is crucial for manufacturing complex structures such as silicon needles and V-grooves.
[0003] During the etching process of silicon needles, a groove is first etched on the surface of the silicon wafer, and a 5000 angstrom oxide film and a 2000 angstrom nitride film are retained at the bottom and sidewalls of the groove. Due to the large difference in the etching rate of TMAH in the (110) crystal orientation and the (111) crystal orientation, the silicon material in the trench protection area will be corroded downward at an angle of 54.74° to form a needle-like structure. However, in the unprotected area, since multiple crystal planes are exposed to the TMAH solution at the same time, no obvious slope will be formed.
[0004] At present, the technical challenges in the TMAH etching process include: the traditional TMAH etching method usually uses a high concentration of 25% solution and adds an active agent to improve the uniformity and roughness of the corrosion. However, in terms of the process requirements of silicon needles, it is necessary to form a silicon needle with a needle length of about 600 microns. The etching rate of a 25% TMAH solution at a temperature of 80°C is 10 to 15 microns per hour, and it takes about 48 hours to etch to the required needle length. Long-term corrosion will seriously affect the process stability and the uniformity of the needle length. Moreover, high-concentration TMAH solution is volatile at high temperatures, and its neurotoxicity also increases the danger of operation. On the other hand, when using a low-concentration TMAH solution, the hydrogen produced during the reaction will form bubbles. The accumulation of these bubbles will seriously affect the uniformity and surface roughness of the silicon needle corrosion, resulting in inconsistent silicon needle lengths.
[0005] The uniformity of TMAH corrosion is closely related to the concentration, flow rate and temperature of the chemical solution. In order to obtain the best uniformity, the minimum circulation flow rate needs to be guaranteed. However, a smaller circulation flow rate may reduce the heating efficiency of the heater, resulting in uneven temperature of the chemical solution in the TMAH tank, which in turn affects the uniformity of corrosion. Therefore, how to solve the problems of bubble accumulation and chemical solution temperature control while ensuring corrosion efficiency is a key technical problem that needs to be solved in the TMAH corrosion process. Summary of the invention
[0006] In order to solve all or part of the problems of the above prior art, the present invention provides a method and equipment for improving the uniformity of low-concentration TMAH etching, by optimizing the circulation system and heating efficiency of the etching solution, regularly lifting the wafer from the etching solution, and releasing the hydrogen bubbles generated during the etching process, thereby effectively improving the uniformity and stability of the low-concentration TMAH etching process.
[0007] To achieve the above object, the present invention provides the following technical solutions:
[0008] A method for improving the uniformity of low-concentration TMAH corrosion comprises the following steps:
[0009] S1. Prepare TMAH etching solution with a concentration of 2.38±0.003%, pour it into the etching tank, place the wafer in the pulling device, and make the wafer completely immersed in the etching solution;
[0010] S2. Start the circulation system, control the circulation flow rate of the corrosive liquid within the range of 2-4 liters / minute, and turn on the heating device to heat the corrosive liquid to 78-82°C;
[0011] S3. The lifting device performs a lifting operation once every hour to completely separate the wafer from the etching solution for 3-5 seconds to release bubbles generated during the etching process;
[0012] S4. After the etching reaction is completed, the wafer is taken out and cleaned and dried to remove surface residues.
[0013] This method significantly reduces the risk of operators being exposed to harmful substances by reducing the reliance on high-concentration TMAH solution. The neurotoxicity of TMAH solution is effectively controlled at low concentrations, thereby protecting the health of operators. At the same time, by precisely controlling the temperature and circulation flow of the etching solution, the consistency and stability of the etching process are ensured, and the problem of uneven etching caused by temperature fluctuations or uneven flow is avoided. In addition, by regularly lifting the wafer, the bubbles generated during the etching process are effectively released, reducing the adverse effects of bubbles on the wafer surface, and further improving the uniformity of etching.
[0014] The present invention also provides a TMAH etching device, which is implemented by the above method and comprises:
[0015] An etching tank is used to contain an etching liquid and perform etching treatment on the wafer placed therein;
[0016] A lifting device is arranged in the etching tank, the wafer is placed in the lifting device, and the lifting device regularly lifts the wafer above the level of the etching solution to release bubbles produced by the reaction;
[0017] The circulation system is used for circulating the etching liquid in the etching tank so that the etching liquid is evenly distributed in the tank.
[0018] The lifting device in this equipment is designed to lift the wafer at a fixed time to temporarily separate it from the etching liquid surface, thereby effectively releasing the hydrogen bubbles generated during the etching reaction. This mechanism significantly reduces the adhesion of bubbles on the wafer surface, avoids the surface unevenness and roughness problems caused by bubble accumulation, and improves the overall quality of the silicon wafer after etching.
[0019] The etching tank comprises an outer tank and an inner tank, both of which are filled with etching liquid. The pulling device is placed in the inner tank. The circulation system extracts the etching liquid from the outer tank and transports it to the inner tank, and then overflows from the inner tank back to the outer tank, forming a circulating flow, thereby ensuring the uniform distribution of the etching liquid in the two tanks.
[0020] The corrosive liquid in the inner tank overflows into the outer tank through the overflow channel, and the overflow channel is an opening above the inner tank or an overflow hole opened on the side wall of the inner tank. This natural overflow method reduces the wear of mechanical parts and prolongs the service life of the equipment.
[0021] The outer tank is installed on the outer wall of the inner tank, and the volume of the corrosive liquid contained by the outer tank and the inner tank is greater than the designed volume of the inner tank. The outer tank is installed on the outer wall of the inner tank to form a double-layer structure. The outer tank acts as an insulation layer and contains liquid overflow. This design not only provides additional insulation effect, but also increases the ability to contain corrosive liquid.
[0022] The side walls of the inner tank in contact with the air are all installed with heat-insulating components, so that the temperature of the inner tank is maintained at 78-82° C. The installation of the heat-insulating components can effectively reduce the heat loss caused by contact with the air, thereby reducing the temperature fluctuation.
[0023] The circulation system includes a circulation pipeline and a power device. The inlet end of the circulation pipeline is connected to the bottom of the outer tank, and the outlet end extends into the inner tank. The power device is arranged on the circulation pipeline to provide the power required for the circulation of the corrosive liquid in the outer tank and the inner tank.
[0024] The circulation pipeline is also provided with a heating device, which is used to heat the corrosive liquid to a preset temperature.
[0025] The circulation pipeline is also provided with a filtering device to remove impurities in the corrosive liquid.
[0026] The lifting device includes a lifting arm and a carrying platform connected to the bottom of the lifting arm, a bracket is placed on the carrying platform, and the wafer is placed on the bracket. Through the design of the lifting arm, the operator can easily move the wafer to the desired position and ensure that the wafer is not accidentally damaged or contaminated during the operation.
[0027] The present invention has at least the following beneficial effects:
[0028] 1) The present invention reduces the dependence on high-concentration TMAH solution and significantly reduces the risk of operators being exposed to harmful substances. The neurotoxicity of low-concentration TMAH solution is effectively controlled, protecting the health of operators. By accurately controlling the temperature and circulation flow of the etching solution, the problem of uneven corrosion caused by temperature fluctuations or uneven flow is effectively avoided. The operation of regularly lifting the wafer reduces the adhesion of bubbles on the wafer surface and prevents the surface unevenness and roughness problems caused by bubble accumulation, thereby significantly improving the overall quality of the silicon wafer after etching.
[0029] 2) The equipment's corrosion tank adopts a double-layer structure design of outer tank and inner tank. This structure enhances the insulation effect. The outer tank surrounds the inner tank to form a natural insulation layer. Together with the insulation components on the side wall of the inner tank, the corrosion liquid is effectively maintained at a stable temperature of 78-82°C, reducing unnecessary heat loss and improving overall thermal efficiency. The integration of the circulation system further optimizes the flow and temperature control of the corrosion liquid. By extracting the corrosion liquid from the outer tank and transporting it to the inner tank, and then returning it to the outer tank through overflow, an efficient circulation flow is formed, which not only promotes the uniform transfer of heat, but also enhances the uniformity of the corrosion liquid. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] In order to more clearly illustrate the technical solutions in the specific embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0031] Figure 1 It is a front view of the TMAH etching equipment in an embodiment of the present invention.
[0032] Figure 2 It is a top view of the etching tank of the TMAH etching equipment in an embodiment of the present invention.
[0033] Figure numerals: 1-outer tank; 2-inner tank; 201-heat-insulating component; 3-lifting device; 301-lifting arm; 302-carrying platform; 4-circulation pipeline; 5-power device; 6-heating device; 7-filtering device. DETAILED DESCRIPTION
[0034] The technical solutions in the specific embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] Combined with reference Figure 1 , Figure 2 As shown, the present invention provides a method for improving the corrosion uniformity of low-concentration TMAH (tetramethylammonium hydroxide), comprising the following steps:
[0036] S1. Prepare TMAH etching solution with a concentration of 2.38±0.003% and pour it into the etching tank. Then, place the wafer on the carrying platform 302 of the lifting device 3 to ensure that the wafer is completely immersed in the etching solution to facilitate uniform etching;
[0037] S2. Start the circulation system, adjust the circulation flow rate to 2 to 4 liters / minute, and start the heating device 6 to heat the corrosion liquid to 78 to 82°C to ensure that the corrosion reaction is carried out at the optimal temperature;
[0038] S3. Every 1 hour, the lifting device 3 automatically performs a lifting action to completely separate the wafer from the etching solution for 3 to 5 seconds to release gas bubbles that may be generated during the etching process, thereby avoiding damage to the wafer surface caused by bubble accumulation;
[0039] S4. After the corrosion reaction is completed, the wafer is taken out and necessary cleaning and drying treatments are performed to completely remove the corrosion residues on the surface of the wafer to ensure the cleanliness of the wafer and the smooth progress of subsequent processes.
[0040] This method significantly reduces the risk of operators being exposed to harmful substances by using a low-concentration TMAH etching solution. At the same time, by precisely controlling the temperature and circulation flow of the etching solution, the consistency and stability of the etching process are ensured, effectively avoiding the problem of uneven corrosion caused by temperature fluctuations or uneven flow. In addition, the wafer is lifted every hour to release the bubbles generated during the etching process, which further improves the uniformity of the corrosion. After the etching reaction is completed, the surface residue is removed by cleaning and drying, which improves the cleanliness of the wafer and reduces the pollution problem in the subsequent processing process. This method not only improves the safety and environmental friendliness of the operation, but also reduces the material cost and wafer scrap rate in the long run, thereby improving the economic benefits.
[0041] The present invention also provides a TMAH etching device, which is implemented in conjunction with the above method. The device is mainly composed of the following parts: an etching tank, a pulling device 3 and a circulation system. The etching tank is used to contain the TMAH etching solution and to perform etching treatment on the wafer placed therein. The pulling device 3 is arranged in the etching tank, and the wafer is placed in the pulling device 3, which is used to carry and regularly lift the wafer so that it is temporarily separated from the etching solution surface. This step helps to release the gas bubbles generated by the chemical reaction, thereby avoiding the accumulation of bubbles on the surface of the wafer, thereby reducing the risk of surface damage. The circulation system ensures that the etching solution forms a uniform flow in the tank, and through continuous circulation, maintains the uniform distribution of the etching solution, and achieves a uniform etching effect on the surface of the wafer.
[0042] The etching tank includes an outer tank 1 and an inner tank 2, both of which are filled with etching liquid. A lifting device 3 is provided in the inner tank 2 for placing and manipulating the wafer to achieve its precise positioning and timed lifting in the etching liquid. The circulation system is responsible for extracting the etching liquid from the outer tank 1 and transporting it to the inner tank 2, and realizing the reflux of the etching liquid to the outer tank 1 through the overflow channel of the inner tank 2, forming an effective circulation flow. These overflow channels can be openings located above the inner tank 2 or overflow holes on the side wall of the inner tank 2. The outer tank 1 is fixed to the outer wall of the inner tank 2, and the design ensures that the total amount of etching liquid contained by the outer tank 1 and the inner tank 2 exceeds the independent capacity of the inner tank 2, thereby providing sufficient space for the overflow circulation of the etching liquid. In addition, the side wall of the inner tank 2 is equipped with a heat preservation component 201 in contact with the air. In this embodiment, a heat preservation heating patch is specifically used. The function of these components is to maintain the temperature of the etching liquid in the inner tank 2 within the range of 78-82°C, providing a stable thermal environment for the TMAH etching process. Through this design, the present invention not only ensures the uniform distribution and flow of the etching liquid, but also improves the efficiency of the etching process and the quality of the wafer surface treatment through precise temperature control. In addition, the use of the lifting device 3 reduces the risk of bubble attachment, further improving the precision and consistency of wafer processing.
[0043] The circulation system includes a circulation pipeline 4 and a power device 5. The inlet end of the circulation pipeline 4 is located at the bottom of the outer tank 1 to ensure that the corrosive liquid in the outer tank 1 can be extracted, and the outlet end extends to the bottom of the inner tank 2 to achieve uniform delivery to the inner tank 2. The power device 5 is installed on the circulation pipeline 4 to provide the necessary power for the circulation of the corrosive liquid between the inner and outer tanks. In this embodiment, the power device 5 is a diaphragm pump, which reduces the circulation flow rate to the minimum (2-4 liters / minute) by reducing the input air pressure of the diaphragm pump. In order to ensure that the corrosive liquid is maintained at the optimal temperature during the reaction process, the circulation pipeline 4 is equipped with a heating device 6, which can heat the corrosive liquid to a predetermined temperature range to optimize the corrosion effect. In addition, a filtering device 7 is also integrated on the circulation pipeline 4, which specifically adopts an Interg filter with a precision of 0.1 microns. This high-precision filter can effectively remove tiny impurities in the corrosive liquid, ensure the purity of the corrosive liquid, and thus improve the quality of wafer corrosion. In other specific embodiments, other types of filters can also be used.
[0044] The lifting device 3 includes a lifting arm 301 and a carrying platform 302. The lifting arm 301 is designed to perform vertical movement, and the bottom of the lifting arm 301 is fixedly connected to the carrying platform 302. The carrying platform 302 is specifically used to place wafers, and the wafers are fixed on the carrying platform 302 through special brackets to ensure stability during the entire lifting process. Through the precise control of the lifting arm 301, the wafer can be smoothly lowered into the corrosive liquid for predetermined treatment, or lifted above the liquid surface when necessary. This operation not only promotes the release of gases generated during the chemical reaction, but also effectively avoids the accumulation of bubbles on the surface of the wafer, thereby significantly reducing the risk of surface damage caused by bubble adhesion.
[0045] The equipment provided by the present invention realizes the uniform distribution and flow of the etching liquid on the surface of the wafer through the inner and outer groove design and the circulation system of the etching groove, and effectively avoids the problem of uneven etching of the wafer surface caused by uneven distribution of the etching liquid. The heat preservation heating patch equipped on the side wall of the inner groove 2 can maintain the etching liquid in a stable temperature range of 78-82°C, providing an ideal thermal environment for the TMAH etching process, thereby improving the etching efficiency and quality. The design of the pulling device 3 allows the wafer to be separated from the etching liquid at a fixed time, releasing the gas bubbles generated by the chemical reaction, reducing the possibility of bubbles accumulating on the surface of the wafer, and reducing the risk of surface damage. In addition, the automated operation of the equipment reduces the possibility of human operation errors and improves operational safety. By accurately controlling the etching process, the scrapping of wafers caused by uneven corrosion is reduced, and the utilization rate and production efficiency of materials are improved. The circulation system and the filter device 7 ensure the purity and stability of the etching liquid, reduce the frequency of replacing the etching liquid, and thus reduce the production cost. At the same time, the use of low-concentration TMAH and the high-precision filter device 7 reduce potential pollution to the environment, meeting the requirements of green production. The modular design of the equipment facilitates maintenance and cleaning, helps maintain long-term stable operation of the equipment, ensures process continuity and consistency, and facilitates large-scale production.
[0046] In summary, the technical solution and equipment design of the present invention show significant advantages in improving production efficiency, ensuring operational safety, and reducing environmental impact, providing an innovative, efficient and environmentally friendly solution for the wet etching process in the semiconductor manufacturing industry.
[0047] It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made to the present invention without departing from the principles of the present invention. These improvements and modifications also fall within the scope of protection of the claims of the present invention.
Claims
1. A method for improving the uniformity of low-concentration TMAH corrosion, characterized in that: The following steps are involved: S1. Prepare a TMAH etching solution with a concentration of 2.38±0.003%, pour it into the etching tank, place the wafer in the pulling device (3), and completely immerse the wafer in the etching solution; S2. Start the circulation system, control the circulation flow rate of the corrosion liquid within the range of 2-4 liters / minute, and turn on the heating device (6) to heat the corrosion liquid to 78-82°C; S3. The lifting device (3) performs a lifting operation once every hour to completely separate the wafer from the etching solution for 3-5 seconds to release bubbles generated during the etching process; S4. After the etching reaction is completed, the wafer is taken out and cleaned and dried to remove surface residues.
2. A TMAH etching device, implemented by the method of claim 1, characterized in that: include: An etching tank is used to contain an etching liquid and perform etching treatment on the wafer placed therein; A lifting device (3) is arranged in the etching tank, the wafer is placed in the lifting device (3), and the lifting device (3) regularly lifts the wafer above the level of the etching solution to release bubbles produced by the reaction; The circulation system is used for circulating the etching liquid in the etching tank so that the etching liquid is evenly distributed in the tank.
3. The device according to claim 2, characterized in that The etching tank comprises an outer tank (1) and an inner tank (2), wherein the outer tank (1) and the inner tank (2) are both filled with etching liquid, the pulling device (3) is placed in the inner tank (2), and the circulation system extracts the etching liquid from the outer tank (1) and transports it to the inner tank (2), and then overflows from the inner tank (2) back to the outer tank (1), thereby forming a circulation flow.
4. The device according to claim 3, characterized in that The corrosive liquid in the inner groove (2) overflows into the outer groove (1) through an overflow channel, wherein the overflow channel is an upper opening of the inner groove (2) or an overflow hole opened on a side wall of the inner groove (2).
5. The device according to claim 3, characterized in that The outer tank (1) is installed on the outer wall of the inner tank (2), and the volume of the corrosive liquid contained in the outer tank (1) and the inner tank (2) is greater than the designed volume of the inner tank (2).
6. The device according to claim 5, characterized in that The side walls of the inner tank (2) in contact with the air are all installed with heat-insulating components (201), so that the temperature of the inner tank (2) is maintained at 78-82°C.
7. The device according to claim 3, characterized in that The circulation system comprises a circulation pipeline (4) and a power device (5); the inlet end of the circulation pipeline (4) is connected to the bottom of the outer tank (1), and the outlet end extends into the inner tank (2); the power device (5) is arranged on the circulation pipeline (4) and is used to provide the power required for the circulation of the corrosive liquid in the outer tank (1) and the inner tank (2).
8. The device according to claim 7, characterized in that The circulation pipeline (4) is also provided with a heating device (6), and the heating device (6) is used to heat the corrosive liquid to a preset temperature.
9. The device according to any one of claims 7 or 8, characterized in that The circulation pipeline (4) is also provided with a filtering device (7) to remove impurities in the corrosive liquid.
10. The device according to claim 2, characterized in that The lifting device (3) comprises a lifting arm (301) and a carrying platform (302) connected to the bottom of the lifting arm (301), a bracket is placed on the carrying platform (302), and the wafer is placed on the bracket.