Sintering paste for electrically conductive and integrally bonded connection of aluminum conductor covered with oxide layer to electronic component, method and electronic product
The connection between aluminum conductors and electronic components covered by the oxide layer of nano-scale particle sintering paste is solved by diffusion of nano-scale particle sintering paste and electronic components at low pressure and low temperature, and the problem of bonding of aluminum conductors and electronic components is achieved, and the cost-effective locking of conductive materials is improved. The reliability and service life of the connection are provided.
Patent Information
- Application Number
- CN202410559860.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-10
- Filing Date
- 2024-05-08
- Publication Date
- 2024-11-12
AI Technical Summary
Since the Al2O3 oxide layer formed on the surface of the aluminum conductor is difficult to efficiently engage with the electronic components, the existing methods are complex and costly.
Using sintered paste composed of nano-scale particles, the aluminum conductor covered with the oxide layer is locked and connected to the conductive material of the electronic component through the diffusion process at low pressure and low temperature, and the nano-scale particles pass through the lattice defect of the oxide layer. Alloy with electronic components.
The conductive and material-locking connection between the aluminum conductor and the electronic component is realized, which reduces costs, improves the reliability and service life of the connection, and avoids the use of aggressive fluxes.
Smart Images

Figure CN118946030A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a sintering paste according to the subject matter of claim 1. In particular, the invention relates to a method for electrically conductively and cohesively connecting an aluminum conductor covered with an oxide layer to an electronic component and in particular also to an electronic product having a corresponding connection. Background Art
[0002] Due to various physical and technical advantages, copper is a material that is dominant in many technical fields and is used to produce electrical conductors. In electronic devices, soldering, as a prior art, with the aid of (now mainly lead-free) tin-based solders has been established as a material-locking joining method for corresponding copper conductors and electronic components. An economically and technically interesting alternative for copper conductors is electrical conductors made of aluminum materials, because they can currently be provided more cost-effectively than copper conductors and at the same time have a more favorable conductivity and density ratio than copper conductors. However, especially due to the spontaneously formed, high-melting, only a few nanometers thick and firmly adhered Al2O3 oxide layer on the surface of the aluminum conductor in the air, aluminum electrical conductors can only be joined to electronic components in a material-locking manner according to complex and expensive methods (see, for example, US2019 / 0035764 A1 or DE 3115856 A, 1). Summary of the invention
[0003] It is therefore an object of the present invention to provide an improved or at least a different embodiment for a material-locking joining method for aluminum electrical conductors.
[0004] In the invention, this object is achieved in particular by the subject matter of the independent claims. Advantageous embodiments are the subject matter of the dependent claims and the description.
[0005] The invention makes use of the knowledge that the Al2O3 oxide layer adhering to the aluminum conductor has imperfections, such as lattice defects and the like, which allow diffusion processes under given marginal conditions. The basic idea of the invention is therefore to enable an electrically conductive, materially bonded connection between an aluminum conductor covered with an oxide layer on the one hand and an electronic component on the other hand by means of a sintering paste according to the invention and under the influence of pressure and relatively low temperatures.
[0006] According to the invention, a sintering paste is proposed for connecting an aluminum conductor covered with an oxide layer to an electronic component in an electrically conductive and material-locking manner, wherein the sintering paste has nanoscale particles. These nanoscale particles are suitable for or are provided for forming an electrically conductive, heat-conducting, material-locking connection between an aluminum conductor covered with an oxide layer and an electronic component by diffusion under the influence of pressure and temperature. Due to the nanoscale particles and under the influence of pressure and temperature, the material of the aluminum conductor can be alloyed on the one hand, wherein the invention makes use of the knowledge that the nanoscale particles diffuse through lattice defects and the like of the Al2O3 oxide layer covering the aluminum conductor. On the other hand, the nanoscale particles alloy the material of the contact element of the electronic component. As a result, despite the presence of an Al2O3 oxide layer on the aluminum conductor, an electrically conductive, material-locking connection between the aluminum conductor and the electronic component can be provided according to the proposed sintering paste. The nanoscale particles have a size suitable for the purpose, which is in the nanometer range.
[0007] Generally, the range of about 1 to 100 nm is referred to as the nanoscale.
[0008] Pure aluminum or aluminum alloys, in particular alloys consisting of aluminum and, for example, small proportions of copper and / or silicon, are expediently conceivable as materials for the aluminum conductor.
[0009] In the present case, the term "aluminum conductor" is to be understood in a broad sense. The aluminum conductor can particularly represent any electrically conductive body made of an aluminum material as defined above. In the present case, the aluminum conductor can be, for example, an aluminum conductor track, an electrical busbar or any aluminum conductor component. The corresponding aluminum conductor track can have, in addition to the actual conductor track, an integral connecting element made of aluminum material, such as an aluminum contact pin or an aluminum contact lead, and / or at least one connecting surface made of aluminum material, such as an aluminum material coating. The actual conductor track can be made of aluminum material or another material.
[0010] The aluminum conductor can be arranged on a supporting structure. The supporting structure is expediently implemented as a PCB (printed circuit board, PCB) or an IMS (insulated metal substrate), wherein the aluminum conductor arranged on the PCB or IMS is implemented as an aluminum conductor circuit.
[0011] Furthermore, in the present case, the term “electronic component” is expediently to be understood in a broad sense, ie in the present case, the electronic component may be any electronic component.
[0012] It can be expediently provided that the nanoscale particles are nanoscale nonferrous metal particles. Nonferrous metals within the meaning of the invention are non-ferrous metals, wherein light metals and / or the noble metals gold and platinum are expediently excluded.
[0013] In particular, it can be provided that the nanoscale particles are formed from one or more of the following non-ferrous metals or at least contain one or more of the following non-ferrous metals in proportion: copper, silver or silicon. Depending on the non-ferrous metals specified, the material-bonded connection of the aluminum conductor covered with an oxide layer to the electronic component according to the invention can be achieved at relatively low pressures and relatively low temperatures. The applicant has found in experiments that the non-ferrous metal migrates (diffuses) particularly well and especially at relatively low temperatures through lattice defects and the like in the Al2O3 oxide layer covering the aluminum conductor, which supports the formation of a material-bonded connection of the aluminum conductor covered with an oxide layer to the electronic component.
[0014] It can be expedient to provide that the sintering paste is iron-free. This means that the sintering paste is iron-free. This further helps to facilitate the formation of a material-locking connection between the aluminum conductor covered with the oxide layer and the electronic component.
[0015] According to another basic concept of the present invention, a method for connecting an aluminum conductor covered with an oxide layer to an electronic component in an electrically conductive and material-locked manner is proposed. In the framework of the method according to the present invention, it is provided that first, an aluminum conductor covered with an oxide layer and an electronic component that can be electrically conductive are provided. Next, a sintering paste according to the above description is applied to, in particular only to, the surface of the aluminum conductor covered with an oxide layer. Then, the electronic component is positioned on the aluminum conductor covered with an oxide layer provided with the sintering paste so that the contact surface of the electronic component and the surface of the aluminum conductor covered with an oxide layer are wetted with the sintering paste. Finally, the composite structure formed by the electronic component, the sintering paste and the aluminum conductor covered with an oxide layer is sintered by means of a sintering press under a predetermined joining pressure and a predetermined joining temperature. Thus, an advantageous method is shown, in which, based on the sintering paste according to the present invention and by means of, for example, a commercially common sintering press, an electrically conductive and material-locked connection between an aluminum conductor covered with an oxide layer and any electronic component having a contact surface can be achieved. The bonding pressure and the bonding temperature set are relatively low, in particular so low that the electronic components are not negatively influenced or damaged when forming the material-locked connection. The proposed method can also be used as an alternative to the bonding of aluminum conductors that is common in practice and to increase the service life and reliability of such bonded connections. According to the proposed method, aluminum can be used as a more cost-effective conductor material, thereby providing cost reduction potential for a large number of electronic products. In addition, the proposed method can save the use of aggressive flux or the like.
[0016] It can be expediently provided within the scope of the method that the sintering paste is applied to the surface of the oxide-layer-covered aluminum conductor by means of a printing method, in particular a screen printing method. As a result, a layer of sintering paste with a uniform layer thickness can be applied to the surface by simple and cost-effective means. It is obvious that the present inventive method is not limited to the use of printing methods, but in principle also can be used for application methods that have the same effect.
[0017] Furthermore, it is expedient to provide within the scope of the method that during the sintering of the composite structure, a predetermined joining pressure of 5 MPa to 50 MPa, in particular 10 MPa to 20 MPa, and / or during the sintering of the composite structure, a predetermined joining temperature of 100° C. to 400° C., in particular 150° C. to 250° C. has been found that, given a corresponding joining pressure and a corresponding joining temperature, the nanoscale particles contained in the sintering paste used can migrate (diffuse) particularly well through lattice defects and the like of the Al2O3 oxide layer covering the aluminum conductor and can alloy with the material of the aluminum conductor. Preferably, during the sintering of the composite structure, the joining pressure set in the method is in the range of 10 MPa to 20 MPa, and / or during the sintering of the composite structure, the joining temperature is in the range of 150° C. to 250° C. With these method parameters (joining pressure and / or joining temperature), pressure-sensitive and / or temperature-sensitive electronic components can also be connected to the aluminum conductor covered by the oxide layer in a material-locking manner.
[0018] It is expedient to provide, within the framework of the method, that the sintering paste is additionally applied to the contact surface of the electronic component. This can also be expediently performed by means of a printing method, in particular a screen printing method. It can be said that a wetting with the sintering paste is thus provided on both sides, namely on the surface of the aluminum conductor covered with the oxide layer on the one hand, and on the contact surface of the electronic component on the other hand. In principle, the application of the sintering paste to the contact surface of the electronic component can be carried out after, before or simultaneously with the application of the sintering paste to the surface of the aluminum conductor covered with the oxide layer. By means of the wetting on both sides, it can be ensured that the surface of the aluminum conductor covered with the oxide layer and the surface of the electronic component are completely, i.e. without gaps, covered by the sintering paste.
[0019] In addition, it is suitable to provide in the framework of the method that the surface of the aluminum conductor covered with an oxide layer is pretreated with the help of an iron-free pretreatment agent before the sintering paste is applied to the surface of the aluminum conductor covered with an oxide layer. Suitable, the iron-free pretreatment agent has metal pretreatment particles. Preferably, these metal pretreatment particles can be formed by one or more of the following non-ferrous metals or at least have these non-ferrous metals in proportion: copper, silver or silicon. The metal pretreatment particles of the pretreatment agent adhere to the lattice defects or the like present in the Al2O3 oxide layer of the aluminum conductor, which supports the diffusion process when the composite structure is subsequently sintered. This has the following advantages: the conductive, material-locked connection between the aluminum conductor covered with an oxide layer and the electronic component is constructed more smoothly and with improved process safety. The pretreatment agent can have, for example, an aqueous solution, a salt solution or a diluted acid, the aqueous solution is especially water.
[0020] According to another basic concept of the invention, an electronic product is provided, which has at least one electrically conductive, materially bonded connection between an aluminum conductor covered with an oxide layer of the product and an electronic component of the product, wherein the at least one connection is produced by means of a sinter paste according to the above description and / or by a method according to the above description. This provides an advantageous electronic product, which has at least one advantageous, electrically conductive, materially bonded connection. Depending on the connection implemented accordingly, heat conduction in the electronic product can be improved. In addition, the operating temperature of the corresponding electronic products can be increased, because these electronic products are no longer limited by solder connections (melting temperature of tin is 232° C.) as in typical printed circuit boards, but are only limited by the organic printed circuit board material.
[0021] In summary, it should be pointed out that the present invention preferably relates to a sintering paste for electrically conductively and materially connecting an aluminum conductor covered with an oxide layer to an electronic component, wherein the sintering paste has nanoscale particles which are suitable for forming an electrically conductive, materially connecting the aluminum conductor covered with an oxide layer to the electronic component by diffusion under the influence of pressure and temperature. The present invention particularly relates to a method for electrically conductively and materially connecting an aluminum conductor covered with an oxide layer to an electronic component, and furthermore particularly to an electronic product having at least one electrically conductive, materially connecting connection.
[0022] Further important features and advantages of the invention emerge from the dependent claims, the drawings and the associated description of the figures with the aid of the drawings.
[0023] It is self-evident that the features mentioned above and those yet to be explained below can be used not only in the respectively specified combination but also in other combinations or alone without departing from the scope of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Preferred embodiments of the invention are shown in the drawings and are explained in more detail in the following description, wherein identical reference numerals refer to identical or similar components or components having the same function.
[0025] The accompanying drawings schematically show:
[0026] Figure 1 An aluminum conductor covered with an oxide layer is shown in cross section, which is arranged on a carrier structure designed as a PCB circuit board.
[0027] Figure 2 and 3 Show Figure 1 A cross section in which a method for separating an aluminum conductor covered with an oxide layer and a conductor only at Figure 3 Method for electrically conductively and materially connecting electronic components indicated in the specification. DETAILED DESCRIPTION
[0028] Figure 1 A preferred embodiment of an aluminum conductor 2 is shown, which is arranged on a supporting structure 10 implemented as a PCB circuit board. In the present case, the aluminum conductor 2 exemplarily has an aluminum conductor track 11 composed of an aluminum material capable of conducting electricity and a connecting element 12 mounted on the aluminum conductor track in an integral manner, which connecting element is composed of the same aluminum material. The aluminum conductor 2 is covered with an Al2O3 oxide layer that is only a few nanometers thick, which spontaneously forms on the surface of the aluminum conductor 2 in the air and firmly adheres to the aluminum conductor 2. The PCB circuit board is realized in a manner known per se from an organic printed circuit board material. The aluminum conductor 2 and the supporting structure 10 exemplarily form an arbitrary electronic product 9.
[0029] Figure 2 and 3 The aluminum conductor 2, which is generally designated by 6, is provided for covering the oxide layer with a Figure 3 Method for electrically conductively and cohesively connecting the electronic component 3 indicated in FIG.
[0030] exist Figure 2 As can be seen in the figure, after the electrically conductive, oxide-layer-covered aluminum conductor 2 and the electronic component 3 have been provided, a relatively thin layer of sinter paste 1, symbolized by the cross-hatched small frame, is applied only to the surface 5 of the oxide-layer-covered aluminum conductor 2, which in the present case is formed by the connecting element 12. Next, the electronic component 3 is placed in a Figure 3 1 is positioned in the manner shown in the figure on the aluminum conductor 2 covered with an oxide layer produced with the sintering paste 1. As a result, the contact surface 7 of the contact element 8 of the electronic component 3 facing the aluminum conductor 2 and the surface 5 of the aluminum conductor 2 covered with the oxide layer are completely and in particular without gaps wetted with the sintering paste 1. Subsequently, in a step not shown here, the composite structure formed by the electronic component 3, the sintering paste 1 and the aluminum conductor 2 covered with the oxide layer is sintered by means of a sintering press at a predetermined joining pressure in the range of 5 MPa to 50 MPa, in particular 10 MPa to 20 MPa, and a predetermined joining temperature in the range of 100° C. to 400° C., in particular 150° C. to 250° C.
[0031] The sintering paste 1 has nanoscale particles which are suitable for forming an electrically conductive, material-bonded connection 4 between an oxide-layer-covered aluminum conductor 2 and an electronic component 3 by diffusion under the influence of the joining pressure and the joining temperature within the scope of the method 6. In this context, the invention makes use of the knowledge that the Al2O3 oxide layer adhering to the oxide-layer-covered aluminum conductor 2 has imperfections, such as lattice defects and the like, which allow diffusion processes during sintering under the specified marginal conditions. As a result, despite the presence of the Al2O3 oxide layer on the oxide-layer-covered aluminum conductor 2, an electrically conductive, material-bonded connection between the oxide-layer-covered aluminum conductor 2 and the electronic component 3 can be established according to the proposed sintering paste 1 at relatively low joining pressures and at relatively low joining temperatures.
Claims
1. A sintering paste (1) for electrically conductively and cohesively connecting an aluminum conductor (2) covered with an oxide layer to an electronic component (3), in, The sintering paste (1) comprises nanoscale particles which are suitable for forming an electrically conductive, material-bonded connection (4) between the oxide-layer-covered aluminum conductor (2) and the electronic component (3) by diffusion under the influence of pressure and temperature.
2. The sintering paste (1) according to claim 1, It is characterized in that The nano-scale particles are nano-scale non-ferrous metal particles.
3. The sintering paste (1) according to claim 1 or 2, It is characterized in that The nanoscale particles are formed from one or more of the following non-ferrous metals or contain at least a proportion of one or more of the following non-ferrous metals: copper, silver or silicon.
4. Sintering paste (1) according to any one of the preceding claims, It is characterized in that The sintering paste (1) does not contain iron.
5. A method (6) for electrically conductively and cohesively connecting an aluminum conductor (2) covered with an oxide layer to an electronic component (3), wherein: - firstly, providing an electrically conductive, oxide-layer-covered aluminum conductor (2) and an electronic component (3), - applying the sinter paste (1) according to any one of claims 1 to 4 onto, in particular exclusively onto, the surface (5) of the aluminum conductor (2) covered with the oxide layer, - positioning the electronic component (3) on an aluminum conductor (2) covered with an oxide layer and provided with sintering paste (1) so that the contact surface (7) of the electronic component (3) and the surface (5) of the aluminum conductor (2) covered with the oxide layer are wetted with the sintering paste (1), - sintering the composite structure formed by the electronic component (3), the sintering paste (1) and the aluminum conductor (2) covered with the oxide layer at a predetermined joining pressure and a predetermined joining temperature by means of a sintering press.
6. The method (6) according to claim 5, It is characterized in that The sintering paste (1) is applied to the surface (5) of the oxide-layer-covered aluminum conductor (2) by means of a printing method, in particular a screen printing method.
7. The method (6) according to claim 5 or 6, It is characterized in that - during sintering of the composite structure, the predetermined joining pressure is 5 MPa to 50 MPa, in particular 10 MPa to 20 MPa, and During the sintering of the composite structure, the predefined joining temperature is 100° C. to 400° C., in particular 150° C. to 250° C.
8. The method (6) according to any one of claims 5 to 7, It is characterized in that The sintering paste (1) is additionally applied to the contact surface (7) of the electronic component (3).
9. The method (6) according to any one of claims 5 to 8, It is characterized in that Before applying the sintering paste (1) to the surface (5) of the oxide-layer-covered aluminum conductor (2), the surface (5) of the oxide-layer-covered aluminum conductor (2) is pretreated by means of an iron-free pretreatment agent.
10. An electronic product (9) having at least one electrically conductive, materially bonded connection (4) between an aluminum conductor (2) covered with an oxide layer of the product (9) and an electronic component (3) of the product (9), in, The at least one connection (4) is produced by means of a sinter paste (1) according to any one of claims 1 to 4 or by a method (6) according to any one of claims 5 to 9.
Citation Information
Patent Citations
Electrical circuit configuration
DE3115856A1
Soldering a conductor to an aluminum metallization
US20190035764A1