Non-pathogenic coating of object, object having non-pathogenic coating, and method for arranging non-pathogenic coating on object

By forming a primary cell structure of porous anode and cathode materials on the surface of the object, and using electrochemical reactions to kill pathogens, the environmental pollution caused by copper or silver compounds in the prior art is solved, and non-toxic, environmentally friendly and durable antibacterial and Antiviral coating effect.

CN118946372APending Publication Date: 2024-11-12SIEMENS AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380030496.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-14
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In the prior art, non-pathogenic coatings used to inhibit the growth of pathogens on the surface of objects often use copper or silver compounds. Although effective, they can lead to environmental pollution and are also potentially dangerous to higher organisms.

Method used

A non-pathogenic coating is designed, including at least one anode material and a cathode material, configured to form a primary cell in the presence of moisture, creating an electrochemical reaction to kill the pathogen without releasing toxic metal ions. The coating consists of porous anode material and cathode material, anode material such as titanium, cathode material such as porous manganese dioxide, generates reactive oxygen radicals through electrochemical reactions, destroying the cell membrane and DNA of the pathogen, and inhibiting its growth.

Benefits of technology

Effectively inhibit the proliferation and accumulation of microorganisms and viruses on the surface of objects, prevent the spread of diseases, and avoid environmental pollution. It does not require replacement or supplementation of coating materials. It has the characteristics of long-term durability and environmental protection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946372A_ABST
    Figure CN118946372A_ABST
Patent Text Reader

Abstract

The invention relates to a non-pathogenic (antimicrobial and / or antiviral) coating of an object surface of an object, having at least one anode layer containing at least one anode material and at least one cathode layer containing at least one cathode material, the layers being configured such that a galvanic cell is formed in the presence of moisture. As a result, the components of the pathogen are destroyed by oxidation. This inhibits proliferation of pathogens on the surface of the object. And the surface of an object can be effectively disinfected. Objects provided with the coating, in particular medical implants, such as stents.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a non-pathogenic coating on an object surface of an object, an object having a non-pathogenic coating arranged on the object surface, and a method of arranging a non-pathogenic coating on an object surface of an object.

[0002] The non-pathogenic (antipathogenic or antimicrobial and / or antiviral) coating for inhibiting the growth of pathogens on the surface of an object comprises a non-pathogenic substance, such as a metal or a metal compound (such as a metal oxide). The non-pathogenic substance is mixed with a paint, varnish or polymer material and then applied to the surface of the object by painting or spraying.

[0003] Common non-pathogenic substances are copper or copper compounds such as cuprite (copper oxide), copper thiocyanate, copper pyridine or silver (e.g. in the form of silver nanoparticles) or silver compounds such as silver chloride, silver nitrate, silver oxide, sodium silver zirconium hydrogen phosphate and silver zeolite A.

[0004] The metal ions (copper or silver ions) released from their metal compounds, as well as the silver nanoparticles, react with enzymes containing sulfur and phosphate in the cell membrane (cell wall) of the pathogen cells, thereby disrupting the life-essential transport function of the cell membrane. The metal ions (e.g. essential calcium ions) are taken up by the cells and bind to macromolecules containing sulfur and phosphate (e.g. amino acids of proteins). The metal ions can also bind to the DNA (deoxyribonucleic acid) in the cells, thus preventing the cells from multiplying. The described effects lead to cell death.

[0005] However, copper and silver compounds are not only toxic to microorganisms and / or viruses, but can also be dangerous to higher organisms by the same mechanism, especially because they accumulate in the environment.

[0006] The object of the present invention is how to design a non-pathogenic coating of an object so that contamination of the environment with metal ions can be avoided (for example by using the object with the non-pathogenic coating or during the production of the object with this coating).

[0007] To solve this problem, a non-pathogenic coating of an object surface is provided, which has at least one anode layer containing at least one anode material and at least one cathode layer containing at least one cathode material, wherein the layers are configured such that a galvanic cell is formed in the presence of moisture.

[0008] According to another aspect of the present invention, an object is provided, which has a non-pathogenic coating disposed on a surface of the object, wherein the non-pathogenic coating at least inhibits the proliferation of pathogens on the surface of the object.

[0009] Finally, in order to achieve this object, a method for arranging a non-pathogenic coating on the surface of an object is also proposed, which has the following method steps: a) providing an object having an object surface, b) arranging the coating on the object surface so that a galvanic cell is formed in the presence of moisture.

[0010] The coating has a non-pathogenic effect. It completely or partially prevents the deposition or proliferation of microorganisms (such as bacteria, fungi or algae) and / or viruses on the surface of the object and the accumulation thereof. Therefore, the coating has a disease-preventing effect and does not release materials that pollute the environment (such as metal ions).

[0011] A galvanic cell is an electrochemical reactor. In the presence of moisture, the electrolyte required for the galvanic cell is produced. These layers form the electrodes of the galvanic cell.

[0012] Moisture can be present in various media, such as air (air humidity) or vapor (sweat), secretions and excretions of organisms. With the help of moisture in various media, the coating forms a (micro) galvanic cell. A (micro) electric field is generated. At the (micro) cathode, reactive oxygen radicals such as superoxide and hydroxyl radicals are electrochemically formed with the help of oxygen dissolved in water. Nucleobases (which are present in nucleic acids DNA and RNA (ribonucleic acid) and are responsible for genetic information) consist of the basic structure of heterocyclic aromatic amines (purines and pyrimidines) with double bonds. The free radicals mentioned have lone pairs of electrons in the outer electron layer and attack the double bonds of the amines by filling their outer electron layer with π electrons to achieve a noble gas configuration. This is accompanied by the loss of the double bond system in the ring, the nucleobase can no longer transmit information for protein biosynthesis, and the replication of nucleic acids DNA and RNA is interrupted. Microorganisms (microorganisms) are killed by oxidation.

[0013] For example, microorganisms also have sulfur-containing proteinogenic amino acids. The sulfur of the amino acid can be oxidized by reactive oxygen species to form sulfoxides. The hydroxyl groups on the side chains of proteinogenic amino acids can be oxidized by reactive oxygen species to form aldehyde groups or carboxyl groups. In each case, chemically altered amino acids are formed. The chemically altered amino acids no longer participate in the construction of proteins essential for life. As a result, the microorganism dies.

[0014] According to a specific embodiment, the anode material and / or cathode material is porous. The electrodes of the galvanic cell have pores. The pores are preferably open. This increases the active surface of the respective electrode. In addition, the electrolyte formed by moisture can be absorbed by the respective electrode.

[0015] This is particularly advantageous if the anode material has a redox potential (standard potential) exceeding +1 V and the cathode material has a redox potential below -1 V. These redox potentials are particularly suitable for initiating electrochemical reactions to kill pathogens, thereby effectively disinfecting the surface of an object.

[0016] In particular, the anode material and / or cathode material comprises a simple metal. According to a specific embodiment, the simple metal is titanium. Titanium is particularly used as the anode material of the anode layer. Titanium is an example of a refractory metal (base metal, high melting point metal). Other examples of refractory metals are zirconium and hafnium (fourth subgroup of the periodic table), vanadium, niobium and tantalum (fifth subgroup) and chromium, molybdenum and tungsten (sixth subgroup).

[0017] In a specific embodiment, the anode material and / or cathode material has at least one metal compound. The metal compound is preferably manganese dioxide (pyrolusite, MnO2). Manganese dioxide is particularly used as the cathode material of the cathode layer. It is particularly advantageous to use porous manganese dioxide.

[0018] Regarding the method for arranging a coating on an object surface, it preferably comprises depositing an anodic material and depositing a cathodic material on the object surface. These layers can be applied directly or indirectly to the object surface. If these layers are arranged one above the other on the object surface, these layers can also be applied indirectly, for example. If these layers are arranged adjacent to one another, these layers can also be applied directly to one object surface or to multiple object surfaces.

[0019] With the deposition of the anodic material or with the deposition of the cathodic material, a non-pathogenic coating is produced, resulting in at least one layer having at least one deposit.

[0020] Depending on the type of deposition, each layer may have a different layer thickness, for example in the μm or nm range. According to a specific embodiment, at least one layer has a layer thickness selected from the range of 1 nm to 100 μm and in particular from the range of 10 nm to 10 μm.

[0021] The corresponding electrode material can be deposited directly. However, it is also conceivable that, instead of depositing the electrode material, the starting material (precursor) of the electrode material is first deposited and then the deposited starting material is converted into the (actual) electrode material. According to a specific embodiment, the application of the anode material and / or the application of the cathode material thus comprises applying at least one anode starting material for the anode material and / or applying at least one cathode starting material for the cathode material.

[0022] In a specific embodiment, the coating is arranged using physical, chemical and / or physical-chemical deposition methods. Physical deposition methods are, for example, cathode ray atomization (sputtering), electron beam evaporation or cold gas spraying. For very thin layers with layer thicknesses in the nanometer or subnanometer (atomic) range, deposition methods in the form of chemical vapor deposition or atomic layer deposition can be used.

[0023] For example, manganese dioxide can be applied to various materials (metals, ceramics, plastics) by various physical methods on the one hand and by chemical deposition on the other hand. Possible physical methods include reactive cathode ray atomization (reactive sputtering), electron beam evaporation of manganese and subsequent oxidation with dry air at 400 to 450° C., and cold gas spraying.

[0024] The object is any object or any workpiece or any practical object on one of the surfaces of which pathogens can settle and multiply. For example, the object is an everyday object, such as a stair railing or a handle of a public transport vehicle.

[0025] The object or the object surface of the object can consist of any object material. Object materials are, for example, metal, ceramic or plastic. Natural materials (such as stone) are also conceivable.

[0026] Preferably, the object is a medical object. In particular, the medical object is a medical implant, a medical device or a control element of a medical device. Medical devices are, for example, surgical instruments, auxiliary devices for surgical instruments or diagnostic devices. Medical devices or control elements of medical devices are often used precisely in a sterile or minimally sterile environment in order to prevent the proliferation of pathogens and thus prevent infection of the patient.

[0027] A medical implant is an object that is inserted (implanted) into a patient's body and remains there temporarily (over a longer period of time) or permanently. Examples of such medical implants are pacemakers or endoprostheses (joint replacements) such as artificial hip joints, etc. In particular, medical implants are vascular prostheses or stents (medical implants used to keep blood vessels and cavities in the body open). In order to be inserted into a patient's body, medical implants must also be sterile.

[0028] The invention eliminates the need for sterilizing medical instruments, sterilizing control elements of medical instruments and / or sterilizing medical implants. Sterility is ensured.

[0029] The anode layer and the cathode layer can be arranged arbitrarily on the object surface of the object. Thus, they can be arranged on top of each other or next to each other. These layers can also be in direct or indirect contact with the object surface.

[0030] In summary, the present invention has the following advantages:

[0031] -Non-pathogenic coatings are highly effective and can be flexibly used on a wide range of objects and applications.

[0032] - No release of toxic particles (ions, atoms or nanoparticles) into the environment by the non-pathogenic coating.

[0033] - Non-pathogenic coatings are durable and do not undergo chemical changes. The coating acts like a catalyst, which allows or accelerates chemical reactions without being consumed itself. Thus, the environment can be protected from toxic or corrosive chemicals used to decontaminate surfaces or disinfect water or aqueous solutions (e.g. substances containing formaldehyde, phenols, hypochlorites, cuprite, copper pyridine or silver nanoparticles).

[0034] - Multiple catalytic cycles are possible (especially when using titanium and manganese dioxide layers). The antibacterial or antiviral active substances are not consumed and do not need to be replenished or replaced.

[0035] -No waste is generated.

[0036] -No consumption of coating material. No need to renew or reapply coating.

[0037] - There is no need to use disinfectants either.

[0038] -To date, most medical implants such as stents are made of inert, corrosion-resistant alloys such as 316L stainless steel, titanium alloys, and cobalt-chromium alloys. Despite the success of stent applications in treating arterial occlusions, their permanent presence in arterial vessels may lead to long-term complications such as thrombosis or in-stent restenosis. New stents are made of biodegradable metals such as iron, magnesium and zinc alloys. These temporary medical implants with very thin titanium / manganese dioxide layers (layer thickness in the nanometer range) prevent microbial infections. In ureteral stents, a thin Ti / MnO2 coating can prevent the adhesion of biofilms.

[0039] -In the medical field, imaging equipment such as CT scanners, MRI scanners and X-ray devices must be calibrated. Phantomes are used for this purpose; they are filled with water. If the liquid is kept in the phantome for a long time, the liquid quality should remain unchanged. By applying a non-pathogenic coating on the inside of the phantome, colonization of bacteria and microorganisms can be prevented.

[0040] - The control elements of the medical devices mentioned and their surfaces which are in contact with the operator and the patient may also have a non-pathogenic coating in order to ensure that they are sterile.

[0041] - In public transport such as trains, contact surfaces that passengers come into contact with can also be protected from germs by means of a non-pathogenic coating. This applies in particular to hygiene areas in trains.

[0042] - In water-managed drive technology, low-pressure and high-pressure motors are used which require air / water heat exchangers or water jackets for cooling. With the invention, surfaces exposed to cooling water can also be protected from the adhesion of microorganisms and the formation of biofilms.

[0043] The invention is described in more detail using exemplary embodiments and the related drawings.The drawings are schematic and not true-to-scale illustrations.

[0044] Figure 1 A cross-sectional view of an object with a non-pathogenic coating is shown.

[0045] Figure 2A The different oxidation valences of manganese and their interconversions are shown.

[0046] Figures 2B to 2D Possible reactions at the microcathode are shown.

[0047] Figure 2E and 2F Possible reactions at the microanode are shown.

[0048] Figure 3A The structural formula of methionine is shown.

[0049] Figure 3B The structural formula of serine is shown.

[0050] Figure 3C The oxidation of adenine, a nucleobase in DNA and RNA, is shown.

[0051] According to a first exemplary embodiment, the object 1 is given in the form of a stent (medical object 11 , medical implant 110 ). According to another exemplary embodiment, the object 1 is a control element 112 of a medical device 111 .

[0052] On the object surface 10 of the object 1 , a non-pathogenic coating 2 having an anodic layer (microanode) 22 containing elemental titanium 2201 as anodic material 220 is applied directly onto the object surface 11 .

[0053] On the anode layer 22 there is a cathode layer (microcathode) 21 with cathode material 210 in the form of porous manganese dioxide (metal compound 2101). The layer thickness of the anode layer 21 and the cathode layer 22 is about 100 nm respectively. Both layers are vapor deposits 230, wherein for the arrangement of the manganese dioxide layer 21, elemental manganese is first applied by electron beam evaporation as cathode starting material 211, which is then oxidized at 400 to 450°C.

[0054] The layers 21 , 22 are arranged such that galvanic cells (microgalvanic cells) 20 are formed in the presence of moisture 23 . This inhibits the proliferation of pathogens 3 on the surface 10 of the object.

[0055] Since manganese dioxide is more noble than titanium according to the electrochemical standard potential, an electric field is formed between the metal dioxide pyrolusite and the metal titanium in the presence of moisture. This means that redox processes can occur on the pyrolusite and titanium, and microorganisms can be killed by the electron transfer that occurs.

[0056] To place the non-pathogenic coating 2 on the surface 10 of an object, the steps are as follows:

[0057] a) providing an object 1 having an object surface 10, and

[0058] b) Arranging the coating 2 on the surface ( 10 ) of the object in such a way that a galvanic cell 20 is formed in the presence of moisture 23 .

[0059] The following reactions with their respective standard potentials can be identified at the microcathode (see Figure 2A ):

[0060] MnO4 - →MnO4 2- : 0.56V

[0061] MnO4 - →Mn 2+ : 1.51V

[0062] MnO4 2- →MnO2: 2.09V

[0063] MnO2→Mn 3+ : 0.95V

[0064] Mn 3+ →Mn 2+ : 1.54V

[0065] MnO2→Mn 2+ : 1.23V

[0066] Mn 2+ →Mn: -1.185V

[0067] At the micro cathode 21, Figure 2B , 2C and 2D. At the microanode 22, a reaction occurs according to Figure 2E and 2F reaction.

[0068] Figure 3A and 3B (Methionine and serine) are examples of proteinogenic amino acids whose functional groups can be oxidatively altered by the present invention.

[0069] Figure 3C The basic reaction based on the oxidation of adenine (nucleobase in DNA and RNA) is shown, which is triggered in pathogen molecules by means of the present invention, making the pathogen unable to proliferate.

Claims

1. A non-pathogenic coating (2) on a surface (10) of an object (1), having - at least one anode layer (22) comprising at least one anode material (220), and at least one cathode layer (21) comprising at least one cathode material (210), The layers (21, 22) are arranged in such a way that a galvanic cell (20) is formed in the presence of moisture (23).

2. The non-pathogenic coating (2) according to claim 1, wherein the anode material (220) and / or the cathode material (210) is porous.

3. The non-pathogenic coating (2) according to claim 1 or 2, wherein the anode material (220) has a redox potential exceeding +1V and the cathode material (210) has a redox potential less than -1V.

4. The non-pathogenic coating (2) according to any one of claims 1 to 3, wherein the anode material (220) and / or the cathode material (210) comprises a single metal (2201).

5. The non-pathogenic coating (2) according to claim 4, wherein the elemental metal (2201) is titanium.

6. The non-pathogenic coating (2) according to any one of claims 1 to 5, wherein the anode material (220) and / or the cathode material (210) comprises at least one metal compound (2101).

7. The non-pathogenic coating (2) according to claim 6, wherein the metal compound (2101) is manganese dioxide.

8. The non-pathogenic coating according to any one of claims 1 to 7, wherein at least one of the layers (21, 22) has at least one deposit (230).

9. The non-pathogenic coating according to any one of claims 1 to 8, wherein at least one of the layers (21, 22) has a layer thickness selected from the range of 1 nm to 100 μm, and in particular has a layer thickness selected from the range of 10 nm to 10 μm.

10. An object (1) having a non-pathogenic coating (2) according to any one of claims 1 to 9 arranged on an object surface (10) of the object (1), wherein the non-pathogenic coating (2) at least inhibits the proliferation of pathogens (3) on the object surface (10).

11. The object (1) according to claim 10, wherein the object (1) is a medical object (11).

12. The object (1) according to claim 11, wherein the medical object (11) is a medical implant (110), a medical device (111) or a control element (112) of the medical device (111).

13. The object according to claim 12, wherein the medical implant (110) is a vascular prosthesis or a stent.

14. A method for arranging a non-pathogenic coating (2) on an object surface (10) of an object (1) according to any one of claims 10 to 13, comprising the following method steps: a) providing an object (1) having an object surface (10), and b) Arranging the coating (2) on the surface (10) of the object such that a galvanic cell (20) is formed in the presence of moisture (23).

15. The method of claim 14, wherein arranging the coating (2) on the surface (10) of the object comprises applying the anode material (220) and the cathode material (210) to the surface (10) of the object.

16. A method according to claim 15, wherein applying the anode material (220) includes applying at least one anode starting material (221) of the anode material (220) and / or applying the cathode material (210) includes applying at least one cathode starting material (211) of the cathode material (220).

17. Method according to any one of claims 14 to 16, wherein the coating (2) is arranged using a physical, chemical and / or physico-chemical deposition method.