Hair swelling agent system and packaging and mixing method thereof

By controlling the average particle size of calcium hydroxide within 8 microns to 30 microns, the problem of the uneven mixing uniformity of hair fluffy agent and insufficient amount of alkaline substances is solved, and the fluffy effect and safety of use is improved. It is suitable for current Have technology and equipment.

CN118948635APending Publication Date: 2024-11-15HUZHOU MINO DAILY CHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411098153.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing non-lye-type hair fluffing agents have insufficient mixing uniformity and alkaline substance use, resulting in poor fluffy effect and high irritation to the hair, and the need for the introduction of new chemical ingredients may bring potential problems.

Method used

Guanidine hydroxide is generated by reacting alkaline earth metal hydroxide and guanidine salt in non-alkali hair fluffing agents, and the average particle size of calcium hydroxide is controlled within 8 microns to 30 microns to ensure uniform mixing and reaction of the two components. Efficiency, reduce the amount of calcium hydroxide and improve the fluffy effect.

Benefits of technology

It achieves better mixing reaction efficiency and use safety, reduces damage to hair, improves fluffy effect, and does not introduce new chemical components. It is suitable for existing preparation processes and equipment, and is suitable for expanding production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention belongs to a novel material in the field of daily chemicals. In particular to a hair leavening agent containing at least two components and a preparation, packaging and mixing method of the leavening agent. A hair leavening agent comprising a first component comprising a water-soluble salt comprising anions capable of being precipitated by alkaline earth metal ions under alkaline conditions, selected from guanidines or guanidine derivatives, and a second component comprising a liquid carrier, and at least one alkaline earth metal hydroxide dispersed in the liquid carrier, the alkaline earth metal hydroxide comprising at least calcium hydroxide, the calcium hydroxide dispersed in the liquid carrier having an average particle size ranging from 8 [mu] m to 30 [mu] m, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is measured by using a laser particle analyzer. According to the hair swelling agent system disclosed by the invention, the component combination reaction efficiency is improved, the use amount of calcium hydroxide can be greatly reduced, the damage to the hair quality is reduced, and the use safety is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to a new material in the field of daily chemicals; specifically, it relates to a hair relaxer comprising at least two components, and a preparation, packaging and mixing method of the relaxer. In particular, it relates to a hair relaxer comprising at least two components, wherein the average particle size of alkaline earth metal calcium hydroxide dispersed in a liquid carrier is within 8 microns to 30 microns. Background Art

[0002] Hair relaxers, also known as relaxers, softeners, hair straighteners, or hair straighteners, are often used to change the appearance of hair through chemical treatment, such as straightening or curling the hair. Hair relaxers usually use strong bases, thioglycolic acid, cysteine, or reducing agents to break the alkyl disulfide bonds in the hair, causing the protein structure to mechanically relax so that the hair can be subsequently shaped. This chemical process often causes irreversible damage to the hair, making it dry, brittle, and more susceptible to breakage and damage. However, the pursuit of beauty by humans has led to an increasing demand for hair relaxers in the market, and has also put forward further requirements for the fluffy effect and mildness of hair relaxers.

[0003] Hair relaxers usually start an alkaline reaction with hydroxide ions. Common hair relaxers on the market are usually divided into alkaline and non-alkaline types. Alkaline hair relaxers usually use a strong base, sodium hydroxide, which is very effective in the treatment of hair relaxation, but because sodium hydroxide has a high pH and strong irritation, it can strongly irritate and damage the hair. Non-alkaline hair relaxers usually use the active substance organic chemical guanidine (usually guanidine hydroxide) to reduce the hair. Guanidine hydroxide is obtained by the reaction of a slightly soluble alkaline earth metal hydroxide and a guanidine salt. For example, slightly soluble calcium hydroxide is mixed with guanidine carbonate to form soluble but unstable guanidine hydroxide and water-insoluble calcium carbonate. Because guanidine hydroxide is unstable in water, the two components of the reaction need to be kept separately before use and need to be freshly prepared before use. Therefore, non-alkaline hair relaxers are usually two-component systems, one of which is an alkaline earth metal hydroxide (such as calcium hydroxide) and the other is a guanidine salt (such as guanidine carbonate). The alkaline earth metal hydroxide component and the guanidine salt component are stored separately, and the alkaline earth metal hydroxide and the guanidine salt can be dispersed in the respective components by dissolving, emulsifying, suspending, etc., and the respective components can be in the form of cream, emulsion, suspension or gel, etc. When using, the two components are mixed and reacted, and then evenly applied to the hair.

[0004] Compared with alkali-based hair relaxers, the alkaline substances used in non-alkali-based hair relaxers are milder and less irritating to hair, but the fluffing effect needs to be improved. In addition, since non-alkali-based hair relaxers need to be mixed with different components when used, how to ensure uniform mixing and effective reaction between components so that the generated active ingredients are at an appropriate level is a key issue in improving the fluffing effect. In order to generate more active ingredient guanidine hydroxide, the existing solution is generally to increase the amount of calcium hydroxide (at least 4%-10% by mass), and some manufacturers even provide 2 times the amount of calcium hydroxide (mostly in two separate packages) to ensure the full reaction of guanidine salt. However, high amounts of calcium hydroxide and the by-product calcium carbonate generated often remain in the hair, causing graying problems, and too much alkaline residue will also damage the hair quality. Many prior arts describe the shortcomings, expectations and possible solutions to the problems of non-alkaline hair relaxers, such as U.S. Pat. Nos. 5,077,042, 5,476,650, 5,565,216, 5,679,327, 6,435,193 and 9,205,038. U.S. Pat. No. 6,435,193 proposes the use of ion exchangers or chelates to increase stability and reduce the amount of hydroxide. U.S. Patent Application No. 20040166074 proposes the use of mineral oil to disperse hydroxide to obtain a more stable agent using less alkaline substances. It is a common practice for hair relaxers to use an emulsion whose main component is oil (such as mineral oil) to disperse calcium hydroxide to form a thickening emulsion component. U.S. Patent No. 5565216 describes the role of different carriers in achieving uniform mixing and / or reducing the amount of alkaline substances used. However, the introduction of new substances into the system often brings new potential problems, such as the need to consider the potential harm of the new substances to hair, whether the obtained products meet national standards (including but not limited to GB / T29678-2013), the need for re-certification (including but not limited to FDA), the increase in raw material and manufacturing costs, etc. European Patent Publication No. 0645998 uses microemulsion to prepare hair relaxers, but a large amount of surfactants are used in the preparation process. Summary of the invention

[0005] The purpose of the present invention is to provide a non-alkaline liquid type hair relaxer system to solve the problem of uniform mixing of the above two components and reducing the amount of alkaline substances used. The hair relaxer of the present invention is based on currently commonly used ingredients, and utilizes alkaline earth metal hydroxide and guanidine salt to react to generate guanidine hydroxide. No new chemical components are introduced into the system, and the system is applicable to the existing preparation process and preparation equipment of the hair relaxer, and is suitable for expanding production.

[0006] The invention relates to a hair relaxer system, comprising at least two components, wherein the first component comprises a water-soluble salt selected from guanidine, wherein the water-soluble salt comprises anions which can be precipitated by alkaline earth metal ions under alkaline conditions; the second component of the system comprises a liquid carrier and at least one alkaline earth metal hydroxide dispersed in the liquid carrier, wherein the alkaline earth metal hydroxide at least comprises calcium hydroxide, wherein the average particle size of the calcium hydroxide dispersed in the liquid carrier is within a range of 8 to 30 microns, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

[0007] Guanidine salt refers to a water-soluble salt selected from guanidine and its derivatives. Guanidine derivatives refer to compounds formed by the substitution of atoms or atomic groups in the guanidine molecule by other atoms or atomic groups. The term "substituted" means that one or more hydrogen atoms, or one or more atomic groups, in the guanidine structure are substituted by one or more substituent groups. One or more substituent groups can be substituted at each substitutable position. Substituent groups include but are not limited to alkyl, alkenyl, alkynyl, aryl, heterocyclic, alkoxy, alkylthio, alkylamino, haloalkyl or cycloalkyl. Guanidine derivatives include but are not limited to methoxyphenylguanidine, N-methylguanidine, dimethylguanidine or metformin. Anions precipitated by alkaline earth metal ions under alkaline conditions can come from but are not limited to carbonates, sulfates, sulfites, phosphates, oxalates, citrates, acetates, tartrates or laurates. Preferably carbonate ions. Guanidine salts are preferably guanidine carbonate.

[0008] The present invention conducts a detailed study on the two components of the non-alkaline liquid hair relaxer. On the basis of not introducing new chemical components, it is found that replacing the ordinary calcium hydroxide in the two-component hair relaxer with calcium hydroxide of a certain micrometer range can increase the amount of the first component under the same amount of calcium hydroxide to achieve a uniform mixing effect and improve the mixing reaction efficiency, or reduce the amount of calcium hydroxide under the same amount of the first component to achieve an effective mixing effect and reduce damage to the hair quality. The present invention provides a hair relaxer system comprising at least two components, which improves the safety of the hair relaxer.

[0009] The alkaline earth metal in the alkaline earth metal hydroxide refers to the IIA group elements in the periodic table, including beryllium, magnesium, calcium, strontium, barium and radium. Alkaline earth metal hydroxide has a certain alkalinity and dissolves in water to form an alkaline solution. In this application, the second component contains at least one alkaline earth metal hydroxide, and calcium hydroxide is most commonly used in consideration of safety and cost. The second component contains at least calcium hydroxide.

[0010] The term "liquid carrier" refers to a substance with a certain fluidity used to carry and disperse calcium hydroxide, including but not limited to a single or multiple oily substances, water or an oil-water mixture. The amount of liquid carrier in the component is generally greater than 20 wt.%, and the amount of liquid carrier can be increased to more than 50 wt.% according to the different added ingredients and the dispersion. Oily substances include but are not limited to vaseline, mineral oil, vegetable oil or animal oil. Vaseline, mineral oil or a mixture of the two is preferred. Water can directly use tap water, or natural surface water or groundwater such as well water, river and lake water, or treated water or purified water that has been filtered or softened. The water quality of the water used must at least meet the sanitary standard for drinking water GB5749-2006. Deionized water (such as reverse osmosis water) is preferred. An oil-water mixture refers to a mixture of an oily substance and water, including an oil-in-water type and an oil-in-water type, and a surfactant is usually required to be added. The surfactant may include one or more of a nonionic surfactant, a cationic surfactant, an anionic surfactant, and an amphoteric surfactant. Surfactants applicable to the cosmetics industry can be applied to the present invention.

[0011] Calcium hydroxide can be dispersed in the liquid carrier by dissolving, suspending, emulsifying, etc., preferably using a surfactant for emulsification. Under different temperatures, different types and amounts of additives, and different storage conditions, calcium hydroxide may agglomerate or precipitate in the liquid carrier.

[0012] The average diameter of human hair is about 50 microns. The epidermis is composed of flat epidermal keratin cells that overlap and form fish scales. It is hydrophilic and has a thickness of about 10 microns. The hair cortex wrapped in the epidermis is composed of keratin, which makes the main part of the hair hydrophilic. The medulla is located in the center of the hair. The non-alkaline hair relaxer system generates water-soluble guanidine hydroxide, which dissolves in water to form an aqueous solution, contacts the hair cuticle to open it, contacts the hair cortex, opens the alkyl disulfide bond, and relaxes the hair. To ensure that there is a sufficient amount of guanidine hydroxide, the first component and the second component must be fully mixed to ensure an effective reaction between the guanidine salt and calcium hydroxide, and at the same time ensure that other suspended, emulsified, and precipitated ingredients do not have a negative impact on the hair quality.

[0013] Calcium hydroxide is slightly soluble in water and is generally considered to be configured in the oil phase. Guanidine carbonate dissolves in the water phase. In order to have a good mixed contact with the calcium hydroxide of the oil phase, the oil phase will be added to the water phase of guanidine carbonate to form an oil-in-water or oil-in-water state. In the mixing process, the mixing diffusion speed between different particles is related to the size of the particles. The smaller the size, the greater the diffusion speed. But the smaller the size, the easier it is for particles to agglomerate. The inventors have found that when the average particle size range of the calcium hydroxide dispersed in the liquid carrier in the second component is within 8 microns to 30 microns, it is possible to reduce the amount of calcium hydroxide in the system without introducing new chemical components. Just good reaction effects can be achieved, so using less calcium hydroxide components can achieve excellent fluffy effects. At this time, the average particle size range of the raw calcium hydroxide is within 8 microns to 15 microns.

[0014] Calcium hydroxide itself is an important chemical raw material, and its particle size range is usually 100-500 microns. Nano-scale calcium hydroxide is also often used as an additive and is widely used in the fields of construction, medicine, food additives, etc. The average particle size of the raw calcium hydroxide powder used in the present invention is selected within 8 microns to 15 microns, and more preferably 10 microns. When the particle size of the raw calcium hydroxide powder is less than 8 microns, dust is easily raised during the material mixing operation, and the particles may be suspended in the air for a long time, which has a great impact on human health and the quality of the atmospheric environment; the fine particle size also increases the risk of dust explosion during storage and operation. The most critical thing is that the inventors found that even if calcium hydroxide powder with a small particle size of micron level is used, when the calcium hydroxide powder is dispersed in the water phase or the oil phase, the average particle size of the obtained calcium hydroxide dispersion system is basically close to 10 microns, so there is no need to increase the cost and use a finer particle size calcium hydroxide powder. When the particle size of the raw calcium hydroxide powder is greater than 15 microns, the degree of dispersion of the raw material in the liquid carrier and the reaction effect with the guanidine salt in another component are significantly reduced. Therefore, as a selection of the present invention, the average particle size range of the raw material calcium hydroxide powder in the second component of the present invention is selected within 8 microns to 15 microns, more preferably 10 microns. The average particle size of the raw material calcium hydroxide powder can be obtained by sieving with a sieve. As another selection of the present invention, the average particle size range of the calcium hydroxide always dispersed in the liquid carrier of the second component of the present invention is selected within 8 microns to 30 microns, preferably within 8 microns to 15 microns, more preferably 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

[0015] The raw calcium hydroxide powder can be sieved using sieves of different mesh sizes to confirm the particle size range. The relationship between sieves of different mesh sizes and particle sizes is calculated using the formula: Mesh size (mesh) = 15000 / size (micrometer). For example, 3000 mesh corresponds to a size of 5 micrometers, 1500 mesh corresponds to a size of 10 micrometers, and 500 mesh corresponds to a size of 30 micrometers.

[0016] After the raw calcium hydroxide powder is dispersed into the carrier, the average particle size of the calcium hydroxide dispersed in the liquid carrier may be different from the average particle size of the raw calcium hydroxide powder. Considering that during long-term transportation and storage, the components may change from a stable state to an unstable state, and the calcium hydroxide powder may undergo relatively serious and obvious agglomeration, the average particle size of the calcium hydroxide dispersed in the liquid carrier will be much larger than the average particle size of the calcium hydroxide in the uniformly dispersed state. In principle, this agglomeration does not fall within the particle size range discussed in the present invention. When it is observed that the calcium hydroxide in the second component is suspected of agglomeration or the components are separated, the second component can be slowly heated to 70°C with continuous stirring. o C (preferably using a water bath for heating), and continue stirring for 10 minutes or more after reaching a predetermined temperature to mix the components evenly. At this time, the average particle size of the calcium hydroxide dispersed in the liquid carrier is the "average particle size of the calcium hydroxide dispersed in the liquid carrier". In an emulsified system, the "average particle size of the calcium hydroxide dispersed in the liquid carrier" may be the size of the micelles containing calcium hydroxide. Due to hydration and / or slight agglomeration in an aqueous solution, the "average particle size of the calcium hydroxide dispersed in the liquid carrier" may be the size of the calcium hydroxide after hydration and / or slight agglomeration after the average particle size measured. The average particle size range of the calcium hydroxide dispersed in the liquid carrier is selected within 8 microns to 30 microns, preferably within 8 microns to 15 microns, and more preferably 10 microns. It is preferred to use a laser particle size analyzer to measure the average particle size of the calcium hydroxide dispersed in the liquid carrier.

[0017] Laser particle size analyzer can use Malvern Mastersizer 3000, and the accuracy error is within ± 1%. Use ethanol as a dispersion medium, take the second component sample as the sample to be tested, first place an external ultrasonic pool for ultrasonic mixing, add the sample to be tested into the laser particle size analyzer sample pool after the ultrasonic is finished, measure the sample and take the average value of 10 measurements. The average particle size range of calcium hydroxide dispersed in the liquid carrier is selected within 8 microns to 30 microns, preferably within 8 microns to 15 microns, and more preferably within 10 microns. The particle size value corresponding to the highest peak of the spectrum obtained by laser particle size analyzer measurement is used as the value of the target average particle size. If the peak that appears is greater than one, then when the value corresponding to at least one peak is within the target range of the present invention, that is, the average particle size range of calcium hydroxide dispersed in the liquid carrier is selected within 8 microns to 30 microns, preferably within 8 microns to 15 microns, and more preferably within 10 microns, it is also considered to fall within the scope of the present invention. The reason for the appearance of multiple peaks may be that the raw material powder is a mixture containing multiple different particle sizes, the dispersion is uneven, the calcium hydroxide in the system has a variety of dispersion forms, or the test sample contains bubbles.

[0018] Surfactants can be added to the liquid carrier to better disperse the components, and one or more of nonionic surfactants, cationic surfactants, anionic surfactants, and amphoteric surfactants can be added. It is preferably anionic surfactants, amphoteric surfactants, or anionic surfactants or amphoteric surfactants are used in combination with other surfactants. More preferably, it is anionic surfactants, amphoteric surfactants, or the combination of the two. When using a surfactant, calcium hydroxide can be more evenly dispersed in the liquid carrier. Calcium hydroxide can be dissolved in the aqueous phase, or dispersed in the aqueous phase, oil phase, or mixed phase in the form of suspension or emulsification. Surfactants suitable for the cosmetics industry can be applied to the present invention, including but not limited to sodium laureth sulfate, ammonium laureth sulfate, lauryl hydroxysulfobetaine, cocamidopropyl betaine, disodium cocoamphodiacetate, cocamide MEA, and cocamide DEA.

[0019] The first component and the second component of the non-alkaline hair relaxer can be, but are not limited to, creams, emulsions, suspensions, colloids or gels. The first component and the second component can be in the same type of form or in different types of forms. Examples that are not limited to the present invention include: for example, the first component can be a suspension and the second component can be a cream, for example, the first component can be an emulsion and the second component can be a gel, for example, the first component can be an emulsion and the second component can be a cream, and for example, the first component and the second component can be both emulsions. The first component and the second component should be easy to mix, so the viscosity of at least one component should be moderate and not too thick. The mixture after the two components are mixed should also maintain a certain viscosity because it is to be applied to the hair to avoid excessive dripping of the mixture and affect the use experience. At room temperature, the viscosity of the mixture after the two components are mixed is above 8000cP, and in order to reduce fluidity, it is preferably above 15000cP. The viscosity can be measured using a rotational viscometer. For example, a Rheomat R180 rotational viscometer equipped with a No. 3 rotor is used to test 25 o C. When measuring, first weigh an appropriate amount of sample and put it into a constant temperature water bath to raise the temperature to the test temperature, then insert the rotational viscometer into the sample to start the test. The test time is generally 1-3 minutes.

[0020] Any component can be added with a thickener to adjust the viscosity of the component. Thickeners include, but are not limited to, one or more of methylcellulose, ethylcellulose, hydroxymethylmethylcellulose, hydroxypropylmethylcellulose, hydroxyethylcellulose, carboxymethylcellulose, carboxyethylcellulose, acrylic polymers, polyethylene glycol, polyvinyl alcohol, polyvinyl pyrrolidone, hydrogenated butylene / ethylene / styrene copolymer, anhydrous aluminum silicate, anhydrous aluminum magnesium silicate and silicon dioxide. The hair relaxer system of the present invention can also be added with other functional ingredients, including but not limited to one or more of gelling agents, softeners, vitamins, amino acids, pH regulators, preservatives, humectants, essences, stabilizers, chelating agents, colorants and detergents. Softeners include, but are not limited to, one or more of dipolyglycerol ether and octyldodecyl lauroyl glutamate. Humectants include, but are not limited to, one or more of glycerol, oligofructose, propylene glycol, hexylene glycol, panthenol, coconut oil, serine, glycine, aspartic acid, leucine, glutamic acid and butylene glycol. The pH adjuster includes but is not limited to one or more of succinic acid, arginine, citric acid, citrate, potassium hydroxide and sodium chloride. The chelating agent may use disodium EDTEA. The emulsion stabilizer may use magnesium nitrate.

[0021] In the hair relaxer system of the present invention, the amount of calcium hydroxide in the second component is preferably less than 4.5 wt. % of the total mass of the first component and the second component in the hair relaxer system, wherein the mass of calcium hydroxide accounts for at least 30 wt. % of the mass of the second component.

[0022] Optionally, at least a part of the first component of the present invention can be solid, preferably solid powder, containing a water-soluble salt selected from guanidine or a guanidine derivative, and the water-soluble salt contains anions that can be precipitated by alkaline earth metal ions under alkaline conditions. When the first component is a powder, the transportation and storage of the first component will be much more convenient because the mass of the solvent is reduced. The solid first component can also contain thickeners, emulsifiers, gelling agents, softeners, vitamins, amino acids, pH regulators, preservatives, humectants, flavors, stabilizers, chelating agents, colorants, and other functional additives. Preferably, a thickener is included.

[0023] Optionally, the second component of the present invention comprises a liquid carrier and at least one alkaline earth metal hydroxide dispersed in the liquid carrier. The alkaline earth metal hydroxide comprises at least calcium hydroxide, and the average particle size range of the calcium hydroxide dispersed in the liquid carrier is selected within 5 microns to 30 microns, preferably within 8 microns to 15 microns, and more preferably 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier is preferably measured using a laser particle size analyzer. Thickeners, emulsifiers, gelling agents, softeners, vitamins, amino acids, pH adjusting agents, preservatives, humectants, essences, stabilizers, chelating agents, colorants, and other functional additives can also be included in the second component.

[0024] The hair relaxer of the present invention comprises at least two components, which are respectively packaged in independent packages. The first component is sealed in the first package, and the second component is sealed in the second package. The first component contains a water-soluble salt selected from guanidine or a guanidine derivative, and the water-soluble salt contains anions that can be precipitated by alkaline earth metal ions under alkaline conditions. The second component comprises a liquid carrier and at least one alkaline earth metal hydroxide dispersed in the liquid carrier, the alkaline earth metal hydroxide at least comprises calcium hydroxide, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is 8 microns to 30 microns, preferably within 8 microns to 15 microns, and more preferably 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

[0025] When the first component is solid, at least one scale line on the outer surface of the first package can be used to indicate the water addition capacity when configuring the first component. The scale line is used as a water addition indicator during use, and it is appropriate to add water until the horizontal plane reaches the scale line on the outer surface of the first package. Guanidine salt and other auxiliary agents can be sealed together in the first package. Preferably, the guanidine salt and other auxiliary agents are packaged separately. For example, the package of the first component can include at least two small packages, one of which contains guanidine salt, and other functional auxiliary agents can be packaged together in another small package or separately in several small packages. Preferably, the first package and the second package have reusable sealing components, such as sealing strips, sealing locks or sealing caps. When the first component and the second component of the package are mixed and used, the following steps are included: 1) Open the first package, add water into the first package until the water level reaches the scale line on the outer surface of the first package, and disperse the first component to obtain a mixed solution of the first package; 2) Open the second package; 3) Pour the mixed liquid in the first package into the second package and mix and disperse.

[0026] The first component can be dispersed by stirring, shaking, vibrating, ultrasonic, inverting, heating, etc. The oily substance in the first component can be added to the aqueous solution obtained by adding water to the first package to obtain a water-oil mixture. When the mixed solution of the first package is poured into the second package, it can be poured in batches. First, pour a part of the aqueous solution, and mix and disperse by stirring, shaking, vibrating, ultrasonic, inverting, heating, etc.; then pour a part of the aqueous solution, and mix and disperse by stirring, shaking, vibrating, ultrasonic, inverting, heating, etc.; so on, until the two components are completely mixed. After pouring the water or aqueous solution, the package can be sealed before mixing. DETAILED DESCRIPTION

[0027] The present invention is described in more detail below through specific examples. However, these examples should not be construed as limiting the scope of the present invention. Example 1 to Example 9, Comparative Example 1 to Comparative Example 6 respectively configure the first and second components of the hair relaxer according to certain components and mass ratios. Among them, the calcium hydroxide powder used in the experiment is sieved with a sieve to obtain a specific particle size. Table 1 lists the sieve mesh size and calcium hydroxide particle size used in Example 1 to Example 9, Comparative Example 1 to Comparative Example 6. 30 hairs were used in each experiment, and the hair was washed with shampoo and kept wet before application. Apply the mixture of component one and component two to the hair, let the hair stand at room temperature for 15 minutes, then rinse with tap water for 5 minutes and wash the hair with shampoo and dry it, and test the tensile properties of the hair. At 20 o C. At 45% relative humidity, the elongation at break of the hair sample was tested using an Instron 4466 material tensile tester at a speed of 15 mm / min. The average particle size of the calcium hydroxide dispersed in the liquid carrier was tested using a Malvern Mastersizer 3000 for the second component of each example, and the average value of 10 measurements was taken for each example.

[0028] Table 1 Components and mass ratios 1

[0029] Table 2 Components and mass ratios 2

[0030] Table 3 Components and mass proportions 3 Example 1

[0031] Prepare the first component according to the components and mass ratios in Table 1, calculate and weigh each component, add deionized water to a container, heat to 50 o C-55 o C, add PEG-40, glyceryl stearate, sodium alginate, disodium EDTA and guanidine carbonate while stirring to completely dissolve the guanidine carbonate in the water phase, and then add arginine to adjust the pH to obtain the water phase. Pour the components of the oil phase into another container and place them at 70 o Then slowly add the water phase into the oil phase, stirring while pouring, and then o C for 15 minutes to mix well.

[0032] Prepare the second component according to the components and mass ratios in Table 1. Calculate and weigh each component. Add mineral oil and vaseline into a container and slowly heat it to 70 oC. Stir until the mixture is evenly mixed, add polymethyl methacrylate, polyvinyl pyrrolidone and glycerol stearate while stirring until the mixture is evenly mixed, then slowly add calcium hydroxide powder (1000 mesh, average particle size 15 microns) while stirring until the sodium hydroxide is completely "wetted" in the mixture, and continue stirring for 15 minutes to mix it evenly. The average particle size of calcium hydroxide dispersed in the liquid carrier is 21 microns.

[0033] Slowly add the first component to the second component (component one / component two is 7 parts / 1 part), stir and mix for 2 minutes, leave at room temperature for 10 minutes, observe a uniform mixture without obvious white solid particles, and then apply it on the hair. The hair breaking elongation obtained by the test is 23.7%. Example 2

[0034] Prepare the first component according to the components and mass ratios in Table 2. Calculate and weigh each component. Add deionized water to a container and heat to 50 o C-55 o C, add sodium laureth sulfate, cocamide MEA, magnesium nitrate and guanidine carbonate while stirring to completely dissolve the guanidine carbonate in the water phase, and then add succinic acid to adjust the pH to obtain the water phase. Pour the components of the oil phase into another container and heat at 70 o Then slowly add the water phase into the oil phase, stirring while pouring, and then o C for 15 minutes to mix well.

[0035] Prepare the second component according to the components and mass ratios in Table 2. Calculate and weigh each component. Add mineral oil and vaseline into a container and slowly heat it to 70 o C. Stir until the mixture is evenly mixed, add polymethyl methacrylate, polyvinyl pyrrolidone and sodium laureth sulfate while stirring until the mixture is evenly mixed, then slowly add calcium hydroxide powder (1000 mesh, average particle size 15 microns) while stirring until the sodium hydroxide is completely "wetted" in the mixture, and continue stirring for 15 minutes to mix evenly. The average particle size of calcium hydroxide dispersed in the liquid carrier is 24 microns.

[0036] Slowly add the first component to the second component (component one / component two is 7 parts / 1 part), stir and mix for 2 minutes, leave at room temperature for 10 minutes, observe a uniform mixture without obvious white solid particles, and then apply it on the hair. The hair breaking elongation obtained by the test is 24.2%. Example 3

[0037] Prepare the first component according to the components and mass ratios in Table 3, calculate and weigh each component, add guanidine carbonate, PEG-40, sodium laureth sulfate, cocamide MEA, succinic acid and magnesium nitrate into a container, and stir evenly in a solid state. Then add water and stir at room temperature for 10 minutes, then add mineral oil and stir at room temperature for 15 minutes to form an emulsion.

[0038] Prepare the second component according to the components and mass ratios in Table 3. Calculate and weigh each component. Add mineral oil and vaseline into a container and slowly heat it to 70 o C. Stir until the mixture is evenly mixed, add polymethyl methacrylate, polyvinyl pyrrolidone and sodium laureth sulfate while stirring until the mixture is evenly mixed, then slowly add calcium hydroxide powder (1000 mesh, average particle size 15 microns) while stirring until the sodium hydroxide is completely "wetted" in the mixture, and continue stirring for 15 minutes to mix evenly. The average particle size of calcium hydroxide dispersed in the liquid carrier is 28 microns.

[0039] Slowly add the first component to the second component (component one / component two is 7 parts / 1 part), stir and mix for 2 minutes, leave at room temperature for 10 minutes, observe a uniform mixture, and see a few fine white solid particles with the naked eye, then apply it on the hair. The hair breaking elongation obtained by the test is 23.5%. Example 4

[0040] The first component and the second component were prepared according to the method of Example 1, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 1500 mesh and had an average particle size of 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 10 microns. The hair breaking elongation obtained by testing was 25.3%. Example 5

[0041] The first component and the second component were prepared according to the method of Example 2, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 1500 mesh and had an average particle size of 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 12 microns. The hair breaking elongation obtained by testing was 25.2%. Example 6

[0042] The first component and the second component were prepared according to the method of Example 3, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 1500 mesh and had an average particle size of 10 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 11 microns. The hair breaking elongation obtained by testing was 24.7%. Example 7

[0043] The first component and the second component were prepared according to the method of Example 1, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 1800 mesh and had an average particle size of 8.3 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 10 microns. The hair elongation at break obtained by testing was 25.1%. Example 8

[0044] The first component and the second component were prepared according to the method of Example 2, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles. The mixture was then applied to the hair. The difference was that the calcium hydroxide powder used was 1800 mesh with an average particle size of 8.3 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 10 microns. The elongation at break of the hair obtained by the test was 24.8%. Example 9

[0045] The first component and the second component were prepared according to the method of Example 3, and the first component was slowly added to the second component. After stirring and mixing for 2 minutes, the mixture was placed at room temperature for 10 minutes, and a uniform mixture was observed without the appearance of white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 1800 mesh and had an average particle size of 8.3 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 10 microns. The hair breaking elongation obtained by testing was 24.5%.

[0046] Comparative Example 1 According to the components and mass ratios in Table 1, the first component and the second component were prepared according to the method of Example 1. The first component was slowly added to the second component (component one / component two was 6 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. It was observed that the mixture had obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 300 mesh and the average particle size was 50 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 62 microns. The hair breaking elongation obtained by the test was 24.4%.

[0047] Comparative Example 2 According to the components and mass ratios in Table 2 and the method of Example 2, the first component and the second component were prepared, and the first component was slowly added to the second component (component one / component two was 6 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. It was observed that the mixture had obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 300 mesh and the average particle size was 50 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 62 microns. The hair breaking elongation obtained by the test was 24.2%.

[0048] Comparative Example 3 According to the components and mass ratios in Table 1, the first component and the second component were prepared according to the method of Example 1. The first component was slowly added to the second component (component one / component two was 4 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. A uniform mixture was observed without obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 300 mesh and had an average particle size of 50 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 65 microns. The hair breaking elongation obtained by the test was 24.4%.

[0049] Comparative Example 4 According to the components and mass ratios in Table 2, the first component and the second component were prepared according to the method of Example 2. The first component was slowly added to the second component (component one / component two was 4 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. A uniform mixture was observed without obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 100 mesh and had an average particle size of 150 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 165 microns. The hair breaking elongation obtained by the test was 25.1%.

[0050] Comparative Example 5 According to the components and mass ratios in Table 1, the first component and the second component were prepared according to the method of Example 1. The first component was slowly added to the second component (component one / component two was 4 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. It was observed that the mixture had obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 100 mesh and the average particle size was 150 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 172 microns. The hair breaking elongation obtained by the test was 23.4%.

[0051] Comparative Example 6 According to the components and mass ratios in Table 2 and the method of Example 2, the first component and the second component were prepared, and the first component was slowly added to the second component (component one / component two was 4 parts / 1 part), stirred and mixed for 2 minutes, and then placed at room temperature for 10 minutes. It was observed that the mixture had obvious white solid particles, and then applied to the hair. The difference is that the calcium hydroxide powder used was 100 mesh and the average particle size was 150 microns. The average particle size of the calcium hydroxide dispersed in the liquid carrier was 195 microns. The hair breaking elongation obtained by the test was 22.3%.

[0052] It can be seen from the data of the embodiment and the comparative embodiment that, when using the hair relaxer of the present invention, the amount of the first component can be increased under the condition of the same amount of calcium hydroxide to still achieve the effect of uniform mixing, and the obtained mixture does not have obvious white solid particles. By increasing the ratio of component one to component two, the amount of calcium hydroxide can be relatively reduced, because calcium hydroxide and component one react fully, the reaction efficiency is high, the use safety is improved, the damage to hair is not great, and the measured hair elongation at break is within the normal range of normal hair. When using a hair relaxer outside the scope of the present invention, because calcium hydroxide and component one are not easy to react fully, the proportion of component one needs to be reduced to about 60% of the component one used when using the hair relaxer of the present invention to obtain a relatively uniform mixture without obvious white solid particles. Compared with greatly increasing the amount of calcium hydroxide, although the measured hair elongation at break is also within the normal range of normal hair, it is slightly lower than the effect when using the hair relaxer of the present invention.

Claims

1. A hair relaxer, characterized in that: include: a first component, the first component comprising a water-soluble salt selected from guanidine or a guanidine derivative, the water-soluble salt comprising an anion that can be precipitated by an alkaline earth metal ion under alkaline conditions, and The second component comprises a liquid carrier and at least one alkaline earth metal hydroxide dispersed in the liquid carrier, wherein the alkaline earth metal hydroxide comprises at least calcium hydroxide, and the average particle size of the calcium hydroxide dispersed in the liquid carrier ranges from 8 microns to 30 microns, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

2. The hair relaxer according to claim 1, characterized in that: The average particle size of the calcium hydroxide dispersed in the liquid carrier is within a range of 8 microns to 15 microns, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

3. The hair relaxer according to claim 2, characterized in that: The average particle size of the calcium hydroxide dispersed in the liquid carrier is in the range of 10 micrometers, and the average particle size of the calcium hydroxide dispersed in the liquid carrier is measured using a laser particle size analyzer.

4. The hair relaxer according to claim 1, characterized in that: At least a portion of the first component is in solid form.

5. A method for preparing a hair relaxer, comprising the following steps: preparing a first component, the first component comprising a water-soluble salt selected from guanidine or a guanidine derivative, the water-soluble salt comprising an anion that can be precipitated by an alkaline earth metal ion under alkaline conditions, and The second component is prepared by dispersing at least one alkaline earth metal hydroxide in a liquid carrier, wherein the alkaline earth metal hydroxide comprises at least raw calcium hydroxide, wherein the average particle size range of the raw calcium hydroxide powder is selected within a range of 8 microns to 15 microns, and the average particle size of the raw calcium hydroxide powder is obtained by sieving with a sieve.

6. The preparation method according to claim 5, characterized in that: The average particle size range of the raw calcium hydroxide powder is selected to be 10 microns, and the average particle size of the raw calcium hydroxide powder is obtained by sieving using a sieve.

7. A package for a hair relaxer according to claim 4, comprising: a first package, wherein the first package contains a first component and has at least one scale line on the outer surface of the first package for indicating the water capacity to be added when preparing the first component; and A second package having a second component sealed therein.

8. A method of mixing a packaged hair relaxer as claimed in claim 7, comprising: (1) opening the first package, adding water into the first package until the water level reaches the scale line on the outer surface of the first package, and dispersing the first component to obtain a mixed solution of the first package; (2) Open the second package; (3) Pour the mixed liquid in the first package into the second package and mix and disperse.