Belted drum forming process for improving NVH (Noise Vibration and Harshness) of tire
Through the coordinated work of vacuum adsorption and pneumatic servo drum, the problem of poor film and adhesive bonding during tire forming is solved, high-quality tire forming is achieved, and NVH performance and vehicle comfort and safety are improved.
Patent Information
- Application Number
- CN202410950669.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-15
AI Technical Summary
In the prior art, when the molding drum is completed, the film used for tire processing needs to be covered with multiple layers of mixed glue, resulting in smooth surface of the covered surface, low bonding and bonding, and easy to cause layering after cooling.
The film surface is treated into a frosted layer by using a vacuum adsorption device, and the molding process is accurately controlled through the collaborative work of the pneumatic drum and the servo drum to ensure that the film is closely bonded to the belt layer material to form a high-quality tire structure.
The film and the adhesive are fully bonded and bonded, and there is no layering after cooling, which improves the NVH performance of the tire, ensures that the profile and size of the tire comply with the design specifications, and improves the comfort and safety of the vehicle.
Smart Images

Figure CN118952733A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of tire manufacturing, and in particular relates to a belt drum forming process for improving tire NVH. Background Art
[0002] The tire belt drum forming process is an important technology in the tire manufacturing process, which involves many aspects such as the tire skeleton structure design, material selection, and process flow optimization. In this process, the tire belt (that is, the tire skeleton) is specifically arranged and fixed, and then placed in a drum forming machine, and the machine's power and temperature are used to stretch the tire skeleton and shape the tire.
[0003] NVH is the abbreviation of Noise, Vibration and Harshness. In the automotive industry, NVH performance is one of the important indicators to measure vehicle comfort. For tires, NVH performance is also very important, which is directly related to the comfort and driving experience of the vehicle during driving.
[0004] Improving the NVH performance of tires can not only improve the comfort of the vehicle, but also improve the safety and fuel economy of the vehicle; therefore, tire manufacturers need to comprehensively consider various factors when designing tires to improve the NVH performance of tires.
[0005] In the prior art, when the rubber sheet for tire processing is formed by a forming drum, the surface of the rubber sheet to be formed is covered with multiple layers of mixed rubber. Each time the mixed rubber is covered, the surface of the covered surface is smooth. After the rubber and the rubber sheet are bonded and hot-pressed, the bonding degree is not high and stratification is easily generated after cooling. Summary of the invention
[0006] The purpose of the present invention is to provide a belt drum forming process for improving tire NVH, aiming to solve the problem in the prior art that when the rubber sheet used for tire processing is formed by a forming drum, the surface of the belt-formed rubber sheet needs to be covered with multiple layers of mixed rubber material, and each time the covering is performed, the surface of the covered surface is smooth. After the rubber material and the rubber sheet are bonded and hot-pressed, the bonding degree is not high, and stratification is easily generated after cooling.
[0007] To achieve the above object, the present invention provides the following technical solutions:
[0008] A belt drum forming process for improving tire NVH comprises the following steps:
[0009] S1. Mix the rubber raw materials with carbon black, sulfur, accelerator and additives in a certain proportion, and mix them through a mixing equipment to make the rubber material uniform and fine;
[0010] S2, forming a rubber sheet of a certain thickness through an extruder;
[0011] S3. Clean the surface of the building drum and apply a layer of release agent to prevent rubber from adhering. Stick the film to the surface of the building drum. The film bulges from the inside to the outside to form the shape of the tire through the expansion and contraction of the building drum.
[0012] S4, using a vacuum adsorption device to attach to the outer surface of the film, through vacuum adsorption, making the surface of the film uneven, forming a frosted layer;
[0013] S5, laminating the belt layer material and the intersecting mixed material on the outer surface of the tire, and bonding them tightly with the frosted layer;
[0014] S6, using a forming machine to heat and pressure treat the laminated belt layer to form a belt layer of the tire;
[0015] S7, placing the formed belt layer together with the tire body and the tread into a vulcanizer, and vulcanizing the rubber through heating and pressure to form the final tire structure;
[0016] S8. The vulcanized tire belt layer needs to be cooled, inspected and trimmed to ensure that the tire quality meets the standards;
[0017] S9. Carry out quality inspection on the formed belt layer, including tests on appearance, size and physical properties, to ensure that each tire meets the specified quality requirements.
[0018] As a preferred solution of the present invention, in step S1, the auxiliary agent includes an antioxidant, a plasticizer, a reinforcing agent, a filler, a retarder, an active agent, a protective agent, an adhesive and a colorant.
[0019] As a preferred solution of the present invention, the forming drum used in step S3 includes a pneumatic drum and a servo drum.
[0020] As a preferred solution of the present invention, the vacuum adsorption device used in step S4 is composed of an adjustment component, two driving components and multiple vacuum adsorption components. The multiple vacuum adsorption components are connected, and the adjustment component drives the multiple groups of vacuum adsorption components to move in a ring shape. The multiple groups of vacuum adsorption components are connected to the surface of the film, and multiple protrusions are adsorbed on the surface of the film to form a frosted layer.
[0021] As a preferred solution of the present invention, the adjusting component includes a base, a limiting slide groove, a T-shaped slider, a bidirectional screw, a motor and an electric push rod, and two of the T-shaped sliders and the electric push rod are provided. The base is arranged on the ground, and the limiting slide groove is opened at the upper end of the base. The two T-shaped sliders are both slidably connected in the limiting slide groove, and the bidirectional screw is rotatably connected in the limiting slide groove. The bidirectional screw is threadedly matched with the two T-shaped sliders, and the motor is fixedly connected to one side end of the base. The output end of the motor movably passes through the inner wall of the limiting slide groove and is fixed to one end of the bidirectional screw, and the two electric push rods are respectively fixedly connected to the upper ends of the two electric push rods.
[0022] As a preferred solution of the present invention, each group of the driving components includes a vacuum air pump, a rotating block and a connecting block, the connecting block is fixedly connected to the extended end of the electric push rod, the rotating block is rotatably connected to the surface of the connecting block, and the vacuum air pump is fixedly connected to one end of the rotating block.
[0023] As a preferred solution of the present invention, each group of the vacuum adsorption components includes a vacuum adsorption body, a first mounting block, a second mounting block, an adsorption hole and an adsorption cavity. There are multiple adsorption holes, and the adsorption cavity is fixedly connected to the vacuum adsorption body. The first mounting block is fixedly connected to one side end of the vacuum adsorption body, and the second mounting block is fixedly connected to the other side end of the vacuum adsorption body. The multiple adsorption holes are all opened on the lower surface of the vacuum adsorption body, and the multiple adsorption holes are all connected to the adsorption cavity.
[0024] As a preferred solution of the present invention, when the tire belt needs to be stretched or compressed to adapt to the shape of the mold, the pneumatic drum changes the diameter of the first expansion and contraction area by inflating and deflating, thereby controlling the tension of the belt.
[0025] As a preferred solution of the present invention, the servo drum accurately controls its rotation speed and position through a servo motor to adjust the second expansion and contraction area. During the tire molding process, the servo drum very accurately controls the placement and processing of the tire belt.
[0026] As a preferred solution of the present invention, the pneumatic drum and the servo drum work together. When molding the side of the tire, the pneumatic drum is used to provide tension for the sidewall material, while the servo drum is used to control the molding of the tire.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] 1. In the present invention, by using this process, the surface of the film is subjected to vacuum adsorption treatment during the film expansion stage to make its surface uneven. When the film surface is covered with mixed adhesive, the adhesive and the film are completely bonded and adhered after heat pressing, and no stratification occurs after cooling.
[0029] 2. In the present invention, during the expansion and contraction process, the pressure or mechanical device inside the drum will increase the diameter of the drum, thereby pushing the film to bulge from the inside to the outside, gradually forming the shape of the tire. This process requires precise control to ensure that the profile and size of the tire meet the design specifications.
[0030] 3. In the present invention, during the tire forming process, the pneumatic drum and the servo drum usually work together to optimize the tire profile and structure by precisely controlling the movement of the servo drum, thereby improving the tire's NVH performance. Appropriate air pressure ensures accurate tension of the sidewall material, thereby improving the tire's NVH performance; keeping the drum surface smooth and reducing friction between the material and the drum is beneficial to tire forming and also helps to improve the tire's NVH performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0032] Figure 1 It is a flowchart of the belt drum forming process in the present invention;
[0033] Figure 2 is a three-dimensional diagram of the pneumatic drum of the present invention;
[0034] Figure 3 A stereogram of the servo ancient in the present invention;
[0035] Figure 4 It is a three-dimensional diagram of the vacuum adsorption device in the present invention;
[0036] Figure 5 For the present invention Figure 4 A partial enlarged view of the middle A;
[0037] Figure 6 For the present invention Figure 4 A partial enlarged view of point B in the middle;
[0038] Figure 7 A three-dimensional diagram of the vacuum adsorption assembly of the present invention;
[0039] Figure 8 is a cross-sectional view of the vacuum adsorption assembly of the present invention;
[0040] Fig. 9 It is a schematic diagram of the structure of the vacuum adsorption component in the present invention;
[0041] Fig.10 It is a schematic diagram of the adhesion between the mixture and the tire surface in the present invention.
[0042] In the figure: 1. base; 2. limit slide; 3. T-shaped slider; 4. bidirectional screw; 5. motor; 6. electric push rod; 7. vacuum air pump; 8. rotating block; 9. connecting block; 10. vacuum adsorption body; 11. first mounting block; 12. second mounting block; 13. adsorption hole; 14. adsorption cavity; 15. bellows; 16. pneumatic drum; 1601, first expansion and contraction area; 17. servo drum; 1701, second expansion and contraction area; 18. film; 19. bonding material. DETAILED DESCRIPTION
[0043] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] Example 1
[0045] See also Figure 1-Figure 10 , the present invention provides the following technical solutions:
[0046] A belt drum forming process for improving tire NVH comprises the following steps:
[0047] S1. Mix the rubber raw materials with carbon black, sulfur, accelerator and additives in a certain proportion, and mix them through a mixing equipment to make the rubber material uniform and fine;
[0048] S2, forming a rubber sheet of a certain thickness through an extruder;
[0049] S3. Clean the surface of the building drum and apply a layer of release agent to prevent rubber from adhering. Stick the film to the surface of the building drum. The film bulges from the inside to the outside to form the shape of the tire through the expansion and contraction of the building drum.
[0050] S4, using a vacuum adsorption device to attach to the outer surface of the film, through vacuum adsorption, making the surface of the film uneven, forming a frosted layer;
[0051] S5, laminating the belt layer material and the intersecting mixed material on the outer surface of the tire, and bonding them tightly with the frosted layer;
[0052] S6, using a forming machine to heat and pressure treat the laminated belt layer to form a belt layer of the tire;
[0053] S7, placing the formed belt layer together with the tire body and the tread into a vulcanizer, and vulcanizing the rubber through heating and pressure to form the final tire structure;
[0054] S8. The vulcanized tire belt layer needs to be cooled, inspected and trimmed to ensure that the tire quality meets the standards;
[0055] S9. Carry out quality inspection on the formed belt layer, including tests on appearance, size and physical properties, to ensure that each tire meets the specified quality requirements.
[0056] In a specific embodiment of the present invention, the mixing of rubber raw materials is a crucial step in the tire manufacturing process, which directly affects the performance and quality of the final product. In order to prepare high-quality tires, the rubber raw materials need to be mixed with carbon black, sulfur, accelerators and other additives in precise proportions. These additives enhance specific properties of rubber, such as wear resistance, aging resistance, strength and elasticity; the mixing process is usually carried out in dedicated mixing equipment, which can be an open mill or an internal mixer. During the mixing process, the rubber raw materials and additives are heated to a certain temperature so that they can be better blended together. Heating also helps to improve the fluidity of the rubber, making it easier to mix evenly with the additives. The purpose of mixing is to ensure that all ingredients are evenly distributed, thereby eliminating any potential defects, such as pores or areas that are not fully mixed; the uniformity and fineness of the mixing have a direct impact on the performance of the tire. Uniform mixing ensures that each part of the tire has consistent physical and chemical properties, thereby improving the durability and reliability of the tire. Fine rubber means that the additives are fully dispersed in the rubber matrix, which helps to improve the processing performance of the tire and the quality of the final product; after mixing, the mixed rubber will enter the next process, such as extrusion, calendering or molding, and finally form the various components of the tire. Quality control is crucial throughout the manufacturing process to ensure that each tire can meet the highest performance standards; during the extrusion process, temperature control is very critical. Too high or too low temperature may cause quality problems of the rubber, such as uneven viscosity, unstable vulcanization speed or inconsistent physical properties. Therefore, the extruder is usually equipped with a precise temperature control system to ensure the stability of the rubber temperature throughout the extrusion process; the preparation of the building drum surface and the lamination of the film are crucial steps that directly affect the final shape and quality of the tire; the building drum is a key process in the tire building process, and its shape and size determine the basic profile of the tire. Before use, the surface of the building drum needs to be thoroughly cleaned to remove any dust, oil or residual rubber. This can be done by wiping with solvent, brush cleaning or compressed air blowing; In order to prevent the rubber from sticking to the drum during the vulcanization process, a layer of release agent needs to be evenly applied to the clean and dry drum surface. Release agent is a special chemical that can prevent rubber from coming into direct contact with metal at the high temperature of vulcanization, thereby preventing the rubber from adhering to the drum and facilitating the smooth demoulding of the tire from the drum; Carefully apply the film pre-made by the extruder or calender to the surface of the drum coated with the release agent. The thickness and size of the film should be determined according to the requirements of the tire design. During the lamination process, ensure that the film is flat, wrinkle-free, and completely fits the drum to avoid leaving bubbles or gaps; Once the film is attached, the drum will expand and contract according to the set program. During the expansion and contraction process, the pressure or mechanical device inside the drum will increase the diameter of the drum, thereby pushing the film from the inside out to gradually form the shape of the tire.This process requires precise control to ensure that the profile and size of the tire meet the design specifications; after the film is bonded and forms the tire profile, some additional processing may be performed, such as trimming excess rubber, checking the quality of the fit, repairing any defects, etc., to ensure the quality of tire molding; using a vacuum adsorption device, the film is attached to the outer surface of the film, and through vacuum adsorption, the surface of the film is made uneven to form a frosted layer. The belt layer material and the intersecting mixture are bonded to the outer surface of the tire and tightly bonded to the frosted layer. The belt layer is a key structural part of the tire, which provides the tire's strength, stability and NVH performance. Using a molding machine to heat and pressurize the laminated belt layer is an important step to ensure that the belt layer is tightly combined with other parts of the tire to form a strong and uniform tire structure; the molded belt layer is placed in a vulcanizer together with the tire body and tread, and the rubber is vulcanized through heating and pressure to form the final tire structure; the vulcanized tire belt layer needs to be cooled, inspected and trimmed after curing to ensure that the quality of the tire meets the standards; quality inspection includes appearance inspection, size measurement, physical property testing and quality control; the intersection mixture is composed of a variety of rubber materials.
[0057] For details, please refer to Figure 1-Figure 10 In step S1, the auxiliary agents include antioxidants, plasticizers, reinforcing agents, fillers, delay agents, active agents, protective agents, adhesives and colorants.
[0058] In this embodiment, the auxiliary agent is composed of an antioxidant, a plasticizer, a reinforcing agent, a filler, a retarder, an active agent, a protective agent, a binder and a colorant.
[0059] For details, please refer to Figure 1-Figure 10 The forming drum used in step S3 includes a pneumatic drum and a servo drum.
[0060] In this embodiment: the pneumatic drum is composed of left and right end covers, a tapered piston, a support plate, an expansion and contraction belt, an adjusting pad and other components. The support plate is in direct contact and friction with the tapered piston and the end cover to achieve expansion and contraction. A pneumatic rotary joint is added at the tail end of the shaft to introduce gas into the tapered piston of the belt drum to push the piston to achieve expansion and contraction. The forming drum is composed of left and right end covers, a tapered piston, a support plate, a guide rail, a slider bearing and other components. The support plate, the tapered piston and the end cover are added with a guide rail, and the expansion and contraction is achieved through a linear bearing. A servo motor is added at the tail end of the shaft, and the piston is pushed to move through a screw drive to achieve expansion and contraction.
[0061] For details, please refer to Figure 1-Figure 10The vacuum adsorption device used in step S4 is composed of an adjustment component, two driving components and multiple vacuum adsorption components. The multiple vacuum adsorption components are connected, and the adjustment component drives the multiple groups of vacuum adsorption components to move in a ring shape. The multiple groups of vacuum adsorption components are connected to the surface of the film 18, and multiple protrusions are adsorbed on the surface of the film 18 to form a frosted layer.
[0062] In this embodiment: two adjacent vacuum adsorption bodies 10 are rotatably connected through the first mounting block 11 and the second mounting block 12, and the two adjacent vacuum adsorption bodies 10 are connected to two bellows 15. When the vacuum air pump 7 is running, it reduces the pressure in the adsorption chamber 14 through the bellows 15. When the pressure in the adsorption chamber 14 is reduced, the lower surface of the vacuum adsorption body 10 is attached to the outer surface of the film, and the pressure in the adsorption chamber 14 is reduced until it reaches a vacuum state. The surface of the film is adsorbed by the adsorption holes 13, resulting in bulges, making the surface of the film uneven.
[0063] For details, please refer to Figure 1-Figure 10 The adjusting component includes a base 1, a limiting slide groove 2, a T-shaped slider 3, a bidirectional screw 4, a motor 5 and an electric push rod 6. Two T-shaped sliders 3 and two electric push rods 6 are provided. The base 1 is arranged on the ground, the limiting slide groove 2 is opened at the upper end of the base 1, the two T-shaped sliders 3 are slidably connected in the limiting slide groove 2, the bidirectional screw 4 is rotatably connected in the limiting slide groove 2, the bidirectional screw 4 is threadedly matched with the two T-shaped sliders 3, the motor 5 is fixedly connected to one side end of the base 1, the output end of the motor 5 movably passes through the inner wall of the limiting slide groove 2 and is fixed to one end of the bidirectional screw 4, and the two electric push rods 6 are respectively fixedly connected to the upper ends of the two electric push rods 6.
[0064] In this embodiment: the base 1 in the adjustment component is placed on the ground, and the operation of the motor 5 and the electric push rod 6 drives the multiple groups of vacuum adsorption components to move. When in use, the multiple groups of vacuum adsorption components form a ring and adhere to the surface of the film. Then, through the operation of the multiple groups of vacuum adsorption components, a frosted layer is formed on the surface of the film. When running, the motor 5 in the adjustment component drives the bidirectional screw 4 connected to its output end to rotate. The threads on both sides of the surface of the bidirectional screw 4 are in opposite directions. The rotation of the bidirectional screw 4 drives the T-shaped slider 3 to slide in the limiting slide groove 2, and the two T-shaped sliders 3 move towards or away from each other at the same time, and the extended end of the electric push rod 6 is connected to the connecting block 9.
[0065] For details, please refer to Figure 1-Figure 10 Each set of driving components includes a vacuum air pump 7, a rotating block 8 and a connecting block 9. The connecting block 9 is fixedly connected to the extended end of the electric push rod 6. The rotating block 8 is rotatably connected to the surface of the connecting block 9. The vacuum air pump 7 is fixedly connected to one end of the rotating block 8.
[0066] In this embodiment, the connecting block 9 in the driving assembly is fixed to the extended end of the electric push rod 6, and the vacuum air pump 7 reduces the pressure in the adsorption chamber 14 through the bellows 15 to generate a vacuum during operation.
[0067] For details, please refer to Figure 1-Figure 10 Each set of vacuum adsorption components includes a vacuum adsorption body 10, a first mounting block 11, a second mounting block 12, an adsorption hole 13 and an adsorption chamber 14. A plurality of adsorption holes 13 are provided. The adsorption chamber 14 is fixedly connected to the vacuum adsorption body 10. The first mounting block 11 is fixedly connected to one side end of the vacuum adsorption body 10, and the second mounting block 12 is fixedly connected to the other side end of the vacuum adsorption body 10. The plurality of adsorption holes 13 are all opened on the lower surface of the vacuum adsorption body 10, and the plurality of adsorption holes 13 are all connected to the adsorption chamber 14.
[0068] In this embodiment: the vacuum adsorption component is formed into a ring and attached to the surface of the film, and then a frosted layer is formed on the surface of the film through the operation of multiple groups of vacuum adsorption components. The lower surface of the vacuum adsorption body 10 is an arc surface, which conforms to the shape of the film after expansion.
[0069] For details, please refer to Figure 1-Figure 10 When the tire belt needs to be stretched or compressed to adapt to the shape of the mold, the pneumatic drum 16 changes the diameter of the first expansion and contraction area 1601 by inflating and deflating, thereby controlling the tension of the belt.
[0070] In this embodiment, the surface of the pneumatic drum 16 is in contact with the film when in use, and a pneumatic rotary joint is added at the rear end of the shaft to introduce gas into the tapered piston of the belt drum to push the piston to move and achieve expansion and contraction.
[0071] For details, please refer to Figure 1-Figure 10 The servo drum 17 accurately controls its rotation speed and position through the servo motor to adjust the second expansion and contraction area 1701. During the tire molding process, the servo drum 17 very accurately controls the placement and processing of the tire belt.
[0072] In this embodiment, when the servo drum 17 is in use, its surface is in contact with the film, and the expansion and contraction action is achieved through the linear bearing, and the servo motor is added to the tail end of the shaft, and the piston is driven by the screw to achieve expansion and contraction.
[0073] For details, please refer to Figure 1-Figure 10 The pneumatic drum 16 and the servo drum 17 work together. When molding the side of the tire, the pneumatic drum 16 is used to provide tension for the sidewall material, while the servo drum 17 is used to control the molding of the tire.
[0074] In this embodiment: During the tire forming process, the pneumatic drum and the servo drum usually work together to optimize the tire profile and structure by precisely controlling the movement of the servo drum, thereby improving the tire's NVH performance. Appropriate air pressure ensures accurate tension of the sidewall material, thereby improving the tire's NVH performance. Keeping the drum surface smooth reduces friction between the material and the drum, which is beneficial to tire forming and also helps to improve the tire's NVH performance.
[0075] It should be noted that the specific types of motor 5, electric push rod 6, vacuum air pump 7, pneumatic drum 16 and servo drum 17 to be used are selected by relevant technical personnel familiar with the field, and the above motor 5, electric push rod 6, vacuum air pump 7, pneumatic drum 16 and servo drum 17 are all existing technologies and will not be elaborated in this solution.
[0076] The working principle and use process of the present invention are as follows: when using the present process, firstly, the rubber raw material is mixed with carbon black, sulfur, accelerator and auxiliary agent in a certain proportion, and then mixed by a mixing device to make the rubber material uniform and fine; then the rubber mixture is formed into a film of a certain thickness by an extruder; the surface of the forming drum is cleaned and coated with a layer of release agent to prevent rubber adhesion, and the film is attached to the surface of the forming drum, and the film is bulged from the inside to the outside to form the shape of the tire through the expansion and contraction of the forming drum; a vacuum adsorption device is used to attach the film to the outer surface of the film, and the film surface is made uneven through vacuum adsorption to form a frosted layer; the belt layer material and the intersecting mixture are attached to the outer surface of the tire, and are tightly bonded to the frosted layer; the bonded belt layer is subjected to Heating and pressure treatment are used to form the belt layer of the tire; the formed belt layer is placed in a vulcanizer together with the tire body and tread, and the rubber is vulcanized by heating and pressure to form the final tire structure; the vulcanized tire belt layer needs to undergo post-processing steps such as cooling, inspection and trimming to ensure that the quality of the tire meets the standards; finally, the formed belt layer is subjected to quality inspection, including tests on appearance, size and physical properties, to ensure that each tire meets the specified quality requirements; by using this process, the surface of the film is vacuum-adsorbed during the film expansion stage to make its surface uneven, and when the film surface is covered with the bonding material 19, it is hot-pressed so that the rubber and the film are completely bonded and bonded, and no stratification will occur after cooling.
[0077] Finally, it should be noted that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A belt drum forming process for improving tire NVH, characterized in that: The steps include: S1. Mix the rubber raw materials with carbon black, sulfur, accelerator and additives in a certain proportion, and mix them through a mixing equipment to make the rubber material uniform and fine; S2, forming a rubber sheet of a certain thickness through an extruder; S3. Clean the surface of the building drum and apply a layer of release agent to prevent rubber from adhering. Stick the film to the surface of the building drum. The film bulges from the inside to the outside to form the shape of the tire through the expansion and contraction of the building drum. S4, using a vacuum adsorption device to attach to the outer surface of the film, through vacuum adsorption, making the surface of the film uneven, forming a frosted layer; S5, laminating the belt layer material and the intersecting mixed material on the outer surface of the tire, and bonding them tightly with the frosted layer; S6, using a forming machine to heat and pressure treat the laminated belt layer to form a belt layer of the tire; S7, placing the formed belt layer together with the tire body and the tread into a vulcanizer, and vulcanizing the rubber through heating and pressure to form the final tire structure; S8. The vulcanized tire belt layer needs to be cooled, inspected and trimmed to ensure that the tire quality meets the standards; S9. Carry out quality inspection on the formed belt layer, including tests on appearance, size and physical properties, to ensure that each tire meets the specified quality requirements.
2. A belt drum forming process for improving tire NVH according to claim 1, characterized in that: In the step S1, the auxiliary agents include antioxidants, plasticizers, reinforcing agents, fillers, delay agents, active agents, protective agents, adhesives and colorants.
3. A belt drum forming process for improving tire NVH according to claim 2, characterized in that: The forming drum used in step S3 includes a pneumatic drum and a servo drum.
4. A belt drum forming process for improving tire NVH according to claim 3, characterized in that: The vacuum adsorption device used in step S4 is composed of an adjustment component, two driving components and a plurality of vacuum adsorption components. The plurality of vacuum adsorption components are connected to each other, and the adjustment component drives the plurality of vacuum adsorption components to move in a ring shape. The plurality of vacuum adsorption components are connected to the surface of the film (18) to adsorb a plurality of protrusions on the surface of the film (18) to form a frosted layer.
5. A belt drum forming process for improving tire NVH according to claim 4, characterized in that: The adjustment component comprises a base (1), a limiting slide groove (2), a T-shaped slider (3), a bidirectional screw (4), a motor (5) and an electric push rod (6), wherein two T-shaped sliders (3) and two electric push rods (6) are provided, the base (1) is arranged on the ground, the limiting slide groove (2) is arranged at the upper end of the base (1), the two T-shaped sliders (3) are slidably connected in the limiting slide groove (2), the bidirectional screw (4) is rotatably connected in the limiting slide groove (2), the bidirectional screw (4) is threadedly matched with the two T-shaped sliders (3), the motor (5) is fixedly connected to one side end of the base (1), the output end of the motor (5) movably passes through the inner wall of the limiting slide groove (2) and is fixed to one end of the bidirectional screw (4), and the two electric push rods (6) are respectively fixedly connected to the upper ends of the two electric push rods (6).
6. A belt drum forming process for improving tire NVH according to claim 5, characterized in that: Each group of the driving components comprises a vacuum air pump (7), a rotating block (8) and a connecting block (9); the connecting block (9) is fixedly connected to the extended end of the electric push rod (6); the rotating block (8) is rotatably connected to the surface of the connecting block (9); and the vacuum air pump (7) is fixedly connected to one end of the rotating block (8).
7. A belt drum forming process for improving tire NVH according to claim 6, characterized in that: Each group of the vacuum adsorption components comprises a vacuum adsorption body (10), a first mounting block (11), a second mounting block (12), an adsorption hole (13) and an adsorption cavity (14); a plurality of the adsorption holes (13) are provided; the adsorption cavity (14) is fixedly connected to the vacuum adsorption body (10); the first mounting block (11) is fixedly connected to one side end of the vacuum adsorption body (10); the second mounting block (12) is fixedly connected to the other side end of the vacuum adsorption body (10); the plurality of adsorption holes (13) are all provided on the lower surface of the vacuum adsorption body (10); and the plurality of adsorption holes (13) are all connected to the adsorption cavity (14).
8. A belt drum forming process for improving tire NVH according to claim 7, characterized in that: When the tire belt needs to be stretched or compressed to adapt to the shape of the mold, the pneumatic drum (16) changes the diameter of the first expansion and contraction area (1601) by inflating and deflating, thereby controlling the tension of the belt.
9. A belt drum forming process for improving tire NVH according to claim 8, characterized in that: The servo drum (17) accurately controls its rotation speed and position through a servo motor to adjust the second expansion and contraction area (1701). During the tire molding process, the servo drum (17) very accurately controls the placement and processing of the tire belt.
10. A belt drum forming process for improving tire NVH according to claim 9, characterized in that: The pneumatic drum (16) and the servo drum (17) work together. When forming the side of the tire, the pneumatic drum (16) is used to provide tension on the sidewall material, while the servo drum (17) is used to control the forming of the tire.