Method for simultaneously determining surface charge density and hami constant of micro-nano particles
Through dynamic light scattering technology and DLVO theory, using Na+ and K+ ion specific effects to quantify the surface charge density and Hamek constant of micro-nanoparticles, the problem that the existing technology cannot be measured simultaneously is solved, and high accuracy is achieved. Determination of interfacial properties of micro-nanoparticles.
Patent Information
- Application Number
- CN202411293925.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-11-15
AI Technical Summary
The prior art cannot accurately determine the surface charge density and Hamek constant of micro-nano particles at the same time, and the measurement process is complex, difficult, large sample volume and low accuracy, which affects the catalytic efficiency and bioavailability of micro-nano materials.
Based on the ion-specific effect of the aggregation of micro-nanocolloid particles caused by Na+ and K+, the CCC value of the aggregation is determined by dynamic light scattering technology, combined with DLVO theory, the relationship curve between the surface charge density and Hamek constant is obtained through the simultaneous equation, and the relationship curve between the surface charge density and the Hamek constant is quantitatively Related to both.
The simultaneous accurate determination of the charge density and Hamek constant of the micro-nanoparticles was achieved, which overcomes the shortcomings of the existing methods, improves the accuracy and reliability of the measurement, and is widely used in the study of the interfacial properties of micro-nanomaterials.
Smart Images

Figure CN118961549A_ABST
Abstract
Description
Technical Field
[0001] The invention provides a method for simultaneously measuring the surface charge density and the Hamaker constant of micro-nano particles, belonging to the technical field of performance measurement of nano-micron particles. Background Art
[0002] Surface charge density and Hamaker constant are two very important parameters in the interface properties of micro-nanoparticles. They determine the electrostatic repulsion and van der Waals attraction between micro-nanoparticles, respectively. They further affect the catalytic efficiency of micro-nano materials, the migration and transformation of new micro-nano pollutants, and the bioavailability of drug-loaded micro-nanoparticles by regulating the agglomeration and dispersion characteristics of micro-nanoparticles. Currently, there are many methods to measure the surface charge density and Hamaker constant of different micro-nanoparticles.
[0003] There are several main methods for measuring surface charge density: 1) The surface charge of micro-nanoparticles in suspension is measured by potentiometric titration, and the specific surface area of solid micro-nanoparticles is measured by BET specific surface area determination method, and the surface charge density is calculated using the ratio of the two. Since the micro-nanoparticles are in different states during the measurement of this method, and the BET method has the disadvantages of large sample amount and inability to accurately characterize the inner surface of the particles, the accuracy and reliability of the calculation results are questionable; 2) Using atomic force microscopy technology, by drawing the force curve between the tip of the probe cantilever and the interface of the particle to be measured, the force is associated with the inhomogeneity of the particle surface charge, and the surface charge density of the micro-nanoparticles is quantitatively calculated. This method is difficult to prepare samples, and the measurement results are greatly affected by the roughness of the particle surface, and there are very large random errors; 3) The ion selective electrode method based on the principle of multi-parameter joint analysis of the surface properties of micro-nanoparticles can realize the joint measurement of multiple surface properties including surface charge density and specific surface area. However, this method currently also has problems such as large sample amount required and unstable measurement results of ion selective electrodes; 4) Based on the double layer theory, the surface charge density is estimated by measuring the surface potential. Since it is difficult to directly measure the surface potential, the Zeta potential of the shear surface is usually measured to replace the surface potential. However, the value of the Zeta potential is usually only 1 / 3 to 1 / 6 of the surface potential, and this method will greatly underestimate the surface charge density of micro-nanoparticles.
[0004] The main methods for determining the Hamaker constant are as follows: 1) Using Lifshitz theory to calculate the Hamaker constant. This method requires obtaining the dielectric constant, polarizability or full spectrum characteristics of micro-nanoparticles in advance, which are difficult to obtain characteristic parameters, so the test is difficult; 2) Using atomic force microscopy technology, the Hamaker constant is estimated by measuring the surface force of the particles to be tested. This method has the sample preparation difficulties mentioned above, and the test results are greatly affected by impurities. 3) Using dynamic light scattering technology, based on the colloidal stability (DLVO) theory, the surface potential of the system under CCC conditions is measured to estimate the electrostatic repulsion, and then estimate the Hamaker constant. This method usually also requires the use of Zeta potential instead of surface potential, which makes the Hamaker constant underestimated.
[0005] In summary, existing methods and technologies are unable to simultaneously measure the surface charge density and Hamaker constant of micro-nanoparticles, and the technology itself has problems such as complex measurement process, high technical difficulty, large sample volume and low measurement accuracy, making it difficult to promote and apply. Given that the particle size of micro-nanoparticles is relatively small, they are easily suspended in water to form a stable colloidal system. The stability of micro-nano colloidal particles in aqueous solution depends on the magnitude of the total force acting on the colloidal particles, which is composed of the electrostatic repulsion regulated by the surface charge density and the van der Waals attraction regulated by the Hamaker constant of the particles. Among them, the interaction between ions and micro-nanoparticles will significantly affect the electrostatic repulsion between particles, thereby affecting the stability of micro-nano colloidal particles. In previous studies, we have found that the surface of micro-nanoparticles interacts with counterions of the same valence but with different ions (such as Na + and K + ) between them, which will induce the ion-specific effect of micro-nanoparticle aggregation and produce CCC Na >CCC K Therefore, quantifying the ion-specific effect and establishing a quantitative correlation between the CCC value of micro-nanoparticle aggregation and the interaction between micro-nanoparticles in different ion systems has become a feasible approach to simultaneously determine the surface charge density and Hamaker constant of micro-nanoparticles. Summary of the invention
[0006] In view of the above technical problems, the present invention intends to + and K + Based on the ion-specific effect caused by the aggregation of micro-nano colloidal particles, an effective method was established using dynamic light scattering technology, which can accurately determine the surface charge density and Hamaker constant of micro-nano particles at the same time. This method can overcome the obvious defects of existing methods and technologies and will be a major breakthrough in the study of the interfacial properties of micro-nano materials.
[0007] The specific technical solution is:
[0008] A method for simultaneously determining the surface charge density and Hamaker constant of micro-nanoparticles.
[0009] First, the Na + and K + CCC of micro-nanoparticles under different conditions Na and CCC K ;
[0010] Secondly, in CCC Na and CCC K Under these conditions, the combined forces of electrostatic repulsion and long-range molecular attraction between particles were calculated by quantifying the ion-specific effects of the two ions interacting with the micro-nanoparticle interface.
[0011] Finally, the simultaneous equations give Na + and K + The relationship curve between the surface charge density and the Hamaker constant in the system, the intersection of the two is the surface charge density and the Hamaker constant of the micro-nanoparticles to be measured.
[0012] The specific steps include:
[0013] S1. Prepare a stable colloidal dispersion system of micro-nano particles: dissolve the micro-nano particles in ultrapure water, add NaOH or KOH as a dispersant, adjust the pH of the colloidal suspension to near neutral, use a probe-type ultrasonic processor to ultrasonically disperse, and store for later use.
[0014] S2, based on the dynamic light scattering method, using a laser scattering instrument to determine Na + and K + The CCC value of micro-nanoparticle aggregation under the system, that is, CCC Na and CCC k .
[0015] The specific methods and processes are as follows:
[0016] At a given Na + or K + Under the condition of concentration c0 (mol / L), the dynamic light scattering technology was used to measure the change of the effective diameter of the micro-nano colloidal particles with time during the aggregation process. The growth of the aggregate particle size was derived with respect to time to obtain the relationship between the aggregation rate and time. Then, the overall average aggregation rate of the micro-nano colloidal particles from t = 0 to any t = t0 was calculated by formula (1):
[0017]
[0018] Where D(t) (nm) and D(0) (nm) are the effective diameters of the micro / nanoparticles at time t (t>0) and the initial time (t=0), respectively.
[0019] Build The relationship curve of the inflection point is the CCC value of the aggregation of micro-nanoparticles under this ion condition. According to this method, CCC is obtained respectively. Na and CCC k .
[0020] S3. Calculate Na + and K + Electrostatic repulsion between micro-nanoparticles under the following conditions:
[0021] For a 1:1 electrolyte system, the electrostatic repulsion (P EDL (x)) can be expressed as:
[0022]
[0023] Where, CCC (mol / L) is Na + or K + Critical coagulation concentration under conditions, CCC Na or CCC k ; R (J / mol·K) is the gas constant; T (K) is the absolute temperature; β i for Na + or K + The ionic polarization effective charge coefficients of Z and Z are 1.21 and 1.434, respectively, which reflects the ion-specific effect of the interaction between the two ions and the surface. i for Na + or K + The ion valence is 1; F (C / mol) is the Faraday constant; is the midpoint potential between particles, which can be obtained by formula (3):
[0024]
[0025] Where ε is the dielectric constant of water, 8.9×10 -10 C 2 / J·dm; π is the circumference of a circle; and is the surface potential.
[0026] S4. Calculate Na + and K + Van der Waals attraction when the distance between micro-nanoparticles is x under the following conditions:
[0027]
[0028] In the formula, A eff (J) is the effective Hamaker constant of micro-nanoparticles.
[0029] S5. Based on the classic DLVO theory, Na is calculated by formula (5) + and K + The total force when the distance between micro-nano particles is x under the given conditions, and the relationship between the total force and the distance x between particles is obtained:
[0030] P net (x) = P EDL (x)+P vdw (x) (5)
[0031] S6. Solve the total force equation by assigning approximation method: In Na + or K + In the system, assuming that the A of micro-nanoparticles eff Set the surface potential to any value. Calculate P using equation (2) or (3) EDL (x), and further calculate P by equations (4) and (5) net (x). If at this time P net (x) The highest point>0, then the preset Too high, set it lower Recalculate P net (x), until P net (x) until the highest point = 0, record the A eff The corresponding condition
[0032] S7, based on S6 According to formula (6), the The surface charge density σ0 of the micro-nanoparticles corresponding to the condition is the preset A eff The surface charge density σ0 of micro-nanoparticles under the following conditions:
[0033] In the formula, is a symbolic function, when hour when hour It means that the micro-nanoparticles are positively charged. hour Indicates that the micro-nanoparticles are negatively charged; ε0 is the vacuum dielectric constant of 8.85×10 -12 C 2 / J·m; D=80 represents the relative dielectric constant of water.
[0034] S8. Based on the method flow of S6 and S7, a series of settings A are obtained. eff σ0 under the conditions of Na + and K +A eff vsσ0, the intersection of the two curves is the true surface charge density and Hamaker constant value of the micro-nanoparticles.
[0035] According to the method of the present invention, as long as the laser scattering instrument is used to obtain the micro-nano colloidal particles to be measured in Na + and K + By establishing the CCC value of the micro-nanoparticle agglomeration under the two-ion system and the quantitative correlation between the CCC value and the interaction between the particles, the surface charge density and the Hamaker constant of the micro-nanoparticles can be determined simultaneously. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is a schematic diagram of CCC determination of the present invention;
[0037] Figure 2 Schematic diagram of the relationship between the total force between micro-nanoparticles and the distance of the present invention;
[0038] Figure 3 A schematic diagram for determining the surface charge properties of the present invention;
[0039] Figure 4 The change of the particle size of montmorillonite nano-colloidal particles agglomerates over time under the NaNO3 condition of the embodiment;
[0040] Figure 5 The change of the particle size of montmorillonite nano-colloidal particles agglomerates over time under the KNO3 condition of the embodiment;
[0041] Figure 6 The overall average aggregation rate of montmorillonite nano-colloidal particles under the NaNO3 condition of the embodiment varies with the electrolyte concentration;
[0042] Figure 7 The overall average aggregation rate of montmorillonite nano-colloidal particles under the KNO3 condition of the embodiment varies with the electrolyte concentration;
[0043] Figure 8 Schematic diagram for determining the surface charge density and Hamaker constant of montmorillonite nanoparticles of the embodiment. DETAILED DESCRIPTION
[0044] The specific technical solution of the present invention is explained in conjunction with embodiments.
[0045] The method for simultaneously measuring the surface charge density and the Hamaker constant of micro-nano particles provided by the present invention comprises the following steps:
[0046] S1. Prepare a stable colloidal dispersion system of micro-nano particles: dissolve the micro-nano particles in ultrapure water, add a small amount of NaOH or KOH as a dispersant, adjust the pH of the colloidal suspension to near neutral, use a probe-type ultrasonic processor to ultrasonically disperse, and store for later use.
[0047] S2, based on the dynamic light scattering method, using a laser scattering instrument to determine Na + and K + The CCC value of micro-nanoparticle aggregation under the system, that is, CCC Na and CCC k The specific methods and processes are as follows:
[0048] At a given Na + or K + Under the condition of concentration c0 (mol / L), the dynamic light scattering technology was used to measure the change of the effective diameter of the micro-nano colloidal particles with time during the aggregation process. The growth of the aggregate particle size was derived with respect to time to obtain the relationship between the aggregation rate and time. Then, the overall average aggregation rate of the micro-nano colloidal particles from t = 0 to any t = t0 was calculated by the following formula (1):
[0049]
[0050] Where D(t) (nm) and D(0) (nm) are the effective diameters of the micro / nanoparticles at time t (t>0) and the initial time (t=0), respectively.
[0051] Build The relationship curve of , the ion concentration corresponding to the inflection point is the CCC value of the micro-nanoparticle aggregation under the ion condition, such as Figure 1 According to this method, CCC is obtained respectively. Na and CCC k .
[0052] S3. Calculate Na + and K + Electrostatic repulsion between micro-nanoparticles under the following conditions:
[0053] For a 1:1 electrolyte system, the electrostatic repulsion (P EDL (x)) can be expressed as:
[0054]
[0055] Where, CCC (mol / L) is Na + or K + Critical coagulation concentration under conditions, CCC Na or CCC k; R (J / mol·K) is the gas constant; T (K) is the absolute temperature; β i for Na + or K + The ionic polarization effective charge coefficients of Z and Z are 1.21 and 1.434, respectively, which reflects the ion-specific effect of the interaction between the two ions and the surface. i for Na + or K + The ion valence is 1; F (C / mol) is the Faraday constant; is the midpoint potential between particles, which can be obtained by formula (3):
[0056]
[0057] Where ε is the dielectric constant of water, 8.9×10 -10 C 2 / J·dm; π is the circumference of a circle; and is the surface potential.
[0058] S4. Calculate Na + and K + Van der Waals attraction when the distance between micro-nanoparticles is x under the following conditions:
[0059]
[0060] In the formula, A eff (J) is the effective Hamaker constant of micro-nanoparticles.
[0061] S5. Based on the classic DLVO theory, Na is calculated by formula (5) + and K + The total force when the distance between micro-nano particles is x under the given conditions, and the relationship between the total force and the distance x between particles is obtained:
[0062] P net (x) = {P EDL (x)+P vdw (x) (5)
[0063] S6. Solve the total force equation by assigning approximation method: In Na + or K + In the system, assuming that the A of micro-nanoparticles eff Set the surface potential to any value. Calculate P using equation (2) or (3) EDL (x), and further calculate P by equations (4) and (5) net (x). If at this time P net(x) The highest point>0, then the preset Too high, further assume a lower Recalculate P net (x), until P net (x) The highest point = 0, such as Figure 2 As shown, record the A eff The corresponding condition
[0064] S7, based on S6 According to formula (6), the The surface charge density σ0 of the micro-nanoparticles corresponding to the condition is the preset A eff The surface charge density σ0 of micro-nanoparticles under the following conditions:
[0065]
[0066] In the formula, is a symbolic function, when hour when hour It means that the micro-nanoparticles are positively charged. hour Indicates that the micro-nanoparticles are negatively charged; ε0 is the vacuum dielectric constant of 8.85×10 -12 C 2 / J·m; D=80 represents the relative dielectric constant of water.
[0067] S8. Based on the method flow of S6 and S7, a series of settings A are obtained. eff σ0 under the conditions of Na + and K + A eff vsσ0 plot, such as Figure 3 As shown, the intersection of the two curves is the true surface charge density and Hamaker constant value of the micro-nanoparticles.
[0068] The following is an example of the determination of the surface charge density and Hamaker constant of montmorillonite nanoparticles:
[0069] Firstly, the changes of hydrodynamic diameter of montmorillonite nano-colloidal particles with time under NaNO3 and KNO3 electrolyte conditions were measured by laser scattering instrument. Figure 4 and Figure 5 As shown:
[0070] based on Figure 4 and Figure 5 The overall average aggregation rate of montmorillonite nanoparticles under NaNO3 and KNO3 conditions was calculated using equation (1). Build Relationship curve, such as Figure 6 and Figure 7 The concentration corresponding to the inflection point is the CCC value of montmorillonite nanocolloid particles under this ionic condition, that is, CCC Na and CCC k They are 0.1328mol / L and 0.0803mol / L respectively.
[0071] Using equations (2)-(5), calculate CCC Na and CCC k The total force of montmorillonite nano-colloidal particles coagulation under the conditions. Set a series of Hamaker constants A eff Numerical value, find P net When (x) is 0 The specific A is further calculated using formula (6) eff The surface charge density σ0 corresponds to the condition.
[0072] In Na + and K + A eff vsσ0 plot, such as Figure 8 As shown in the figure, the values corresponding to the intersection coordinates of the two curves are the surface charge density of montmorillonite nano-colloidal particles 0.0874C / m 2 and the Hamaker constant of 6.15×10 -20 J.
Claims
1. Method for simultaneous determination of surface charge density and Hamaker constant of micro-nanoparticles, It is characterized in that The process includes: First, Na was determined by light scattering technique. + and K + Critical coagulation concentration (CCC) of micro-nanoparticles under certain conditions; Secondly, under this concentration condition, the combined force of electrostatic repulsion and long-range molecular attraction between particles was calculated by quantifying the ion-specific effects of the two ions interacting with the micro-nanoparticle interface; Finally, the simultaneous equations give Na + and K + The relationship curve between the surface charge density and the Hamaker constant in the system, the intersection of the two is the surface charge density and the Hamaker constant of the micro-nanoparticles to be measured.
2. The method for simultaneously measuring the surface charge density and the Hamaker constant of micro-nanoparticles according to claim 1, It is characterized in that The following steps are involved: S1. Prepare a stable micro-nano particle colloidal dispersion system: dissolve the micro-nano particles in ultrapure water, add NaOH or KOH as a dispersant, adjust the pH of the colloidal suspension to near neutral, use a probe-type ultrasonic processor to ultrasonically disperse, and store for later use; S2, based on the dynamic light scattering method, using a laser scattering instrument to determine Na + and K + The CCC value of micro-nanoparticle aggregation under the system, that is, CCC Na and CCC k ; S3. Calculate Na + and K + Electrostatic repulsion between micro-nanoparticles under the following conditions: For a 1:1 electrolyte system, the electrostatic repulsion force P when the distance between micro-nanoparticles is x (nm) EDL (x) is: Where, CCC (mol / L) is Na + or K + Critical coagulation concentration under conditions, CCC Na or CCC k ; R (J / mol·K) is the gas constant; T (K) is the absolute temperature; β i for Na + or K + The ionic polarization effective charge coefficients of Z and Z are 1.21 and 1.434, respectively, which reflects the ion-specific effect of the interaction between the two ions and the surface. i for Na + or K + The ion valence is 1; F (C / mol) is the Faraday constant; is the midpoint potential between particles, which can be obtained by formula (2): Where ε is the dielectric constant of water, 8.9×10 -10 C 2 / J·dm; π is the circumference of a circle; and is the surface potential. S4. Calculate Na + and K + The van der Waals force P when the distance between micro-nanoparticles is x under the condition vdw (x): In the formula, A eff (J) is the effective Hamaker constant of micro-nanoparticles; S5. Based on the classic DLVO theory, Na is calculated by formula (4) + and K + The total force when the distance between micro-nano particles is x under the given conditions, and the relationship between the total force and the distance x between particles is obtained: P net (x)=P EDL (x)+P vdw (x) (4) S6. Solve the total force equation by assigning approximation method. + or K + In the system, assuming that the micro-nanoparticle A eff Set the surface potential to any value. Using equations (1) and (2) to calculate P EDL (x), and further calculate P by equations (3) and (4) net (x); if at this time P net (x) The highest point>0, then the preset Too high, set it lower Recalculate P net (x), until P net (x) until the highest point = 0, record the A eff The corresponding condition S7, based on S6 According to formula (5), the The surface charge density of micro-nanoparticles under the conditions 0 , which is the preset A eff The surface charge density σ of micro / nanoparticles under the condition 0 : In the formula, is a symbolic function, when hour when hour It means that the micro-nanoparticles are positively charged. hour Indicates that the micro-nanoparticles are negatively charged; ε 0 The dielectric constant of vacuum is 8.85×10 - 12 C 2 / J·m; D=80 represents the relative dielectric constant of water; S8. Based on the method flow of S6 and S7, a series of settings A are obtained. eff σ under the condition 0 , respectively in Na + and K + A eff vsσ 0 Plot the graph, and the intersection of the two curves is the true surface charge density and Hamaker constant value of the micro-nanoparticles to be tested.
3. The method for simultaneously measuring the surface charge density and the Hamaker constant of micro-nanoparticles according to claim 2, It is characterized in that S2 specific methods and processes are as follows: At a given Na + or K + Concentration 0 Under the condition of (mol / L), the dynamic light scattering technology was used to measure the change of effective diameter of micro-nano colloidal particles with time during the aggregation process. The growth of the aggregate size was derived with respect to time to obtain the relationship between the aggregation rate and time. Then, the micro-nano colloidal particles from t = 0 to any t = t were calculated by formula (6). 0 The overall average condensation rate at time (nm / min): Where D(t) (nm) and D(0) (nm) are the effective diameters of the micro / nanoparticles at time t (t>0) and the initial time (t=0), respectively; Build vsc 0 The relationship curve of the inflection point is the CCC value of the aggregation of micro-nanoparticles under this ion condition. According to this method, CCC is obtained respectively. Na and CCC k .
Citation Information
Cited By
A method and system for automated determination of nanoparticle hamaker constant based on dynamic light scattering data
CN123028994A