Semiconductor device
By adopting the combination of alternating laminates, memory laminate structures and sealing spacers in a vertical semiconductor device, the problem of gap filling of high aspect ratio structures is solved, the reliability of the device and the compactness of the chip are improved, and the defect of growth bad blocks is avoided .
Patent Information
- Application Number
- CN202411021725.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2019-11-29
- Filing Date
- 2020-06-05
- Publication Date
- 2024-11-15
AI Technical Summary
When manufacturing vertical semiconductor devices, the prior art is difficult to effectively solve the gap filling problem of high-profile structures, resulting in increased device reliability and chip size.
Using the combination of alternating laminates, memory laminate structures, source contact layer and sealing spacer, a vertical semiconductor device is formed through specific process steps, including forming a memory laminate structure on the alternating laminates, using the source contact layer and sealing spacer. Improve the etch resistance and sealing properties of the device.
The reliability of the vertical semiconductor device is improved, the chip size is reduced, and the filling characteristics of the contact plug are improved by optimizing the wet etch resistance of the sealing spacer to prevent growth of bad block defects.
Smart Images

Figure CN118973267A_ABST
Abstract
Description
[0001] This application is a divisional application of the original invention patent application with application number 202010503428.3 (application date: June 5, 2020, invention name: vertical semiconductor device and manufacturing method thereof). Technical Field
[0002] Embodiments of the present disclosure relate to semiconductor devices, and more particularly, to a method of manufacturing a vertical semiconductor device. Background Art
[0003] The manufacture of electronic devices such as semiconductor devices includes a gap filling process for forming a three-dimensional structure or a high aspect ratio structure. For example, a gap filling process for forming a high aspect ratio structure is performed when manufacturing a vertical semiconductor device. Summary of the invention
[0004] Embodiments of the present disclosure relate to a vertical semiconductor device having improved reliability and a method of manufacturing the vertical semiconductor device.
[0005] According to an embodiment of the present disclosure, a semiconductor device includes: an alternating stack, which is arranged above a lower structure and includes a plurality of gate electrodes and a plurality of dielectric layers stacked alternately; a memory stack structure, which includes a channel layer extending to penetrate the alternating stack and a memory layer surrounding the channel layer; a source contact layer, which contacts the lower outer wall of the vertical channel layer and is arranged between the lower structure and the alternating stack; a source contact plug, which is spaced apart from the memory stack structure and extends to penetrate the alternating stack; and a sealing spacer, which is arranged to seal the gate electrode and is arranged between the source contact plug and the gate electrode, the etching resistance of the sealing spacer being different from the etching resistance of the dielectric layer.
[0006] According to another embodiment of the present disclosure, a method for manufacturing a semiconductor device includes the following steps: forming a source sacrificial layer above a lower structure; forming a multilayer stack in which multiple dielectric layers and multiple sacrificial layers are alternately stacked above the source sacrificial layer; forming a memory stack structure including a channel layer and a memory layer, the memory stack structure extending to penetrate the multilayer stack and the source sacrificial layer; forming a vertical contact recess spaced apart from the memory stack structure and extending to penetrate the multilayer stack and the source sacrificial layer; exposing a lower outer wall of the channel layer by selectively removing the source sacrificial layer and the lower portion of the memory layer of the memory stack structure through the vertical contact recess; forming a source contact layer surrounding the lower outer wall of the channel layer; replacing the sacrificial layer of the multilayer stack with a gate electrode to form an alternating stack; forming a carbon-containing spacer above the source contact layer and the gate electrode to seal the sidewalls of the vertical contact recess; and forming a source contact plug in the vertical contact recess.
[0007] According to another embodiment of the present disclosure, a method for manufacturing a semiconductor device includes the following steps: forming a first multilayer stack including a liner layer and a source sacrificial layer above a lower structure; forming a second multilayer stack including a dielectric layer and a sacrificial layer above the first multilayer stack; forming a vertical contact recess extending through the second multilayer stack and the source sacrificial layer; replacing the source sacrificial layer with a source contact layer; forming a carbon-containing spacer on a sidewall of the vertical contact recess; replacing the sacrificial layer with a conductive layer; and forming a source contact plug in the vertical contact recess. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 is a cross-sectional view illustrating a vertical semiconductor device according to an embodiment of the present disclosure.
[0009] Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 and Fig.14 is a cross-sectional view illustrating a method of manufacturing a vertical semiconductor device according to an embodiment of the present disclosure.
[0010] Fig.15 is a cross-sectional view illustrating a vertical semiconductor device according to another embodiment of the present disclosure.
[0011] Fig.16 , Fig.17 , Fig.18 , Fig.19 , Fig. 20 , Fig.21 , Fig. 22 , Fig.23 , Fig.24 , Fig.25 , Fig.26 , Fig. 27 and Fig.28 is a cross-sectional view illustrating a method of manufacturing a vertical semiconductor device according to another embodiment of the present disclosure. DETAILED DESCRIPTION
[0012] Embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. However, embodiments of the present disclosure may be implemented in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided so that the present disclosure will be thorough and complete, and will fully convey the scope of the various embodiments of the present disclosure to those skilled in the art. Throughout the present disclosure, similar reference numerals throughout the various drawings and embodiments of the present disclosure represent similar components.
[0013] The drawings are not necessarily to scale, and in some cases, the proportions may be exaggerated to clearly illustrate features of the embodiments. When a first layer is referred to as being "on" a second layer or "on" a substrate, it refers not only to the case where the first layer is directly formed on the second layer or substrate, but also to the case where a third layer exists between the first layer and the second layer or substrate.
[0014] Figure 1 is a cross-sectional view showing a vertical semiconductor device 100 according to an embodiment of the present disclosure.
[0015] Reference Figure 1 , the vertical semiconductor device 100 may be disposed above the lower structure 101, and the vertical semiconductor device 100 may include: an alternating stack 120 in which dielectric layers 111 and gate electrodes 127 are alternately stacked; a memory stack structure 120P, which includes a channel layer 118 extending to penetrate the alternating stack 120 and a stack of layers (or memory layers) 115, 116 and 117 surrounding the channel layer 118; a source contact layer 124, which is disposed between the lower structure 101 and the alternating stack 120, while contacting the outer wall of the bottom of the channel layer 118; a source contact plug 132, which is spaced apart from the memory stack structure 120P and extends through the alternating stack 120; and a sealing spacer 128, which has an etching resistance different from that of the dielectric layer 111, while sealing the outer wall of the source contact plug 132. The sealing spacer 128 may seal the gate electrode 127 and be disposed between the source contact plug 132 and the gate electrode 127, and may have a different etching resistance than the dielectric layer 111. The outer wall of the source contact plug 132 may be surrounded by the sealing spacer 128, and the sealing spacer 128 may extend vertically to cover the gate electrode 127, the dielectric layer 111, and the source contact layer 124.
[0016] The lower structure 101 may include a material suitable for semiconductor processing. The lower structure 101 may include a substrate, and the substrate may include a semiconductor substrate. For example, the lower structure 101 may be a silicon substrate, a single crystal silicon substrate, a polycrystalline silicon substrate, an amorphous silicon substrate, a silicon germanium substrate, a single crystal silicon germanium substrate, a polycrystalline silicon germanium substrate, a carbon-doped silicon substrate, a combination thereof, or a multilayer thereof. The lower structure 101 may include other semiconductor materials, such as germanium. The lower structure 101 may include a III / V semiconductor substrate such as a compound semiconductor substrate, such as GaAs. The lower structure 101 may include a silicon on insulator (SOI) substrate. Although not shown, according to another embodiment of the present disclosure, the lower structure 101 may include a substrate, at least one control circuit formed above the substrate, and a multilayer metal line.
[0017] A multi-layer stack structure may be formed over the lower structure 101. The multi-layer stack structure may include a source horizontal stack 110 and an alternating stack 120 over the source horizontal stack 110. The source horizontal stack 110 may have a lower height than the alternating stack 120.
[0018] The source horizontal stack 110 may include a lower source layer 102, a source contact layer 124, and an upper source layer 106. The source contact layer 124 may be formed above the lower source layer 102, and the upper source layer 106 may be formed above the source contact layer 124. The source contact layer 124 may be disposed between the lower source layer 102 and the upper source layer 106. The lower source layer 102, the upper source layer 106, and the source contact layer 124 may include semiconductor materials. The lower source layer 102, the upper source layer 106, and the source contact layer 124 may include polysilicon. The source contact layer 124 may include polysilicon doped with phosphorus (P). The source contact layer 124 may include polysilicon containing carbon. The source contact layer 124 may include a stack of phosphorus-doped polysilicon (SiP) and carbon-doped polysilicon (SiC). The lower source layer 102 and the upper source layer 106 may include undoped polysilicon or doped polysilicon.
[0019] The alternating stack 120 may be referred to as a memory cell stack or a memory cell string. The alternating stack 120 may have a structure in which a plurality of dielectric layers 111 and a plurality of gate electrodes 127 are alternately stacked. The top dielectric layer 113 among the dielectric layers 111 may be thicker than the dielectric layer 111 at a level lower than the top dielectric layer 113. The dielectric layer 111 may include silicon oxide. The gate electrode 127 may include a low resistance material. The gate electrode 127 may include a metal-based material. The gate electrode 127 may include a metal, a metal silicide, a metal nitride, or a combination thereof. For example, the metal may include nickel, cobalt, platinum, titanium, tantalum, or tungsten. The metal silicide may include nickel silicide, cobalt silicide, platinum silicide, titanium silicide, tantalum silicide, or tungsten silicide. The gate electrode 127 may include a stack of titanium nitride and tungsten. The end of the gate electrode 127 may have a shape that is horizontally recessed from the end of the dielectric layer 111.
[0020] The memory stack structure 120P may extend vertically to penetrate the alternating stack 120. The memory stack structure 120P may have a columnar shape. The memory stack structure 120P may include a blocking layer 115, a charge trapping layer 116, a tunnel dielectric layer 117, a channel layer 118, and a core dielectric layer 119. The memory stack structure 120P may include an ONOP structure. The ONOP structure may include a stack of oxide, nitride, oxide, and polysilicon layers. The blocking layer 115 and the tunnel dielectric layer 117 may include an oxide, the charge trapping layer 116 may include a nitride, and the channel layer 118 may include polysilicon. According to an embodiment of the present disclosure, the blocking layer 115 may include a high dielectric material, and the high dielectric material may include aluminum oxide or hafnium oxide. The channel layer 118 may have a cylindrical shape including an internal space. The tunnel dielectric layer 117 may be formed on the outer wall of the channel layer 118, and the charge trapping layer 116 may be formed on the outer wall of the tunnel dielectric layer 117. The barrier layer 115 may be formed on the outer wall of the charge trapping layer 116. The inner space of the channel layer 118 may be substantially completely filled with the core dielectric layer 119. The core dielectric layer 119 may include silicon oxide or silicon nitride. The stack of the barrier layer 115, the charge trapping layer 116, and the tunnel dielectric layer 117 may be referred to as a memory layer 115 / 116 / 117, which may be in a ring shape surrounding the outer wall of the channel layer 118.
[0021] The source contact layer 124 may selectively and horizontally penetrate the bottom of the memory layer 115 / 116 / 117 of the memory stack structure 120P to contact the lower outer wall of the channel layer 118. The source contact layer 124 may have a shape surrounding the lower outer wall of the channel layer 118.
[0022] The source contact plug 132 may include a stack of a silicon-containing material (or a silicon-containing material pattern) 129 and a metal-containing material (or a metal-containing material pattern) 131, and may further include a barrier material (or barrier material layer) 130 between the silicon-containing material 129 and the metal-containing material 131. The silicon-containing material 129 may include polysilicon, and the metal-containing material 131 may include tungsten. The barrier material 130 may include titanium nitride. According to another embodiment of the present disclosure, the source contact plug 132 may be formed only of tungsten. The lower portion of the source contact plug 132 may be connected to the lower source layer 102 of the source horizontal stack 110.
[0023] The sealing spacer 128 may be formed between the source contact plug 132 and the gate electrode 127. The sealing spacer 128 may extend to be formed between the dielectric layers 111 and 113 and the source contact plug 132. For example, the sealing spacer 128 may extend along a vertical direction in which the gate electrode 127 and the dielectric layers 111 and 113 of the alternating stack 120 are stacked, so that the sealing spacer 128 may be disposed between the source contact plug 132 and the dielectric layers 111 and 113. The sealing spacer 128 may be continuous in the stacking direction of the alternating stack 120. The sealing spacer 128 may include one or more protrusions 128P, and the protrusions 128P may be respectively connected to ends of the gate electrode 127 (for example, Fig.10 The protrusion 128P of the sealing spacer 128 may extend in a horizontal direction perpendicular to the stacking direction of the alternating stack 120. The protrusion 128P of the sealing spacer 128 may seal the recessed end of the gate electrode 127. The sealing spacer 128 may seal the side surfaces of the dielectric layers 111 and 113. The sealing spacer 128 may seal the side surfaces of the source contact layer 124. The sealing spacer 128 may seal the side surfaces of the upper source layer 106, and may not seal a portion of the surface of the lower source layer 102. The sealing spacer 128 may substantially completely surround the outer wall of the source contact plug 132.
[0024] The sealing spacer 128 may include a silicon oxide-based material. The sealing spacer 128 may include a low dielectric material. The low dielectric material may have a dielectric constant lower than that of silicon nitride. The sealing spacer 128 may have a dielectric constant lower than about 7. The sealing spacer 128 may be thinner than the dielectric layers 111 and 113 and the gate electrode 127. Figure 1In the illustrated embodiment, the thickness of the sealing spacer 128 in the horizontal direction may be smaller than the thickness of each of the dielectric layers 111 and 113 and the gate electrode 127 in the vertical direction. For example, the thickness of the protrusion 128P of the sealing spacer 128 in the horizontal direction may be smaller than the thickness of each of the dielectric layers 111 and 113 and the gate electrode 127 in the vertical direction. The sealing spacer 128 may be a layer of a different material from the dielectric layers 111 and 113. The sealing spacer 128 may be a layer of a different material from the gate electrode 127. The sealing spacer 128 may include a material having high wet etching resistance. The wet etching resistance of the sealing spacer 128 may be derived from carbon. The sealing spacer 128 may include a carbon-containing material, and the dielectric layers 111 and 113 may be carbon-free materials. The dielectric layers 111 and 113 may be formed of carbon-free silicon oxide, and the sealing spacer 128 may be formed of carbon-containing silicon oxide. For example, dielectric layers 111 and 113 may be formed of SiO2, and sealing spacer 128 may be formed of SiCO. SiCO may be more etch-resistant than SiO2. The carbon content of SiCO may be less than the silicon content and the oxygen content. For example, SiCO may have a composition ratio of 34 at% silicon (Si), 40 at% oxygen, and 17 at% carbon. SiCO may have a lower dielectric constant than silicon nitride (Si3N4).
[0025] The sealing spacer 128 may be formed to have a size of approximately to For example, the protrusion 128P of the sealing spacer 128 may be relatively Figure 1 The orientation in the horizontal direction has to range. The high wet etching resistance of SiCO can reduce the thickness of the sealing spacer 128. Specifically, the high wet etching resistance of SiCO can prevent the sealing spacer 128 from being significantly etched when one or more cleaning processes are performed. Therefore, even when the sealing spacer 128 is formed to have a relatively small thickness and one or more cleaning processes are performed on the sealing spacer 128, the thickness of the sealing spacer 128 can be kept thick enough to substantially prevent the growth of bad block (GBB) defects. As a result, the size of the source contact plug 132 for separating the unit blocks can be reduced, which ultimately reduces the chip size. In addition, even when the vertical contact recess in which the source contact plug 132 is formed has a relatively small size (for example, Figure 1 When the width in the horizontal direction is 0.0447 W (in the horizontal direction), since the sealing spacer 128 may be formed to have a relatively small thickness, the vertical contact recess may be filled with the source contact plug 132 without a gap.
[0026] According to another embodiment of the present disclosure, the sealing spacer 128 may include SiCN, SiBCN, SiBN, or a combination thereof. The wet etching resistance of the sealing spacer 128 may be obtained by carbon, nitrogen, boron, or a combination thereof.
[0027] According to another embodiment of the present disclosure, the sealing spacer 128 may include a stack of one or more carbon-free silicon oxide layers and one or more carbon-containing silicon oxide layers. For example, after thinly depositing a carbon-free silicon oxide layer (e.g., a SiO2 layer), a carbon-containing silicon oxide layer (e.g., a SiCO layer) may be deposited over the carbon-free silicon oxide layer. As a result, the carbon-containing silicon oxide layer may be in direct contact with the source contact plug 132.
[0028] Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 and Fig.14 is a cross-sectional view showing a method for manufacturing a vertical semiconductor device according to an embodiment of the present disclosure. For example, Figures 2 to 14 Show Figure 1 A method for manufacturing a vertical semiconductor device 100 is provided.
[0029] Reference Figure 2 , a first multi-layer stack 110S may be formed over the lower structure 101. A second multi-layer stack 120M may be formed over the first multi-layer stack 110S.
[0030] The first multi-layer stack 110S may be a stack including a lower source layer 102, a first liner layer 103, a source sacrificial layer 104, a second liner layer 105, and an upper source layer 106. Figure 2 In the illustrated embodiment, the first multi-layer stack 110S may have a source sacrificial layer 104 formed between a lower source layer 102 and an upper source layer 106, a first liner layer 103 formed between the source sacrificial layer 104 and the lower source layer 102, and a second liner layer 105 formed between the source sacrificial layer 104 and the upper source layer 106. The lower source layer 102, the upper source layer 106, and the source sacrificial layer 104 may include the same material, and the first liner layer 103 and the second liner layer 105 may include a material different from that of the lower source layer 102, the upper source layer 106, and the source sacrificial layer 104.
[0031] The lower source layer 102 and the upper source layer 106 may have an etching selectivity with respect to the first liner layer 103 and the second liner layer 105. The lower source layer 102, the upper source layer 106, and the source sacrificial layer 104 may include a semiconductor material, and the first liner layer 103 and the second liner layer 105 may include a dielectric material. The lower source layer 102, the upper source layer 106, and the source sacrificial layer 104 may include polysilicon, and the first liner layer 103 and the second liner layer 105 may include silicon oxide. The first liner layer 103 and the second liner layer 105 may be thinner than the lower source layer 102, the upper source layer 106, and the source sacrificial layer 104. For example, the lower source layer 102 and the upper source layer 106 may be Figure 2 The first liner layer 103 and the second liner layer 105 may each have a thickness of about 8 nm in the vertical direction. The thickness of the source sacrificial layer 104 may be the same as or thinner than that of the lower source layer 102 and the upper source layer 106.
[0032] The first liner layer 103 and the second liner layer 105 may protect the lower source layer 102 and the upper source layer 106 while the source sacrificial layer 104 is removed.
[0033] The first liner layer 103 and the second liner layer 105 may include a silicon oxide-based material. One or both of the first liner layer 103 and the second liner layer 105 may include SiO2, SiCO, or a combination thereof.
[0034] The second multilayer stack 120M may be thicker than the first multilayer stack 110S. The second multilayer stack 120M may include a dielectric layer 111 and a sacrificial layer 112. The second multilayer stack 120M may include an alternating stack of dielectric layers 111 and sacrificial layers 112. The dielectric layers 111 and sacrificial layers 112 may be alternately stacked multiple times. The dielectric layers 111 and sacrificial layers 112 may include different materials. The dielectric layer 111 may have an etching selectivity relative to the sacrificial layer 112. The dielectric layer 111 may include silicon oxide, and the sacrificial layer 112 may include silicon nitride. The dielectric layer 111 and the sacrificial layer 112 may have substantially the same thickness. The dielectric layer 111 and the sacrificial layer 112 may be thicker than the first liner layer 103 and the second liner layer 105, and the dielectric layer 111 and the sacrificial layer 112 may be thinner than the lower source layer 102 and the upper source layer 106.
[0035] The dielectric layer 111 and the sacrificial layer 112 may be formed using chemical vapor deposition (CVD) or atomic layer deposition (ALD). The uppermost dielectric layer (or top dielectric layer) 113 formed on top of the second multilayer stack 120M may be attacked and damaged by subsequent processes. Therefore, the top dielectric layer 113 may be formed to be thicker than other dielectric layers 111 below the top dielectric layer 113. The top dielectric layer 113 may be used as an etching barrier.
[0036] The first liner layer 103 and the second liner layer 105 may be thinner than the dielectric layers 111 and 113, the lower source layer 102, the upper source layer 106, and the source sacrificial layer 104. The first liner layer 103 and the second liner layer 105 may include a material different from the dielectric layers 111 and 113. The first liner layer 103 and the second liner layer 105 may include a material having high wet etching resistance. The wet etching resistance of the first liner layer 103 and the second liner layer 105 may be derived from carbon. The first liner layer 103 and the second liner layer 105 may include a carbon-containing material, and the dielectric layers 111 and 113 may include a carbon-free material. The dielectric layers 111 and 113 may include carbon-free silicon oxide, and the first liner layer 103 and the second liner layer 105 may include carbon-containing silicon oxide. For example, the dielectric layers 111 and 113 may be SiO2, and the first liner layer 103 and the second liner layer 105 may be SiCO. SiCO may be more etch-resistant than SiO2. The carbon content of SiCO may be less than the silicon content and the oxygen content. For example, SiCO may have a composition ratio of 34 at% silicon (Si), 40 at% oxygen, and 17 at% carbon.
[0037] The first liner layer 103 and the second liner layer 105 may be formed to have approximately to For example, each of the first liner layer 103 and the second liner layer 105 may be relative to Figure 2 The orientation in the vertical direction has to The thickness of the first liner layer 103 and the second liner layer 105 can be within a range. The high wet etching resistance of SiCO can reduce the thickness of the first liner layer 103 and the second liner layer 105. For example, the high wet etching resistance of SiCO can prevent the first liner layer 103 and the second liner layer 105 from being significantly etched while the source sacrificial layer 104 is removed in the wet etching process. Therefore, even when each of the first liner layer 103 and the second liner layer 105 is formed to have a relatively small thickness, the first liner layer 103 and the second liner layer 105 can protect the lower source layer 102 and the upper source layer 106, respectively, while the source sacrificial layer 104 is removed in the wet etching process. As a result, the height of the first multi-layer stack 110S including the first liner layer 103 and the second liner layer 105 can be reduced.
[0038] According to another embodiment of the present disclosure, the first liner layer 103 and the second liner layer 105 may further include nitrogen, boron, or a combination thereof in addition to carbon.
[0039] According to another embodiment of the present disclosure, the first liner layer 103 and the second liner layer 105 may include a stack of one or more carbon-free silicon oxide layers and one or more carbon-containing silicon oxide layers. For example, after thinly depositing the carbon-free silicon oxide layer, the carbon-containing silicon oxide layer may be deposited on the carbon-free silicon oxide layer.
[0040] According to another embodiment of the present disclosure, the first liner layer 103 may be formed of SiO 2 , and the second liner layer 105 may be formed of SiCO.
[0041] According to another embodiment of the present disclosure, the stack of the second liner layer 105 and the upper source layer 106 may be replaced by a layer of SiCO.
[0042] As described above, when one or both of the first liner layer 103 and the second liner layer 105 are formed of SiCO and when the stack of the second liner layer 105 and the upper source layer 106 is replaced by a layer of SiCO, not only is there no significant thickness loss due to wet etching chemicals, but also while performing subsequent processes for forming a horizontal contact recess and a process for expanding the horizontal contact recess (i.e., a dry etching process and a wet etching process for removing the blocking layer, the charge trapping layer, and the tunnel dielectric layer), the breakdown voltage (BV) characteristics of the source contact plug can be improved due to the small thickness loss of SiCO.
[0043] Reference Figure 3 , a vertical opening 114 may be formed. The vertical opening 114 may be formed by sequentially etching the second multi-layer stack 120M and partially etching the first multi-layer stack 110S.
[0044] The vertical opening 114 may be formed substantially perpendicular to the surface (e.g., top surface) of the lower structure 101. The vertical opening 114 may be formed to penetrate the second multilayer stack 120M and partially penetrate the first multilayer stack 110S. Although not shown, from the perspective of the plan view, a plurality of vertical openings 114 may be formed in a hole array structure. When the vertical opening 114 is formed, the surface of the lower structure 101 may not be exposed. For example, a portion of the lower source layer 102 may remain below the bottom surface of the vertical opening 114. The vertical opening 114 may be referred to as a vertical recess, a through hole, a vertical hole, or a channel hole.
[0045] Reference Figure 4 , a memory stack structure 120P may be formed in the vertical opening 114. The memory stack structure 120P may have a pillar shape filling the vertical opening 114.
[0046] The memory stack structure 120P may include a blocking layer 115, a charge trapping layer 116, a tunnel dielectric layer 117, and a channel layer 118. The memory stack structure 120P may include an ONOP structure. The ONOP structure may include a stack of an oxide layer, a nitride layer, an oxide layer, and a polysilicon layer. The blocking layer 115 and the tunnel dielectric layer 117 may include an oxide, the charge trapping layer 116 may include a nitride, and the channel layer 118 may include a polysilicon layer. According to an embodiment of the present disclosure, the blocking layer 115 may include a high dielectric material, and the high dielectric material may include aluminum oxide or hafnium oxide.
[0047] The channel layer 118 may be cylindrical with an inner space. The tunnel dielectric layer 117 may be formed on the outer wall of the channel layer 118, and the charge trapping layer 116 may be formed on the outer wall of the tunnel dielectric layer 117. The blocking layer 115 may be formed on the outer wall of the charge trapping layer 116.
[0048] The memory stack structure 120P may further include a core dielectric layer 119. The inner space of the channel layer 118 may be substantially completely filled with the core dielectric layer 119. The core dielectric layer 119 may include silicon oxide or silicon nitride. Although not shown, a conductive pad coupled to the upper end of the channel layer 118 may be further formed after the core dielectric layer 119 is recessed.
[0049] The stack of the blocking layer 115 , the charge trapping layer 116 , and the tunnel dielectric layer 117 may be referred to as a memory layer, and the charge trapping layer 116 may be referred to as a memory material layer.
[0050] Reference Figure 5 , a vertical contact recess 121 may be formed. The vertical contact recess 121 may be formed to be spaced apart from the memory stack structure 120P. The vertical contact recess 121 may be formed by etching the second multilayer stack 120M, and the vertical contact recess 121 may extend downward to a portion of the first multilayer stack 110S. The bottom of the vertical contact recess 121 may penetrate the upper source layer 106 and the second liner layer 105. The etching process for forming the vertical contact recess 121 may stop on the upper surface of the source sacrificial layer 104. According to another embodiment of the present disclosure, while forming the vertical contact recess 121, the top surface of the source sacrificial layer 104 may be partially recessed. The vertical contact recess 121 may be referred to as a slit or a groove. From the perspective of the top view, the vertical contact recess 121 may have a line shape extending in one direction. The vertical contact recess 121 may have a high aspect ratio perpendicular to the surface of the lower structure 101.
[0051] Reference Figure 6 , a sacrificial sealing layer 122 may be formed on the sidewall of the vertical contact recess 121. The sacrificial sealing layer 122 may be formed as a spacer on the sidewall of the vertical contact recess 121. The sacrificial sealing layer 122 may be formed by conformally forming a sacrificial sealing material layer and then performing a cutting process on the sacrificial sealing material layer.
[0052] The sacrificial sealing material layer used to form the sacrificial sealing layer 122 may include an oxide, a nitride, or a combination thereof. For example, the sacrificial sealing material layer used for the sacrificial sealing layer 122 may include a first sealing layer, a second sealing layer, and a third sealing layer. The first sealing layer and the third sealing layer may include the same material, and the second sealing layer may include a material different from the materials of the first sealing layer and the third sealing layer. The second sealing layer may have an etching selectivity relative to the first sealing layer and the third sealing layer. The first sealing layer and the third sealing layer may include an oxide, and the second sealing layer may include a nitride. Therefore, the sacrificial sealing layer 122 may include a NON structure. The NON structure may refer to a stack of nitrides, oxides, and nitrides. The sacrificial sealing material layer may cover the bottom surface and sidewalls of the vertical contact recess 121.
[0053] The sacrificial sealing material layer may be cut, and as a result, a sacrificial sealing layer 122 may be formed. The cutting process of the sacrificial sealing material layer may include an etching process, and a surface (e.g., a top surface) of the source sacrificial layer 104 may be exposed by the cutting process. After the cutting process, the sacrificial sealing material layer may remain on the sidewall of the vertical contact recess 121 as a spacer-type sacrificial sealing layer 122. The cutting process of the sacrificial sealing material layer may include an etch-back process.
[0054] Subsequently, the source sacrificial layer 104 may be selectively removed through the vertical contact recess 121. As a result, a horizontal contact recess 123 may be formed. The vertical contact recess 121 and the horizontal contact recess 123 may be connected to each other. The horizontal contact recess 123 may be formed between the first liner layer 103 and the second liner layer 105 by removing the source sacrificial layer 104 through a leaching process. The horizontal contact recess 123 may be parallel to the surface of the lower structure 101. When the source sacrificial layer 104 is removed, the first liner layer 103 and the second liner layer 105 may have an etching selectivity relative to the source sacrificial layer 104, and thus remain without being significantly etched. The horizontal contact recess 123 may be formed in the first multilayer stack 110S. When the source sacrificial layer 104 is removed, the lower source layer 102 and the upper source layer 106 may not be removed. A wet etching process may be applied to remove the source sacrificial layer 104. Since the source sacrificial layer 104 includes a polysilicon layer, the wet etching process may include chemicals capable of etching the polysilicon layer.
[0055] A portion of the horizontal contact recess 123 may expose the lower sidewall of the memory stack structure 120P. The outer wall of the memory stack structure 120P may be a barrier layer 115, and the barrier layer 115 of the memory stack structure 120P may be exposed through the horizontal contact recess 123. Since the barrier layer 115 includes an oxide, the barrier layer 115 of the memory stack structure 120P may have an etching selectivity relative to the source sacrificial layer 104, and will not be etched while the source sacrificial layer 104 is removed. From the perspective of the top view, the horizontal contact recess 123 may have a ring shape surrounding the lower sidewall of the memory stack structure 120P. The horizontal contact recess 123 may be referred to as a source horizontal air gap.
[0056] Subsequently, the first liner layer 103 and the second liner layer 105 may be removed. Figure 6 In the vertical direction, the height of the horizontal contact recess 123 may increase depending on the orientation of the horizontal contact recess 123. The horizontal contact recess 123 having the expanded height may directly contact the lower source layer 102 and the upper source layer 106.
[0057] The barrier layer 115 of the memory stack structure 120P may be removed while the first liner layer 103 and the second liner layer 105 are removed. Thus, the charge trapping layer 116 of the memory stack structure 120P may be exposed. A wet etching process may be applied to remove the first liner layer 103 and the second liner layer 105. The wet etching process may include chemicals that may selectively remove silicon oxide.
[0058] Subsequently, the charge trapping layer 116 of the memory stack structure 120P may be removed through the vertical contact recess 121 and the horizontal contact recess 123. The charge trapping layer 116 may be removed through a wet etching process. When the charge trapping layer 116 includes nitride, the wet etching process may include chemicals capable of etching nitride.
[0059] By removing the charge trapping layer 116 , the horizontal length of the horizontal contact recess 123 may be increased.
[0060] Subsequently, the tunnel dielectric layer 117 of the memory stack structure 120P may be removed through the vertical contact recess 121 and the horizontal contact recess 123. The tunnel dielectric layer 117 may be removed by a wet etching process. When the tunnel dielectric layer 117 includes oxide, the wet etching process may include chemicals capable of etching oxide.
[0061] By removing the tunnel dielectric layer 117 , the horizontal length of the horizontal contact recess 123 may be increased.
[0062] As described above, when the process of removing the source sacrificial layer 104, the process of removing the first liner layer 103 and the second liner layer 105, the process of removing the blocking layer 115, the process of removing the charge trapping layer 116, and the process of removing the tunnel dielectric layer 117 are performed, the sacrificial sealing layer 122 can be used as an etching barrier to protect the dielectric layers 111 and 113 and the sacrificial layer 112.
[0063] The lower outer wall of the channel layer 118 of the memory stack structure 120P may be exposed by the process of enlarging the horizontal contact recess 123. For example, the annular air gap may expose the lower outer wall of the channel layer 118. The annular air gap may refer to the portion where the blocking layer 115, the charge trapping layer 116, and the tunnel dielectric layer 117 are removed.
[0064] The first multi-layer stack formed with one or more horizontal contact recesses 123 may be denoted by 110S′.
[0065] pass Figures 2 to 6 The series of processes shown can form a contact opening that penetrates the first multilayer stack 110S' and the second multilayer stack 120M. The contact opening may include a vertical contact recess 121 and a horizontal contact recess 123. The horizontal contact recess 123 may extend from the vertical contact recess 121. The vertical contact recess 121 may extend in a direction (e.g., a vertical direction) perpendicular to the surface (e.g., a top surface) of the lower structure 101, and the horizontal contact recess 123 may extend in a direction (e.g., a horizontal direction) parallel to the surface of the lower structure 101. The horizontal contact recess 123 may have a high aspect ratio parallel to the surface of the lower structure 101. For example, the horizontal contact recess 123 may have a relatively high ratio of width in the horizontal direction to height in the vertical direction. The vertical contact recess 121 may have a high aspect ratio perpendicular to the lower structure 101. For example, the vertical contact recess 121 may have a relatively high ratio of height in the vertical direction to width in the horizontal direction.
[0066] Reference Figure 7 , a source contact material 124A may be formed to fill the contact openings (e.g., vertical contact recess 121 and horizontal contact recess 123). Source contact material 124A may include a conductive material. Source contact material 124A may include polysilicon. Source contact material 124A may include polysilicon doped with phosphorus (P). Source contact material 124A may include polysilicon containing carbon. Source contact material 124A may include a stack of phosphorus-doped polysilicon (SiP) and carbon-doped polysilicon (SiC).
[0067] Subsequently, the source contact material 124A may be selectively removed. The process of selectively removing the source contact material 124A may include a recess process, and the recess process may include a wet etching process. The source contact layer 124 may be formed in the horizontal contact recess 123 by performing a wet etching process on the source contact material 124A. The source contact layer 124 may fill the horizontal contact recess 123. For example, the sidewall of the sacrificial sealing layer 122 may be used to etch the source contact material 124A so that the source contact layer 124 is self-aligned with the sidewall of the sacrificial sealing layer 122. As a result, the bottom surface of the vertical contact recess 121 may directly contact the lower source layer 102. The source contact layer 124 may remain in the horizontal contact recess 123, and the source contact layer 124 may not remain in the vertical contact recess 121.
[0068] Although not shown, the source contact layer 124 may be subsequently exposed to an oxidation process. The oxidation process may include a dry oxidation process or a wet oxidation process. The edge of the source contact layer 124 may be oxidized by the oxidation process. As a result, a barrier oxide (not shown) may be formed at the edge of the source contact layer 124 (i.e., the portion exposed by the bottom of the vertical contact recess 121). The barrier oxide may include silicon oxide. The barrier oxide may protect the source contact layer 124 from being attacked during subsequent processes.
[0069] The first multilayer stack 110S' formed with the source contact layer 124 may be simply referred to as a source horizontal stack 110. The source horizontal stack 110 may be disposed below the second multilayer stack 120M, and the source contact layer 124 may be directly coupled to the channel layer 118 of the memory stack structure 120P.
[0070] As described above, the source horizontal stack 110 formed through a series of processes of replacing the source sacrificial layer 104 with the source contact layer 124 may have a structure in which the source contact layer 124 is embedded.
[0071] Reference Figures 8 to 10 , the sacrificial layer 112 may be replaced by the gate electrode 127 .
[0072] like Figure 8 As shown, the sacrificial layer 112 of the second multilayer stack 120M may be selectively removed. As a result, a horizontal gate recess 125 may be formed between the dielectric layers 111. Since the sacrificial layer 112 includes nitride, the sacrificial layer 112 may be removed by a chemical including phosphoric acid (H3PO4). While the sacrificial layer 112 is being removed, the sacrificial sealing layer 122 may also be removed at the same time. According to another embodiment of the present disclosure, the sacrificial sealing layer 122 may be removed after the sacrificial layer 112 is removed.
[0073] While the sacrificial layer 112 is removed, the source contact layer 124 can be fully protected by the barrier oxide. The barrier oxide can serve as a protective layer to protect the source contact layer 124 from attack.
[0074] The horizontal gate recess 125 may be continuous from the vertical contact recess 121 . A portion of the barrier layer 115 of the memory stack structure 120P may be exposed through the horizontal gate recess 125 .
[0075] exist Figure 7 After forming the horizontal gate recess 125 in the second multilayer stack 120M in the first embodiment, the first intermediate multilayer stack 120' may be formed. The first intermediate multilayer stack 120' may have a structure of alternating dielectric layers 111 and horizontal gate recesses 125. The horizontal gate recess 125 may also be formed between the top dielectric layer 113 and the adjacent dielectric layer 111.
[0076] Reference Fig. 9 and Fig.10 , the gate electrodes 127 may fill the horizontal gate recesses 125, respectively. The gate electrodes 127 may be formed by forming a gate material layer 126 to fill the horizontal gate recesses 125 (see Fig. 9 ). After forming the gate material layer 126 , a second intermediate multilayer stack 120 ″ may be formed. The second intermediate multilayer stack 120 ″ may have a structure in which dielectric layers 111 and gate material layers 126 are alternately formed. The gate material layer 126 may cover the sidewalls of the vertical contact recess 121 .
[0077] Then, if Fig.10 As shown, a gate electrode 127 may be formed by performing an etch-back process on the gate material layer 126. The gate electrode 127 may include a low resistance material. The gate electrode 127 may include a metal-based material. The gate electrode 127 may include a metal, a metal silicide, a metal nitride, or a combination thereof. For example, the metal may include nickel, cobalt, platinum, titanium, tantalum, or tungsten. The metal silicide may include nickel silicide, cobalt silicide, platinum silicide, titanium silicide, tantalum silicide, or tungsten silicide. The gate electrode 127 may include a stack of titanium nitride and tungsten.
[0078] An end portion 127R of the gate electrode 127 may have a shape horizontally recessed from an end portion of the dielectric layer 111. The end portion 127R of the gate electrode 127 may be exposed through the vertical contact recess 121. The gate electrode 127 may not contact the upper source layer 106, the lower source layer 102, and the source contact layer 124.
[0079] After forming the gate electrode 127, the alternating stack 120 may be formed. The alternating stack 120 may have a structure in which the dielectric layers 111 and the gate electrodes 127 are alternately stacked. The memory stack structure 120P may penetrate the alternating stack 120, and the vertical contact recess 121 may penetrate the alternating stack 120.
[0080] Reference Fig.11 , the surface of the vertical contact recess 121 may be sealed. The surface of the vertical contact recess 121 may be sealed by a sealing layer 128S. The sealing layer 128S may include one or more protrusions 128P, and the protrusion 128P may seal the end 127R of the gate electrode 127. The sealing layer 128S may seal the side surfaces of the dielectric layers 111 and 113. The sealing layer 128S may seal the side surface of the source contact layer 124. The sealing layer 128S may seal the side surface of the upper source layer 106, and may seal the exposed surface of the lower source layer 102. The sealing layer 128S may include a silicon oxide-based material. The sealing layer 128S may include a low dielectric material. The low dielectric material may have a dielectric constant lower than that of silicon nitride. The material of the sealing layer 128S may have a dielectric constant lower than about 7.
[0081] The sealing layer 128S may be thinner than the dielectric layers 111 and 113 and the gate electrode 127. The sealing layer 128S may be a layer of a different material from the dielectric layers 111 and 113. The sealing layer 128S may be a layer of a different material from the gate electrode 127. The sealing layer 128S may include a material having high wet etching resistance. The wet etching resistance of the sealing layer 128S may be obtained by carbon. The sealing layer 128S may be formed of a carbon-containing material, and the dielectric layers 111 and 113 may be formed of a carbon-free material. The dielectric layers 111 and 113 may be formed of carbon-free silicon oxide, and the sealing layer 128S may be formed of carbon-containing silicon oxide. For example, the dielectric layers 111 and 113 may be formed of SiO2, and the sealing layer 128S may be formed of SiCO. SiCO may be more etch-resistant than SiO2. The carbon content in SiCO may be less than the silicon content and the oxygen content. For example, SiCO may have a composition ratio of 34 at% silicon (Si), 40 at% oxygen, and 17 at% carbon. SiCO may have a lower dielectric constant than silicon nitride (Si3N4).
[0082] The sealing layer 128S may be formed to be approximately to The high wet etching resistance of SiCO can reduce the thickness of the sealing layer 128S. As a result, the size of the vertical contact recess 121 for separating the unit blocks can be reduced, which can reduce the chip size. In the comparative example, when the sealing layer is formed of SiO2, the sealing layer should be formed to have a thickness of about 1000 nm in consideration of the loss in the subsequent process (e.g., the cleaning process). or greater, and thick SiO2 may prevent the vertical contact recess from being filled with a source contact plug without a gap. In order to improve the gap filling characteristics of the source contact plug, the vertical contact recess in the comparative example should be formed to have a relatively large size. On the contrary, since SiCO of the sealing layer 128S in the embodiment of the present disclosure has greater wet etching resistance than SiO2, the sealing layer 128S of SiCO can be formed to be thinner than the sealing layer of SiO2 in the comparative example. Therefore, even if the size of the vertical contact recess 121 is small, the source contact plug can fill the vertical contact recess 121 without a gap.
[0083] According to another embodiment of the present disclosure, the sealing layer 128S may include a material having wet etching resistance to subsequent processes. The sealing layer 128S may include SiCN, SiBCN, SiBN, or a combination thereof. The wet etching resistance of the sealing layer 128S may be derived from carbon, nitrogen, boron, or a combination thereof.
[0084] According to another embodiment of the present disclosure, a seed layer may be formed before forming the sealing layer 128S. The seed layer may form a thin silicon oxide or silicon nitride. By forming the seed layer, the conformability of the sealing layer 128S may be improved.
[0085] According to another embodiment of the present disclosure, the sealing layer 128S may include a stack of one or more carbon-free silicon oxide layers and one or more carbon-containing silicon oxide layers. For example, after thinly depositing the carbon-free silicon oxide layer, the carbon-containing silicon oxide layer may be deposited over the carbon-free silicon oxide layer. The carbon-free silicon oxide may improve the conformability of the carbon-containing silicon oxide as a seed layer.
[0086] Although not shown, the sealing layer 128S may seal the upper surface of the top dielectric layer 113 .
[0087] Reference Fig.12 , the sealing layer 128S may be selectively removed to expose the surface of the lower source layer 102. As a result, a sealing spacer 128 may be formed on the sidewalls of the vertical contact recess 121. The bottom of the sealing spacer 128 may substantially completely cover the side of the source contact layer 124 and the side of the upper source layer 106. The sealing spacer 128 may include one or more protrusions 128P, and the protrusion 128P may seal the end 127R of the gate electrode 127. The sealing spacer 128 may seal the side of the dielectric layers 111 and 113.
[0088] The sealing spacer 128 may be vertically continuous along a stacking direction of the dielectric layers 111 and 113 and the gate electrode 127. From a top view perspective, the sealing spacer 128 may be a closed loop shape that seals a sidewall of the vertical contact recess 121.
[0089] Since the thickness of the sealing layer 128S is thin, an open area of the bottom surface of the vertical contact recess 121 may be increased in an etching process for forming the sealing spacer 128. As a result, low resistance and process stability may be ensured.
[0090] After forming the sealing spacer 128 , a post-cleaning process may be performed.
[0091] Reference Fig.13 and Fig.14 , the vertical contact recess 121 may be filled with a contact material. For example, a source contact plug 132 may be formed in the vertical contact recess 121. The source contact plug 132 may fill the vertical contact recess 121. The source contact plug 132 may include a stack of a silicon-containing material 129 and a metal-containing material 131, and may further include a barrier material 130 between the silicon-containing material 129 and the metal-containing material 131. The silicon-containing material 129 may include polysilicon, and the metal-containing material 131 may include tungsten. The barrier material 130 may include titanium nitride. According to another embodiment of the present disclosure, the source contact plug 132 may be formed of only tungsten.
[0092] The silicon-containing material 129 may be formed by depositing polysilicon to fill the vertical contact recess 121 and performing an etch-back process on the polysilicon. A pre-cleaning process may be performed before depositing the polysilicon, and a post-cleaning process may be performed after the etch-back process of the polysilicon. The silicon-containing material 129 may contact the sealing spacer 128.
[0093] After forming the silicon-containing material 129, the barrier material 130 may be conformally deposited. A pre-cleaning process may be performed before depositing the barrier material 130. After conformally depositing the barrier material 130, the remaining portion of the vertical contact recess 121 may be filled with the metal-containing material 131. After sequentially depositing the barrier material 130 and the metal-containing material 131, a planarization process using chemical mechanical polishing (CMP) may be performed. As a result, the barrier material 130 and the metal-containing material 131 may remain only in the vertical contact recess 121. The barrier material 130 may be in direct contact with the sealing spacer 128, and the metal-containing material 131 may not contact the sealing spacer 128.
[0094] Although a plurality of cleaning processes are performed during the process of forming the sealing spacer 128 , the process of forming the silicon-containing material 129 , and the process of depositing the barrier material 130 , a thickness loss of the sealing spacer 128 hardly occurs.
[0095] As described above, the source horizontal stack 110 and the alternating stack 120 may be formed above the lower structure 101. The source horizontal stack 110 may include a lower source layer 102, a source contact layer 124, and an upper source layer 106. The alternating stack 120 may be formed by alternately stacking dielectric layers 111 and gate electrodes 127. The memory stack structure 120P may penetrate the alternating stack 120 and the source horizontal stack 110. The lower outer wall of the channel layer 118 of the memory stack structure 120P may directly contact the source contact layer 124. The channel layer 118, the lower source layer 102, the upper source layer 106, and the source contact plug 132 may be electrically connected through the source contact layer 124.
[0096] The gate electrode 127 and the source contact plug 132 may be electrically disconnected from each other by the sealing spacer 128. The gate electrode 127 and the source contact plug 132 may be physically disconnected by the sealing spacer 128. A high voltage may be repeatedly applied between the gate electrode 127 and the source contact plug 132, thereby increasing the growth bad block (GBB). GBB is a phenomenon in which the number of bad blocks may increase as the number of operations increases. According to an embodiment of the present disclosure, the sealing spacer 128 may include a carbon-containing material to prevent GBB defects. In other words, since the sealing spacer 128 is formed of a material having high wet etching resistance, the thickness loss of the sealing spacer 128 does not substantially occur during the subsequent cleaning process, and thus it is ensured that the sealing spacer 128 has a thickness thick enough to withstand the high voltage applied between the gate electrode 127 and the source contact plug 132.
[0097] In addition, since the sealing spacer 128 is formed of a low dielectric material according to an embodiment of the present disclosure, a parasitic capacitance between the gate electrode 127 and the source contact plug 132 may be relatively small.
[0098] Reference Figures 2 to 14A method for manufacturing a vertical semiconductor device may include the following steps: forming a first multi-layer stack 110S including a source sacrificial layer 104 above a lower structure 101; forming a second multi-layer stack 120M in which dielectric layers 111 and sacrificial layers 112 are alternately stacked above the first multi-layer stack 110S; forming a memory stack structure 120P, the memory stack structure 120P including a channel layer 118 extending through the second multi-layer stack 120M and the first multi-layer stack 110S; forming a vertical contact recess 121 to be spaced apart from the memory stack structure 120P and extending through The second multilayer stack 120M and the first multilayer stack 110S; forming a horizontal contact recess 123 by selectively removing the source sacrificial layer 104 through the vertical contact recess 121; expanding the horizontal contact recess 123 to expose the lower outer wall of the channel layer 118; filling the expanded horizontal contact recess 123 with a source contact layer 124; replacing the sacrificial layer 112 with a gate electrode 127; forming a sealing spacer 128 that seals the sidewall of the vertical contact recess 121 over the source contact layer 124 and the gate electrode 127; and forming a source contact plug 132 in the vertical contact recess 121. The sealing spacer 128 may be formed of carbon-containing silicon oxide.
[0099] Fig.15 is a cross-sectional view illustrating a vertical semiconductor device 200 according to another embodiment of the present disclosure.
[0100] Reference Fig.15 , the vertical semiconductor device 200 may be positioned above the lower structure 101, and the vertical semiconductor device 200 may include: an alternating stack 120 in which gate electrodes 127 and dielectric layers 111 are alternately stacked; a memory stack structure 120P, which includes a channel layer 118 extending to penetrate the alternating stack 120 and a stack of layers (or memory layers) 115, 116 and 117 surrounding the channel layer 118; a source contact layer 124, which is disposed between the lower structure 101 and the alternating stack 120 to contact a lower outer wall of the channel layer 118; and a source contact plug 132, which extends through the alternating stack 120 to be spaced apart from the memory stack structure 120P; and a sealing spacer 128, which has an etching resistance different from that of the dielectric layer 111 while sealing the outer wall of the source contact plug. The sealing spacer 128 may seal the gate electrode 127 and be disposed between the source contact plug 132 and the gate electrode 127, and may have a different etching resistance than the dielectric layer 111. The outer wall of the source contact plug 132 may be surrounded by the sealing spacer 128, which may extend vertically to cover the gate electrode 127, the dielectric layer 111, the carbon-containing liner layer 105', and the source contact layer 124.
[0101] The lower structure 101 may include a material suitable for semiconductor processing. The lower structure 101 may include a substrate, and the substrate may include a semiconductor substrate. For example, the lower structure 101 may include a silicon substrate, a single crystal silicon substrate, a polycrystalline silicon substrate, an amorphous silicon substrate, a silicon germanium substrate, a single crystal silicon germanium substrate, a polycrystalline silicon germanium substrate, a carbon-doped silicon substrate, a combination thereof, or a multilayer thereof. The lower structure 101 may include other semiconductor materials, such as germanium. The lower structure 101 may include a III / V semiconductor substrate such as a compound semiconductor substrate, such as GaAs. The lower structure 101 may include a silicon on insulator (SOI) substrate. Although not shown, according to another embodiment of the present disclosure, the lower structure 101 may include a substrate, at least one or more control circuits formed above the substrate, and a multilayer metal line.
[0102] The multi-layer stack structure may be disposed over the lower structure 101 and include a source horizontal stack 110 and an alternating stack 120 over the source horizontal stack 110. The source horizontal stack 110 may have a lower height than the alternating stack 120.
[0103] The source horizontal stack 110 may include a lower source layer 102, a source contact layer 124, and a carbon-containing liner layer 105'. The source contact layer 124 may be formed above the lower source layer 102, and the carbon-containing liner layer 105' may be formed above the source contact layer 124. The source contact layer 124 may be disposed between the lower source layer 102 and the carbon-containing liner layer 105'. The lower source layer 102 and the source contact layer 124 may include a semiconductor material. The lower source layer 102 and the source contact layer 124 may include polysilicon. The source contact layer 124 may include polysilicon doped with phosphorus (P). The source contact layer 124 may include carbon-containing polysilicon. The source contact layer 124 may include a stack of phosphorus-doped polysilicon (SiP) and carbon-doped polysilicon (SiC). The lower source layer 102 may include undoped polysilicon or doped polysilicon.
[0104] The carbon-containing liner layer 105' may include a silicon oxide-based material. The carbon-containing liner layer 105' may include at least SiCO.
[0105] The carbon-containing liner layer 105' may be a layer of a different material from the dielectric layers 111 and 113. The carbon-containing liner layer 105' may include a material having high wet etching resistance. The wet etching resistance of the carbon-containing liner layer 105' may be derived from carbon. The carbon-containing liner layer 105' may be a carbon-containing material, and the dielectric layers 111 and 113 may be carbon-free materials. The dielectric layers 111 and 113 may be carbon-free silicon oxide, and the carbon-containing liner layer 105' may be carbon-containing silicon oxide. For example, the dielectric layers 111 and 113 may be SiO2, and the carbon-containing liner layer 105' may be SiCO. SiCO may be more etch-resistant than SiO2. The carbon content in SiCO may be less than the silicon content and the oxygen content. For example, SiCO may have a composition ratio of 34at% silicon (Si), 40at% oxygen, and 17at% carbon.
[0106] The carbon-containing liner layer 105' may be formed to be approximately to For example, the carbon-containing liner layer 105' may be relative to Fig.15 The orientation in the vertical direction has to The high wet etching resistance of SiCO can reduce the thickness of the carbon-containing liner layer 105'. As a result, the height of the source horizontal stack 110 can be reduced. The thickness of the bottom dielectric layer 111 among the dielectric layers 111 can be thinner than the individual dielectric layers 111 at a higher level of the bottom dielectric layer 111. For example, when the carbon-containing liner layer 105' is formed of SiCO, the thickness of the bottom dielectric layer 111 can be relatively thin (e.g., about 1000 Å). As a result, the dopant diffusion movement distance from the source contact layer 124 to the channel layer 118 adjacent to the bottom gate electrode 127 can be shortened. The dielectric layer 111 at a higher level than the bottom dielectric layer 111 can be approximately thick.
[0107] According to another embodiment of the present disclosure, the carbon-containing liner layer 105 ′ may be replaced with a material containing nitrogen, boron, or a combination thereof, in addition to carbon.
[0108] The alternating stack 120 may be referred to as a memory cell stack or a memory cell string. The alternating stack 120 may have a structure in which a plurality of dielectric layers 111 and a plurality of gate electrodes 127 are alternately stacked. The uppermost dielectric layer 113 among the dielectric layers 111 may be thicker than the other dielectric layers 111. The dielectric layer 111 may include silicon oxide. The gate electrode 127 may include a low resistance material. The gate electrode 127 may include a metal-based material. The gate electrode 127 may include a metal, a metal silicide, a metal nitride, or a combination thereof. For example, the metal may include nickel, cobalt, platinum, titanium, tantalum, or tungsten. The metal silicide may include nickel silicide, cobalt silicide, platinum silicide, titanium silicide, tantalum silicide, or tungsten silicide. The gate electrode 127 may include a stack of titanium nitride and tungsten. The end portion (e.g., Fig.24The end portion 127R) in the dielectric layer 111 may have a shape horizontally recessed from the end portion of the dielectric layer 111.
[0109] The memory stack structure 120P may extend vertically to penetrate the alternating stack 120. The memory stack structure 120P may have a columnar shape. The memory stack structure 120P may include a blocking layer 115, a charge trapping layer 116, a tunnel dielectric layer 117, a channel layer 118, and a core dielectric layer 119. The memory stack structure 120P may include an ONOP structure. The ONOP structure may include a stack of an oxide layer, a nitride layer, an oxide layer, and a polysilicon layer. The blocking layer 115 and the tunnel dielectric layer 117 may include an oxide, the charge trapping layer 116 may include a nitride, and the channel layer 118 may include polysilicon. According to an embodiment of the present disclosure, the blocking layer 115 may include a high dielectric material, and the high dielectric material may include aluminum oxide or hafnium oxide. The channel layer 118 may be a cylindrical shape with an internal space. The tunnel dielectric layer 117 may be formed on the outer wall of the channel layer 118, and the charge trapping layer 116 may be formed on the outer wall of the tunnel dielectric layer 117. The barrier layer 115 may be formed on the outer wall of the charge trapping layer 116. The inner space of the channel layer 118 may be substantially completely filled with the core dielectric layer 119. The core dielectric layer 119 may include silicon oxide or silicon nitride. The stack of the barrier layer 115, the charge trapping layer 116, and the tunnel dielectric layer 117 may be referred to as a memory layer 115 / 116 / 117.
[0110] The source contact plug 132 may include a stack of a silicon-containing material 129 and a metal-containing material 131, and it may also include a barrier material 130 between the silicon-containing material 129 and the metal-containing material 131. The silicon-containing material 129 may include polysilicon, and the metal-containing material 131 may include tungsten. The barrier material 130 may include titanium nitride. According to another embodiment of the present disclosure, the source contact plug 132 may be formed of only tungsten. The lower portion of the source contact plug 132 may be coupled to the lower source layer 102 of the source horizontal stack 110.
[0111] The sealing spacer 128 may be formed between the source contact plug 132 and the gate electrode 127. The sealing spacer 128 may extend to be formed between the dielectric layers 111 and 113 and the source contact plug 132. The sealing spacer 128 may be continuous along the stacking direction of the alternating stack 120. The sealing spacer 128 may include one or more protrusions 128P, and the protrusions 128P may be respectively coupled to the ends of the gate electrode 127. The protrusions 128P of the sealing spacer 128 may seal the ends of the gate electrode 127. The sealing spacer 128 may seal the sides of the dielectric layers 111 and 113. The sealing spacer 128 may seal the sides of the source contact layer 124. The sealing spacer 128 may seal the sides of the carbon-containing liner layer 105', and may not seal a portion of the surface of the lower source layer 102. The sealing spacer 128 may substantially completely surround the outer wall of the source contact plug 132.
[0112] The sealing spacer 128 may include a silicon oxide-based material. The sealing spacer 128 may include a low dielectric material. The low dielectric material may have a dielectric constant lower than that of silicon nitride. The sealing spacer 128 may have a dielectric constant lower than about 7. The sealing spacer 128 may be thinner than the dielectric layers 111 and 113 and the gate electrode 127. The sealing spacer 128 may be a layer of a different material from the dielectric layers 111 and 113. The sealing spacer 128 may be a layer of a different material from the gate electrode 127. The carbon-containing liner layer 105' and the sealing spacer 128 may include the same material. The sealing spacer 128 may include a material having high wet etching resistance. The wet etching resistance of the sealing spacer 128 may be derived from carbon. The sealing spacer 128 may include a carbon-containing material, and the dielectric layers 111 and 113 may include a carbon-free material. The dielectric layers 111 and 113 may be formed of carbon-free silicon oxide, and the sealing spacer 128 may be formed of carbon-containing silicon oxide. For example, dielectric layers 111 and 113 may be formed of SiO2, and sealing spacer 128 may be formed of SiCO. SiCO may be more etch-resistant than SiO2. The carbon content of SiCO may be less than the silicon content and oxygen content of SiCO. For example, SiCO may have a composition ratio of 34 at% silicon (Si), 40 at% oxygen, and 17 at% carbon. SiCO may have a lower dielectric constant than silicon nitride (Si3N4).
[0113] The sealing spacer 128 may be formed to have a size of approximately to The high wet etching resistance of SiCO can reduce the thickness of the sealing spacer 128. As a result, the size of the source contact plug 132 for separating the unit block can be reduced, and thus, the chip size can be reduced. The sealing spacer 128 can be thinner than the carbon-containing liner layer 105'.
[0114] According to another embodiment of the present disclosure, the sealing spacer 128 may include SiCN, SiBCN, SiBN, or a combination thereof. The wet etching resistance of the sealing spacer 128 may be derived from carbon, nitrogen, boron, or a combination thereof.
[0115] According to another embodiment of the present disclosure, the sealing spacer 128 may include a stack of one or more carbon-free silicon oxide layers and one or more carbon-containing silicon oxide layers. For example, after thinly depositing the carbon-free silicon oxide layer, the carbon-containing silicon oxide layer may be deposited over the carbon-free silicon oxide layer.
[0116] Fig.16 , Fig.17 , Fig.18 , Fig.19 , Fig. 20 , Fig.21 , Fig. 22 , Fig.23 , Fig.24 , Fig.25 , Fig.26 , Fig. 27 and Fig.28 is a cross-sectional view showing a method for manufacturing a vertical semiconductor device according to another embodiment of the present disclosure. For example, Figures 16 to 28 Show Figure 5 A method for manufacturing a vertical semiconductor device 200 is provided.
[0117] Reference Fig.16 , a first multi-layer stack 110S may be formed over the lower structure 101. The first multi-layer stack 110S may have a stacked structure including a lower source layer 102, a first liner layer 103, a source sacrificial layer 104, and a second liner layer 105'. Fig.16 In the first multilayer stack 110S of the illustrated embodiment, the first liner layer 103 may be formed between the lower source layer 102 and the source sacrificial layer 104, and the second liner layer 105' may be formed above the source sacrificial layer 104. The lower source layer 102 and the source sacrificial layer 104 may include the same material, and the first liner layer 103 and the second liner layer 105' may include a material different from that of the lower source layer 102 and the source sacrificial layer 104. The first liner layer 103 and the second liner layer 105' may have an etching selectivity relative to the source sacrificial layer 104. The lower source layer 102 and the source sacrificial layer 104 may include a semiconductor material, and the first liner layer 103 and the second liner layer 105' may include a dielectric material. The lower source layer 102 and the source sacrificial layer 104 may include polysilicon, and the first liner layer 103 and the second liner layer 105' may include silicon oxide. The source sacrificial layer 104 may have the same thickness as or thinner than the lower source layer 102 and the second liner layer 105 ′. The second liner layer 105 ′ may be thicker than the first liner layer 103 .
[0118] While the source sacrificial layer 104 is removed, the first liner layer 103 and the second liner layer 105 ′ may protect the lower source layer 102 .
[0119] The first liner layer 103 and the second liner layer 105' may include a silicon oxide-based material. One or both of the first liner layer 103 and the second liner layer 105' may include SiO2, SiCO, or a combination thereof.
[0120] The second pad layer 105' may be a layer of a material different from that of the first pad layer 103. The second pad layer 105' may include a material having high wet etching resistance. The wet etching resistance of the second pad layer 105' may be derived from carbon. The second pad layer 105' may include a carbon-containing material, and the first pad layer 103 may include a carbon-free material. The first pad layer 103 may be formed of carbon-free silicon oxide, and the second pad layer 105' may be formed of carbon-containing silicon oxide. For example, the first pad layer 103 may be formed of SiO2, and the second pad layer 105' may be formed of SiCO. SiCO may be more etch-resistant than SiO2. The carbon content of SiCO may be less than the silicon content and oxygen content of SiCO. For example, SiCO may have a composition ratio of 34at% silicon (Si), 40at% oxygen, and 17at% carbon.
[0121] The first liner layer 103 and the second liner layer 105' may be formed to have approximately to The high wet etching resistance of SiCO can reduce the thickness of the second liner layer 105'. As a result, the height of the first multi-layer stack 110S can be reduced.
[0122] According to another embodiment of the present disclosure, the second liner layer 105 ′ may further include nitrogen, boron, or a combination thereof in addition to carbon.
[0123] As described above, the first liner layer 103 may be formed of SiO2, and the second liner layer 105' may be formed of SiCO. Figure 2 Different, in Fig.16 In the embodiment of the present invention, the upper source layer 106 may be omitted, and only the second liner layer 105 ′ may be formed. The thickness of the second liner layer 105 ′ is smaller than that of the upper source layer 106 .
[0124] Subsequently, a second multilayer stack 120M may be formed over the first multilayer stack 110S. The second multilayer stack 120M may be thicker than the first multilayer stack 110S. The second multilayer stack 120M may include a dielectric layer 111 and a sacrificial layer 112. The second multilayer stack 120M may include an alternating stack of dielectric layers 111 and sacrificial layers 112. The dielectric layers 111 and sacrificial layers 112 may be alternately stacked multiple times. The dielectric layers 111 and sacrificial layers 112 may include different materials. The dielectric layer 111 may have an etching selectivity relative to the sacrificial layer 112. The dielectric layer 111 may include silicon oxide, and the sacrificial layer 112 may include silicon nitride. The dielectric layer 111 and the sacrificial layer 112 may have substantially the same thickness.
[0125] The dielectric layer 111 and the sacrificial layer 112 may be formed by chemical vapor deposition (CVD) or atomic layer deposition (ALD). The uppermost dielectric layer (or top dielectric layer) 113 formed on top of the second multilayer stack 120M may be attacked and damaged by subsequent processes. Therefore, the top dielectric layer 113 may be formed to be thicker than the dielectric layer 111 disposed below the top dielectric layer 113. The top dielectric layer 113 may serve as an etching barrier. The lowermost dielectric layer (or bottom dielectric layer) 111 in contact with the second liner layer 105' among the dielectric layers 111 may be thinner than the other dielectric layers 111 above the bottom dielectric layer 111. For example, when the second liner layer 105' is formed of SiCO, the thickness of the lowermost dielectric layer 111 may be formed to be thinner (e.g., about 1000 Å). ). The other dielectric layer 111 above the bottom dielectric layer 111 may have a thickness of approximately Thickness.
[0126] Reference Fig.17 , a vertical opening 114 may be formed. The vertical opening 114 may be formed by sequentially etching the second multi-layer stack 120M and partially etching the first multi-layer stack 110S.
[0127] The vertical opening 114 may be formed substantially perpendicular to the surface (e.g., top surface) of the lower structure 101. The vertical opening 114 may be formed to penetrate the second multilayer stack 120M, or it may be formed to partially penetrate the first multilayer stack 110S. Although not shown, from the perspective of the plan view, the vertical opening 114 may be formed in multiples and may have a hole array structure. When the vertical opening 114 is formed, the surface of the lower structure 101 may not be exposed. For example, a portion of the lower source layer 102 may remain below the bottom of the vertical opening 114. The vertical opening 114 may be referred to as a vertical depression, a vertical hole, or a channel hole.
[0128] Reference Fig.18 , a memory stack structure 120P may be formed in the vertical opening 114. The memory stack structure 120P may have a pillar shape filling the vertical opening 114.
[0129] The memory stack structure 120P may include a blocking layer 115, a charge trapping layer 116, a tunnel dielectric layer 117, and a channel layer 118. The memory stack structure 120P may include an ONOP structure. The ONOP structure may include a stack of an oxide layer, a nitride layer, an oxide layer, and a polysilicon layer. The blocking layer 115 and the tunnel dielectric layer 117 may include an oxide, the charge trapping layer 116 may include a nitride, and the channel layer 118 may include a polysilicon layer. According to an embodiment of the present disclosure, the blocking layer 115 may include a high dielectric material, and the high dielectric material may include aluminum oxide or hafnium oxide.
[0130] The channel layer 118 may have a cylindrical shape including an inner space. The tunnel dielectric layer 117 may be formed on an outer wall of the channel layer 118, and the charge trapping layer 116 may be formed on an outer wall of the tunnel dielectric layer 117. The blocking layer 115 may be formed on an outer wall of the charge trapping layer 116.
[0131] The memory stack structure 120P may further include a core dielectric layer 119. The inner space of the channel layer 118 may be substantially completely filled with the core dielectric layer 119. The core dielectric layer 119 may include silicon oxide or silicon nitride. Although not shown, a conductive pad coupled to the upper end of the channel layer 118 may be further formed after the core dielectric layer 119 is recessed.
[0132] The stack of the blocking layer 115 , the charge trapping layer 116 , and the tunnel dielectric layer 117 may be referred to as a memory layer, and the charge trapping layer 116 may be referred to as a memory material layer.
[0133] Reference Fig.19 , a vertical contact recess 121 may be formed. The vertical contact recess 121 may be formed to be spaced apart from the memory stack structure 120P. The vertical contact recess 121 may be formed by etching the second multilayer stack 120M, and the vertical contact recess 121 may extend downward to a portion of the first multilayer stack 110S. The bottom of the vertical contact recess 121 may penetrate the second liner layer 105'. The etching process for forming the vertical contact recess 121 may stop at the source sacrificial layer 104. According to another embodiment of the present disclosure, during the formation of the vertical contact recess 121, the top surface of the source sacrificial layer 104 may be partially recessed. The vertical contact recess 121 may be referred to as a slit or a groove. From the perspective of the top view, the vertical contact recess 121 may have a line shape extending in one direction. The vertical contact recess 121 may have a high aspect ratio perpendicular to the surface of the lower structure 101.
[0134] Reference Fig. 20, a sacrificial sealing layer 122 may be formed on the sidewall of the vertical contact recess 121. The sacrificial sealing layer 122 may be formed as a spacer on the sidewall of the vertical contact recess 121. The sacrificial sealing layer 122 may be formed by conformally forming a sacrificial sealing material layer and then performing a cutting process on the sacrificial sealing material layer.
[0135] The sacrificial sealing material layer used to form the sacrificial sealing layer 122 may include an oxide, a nitride, or a combination thereof. For example, a sacrificial sealing material layer including a combination of oxides and nitrides may include a first sealing layer, a second sealing layer, and a third sealing layer. The first sealing layer and the third sealing layer may include the same material, and the second sealing layer may include a material different from the materials of the first sealing layer and the third sealing layer. The second sealing layer may have an etching selectivity relative to the first sealing layer and the third sealing layer. The first sealing layer and the third sealing layer may include an oxide, and the second sealing layer may include a nitride. Therefore, the sacrificial sealing layer 122 may include a NON structure. The NON structure may refer to a stack of nitrides, oxides, and nitrides. The sacrificial sealing material layer may cover the bottom and sidewalls of the vertical contact recess 121.
[0136] The sacrificial sealing material layer may be subjected to a cutting process, and as a result, a sacrificial sealing layer 122 may be formed. The cutting process of the sacrificial sealing material layer may include an etching process, and a surface (e.g., a top surface) of the source sacrificial layer 104 may be exposed due to the cutting process. After the cutting process, the sacrificial sealing material layer may remain on the sidewall of the vertical contact recess 121 as a spacer-type sacrificial sealing layer 122. The cutting process of the sacrificial sealing material layer may include an etch-back process.
[0137] Subsequently, the source sacrificial layer 104 may be selectively removed through the vertical contact recess 121. As a result, a horizontal contact recess 123 may be formed. The vertical contact recess 121 and the horizontal contact recess 123 may be connected to each other. The horizontal contact recess 123 may be formed between the second pad layer 105' and the first pad layer 103 by removing the source sacrificial layer 104 through a leaching process. The horizontal contact recess 123 may be parallel to the surface of the lower structure 101. When the source sacrificial layer 104 is removed, the first pad layer 103 and the second pad layer 105' may be retained due to their etching selectivity and not removed. The horizontal contact recess 123 may be formed in the first multilayer stack 110S. When the source sacrificial layer 104 is removed, the lower source layer 102 may not be removed. A wet etching process may be applied to remove the source sacrificial layer 104. Since the source sacrificial layer 104 includes a polysilicon layer, the wet etching process may include chemicals capable of etching the polysilicon layer.
[0138] A portion of the horizontal contact recess 123 may expose the lower sidewall of the memory stack structure 120P. The outer wall of the memory stack structure 120P may be the barrier layer 115, and the barrier layer 115 of the memory stack structure 120P may be exposed through the horizontal contact recess 123. Since the barrier layer 115 includes an oxide, the barrier layer 115 of the memory stack structure 120P may have an etching selectivity relative to the source sacrificial layer 104, and thus will not be etched while the source sacrificial layer 104 is removed. From the perspective of the top view, the horizontal contact recess 123 may be shaped as an outer wall surrounding the bottom of the memory stack structure 120P.
[0139] Subsequently, the first liner layer 103 may be removed. Fig. 20 In the vertical direction, the height of the horizontal contact recess 123 may be increased. The enlarged horizontal contact recess 123 may directly contact the lower source layer 102 and the second liner layer 105'.
[0140] While the first liner layer 103 is removed, the barrier layer 115 at the bottom of the memory stack structure 120P may be removed. Therefore, the charge trapping layer 116 of the memory stack structure 120P may be exposed. A wet etching process may be applied to remove the first liner layer 103. The wet etching process may include chemicals that can selectively remove silicon oxide. While the first liner layer 103 is removed, the second liner layer 105' may not be removed because it has wet etching resistance.
[0141] Subsequently, the charge trapping layer 116 in the bottom of the memory stack structure 120P may be removed through the vertical contact recess 121 and the horizontal contact recess 123. The charge trapping layer 116 may be removed through a wet etching process. When the charge trapping layer 116 includes nitride, the wet etching process may include chemicals capable of etching nitride.
[0142] By removing the charge trapping layer 116 , the horizontal length of the horizontal contact recess 123 may be increased.
[0143] Subsequently, the tunnel dielectric layer 117 in the bottom of the memory stack structure 120P may be removed through the vertical contact recess 121 and the horizontal contact recess 123. The tunnel dielectric layer 117 may be removed by a wet etching process. When the tunnel dielectric layer 117 includes oxide, the wet etching process may include chemicals capable of etching oxide.
[0144] By removing the tunnel dielectric layer 117 , the horizontal length of the horizontal contact recess 123 may be increased.
[0145] While performing the processes of removing the source sacrificial layer 104, removing the first liner layer 103, removing the blocking layer 115, removing the charge trapping layer 116, and removing the tunnel dielectric layer 117 as described above, the sacrificial sealing layer 122 can be used as an etching barrier to protect the dielectric layers 111 and 113 and the sacrificial layer 112.
[0146] An outer wall of the bottom of the channel layer 118 of the memory stack structure 120P may be exposed through a process of enlarging the horizontal contact recess 123 .
[0147] The first multi-layer stack formed with one or more horizontal contact recesses 123 may be denoted by 110S'. The remaining second liner layer 105' may be referred to as a carbon-containing liner layer.
[0148] pass Figures 16 to 20 The series of processes shown may form a contact opening penetrating the first multilayer stack 110S' and the second multilayer stack 120M. The contact opening may include a vertical contact recess 121 and a horizontal contact recess 123. The horizontal contact recess 123 may extend from the vertical contact recess 121. The vertical contact recess 121 may extend in a direction (e.g., a vertical direction) perpendicular to a surface (e.g., a top surface) of the lower structure 101, and the horizontal contact recess 123 may extend in a direction (e.g., a horizontal direction) parallel to the surface of the lower structure 101. The horizontal contact recess 123 may have a high aspect ratio parallel to the surface of the lower structure 101. The vertical contact recess 121 may have a high aspect ratio perpendicular to the lower structure 101.
[0149] Afterwards, you can Fig. 20 The resulting structure shown above is executed with Figures 7 to 14 The following will refer to Figures 21 to 28 Give a description.
[0150] Reference Fig.21 , a source contact material 124A may be formed to fill the contact openings (e.g., vertical contact recess 121 and horizontal contact recess 123). The source contact material 124A may include a conductive material. The source contact material 124A may include polysilicon. The source contact material 124A may include phosphorus (P) doped polysilicon. The source contact material 124A may include carbon-containing polysilicon. The source contact material 124A may include a stack of phosphorus doped polysilicon (SiP) and carbon doped polysilicon (SiC).
[0151] Subsequently, the source contact material 124A may be selectively removed. The selective removal of the source contact material 124A may include a recess process, and the recess process may include a wet etching process. As a result of performing the wet etching process on the source contact material 124A, a source contact layer 124 may be formed in the horizontal contact recess 123. The source contact layer 124 may partially fill the horizontal contact recess 123. For example, the source contact material 124A may be etched so that the source contact layer 124 is self-aligned with the sidewall of the sacrificial sealing layer 122, and therefore, the bottom of the vertical contact recess 121 may directly contact the lower source layer 102. The source contact layer 124 may remain in the horizontal contact recess 123, and the source contact layer 124 may not remain in the vertical contact recess 121.
[0152] Although not shown, the source contact layer 124 may be subsequently exposed to an oxidation process. The oxidation process may include dry oxidation or wet oxidation. The edge of the source contact layer 124 may be oxidized by the oxidation process. As a result, a barrier oxide (not shown) may be formed at the edge of the source contact layer 124. The barrier oxide may include silicon oxide. The barrier oxide may protect the source contact layer 124 from being attacked during subsequent processes.
[0153] The first multilayer stack 110S' formed with the source contact layer 124 may be simply referred to as a source horizontal stack 110. The source horizontal stack 110 may be disposed below the second multilayer stack 120M, and the source contact layer 124 may be directly coupled to the channel layer 118 of the memory stack structure 120P.
[0154] As described above, the source horizontal stack 110 formed through a series of processes of replacing the source sacrificial layer 104 with the source contact layer 124 may have a structure in which the source contact layer 124 is embedded.
[0155] Reference Fig. 22 , the sacrificial layer 112 of the second multilayer stack 120M may be selectively removed. As a result, a horizontal gate recess 125 may be formed between the dielectric layers 111. Since the sacrificial layer 112 includes a nitride, the sacrificial layer 112 may be removed by a chemical including phosphoric acid (H3PO4). While the sacrificial layer 112 is being removed, the sacrificial sealing layer 122 may also be removed at the same time. According to another embodiment of the present disclosure, the sacrificial sealing layer 122 may be removed after the sacrificial layer 112 is removed.
[0156] While the sacrificial layer 112 is removed, the source contact layer 124 can be fully protected by the barrier oxide. The barrier oxide can serve as a protective layer to protect the source contact layer 124 from attack.
[0157] The horizontal gate recess 125 may be continuous from the vertical contact recess 121 . A portion of the barrier layer 115 of the memory stack structure 120P may be exposed through the horizontal gate recess 125 .
[0158] exist Fig.21 After forming the horizontal gate recess 125 in the second multilayer stack 120M in the first embodiment, the first intermediate multilayer stack 120' may be formed. The first intermediate multilayer stack 120' may have a structure of alternating dielectric layers 111 and horizontal gate recesses 125. The horizontal gate recess 125 may also be formed between the top dielectric layer 113 and the adjacent dielectric layer 111.
[0159] Reference Fig.23 and Fig.24 , the gate electrodes 127 may fill the horizontal gate recesses 125, respectively. In order to form the gate electrodes 127, a gate material layer 126 may be deposited to fill the horizontal gate recesses 125 (see Fig.23 ). After forming the gate material layer 126 , a second intermediate multilayer stack 120 ″ may be formed. The second intermediate multilayer stack 120 ″ may have a structure in which dielectric layers 111 and gate material layers 126 alternate, and the gate material layer 126 may cover the sidewalls of the vertical contact recess 121 .
[0160] Then, if Fig.24 As shown, a gate electrode 127 may be formed by performing an etch-back process on the gate material layer 126. The gate electrode 127 may include a low resistance material. The gate electrode 127 may include a metal-based material. The gate electrode 127 may include a metal, a metal silicide, a metal nitride, or a combination thereof. For example, the metal may include nickel, cobalt, platinum, titanium, tantalum, or tungsten. The metal silicide may include nickel silicide, cobalt silicide, platinum silicide, titanium silicide, tantalum silicide, or tungsten silicide. The gate electrode 127 may include a stack of titanium nitride and tungsten.
[0161] The end portion 127R of the gate electrode 127 may have a shape horizontally recessed from the end portion of the dielectric layer 111. The end portion 127R of the gate electrode 127 may be exposed through the vertical contact recess 121. The gate electrode 127 may not contact the second liner layer 105', the lower source layer 102, and the source contact layer 124.
[0162] After forming the gate electrode 127, the alternating stack 120 may be formed. The alternating stack 120 may have a structure in which the dielectric layers 111 and the gate electrodes 127 are alternately stacked. The memory stack structure 120P may penetrate the alternating stack 120, and the vertical contact recess 121 may penetrate the alternating stack 120.
[0163] The source horizontal stack 110 may include a lower source layer 102, a source contact layer 124, and a second liner layer 105', and the bottom of the vertical contact recess 121 may not penetrate the lower source layer 102. Hereinafter, the second liner layer 105' may be referred to as a carbon-containing liner layer 105'.
[0164] Reference Fig.25 , which may seal the surface of the vertical contact recess 121. The surface of the vertical contact recess 121 may be sealed by a sealing layer 128S. The sealing layer 128S may include one or more protrusions 128P, and the protrusion 128P may seal the end 127R of the gate electrode 127. The sealing layer 128S may seal the sides of the dielectric layers 111 and 113. The sealing layer 128S may seal the sides of the source contact layer 124. The sealing layer 128S may seal the sides of the carbon-containing liner layer 105' and may seal the exposed surface of the lower source layer 102. The sealing layer 128S may include a silicon oxide-based material. The sealing layer 128S may include a low dielectric material. The low dielectric material may have a dielectric constant lower than that of silicon nitride. The material of the sealing layer 128S may have a dielectric constant lower than about 7.
[0165] The sealing layer 128S may be thinner than the dielectric layers 111 and 113 and the gate electrode 127. The sealing layer 128S may be a layer of a material different from that of the dielectric layers 111 and 113. The sealing layer 128S may be a layer of a material different from that of the gate electrode 127. The sealing layer 128S may include a material having high wet etching resistance. The wet etching resistance of the sealing layer 128S may be derived from carbon. The sealing layer 128S may be formed of a carbon-containing material, and the dielectric layers 111 and 113 may be formed of a carbon-free material. The dielectric layers 111 and 113 may be formed of carbon-free silicon oxide, and the sealing layer 128S may be formed of carbon-containing silicon oxide. For example, the dielectric layers 111 and 113 may be formed of SiO2, and the sealing layer 128S may be formed of SiCO. SiCO may be more etch-resistant than SiO2. The carbon content of SiCO may be less than the silicon content and the oxygen content. For example, SiCO may have a composition ratio of 34 at% silicon (Si), 40 at% oxygen, and 17 at% carbon. SiCO may have a lower dielectric constant than silicon nitride (Si3N4).
[0166] The sealing layer 128S may be formed to have approximately to The high wet etching resistance of SiCO can reduce the thickness of the sealing layer 128S. As a result, the size of each vertical contact recess 121 for separating the unit blocks can be reduced, which ultimately leads to a reduction in chip size. In the comparative example, when the sealing layer is formed of SiO2, the sealing layer should be formed to have a thickness of about 1000 nm in consideration of the loss in the subsequent process (e.g., the cleaning process). or thicker. The thick SiO2 sealing layer of the comparative example may make it difficult to fill the vertical contact recess with the source contact plug without a gap, and each vertical contact recess of the comparative example should have a relatively large size in order to improve the gap filling characteristics of the source contact plug. In contrast, since SiCO of the sealing layer 128S according to the embodiment of the present disclosure has higher wet etching resistance than SiO2, the sealing layer 128S can be formed to be thinner than the sealing layer of SiO2 in the comparative example. Therefore, even if the size of the vertical contact recess 121 is small, the vertical contact recess 121 can be filled with the source contact plug without a gap.
[0167] According to another embodiment of the present disclosure, the sealing layer 128S may include a material having wet etching resistance relative to subsequent processes. The sealing layer 128S may include SiCN, SiBCN, SiBN, or a combination thereof. The wet etching resistance of the sealing layer 128S may be derived from carbon, nitrogen, boron, or a combination thereof.
[0168] According to another embodiment of the present disclosure, a seed layer may be formed before forming the sealing layer 128S. The seed layer may form a thin silicon oxide layer or a thin silicon nitride layer. By forming the seed layer, the conformability of the sealing layer 128S may be improved.
[0169] According to another embodiment of the present disclosure, the sealing layer 128S may include a stack of one or more carbon-free silicon oxide layers and one or more carbon-containing silicon oxide layers. For example, after thinly depositing the carbon-free silicon oxide layer, the carbon-containing silicon oxide layer may be deposited over the carbon-free silicon oxide layer. The carbon-free silicon oxide may improve the conformability of the carbon-containing silicon oxide as a seed layer.
[0170] Reference Fig.26 , the sealing layer 128S may be selectively removed to expose the surface of the lower source layer 102. As a result, a sealing spacer 128 may be formed on the sidewalls of the vertical contact recess 121. The bottom of the sealing spacer 128 may substantially completely cover the side of the source contact layer 124 and the side of the carbon-containing liner layer 105'. The sealing spacer 128 may include one or more protrusions 128P, and the protrusion 128P may seal the end 127R of the gate electrode 127. The sealing spacer 128 may seal the side of the dielectric layers 111 and 113.
[0171] The sealing spacer 128 may be vertically continuous along a stacking direction of the dielectric layer 111 and the gate electrode 127. From a top view perspective, the sealing spacer 128 may have a closed loop shape sealing a sidewall of the vertical contact recess 121.
[0172] Since the thickness of the sealing layer 128S is thin, an open area of the bottom surface of the vertical contact recess 121 may be increased in an etching process for forming the sealing spacer 128. As a result, low resistance and process stability may be ensured.
[0173] After forming the sealing spacer 128 , a post-cleaning process may be performed.
[0174] Reference Fig. 27 and Fig.28 , the vertical contact recesses 121 may be filled with a conductive contact material. For example, a source contact plug 132 may be formed in each vertical contact recess 121. The source contact plug 132 may fill the vertical contact recess 121. Each source contact plug 132 may include a stack of a silicon-containing material 129 and a metal-containing material 131, and it may also include a barrier material 130 between the silicon-containing material 129 and the metal-containing material 131. The silicon-containing material 129 may include polysilicon, and the metal-containing material 131 may include tungsten. The barrier material 130 may include titanium nitride. According to another embodiment of the present disclosure, the source contact plug 132 may be formed of only tungsten.
[0175] The silicon-containing material 129 may be formed by depositing polysilicon to fill the vertical contact recess 121 and then performing an etch-back process on the polysilicon. A pre-cleaning process may be performed before depositing the polysilicon, and a post-cleaning process may be performed after the etch-back process of the polysilicon. The silicon-containing material 129 may contact the sealing spacer 128.
[0176] After forming the silicon-containing material 129, the barrier material 130 may be conformally deposited. A pre-cleaning process may be performed before depositing the barrier material 130. After conformally depositing the barrier material 130, the remaining portion of the vertical contact recess 121 may be filled with the metal-containing material 131. After sequentially depositing the barrier material 130 and the metal-containing material 131, a planarization process using chemical mechanical polishing (CMP) may be performed. As a result, the barrier material 130 and the metal-containing material 131 may remain only inside the vertical contact recess 121. The barrier material 130 may be in direct contact with the sealing spacer 128, and the metal-containing material 131 may not contact the sealing spacer 128.
[0177] Although a plurality of cleaning processes are performed during the process of forming the sealing spacer 128 , the process of forming the silicon-containing material 129 , and the process of depositing the barrier material 130 , a thickness loss of the sealing spacer 128 hardly occurs.
[0178] As described above, the source horizontal stack 110 and the alternating stack 120 may be formed above the lower structure 101. The source horizontal stack 110 may include a lower source layer 102, a source contact layer 124, and a carbon-containing liner layer 105'. The alternating stack 120 may be formed by alternately stacking dielectric layers 111 and gate electrodes 127. The memory stack structure 120P may completely penetrate the alternating stack 120, and may not completely penetrate the source horizontal stack 110. The bottom of the memory stack structure 120P may penetrate the carbon-containing liner layer 105' and the source contact layer 124 of the source horizontal stack 110, but may not penetrate the lower source layer 102. The outer wall of the bottom of the channel layer 118 of the memory stack structure 120P may directly contact the source contact layer 124. The channel layer 118 , the lower source layer 102 , and the source contact plug 132 may be electrically connected through the source contact layer 124 .
[0179] The gate electrode 127 and the source contact plug 132 may be electrically disconnected by the sealing spacer 128. The gate electrode 127 and the source contact plug 132 may be physically disconnected by the sealing spacer 128. A high voltage may be repeatedly applied between the gate electrode 127 and the source contact plug 132, which increases GBB. This is called a growth bad block phenomenon. According to an embodiment of the present disclosure, GBB defects may be prevented by forming a sealing spacer 128 including a carbon-containing material. In other words, since the sealing spacer 128 is formed of a material having high wet etching resistance, the thickness loss of the sealing spacer 128 does not substantially occur during a subsequent cleaning process. Therefore, the sealing spacer 128 may be formed to be thick enough to withstand the high voltage applied between the gate electrode 127 and the source contact plug 132.
[0180] In addition, since the sealing spacer 128 is formed of a low dielectric material, parasitic capacitance between the gate electrode 127 and the source contact plug 132 may be reduced.
[0181] In addition, according to an embodiment of the present disclosure, since the carbon-containing liner layer 105′ is formed of SiCO, a significant thickness loss is not caused by wet etching chemicals, and the thickness loss of SiCO caused during the process of forming the horizontal contact recess 123 and the process of expanding the horizontal contact recess 123 (i.e., the dry etching process and the wet etching process for removing the blocking layer 115, the charge trapping layer 116, and the tunnel dielectric layer 117) is so small that the breakdown voltage (BV) characteristics with the source contact plug 132 can be improved.
[0182] In addition, when the carbon-containing liner layer 105' is formed of SiCO, the bottom dielectric layer 111 may be formed to be relatively thin (eg, about 100 mm thick). ). Therefore, the dopant diffusion movement distance from the source contact layer 124 to the channel layer 118 adjacent to the bottom gate electrode 127 can be shortened. Figure 2As shown, when a stack of the second liner layer 105 and the upper source layer 106 is applied, the dopant diffusion movement distance may be approximately (About Bottom dielectric layer + approx. In contrast, when only the second liner layer 105' is applied, the dopant diffusion movement distance may be approximately (About The bottom dielectric layer 111+approximately The second pad layer 105').
[0183] Reference Figures 16 to 28 , a method for manufacturing a vertical semiconductor device may include the following steps: forming a first multi-layer stack 110S including a source sacrificial layer 104 and a carbon-containing liner layer 105' above a lower structure 101; forming a second multi-layer stack 120M in which dielectric layers 111 and sacrificial layers 112 are alternately stacked above the first multi-layer stack 110S; forming a memory stack structure 120P, the memory stack structure 120P including a channel layer 118 extending to penetrate the second multi-layer stack 120M and the first multi-layer stack 110S; forming a channel layer 118 extending to penetrate the second multi-layer stack 120M and the first multi-layer stack 110S by being spaced apart from the memory stack structure 120P; The invention relates to a first multilayer stack 120M and a first multilayer stack 110S; forming a horizontal contact recess 123 by selectively removing the source sacrificial layer 104 through the vertical contact recess 121; expanding the horizontal contact recess 123 to expose the lower outer wall of the channel layer 118; filling the expanded horizontal contact recess 123 with a source contact layer 124; replacing the sacrificial layer 112 with a gate electrode 127; forming a sealing spacer 128 sealing the sidewall of the vertical contact recess 121 over the source contact layer 124 and the gate electrode 127; and forming a source contact plug 132 in the vertical contact recess 121. The carbon-containing liner layer 105' and the sealing spacer 128 may be formed of carbon-containing silicon oxide.
[0184] Carbon-containing silicon oxide (i.e., SiCO) can be applied to a process for forming a contact plug in a DRAM, a logic device, etc. For example, after performing a contact etching process for forming a contact hole in an interlayer dielectric layer, a SiCO spacer can be formed on the sidewall of the contact hole by depositing SiCO and performing an etch-back process. After forming the SiCO spacer, the contact hole can be filled with a conductive contact plug. The SiCO spacer can be exposed to a plurality of cleaning processes such as post-cleaning after forming the SiCO spacer, post-cleaning before forming the conductive contact plug, etc. Even if the SiCO spacer is exposed to a subsequent cleaning process, since the SiCO spacer is a material with high wet etching resistance, the thickness loss will be small.
[0185] According to an embodiment of the present disclosure, since a sealing spacer is formed of a material having high wet etching resistance between a gate electrode and a source contact plug, electrical characteristics may be improved.
[0186] According to an embodiment of the present disclosure, the sealing spacer may be formed to be thick enough to withstand a high voltage applied between the gate electrode and the source contact plug.
[0187] According to an embodiment of the present disclosure, since the sealing spacer is formed of a low dielectric material, parasitic capacitance between a gate electrode and a source contact plug may be reduced.
[0188] According to the embodiments of the present disclosure, the reliability of a vertical semiconductor device may be improved.
[0189] While the present disclosure has been described with respect to specific embodiments, it will be apparent to those skilled in the art that various changes and modifications may be made without departing from the spirit and scope of the disclosure as defined in the following claims.
[0190] CROSS-REFERENCE TO RELATED APPLICATIONS
[0191] This application claims priority to Korean Patent Application No. 10-2019-0156872, filed on November 29, 2019, which is hereby incorporated by reference in its entirety.
Claims
1. A semiconductor device, comprising: an alternating stack disposed over the lower structure and comprising a plurality of gate electrodes and a plurality of dielectric layers alternately stacked; a memory stack structure including a channel layer extending to penetrate the alternating stack and a memory layer surrounding the channel layer; a source layer, the source layer being in contact with an outer wall of the vertical channel layer and being disposed above the alternating stack; a trench spaced apart from the memory stack structure and extending to penetrate the alternating stack; as well as a sealing spacer, the sealing spacer being configured to seal the gate electrode and being disposed between the trench and the gate electrode, the etching resistance of the sealing spacer being different from the etching resistance of the dielectric layer, The sealing spacer includes a material having a wet etching resistance greater than that of the dielectric layer.
2. The semiconductor device according to claim 1, wherein The sealing spacer includes a carbon-containing material.
3. The semiconductor device according to claim 1, wherein The sealing spacer includes carbon-containing silicon oxide.
4. The semiconductor device according to claim 1, wherein The sealing spacer includes a material having wet etching resistance greater than that of SiO 2 and a dielectric constant lower than that of silicon nitride.
5. The semiconductor device according to claim 1, wherein The sealing spacer includes SiCO.
6. The semiconductor device according to claim 1, wherein The sealing spacer includes a stack of a SiO 2 layer and a SiCO layer, and the SiCO layer is in direct contact with the trench.
7. The semiconductor device according to claim 1, wherein The sealing spacer includes SiCO, and a carbon content of the SiCO is smaller than a silicon content and an oxygen content.
8. The semiconductor device according to claim 1, wherein The outer wall of the groove is surrounded by the sealing spacer, and The sealing spacer extends in a specific direction to cover the gate electrode, the dielectric layer and the source layer, and the gate electrode and the dielectric layer are stacked in the specific direction.
9. The semiconductor device according to claim 1, wherein: The sealing spacer includes one or more protrusions extending in a specific direction perpendicular to a direction in which a plurality of the gate electrodes and a plurality of the dielectric layers are stacked to respectively seal one or more end portions of the gate electrode.
10. The semiconductor device according to claim 1, wherein The sealing spacer has to Thickness within the range.
11. The semiconductor device according to claim 1, further comprising: an upper source layer between the alternating stack and the source layer; as well as a lower source layer between the source layer and the lower structure, Wherein, each of the upper source layer and the lower source layer comprises a semiconductor material.
12. The semiconductor device according to claim 1, wherein The groove comprises: Silicon-containing material pattern; a metal-containing material pattern disposed above the silicon-containing material pattern; and A barrier material layer is disposed between the silicon-containing material pattern and the metal-containing material pattern.
13. The semiconductor device according to claim 1, wherein The sealing spacer includes SiCN, SiBCN or SiBN.
14. The semiconductor device according to claim 1, wherein The liner layer and the sealing spacer include carbon-containing silicon oxide.
15. The semiconductor device according to claim 14, wherein: The plurality of dielectric layers of the alternating stack include a bottom dielectric layer and a plurality of remaining dielectric layers of the alternating stack disposed above the bottom dielectric layer, wherein the bottom dielectric layer is thinner than the thickness of each of the remaining dielectric layers.
16. The semiconductor device according to claim 1, further comprising: A liner layer is between the alternating stack and the source layer.
17. The semiconductor device according to claim 16, wherein: The gasket layer and the sealing spacer include the same material.
18. A semiconductor device, comprising: an alternating stack disposed over the lower structure and comprising a plurality of gate electrodes and a plurality of dielectric layers alternately stacked; a memory stack structure including a channel layer extending to penetrate the alternating stack and a memory layer surrounding the channel layer; a source layer, the source layer being in contact with an outer wall of the vertical channel layer and being disposed above the alternating stack; a trench spaced apart from the memory stack structure and extending to penetrate the alternating stack; as well as A sealing spacer is provided to seal the gate electrode and is provided between the trench and the gate electrode, wherein a thickness of the sealing spacer in a horizontal direction is smaller than a thickness of each of the dielectric layer and the gate electrode in a vertical direction.
19. The semiconductor device according to claim 18, wherein: A thickness of the protrusion of the sealing spacer in the horizontal direction is smaller than a thickness of each of the dielectric layer and the gate electrode in the vertical direction.
20. The semiconductor device according to claim 18, wherein The sealing spacer includes a carbon-containing material.
21. The semiconductor device according to claim 18, wherein The sealing spacer includes carbon-containing silicon oxide.
22. The semiconductor device according to claim 18, wherein The sealing spacer includes a material having wet etching resistance greater than that of SiO 2 and a dielectric constant lower than that of silicon nitride.
23. The semiconductor device according to claim 18, wherein The sealing spacer includes SiCO.
24. The semiconductor device according to claim 18, wherein The sealing spacer includes a stack of a SiO 2 layer and a SiCO layer, and the SiCO layer is in direct contact with the trench.
25. The semiconductor device according to claim 18, wherein The sealing spacer includes SiCO, and a carbon content of the SiCO is smaller than a silicon content and an oxygen content.
26. The semiconductor device according to claim 18, wherein The outer wall of the groove is surrounded by the sealing spacer, and The sealing spacer extends in a specific direction to cover the gate electrode, the dielectric layer and the source layer, and the gate electrode and the dielectric layer are stacked in the specific direction.
27. The semiconductor device according to claim 18, wherein The sealing spacer includes one or more protrusions extending in a specific direction perpendicular to a direction in which a plurality of the gate electrodes and a plurality of the dielectric layers are stacked to respectively seal one or more end portions of the gate electrode.
28. The semiconductor device according to claim 18, wherein The sealing spacer has to Thickness within the range.
29. The semiconductor device according to claim 18, further comprising: an upper source layer between the alternating stack and the source layer; as well as a lower source layer between the source layer and the lower structure, Wherein, each of the upper source layer and the lower source layer comprises a semiconductor material.
30. The semiconductor device according to claim 18, wherein The groove comprises: Silicon-containing material pattern; a metal-containing material pattern disposed above the silicon-containing material pattern; and A barrier material layer is disposed between the silicon-containing material pattern and the metal-containing material pattern.
31. The semiconductor device according to claim 18, wherein The sealing spacer includes SiCN, SiBCN or SiBN.
32. The semiconductor device according to claim 18, wherein: The liner layer and the sealing spacer include carbon-containing silicon oxide.
33. The semiconductor device according to claim 18, wherein: The plurality of dielectric layers of the alternating stack include a bottom dielectric layer and a plurality of remaining dielectric layers of the alternating stack disposed above the bottom dielectric layer, wherein the bottom dielectric layer is thinner than the thickness of each of the remaining dielectric layers.
34. The semiconductor device according to claim 18, further comprising: A liner layer is between the alternating stack and the source layer.
35. The semiconductor device according to claim 34, wherein: The gasket layer and the sealing spacer include the same material.
36. The semiconductor device according to claim 18, wherein A top dielectric layer among the plurality of dielectric layers is thicker than dielectric layers located at a lower level than the top dielectric layer.
37. The semiconductor device according to claim 18, wherein: The dielectric layer includes SiO2.
38. The semiconductor device according to claim 18, wherein: The end portion of the dielectric layer has a shape that is horizontally recessed from the end portion of the dielectric layer.
39. The semiconductor device according to claim 18, wherein: The sealing spacer includes one or more protrusions respectively coupled to ends of the gate electrode.
40. The semiconductor device according to claim 18, wherein A thickness of the protrusion of the sealing spacer in the horizontal direction is smaller than a thickness of each of the dielectric layer and the gate electrode in the vertical direction.
41. The semiconductor device according to claim 18, wherein The protrusion of the sealing spacer has a to Thickness within the range.