Method and device for testing photoluminescence characteristic of epitaxial wafer
By heating on the epitaxial sheet and using the laser beam to excite the optical signal, the photoluminescence characteristics within the range of 300-475K are directly tested, which solves the complexity of the high-temperature stability evaluation of the epitaxial sheet in the prior art, and achieves simple high-temperature performance evaluation .
Patent Information
- Application Number
- CN202411070384.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-11-19
AI Technical Summary
The photoluminescence characteristics test of epitaxial sheets in the prior art requires complex process preparation cycles and high-temperature performance verification, making it difficult to simply and directly evaluate the stability of the material at high temperatures.
Provide a testing method and device to determine the material by heating the epitaxial sheet to a range of 300-475K, using the target laser beam to excite and detect the optical signal, and record the photoluminescence characteristics, including peak intensity, wavelength redshift and half-maximum width. High temperature stability.
The test process is simplified, complex process verification is avoided, and the photoluminescence quality of epitaxial materials is directly evaluated at high temperatures. The high temperature stability of the material can be judged by simple physical quantities.
Smart Images

Figure CN118980429A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor technology, and in particular to a testing method and a testing device for photoluminescence characteristics of an epitaxial wafer. Background Art
[0002] Photoluminescence (PL) is an emission spectrum produced by a material after being excited. For semiconductor materials, electrons in the valence band are excited to the conduction band and a hole is generated in the valence band. The electrons and holes relax to the excited state of the conduction band and the excited state of the top of the valence band, respectively. Since the carriers are in an unstable state in the excited state, the electrons and holes will further relax to the bottom of the conduction band and the top of the valence band, respectively. Eventually, the electrons and holes will recombine, and the energy generated by the recombination will be released in the form of radiation and generate a photon. The re-radiated photons have different polarization states and energy sizes. This information contains information such as the crystal structure, material composition, and carrier relaxation process in the material. Therefore, the study of semiconductor photoluminescence spectra is a commonly used means to reveal the reaction of complex physical processes inside the material, and is a commonly used optical non-destructive characterization method for materials.
[0003] Usually, when characterizing the photoluminescence spectrum of semiconductor materials, a liquid helium circulating cooling table is required to cool the sample to reduce the influence of hot carrier excitation, background noise and lattice thermal expansion on the spectral signal. In order to verify the stability of the luminescence intensity and luminescence wavelength of epitaxial materials with temperature rise in a high-temperature environment, it is necessary to grow a pin full structure containing upper and lower cladding layers and a multi-layer active area in the center and prepare it as a Fabry-Perot cavity (F-Pcavity) laser to test the variable temperature current-power-voltage (PIV) performance. This method of verifying the high-temperature performance of the material requires a long process preparation cycle, which is not conducive to the iterative optimization of the epitaxial material structure. Therefore, a simple and direct method is needed to characterize the high-temperature stability of the epitaxial material by testing the high-temperature PL performance, avoiding the involvement of complex process flows at the stage of growing test pieces. Summary of the invention
[0004] 1. Technical issues to be resolved
[0005] In order to solve at least one of the above technical problems in the test of the photoluminescence characteristics of epitaxial wafers in the prior art, the embodiments of the present invention provide a test method and a test device for the photoluminescence characteristics of epitaxial wafers, which can directly test the PL spectrum within the temperature range of 300-475 K. The photoluminescence quality of the material at different temperatures is judged based on the decrease degree of the peak intensity (PeakIntensity) of the photoluminescence spectrum obtained from the test results, the red shift amount of the peak wavelength (Red Shift) and the widening amount of the half-peak width (Full Width Half Max, FWHM) of the spectrum. The better the high-temperature stability of the epitaxial wafer, the lower the decrease degree of the peak intensity, the smaller the wavelength red shift amount, and the insignificant widening amount of the half-peak width. The quality of the epitaxial material can be judged only by three simple and easy-to-obtain physical quantities, avoiding complicated process verification.
[0006] (II) Technical solution
[0007] In view of the above technical problems, an embodiment of the present invention provides a method and a device for testing the photoluminescence characteristics of an epitaxial wafer.
[0008] According to a first aspect of the present invention, a method for testing the photoluminescence characteristics of an epitaxial wafer is provided, comprising the following steps: heating the epitaxial wafer to a preset temperature; stimulating the epitaxial wafer to generate an optical signal using a target laser beam; detecting and recording the optical signal using a detector; and judging the photoluminescence characteristics of the epitaxial wafer based on the optical signal.
[0009] In some exemplary embodiments, before heating the epitaxial wafer to a preset temperature, the method further includes: cooling the detector to reduce the influence of the thermal background on the detection result of the detector.
[0010] In some exemplary embodiments, heating the epitaxial wafer to a preset temperature includes: placing the epitaxial wafer on a baking plate plane; adjusting the temperature of the baking plate to a preset temperature through a temperature regulating panel; and covering the baking plate with a thermal insulation cover so that the baking plate can evenly transfer heat to the epitaxial wafer.
[0011] In some exemplary embodiments, using a target laser beam to stimulate an epitaxial wafer to generate an optical signal includes: turning on a switch of a laser to generate an initial laser beam; using a beam splitter to split the initial laser beam into a first laser beam and a second laser beam; the first laser beam is input to an input end of a multimode beam splitter through an attenuation plate, and a target laser beam is output from an optical fiber head at a first output end of the multimode beam splitter; the second laser beam is input to a power meter to calibrate the power of the initial laser beam; and the optical fiber head is placed vertically on the surface of the epitaxial wafer so that the target laser beam stimulates the epitaxial wafer to generate an optical signal.
[0012] In some exemplary embodiments, recording and recording the optical signal with the detector includes: transmitting the optical signal to the multimode optical splitter through the optical fiber head, and transmitting the optical signal to the detector through the second output end of the multimode optical splitter.
[0013] In some exemplary embodiments, the laser comprises a helium-neon laser; and / or the beam splitter comprises a 50:50 beam splitter; and / or the multimode beam splitter comprises a 70:30 multimode beam splitter; and / or the detector comprises a gallium indium arsenide detector.
[0014] In some exemplary embodiments, the preset temperature is 300K-475K.
[0015] According to a second aspect of the present invention, there is provided a testing device for photoluminescence characteristics of an epitaxial wafer, comprising: a laser for generating an initial laser beam; a beam splitter for splitting the initial laser beam into a first laser beam and a second laser beam; an attenuation plate for adjusting the power of the first laser beam; a power meter for receiving the second laser beam to calibrate the power of the initial laser beam; a multimode beam splitter, comprising an input end, a first output end, and a second output end, wherein the first laser beam after power adjustment by the attenuation plate is input into the multimode beam splitter through the input end and outputs a target laser beam from the optical fiber head at the first output end; a baking plate, comprising a baking plate plane, a temperature adjustment panel, and a heat preservation cover, wherein the baking plate plane is used to place the epitaxial wafer; the temperature adjustment panel is used to adjust the temperature of the baking plate; and the heat preservation cover is used to make the baking plate evenly conduct heat to the epitaxial wafer to ensure the stability of the test environment; and a detector connected to the second output end, and used to detect and record the optical signal generated by the epitaxial wafer.
[0016] In some exemplary embodiments, the testing device further includes: a display for displaying the optical signal detected by the detector.
[0017] In some exemplary embodiments, the laser comprises a helium-neon laser; and / or the beam splitter comprises a 50:50 beam splitter; and / or the multimode beam splitter comprises a 70:30 multimode beam splitter; and / or the detector comprises a gallium indium arsenide detector.
[0018] (III) Beneficial effects
[0019] It can be seen from the above technical solutions that the method and device for testing the photoluminescence characteristics of an epitaxial wafer provided by the embodiments of the present invention have at least the following beneficial effects:
[0020] (1) The PL spectrum in the temperature range of 300K-475K can be directly tested, avoiding complex process verification.
[0021] (2) Use a 70:30 multimode splitter, where the 70% input end of the multimode splitter is connected to the output end of the He-Ne laser, and the 30% output end is connected to the input end of the detector. This connection method can reduce the background 632nm pump light component reflected from the detection end of the epitaxial wafer and avoid submerging the excitation signal.
[0022] (3) Cool down the detector before testing to reduce the impact of thermal background on the detector. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The above contents and other objects, features and advantages of the present invention will become more apparent through the following description of the embodiments of the present invention with reference to the accompanying drawings, in which:
[0024] Figure 1 A schematic diagram of a process of testing a photoluminescence property of an epitaxial wafer according to an embodiment of the present invention is shown;
[0025] Figure 2 A schematic diagram of a process of heating an epitaxial wafer to a preset temperature according to an embodiment of the present invention is shown;
[0026] Figure 3 A schematic diagram of a process of using a target laser beam to stimulate an epitaxial wafer to generate an optical signal according to an embodiment of the present invention is shown;
[0027] Figure 4 A schematic diagram of a process flow of another method for testing photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is shown;
[0028] Figure 5 A schematic diagram schematically shows a photoluminescence spectrum measured by a testing method according to an embodiment of the present invention; and
[0029] Figure 6 A schematic diagram of a device for testing photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is schematically shown.
[0030] Reference numerals:
[0031] 1-Laser; 2-Beam splitter; 3-Attenuator; 4-Power meter; 5-Multimode beam splitter; 6-Drying plate; 7-Detector; 8-Display. DETAILED DESCRIPTION
[0032] In order to make the purpose, technical scheme and advantages of the present invention more clearly understood, the present invention is further described in detail below in combination with specific embodiments and with reference to the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0033] Figure 1 The flowchart of a method for testing photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is schematically shown.
[0034] like Figure 1 As shown, a method for testing photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention includes steps S110-S140.
[0035] In step S110, the epitaxial wafer is heated to a preset temperature. Optionally, the preset temperature is 300K-475K.
[0036] In some exemplary embodiments, step S110 includes steps S111-S113, see Figure 2 .
[0037] In step S111, the epitaxial wafer is placed on a baking plate plane.
[0038] In step S112, the temperature of the baking plate 6 is adjusted to a preset temperature through the temperature adjustment panel.
[0039] In step S113, the heat preservation cover of the baking plate 6 is put on to make the baking plate 6 conduct heat to the epitaxial wafer evenly, while ensuring the test temperature is accurate and the test environment is stable.
[0040] In step S120, the target laser beam is used to excite the epitaxial wafer to generate an optical signal.
[0041] In some exemplary embodiments, step S120 includes steps S121-S125, see Figure 3 .
[0042] In step S121, the laser 1 is turned on to generate an initial laser beam. Optionally, the laser 1 comprises a helium-neon laser.
[0043] In step S122, the initial laser beam is split into a first laser beam and a second laser beam using a beam splitter 2. Optionally, the beam splitter 2 comprises a 50:50 beam splitter.
[0044] In step S123, the first laser beam is input to the input end of the multimode optical splitter 5 through the attenuation plate 3, and the target laser beam is output from the optical fiber head at the first output end of the multimode optical splitter 5. Optionally, the multimode optical splitter 5 includes a 70:30 multimode optical splitter.
[0045] In step S124, the second laser beam is input into the power meter 4 to calibrate the power of the initial laser beam.
[0046] In step S125, the optical fiber head is placed vertically on the surface of the epitaxial wafer so that the target laser beam excites the epitaxial wafer to generate an optical signal. For example, the optical fiber head at the single output end of the 70:30 multimode optical splitter 5 is placed vertically on the surface of the epitaxial wafer. At this time, the material will be stimulated to generate a photoluminescence signal with a wavelength range of 1250-1320nm. The signal is transmitted to the multimode optical splitter 5 through the output end optical fiber head, and is transmitted to one end of the detector 7 through the 30% end. Due to the ratio of the optical splitter, the 30% end can significantly attenuate the intrinsic signal of the laser, so that it cannot become an intensity background that drowns the spectral signal of the sample.
[0047] In step S130, the optical signal is detected and recorded by the detector 7. Optionally, the optical signal is transmitted to the multimode optical splitter 5 through the optical fiber head, and is transmitted to the detector 7 through the second output end of the multimode optical splitter 5. Optionally, the detector 7 includes a gallium arsenide indium detector. For example, the 70% input end of the 70:30 multimode optical splitter is connected to the output end of the helium-neon (He-Ne) laser, and the 30% output end is connected to the input end of the detector 7. The purpose of this connection method is to reduce the background 632nm pump light component reflected from the detection end of the epitaxial wafer to avoid drowning the excitation signal.
[0048] In step S140 , the photoluminescence characteristics of the epitaxial wafer are determined based on the optical signal.
[0049] Figure 4 The flowchart of another method for testing the photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is schematically shown.
[0050] like Figure 4 As shown in FIG. 1 , another method for testing the photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is Figure 1 The method further includes step S150, wherein step S150 is located before step S110.
[0051] In step S150 , the detector 7 is cooled to reduce the influence of the thermal background on the detection result of the detector 7 .
[0052] For example, the temperature of the indium gallium arsenide (InGaAs) detector 7 is lowered to reduce the influence of the thermal background on the detector 7. Take an epitaxial wafer containing three layers of indium arsenide / gallium arsenide (InAs / GaAs) quantum dots in the active region, heat the epitaxial wafer, obtain the photoluminescence signal of the test wafer after the temperature stabilizes, and record the signal in the display 8. The test temperature range is 300~395K, wherein, when the test temperature range is 300~315K, the temperature is increased by 15K each time; when the test temperature range is 315~395K, the temperature is increased by 20K each time. The central emission wavelength of the quantum dots is around 1300nm. The test results are as follows: Figure 5 As shown by Figure 5It can be seen that as the temperature rises, the peak intensity shows a downward trend, the peak wavelength red shifts and the half-peak width widens, which is in line with the expectations of the test results. The photoluminescence quality of the epitaxial wafer at different temperatures is judged based on the decrease in the peak intensity (Peak Intensity) of the photoluminescence spectrum obtained from the test results, the red shift of the peak wavelength (Red Shift) and the widening of the half-peak width (Full Width HalfMax, FWHM) of the spectrum. The better the high-temperature stability of the epitaxial wafer, the lower the decrease in the peak intensity, the smaller the wavelength red shift, and the insignificant widening of the half-peak width. The quality of the epitaxial wafer can be judged only by three simple and easy-to-obtain physical quantities, avoiding complex process verification.
[0053] Figure 6 A schematic diagram of a device for testing photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention is schematically shown.
[0054] like Figure 6 As shown, a testing device for photoluminescence characteristics of an epitaxial wafer according to an embodiment of the present invention comprises: a laser 1 for generating an initial laser beam, and optionally, the laser 1 comprises a helium-neon laser; a beam splitter 2 for splitting the initial laser beam into a first laser beam and a second laser beam, and optionally, the beam splitter 2 comprises a 50:50 beam splitter; an attenuation plate 3 for adjusting the power of the first laser beam; a power meter 4 for receiving the second laser beam to calibrate the power of the initial laser beam; a multimode beam splitter 5 comprising an input end, a first output end and a second output end, wherein the first laser beam after power adjustment by the attenuation plate 3 is input into the multimode beam splitter 5 through the input end and outputs a target laser beam from the optical fiber head at the first output end, and optionally, the multimode beam splitter 5 comprises a 70:30 multimode beam splitter; a baking plate 6 comprising a baking plate plane, a temperature adjustment panel and a heat preservation cover, wherein the baking plate plane is used to place the epitaxial wafer; the temperature adjustment panel is used to adjust the temperature of the baking plate 6; and the heat preservation cover is used to make the baking plate 6 evenly conduct heat to the epitaxial wafer to ensure the stability of the test environment. The detector 7 is connected to the second output terminal and is used to detect and record the optical signal generated by the epitaxial wafer. Optionally, the detector 7 includes a gallium indium arsenide detector. The test device of the embodiment of the present invention can be used to perform Figure 1-Figure 4 The test method shown will not be repeated here.
[0055] In some exemplary embodiments, the testing device further includes: a display 8 for displaying the optical signal detected by the detector 7 .
[0056] The above specific embodiments further illustrate the purpose, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above are only specific embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for testing the photoluminescence properties of an epitaxial wafer, characterized in that: The following steps are involved: heating the epitaxial wafer to a preset temperature; Using a target laser beam to stimulate the epitaxial wafer to generate an optical signal; Detecting and recording the optical signal with a detector; and Based on the optical signal, the photoluminescence characteristics of the epitaxial wafer are determined.
2. The testing method according to claim 1, characterized in that: Before heating the epitaxial wafer to a preset temperature, the method further comprises: The detector is cooled to reduce the influence of the thermal background on the detection result of the detector.
3. The testing method according to claim 1 or 2, characterized in that: The step of heating the epitaxial wafer to a preset temperature comprises: Place the epitaxial wafer on the baking plate plane; Adjusting the temperature of the baking plate to a preset temperature through a temperature adjustment panel; and The baking plate is covered with a heat-insulating cover to allow the baking plate to evenly transfer heat to the epitaxial wafer.
4. The testing method according to claim 1 or 2, characterized in that: The step of using a target laser beam to stimulate the epitaxial wafer to generate an optical signal comprises: Turn on the laser switch to generate an initial laser beam; Splitting the initial laser beam into a first laser beam and a second laser beam using a beam splitter; The first laser beam is input into the input end of the multimode beam splitter through the attenuation plate, and the target laser beam is output from the optical fiber head at the first output end of the multimode beam splitter; The second laser beam is input into a power meter to calibrate the power of the initial laser beam; and The optical fiber head is vertically placed on the surface of the epitaxial wafer so that the target laser beam can stimulate the epitaxial wafer to generate an optical signal.
5. The testing method according to claim 4, characterized in that: The detecting and recording of the optical signal by a detector comprises: The optical signal is transmitted to the multi-mode optical splitter through the optical fiber head, and is transmitted to the detector through the second output end of the multi-mode optical splitter.
6. The testing method according to claim 4, characterized in that: The laser comprises a helium-neon laser; and / or The beam splitter comprises a 50:50 beam splitter; and / or The multimode optical splitter comprises a 70:30 multimode optical splitter; and / or The detector includes a gallium indium arsenide detector.
7. The testing method according to claim 1, characterized in that: The preset temperature is 300K-475K.
8. A device for testing the photoluminescence properties of an epitaxial wafer, characterized in that: include: A laser for generating an initial laser beam; A beam splitter, configured to split the initial laser beam into a first laser beam and a second laser beam; An attenuation sheet, used for adjusting the power of the first laser beam; A power meter, used for receiving the second laser beam to calibrate the power of the initial laser beam; A multimode optical splitter, comprising an input end, a first output end, and a second output end, wherein the first laser beam after power adjustment by the attenuation plate is input into the multimode optical splitter through the input end and outputs a target laser beam from the optical fiber head of the first output end; A baking plate, comprising a baking plate plane, a temperature regulating panel and a heat preservation cover, wherein the baking plate plane is used to place the epitaxial wafer; the temperature regulating panel is used to regulate the temperature of the baking plate; and the heat preservation cover is used to make the baking plate evenly transfer heat to the epitaxial wafer to ensure the stability of the test environment; and A detector is connected to the second output end and is used to detect and record the optical signal generated by the epitaxial wafer.
9. The testing device according to claim 8, characterized in that: Also includes: A display is used to display the optical signal detected by the detector.
10. The testing device according to claim 8 or 9, characterized in that: The laser comprises a helium-neon laser; and / or The beam splitter comprises a 50:50 beam splitter; and / or The multimode optical splitter comprises a 70:30 multimode optical splitter; and / or The detector includes a gallium indium arsenide detector.
Citation Information
Cited By
Quantitative analysis method for migration characteristics of indium component in epitaxial wafer
CN121541015A