Semiconductor structure and manufacturing method thereof

By adopting a stacked structure of silicide layer and dielectric layer in semiconductor devices, combining the embedded structure and metal gate, the problem of insufficient performance of the device in the prior art under the small size range is solved, and capacitance and integrated density are achieved. promote.

CN118983350APending Publication Date: 2024-11-19TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411002433.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-10-26
Filing Date
2024-07-25
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

Existing semiconductor devices have difficulty meeting the performance requirements of advanced devices in reduced size range, especially with challenges in improving integration density and capacitance enhancement.

Method used

Using a stacked structure including a silicide layer, a first dielectric layer, a metal structure and a second dielectric layer, the capacitance of the capacitor is increased by forming an embedded structure and a trench structure on the substrate, while using a metal gate and conductivity. Structure to improve device performance.

Benefits of technology

Without increasing the device plane size, the capacitance and performance of MOS capacitors are improved, and the integrated density and stability of the device are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983350A_ABST
    Figure CN118983350A_ABST
Patent Text Reader

Abstract

The semiconductor structure includes a substrate and a capacitor over the substrate. The capacitor includes a silicide layer over a substrate. The capacitor includes a first dielectric layer over the silicide layer. The capacitor includes a metal gate structure over the first dielectric layer, with a top portion of the metal gate structure over the substrate and a bottom portion of the metal gate structure extending into the substrate. The capacitor includes a second dielectric layer over the metal gate structure. The capacitor also includes a conductive structure over the second dielectric layer. The embodiment of the invention also relates to a method for manufacturing the semiconductor structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present application relate to semiconductor structures and methods for manufacturing the same. Background Art

[0002] The semiconductor industry has experienced rapid development due to the continuous improvement of the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.). To a large extent, the improvement of this integration density comes from the repeated reduction of the minimum component size, which allows more components or devices to be integrated into a given area. Although existing strategies for integrating capacitive devices (such as capacitors based on metal oxide semiconductors (MOS)) are generally sufficient, they are not completely satisfactory in all aspects. For example, meeting improved device performance under a reduced length range to meet various goals for advanced devices remains a challenge. Summary of the invention

[0003] Some embodiments of the present application provide a semiconductor structure, comprising: a substrate; a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal structure located above the first dielectric layer, wherein the metal structure comprises a gate electrode; a second dielectric layer located above the metal structure; and a conductive structure located above the second dielectric layer.

[0004] Other embodiments of the present application provide a semiconductor structure, including: a substrate; and a capacitor located above the substrate, including: a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal gate structure located above the first dielectric layer, wherein a top portion of the metal gate structure is located above the substrate and a bottom portion of the metal gate structure extends into the substrate; a second dielectric layer located above the metal gate structure; and a conductive structure located above the second dielectric layer.

[0005] Still other embodiments of the present application provide a method for manufacturing a semiconductor structure, comprising: providing a substrate including a doped region; patterning the doped region to form a trench; forming a silicide layer in the trench; forming a first dielectric layer above the silicide layer; forming a dummy gate above the first dielectric layer, the dummy gate having a bottom portion filling the trench and a top portion located above the bottom portion; forming a gate spacer along the sidewall of the dummy gate; replacing the dummy gate with a metal gate; forming a second dielectric layer above the metal gate; and forming a conductive structure above the second dielectric layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] When read in conjunction with the accompanying drawings, various aspects of the disclosed embodiments can be best understood from the following detailed description. It should be noted that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, for clarity of discussion, the size of the various components may be arbitrarily increased or reduced.

[0007] Figure 1 , Figure 5 and Figure 6 Each shows a schematic top view of an exemplary semiconductor device according to some embodiments.

[0008] Figure 2 and Figure 3 Each shows a diagram according to some embodiments Figure 1 Schematic cross-sectional view of an exemplary semiconductor device taken along line AA′.

[0009] Figure 4 According to some embodiments Figure 1 Schematic cross-sectional view of an exemplary semiconductor device taken along line BB'.

[0010] Figure 7 According to some embodiments Figure 5 or Figure 6 Schematic cross-sectional view of an exemplary semiconductor device taken along line CC'.

[0011] Figure 8 According to some embodiments Figure 5 or Figure 6 Schematic cross-sectional view of an exemplary semiconductor device taken along line CC'.

[0012] Fig. 9 According to some embodiments Figure 5 or Figure 6 Schematic cross-sectional view of an exemplary semiconductor device taken along line CC'.

[0013] Fig. 10A , Fig. 10B and Fig. 10C Each shows a flow chart of an exemplary method of fabricating a semiconductor device according to some embodiments.

[0014] Fig.11 , Fig.12 , Fig.13 , Fig.14 , Fig.15 , Fig.16 , Fig.17 , Fig.18 , Fig.19 , Fig. 20 , Fig.21 , Fig. 22 and Fig.23 Each shows a schematic diagram of a Fig. 10A, Fig. 10B and / or Fig. 10C Schematic cross-sectional view of an exemplary semiconductor device during an intermediate stage of an exemplary method. DETAILED DESCRIPTION

[0015] The following disclosure provides many different embodiments or examples for realizing the different features of the provided subject matter. Specific examples of components and arrangements are described below to simplify the disclosed embodiments. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly contacted, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the disclosed embodiments may repeat reference numerals and / or characters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or configurations discussed.

[0016] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or component to another (or additional) elements or components as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should likewise be interpreted accordingly.

[0017] In the embodiments of the present disclosure, metal oxide semiconductor (MOS) devices (such as MOS capacitors) and methods of manufacturing the same are provided. Intermediate stages of manufacturing various embodiments of the present disclosure are shown. Throughout the various views and illustrative embodiments of the present disclosure, the same reference numerals are used to represent the same elements.

[0018] Figure 1 A top view of an embodiment of a semiconductor structure 200A is shown. The semiconductor structure 200A includes a device region 202A and a device region 204A, wherein the device region 202A includes a plurality of semiconductor devices 100A, and the device region 204A includes a plurality of semiconductor devices 150. In the present embodiment, the semiconductor device 100A includes a MOS device, such as a MOS capacitor, a MOS transistor, etc., or a combination thereof. In some embodiments, the semiconductor device 100A includes a MOS capacitor and is arranged in an array in the semiconductor structure 200A. In some embodiments, for example, the semiconductor device 150 includes a logic device coupled to the array of semiconductor devices 100A.

[0019] Each semiconductor device 100A includes a first region R1 surrounded by a second region R2, wherein the regions R1 and R2 include different structures, as described in detail below. The first region R1 includes at least a conductive structure (e.g., conductive structure 48) above a substrate (e.g., substrate 10), and the second region R2 includes a different metal structure (e.g., metal structure 36) above the substrate. It should be noted that for the purpose of clarity, portions of the semiconductor structure 200A are omitted from subsequent figures. For example, an interlayer dielectric (ILD) layer adjacent to an active component (e.g., a metal gate structure) of the semiconductor structure 200A is omitted.

[0020] refer to Figure 2 , Figure 2 The first region R1 of the semiconductor device 100A is shown along Figure 1 , the semiconductor device 100A is provided above the substrate 10 and separated (or isolated) by the isolation structure 12. The substrate 10 includes a semiconductor substrate, such as a bulk semiconductor, a semiconductor on insulator (SOI) substrate, etc., which may be doped (e.g., with a p-type or n-type dopant) or undoped. The substrate 10 may be a wafer, such as a silicon wafer. Typically, the SOI substrate includes a semiconductor material layer formed on an insulating layer. The insulating layer may be, for example, a buried oxide (BOX) layer, a silicon oxide layer, etc. The insulating layer is provided on a substrate, which is typically a silicon or glass substrate. Other substrates, such as multilayer or gradient substrates, may also be used. In some embodiments, the semiconductor material of the substrate 10 may include: silicon; germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide and / or indium antimonide; alloy semiconductors, including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP and / or GaInAsP; or combinations thereof.

[0021] In some embodiments, substrate 10 includes an intrinsic semiconductor material, such as intrinsic silicon. In some embodiments, substrate 10 includes a semiconductor material doped with a suitable dopant according to the conductivity type of semiconductor device 100A. For example, if semiconductor device 100A is configured as an n-type device, substrate 10 may include an n-type dopant. Exemplary n-type dopants include phosphorus, arsenic, etc., or a combination thereof, and exemplary p-type dopants include boron, gallium, indium, etc., or a combination thereof.

[0022] refer to Figure 2, the semiconductor device 100A includes a doped well 14 disposed above or within the substrate 10, wherein the doped well 14 includes a dopant having a conductivity type different from the conductivity type of the semiconductor device 100A. For example, if the semiconductor device 100A is configured as an n-type device, the doped well 14 includes a p-type dopant. In some embodiments, the doped well 14 extends across the entire substrate 10 and is configured as a doped substrate of the semiconductor device 100A.

[0023] The semiconductor device 100A includes a doping layer (or impurity layer) 20 located in the doping well 14. In the depicted embodiment where the semiconductor device 100A is configured as an n-type device, the doping layer 20 includes an n-type dopant. For embodiments where the semiconductor device 100A is configured as a p-type device, the doping layer 20 includes a p-type dopant. In the present embodiment, the doping layer 20 is a heavily doped layer including an n-type dopant.

[0024] refer to Figure 1 and Figure 2 , the semiconductor device 100A is surrounded by an isolation structure 12. In some embodiments, each isolation structure 12 separates two adjacent doped layers and / or conductive components in the substrate 10. In some embodiments, the isolation structure 12 includes at least one dielectric layer having an oxide, such as silicon oxide (SiO and / or SiO2), nitride, etc., or a combination thereof. In some embodiments, the isolation structure 12 includes a shallow trench isolation (STI) structure.

[0025] In some embodiments, semiconductor device 100A further includes a doped layer 11 adjacent to isolation structure 12. Doped layer 11 includes one or more dopants of the same conductivity as doped well 14 but at a higher concentration. For example, in the depicted embodiment, doped well 14 includes a p-type dopant at a first concentration, and doped layer 11 includes a p-type dopant at a second concentration greater than the first concentration. In some embodiments, doped layer 11 provides a location for coupling substrate 10 and / or doped well 14 to contact 50, which is a substrate contact for a MOS capacitor structure of semiconductor device 100A. In some embodiments, doped layer 11 is optional and is excluded from semiconductor device 100A.

[0026] Still reference Figure 2, the semiconductor device 100A includes a pair of source / drain regions 22 in the doped layer 20. The source / drain regions 22 each include a dopant suitable for forming a semiconductor device 100A of a specified conductivity type. For example, the source / drain regions 22 in the depicted embodiment include n-type dopants to form an n-type semiconductor device 100A. In this embodiment, the source / drain regions 22 each include a dopant of the same conductivity type as the doped layer 20 but at a different concentration. For example, the concentration of the n-type dopant in the source / drain regions 22 is greater than the concentration in the doped layer 20, such as at least one order of magnitude greater.

[0027] In some embodiments, the source / drain regions 22 are formed adjacent to the isolation structures 12, wherein the bottom surface of each isolation structure 12 vertically extends below the bottom surface of each source / drain region 22. In this regard, the source / drain regions 22 are electrically isolated from adjacent devices (e.g., another semiconductor device 100A in the array of semiconductor structures 200A) by the isolation structures 12.

[0028] The semiconductor device 100A further includes a silicide layer 26 extending laterally across the top surface of the doped layer 20 (including the top surface of each of the source / drain regions 22). In other words, the sidewalls of the silicide layer 26 substantially coincide with the sidewalls of the doped layer 20 that are laterally spaced apart along the X-axis. Figure 2 As depicted in FIG. 1 , the silicide layer 26 is completely located above the top surface of the doped layer 20. In the depicted embodiment, the silicide layer 26 is laterally located between two opposing isolation structures 12. In the present embodiment, the silicide layer 26 includes a metal silicide material having at least one metal selected from Ti, W, Mo, Ni, Co, etc. Other silicide materials may also be suitable for the disclosed embodiments.

[0029] Still reference Figure 2 , the semiconductor device 100A further includes a stack S1 of dielectric layers and conductive layers (or metal structures) located above the silicide layer 26. In the present embodiment, the stack S1 includes a first dielectric layer 32, a metal structure 36, an interface layer 44, a second dielectric layer 46, and a conductive structure (e.g., a metal structure) 48 arranged vertically along the Z-axis, and stacked in this order above the silicide layer 26. In the present embodiment, the stack S1 is completely located above the top surface of the doped layer 20. In other words, the bottommost surface of the stack S1, i.e., the first dielectric layer 32, is completely located above the top surface of the doped layer 20.

[0030] The semiconductor device 100A includes a gate spacer 38 extending along the sidewall of the stack S1. The gate spacer 38 may include a suitable dielectric material, such as silicon oxide, silicon oxycarbonitride, silicon nitride, silicon oxynitride, silicon carbonitride, etc., or a combination thereof. The gate spacer 38 may include one or more layers of a suitable dielectric material.

[0031] In the present embodiment, the stack S1 includes a first dielectric layer 32 above the silicide layer 26. In the present embodiment, the first dielectric layer 32 extends laterally across a portion of the silicide layer 26 between the source / drain regions 22. In some embodiments, the first dielectric layer 32 is configured as a gate dielectric layer. Therefore, the first dielectric layer 32 may include any suitable dielectric material, such as silicon oxide, silicon nitride, a high-k dielectric material (i.e., having a dielectric constant greater than the dielectric constant of silicon oxide, the dielectric constant of silicon oxide being about 3.9), or the like, or a combination thereof. The high-k dielectric material may include an oxide or silicate of Hf, Al, Y, Zr, La, Mg, Ba, Ti, Pb, or the like, or a combination thereof. The high-k dielectric material may additionally or alternatively include a composite oxide, such as a compound of ZrO2, Al2O3, and ZrO2 (Z a A b Z c , wherein a, b and c satisfy a suitable stoichiometric relationship), Al2O3, ZrO2, Al2O3 compound (A a Z b A c , wherein a, b and c satisfy a suitable stoichiometric relationship) or a compound of ZrO2, Al2O3, ZrO2, Al2O3, ZrO2 (Z a A b Z c A d Z e , wherein a, b, c, d and e satisfy a suitable stoichiometric relationship). In some embodiments, the first dielectric layer 32 has a multi-layer structure.

[0032] The stack S1 includes a metal structure 36 located above the first dielectric layer 32. In the present embodiment, the metal structure 36 is configured as a metal gate structure. Therefore, the metal structure 36 includes at least a metal gate electrode. In some embodiments, although not separately depicted, the metal gate structure also includes one or more work function metal layers, each having a compound metal or a single metal. The metal gate electrode includes any suitable metal, such as tungsten (W), copper (Cu), ruthenium (Ru), aluminum (Al), gold (Au), cobalt (Co), etc., or a combination thereof. The work function metal layer may include an n-type work function metal having a work function in the range of about 3.9 to about 4.5, a p-type work function metal having a work function in the range of about 4.5 to about 5.2, or a combination thereof. Examples of work function layers include TiN, TaN, Ru, Mo, Al, W, HfN, Ir, Pt, PtSi, MoN, ZrSi2, MoSi2, NiSi x 、WN、Ti、Ta、Ag、TaSi x, TaAl, TaAlC, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, etc. The metal gate electrode can be formed over one or more work function metal layers. In some embodiments, the metal structure 36 does not include any work function metal layer. Therefore, the metal structure 36 only includes the metal gate electrode. In some embodiments, the metal structure 36 includes additional layers, such as a capping layer, a glue layer, etc., or a combination thereof.

[0033] The stack S1 further includes an interface layer 44 and a second dielectric layer 46 located above the metal structure 36. In the present embodiment, the interface layer 44 and the second dielectric layer 46 are each formed in a U-shape including a sidewall extending along the gate spacer 38. In other words, the sidewall of the interface layer 44 is vertically aligned with the sidewall of the metal structure 36.

[0034] In some embodiments, the second dielectric layer 46 is configured as a gate dielectric layer. Therefore, the second dielectric layer 46 may include any suitable dielectric material, such as silicon oxide, silicon nitride, a high-k dielectric material provided herein, or the like, or a combination thereof. In some embodiments, the second dielectric layer 46 has the same composition as the first dielectric layer 32. In some embodiments, the second dielectric layer 46 has a composition different from that of the first dielectric layer 32. In some embodiments, the interface layer 44 includes an oxide, such as silicon oxide. In the present embodiment, the interface layer 44 includes a dielectric material having a lower dielectric constant (i.e., k value) than the dielectric material included in the second dielectric layer 46. For example, the interface layer 44 may include silicon oxide, which has a dielectric constant less than about 3.9, and the second dielectric layer 46 may include a high-k dielectric material, such as a metal oxide or a metal silicide, which has a dielectric constant greater than about 3.9. In some embodiments, the interface layer 44 is optional.

[0035] In addition, still refer to Figure 2 , the stack S1 includes a conductive structure 48 located above the second dielectric layer 46, wherein the second dielectric layer 46 surrounds the bottom surface and sidewall surfaces of the conductive structure 48. In the depicted embodiment, the top surface of the conductive structure 48 is substantially coplanar with the top surface of each of the second dielectric layer 46, the interface layer 44, and the gate spacer 38. In some embodiments, the conductive structure 48 is configured as a metal gate structure, similar to the metal structure 36 described in detail above. For example, the conductive structure 48 includes at least the metal gate electrode and one or more work function metal layers described in detail above with respect to the metal structure 36. In some embodiments, the conductive structure 48 includes a metal gate electrode, but does not include any work function metal layer. Therefore, in some embodiments, the conductive structure 48 is optionally referred to as a metal structure 48. In some embodiments, the conductive structure 48 includes conductive polysilicon instead of metal.

[0036] In some embodiments, the portion of the semiconductor device 100A located in the first region R1 is arranged with Figure 2 For example, the arrangement depicted in Figure 3 , the semiconductor device 100A includes a stack S2 arranged in a manner similar to the stack S1. In the stack S2, the interface layer 44 and the second dielectric layer 46 do not include any portion extending along the gate spacer 38, so that their sidewalls are vertically aligned with those of the metal structure 36 and the conductive structure 48. In addition, the gate spacer 38 is formed to surround only the sidewalls of the metal structure 36, and an additional gate spacer 39 is formed to extend along the sidewalls of the stack S2, which includes the interface layer 44, the second dielectric layer 46, and the conductive structure 48. As depicted, the gate spacers 38 and the gate spacers 39 are stacked together and vertically aligned with each other to form the gate spacer 40.

[0037] In this embodiment, such as Figure 2 As depicted in FIG. 1 , the combination of the silicide layer 26 and the stack S1 in the first region R1 of the semiconductor device 100A provides a MOS capacitor having a stack structure of “M1I1M2I2M3”, where M1, M2, and M3 each represent a conductive plate (or conductive layer, metal layer, metal plate), and I1 and I2 each represent an insulator (or dielectric layer). Therefore, the semiconductor device 100A provides two MOS capacitors, a first capacitor M1I1M2 and a second capacitor M2I2M3 connected in parallel. The combined capacitance C of the MOS capacitors provided in the first region R1 of the semiconductor device 100A is comp It is the sum of the capacitance of the first capacitor M1I1M2 and the capacitance of the second capacitor M2I2M3.

[0038] In the present embodiment, the conductive plate M1 corresponds to the silicide layer 26, the dielectric layer I1 corresponds to the first dielectric layer 32, the conductive plate M2 corresponds to the metal structure 36, the dielectric layer I2 corresponds to the second dielectric layer 46 (and the interface layer), and the conductive plate M3 corresponds to the conductive structure 48. In the prior art, MOS capacitors generally have an "M1IM2" structure, where "M1" generally corresponds to the semiconductor substrate of the MOS capacitor, "I" generally corresponds to an insulator (e.g., an oxide-containing gate dielectric layer), and "M2" generally corresponds to a metal gate structure. Therefore, forming an additional insulator (e.g., the second dielectric layer 46 and / or the interface layer 44) and an additional conductive plate (e.g., the conductive structure 48) in the stack S1, and forming a silicide layer (e.g., the silicide layer 26) below the stack S1 in contact with the stack S1, provides a method for increasing the capacitance of the MOS capacitor in a compact design, thereby improving the performance of the device without substantially increasing the planar size of the device.

[0039] In some embodiments, the semiconductor device 100A in the first region R1 further includes a plurality of contacts configured to couple components of the device with subsequently formed interconnect components (not depicted). Figure 2 , semiconductor device 100A may include source / drain contacts 54A and 54B coupled to respective source / drain regions 22 and gate contacts 58A and 58B each coupled to metal structure 36 and conductive structure 48, respectively. In some embodiments, source / drain contacts 54A and 54B are coupled to contact 50, which is electrically coupled to doped well 14 (e.g., doped layer 11).

[0040] refer to Figure 1 and Figure 4 , Figure 4 The second region R2 of the semiconductor device 100A is shown along Figure 1 In the cross-sectional view of line BB' of FIG. 1 , the second region R2 includes a stack S3 disposed above the silicide layer 26, wherein the stack S3 includes only the first dielectric layer 32 and the metal structure 36, but does not include the second dielectric layer 46, the interface layer 44, or the conductive structure 48. In this aspect, the stack S3 forms a MOS capacitor having a stacked structure of M1IM2 with the silicide layer 26. In some embodiments, the stack S3 allows the gate contact 58A to be coupled to the metal structure 36.

[0041] Figure 5 A top view of an embodiment of a semiconductor structure 200B is shown. The semiconductor structure 200B includes a device region 202B and a device region 204B, wherein the device region 202B includes a plurality of semiconductor devices 100B, and the device region 204B includes a plurality of semiconductor devices 150, as described above. In this embodiment, the semiconductor device 100B includes MOS capacitors that are similar in structure to those of the semiconductor device 100A described above.

[0042] Each semiconductor device 100B includes a third region R3 surrounded by a fourth region R4 that is different in structure from the third region R3, similar to the way the first region R1 is surrounded by the second region R2 in the semiconductor device 100A. Figure 5 and Figure 7 Described in Figure 7 The third region R3 is shown along Figure 5 In the cross-sectional view taken along line CC′ of FIG. 1 , the third region R3 includes a conductive structure 48 over the substrate 10 , and the fourth region R4 includes a metal structure 36 over the substrate 10 .

[0043] However, unlike the semiconductor device 100A, the third region R3 of the semiconductor device 100B includes a plurality of embedded structures 60A, 60B, and 60C in the doping layer 20, collectively referred to as embedded structures 60. Figure 5 and Figure 7 , the bottom portion of the silicide layer 26 and the bottom portion of the stack S1 (which include portions of the first dielectric layer 32 and the metal structure 36) extend into the doped layer 20 to form an embedded structure 60. In this respect, the embedded structure 60 is similar to a pillar enclosed in or surrounded by the doped layer 20.

[0044] In this embodiment, embedded structures 60A-60C provide additional surface area for at least one of the conductive plates M1, M2, and M3 in the MOS capacitor having the stacked structure M1I1M2I2M3 described in detail above. Figure 7 , the embedded structure 60 increases the surface area of ​​the silicide layer 26 (corresponding to M1) and the metal structure 36 (corresponding to M2). As described above, the composite capacitance C of the MOS capacitor having the stacked structure M1I1M2I2M3 is comp is the sum of the capacitance of the first capacitor M1I1M2 and the capacitance of the second capacitor M2I2M3. Therefore, by vertically extending the silicide layer 26 and the portion of the stack S1 into the doped layer 20 to form the embedded structure 60, the surface area of ​​the conductive plates M1 and M2 is increased, thereby increasing the capacitance of the first capacitor M1I1M2, and thus increasing the composite capacitance C of the MOS capacitor having the stacked structure M1I1M2I2M3. comp .

[0045] In the depicted embodiment, reference is still made to Figure 7 , each of the embedded structures 60 includes a depth D1 along the Z axis, a first width W1 along the X axis, and a second width W2 along the Y axis. In some embodiments, the depth D1 is substantially greater than at least the first width W1. In the present embodiment, the embedded structure 60 does not penetrate the doped layer 20, so that the depth D1 is less than the depth of the doped layer 20. In some instances, the depth D1 may be greater than 0 and less than about 300 nm. In some embodiments, the smaller of the first width W1 and the second width W2 (also referred to as the critical dimension (CD) of the semiconductor device 100B) is at least about 40 nm. In some embodiments, the sidewalls of the silicide layer 26, the first dielectric layer 32, and the metal structure 36 in each embedded structure 60 are substantially vertical along the Z axis, that is, exhibit little to no lateral deviation along the X axis. In some embodiments, the composite capacitance C comp The increase of is adjusted by adjusting the size of the embedded structure 60. For example, increasing the depth D1, the first width W1, the second width W2, or a combination thereof can increase the composite capacitance C of the MOS capacitor. comp .

[0046] In some embodiments, the aspect ratio (AR) (defined as the ratio of the depth D1 to the width W1 of each of the embedded structures 60) is about 1 to about 10. In some embodiments, an increase in the AR of the embedded structures 60 generally produces a higher capacitance between the conductive plates M1 and M2 (i.e., the silicide layer 26 and the metal structure 36). However, if the AR is too large (e.g., significantly greater than about 10), it may become challenging to obtain a trench having a desired size due to limitations associated with the photolithography and etching processes used to form such a trench.

[0047] In some embodiments, the depth D1 is greater than the depth D2 of the isolation structure 12, and the depth D2 is greater than the depth D3 of the source / drain region 22. In some embodiments, the depth D1 may be less than the depth D2. In some embodiments, the embedded structures 60 are formed to have different depths (e.g., depth D1), different widths (e.g., first width W1 and / or second width W2), or both. In addition, although three embedded structures 60 are depicted, the number of embedded structures 60 may vary between one and ten, including one and ten. In some embodiments, the number of embedded structures 60 is determined based on the width W3 of the stack S1 along the X-axis, wherein the embedded structures 60 are spaced apart along the width W3. A greater number of embedded structures 60 may be applied, as long as the size of each embedded structure 60 is allowed by the design rules for a given width W3 of the stack S1, and is not too high to adversely affect the process of manufacturing components of the semiconductor device 100B (including, for example, a metal filling (or deposition) process).

[0048] In some embodiments, reference Figure 5 , each of the embedded structures 60 has a columnar configuration, wherein the widths W1 and W2 are similar or substantially the same, such that each of the embedded structures 60 has a square shape in top view. Figure 6 , semiconductor device 100B includes embedded structures 61A, 61B, and 61C (collectively referred to as embedded structures 61), each having a configuration different from that of embedded structure 60. For example, embedded structures 61 each have a beam-shaped configuration, wherein second width W2 is substantially greater than first width W1, such that embedded structures 61 each have an elongated shape (e.g., a rectangular shape) in a top view. In this regard, embedded structures 61 are disposed along the length of conductive structure 48 (e.g., along the length of conductive structure 48) in third region R3. Figure 6 The Y-axis in FIG. 4 is elongated and has a width W3 (e.g., along the Y-axis in FIG. 4 ) of the conductive structure 48. Figure 7 It should be noted that since the embedded structures 60 and 61 are shown as having the same first width W1, as shown in FIG. Figure 5 and Figure 6 As described in Figure 7Also along Figure 6 An embodiment of a semiconductor device 100B including an embedded structure 61 is depicted in a cross-sectional view taken along line CC′ of FIG.

[0049] Figure 8 An embodiment of a semiconductor device 100B in region R3 is shown, which is similar to Figure 7 However, Figure 8 The semiconductor device 100B depicted in FIG. 1 includes an additional gate spacer 39 extending from the gate spacer 38 and contacting the sidewalls of the interface layer 44, the second dielectric layer 46, and the conductive structure 48. In this regard, Figure 7 The embodiment of the semiconductor device 100B depicted in FIG. Figure 2 An embodiment of a semiconductor device 100A depicted in FIG. Figure 8 The embodiment of the semiconductor device 100B depicted in FIG. Figure 3 An embodiment of a semiconductor device 100A is depicted in FIG.

[0050] In some embodiments, reference Fig. 9 , an embodiment of semiconductor device 100B includes embedded structures 62A, 62B, and 62C (collectively, embedded structures 62), which are similar to embedded structure 60, except that the surface of doped layer 20 in contact with embedded structure 62 exhibits roughness and corrugation. In this regard, portions of the sidewalls of silicide layer 26, first dielectric layer 32, and metal structure 36 in each embedded structure 62 extend or deviate laterally toward doped layer 20, such as Fig. 9 . In some non-limiting examples, such extension or deviation may be less than about 10% of a width W4 (e.g., along the X-axis) of the metal structure 36 in the embedded structure 62, wherein the width W4 is defined between two contour midlines extending vertically (e.g., along the Z-axis) through the surface roughness on opposite sidewalls of the metal structure 36. In some embodiments, such surface roughness causes a portion of the metal structure 36 to be embedded in the first dielectric layer 32 along the sidewalls of the embedded structure 62. In the present embodiment, the surface roughness of the embedded structure 62 is configured to further increase the surface area of ​​the conductive plates M1 and M2, which together increases the capacitance of the first capacitor M1, M1, M2 compared to the embedded structure 60.

[0051] FIG. 10A to FIG. 10CA flow chart of a method 300 of forming a semiconductor device 400 according to one or more embodiments of the present disclosure is shown. The semiconductor device 400 may be similar in part or in whole to the semiconductor devices 100A and 100B as described in detail above. In this regard, the method 300 is applicable to forming at least a portion of the semiconductor devices 100A and 100B, such as forming a first region R1 of the semiconductor device 100A and a third region R3 of the semiconductor device 100B. In some embodiments, the operations of the method 300 may be associated with a cross-sectional view of the semiconductor device 400 in a plane defined by axes X and Z at various stages of manufacture, such as Figures 11 to 23 It should be noted that method 300 is merely an example and is not intended to limit the disclosed embodiments. Therefore, it should be understood that the method 300 may be used in FIG. 10A to FIG. 10C Additional operations are provided before, during, and after method 300, and some other operations may only be briefly described herein.

[0052] refer to Fig. 10A and Fig.11 In operation 302 , a substrate 10 for a semiconductor device 400 is provided.

[0053] In some embodiments, Fig.11 As depicted in FIG. 4 , in operation 302, a doped well 14 is first formed in the substrate 10, wherein the doped well 14 includes a dopant having a conductivity type different from that of the semiconductor device 400. Subsequently, still referring to FIG. Fig. 10A and Fig.11 The doping layer (or impurity layer) 20 is formed in the doping well 14 , so that the doping well 14 surrounds the bottom surface and the sidewall surface of the doping layer 20 .

[0054] In some embodiments, the doped layer 20 is formed by implementing a series of patterning and doping processes. For example, a patterned mask layer (not depicted) can be formed above the doped well 14 to expose a portion of the doped well 14. The patterned mask layer may include a photoresist material that can be patterned using a photolithography technique. Typically, photolithography utilizes a photoresist material that is deposited, irradiated (or exposed) and developed to remove a portion of the photoresist material. The remaining photoresist material (which forms the patterned mask layer) protects the underlying material from subsequent processing steps, such as doping or etching. For example, the patterned mask layer may optionally or additionally include a dielectric material, such as an oxide, patterned by a photolithography technique. Then, a doping process is implemented on the exposed portion of the doped well 14 to form the doped layer 20. The doping process may be an implantation process, a diffusion process, etc. After the doping process is implemented, the patterned mask is removed from the semiconductor device 400 by any suitable process, such as plasma ashing or resist stripping.

[0055] Still reference Fig.11In operation 302, a plurality of isolation structures 12 are formed in the doped well 14 adjacent to the doped layer 20. The isolation structure 12 may be formed by patterning a mask layer (not depicted) to expose portions of the doped well 14 located between adjacent doped layers 20. The mask layer may be patterned by a photolithography process similar to that described above with respect to forming the doped layer 20, and a subsequent etching process using the patterned mask layer as an etching mask to form trenches (not depicted) penetrating the doped well 14. The etching process may include dry etching, wet etching, reactive ion etching (RIE), etc., or a combination thereof. Subsequently, at least one dielectric layer is deposited in the trenches by any suitable process, such as high density plasma CVD (HDPCVD), flowable CVD (FCVD) (e.g., CVD-based material deposition in a remote plasma system, followed by an annealing or curing process to densify the deposited material into another material, such as an oxide), spin coating, etc., or a combination thereof. Other dielectric materials and / or other formation processes may be used to form the isolation structure 12. Subsequently, a planarization process, such as a chemical mechanical polishing / planarization (CMP) process, may be performed to remove any excess material of the at least one dielectric layer. The patterned mask layer may also be removed by the planarization process or by any other suitable process.

[0056] In some embodiments, a doped layer 11 is then formed in the doped well 14 adjacent to the isolation structure 12 (eg, see Figures 2 to 4 ). The doping layer 11 may be formed by a series of patterning and doping processes similar to those described above with respect to forming the doping layer 20. In some embodiments, the doping layer 11 is omitted.

[0057] refer to Fig. 10A and Fig.11 , in operation 304, source / drain regions 22 are formed in the doped layer 20. The source / drain regions 22 may be formed by any suitable doping process, such as an implantation process or a diffusion process. In some embodiments, a patterned mask layer (not depicted) is first formed over the substrate 10 to expose portions of the doped layer 20 corresponding to locations of the source / drain regions 22. The method of forming the patterned mask layer is similar to the method described above for forming the patterned mask layer for the doped layer 20. Subsequently, a suitable doping process is performed to introduce an n-type dopant into the exposed portion of the doped layer 20, thereby producing the source / drain regions 22. After the doping process is performed, the patterned mask layer is removed by any suitable process described herein.

[0058] In some embodiments, although not depicted, forming the source / drain region 22 includes a series of etching and epitaxial processes. For example, a portion of the doped layer 20 corresponding to the location of the source / drain region 22 is first removed in an etching process (e.g., using a patterned mask) to form a source / drain recess. Subsequently, one or more epitaxial processes are performed to grow the source / drain region 22 in the source / drain recess. The epitaxial growth process can be implemented using any suitable process, such as metal organic CVD (MOCVD), molecular beam epitaxy (MBE), liquid phase epitaxy (LPE), vapor phase epitaxy (VPE), selective epitaxial growth (SEG), etc., or a combination thereof.

[0059] refer to Fig. 10A and Fig.12 In operation 306 , trenches 24A, 24B, and 24C are formed in the doped layer 20 .

[0060] In the present embodiment, trenches 24A-24C are formed along the X-axis in a region of doped layer 20 between source / drain regions 22, wherein each of trenches 24A-24C is embedded in doped layer 20. In this regard, trenches 24A-24C do not extend through the entire thickness of doped layer 20, such that a bottom surface of each of trenches 24A-24C is separated from underlying doped well 14 by portions of doped layer 20.

[0061] In some embodiments, the grooves 24A-24C are formed to have a first width W1 along the X-axis, a second width W2 along the Y-axis (see, for example, Figure 5 and Figure 6 ) and a depth D1 along the Z axis. In some embodiments, the first width W1 (also referred to as the critical dimension (CD) of the semiconductor device 400) is at least about 40 nm. In some embodiments, the trenches 24A-24C are formed to have different depths, different widths, or both. In addition, although Fig.12 Three trenches are depicted in FIG. 3 , but the number of trenches may vary between one and ten, inclusive. A higher number of trenches is possible, as long as the number of trenches is permitted by design rules and is not too high to adversely affect subsequent operations of method 300 (such as metal filling (or deposition) processes). In some embodiments, trenches 24A-24C are formed in a columnar configuration to provide a Figure 5 In some embodiments, the grooves 24A-24C are formed in a beam-shaped configuration to provide Figure 6 The embedded structure 61 depicted in .

[0062] The grooves 24A-24C can be formed by a series of patterning and etching processes. For example, a patterned mask (not depicted) including openings corresponding to the positions of the grooves 24A-24C is formed above the semiconductor device 400. The method of forming such a patterned mask is similar to the method described above for forming a patterned mask layer for the doped layer 20. The patterned mask layer is then used as an etching mask to remove portions of the doped layer 20 by a suitable etching process 502, such as a dry etching process (or a plasma etching process). The duration of the etching process 502 can be controlled to form the grooves 24A-24C to a depth D1. After the grooves 24A-24C are formed, the patterned mask layer is removed from the semiconductor device 400 by any suitable process, such as plasma ashing or resist stripping.

[0063] refer to Fig. 10A and Fig.13 In operation 308 , a silicide layer 26 is formed over the doped layer 20 , including over the source / drain regions 22 .

[0064] In the present embodiment, the silicide layer 26 is formed over the silicon-containing semiconductor surface of the semiconductor device 400. For example, the silicide layer 26 is formed over the top surface of the doped layer 20, the sidewalls and bottom surface of the doped layer 20 exposed in the trenches 24A-24C, and the source / drain regions 22. In this regard, the silicide layer 26 is not formed over the isolation structure 12.

[0065] The silicide layer 26 can be formed by any suitable process. For example, the silicide layer 26 can be formed by depositing a metal-containing precursor in the presence of a gas using a suitable deposition technique (such as CVD). In some embodiments, the deposition process is implemented at an elevated temperature. The metal-containing precursor may include TiCl4, WCl5, MoCl5, Ni(CO)4, Co2(CO6)[HCC(C(CH3)3)], etc. or a combination thereof, and the gas may include hydrogen (H2), argon (Ar), or a combination thereof. Subsequently, the deposited metal-containing precursor reacts with silicon in the doped layer 20 and the source / drain region 22 to form the silicide layer 26. After the silicidation process is completed, any unreacted metal, such as Ti, W, Mo, Ni, Co, etc., may be removed from the metal-containing precursor.

[0066] refer to Fig. 10A and Fig.14 In operation 310 , a first dielectric layer 32 is formed over the substrate 10 .

[0067] In the present embodiment, the first dielectric layer 32 is deposited as a blanket layer (not depicted) over the semiconductor device 400. For example, portions of the first dielectric layer 32 are formed over the silicide layer 26 inside and outside the trenches 24A-24C. In this regard, the first dielectric layer 32 and the silicide layer 26 partially fill the trenches 24A-24C. The first dielectric layer 32 may be formed by any suitable deposition technique, such as chemical oxidation, thermal oxidation, CVD, atomic layer deposition (ALD), physical vapor deposition (PVD), etc., or a combination thereof.

[0068] refer to Fig. 10A and Fig.14 In operation 312 , a dummy gate structure 35 including a first dielectric layer 32 and a dummy gate electrode 33 is formed over the trenches 24A- 24C.

[0069] The dummy gate electrode 33 may include any suitable material, such as a polysilicon layer, and may be formed over the semiconductor device 400 as a blanket layer (not depicted). In the present embodiment, the dummy gate electrode 33 completely fills the trenches 24A-24C. Fig.14 Described in.

[0070] Subsequently, the dummy gate electrode 33 and the first dielectric layer 32 are patterned to form a dummy gate structure 35. The dummy gate structure 35 can be formed by a series of patterning and etching processes similar to those used to form the trenches 24A-24C. For example, a patterned mask layer (not depicted) is first formed over the dummy gate electrode 33 as an etching mask. An etching process, such as a dry etching process or a wet etching process, is performed to remove the portions of the dummy gate electrode 33 and the first dielectric layer 32 exposed by the patterned mask layer, wherein the dummy gate structure 35 remains above the doped layer 20. After the etching process is performed, the patterned mask layer is removed by any suitable process, such as plasma ashing or resist stripping.

[0071] In the present embodiment, the dummy gate structure 35 is interposed between the source / drain regions 22 and extends laterally (e.g., along the X-axis) over the trenches 24A-24C by a width W3. Thus, the dummy gate structure 35 includes a top portion 35D over bottom portions 35A, 35B, and 35C, which correspond to the trenches 24A, 24B, and 24C, respectively. In this regard, the bottom portions 35A-35C are extensions of the dummy gate structure 35 that are embedded in the doped layer 20.

[0072] refer to Fig. 10A and Fig.14 In operation 314 , a gate spacer 38 is formed along the sidewall of the dummy gate electrode 33 .

[0073] The gate spacer 38 can be formed by: first conformally depositing a dielectric layer over the dummy gate structure 35 using any suitable deposition process, such as thermal oxidation, CVD, etc.; and then using a suitable etching process, such as a directional or anisotropic dry etching process, to remove a portion of the dielectric layer, leaving the gate spacer 38 along the sidewall of the dummy gate structure 35.

[0074] refer to Fig. 10A and Fig.15 In operation 316 , an interlayer dielectric (ILD) layer 42 is formed over the dummy gate structure 35 and the source / drain regions 22 .

[0075] The ILD layer 42 may include any suitable dielectric material, such as silicon oxide, a low-k dielectric material, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), etc., or a combination thereof, and may be deposited by any suitable method, such as CVD, PECVD, FCVD, etc. Subsequently, a planarization process, such as a CMP process, is performed to remove a portion of the ILD layer 42 from the top surface of the dummy gate structure 35 , so that the ILD layer 42 remains above the sidewalls of the gate spacers 38 and the top surfaces of the source / drain regions 22 .

[0076] In some embodiments, before forming the ILD layer 42, a contact etch stop layer (CESL; not depicted) is formed over the semiconductor device 400. The ILD layer 42 and the CESL include different materials to provide etching selectivity therebetween in subsequent manufacturing processes. The CESL may include any suitable dielectric material, such as silicon nitride, silicon oxynitride, silicon oxide, etc., or a combination thereof, and may be formed by a suitable formation method, such as CVD, ALD, PVD, etc., or a combination thereof.

[0077] refer to Fig. 10A and Fig.15 In operation 318 , the dummy gate structure 35 is removed from the semiconductor device 400 , thereby creating gate trenches 37 between the gate spacers 38 .

[0078] In some embodiments, the dummy gate structure 35 is removed by one or more etching processes, such as a dry etching process or a wet etching process, to form a gate trench 37 between the gate spacers 38. In this regard, the bottom portions 35A-35C are partially removed to expose the first dielectric layer 32 in the trenches 24A-24C. In some embodiments, when etching the dummy gate electrode 33, the first dielectric layer 32 serves as an etch stop layer. In this embodiment, the first dielectric layer 32 remains in the trenches 24A-24C, as shown in FIG. Fig.15 Described in.

[0079] In some embodiments, the method 300 continues from operation 318 to operation 330 to form a semiconductor device 400, such as Fig. 10B Depicted in . Reference Fig. 10B and Fig.16 In operation 330 , a metal structure 36 is formed over the first dielectric layer 32 to partially fill the gate trench 37 .

[0080] In the present embodiment, the bottom portion of the metal structure 36 is formed over the first dielectric layer 32 to completely fill the trenches 24A-24C, and the top portion of the metal structure 36 is formed in the gate trench 37 without completely filling the gate trench 37. The metal structure 36, the first dielectric layer 32, and the bottom portion of the silicide layer 26 located in the trenches 24A-24C form embedded structures 60A-60C, respectively, similar to Figure 7 In addition, a portion of metal structure 36 is formed over a top surface of ILD layer 42 .

[0081] In the present embodiment, the metal structure 36 is configured as a metal gate structure. Therefore, the metal structure 36 includes at least a metal gate electrode. In some embodiments, the metal gate structure further includes one or more work function metal layers, each having a compound metal or a single metal. The various layers of the metal structure 36 can be formed by any suitable deposition process, such as CVD, PVD, ALD, plating (e.g., electroplating, chemical plating, etc.), etc., or a combination thereof.

[0082] refer to Fig. 10B and Fig.17 In operation 332 , a second dielectric layer 46 is formed over the portion of the metal structure 36 in the gate trench 37 .

[0083] In the present embodiment, the second dielectric layer 46 is deposited as a blanket layer (not depicted) over the semiconductor device 400. For example, a portion of the second dielectric layer 46 is conformally formed over the metal structure 36 in the gate trench 37, and a portion of the second dielectric layer 46 is formed over the ILD layer 42. In this regard, the second dielectric layer 46 and the metal structure 36 partially fill the gate trench 37, and a portion of the second dielectric layer 46 is formed along the sidewalls of the gate spacer 38. The second dielectric layer 46 may be formed by any suitable deposition technique, such as CVD, ALD, PVD, etc., or a combination thereof.

[0084] In some embodiments, an interfacial layer 44 is formed over the metal structure 36 before forming the second dielectric layer 46. Similar to the second dielectric layer 46, the interfacial layer 44 is deposited over the semiconductor device 400 as a blanket layer (not depicted) such that a portion of the interfacial layer 44 is conformally formed over the metal structure 36 in the gate trench 37, and a portion of the interfacial layer 44 is formed over the ILD layer 42. In this regard, a portion of the interfacial layer 44 is formed along the sidewalls of the gate trench 37 between the sidewalls of the second dielectric layer 46 and the sidewalls of the gate spacers 38. The second dielectric layer 46 may be formed by any suitable deposition technique, such as CVD, ALD, PVD, etc., or a combination thereof.

[0085] refer to Fig. 10B and Fig.17 In operation 334 , a conductive structure 48 is formed over the second dielectric layer 46 to fill the gate trench 37 .

[0086] In some embodiments, the conductive structure 48 is configured as a metal gate structure, similar to the metal structure 36 described in detail above. In the present embodiment, the conductive structure 48 is formed as a blanket layer (or multiple layers; not depicted) over the semiconductor device 400. For example, a portion of the conductive structure 48 is formed over the second dielectric layer 46 to completely fill the gate trench 37, and a portion of the conductive structure 48 is formed over the second dielectric layer 46 on the top surface of the ILD layer 42. In this regard, after forming the conductive structure 48, a CMP process is performed to planarize the top surfaces of the conductive structure 48, the second dielectric layer 46, and the interface layer 44 and the ILD layer 42, as shown in FIG. Fig.17 Thus, in the resulting stack S1 , the second dielectric layer 46 and the interface layer 44 are configured to have a U-shape, each surrounding the bottom surface and the sidewall surface of the conductive structure 48 .

[0087] In some embodiments, reference Fig.18Instead of forming trenches 24A-24C in operation 306, where the sidewalls of trenches 24A-24C are substantially smooth and vertical, trenches 25A-25C are formed in operation 306 using an etching process 504 that is different from etching process 502. For example, after forming a patterned mask layer over doped layer 20 between source / drain regions 22, an etching process 504 using a periodically oscillating plasma of different composition is performed to produce roughness along the sidewalls and bottom surfaces of trenches 25A-25C. In some embodiments, performing etching process 504 includes alternately applying an etching gas (i.e., a first plasma) and a protective gas (i.e., a second plasma) over semiconductor device 400. The etching gas is configured to remove portions of doped layer 20 to form and deepen trenches 25A-25C, and the protective gas is configured to deposit a polymer (or passivation) layer over etched surfaces (e.g., sidewall surfaces) of trenches 25A-25C. The etching gas and the protective gas are cyclically applied to deepen the trenches 25A-25C, thereby causing the surface exposed in the trenches 25A-25C to exhibit roughness. In some embodiments, the surface roughness increases the surface area of ​​the doped layer 20 exposed in the trenches 25A-25C, which in turn increases the surface area of ​​the embedded structures 62A-62C formed in the trenches 25A-25C, respectively, similar to Fig. 9 The semiconductor device 100B is depicted in FIG.

[0088] Subsequently, operations 308-318 and 330-334 are performed in a manner similar to those described above, thereby producing a semiconductor device 400 including embedded structures 62A-62C corresponding to trenches 25A-25C, respectively. Fig.19 In the present embodiment, embedded structures 62A- 62C (collectively referred to as embedded structures 62 ) each include silicide layer 26 , first dielectric layer 32 , and a bottom portion of metal structure 36 .

[0089] In some embodiments, the method 300 continues from operation 318 to operation 350 to form a semiconductor device 400, such as Fig. 10C Depicted in . Reference Fig. 10C and Fig. 20 In operation 350 , a metal structure 36 is formed over the first dielectric layer 32 to completely fill the gate trench 37 .

[0090] In the present embodiment, the metal structure 36 is formed in a process similar to that described above with respect to operation 330. For example, a bottom portion of the metal structure 36 is formed over the first dielectric layer 32 to completely fill the trenches 24A-24C, respectively creating embedded structures 60A-60C extending into the doped layer 20 and laterally interposed between the source / drain regions 22. However, unlike operation 330, a top portion of the metal structure 36 completely fills the gate trench 37. In this regard, the process of depositing the metal structure 36 is terminated when a blanket layer (not depicted) of the metal structure 36 completely fills the gate trench 37. The metal structure 36 is then planarized with the ILD layer 42 by a CMP process, such as Fig. 20 Described in.

[0091] refer to Fig. 10C and Fig.21 In operation 352 , a second dielectric layer 46 is formed over the metal structure 36 and the ILD layer 42 .

[0092] In the present embodiment, second dielectric layer 46 is deposited as a blanket layer over metal structure 36 and ILD layer 42. In some embodiments, an interfacial layer is deposited over metal structure 36 and ILD layer 42 prior to depositing second dielectric layer 46. Second dielectric layer 46 and interfacial layer 44 may be formed in a process similar to that described above with respect to operation 332.

[0093] refer to Fig. 10C and Fig.21 In operation 354, a conductive structure 48 is formed over the second dielectric layer 46, resulting in a stack S2. In this embodiment, the conductive structure 48 is formed over the second dielectric layer 46 as a blanket layer by a process similar to that described above with respect to operation 334.

[0094] refer to Fig. 10C and Fig. 22 , in operation 356 , stack S2 is patterned so that their sidewalls are aligned with those of underlying metal structures 36 .

[0095] In some embodiments, the stack S2 including the conductive structure 48 and the second dielectric layer 46 and the interface layer 44 is patterned by a series of photolithography and etching processes. For example, a patterned mask layer (not depicted) including openings corresponding to the portions of the stack S2 to be removed is formed above the semiconductor device 400. The method of forming such a patterned mask layer is similar to the method described above for forming the doped layer 20. Then, using the patterned mask layer as an etching mask, portions of the stack S2 are removed by a suitable etching process, such as a dry etching process (or a plasma etching process). The etching process terminates when the underlying ILD layer 42 is exposed. After patterning the stack S2, the patterned mask layer is removed from the semiconductor device 400 by any suitable process, such as plasma ashing or resist stripping.

[0096] refer to Fig. 10C and Fig. 22 In operation 358, gate spacers 39 are then formed along sidewalls of patterned stack S2, which includes patterned conductive structure 48, patterned second dielectric layer 46, and patterned interface layer 44, such that gate spacers 39 extend vertically from gate spacers 38. In this regard, gate spacers 38 and gate spacers 39 are collectively referred to as gate spacers 40.

[0097] In some embodiments, the gate spacer 39 is configured as a dielectric seal around the sidewalls of the patterned conductive structure 48, the patterned second dielectric layer 46, and the patterned interface layer 44, thereby isolating these layers from subsequently formed components. In this regard, the gate spacer 39 may alternatively be referred to as a dielectric seal 39. In some embodiments, the gate spacer 39 and the gate spacer 38 have the same composition. In some embodiments, the gate spacer 39 and the gate spacer 38 have different compositions. The gate spacer 39 can be formed by a process similar to that of forming the gate spacer 38 in operation 314.

[0098] For an embodiment in which trenches 25A-25C are formed by etching process 504 in operation 306, as shown in FIG. Fig.18 As depicted in FIG. 4 , operations 308 - 318 and 350 - 358 are then performed in a manner similar to that described above to form a semiconductor device 400 including embedded structures 62A- 62C, such as Fig.23 Described in.

[0099] In some embodiments, although not depicted, operation 306 is omitted, such that no trenches are formed in doped layer 20. In other words, subsequent layers (e.g., silicide layer 26, first dielectric layer 32, metal structure 36, and conductive structure 48) are formed completely above the top surface of doped layer 20, rather than being partially embedded within doped layer 20. Figure 2An exemplary embodiment without any trenches is depicted in FIG. 4 , which corresponds to an embodiment of a semiconductor device 400 formed by operations 308 - 318 and 330 - 334 and in FIG. Figure 3 , which corresponds to an embodiment of a semiconductor device 400 formed by operations 308 - 318 and 350 - 358 .

[0100] In this embodiment, Fig.17 The embodiment of the semiconductor device 400 depicted in FIG. 4 (wherein the optional doping layer 11 is omitted for simplicity) corresponds to Figure 7 The semiconductor device 100B; Fig.19 The embodiment of the semiconductor device 400 depicted in Fig. 9 The semiconductor device 100B in; and Fig. 22 The embodiment of the semiconductor device 400 depicted in Figure 8 The semiconductor device 100B in FIG.

[0101] In implementing FIG. 10A to FIG. 10C , additional operations may be performed. For example, additional ILD layers (not depicted) may be formed over the conductive structure 48 and the ILD layer 42. Furthermore, various contacts, such as the substrate contact 50, the source / drain contacts 54A and 54B, the gate contact 58A, and the gate contact 58B, are formed to electrically couple to portions of the doped well 14, the source / drain regions 22, and the metal structure 36, and the conductive structure 48, respectively.

[0102] One aspect of the specification relates to a semiconductor structure. The semiconductor structure includes a substrate and a silicide layer above the substrate. The semiconductor structure includes a first dielectric layer above the silicide layer. The semiconductor structure includes a first metal structure above the first dielectric layer. The semiconductor structure includes a second dielectric layer above the first metal structure. The semiconductor structure also includes a conductive structure above the second dielectric layer.

[0103] Another aspect of the specification relates to a semiconductor structure. The semiconductor structure includes a substrate and a capacitor above the substrate. The capacitor includes a silicide layer above the substrate. The capacitor includes a first dielectric layer above the silicide layer. The capacitor includes a metal gate structure above the first dielectric layer, wherein a top portion of the metal gate structure is located above the substrate and a bottom portion of the metal gate structure extends into the substrate. The capacitor includes a second dielectric layer above the metal gate structure. The capacitor also includes a metal structure above the second dielectric layer.

[0104] Another aspect of the specification relates to a method for manufacturing a semiconductor structure. The method includes providing a substrate including a doped region. The method includes patterning the doped region to form a trench. The method includes forming a silicide layer in the trench. The method includes forming a first dielectric layer above the silicide layer. The method includes forming a dummy gate above the first dielectric layer, the dummy gate having a bottom portion filling the trench and a top portion above the bottom portion. The method includes forming a gate spacer along a sidewall of the dummy gate. The method includes replacing the dummy gate with a metal gate. The method includes forming a second dielectric layer above the metal gate. The method also includes forming a metal structure above the second dielectric layer.

[0105] Some embodiments of the present application provide a semiconductor structure, comprising: a substrate; a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal structure located above the first dielectric layer, wherein the metal structure comprises a gate electrode; a second dielectric layer located above the metal structure; and a conductive structure located above the second dielectric layer.

[0106] In some embodiments, the metal structure includes a first portion located above the substrate and a plurality of second portions embedded in the substrate.

[0107] In some embodiments, the silicide layer and the first dielectric layer are located between the first portion of the metal structure and the substrate, and between the plurality of second portions of the metal structure and the substrate.

[0108] In some embodiments, the substrate includes a doped region embedding the plurality of second portions.

[0109] In some embodiments, each of the plurality of second portions of the metal structure has a rough surface.

[0110] In some embodiments, the second dielectric layer traverses the bottom surface and sidewall surfaces of the conductive structure.

[0111] In some embodiments, the second dielectric layer only crosses the bottom surface of the conductive structure but does not cross the sidewall surface of the conductive structure.

[0112] In some embodiments, the semiconductor structure further includes spacers along sidewalls of the metal structure and the conductive structure.

[0113] Other embodiments of the present application provide a semiconductor structure, including: a substrate; and a capacitor located above the substrate, including: a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal gate structure located above the first dielectric layer, wherein a top portion of the metal gate structure is located above the substrate and a bottom portion of the metal gate structure extends into the substrate; a second dielectric layer located above the metal gate structure; and a conductive structure located above the second dielectric layer.

[0114] In some embodiments, the bottom portion of the metal gate structure includes at least one pillar structure surrounded by the first dielectric layer and the silicide layer.

[0115] In some embodiments, the bottom portion of the metal gate structure has a rough surface.

[0116] In some embodiments, the metal gate structure includes at least one work function metal layer.

[0117] In some embodiments, the second dielectric layer includes a high-k dielectric material.

[0118] In some embodiments, the semiconductor structure further includes: a third dielectric layer located between the metal gate structure and the second dielectric layer, wherein the third dielectric layer has a composition different from that of the second dielectric layer.

[0119] In some embodiments, the substrate includes: a doped region surrounding the bottom portion of the metal gate structure; and a source / drain region disposed in the doped region, wherein the bottom portion of the metal gate structure is between the source / drain regions, and wherein the silicide layer extends above the source / drain regions.

[0120] Still other embodiments of the present application provide a method for manufacturing a semiconductor structure, comprising: providing a substrate including a doped region; patterning the doped region to form a trench; forming a silicide layer in the trench; forming a first dielectric layer above the silicide layer; forming a dummy gate above the first dielectric layer, the dummy gate having a bottom portion filling the trench and a top portion located above the bottom portion; forming a gate spacer along the sidewall of the dummy gate; replacing the dummy gate with a metal gate; forming a second dielectric layer above the metal gate; and forming a conductive structure above the second dielectric layer.

[0121] In some embodiments, replacing the dummy gate includes: removing the dummy gate to form a gate trench between the gate spacers; and partially filling the gate trench with the metal gate, thereby forming a portion of the second dielectric layer along the sidewalls of the gate spacers in the gate trench, and forming the conductive structure and then filling the gate trench.

[0122] In some embodiments, partially filling the gate trench with the metal gate includes: forming a work function metal layer on the first dielectric layer; and forming a gate electrode over the work function metal layer.

[0123] In some embodiments, the gate spacer is a first gate spacer, and wherein the second dielectric layer and the conductive structure are formed across a top surface of the first gate spacer, the method further comprising: etching the conductive structure and the second dielectric layer; and forming a second gate spacer along side walls of the etched conductive structure and the etched second dielectric layer, such that the second gate spacer extends from the first gate spacer.

[0124] In some embodiments, the method further includes: forming source / drain regions in the doped regions, wherein the trench is formed in a portion of the doped regions between the source / drain regions.

[0125] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the embodiments of the present disclosure. Those skilled in the art should understand that they can easily use the embodiments of the present disclosure as a basis to design or modify other processes and structures for performing the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also appreciate that such equivalent configurations do not deviate from the spirit and scope of the embodiments of the present disclosure, and that they can make various changes, substitutions, and modifications herein without departing from the spirit and scope of the embodiments of the present disclosure.

Claims

1. A semiconductor structure, include: substrate; a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal structure located above the first dielectric layer, wherein the metal structure includes a gate electrode; a second dielectric layer located above the metal structure; and The conductive structure is located above the second dielectric layer.

2. The semiconductor structure according to claim 1, in, The metal structure includes a first portion located above the substrate and a plurality of second portions embedded in the substrate.

3. The semiconductor structure according to claim 2, in, The silicide layer and the first dielectric layer are located between the first portion of the metal structure and the substrate, and between the plurality of second portions of the metal structure and the substrate.

4. The semiconductor structure according to claim 2, in, The substrate includes a doped region embedding the plurality of second portions.

5. The semiconductor structure according to claim 2, in, Each of the plurality of second portions of the metal structure has a rough surface.

6. The semiconductor structure according to claim 1, in, The second dielectric layer traverses the bottom surface and sidewall surfaces of the conductive structure.

7. The semiconductor structure according to claim 1, in, The second dielectric layer only crosses the bottom surface of the conductive structure but does not cross the sidewall surface of the conductive structure.

8. The semiconductor structure of claim 1 further comprising spacers along sidewalls of the metal structure and the conductive structure.

9. A semiconductor structure, include: substrate; as well as A capacitor, located above the substrate, comprises: a silicide layer located above the substrate; a first dielectric layer located above the silicide layer; a metal gate structure located above the first dielectric layer, wherein a top portion of the metal gate structure is located above the substrate and a bottom portion of the metal gate structure extends into the substrate; a second dielectric layer located above the metal gate structure; and The conductive structure is located above the second dielectric layer.

10. A method of manufacturing a semiconductor structure, include: providing a substrate including a doped region; patterning the doped region to form a trench; forming a silicide layer in the trench; forming a first dielectric layer over the silicide layer; forming a dummy gate over the first dielectric layer, the dummy gate having a bottom portion filling the trench and a top portion over the bottom portion; forming a gate spacer along a sidewall of the dummy gate; replacing the dummy gate with a metal gate; forming a second dielectric layer over the metal gate; as well as A conductive structure is formed over the second dielectric layer.