Manufacturing method of carbon dioxide near-dry fracturing fracture net model

The method of decomposing plant fibers by microorganisms to generate complex slit nets in the core, which solves the problem that the existing technology cannot effectively simulate CO2 quasi-drying method fracturing nets, and realizes the formation of highly complex slit nets without damaging the core. Meet the simulation requirements of seam model after CO2 quasi-dry fracturing.

CN118990738APending Publication Date: 2024-11-22SINOPEC OILFIELD SERVICE CORPORATION +2
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310555632.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-17
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing fracturing mesh model manufacturing method cannot effectively simulate the complex fracturing pattern after CO2 quasi-drying method, and the existing method has limited seam-making capabilities and cannot meet the requirements of CO2 quasi-drying method.

Method used

Using a method based on microbial decomposition of plant fibers, by mixing quartz sand and cement and laying them in the core mold, different sizes of conical cellulose fibers are added, and cellulose decomposition bacteria are used to decompose cellulose fibers to form main cracks and branch joints. , and then sterilize and inject proppant to prepare a core that meets the CO2 quasi-drying method fracturing mesh model.

Benefits of technology

It is achieved that highly complex seam networks are generated in situ without damaging the physical and chemical properties of the core, and the seam network pattern can be controlled to meet the seam network model simulation requirements after CO2 quasi-dry fracturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004233003330000041
    Figure BDA0004233003330000041
  • Figure HDA0004233003340000011
    Figure HDA0004233003340000011
  • Figure HDA0004233003340000012
    Figure HDA0004233003340000012
Patent Text Reader

Abstract

The invention belongs to the field of exploration and development of oil and gas fields, and discloses a method for manufacturing a carbon dioxide near-dry fracturing crack net model, which specifically comprises the following steps of: stirring quartz sand, cement and clear water into a uniform mixture, inserting an iron wire wound with a preservative film into a bottom plate fixing hole, alternately placing the mixture and plant fibers into a mold, and forming a mold; the top plate is sealed after the inner cavity is filled with the mixture; pulling out the iron wire and the preservative film to form a main crack, and injecting a bacterial liquid containing plant fiber decomposition bacteria into the formed main crack; discharging the bacterial liquid, and injecting a bactericide into the main crack; after the rock core is cleaned, quartz sand with different mesh numbers is injected into the rock core in sequence to fill a main crack, a branch crack and a branch crack, and a sand-filled crack with high flow conductivity is formed; according to the method, based on the plasticity of the plant fibers, the plant fibers of different sizes are freely spread in the mixture, fracturing fracture net models of different complexity degrees can be designed, pollution to the rock core is small, and the influence is small.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of oil and gas field exploration and development, and in particular relates to a method for manufacturing a carbon dioxide quasi-dry method fracturing network model. Background Art

[0002] At present, the conventional fracturing methods used in oil and gas exploration mainly include: oil-based fracturing, water-based fracturing and carbon dioxide dry fracturing, and further developed quasi-dry fracturing methods. Quasi-dry fracturing technology is to mix a certain proportion of liquid CO2 and clean water, and add CO2-based and clean water-based thickeners to form a mixed phase liquid with a certain viscosity, which is injected with a large displacement through a ground high-pressure pump to press open the formation to form a dynamic crack, and then fill the dynamic crack with sand; after the construction is completed, it can provide a highly permeable seepage channel for the outflow of oil and gas, thereby achieving the purpose of increasing production and transformation.

[0003] In the prior art, a Chinese patent document with publication number CN 111363533 A discloses a fracturing fluid used in a normal pressure sand mixing quasi-dry fracturing method. When the normal pressure sand mixing quasi-dry fracturing fluid is used as a drag reducing fluid, the mass fraction of the dry fracturing fluid thickener system material in the liquid CO2 phase is 0.1-0.5%, and the mass fraction of the water-based fracturing fluid thickener system material in the water phase is 0.1-0.5%; the viscosity of the normal pressure sand mixing quasi-dry fracturing fluid is 1-20 mPa·s, the drag reduction rate is ≥60%, and the sand ratio is 0-10%. When the atmospheric pressure mixed sand quasi-dry fracturing fluid is used as a sand-carrying fluid, the mass fraction of the dry fracturing fluid thickener system material in the liquid CO2 phase is 0.5% to 3%, and the mass fraction of the water-based fracturing fluid thickener system material in the water phase is 0.5% to 3%; the viscosity of the atmospheric pressure mixed sand quasi-dry fracturing fluid is 50 to 200 mPa·s, 160℃&170s -1 Shear viscosity for 2h ≥20mPa·s, sand ratio of 5% to 45%, core damage rate ≤10%, anti-swelling rate ≥80%, and flowback rate ≥50%.

[0004] Another example: A Chinese patent document with publication number CN 114909117 A discloses a CO2 low-water fracturing fluid system and a supercritical CO2 quasi-dry sand fracturing method, wherein the CO2 low-water fracturing fluid system is composed of 20%-25% water-based fracturing fluid and 75%-80% liquid CO2, and the system is composed of liquid CO2, fracturing fluid, sand-carrying fluid and displacement fluid. Among them, liquid CO2 is used to be injected into the formation before fracturing and seaming to pretreat the formation; the fracturing fluid is used to be injected into the formation for fracturing and seaming, including CO2 low-water fracturing fluid and filter reduction plugs, which are used to be alternately injected into the formation; the filter reduction plugs are composed of CO2 low-water fracturing fluid and proppant; the sand-carrying fluid is used to be injected into the formation after seam formation to play a supporting role, and is composed of CO2 low-water fracturing fluid and proppant; the displacement fluid is used to replace the liquid in the formation.

[0005] Compared with hydraulic fracturing, the advantages of CO2 quasi-dry fracturing include: (1) inhibiting clay expansion and reducing reservoir damage; (2) connecting the reservoir and easily forming a fracture network; (3) when the reservoir is supersaturated with carbon dioxide, it can change the contact angle between the fluid and the capillary or rock wall, the diameter of the capillary and the chemical adsorption of the formation pores, effectively changing the capillary parameters, which is beneficial to post-fracturing flowback; (4) dissolving in crude oil and reducing crude oil viscosity; (5) replacing methane and increasing gas well production. Compared with pure CO2 fracturing, the advantages of CO2 quasi-dry fracturing include: (1) no special closed sand mixing equipment is required; (2) integrated application of drag reduction and sand carrying; (3) quasi-dry fracturing fluid is a structured fluid with good viscoelasticity and excellent temperature and shear resistance; (4) a small amount of water phase is used to prepare a water-based sand-carrying fluid, which has low or even no damage, excellent production increase effect and high cost performance.

[0006] Fresh water fracturing will produce vertical main cracks along the wellbore in the fracturing layer, and there are undeveloped branch cracks and sprawling branch cracks on the main cracks, and the crack tortuosity is small; supercritical CO2 fracturing will form cracks along the rift or bedding plane in the fracturing layer, and the number of crack branches obtained is greater than that of fresh water fracturing, and the crack tortuosity is higher, and the cracks formed are longer, but there are no developed main cracks. CO2 quasi-dry fracturing has the main characteristics of fresh water fracturing and supercritical CO2 fracturing. It forms main channel cracks along the direction of maximum principal stress, and forms branch cracks within a certain range around the main cracks by relying on the high fluidity of carbon dioxide.

[0007] Research on the law of gas seepage in shale fractures is mainly based on small plug-shaped rock samples after artificial fractures. The common methods for making fracture cores after fractures are mainly: splitting fractures, pre-filling decomposable materials inside the core, etc. The Chinese patent document with publication number CN 114526046 A discloses a method for constructing a complex fracture network system under simulated formation conditions, wherein the method is to split the core to form the main fracture, use a core cutter to cut along the center of the cylindrical core end face at a set angle θ, and make natural fractures distributed at a certain angle to the main fracture; according to the fracture network design parameters, the cores of different widths of support fractures are arranged neatly to complete the construction of a complex fracture network. The shape of the natural fractures produced by this method is relatively simple, and the success rate of making the main fracture by splitting is insufficient. A Chinese patent document with publication number CN 109540617A discloses a method for preparing a fractured core, wherein the method comprises the steps of stirring quartz sand and a cementing material into a uniform mixture and pouring the mixture into a mold, pouring a certain thickness and compacting the mixture, laying ammonium chloride on the mixture in the mold according to the desired crack shape and size, laying the mixture again and compacting the mixture to obtain a pressed block core; heating and curing the block core to volatilize the ammonium chloride to prepare fracture pores; and cleaning and drying the ammonium chloride remaining in the core. In this method, there may be a physical and chemical reaction between the ammonium chloride and the cementing agent, and at the same time, it cannot form microcracks.

[0008] In general, the existing splitting fracture-making methods have limited fracture-making capabilities and cannot create fractures according to the expected effects, and it is difficult to manufacture complex fracture networks. The fracture-making effect of pre-filling the core with the above decomposable materials is greatly affected by the materials, and it is difficult to meet the requirements of CO2 quasi-dry fracturing to make a fracture network model. Summary of the invention

[0009] In view of this, the present invention provides a method for making a carbon dioxide quasi-dry fracturing network model based on microbial decomposition of plant fibers. The method for making a complex fracture network core after CO2 quasi-dry fracturing mentioned in the present invention can obtain a complete and undamaged core, and at the same time can form a complex fracture network with a main fracture in the core, and the branch and branch fractures conform to the core fracture network morphology after CO2 quasi-dry fracturing.

[0010] Based on the decomposition of plant fibers by microorganisms, the present invention provides a method for making a carbon dioxide quasi-dry fracturing network model, comprising the following steps:

[0011] S1. Mix quartz sand and cement into a mixture and spread it on the bottom of the inner cavity of the core mold. A removable strip-shaped inert component is fixed vertically in the center of the inner cavity of the core mold. A plurality of conical cellulose fibers of different sizes are placed on the surface of the spread mixture and around the strip-shaped inert component. Repeat the above operation several times until the core mold is filled. After drying and forming, take out the strip-shaped inert component to form a core with a main fracture.

[0012] S2, injecting a bacterial solution containing cellulose decomposing bacteria into the main fracture of the core to decompose the plurality of conical cellulose fibers to form a core having main fractures and branch fractures;

[0013] S3, sterilizing and cleaning the core having the main fracture and the branch fracture, and then injecting a proppant into the core to obtain the desired fracture core.

[0014] Preferably, in step S1, the plurality of tapered cellulose fibers of different sizes include: first tapered fibers arranged radially toward the center of the core mold, and second tapered fibers placed in any direction; the first tapered fibers and the second tapered fibers are independently one or more of artificial cellulose fibers and natural cellulose fibers.

[0015] Preferably, in step S1, among the conical cellulose fibers, the first conical fiber has a thinnest part of 3 mm and a thickest part of 5 mm; the second conical fiber has two types, and is arranged gradually away from the strip-shaped inert component, the closer conical fiber has a thinnest part of 2 mm and a thickest part of 3 mm; the farthest conical fiber has a thinnest part of 1 mm and a thickest part of 2 mm, and the length of the three types is 40 to 50 mm.

[0016] Preferably, in step S1, the strip-shaped inert component is a metal wire wrapped with a plastic film on the outside, and has a cross-sectional diameter of 10 to 15 mm.

[0017] Preferably, in step S2, the cellulose decomposing bacteria are anaerobic plant fiber decomposing bacteria or thermophilic plant fiber decomposing bacteria, the anaerobic plant fiber decomposing bacteria are cellobiose-producing Clostridium or Clostridium ostreatus, and the thermophilic plant fiber decomposing bacteria are Clostridium thermocellum or Sporotrichum thermophilum.

[0018] Preferably, in step S3, a bactericide is injected into the main fracture of the core at regular intervals for sterilization, and the bactericide is one or more of peroxides, hypochlorites and potassium permanganate.

[0019] Preferably, in step S3, the proppant particle size injected into the core branch seams is 100-200 meshes, and the proppant particle size injected into the main fractures is 20-50 meshes, and both are one or more of quartz sand, ceramsite and artificial resin.

[0020] Preferably, the core mold is connected and fixed by the side plate, the bottom plate and the top plate to form an inner cavity, and the size of the inner cavity is

[0021] Compared with the prior art, the present invention provides a method for making a core suitable for a CO2 quasi-dry fracturing network model. A strip-shaped inert component can be inserted into the middle of the assembled core mold, and a main fracture is first formed by laying a mixture of quartz sand and cement, and arranging conical cellulose fibers, etc.; then, the decomposition ability of cellulose decomposing bacteria on pre-filled fibers during core production is utilized to generate multiple branch fractures in situ in the core. Due to the complexity of the spreading morphology of cellulose fibers, a complex core fracture network can be directly formed, thereby realizing the simulation of the "fracture network model" after CO2 quasi-dry fracturing. The most significant advantage of the present invention is that a highly complex fracture network can be generated in situ inside the core without damaging the physical and chemical properties of the core, and the fracture network morphology can be controlled by the experimenter. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Schematic diagram of the structure of a complex seam network core mold for preparing some embodiments of the present invention; 1 is a bottom plate; 2 is a side plate; 3 is a top plate; 4 is an inner cavity; 5 is a wire fixing hole; 6 is a screw hole;

[0023] Figure 2 Schematic diagram of simple seam network core fiber spreading in some embodiments of the present invention; 1 is fiber No. 3; 2 is fiber No. 1; 3 is fiber No. 2;

[0024] Figure 3 Schematic diagram of the spreading of complex seam network core fibers according to some embodiments of the present invention; 1 is fiber No. 3; 2 is fiber No. 1; 3 is fiber No. 2;

[0025] Figure 4 This is the nuclear magnetic resonance imaging image of the core sample produced in Example 1 of the present invention. DETAILED DESCRIPTION

[0026] The technical solutions in the embodiments of the present application are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present application.

[0027] The present invention provides a method for making a carbon dioxide quasi-dry fracturing network model, which is based on the decomposition of plant fibers by microorganisms and includes the following steps:

[0028] S1. Mix quartz sand and cement into a mixture and spread it on the bottom of the inner cavity of the core mold. A removable strip-shaped inert component is fixed vertically in the center of the inner cavity of the core mold. A plurality of conical cellulose fibers of different sizes are placed on the surface of the spread mixture and around the strip-shaped inert component. Repeat the above operation several times until the core mold is filled. After drying and forming, take out the strip-shaped inert component to form a core with a main fracture.

[0029] S2, injecting a bacterial solution containing cellulose decomposing bacteria into the main fracture of the core to decompose the plurality of conical cellulose fibers to form a core having main fractures and branch fractures;

[0030] S3, sterilizing and cleaning the core having the main fracture and the branch fracture, and then injecting a proppant into the core to obtain the desired fracture core.

[0031] In view of the shortcomings and deficiencies of the current methods for making complex fracture network artificial cores, the present invention provides a CO2 quasi-dry method for making a fracture network model based on microbial decomposition of plant fibers, which can obtain complete and undamaged cores and is simple and easy to operate.

[0032] In the embodiment of the present invention, the core mold is first assembled. The mold may include a side plate, a bottom plate and a top plate. Specifically, the side plate, the bottom plate and the top plate form a square mold with an inner cavity. Figure 1 Schematic diagram of the core mold structure. Figure 1 In the figure, 1 is the bottom plate; 2 is the side plate; 3 is the top plate; 4 is the inner cavity; 5 is the wire fixing hole; and 6 is the screw hole.

[0033] The bottom plate 1 and the top plate 3 are parallel and opposite to each other, and each is provided with four screw holes 6 matching the side plates, and a wire fixing hole 5; the lower ends of the two side plates 2 are provided with two screw holes, and the screw holes at the bottom of the bottom plate and the side plates are aligned and the nuts are screwed on. The size of the inner cavity 4 of the core mold is preferably A removable strip of inert components is fixed vertically in the center of the inner cavity. Figure 1 The strip-shaped inert component is preferably a metal wire wrapped with a plastic film, such as an iron wire wrapped with a plastic wrap; its cross-sectional diameter is further 10-15 mm (side length of the square end face of the iron wire) to facilitate subsequent operations.

[0034] In the embodiment of the present invention, a mixture of quartz sand and cement is prepared. Quartz sand of a certain mass ratio (such as 20% to 60%), 60% to 20% cement and 20% clean water can be stirred into a uniform mixture, which is a concrete with a large viscosity; preferably, quartz sand is 60%, M36.7 grade cement is 20%, and clean water is 20%.

[0035] In an embodiment of the present invention, a layer of cling film is wrapped around the iron wire and then inserted longitudinally into the iron wire fixing hole 5 in the center of the bottom plate 1. The iron wire usually leaks out a longer part for easy pulling out; then the obtained mixture is slowly poured into the core mold in a shallow layer. After a certain thickness of quartz sand and cement mixture is poured, a plurality of conical cellulose fibers of different sizes are sprinkled on the surface of the mixture at a certain spreading density, and the operation of spreading sand and spreading fibers is repeated in the same manner until the mold is filled with the mixture and fibers. The iron wire can be fixed and sealed with a perforated top plate; the core can be dried at 0-40°C for 5 days to form, and then the iron wire wrapped with cling film is taken out, thereby obtaining a main crack (referred to as the main crack) that runs through and parallel to the core.

[0036] In the embodiment of the present invention, a seam grid is laid simultaneously during the sand laying process, and the branch seams can be designed arbitrarily, for example, uniform or uneven, and can be laid regularly or irregularly; preferably, the conical natural plant fibers are laid or inserted on the surface of the prepared mixture according to the complex seam grid design diagram, and the laying morphology of each layer of fibers is preferably the same. Figure 2 Schematic diagram of simple seam network core fiber spreading in some embodiments of the present invention; 1 is fiber No. 3; 2 is fiber No. 1; 3 is fiber No. 2; Figure 3 Schematic diagram of the spreading of complex seam network core fibers according to some embodiments of the present invention; 1 is fiber No. 3; 2 is fiber No. 1; and 3 is fiber No. 2.

[0037] like Figure 2 As shown, among the multiple tapered cellulose fibers of different sizes, the first tapered fiber radially pointing to the center of the core mold is fiber No. 1 2, and it is required that when laying the first layer of fibers close to the iron wire, the thick end surface of the fiber must fit the iron wire; the second tapered fiber can have two sizes (different thickness and taper), namely fiber No. 2 3 and fiber No. 3 1, and the two can be placed arbitrarily or spread according to the seam network design drawing. Fiber No. 1 2 is closest to the iron wire, fiber No. 2 3 is second, and fiber No. 3 1 is farthest from the iron wire.

[0038] In a preferred embodiment of the present invention, the tapered cellulose fibers are laid according to the complex seam network design diagram, see Figure 3 ; Among them, the first tapered fiber radially pointing to the center of the core mold is No. 1 fiber 2, and the thinnest part of the first tapered fiber can be 3mm and the thickest part is 5mm. The second tapered fiber has two models, namely No. 2 fiber 3 and No. 3 fiber 1, and they are arranged gradually away from the strip-shaped inert component. The thinnest part of the closer tapered fiber is 2mm and the thickest part is 3mm; the thinnest part of the farthest tapered fiber is 1mm and the thickest part is 2mm. The length of the three models is 40-50mm.

[0039] Specifically, the first tapered fiber and the second tapered fiber are independently one or more of artificial cellulose fibers and natural cellulose fibers. The pre-loaded tapered cellulose fibers of the embodiment of the present invention have a certain volume and strength, and the cracks have a certain sharpness after being decomposed (fractures similar to elliptical pores will not be formed), and the fibers will not produce acidic and alkaline compounds to corrode the core after being decomposed, and the enzymes produced by the decomposing bacteria will not interact with the rock structure; finally, the fracture network morphology can be artificially designed and controlled. The present application scheme is mainly based on CO2 quasi-dry fracturing, and the constructed fracture network model conforms to the fracture network characteristics after quasi-dry fracturing.

[0040] After obtaining the core with the main fracture, the embodiment of the present invention performs the production of the branch fracture: injecting the bacterial solution containing cellulose decomposing bacteria into the main fracture, leaving it to stand for a period of time, preferably placing the mold in an oven at 35-65° C. for 10 days, during which the bacterial solution is continuously injected to decompose the multiple conical cellulose fibers to form a core with the main fracture and the branch fracture.

[0041] In a specific embodiment of the present invention, the cellulose decomposing bacteria are anaerobic plant fiber decomposing bacteria or thermophilic plant fiber decomposing bacteria, the anaerobic plant fiber decomposing bacteria are cellobiose-producing Clostridium or Clostridium ostreatus, and the thermophilic plant fiber decomposing bacteria are Clostridium thermocellum or thermophilic Sporotrichum, and commercially available bacterial powder products can be used.

[0042] In a preferred embodiment of the present invention, a bactericide is injected into the main fracture of the core at regular intervals, preferably placed at 10°C for 5 days, during which the bactericide is continuously injected to achieve a bactericidal effect. The bactericide is generally a strong oxidizing bactericide, including peroxides (such as hydrogen peroxide), hypochlorites, and potassium permanganate. After the sterilization is completed, the embodiment of the present invention rinses the bactericide and bacterial corpses remaining in the core. For example, the cleaning process is to place the core in a vacuum pump, and successively inject saturated anhydrous ethanol and distilled water into the core to clean the core.

[0043] In the embodiment of the present invention, a proppant of a certain particle size and a certain volume is injected into the cleaned core to obtain the desired fracture core, and the obtained fracture core can be dried for later use. Preferably, the particle size of the proppant injected into the branch seam of the core is 100-200 mesh, and the particle size of the proppant injected into the main fracture is 20-50 mesh, all of which are one or more of quartz sand, ceramsite and artificial resin. The preferred filling process includes: carrying sand into the fracture through water, and when filling the proppant, first fill 100-200 mesh, which has a smaller particle size and can enter the micro-cracks, and the particle size of 100-200 mesh quartz sand is very small relative to the main fracture, and cannot form a stable structure by accumulation; after injecting 100-200 mesh quartz sand, inject 20-50 mesh quartz sand to fill the main fracture.

[0044] In summary, the embodiments of the present invention disclose a method for making a CO2 quasi-dry fracturing network model based on microbial decomposition of plant fibers, which specifically includes: stirring quartz sand, cement and clean water into a uniform mixture, inserting an iron wire wrapped with plastic wrap into the iron wire fixing hole of the bottom plate, and then alternately placing the mixture and artificial or natural plant fibers in a mold, and sealing the top plate after the mixture fills the inner cavity; pulling out the iron wire and the plastic wrap to form a main crack, and injecting a bacterial solution containing cellulose-decomposing bacteria into the formed main crack; injecting a bactericide into the main crack after decomposition; using a vacuum pump, successively using anhydrous ethanol and distilled water to clean the core; injecting quartz sand of different mesh sizes into the core to fill the main crack, branch cracks and branch cracks, so as to form sand-filled cracks with high conductivity. The method is based on the plasticity of plant fibers. Plant fibers of different sizes are spread arbitrarily in the mixture, and fracture network models of different complexities (including simple models) can be designed. The method utilizes the characteristic that decomposing bacteria can decompose the skeleton structure of cellulose fibers to decompose the cellulose fibers into soluble substances. The colony corpses, decomposition products and nutrient residues are removed by cleaning fluid, which causes less pollution and damage to the core, and a complex fracture network core can be obtained.

[0045] In order to better understand the technical content of the present invention, specific examples are provided below to further illustrate the present invention. In the following examples, all raw materials used are commercially available, among which the bacterial solution of Clostridium cellobiose-producing bacteria and the bacterial solution of Clostridium thermocellum were purchased from Shanghai Guyan Industrial Co., Ltd.

[0046] Example 1

[0047] (1) Assembling the mold: The mold is a square mold consisting of a side plate, a bottom plate and a top plate. The bottom plate and the top plate are provided with four screw holes and one wire fixing hole. The lower ends of the two side plates are provided with two screw holes. Align the screw holes at the bottom of the bottom plate and the side plates and screw on the nuts. The inner cavity size of the mold is

[0048] Mixture preparation: quartz sand is 60%, M36.7 grade cement is 20%, and clean water is 20%;

[0049] (2) Sanding: Mix quartz sand, cement and water into a uniform mixture, wrap a circle of plastic wrap around a 10-15 mm iron wire and insert it into the iron wire fixing hole on the bottom plate, and slowly pour the mixture into the mold in a shallow layer;

[0050] (3) Laying the seam network: According to the complex seam network design drawing ( Figure 3) Spread conical natural plant fibers on the surface of the mixture; the conical plant fibers have three models, the conical fiber No. 1 has a thinnest part of 3mm and a thickest part of 5mm; the conical fiber No. 2 has a thinnest part of 2mm and a thickest part of 3mm; the conical fiber No. 3 has a thinnest part of 1mm and a thickest part of 2mm, and the lengths of the three models are all 40 to 50mm.

[0051] Repeat the sand spreading and fiber spreading operations in (2) and (3) until the mold is filled with the mixture and fibers, and then use a perforated top plate to fix the wire and seal the top plate;

[0052] (4) Making the main seam: After the core is dried at 20°C for 5 days and formed, the wire and plastic wrap are pulled out to obtain a main seam that runs through and parallel to the core;

[0053] (5) Creating branch cracks: Inject a bacterial solution containing cellobiose-producing Clostridium into the main crack, place the mold in a 35°C oven for 10 days, and continuously inject bacterial solution during this period;

[0054] (6) Sterilization: Inject hydrogen peroxide fungicide into the main crack and place it at 10°C for 5 days, during which time the fungicide is continuously injected;

[0055] (7) Core flushing: Place the core in a vacuum pump and inject saturated anhydrous ethanol and distilled water into the core to clean it;

[0056] (8) Proppant injection: First, inject 100-200 mesh quartz sand to fill micro fractures, and then inject 20-50 mesh quartz sand to fill main fractures;

[0057] (9) Drying: Dry the core to obtain a complex fracture network core.

[0058] The complex fracture network core was subjected to nuclear magnetic resonance imaging test, and the results are shown in Figure 4 .according to Figure 4 , the hydrogen signal is obvious before decomposition, but no obvious hydrogen signal is visible after decomposition, which can confirm that the plant fiber is indeed decomposed by decomposition bacteria in the core. This application does not cause overall damage to the core, but only creates cracks at the designed position. The constructed fracture network model meets the fracture network characteristics after quasi-dry fracturing.

[0059] Example 2

[0060] (1) Assembling the mold: The mold is a square mold consisting of a side plate, a bottom plate and a top plate. The bottom plate and the top plate are provided with four screw holes and one wire fixing hole. The lower ends of the two side plates are provided with two screw holes. Align the screw holes at the bottom of the bottom plate and the side plates and screw on the nuts. The inner cavity size of the mold is

[0061] Mixture preparation: quartz sand is 60%, M36.7 grade cement is 20%, and clean water is 20%;

[0062] (2) Sanding: Mix quartz sand, cement and water into a uniform mixture, wrap a circle of plastic wrap around a 10-15 mm iron wire and insert it into the iron wire fixing hole on the bottom plate, and slowly pour the mixture into the mold in a shallow layer;

[0063] (3) Laying the seam network: According to the complex seam network design drawing ( Figure 3 ) Spread conical natural plant fibers on the surface of the mixture; the conical plant fibers have three models, the conical fiber No. 1 has a thinnest part of 3mm and a thickest part of 5mm; the conical fiber No. 2 has a thinnest part of 2mm and a thickest part of 3mm; the conical fiber No. 3 has a thinnest part of 1mm and a thickest part of 2mm, and the lengths of the three models are all 40 to 50mm.

[0064] Repeat the sand spreading and fiber spreading operations in (2) and (3) until the mold is filled with the mixture and fibers, and then use a perforated top plate to fix the wire and seal the top plate;

[0065] (4) Making the main seam: After the core is dried at 20°C for 5 days and formed, the wire and plastic wrap are pulled out to obtain a main seam that runs through and parallel to the core;

[0066] (5) Creating branch cracks: Inject a bacterial solution containing Clostridium thermocellum into the main crack, place the mold in a 65°C oven for 10 days, and continuously inject bacterial solution during this period;

[0067] (6) Sterilization: Inject hydrogen peroxide fungicide into the main crack and place it at 10°C for 5 days, during which time the fungicide is continuously injected;

[0068] (7) Flushing the core: Place the core in a vacuum pump and inject saturated anhydrous ethanol and distilled water into the core to clean it;

[0069] (8) Proppant injection: First, inject 100-200 mesh quartz sand to fill micro fractures, and then inject 20-50 mesh quartz sand to fill main fractures;

[0070] (9) Drying: Dry the core to obtain a complex fracture network core.

[0071] Example 3

[0072] (1) Assembling the mold: The mold is a square mold consisting of a side plate, a bottom plate and a top plate. The bottom plate and the top plate are provided with four screw holes and one wire fixing hole. The lower ends of the two side plates are provided with two screw holes. Align the screw holes at the bottom of the bottom plate and the side plates and screw on the nuts. The inner cavity size of the mold is

[0073] Mixture preparation: quartz sand is 60%, M36.7 grade cement is 20%, and clean water is 20%;

[0074] (2) Sanding: Mix quartz sand, cement and water into a uniform mixture, wrap a circle of plastic wrap around a 10-15 mm iron wire and insert it into the iron wire fixing hole on the bottom plate, and slowly pour the mixture into the mold in a shallow layer;

[0075] (3) Laying the seam net: Lay the conical artificial plant fiber on the surface of the mixture according to the complex seam net design drawing; the conical plant fiber has three types, the conical fiber No. 1 has a thinnest part of 3 mm and a thickest part of 5 mm; the conical fiber No. 2 has a thinnest part of 2 mm and a thickest part of 3 mm; the conical fiber No. 3 has a thinnest part of 1 mm and a thickest part of 2 mm, and the length of the three types is 40 to 50 mm.

[0076] Repeat the sand spreading and fiber spreading operations in (2) and (3) until the mold is filled with the mixture and fibers, and then use a perforated top plate to fix the wire and seal the top plate;

[0077] (4) Making the main seam: After the core is dried at 20°C for 5 days and formed, the wire and plastic wrap are pulled out to obtain a main seam that runs through and parallel to the core;

[0078] (5) Creating branch cracks: Inject a bacterial solution containing cellobiose-producing Clostridium into the main crack, place the mold in a 35°C oven for 10 days, and continuously inject bacterial solution during this period;

[0079] (6) Sterilization: Inject hydrogen peroxide fungicide into the main crack and place it at 10°C for 5 days, during which time the fungicide is continuously injected;

[0080] (7) Core flushing: Place the core in a vacuum pump and inject saturated anhydrous ethanol and distilled water into the core to clean it;

[0081] (8) Proppant injection: First, inject 100-200 mesh quartz sand to fill micro fractures, and then inject 20-50 mesh quartz sand to fill main fractures;

[0082] (9) Drying: Dry the core to obtain a complex fracture network core.

[0083] Example 4

[0084] (1) Assembling the mold: The mold is a square mold consisting of a side plate, a bottom plate and a top plate. The bottom plate and the top plate are provided with four screw holes and one wire fixing hole. The lower ends of the two side plates are provided with two screw holes. Align the screw holes at the bottom of the bottom plate and the side plates and screw on the nuts. The inner cavity size of the mold is

[0085] Mixture preparation: quartz sand is 60%, M36.7 grade cement is 20%, and clean water is 20%;

[0086] (2) Sanding: Mix quartz sand, cement and water into a uniform mixture, wrap a circle of plastic wrap around a 10-15 mm iron wire and insert it into the iron wire fixing hole on the bottom plate, and slowly pour the mixture into the mold in a shallow layer;

[0087] (3) Laying the seam net: According to the simple seam net design drawing ( Figure 2 ) Spread or insert the conical artificial plant fiber on the surface of the mixture; the conical plant fiber has three models, the conical fiber No. 1 is 3mm at the thinnest part and 5mm at the thickest part; the conical fiber No. 2 is 2mm at the thinnest part and 3mm at the thickest part; the conical fiber No. 3 is 1mm at the thinnest part and 2mm at the thickest part, and the length of the three models are all 40-50mm.

[0088] Repeat the sand spreading and fiber spreading operations in (2) and (3) until the mold is filled with the mixture and fibers, and then use a perforated top plate to fix the wire and seal the top plate;

[0089] (4) Making the main seam: After the core is dried at 20°C for 5 days and formed, the wire and plastic wrap are pulled out to obtain a main seam that runs through and parallel to the core;

[0090] (5) Creating branch cracks: Inject a bacterial solution containing cellobiose-producing Clostridium into the main crack, place the mold in a 35°C oven for 10 days, and continuously inject bacterial solution during this period;

[0091] (6) Sterilization: Inject hydrogen peroxide fungicide into the main crack and place it at 10°C for 5 days, during which time the fungicide is continuously injected;

[0092] (7) Flushing the core: Place the core in a vacuum pump and inject saturated anhydrous ethanol and distilled water into the core to clean it;

[0093] (8) Proppant injection: First, inject 100-200 mesh quartz sand to fill micro fractures, and then inject 20-50 mesh quartz sand to fill main fractures;

[0094] (9) Drying: Dry the core to obtain a simple seam network core.

[0095] From the above embodiments, it can be seen that based on the decomposition of plant fibers by microorganisms, in the production of the carbon dioxide quasi-dry fracturing network model in the embodiment of the present invention, the main fracture is first formed; then, the decomposition ability of cellulose decomposing bacteria on the pre-filled fibers during core production is used to generate multiple branch fractures in situ in the core, which can directly form a complex core fracture network, thereby realizing the simulation of the "fracture network model" after CO2 quasi-dry fracturing. The present invention can generate a highly complex fracture network in situ inside the core without damaging the physical and chemical properties of the core, and the fracture network morphology can be controlled by the experimenter, and the method is simple.

[0096] This article uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core ideas of the present invention. The above is only a preferred implementation of the present invention. It should be pointed out that due to the limitations of textual expression and the objective existence of infinite specific structures, ordinary technicians in this technical field can make several improvements, modifications or changes without departing from the principles of the present invention, and can also combine the above technical features in an appropriate manner; these improvements, modifications, changes or combinations, or the direct application of the inventive concept and technical solution to other occasions without improvement, should be regarded as the protection scope of the present invention.

Claims

1. A method for making a carbon dioxide quasi-dry fracturing network model, characterized in that: The steps include: S1. Mix quartz sand and cement into a mixture and spread it on the bottom of the inner cavity of the core mold. A removable strip-shaped inert component is fixed vertically in the center of the inner cavity of the core mold. A plurality of conical cellulose fibers of different sizes are placed on the surface of the spread mixture and around the strip-shaped inert component. Repeat the above operation several times until the core mold is filled. After drying and forming, take out the strip-shaped inert component to form a core with a main fracture. S2, injecting a bacterial solution containing cellulose decomposing bacteria into the main fracture of the core to decompose the plurality of conical cellulose fibers to form a core having main fractures and branch fractures; S3, sterilizing and cleaning the core having the main fracture and the branch fracture, and then injecting a proppant into the core to obtain the desired fracture core.

2. The method according to claim 1, characterized in that: In step S1, the plurality of tapered cellulose fibers of different sizes include: first tapered fibers arranged radially toward the center of the core mold, and second tapered fibers placed in any direction; the first tapered fibers and the second tapered fibers are independently one or more of artificial cellulose fibers and natural cellulose fibers.

3. The method according to claim 2, characterized in that: In step S1, among the conical cellulose fibers, the first conical fiber has a thinnest part of 3 mm and a thickest part of 5 mm; the second conical fiber has two types, and is arranged gradually away from the strip-shaped inert component, the closer conical fiber has a thinnest part of 2 mm and a thickest part of 3 mm; the farthest conical fiber has a thinnest part of 1 mm and a thickest part of 2 mm, and the length of the three types is 40 to 50 mm.

4. The method according to claim 1, characterized in that: In step S1, the strip-shaped inert component is a metal wire wrapped with a plastic film on the outside, and the cross-sectional diameter is 10 to 15 mm.

5. The method according to claim 1, characterized in that: In step S2, the cellulose decomposing bacteria are anaerobic plant fiber decomposing bacteria or thermophilic plant fiber decomposing bacteria, the anaerobic plant fiber decomposing bacteria are cellobiose-producing Clostridium or Clostridium ostreatus, and the thermophilic plant fiber decomposing bacteria are Clostridium thermocellum or Sporotrichum thermophilum.

6. The method according to claim 1, characterized in that: In step S3, a bactericide is injected into the main fracture of the core at regular intervals for sterilization, wherein the bactericide is one or more of peroxides, hypochlorites and potassium permanganate.

7. The manufacturing method according to claim 1, characterized in that: In step S3, the proppant particle size injected into the core branch seams is 100-200 meshes, and the proppant particle size injected into the main fractures is 20-50 meshes, and both are one or more of quartz sand, ceramsite and artificial resin.

8. The production method according to any one of claims 1 to 7, characterized in that: The core mold is connected and fixed by side plates, a bottom plate and a top plate to form an inner cavity, and the size of the inner cavity is φ100mm×100mm.

Citation Information

Patent Citations

  • Preparation method for fractured core

    CN109540617A

  • Normal-pressure sand mixing quasi-dry fracturing method, and used fracturing fluid, preparation method and application thereof

    CN111363533A

  • Construction method of complex fracturing fracture network system under simulated formation condition

    CN114526046A

  • CO2 less-water fracturing fluid system and supercritical CO2 near-dry sand fracturing method