Emulsion oil sludge combustion rod and preparation method thereof

By preparing the emulsion oil sludge combustion rod, the ratio mixing of PAC deemulsion oil sludge and waste acid deemulsion oil sludge, combined with advanced oxidation treatment, the treatment and resource utilization of emulsion wastewater are solved, and the preparation of high-calorie fuel is realized. The processing cost is reduced and the resource utilization effect of the emulsion is improved.

CN118993391APending Publication Date: 2024-11-22SUZHOU INDAL PARK HESHUN ENTERPRISE ENVIRONMENTAL PROTECTION SERVICE
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411067966.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The prior art cannot efficiently convert emulsion into oil sludge and generate high-calorie fuel, and cannot effectively solve the problems of treatment and resource utilization of emulsion wastewater.

Method used

By preparing PAC deemulsion oil sludge and waste acid deemulsion oil sludge, deemulsion and precipitation are carried out by adjusting pH value and adding flocculant, flocculation and precipitation are carried out in combination with lime milk and PAM to form oil sludge, and the emulsion sludge combustion is prepared by mixing and mixing. Rods, using advanced oxidation to treat wastewater, and finally prepare combustion rods with high calorific value.

Benefits of technology

The effective treatment and resource utilization of emulsion wastewater are realized, the treatment cost is reduced, the calorific value of the prepared combustion rod is close to that of raw coal, the resource utilization effect of emulsion is improved, and economic benefits are created.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118993391A_ABST
    Figure CN118993391A_ABST
Patent Text Reader

Abstract

The invention discloses an emulsion oil sludge combustion rod which is prepared by mixing PAC demulsified oil sludge and waste acid demulsified oil sludge in proportion. The PAC demulsified oil sludge is prepared from the following raw materials in parts by weight: 100 parts of emulsion, 10 parts of 15% PAC, 2 parts of 0.5% PAM and 2 parts of 30% lime milk; the waste acid demulsified oil sludge is prepared from the following raw materials in parts by weight: 100 parts of emulsion, 8 parts of waste acid, 16 parts of 30% lime milk and 2 parts of 0.5% PAM. The invention further discloses a preparation method of the emulsion oil sludge combustion rod. According to the method, the emulsion is recycled, the utilization value of the emulsion is increased, the treatment cost of emulsion wastewater is reduced, waste is turned into wealth, certain economic benefits are created, and the prepared combustion rod has a high calorific value which is close to that of raw coal and is a good fuel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of emulsion wastewater treatment, in particular to an emulsion sludge burning rod and a preparation method thereof. Background Art

[0002] With the rapid development of my country's machinery and manufacturing industries, the use of emulsions is also increasing year by year. Emulsions mainly play the role of lubrication, cooling and cleaning in metal processing processes such as cutting, grinding and forging. The resulting emulsion wastewater has the characteristics of high content of organic matter, oil, impurities and suspended matter, and is a high-concentration difficult to treat wastewater.

[0003] Emulsions are mainly composed of base oil (mineral oil, animal or vegetable oil or synthetic oil), emulsifiers, additives and water mixed in different proportions. The particle size of the oil particles is generally between 0.1-25um. From the appearance, it is generally turbid or emulsified. It is a relatively stable polydisperse system.

[0004] The Chinese invention patent with application number CN202310800924.9 discloses a coking process of adding cold-rolled emulsion sludge to a coke oven, mixing the cold-rolled emulsion sludge with coking coal to form an emulsion mixed sludge, and using the emulsion mixed sludge for coking, and the cold-rolled emulsion sludge is reused in the steel plant. Although this type of treatment method simplifies the treatment process and treatment cost of cold-rolled emulsion sludge, the focus of the treatment is on the mixing ratio of emulsion sludge and coking coal, and it still cannot solve the problem of efficiently converting emulsion into sludge and producing high calorific value fuel. Summary of the invention

[0005] In order to solve the technical problems existing in the prior art, the present invention provides an emulsion sludge combustion rod and a preparation method thereof. The method for preparing the combustion rod increases the utilization value of the emulsion and reduces the disposal cost of the emulsion wastewater through resource utilization of the emulsion, thereby turning waste into treasure and creating certain economic benefits. The prepared combustion rod has a high calorific value, which is close to that of raw coal, and is a very good fuel.

[0006] The invention provides an emulsion oil sludge burning rod, which is prepared by mixing PAC demulsified oil sludge and waste acid demulsified oil sludge in a certain proportion; the raw materials of the PAC demulsified oil sludge include, by weight, 100 parts of emulsion, 10 parts of 15% PAC, 2 parts of 0.5% PAM and 2 parts of 30% lime milk; the raw materials of the waste acid demulsified oil sludge include, by weight, 100 parts of emulsion, 8 parts of waste acid, 16 parts of 30% lime milk and 2 parts of 0.5% PAM.

[0007] Preferably, the ratio of PAC demulsified sludge to waste acid demulsified sludge is 1:2.

[0008] The method for preparing an emulsion oil sludge burning stick of the present invention comprises the following steps:

[0009] S1, preparing PAC demulsified sludge: lifting the emulsion to a reaction tank, adding 30% lime milk to adjust the pH to 8-9, then adding 15% PAC to react and demulsify, continuing to add 30% lime milk during the reaction to ensure that the pH of the emulsion is 8-9, finally adding 0.5% PAM for flocculation and precipitation, filtering the muddy water mixture obtained by the reaction through a filter press, sending the sludge obtained by the filter press to an evaporator for drying, and measuring the calorific value of the PAC demulsified sludge obtained by drying through an oxygen bomb calorimeter;

[0010] S2, preparing waste acid demulsified sludge: the emulsion is lifted to another reaction tank, waste acid is added to adjust the pH value to <2, demulsification is performed by acid, 30% lime milk is added to adjust the pH value to 8-9, and finally 0.5% PAM is added for flocculation precipitation, the mud-water mixture obtained by the reaction is filtered through a filter press, the sludge obtained by the filter press is sent to an evaporator for drying, and the calorific value of the waste acid demulsified sludge obtained by drying is measured by an oxygen bomb calorimeter;

[0011] S3, the prepared PAC demulsified sludge and waste acid demulsified sludge are mixed in proportion, and then prepared into a combustion rod, and the calorific value is measured by an oxygen bomb calorimeter.

[0012] Preferably, in step S1, 15% PAC solution is added and stirred for reaction for 10 minutes, 0.5% PAM solution is added and reacted for 10 minutes, and then allowed to settle for 30 minutes.

[0013] Preferably, in step S2, after the waste acid is added, the mixture is stirred and reacted for 30 minutes to fully break the emulsion, and after the 0.5% PAM solution is added, the mixture is reacted for 10 minutes and allowed to settle for 30 minutes.

[0014] Preferably, in step S3, PAC demulsified sludge and waste acid demulsified sludge are mixed in a ratio of 1:2 to prepare a combustion rod, and the calorific value of the combustion rod is 4853 Kcal / kg.

[0015] Preferably, the effluent from the filter press is treated by a Fenton advanced oxidation system and then enters a biochemical system for treatment, and is finally discharged in compliance with the standards.

[0016] Compared with the prior art, the present invention has the following advantages: the present invention separates oil and water from the emulsion, and the wastewater enters the biochemical treatment system after advanced oxidation, and finally meets the discharge standards, thereby achieving the effect of effectively treating the emulsion wastewater; the generated sludge and other materials are combined to prepare a combustion rod for resource utilization, and the optimal ratio of the sludge and other materials is determined through multiple experiments, thereby increasing the calorific value of the fuel and reducing the ignition point, providing a new method for treating emulsion wastewater, improving the resource utilization effect of the emulsion, turning waste into treasure, and creating certain economic benefits. The prepared combustion rod has a high calorific value, which is close to that of raw coal, and is a very good fuel. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a process flow chart of the present invention. DETAILED DESCRIPTION

[0018] The specific implementation modes of the present invention are described in detail below with reference to the accompanying drawings.

[0019] Example:

[0020] The invention provides an emulsion oil sludge burning rod, which is prepared by mixing PAC demulsified oil sludge and waste acid demulsified oil sludge in a certain proportion, wherein the raw materials of the PAC demulsified oil sludge include, by weight, 100 parts of emulsion, 10 parts of 15% PAC, 2 parts of 0.5% PAM and 2 parts of 30% lime milk; the raw materials of the waste acid demulsified oil sludge include, by weight, 100 parts of emulsion, 8 parts of waste acid, 16 parts of 30% lime milk and 2 parts of 0.5% PAM.

[0021] Preferably, the ratio of PAC demulsified sludge to waste acid demulsified sludge is 1:2.

[0022] The method for preparing an emulsion oil sludge burning stick of the present invention comprises the following steps:

[0023] S1, preparation of PAC demulsified sludge: the emulsion in the raw water pool is lifted to the reaction tank by a pump, lime and water are added to the lime milk agent storage tank to make a 30% lime milk, and the 30% lime milk is pumped into the reaction tank by a pump to adjust the pH to 8-9; solid PAC is added to the PAC agent storage tank, and the concentration is 15% with water, and under the condition that the pH of the emulsion is 8-9, 15% PAC solution is pumped into the reaction tank by a pump to react and demulsify, and the reaction is stirred for 10 minutes. Since the PAC solution is acidic, 30% lime milk is continuously added during the reaction process to ensure that the pH of the emulsion is 8-9; finally, 0.5% PAM solution is added to react for 10 minutes, and the solution is allowed to stand for 30 minutes to flocculate and precipitate; the mud-water mixture obtained by the reaction is filtered by a filter press, and the sludge obtained by the filter press is sent to an evaporator for drying, and the calorific value of the PAC demulsified sludge obtained by drying is measured by an oxygen bomb calorimeter;

[0024] S2, preparing waste acid demulsified sludge: the emulsion in the raw water pool is lifted to another reaction tank, the pH is adjusted to <2 by adding waste acid, the reaction is stirred for 30 minutes to fully demulsify, and then 30% lime milk is added to adjust the pH to 8-9, and finally 0.5% PAM solution is added to react for 10 minutes, and the mixture is allowed to stand for 30 minutes for flocculation and precipitation; the mud-water mixture obtained by the reaction is filtered through a filter press, and the sludge obtained by the filtration is sent to an evaporator for drying, and the calorific value of the waste acid demulsified sludge obtained by drying is measured by an oxygen bomb calorimeter;

[0025] S3, the PAC demulsified sludge and the waste acid demulsified sludge prepared in step S1 and step S2 are mixed in proportion, and then prepared into a combustion rod, and the calorific value is measured by an oxygen bomb calorimeter; preferably, the calorific value of the combustion rod prepared by mixing the PAC demulsified sludge and the waste acid demulsified sludge in a ratio of 1:2 is 4853Kcal / kg, which is close to the calorific value of raw coal 4984Kcal / kg. The combustion rod has a high calorific value, which fully improves the resource utilization effect of the emulsion.

[0026] In addition, the effluent from the filter press is treated by the Fenton advanced oxidation system and then enters the biochemical system for treatment, and is ultimately discharged in compliance with the standards, thus enabling effective treatment of emulsion wastewater.

[0027] The present invention separates oil and water from the emulsion, and the wastewater enters a biochemical treatment system after advanced oxidation, and is finally discharged in compliance with the standards, thereby achieving the effect of effectively treating the emulsion wastewater; the generated oil sludge and other materials are combined to prepare a combustion rod for resource utilization, and the optimal ratio of the oil sludge and other materials is determined through multiple experiments, thereby increasing the calorific value of the fuel and reducing the ignition point, providing a new method for treating the emulsion wastewater, improving the resource utilization effect of the emulsion, turning waste into treasure, and creating certain economic benefits; the prepared combustion rod has a high calorific value, which is close to that of raw coal, and is a very good fuel.

[0028] Of course, the above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any modifications made according to the spirit of the main technical solution of the present invention should be included in the protection scope of the present invention.

Claims

1. An emulsion oil sludge burning stick, characterized in that: The method is prepared by mixing PAC demulsified sludge and waste acid demulsified sludge in a certain proportion; the raw materials of PAC demulsified sludge include, by weight: 100 parts of emulsion, 10 parts of 15% PAC, 2 parts of 0.5% PAM, and 2 parts of 30% lime milk; the raw materials of waste acid demulsified sludge include, by weight: 100 parts of emulsion, 8 parts of waste acid, 16 parts of 30% lime milk, and 2 parts of 0.5% PAM.

2. The emulsion oil sludge burning stick according to claim 1, characterized in that: The ratio of PAC demulsified sludge to waste acid demulsified sludge is 1:

2.

3. A method for preparing an emulsion oil sludge burning stick according to claim 1 or 2, characterized in that: The steps include: S1, preparing PAC demulsified sludge: lifting the emulsion to a reaction tank, adding 30% lime milk to adjust the pH to 8-9, then adding 15% PAC to react and demulsify, continuing to add 30% lime milk during the reaction to ensure that the pH of the emulsion is 8-9, finally adding 0.5% PAM for flocculation and precipitation, filtering the muddy water mixture obtained by the reaction through a filter press, sending the sludge obtained by the filter press to an evaporator for drying, and measuring the calorific value of the PAC demulsified sludge obtained by drying through an oxygen bomb calorimeter; S2, preparing waste acid demulsified sludge: the emulsion is lifted to another reaction tank, waste acid is added to adjust the pH value to <2, demulsification is performed by acid, 30% lime milk is added to adjust the pH value to 8-9, and finally 0.5% PAM is added for flocculation precipitation, the mud-water mixture obtained by the reaction is filtered through a filter press, the sludge obtained by the filter press is sent to an evaporator for drying, and the calorific value of the waste acid demulsified sludge obtained by drying is measured by an oxygen bomb calorimeter; S3, the prepared PAC demulsified sludge and waste acid demulsified sludge are mixed in proportion, and then prepared into a combustion rod, and the calorific value is measured by an oxygen bomb calorimeter.

4. The preparation method according to claim 3, characterized in that: In step S1, 15% PAC solution was added and stirred for reaction for 10 minutes, 0.5% PAM solution was added and reacted for 10 minutes, and then allowed to settle for 30 minutes.

5. The preparation method according to claim 3, characterized in that: In step S2, after the waste acid is added, the mixture is stirred and reacted for 30 minutes to fully break the emulsion, and after the 0.5% PAM solution is added, the mixture is reacted for 10 minutes and allowed to settle for 30 minutes.

6. The preparation method according to claim 3, characterized in that: In step S3, PAC demulsified sludge and waste acid demulsified sludge are mixed in a ratio of 1:2 to prepare a combustion rod, and the calorific value of the combustion rod is 4853 Kcal / kg.

7. The preparation method according to claim 3, characterized in that: The effluent from the filter press is treated by the Fenton advanced oxidation system and then enters the biochemical system for treatment before finally meeting the discharge standards.

Citation Information

Patent Citations

  • Coking process for adding cold-rolled emulsion oil sludge into coke oven

    CN116731737A

  • Emulsified liquid waste water treatment method

    CN101700951A

  • Treatment equipment for oil sludge of waste emulsion

    CN109321318A

  • Waste emulsion sludge treatment method

    CN109385321A

  • Oil sludge fuel preparation system and preparation method for inhibiting leaching toxicity of heavy metals

    CN113956906A