By using screen printing and laser cutting methods in ceramic production, combined with vacuum sintering and etching processes, the ceramic production process is simplified, the problems of complex and low efficiency of traditional processes are solved, and more efficient and more accurate ceramic production is achieved .

CN118993755APending Publication Date: 2024-11-22GUANGZHOU TAOJIDIAN ELECTRONIC TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411024396.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the existing ceramic production process, the activated metal brazing method is complex and has low efficiency and cumbersome operating steps, resulting in low ceramic production efficiency.

Method used

Screen printing is used to coat the conductive paste on the ceramic substrate, laser cutting of oxygen-free copper forms the required circuit pattern, and vacuum sintering is carried out with the ceramic substrate, and then etching is performed to simplify the process flow.

Benefits of technology

It improves the efficiency and graphic accuracy of ceramic production, which is more time-saving and accurate than traditional processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118993755A_ABST
    Figure CN118993755A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of ceramic production, and particularly relates to a novel ceramic production process which comprises the following specific steps: S1, firstly, selecting a ceramic base material with a proper size and shape, pretreating the ceramic base material, and directly coating conductive slurry on the ceramic base body by adopting a silk-screen printing mode; s2, performing laser pattern cutting on the oxygen-free copper to obtain a required circuit pattern made of an oxygen-free copper material; s3, attaching and combining the circuit pattern cut from the oxygen-free copper and the ceramic substrate coated with the conductive slurry, putting the circuit pattern and the ceramic substrate into a vacuum sintering furnace together, and performing high-temperature sintering on the circuit pattern and the ceramic substrate; the cut oxygen-free copper is attached to the surface of the ceramic base material, the ceramic base material is subjected to vacuum sintering processing, and then the ceramic base material is treated in an etching mode, so that compared with a traditional production process, the novel ceramic production process is more time-saving, and meanwhile, the pattern accuracy is higher.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of ceramic production, in particular to a novel ceramic production process. Background Art

[0002] Active metal brazing (AMB) is a method of sealing ceramics to metals. It is developed based on DBC technology. Active metal brazing is a new ceramic substrate production technology that can braze pure copper on ceramics to provide a high-reliability substrate with unique heat dissipation function. Compared with traditional DBC substrates, ceramic linings prepared using the AMB process have higher thermal conductivity, better copper layer bonding, and also have the advantages of lower thermal resistance and higher reliability.

[0003] When processing ceramic materials, oxygen-free copper and ceramic substrates are usually first vacuum sintered. After sintering, the oxygen-free copper and brazing material are sealed on the ceramic substrate by etching. However, this method is relatively cumbersome and complicated, and there are many operating steps during production, resulting in low efficiency of ceramic production.

[0004] Therefore, the present invention provides a novel ceramic production process. Summary of the invention

[0005] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.

[0006] The technical solution adopted by the present invention to solve the technical problem is: a new type of ceramic production process described in the present invention, the specific steps of the production process are as follows:

[0007] S1: First, a ceramic substrate of suitable size and shape is selected, and after pre-treatment of the ceramic substrate, the conductive paste is directly coated on the ceramic substrate by screen printing;

[0008] S2: Laser cutting oxygen-free copper to obtain the required circuit pattern of oxygen-free copper;

[0009] S3: After the circuit pattern cut out of the oxygen-free copper is attached and combined with the ceramic substrate coated with the conductive slurry, they are placed together in a vacuum sintering furnace to sinter the circuit pattern and the ceramic substrate at a high temperature so that the circuit pattern is firmly attached to the surface of the ceramic substrate to obtain a finished soldering material;

[0010] S4: Etching the sintered brazing material. After the etching is completed, the production of the ceramic material can be completed.

[0011] Preferably, the pretreatment of the ceramic substrate in S1 includes cleaning, drying, sandblasting or anodizing.

[0012] Preferably, the etchant used in S4 for etching the solder should be an alkaline etching liquid (such as cupric chloride, ammonia water, ammonium chloride) for etching the solder, and should be used in combination with an accelerator, an anti-side etching agent, and a suppressant.

[0013] Preferably, the accelerator may be an alkaline etching additive (such as CP-320) to promote oxidation reaction and prevent precipitation of cuprous aluminum ions.

[0014] Preferably, the anti-side corrosion agent (bank protection agent) can be sodium benzoate, aniline compounds or pyridine compounds, which can be adsorbed on the metal surface to form a protective film to prevent the etchant from directly contacting the oxygen-free copper surface to prevent the occurrence of lateral corrosion.

[0015] Preferably, the suppressor may be ammonium fluoride, copper sulfate, oxalic acid, oxalic acid or citrate, which can prevent metal ions from reacting with the etchant, thereby reducing the etching rate, and is used to suppress the diffusion of ammonia, the precipitation of copper, and accelerate the oxidation reaction of copper.

[0016] Preferably, the ceramic substrate after vacuum sintering in S3 can be cooled by convection cooling or carbon dioxide cooling.

[0017] Preferably, the time and temperature required for etching in S4 need to be determined according to the etching depth, the etching area and the etching rate of the etchant used.

[0018] The beneficial effects of the present invention are as follows:

[0019] 1. The novel ceramic production process described in the present invention, by attaching the cut oxygen-free copper to the surface of the ceramic substrate, vacuum sintering the ceramic substrate, and then processing the ceramic substrate by etching, can make the novel ceramic production process more time-saving and have higher graphic accuracy than the traditional production process. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] The present invention will be further described below in conjunction with the accompanying drawings.

[0021] Figure 1 It is a process flow chart of the ceramic production process in the present invention. DETAILED DESCRIPTION

[0022] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0023] like Figure 1 As shown, a novel ceramic production process according to an embodiment of the present invention has the following specific steps:

[0024] S1: First, a ceramic substrate of suitable size and shape is selected, and after pre-treatment of the ceramic substrate, the conductive paste is directly coated on the ceramic substrate by screen printing;

[0025] S2: Laser cutting oxygen-free copper to obtain the required circuit pattern of oxygen-free copper;

[0026] S3: After the circuit pattern cut out of the oxygen-free copper is attached and combined with the ceramic substrate coated with the conductive slurry, they are placed together in a vacuum sintering furnace to sinter the circuit pattern and the ceramic substrate at a high temperature so that the circuit pattern is firmly attached to the surface of the ceramic substrate to obtain a finished soldering material;

[0027] S4: Etching the sintered brazing material. After the etching is completed, the production of the ceramic material can be completed.

[0028] The pretreatment of the ceramic substrate in S1 includes cleaning, drying, sandblasting or anodizing.

[0029] The etchant used in S4 for etching the solder should be an alkaline etching liquid (such as cupric chloride, ammonia water, ammonium chloride) for etching the solder, and it should be used in conjunction with an accelerator, an anti-side etching agent, and a suppressant.

[0030] The accelerator may be an alkaline etching additive (such as CP-320) to promote oxidation reaction and prevent the precipitation of cuprous aluminum ions.

[0031] The anti-side corrosion agent (bank protection agent) can be sodium benzoate, aniline compounds or pyridine compounds, which can be adsorbed on the metal surface to form a protective film to prevent the etchant from directly contacting the oxygen-free copper surface to prevent the occurrence of lateral corrosion.

[0032] The suppressor may be ammonium fluoride, copper sulfate, oxalic acid, oxalic acid or citrate, which can prevent metal ions from reacting with the etchant, thereby reducing the etching rate, and is used to suppress the diffusion of ammonia, the precipitation of copper, and accelerate the oxidation reaction of copper.

[0033] The ceramic substrate after vacuum sintering in S3 can be cooled by convection cooling or carbon dioxide cooling.

[0034] The time and temperature required for etching in S4 need to be determined according to the etching depth, etching area and etching rate of the etchant used.

[0035] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A new type of ceramic production process, characterized by:

1. A new type of ceramic production process, It is characterized in that The specific steps of the production process are as follows: S1: First, a ceramic substrate of suitable size and shape is selected, and after pre-treatment of the ceramic substrate, the conductive paste is directly coated on the ceramic substrate by screen printing; S2: Laser cutting oxygen-free copper to obtain the required circuit pattern of oxygen-free copper; S3: After the circuit pattern cut out of the oxygen-free copper is attached and combined with the ceramic substrate coated with the conductive slurry, they are placed together in a vacuum sintering furnace to sinter the circuit pattern and the ceramic substrate at a high temperature so that the circuit pattern is firmly attached to the surface of the ceramic substrate to obtain a finished soldering material; S4: Etching the sintered brazing material. After the etching is completed, the production of the ceramic material can be completed.

2. A novel ceramic production process according to claim 1, Features: The pretreatment of the ceramic substrate in S1 includes cleaning, drying, sandblasting or anodizing.

3. A novel ceramic production process according to claim 1, Features: The etchant used in S4 for etching the solder should be an alkaline etching liquid (such as cupric chloride, ammonia water, ammonium chloride) for etching the solder, and it should be used in conjunction with an accelerator, an anti-side etching agent, and a suppressant.

4. A novel ceramic production process according to claim 3, Features: The accelerator may be an alkaline etching additive (such as CP-320).

5. A novel ceramic production process according to claim 3, Features: The anti-side corrosion agent (bank protection agent) can be sodium benzoate, aniline compounds or pyridine compounds.

6. A novel ceramic production process according to claim 3, Features: The depressant can be ammonium fluoride, copper sulfate, oxalic acid, oxalic acid or citrate.

7. A novel ceramic production process according to claim 1, Features: The ceramic substrate after vacuum sintering in S3 can be cooled by convection cooling or carbon dioxide cooling.

8. A novel ceramic production process according to claim 1, Features: The time and temperature required for etching in S4 need to be determined according to the etching depth, etching area and etching rate of the etchant used.

Citation Information

Patent Citations

  • PCB electroplating etching solution and etching process

    CN114096070A

  • Active metal brazing ceramic substrate and manufacturing method thereof

    CN114373685A

  • Method for manufacturing ceramic circuit board

    US20200170118A1