Non-noble metal catalyst membrane electrode performance recovery method
Through the open circuit voltage detection system hierarchical recovery program, the performance attenuation and carbon corrosion problems of non-precious metal catalyst membrane electrodes are solved, and rapid and effective performance recovery is achieved, improving the stability and efficiency of fuel cells.
Patent Information
- Application Number
- CN202411083015.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
AI Technical Summary
The performance of non-precious metal catalyst membrane electrodes in fuel cells is relatively low and have poor stability. The prior art recovery methods are difficult to effectively remove water accumulation, resulting in performance attenuation, and high and low potential cycles are prone to aggravation of carbon corrosion, long recovery time and low efficiency.
Through the open circuit voltage detection system, it is divided into three types of membrane electrode performance recovery programs. The corresponding programs are selected according to the open circuit voltage value, including switching gas, adjusting the current density and metering ratio, reducing carbon corrosion, protecting non-precious metal catalysts, and improving recovery speed.
Effectively restore the performance of non-precious metal catalyst membrane electrodes, reduce high and low potential cycles, protect the catalyst, shorten the recovery time, improve the overall recovery efficiency, and avoid irreversible performance attenuation.
Smart Images

Figure CN119009014A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of fuel cells and relates to a method for recovering membrane electrode performance, and in particular to a method for recovering non-precious metal catalyst membrane electrode performance. Background Art
[0002] Fuel cells are an efficient and clean energy conversion technology that directly converts the chemical energy of fuel (usually hydrogen) and oxidant (oxygen) into electrical energy through an electrochemical reaction. The process does not involve combustion, so it has higher energy conversion efficiency and lower emissions. The development background of fuel cell technology is closely related to the growth of global energy demand, the intensification of environmental problems, and the pursuit of sustainable energy solutions. Fuel cells have a wide range of applications, from transportation to stationary power generation, to portable power and aerospace. Their high efficiency and environmental protection make them a strong competitor to replace traditional energy. Especially in the field of transportation, fuel cell vehicles have attracted attention due to their zero emissions and fast charging characteristics.
[0003] Although fuel cell technology has shown great application potential, its commercialization process still faces multiple challenges, among which the cost issue is particularly prominent. The high cost mainly comes from the use of precious metal catalysts in fuel cells, especially on the cathode side. In order to promote the oxygen reduction reaction, a large amount of precious metal catalysts are often required. In order to effectively reduce the cost of use, the industry has proposed the use of non-precious metal catalysts to replace the precious metal catalysts on the cathode side. However, the application of non-precious metal catalysts in fuel cells is not smooth sailing. Problems such as low performance, poor stability, and susceptibility to flooding frequently occur, which seriously restricts its performance in the fuel cell membrane electrode. Therefore, improving the membrane electrode performance and stability of non-precious metal catalysts has become an important direction of current development.
[0004] When using non-precious metal catalysts as fuel cell cathode catalysts, the performance is low and the stability is poor during the membrane electrode test. After running for a period of time, the performance of the non-precious metal catalyst membrane electrode is greatly attenuated. In the existing technical scheme, when the performance of the non-precious metal catalyst membrane electrode is significantly attenuated after running for a period of time, the performance of the non-precious metal catalyst membrane electrode is mainly restored by operating the membrane electrode stably at a constant current and operating it in a high-low potential cycle. However, this recovery method is difficult to completely discharge the accumulated water in the non-precious metal catalyst layer, thereby affecting the transmission of gas in the non-precious metal catalyst layer, and it is also easy to cause the active sites of the non-precious metal catalyst to be covered by water, affecting the output of performance; the high-low potential cycle operation method is easy to aggravate the carbon corrosion of the non-precious metal catalyst, resulting in irreversible attenuation of performance, and aggravating the performance degradation of the non-precious metal membrane electrode; the performance recovery time of the non-precious metal catalyst membrane electrode is too long, affecting the overall recovery efficiency; after using the prior art method to restore the performance, the performance recovery effect of the non-precious metal catalyst membrane electrode is poor, and the purpose of recovery cannot be achieved. Summary of the invention
[0005] The present invention overcomes the defects of the prior art and provides a method for restoring the performance of a non-precious metal catalyst membrane electrode. The present invention can effectively reduce the high and low potential cycles during the performance restoration process of the non-precious metal catalyst membrane electrode, reduce carbon corrosion of the catalyst, and accelerate the speed of performance restoration.
[0006] The technical solution of the present invention is as follows.
[0007] A method for restoring the performance of a non-precious metal catalyst membrane electrode comprises the following steps: After the membrane electrode with non-precious metal catalyst at the cathode runs for a period of time, the open circuit voltage detection system is started, and the corresponding membrane electrode performance recovery program is executed according to the size of the open circuit voltage value: When the open circuit voltage U>0.9V, there is no need to perform the membrane electrode performance recovery procedure; When the open circuit voltage is 0.85V≤U≤0.9V, execute the first procedure of membrane electrode performance recovery: When the open circuit voltage U<0.85V, the second procedure of membrane electrode performance recovery is executed. (For the specific flow chart, please refer to Figure 1 ) Furthermore, the first procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 1-3 minutes; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) Increase the current density to 0.3-0.7A / cm 2 , the hydrogen stoichiometric ratio is set to 1.6-1.8, the air stoichiometric ratio is set to 2.3-2.7, and the operation lasts for 3-7 minutes; (4) 0.3-0.7A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.2-0.4V and it continues to operate for 20-40s; (5) Increase the air stoichiometric ratio to 1.8-2.4 and run for 2-6 minutes; (6) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, the membrane electrode performance recovery procedure is completed. If the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, continue to execute the first membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.9 V after three executions, execute the second membrane electrode performance recovery procedure.
[0008] Furthermore, the second procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 1-3 minutes; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.1-0.3A / cm 2 , run for 20-40 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) Increase the current density to 0.8-1.2A / cm 2 , the hydrogen stoichiometric ratio is set to 1.6-1.8, the air stoichiometric ratio is set to 2.1-2.5, and the operation lasts for 3-5 minutes; (5) 0.8-1.2A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0V and it continues to operate for 20-40s; (6) Increase the air stoichiometric ratio to 1.8-2.4 and run for 2-6 minutes; (7) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, complete the membrane electrode performance recovery procedure; if the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, execute the first membrane electrode performance recovery procedure; if the open circuit voltage is lower than 0.85 V, continue to execute the second membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.85 V after three executions, terminate the membrane electrode performance recovery procedure.
[0009] As a specific method of the present invention, a method for restoring the performance of a non-precious metal catalyst membrane electrode comprises the following steps: after the membrane electrode using the non-precious metal catalyst at the cathode runs for a period of time, the open circuit voltage detection system is started, and the corresponding membrane electrode performance recovery program is executed according to the size of the open circuit voltage value: When the open circuit voltage U>0.9V, there is no need to perform the membrane electrode performance recovery procedure; When the open circuit voltage is 0.85V≤U≤0.9V, execute the first procedure of membrane electrode performance recovery: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) The current density was increased to 0.5 A / cm2, the hydrogen stoichiometric ratio was set to 1.6, and the air stoichiometric ratio was set to 2.5, and the operation was continued for 5 minutes; (4) At 0.5A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.3V and it continues to operate for 30s; (5) Increase the air stoichiometric ratio to 2.0 and run for 3 minutes; (6) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, the membrane electrode performance recovery procedure is completed. If the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, continue to execute the first membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.9 V after three executions, execute the second membrane electrode performance recovery procedure.
[0010] When the open circuit voltage U is less than 0.85V, the second procedure of membrane electrode performance recovery is executed: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.1A / cm2 for 30 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) The current density was increased to 1.0 A / cm2, the hydrogen stoichiometric ratio was set to 1.6, and the air stoichiometric ratio was set to 2.5, and the operation was continued for 5 minutes; (5) At a current density of 1.0 A / cm2, the hydrogen stoichiometric ratio was maintained unchanged and the air stoichiometric ratio was reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode was lower than 0 V and continued to operate for 30 s; (6) Increase the air stoichiometric ratio to 2.0 and run for 3 minutes; (7) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, complete the membrane electrode performance recovery procedure; if the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, execute the first membrane electrode performance recovery procedure; if the open circuit voltage is lower than 0.85 V, continue to execute the second membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.85 V after three executions, terminate the membrane electrode performance recovery procedure.
[0011] Compared with the prior art, the advantages of the present invention are: 1) According to the open circuit voltage value of the non-precious metal catalyst membrane electrode, different membrane electrode performance recovery procedures are used to effectively restore the performance of the non-precious metal catalyst membrane electrode; 2) After a period of operation, the non-precious metal catalyst membrane electrode will show obvious performance degradation. This method can effectively restore the reversible performance degradation of the non-precious metal catalyst; 3) When executing the first procedure of membrane electrode performance recovery, the voltage during the recovery process can be lower than 0.3V, which can effectively protect the non-precious metal catalyst and accelerate the performance recovery of the membrane electrode; 4) When executing the second procedure of membrane electrode performance recovery, hydrogen is introduced during the process, which can effectively reduce the non-precious metal catalyst of the cathode and accelerate the recovery of membrane electrode performance; 5) This method can effectively reduce the high and low potential cycles during the performance recovery process of non-precious metal catalytic membrane electrodes, reduce carbon corrosion of the catalyst, and accelerate the speed of performance recovery. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 Flow chart of the method for restoring performance of membrane electrode with non-precious metal catalyst. DETAILED DESCRIPTION
[0013] In the following description, the technical solution is explained in combination with specific diagrams to fully understand the present invention. However, the present invention can be implemented in many other ways different from those described herein. Similar generalized embodiments made by ordinary technicians in this field without creative work are all within the scope of protection of the present invention. Start the membrane electrode test equipment with a non-precious metal catalyst cathode to detect the open circuit voltage of the membrane electrode. The open circuit voltage value test result is 0.87V. Execute the first procedure of membrane electrode performance recovery: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) Increase the current density to 0.5A / cm 2 , the hydrogen stoichiometric ratio was set to 1.7, the air stoichiometric ratio was set to 2.5, and the operation lasted for 5 minutes; (4) At 0.5A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.3V and it continues to operate for 30s; (5) Increase the air stoichiometric ratio to 2.1 and run for 4 minutes; (6) The electric density is reduced to 0, and the open circuit voltage is continuously detected. After the first membrane electrode performance recovery procedure, the open circuit voltage of the membrane electrode increases to 0.94 V, achieving the effect of membrane electrode performance recovery, and the membrane electrode performance recovery procedure is terminated.
[0014] Example 2 Start the membrane electrode test equipment with a non-precious metal catalyst cathode to detect the open circuit voltage of the membrane electrode. The open circuit voltage value detection result is 0.83V. Execute the second membrane electrode performance recovery procedure: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.2A / cm 2 , run for 30 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) Increase the current density to 1.0 A / cm 2 , the hydrogen stoichiometric ratio was set to 1.7, the air stoichiometric ratio was set to 2.3, and the operation lasted for 4 minutes; (5) At 1.0A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0V and it continues to operate for 30s; (6) Increase the air stoichiometric ratio to 2.1 and run for 4 minutes; (7) The electric density is reduced to 0, and the open circuit voltage is monitored. After the second procedure of the first membrane electrode performance recovery is performed, the open circuit voltage of the membrane electrode increases to 0.92 V, achieving the effect of membrane electrode performance recovery, and the membrane electrode performance recovery procedure is terminated.
[0015] Example 3 Start the membrane electrode test equipment with a non-precious metal catalyst cathode to detect the open circuit voltage of the membrane electrode. The open circuit voltage value detection result is 0.83V. Execute the second membrane electrode performance recovery procedure: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.2A / cm 2 , run for 30 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) Increase the current density to 1.0 A / cm 2 , the hydrogen stoichiometric ratio was set to 1.7, the air stoichiometric ratio was set to 2.3, and the operation lasted for 4 minutes; (5) At 1.0A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0V and it continues to operate for 30s; (6) Increase the air stoichiometric ratio to 2.1 and run for 4 minutes; (7) The electric density was reduced to 0, and the open circuit voltage was monitored. After the first membrane electrode performance recovery second procedure, the open circuit voltage of the membrane electrode increased to 0.86 V, which did not achieve the effect of membrane electrode performance recovery.
[0016] Since the open circuit voltage is 0.86V, which is in the range of 0.85V≤U≤0.9V, continue to execute the first procedure of membrane electrode performance recovery: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) Increase the current density to 0.5A / cm2 , the hydrogen stoichiometric ratio was set to 1.7, the air stoichiometric ratio was set to 2.5, and the operation lasted for 5 minutes; (4) At 0.5A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.3V and it continues to operate for 30s; (5) Increase the air stoichiometric ratio to 2.1 and run for 4 minutes; (6) Reduce the electric density to 0, continue to detect the open circuit voltage, and after the second membrane electrode performance recovery sequence, the open circuit voltage of the membrane electrode increases to 0.91V, achieving the effect of membrane electrode performance recovery, and ending the membrane electrode performance recovery procedure.
[0017] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A method for restoring the performance of a non-precious metal catalyst membrane electrode, characterized in that: The steps include: After the membrane electrode with non-precious metal catalyst at the cathode runs for a period of time, the open circuit voltage detection system is started, and the corresponding membrane electrode performance recovery program is executed according to the size of the open circuit voltage value: When the open circuit voltage U>0.9V, there is no need to perform the membrane electrode performance recovery procedure; When the open circuit voltage is 0.85V≤U≤0.9V, execute the first procedure of membrane electrode performance recovery: When the open circuit voltage U is less than 0.85 V, the second membrane electrode performance recovery procedure is executed.
2. A method for restoring the performance of a non-precious metal catalyst membrane electrode according to claim 1, characterized in that: The first procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen for purging; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) Increase the current density to 0.3-0.7A / cm 2 , the hydrogen stoichiometric ratio is set to 1.6-1.8, the air stoichiometric ratio is set to 2.3-2.7, and the operation lasts for 3-7 minutes; (4) 0.3-0.7A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.2-0.4V and it continues to operate for 20-40s; (5) Increase the air stoichiometric ratio to 1.8-2.4 and run; (6) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, the membrane electrode performance recovery procedure is completed. If the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, continue to execute the first membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.9 V after three executions, execute the second membrane electrode performance recovery procedure.
3. A method for restoring the performance of a non-precious metal catalyst membrane electrode according to claim 2, characterized in that: In step (1), the purging time is 1-3 minutes.
4. A method for restoring the performance of a non-precious metal catalyst membrane electrode according to claim 2, characterized in that: In step (5), the running time is: 2-6 minutes.
5. A method for restoring performance of a non-precious metal catalyst membrane electrode according to claim 1 or 2, characterized in that: The second procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen for purging; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.1-0.3A / cm 2 , run for 20-40 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) Increase the current density to 0.8-1.2A / cm 2 , the hydrogen stoichiometric ratio is set to 1.6-1.8, the air stoichiometric ratio is set to 2.1-2.5, and the operation lasts for 3-5 minutes; (5) 0.8-1.2A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0V and it continues to operate for 20-40s; (6) Increase the air stoichiometric ratio to 1.8-2.4 and run; (7) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, complete the membrane electrode performance recovery procedure; if the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, execute the first membrane electrode performance recovery procedure; if the open circuit voltage is lower than 0.85 V, continue to execute the second membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.85 V after three executions, terminate the membrane electrode performance recovery procedure.
6. A method for restoring the performance of a non-precious metal catalyst membrane electrode according to claim 5, characterized in that: In step (1), the purging time is 1-3 minutes.
7. A method for restoring the performance of a non-precious metal catalyst membrane electrode according to claim 5, characterized in that: In step (6), the running time is 2-6 minutes.
8. A method for restoring performance of a non-precious metal catalyst membrane electrode according to claim 1, characterized in that: The first procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen and air are normally introduced into the anode and cathode; (3) Increase the current density to 0.5A / cm 2 , the hydrogen stoichiometric ratio was set to 1.6, the air stoichiometric ratio was set to 2.5, and the operation lasted for 5 minutes; (4) At 0.5A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0.3V and it continues to operate for 30s; (5) Increase the air stoichiometric ratio to 2.0 and run for 3 minutes; (6) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, the membrane electrode performance recovery procedure is completed. If the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, continue to execute the first membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.9 V after three executions, execute the second membrane electrode performance recovery procedure.
9. A method for restoring performance of a non-precious metal catalyst membrane electrode according to claim 1 or 2, characterized in that: The second procedure for recovering the membrane electrode performance is: (1) Switch the anode hydrogen and cathode air to nitrogen and purge for 2 minutes; (2) Hydrogen is introduced into both the anode and cathode, and the current is pulled to 0.1A / cm 2 , run for 30 seconds; (3) Rapidly reduce the current to zero and switch the cathode side to air; (4) Increase the current density to 1.0 A / cm 2 , the hydrogen stoichiometric ratio was set to 1.6, the air stoichiometric ratio was set to 2.5, and the operation lasted for 5 minutes; (5) At 1.0A / cm 2 Under the current density, the hydrogen stoichiometric ratio is maintained unchanged, and the air stoichiometric ratio is reduced to 1.0, so that the operating voltage of the non-precious metal catalyst membrane electrode is lower than 0V and it continues to operate for 30s; (6) Increase the air stoichiometric ratio to 2.0 and run for 3 minutes; (7) Reduce the electric density to 0 and monitor the open circuit voltage. If the open circuit voltage is greater than 0.9 V, complete the membrane electrode performance recovery procedure; if the open circuit voltage is 0.85 V ≤ U ≤ 0.9 V, execute the first membrane electrode performance recovery procedure; if the open circuit voltage is lower than 0.85 V, continue to execute the second membrane electrode performance recovery procedure. If the open circuit voltage is still lower than 0.85 V after three executions, terminate the membrane electrode performance recovery procedure.