Electricity storage device

By designing the rectangular bottom surface and liquid injection hole positions on the sealing plate of the power storage equipment, as well as the symmetrical clamping and inclination design of the inner surface protrusions, the welding problem caused by electrolyte adhesion is solved, and the sealing and manufacturing stability are improved. sex.

CN119009320APending Publication Date: 2024-11-22PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410598663.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-18
Filing Date
2024-05-15
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing power storage equipment is prone to electrolyte adhesion at the liquid injection holes on the inner surface of the sealing plate, resulting in poor welding and gasification problems, affecting sealing properties.

Method used

A power storage device is designed, and its sealing plate has a rectangular bottom surface and a wide and narrow edge facing opposite sides. The liquid injection hole is located near the midpoint of the long side. A protruding part is provided on the inner surface of the sealing plate to sandwich the liquid injection hole in a symmetrical position. The projection is inclined and flat surface designed to suppress the electrolyte adhesion.

Benefits of technology

It effectively suppresses the adhesion of electrolyte on the liquid injection holes on the inner surface of the sealing plate, reduces the risk of welding defects and gasification, and improves sealing and manufacturing stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119009320A_ABST
    Figure CN119009320A_ABST
Patent Text Reader

Abstract

Provided is a power storage device in which an electrolyte is prevented from adhering to the vicinity of a liquid injection hole on the inner surface of a sealing plate. A power storage device (1) is provided with an electrode body (20), an electrolyte solution, and a case (10) that accommodates the electrode body (20) and the electrolyte solution. The housing (10) is provided with a housing main body (12) having an opening (12h), and a rectangular sealing plate (14) for sealing the opening (12h). The sealing plate (14) has a liquid injection hole (17) for injecting the electrolyte at a position closer to the first short side part than a straight line (CL) passing through a midpoint (M1) of the first long side part and a midpoint (M2) of the second long side part. Here, the sealing plate (14) has a pair of protrusions (90) protruding from the inner surface (142) toward the inside of the housing (10). In addition, the pair of protruding parts (90) are arranged on the inner surface (142) in the longitudinal direction of the sealing plate (14), wherein the protruding parts (90) are symmetrical relative to the liquid injection hole (17).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to an electric storage device. Background Art

[0002] The storage element disclosed in Japanese Patent Publication No. 2016-76346 comprises: a container having a liquid injection hole for injecting electrolyte in a partition wall; an electrode body, the electrode body being accommodated in the container; and a plug member, the plug member sealing the liquid injection hole, having a head larger than the inner diameter of the liquid injection hole and a shaft portion inserted into the liquid injection hole. In the storage element, a first concave portion surrounding the liquid injection hole or a convex portion surrounding the liquid injection hole is formed on the inner surface of the partition wall. The publication states that: With this structure, the amount of electrolyte that adheres to the inner surface of the partition wall and moves to the outside through the shaft portion of the plug member and the inner peripheral surface of the liquid injection hole can be suppressed.

[0003] Japanese Patent Publication No. 2013-191450 discloses a method for manufacturing a square secondary battery, which has: a battery can, which accommodates an electrode group; a battery cover, which closes the opening of the battery can; a liquid injection port, which has a recessed portion recessed on the surface of the battery cover and a through hole opening on the bottom surface of the recessed portion and penetrating the battery cover; and a sealing plug, after the electrolyte is injected into the battery can from the liquid injection port, the sealing plug is embedded in the recessed portion and welded to the battery cover in a state of contact with the bottom surface of the recessed portion to seal the liquid injection port. The manufacturing method is characterized in that it includes: an injection process, in which a nozzle head for injecting electrolyte is installed on the liquid injection port, so that the head body of the nozzle head made of elastic material contacts the bottom surface of the recessed portion, and is connected to the through hole in a sealed state to inject electrolyte into the battery can. The publication states that this structure can prevent the electrolyte from adhering to the recessed portion of the injection port when the electrolyte is injected into the battery can, thereby eliminating welding defects caused by the adhesion of the electrolyte when the injection port is sealed.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2016-76346

[0007] Patent Document 2: Japanese Patent Application Publication No. 2013-191450 Summary of the invention

[0008] Problems to be solved by the invention

[0009] The present inventors also considered that it is desirable to suppress the adhesion of the electrolyte solution to the liquid injection hole on the inner surface of the sealing plate.

[0010] Means for solving problems

[0011] The power storage device disclosed herein comprises an electrode body, an electrolyte, and a shell for accommodating the electrode body and the electrolyte. The shell comprises: a shell body having a rectangular bottom surface, an opening facing the bottom surface, a pair of facing wide surfaces extending from a pair of facing long sides in the bottom surface, and a pair of facing narrow surfaces extending from a pair of facing short sides in the bottom surface; and a rectangular sealing plate, the sealing plate sealing the opening. The sealing plate comprises a first long side portion and a second long side portion facing each other and a first short side portion and a second short side portion facing each other. In addition, the sealing plate has an injection hole for injecting the electrolyte at a position closer to the first short side portion than a straight line CL passing through the midpoint M1 of the first long side portion and the midpoint M2 of the second long side portion. Here, the sealing plate has a pair of protrusions protruding from the inner surface of the bottom side toward the inner side of the shell. The pair of protrusions are arranged in the inner surface of the sealing plate in a symmetrical position relative to the injection hole in the long side direction. According to the electric storage device having this structure, it is possible to suppress the electrolytic solution from being attached to the liquid injection hole on the inner surface of the sealing plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 It is a cross-sectional view of the power storage device 1 .

[0013] Figure 2 yes Figure 1 A partial enlarged view of .

[0014] Figure 3 It is a top view of the sealing plate 14 .

[0015] Figure 4 is a schematic diagram of the electrode body 20 .

[0016] Figure 5 It is a partial cross-sectional view of the power storage device 2 .

[0017] Description of Reference Numerals

[0018] 1.2 Power storage equipment

[0019] 10 Housing

[0020] 12 Shell body

[0021] 12h opening

[0022] 14 Sealing plate

[0023] 141 External surface

[0024] 142 Inner surface

[0025] 17 Injection hole

[0026] 20 Electrode body

[0027] 30 Positive terminal

[0028] 40 Negative terminal

[0029] 50, 60 Current collecting components

[0030] 70 Insulation film

[0031] 80, 280 Insulation components

[0032] 90, 290 protrusion DETAILED DESCRIPTION

[0033] Hereinafter, an embodiment of the technology disclosed herein will be described. The embodiment described herein is not intended to limit the technology disclosed herein. Unless otherwise specified, the technology disclosed herein is not limited to the embodiment described herein. The drawings are schematically depicted and may not reflect the actual objects. In addition, the same figure marks are appropriately marked for components and parts that play the same role, and repeated descriptions are omitted. The figure marks "R", "L", "U", "D", "F" and "Rr" in the drawings represent "right", "left", "up", "down", "front" and "back", respectively. In addition, the expression "A~B" indicating a numerical range means "above A and below B" unless otherwise specified, and also includes the meaning of "exceeding A and below B".

[0034] In this specification, "electrical storage device" refers to a device that generates charge and discharge by moving charge carriers between a pair of electrodes (positive and negative electrodes) via an electrolyte. The electrical storage device includes secondary batteries such as lithium-ion secondary batteries, nickel-metal hydride batteries, and nickel-cadmium batteries, and capacitors such as lithium-ion capacitors and double-layer capacitors. Below, as an example of the above-mentioned electrical storage device, an implementation method when a lithium-ion secondary battery is used as an object is described.

[0035] Figure 1 is a cross-sectional view of the power storage device 1. Figure 1 2 shows a cross-sectional structure of the power storage device 1 along the wide surface 12 a. Figure 2 yes Figure 1 A partial enlarged view of the Figure 2 The enlarged part is shown in Figure 1 The cross-sectional structure near the injection hole 17 in FIG. Figure 1 As shown, the power storage device 1 includes a case 10 , an electrode body 20 , a positive electrode terminal 30 , a negative electrode terminal 40 , a positive electrode collector 50 , a negative electrode collector 60 , an insulating film 70 , an insulating member 80 , and an electrolyte solution (not shown).

[0036] The case 10 is a member for housing, for example, the electrode assembly 20 and the electrolyte. Although not particularly limited, the case 10 may be made of aluminum or an aluminum alloy from the viewpoint of reducing weight and ensuring required rigidity.

[0037] like Figure 1 and Figure 2 As shown, the shell 10 has a shell body 12 and a sealing plate 14. The shell body 12 is, for example, the main body of the shell 10 that accommodates the electrode body 20 inside. In this embodiment, the shell body 12 has an opening 12h, a pair of wide width surfaces 12a facing each other, a pair of narrow width surfaces 12b facing each other, and a bottom surface 12c. Here, the bottom surface 12c faces the opening 12h. Here, the bottom surface 12c is rectangular and has a pair of long sides facing each other and a pair of short sides facing each other. The pair of wide width surfaces 12a facing each other are surfaces extending from a pair of long sides facing each other in the bottom surface 12c. The pair of narrow width surfaces 12b facing each other are surfaces extending from a pair of short sides facing each other in the bottom surface 12c. It should be noted that in this specification, the description of "rectangular" or "rectangular" includes a shape in which a straight long side and a short side are connected to each other via a curve, at least one of the long side and the short side is not a straight line but is bent or becomes a concave and convex pressure curve and is composed of a plurality of straight lines or curves.

[0038] The opening 12h is, for example, a location where the sealing plate 14 is installed. Here, the opening 12h is formed by being surrounded by the upper edges of a pair of wide width surfaces 12a and the upper edges of a pair of narrow width surfaces 12b, and is rectangular. The sealing plate 14 is inserted and joined (for example, welded) to the opening 12h, whereby the housing body 12 and the sealing plate 14 are integrated, and the housing 10 is hermetically sealed.

[0039] Figure 3 It is a top view of the sealing plate 14 . Figure 3 1 shows the structure of the sealing plate 14 as viewed from the outside of the housing 10. The sealing plate 14 is, for example, a flat plate-shaped member that seals the opening 12h. Therefore, the shape of the sealing plate 14 may be a shape corresponding to the shape of the opening 12h. In this embodiment, the sealing plate 14 is rectangular. Here, when the sealing plate 14 is mounted on the opening 12h, the sealing plate 14 is, for example, facing the bottom surface 12c. Figure 3 As shown, the sealing plate 14 has a first long side 14a and a second long side 14b facing each other, and a first short side 14c and a second short side 14d facing each other. Figure 3 In the illustrated embodiment, the first long side 14a is the long side on the front (F) side of the pair of long sides facing each other. The second long side 14b is the long side on the rear (Rr) side of the pair of long sides facing each other. The first short side 14c is the short side on the right (R) side of the pair of short sides facing each other. The second short side 14d is the short side on the left (L) side of the pair of short sides facing each other.

[0040] like Figure 3As shown, the sealing plate 14 has a mounting hole, a discharge valve 15, and an injection hole 17, which are not shown in the figure. The mounting hole is, for example, a through hole for mounting an electrode terminal. Therefore, the sealing plate 14 can have a mounting hole for mounting a positive terminal 30 and a mounting hole for mounting a negative terminal 40, respectively. A portion of the electrode terminal is inserted through the mounting hole. The discharge valve 15 is, for example, a thin-walled portion. Here, the discharge valve 15 is configured to break when the pressure in the shell 10 becomes greater than a specified value, thereby discharging the gas in the shell 10 to the outside. The injection hole 17 is a portion where the electrolyte is injected. As shown Figure 1 to Figure 3 As shown, a sealing member 16 is installed in the injection hole 17. In this embodiment, the injection hole 17 is provided on the first short side 14c side (at the position of the injection hole 17) relative to the straight line CL passing through the midpoint M1 of the first long side 14a and the midpoint M2 of the second long side 14b. Figure 3 The position is on the right side.

[0041] The sealing member 16 may be made of metal, for example. Figure 3 In the illustrated embodiment, the sealing member 16 has a flange portion 161 and an insertion portion 162. The flange portion 161 is plate-shaped and is a portion disposed on the sealing plate 14 and welded to the sealing plate 14. The insertion portion 162 is shaft-shaped or protrusion-shaped and is a portion inserted into the injection hole 17. It should be noted that the shape of the sealing member 16 is not limited thereto. In other embodiments, the sealing member 16 may also be composed of the flange portion 161.

[0042] In the welding of the sealing member 16 and the sealing plate 14, for example, the sealing member 16 (here, the flange portion 161) is welded to the outer surface 141 of the sealing plate 14 (see Figure 2 and Figure 3 ). At this time, in the sealing plate 14, for example, near the injection hole 17, the temperature rises more than other parts. Therefore, when the electrolyte adheres to the vicinity of the injection hole 17, the electrolyte may be vaporized due to the temperature rise caused by welding. The inventors consider that it is desirable to suppress the vaporization of the electrolyte near the injection hole 17 during welding. In addition, the inventors believe that by Figure 2 ) inhibits the electrolyte from adhering to the injection hole 17, which can inhibit the vaporization of the electrolyte at this location during welding, thereby reducing the risk of adverse conditions (such as poor welding, etc.) caused by the vaporization of the electrolyte.

[0043] exist Figure 1 to Figure 3In the manner shown, the sealing plate 14 has a pair of protrusions 90. Here, the pair of protrusions 90 protrude from the inner surface 142 on the bottom surface 12c side toward the inner side of the shell 10. The protruding direction of the protrusion 90 can be defined, for example, by a straight line L1 connecting a base end 90B of the protrusion 90 and a top end 90E of the protrusion 90. Here, the base end 90B of the protrusion 90 is a boundary between the inner surface 142 and the protrusion 90. In this embodiment, the pair of protrusions 90 are provided in the inner surface 142 in the long side direction of the sealing plate 14 at positions symmetrical with respect to the injection hole 17. Here, the long side direction of the sealing plate 14 refers to the direction in which the first long side 14a extends. Figure 1 to Figure 3 In the left-right direction, the term "a pair of protrusions 90 are symmetrical with respect to the injection hole 17 in the long-side direction of the sealing plate 14" means that in the long-side direction of the sealing plate 14, the pair of protrusions 90 sandwich the injection hole 17 and the shortest distance from one protrusion 90 to the injection hole 17 is equal to the shortest distance from the other protrusion 90 to the injection hole 17. It should be noted that for the sake of convenience, in the following description, Figure 2 and Figure 3 The protrusion 90 on the left side in the figure is referred to as a first protrusion 901 , and the protrusion 90 on the right side in the figure is referred to as a second protrusion 902 .

[0044] exist Figure 1 and Figure 2 In the embodiment shown, the protrusion 90 is plate-shaped. Figure 2 As shown, the protrusion 90 has a first surface 91 and a second surface 92. Here, the first surface 91 is a flat surface, and is the surface on the other protrusion 90 side. The "surface on the other protrusion 90 side" mentioned here can be any surface provided on the other protrusion 90 side, and is adjusted according to the angle θ (see Figure 2 ) are different in size and do not necessarily face the protrusion 90 on the other side. Figure 2 As shown, the first surface 91 of the first protrusion 901 is the surface on the side of the second protrusion 902. The first surface 91 of the second protrusion 902 is the surface on the side of the first protrusion 901. Here, the second surface 92 is a flat surface, which is the surface on the side opposite to the first surface 91. Figure 2 As shown, the second surface 92 of the first protrusion 901 is a surface facing the side opposite to the second protrusion 902. The second surface 92 of the second protrusion 902 is a surface facing the side opposite to the first protrusion 901.

[0045] In this embodiment, the protrusion 90 is inclined relative to the inner surface 142 of the sealing plate 14. Here, the other side of the angle between the protrusion 90 and the inner surface 142 of the sealing plate 14 (the angle on the side of the injection hole 17) is less than 90 degrees. Figure 2In the embodiment shown, the angle θ formed by the line segment LS and the straight line L1 is less than 90 degrees. Here, the line segment LS is a line segment connecting the base end 90B of the first protrusion 901 and the base end 90B of the second protrusion 902 at the shortest distance. The angle θ may be, for example, 80 degrees or less, preferably 70 degrees or less, more preferably 60 degrees or less, further preferably 50 degrees or less, and particularly preferably 40 degrees or less. The angle θ may be approximately 3 degrees or more, preferably 5 degrees or more, and more preferably 10 degrees or more.

[0046] The shortest distance W1 between the injection hole 17 and the protrusion 90 is not particularly limited as long as the effect of the technology disclosed herein can be achieved. The shortest distance W1 is, for example, the shortest distance between the center P of the injection hole 17 and the base end 90B of the protrusion 90 (see Figure 3 ). When the shortest distance W2 (external dimensions, refer to Figure 3 ) is set to 1, the shortest distance W1 is, for example, greater than 0.02, preferably greater than 0.04, and more preferably greater than 0.06. In addition, when the shortest distance W2 is set to 1, the shortest distance W1 is, for example, less than 0.17, preferably less than 0.15, and more preferably less than 0.13. In one example, when the shortest distance W2 is 120 mm, the shortest distance W1 is preferably 7 mm to 15 mm. In this case, the shortest distance W3 between the base end 90B of the second protrusion 902 and the first short side portion 14c is preferably greater than 31 mm and less than 39 mm.

[0047] In this embodiment, the protrusion 90 is provided continuously and integrally with the sealing plate 14. In this case, the protrusion 90 may be made of the same material as the sealing plate 14. Although not particularly limited, the protrusion 90 may be provided on the sealing plate 14 by press working.

[0048] Figure 4 Schematic diagram of an electrode body 20. The electrode body 20 is, for example, a power generation element of the power storage device 1 having a positive electrode and a negative electrode. The electrode body 20 has, for example, a stacked structure in which a sheet-like positive electrode 22 and a sheet-like negative electrode 24 are stacked with a separator 23 interposed therebetween. The electrode body 20 is housed in the housing 10 in a state in which the sheet-like positive electrode 22 and the sheet-like negative electrode 24 are stacked in a direction facing the pair of wide surfaces 12a.

[0049] like Figure 4 As shown, the electrode body 20 is, for example, a wound electrode body in which a sheet-shaped positive electrode 22 and a sheet-shaped negative electrode 24 are stacked with a separator 23 and wound in the sheet length direction LD. The electrode body 20 can be made, for example, by winding the positive electrode 22, the negative electrode 24 and the separator 23 into a cylindrical body and stamping the cylindrical body. Therefore, the electrode body 20 is flat. The electrode body 20 has, for example, a pair of flat surfaces 20a facing each other (see Figure 1 ).

[0050] In addition, one end face 20b of the electrode body 20 and one narrow width face 12b (at Figure 1 The narrow width surface 12b on the left side is facing each other, and the end surface 20c on the other side is facing the narrow width surface 12b on the other side (in Figure 1 Here, the end face 20b is the stacking surface of the uncoated portion 22c1 of the positive electrode current collector foil 22c, and is an open surface. Here, the end face 20c is the stacking surface of the uncoated portion 24c1 of the negative electrode current collector foil 24c, and is an open surface. Figure 1 and Figure 4 As shown, the electrode body 20 is housed in the case body 12 so that the winding axis direction WD is substantially parallel to the left-right direction of the power storage device 1. The winding axis WL of the electrode body 20 is substantially perpendicular to the wide surface 12a and the narrow surface 12b and substantially parallel to the sealing plate 14.

[0051] like Figure 4 As shown, the positive electrode 22 has a long strip of positive electrode collector foil 22c (such as aluminum foil) and a positive electrode active material layer 22a fixed on the surface of at least one side of the positive electrode collector foil 22c. Although not particularly limited, a protective layer (not shown) can also be provided on the side edge portion of one side in the winding axis direction WD of the positive electrode 22 as needed. It should be noted that as the constituent material of the positive electrode active material layer 22a and the constituent material of the protective layer, the materials used in such a storage device (lithium ion secondary battery in this embodiment) can be used without particular limitation.

[0052] At one end portion ( Figure 4 The uncoated portion 22c1 is provided along the longitudinal direction LD. The uncoated portion 22c1 is a part of the positive electrode current collector foil 22c. The uncoated portion 22c1 is a portion of the positive electrode current collector foil 22c that is not coated with the positive electrode active material layer 22a. In this embodiment, the uncoated portion 22c1 protrudes in the winding axis direction WD from the separator 23. The uncoated portion 22c1 is provided at the end ( Figure 4 The left end of the stack. Figure 1 As shown, the current collecting member 50 is joined to the uncoated portion 22c1.

[0053] like Figure 4 As shown, the negative electrode 24 has a long strip-shaped negative electrode collector foil 24c (e.g., copper foil) and a negative electrode active material layer 24a fixed on at least one surface of the negative electrode collector foil 24c. It should be noted that as the constituent material of the negative electrode active material layer 24a, the material used in such a power storage device (in this embodiment, a lithium ion secondary battery) can be used without particular limitation.

[0054] At one end portion ( Figure 4 The uncoated portion 24c1 is provided along the length direction LD. The uncoated portion 24c1 is a part of the negative electrode current collector foil 24c. The uncoated portion 24c1 is a portion of the negative electrode current collector foil 24c where the negative electrode active material layer 24a is not formed. In this embodiment, the uncoated portion 24c1 protrudes in the winding axis direction WD from the separator 23. For example, the uncoated portion 24c1 is provided at an end portion ( Figure 4 The right end of the stack. Figure 1 As shown, the current collecting member 60 is joined to the uncoated portion 22c1.

[0055] The separator 23 is a member that insulates the positive electrode active material layer 22a of the positive electrode 22 from the negative electrode active material layer 24a of the negative electrode 24. In this embodiment, the separator 23 constitutes the outer surface of the electrode body 20. As the separator 23, for example, a porous sheet made of a resin composed of a polyolefin resin such as polyethylene (PE) or polypropylene (PP) is used.

[0056] The positive terminal 30 is, for example, a member electrically connected to the positive electrode 22 of the electrode body 20. As described above, the positive terminal 30 is inserted through the mounting hole provided in the sealing plate 14 and is arranged on the outside and inside of the case body 12. Therefore, the positive terminal 30 may have, for example, a portion arranged on the outside of the case 10, a portion inserted through the mounting hole, and a portion arranged on the inside of the case 10. The positive terminal 30 is made of, for example, aluminum or an aluminum alloy.

[0057] The current collecting member 50 on the positive electrode side is a member that electrically connects the positive electrode 22 and the positive electrode terminal 30 inside the case 10, for example. Figure 1 In the embodiment shown, the current collecting member 50 is plate-shaped and extends from the sealing plate 14 toward the electrode body 20. Here, the current collecting member 50 is provided at one end (at Figure 1 The upper end in the middle) is connected to the positive terminal 30, and the other end (at Figure 1 The collector member 50 is connected to the electrode body 20 by joining one end of the collector member 50 to the positive terminal 30 (for example, by welding). In addition, in this embodiment, the collector member 50 is connected to the electrode body 20 by joining the other end of the collector member 50 to the uncoated portion 22c1 (for example, by welding). The collector member 50 is made of, for example, aluminum or an aluminum alloy.

[0058] The negative terminal 40 is, for example, a member electrically connected to the negative electrode 24 of the electrode body 20. The negative terminal 40 is, for example, made of copper or a copper alloy. The negative terminal 40 may also have, for example, the same structure as the positive terminal 30. Therefore, the description of the structure of the negative terminal 40 is omitted here. The collector member 60 on the negative electrode side is, for example, a member electrically connecting the negative electrode 24 to the negative terminal 40 on the inner side of the shell 10. The collector member 60 is, for example, made of copper or a copper alloy. The collector member 60 on the negative electrode side may also have, for example, the same structure as the collector member 50 on the positive electrode side. Therefore, the description of the structure of the collector member 60 is omitted here.

[0059] The insulating film 70 is, for example, a member that covers the electrode body 20. The insulating film 70 is, for example, in a bag shape, with a portion thereof opened. Figure 1 As shown in FIG. 1 , the insulating film 70 is closed at the lower end and opened at the upper end. In this embodiment, the insulating film 70 is accommodated in the case 10 in a state where the electrode body 20 is accommodated therein.

[0060] like Figure 1 and Figure 2 As shown, an insulating member 80 is arranged between the positive terminal 30 and the sealing plate 14, and between the negative terminal 40 and the sealing plate 14. The insulating member 80 is arranged, for example, along the outer surface between the positive terminal 30 and the sealing plate 14, between the inner surface of the positive terminal 30 and the sealing plate 14, and the inner circumferential surface of the mounting hole. The same is true for the negative electrode side, and the insulating member 80 is arranged, for example, between the negative terminal 40, the outer surface of the sealing plate 14, the inner surface of the sealing plate 14, and the mounting hole. The insulating member 80 may be an integrally formed member, or a member formed by combining members formed at multiple locations.

[0061] The electrolyte solution, for example, contains an electrolyte salt and a non-aqueous solvent. Examples of the electrolyte salt include LiPF6. The concentration of the electrolyte salt in the electrolyte solution is, for example, 0.7 mol / L to 1.3 mol / L. The non-aqueous solvent may be, for example, a carbonate ester. Examples of the carbonate ester include ethylene carbonate (EC), diethyl carbonate (DEC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), monofluoroethylene carbonate (MFEC), difluoroethylene carbonate (DFEC), monofluoromethyl difluoromethyl carbonate (F-DMC), trifluorodimethyl carbonate (TFDMC), etc. They may be used alone or in combination of two or more.

[0062] The power storage device 1 is used for various purposes, and can be preferably used as a power source (driving power source) for a motor mounted on a vehicle such as a passenger car or a truck. The type of vehicle is not particularly limited, and preferred examples include a plug-in hybrid electric vehicle (PHEV), a hybrid electric vehicle (HEV), and a battery electric vehicle (BEV).

[0063] As described above, the power storage device 1 includes an electrode body 20, an electrolyte, and a case 10 that contains the electrode body 20 and the electrolyte. The case 10 includes: a case body 12 having a rectangular bottom surface 12c, an opening 12h facing the bottom surface 12c, a pair of facing wide surfaces 12a extending from a pair of facing long sides in the bottom surface 12c, and a pair of facing narrow surfaces 12b extending from a pair of facing short sides in the bottom surface 12c; and a rectangular sealing plate 14 that seals the opening 12h. The sealing plate 14 has a first long side 14a and a second long side 14b facing each other, and a first short side 14c and a second short side 14d facing each other. The sealing plate 14 has a liquid injection hole 17 for injecting an electrolyte solution at a position closer to the first short side 14 c than a straight line CL passing through a midpoint M1 of the first long side 14 a and a midpoint M2 of the second long side 14 b .

[0064] Here, the sealing plate 14 has a pair of protrusions 90 (here, a first protrusion 901 and a second protrusion 902) protruding from the inner surface 142 on the bottom surface 12c side toward the inner side of the housing 10. In addition, the pair of protrusions 90 are provided at locations symmetrical with respect to the injection hole 17 in the inner surface 142 in the long side direction of the sealing plate 14.

[0065] In the power storage device 1, a pair of protrusions 90 are provided on the inner surface 142 of the sealing plate 14 in a manner symmetrical with respect to the injection hole 17 in the long side direction. In other words, the injection hole 17 is sandwiched by the pair of protrusions 90 on the inner surface 142 of the sealing plate 14. Therefore, for example, in the manufacturing process of the power storage device 1, for the housing 10 containing the electrode body 20 and the electrolyte before the formal sealing, the protrusion 90 can block the electrolyte splashing from the inner wall surface (for example, the narrow width surface 12b) of the housing body 12 when the housing 10 moves. As a result, the electrolyte can be prevented from adhering to the vicinity of the injection hole 17 on the inner surface 142 of the sealing plate 14. And, for example, the occurrence of a defect (for example, a poor welding between the sealing member 16 and the sealing plate 14) that may be caused by the electrolyte adhering to the vicinity of the injection hole 17 can be suppressed.

[0066] In addition, the protrusion 90 may have a flat surface (here, the second surface 92) facing the side opposite to the other protrusion 90. By setting the surface of the protrusion 90 on the side opposite to the other protrusion 90 as a flat surface without unevenness, the electrolyte splashed from the inner wall surface of the case body 12 can flow more smoothly to the inside of the case 10. Therefore, the effect of suppressing the adhesion of the electrolyte on the inner surface 142 of the sealing plate 14 to the injection hole 17 can be improved.

[0067] In addition, the protrusion 90 may be plate-shaped. The protrusion 90 may have a flat first surface 91 on the other protrusion 90 side, and a flat second surface 92 on the opposite side of the first surface 91. In this case, since the second surface 92 is a flat surface, when the electrolyte is injected into the housing 10, it is possible to suppress the electrolyte from scattering in the housing 10. Thus, the effect of suppressing the adhesion of the electrolyte in the inner surface 142 of the sealing plate 14 to the injection hole 17 can be further improved.

[0068] In addition, the protrusion 90 may be inclined relative to the inner surface 142 of the sealing plate 14. The other angle θ formed by the protrusion 90 and the inner surface 142 on the protrusion 90 side may be less than 90 degrees. Thus, the effect of suppressing the adhesion of the electrolyte in the inner surface 142 of the sealing plate 14 to the injection hole 17 can be further improved.

[0069] In addition, when the shortest distance W2 between the first short side 14c and the second short side 14d is set to 1, the shortest distance W1 from the injection hole 17 to the protrusion 90 can be 0.06 or more and 0.13 or less. This can further improve the effect of suppressing the adhesion of the electrolyte on the inner surface 142 of the sealing plate 14 to the injection hole 17.

[0070] Furthermore, the protrusion 90 can be provided continuously and integrally with the sealing plate 14. Thus, there is no need to prepare a separate member for providing the protrusion 90. Therefore, in addition to the effect of suppressing the adhesion of the electrolyte to the injection hole 17, the ease of forming the electrical storage device 1 can be improved.

[0071] In the above-described embodiment, the protrusion 90 is formed integrally with the sealing plate 14. However, the present invention is not limited thereto. Figure 5 FIG. 2 is a partial cross-sectional view of the power storage device 2. Figure 5 In FIG. 1 , the cross-sectional structure near the injection hole 17 of the power storage device 2 is partially enlarged and shown. Figure 5 As shown, in the power storage device 2, the sealing plate 14 has a pair of protrusions 290 protruding from the inner surface 142 toward the inside of the case 10. The pair of protrusions 290 are provided at locations symmetrical to the injection hole 17 on the inner surface 142 in the longitudinal direction of the sealing plate 14.

[0072] In this embodiment, the sealing plate 14 has an insulating member 280 extending along the inner surface 142. In addition, a portion of the insulating member 280 constitutes a protrusion 290. The insulating member 280 in this embodiment has the function of insulating the positive terminal 30 from the inner surface 142 of the sealing plate 14 and the function of insulating the negative terminal 40 from the inner surface 142 of the sealing plate 14, similarly to the insulating member 80 in the above-mentioned embodiment. Figure 5 As shown, it is configured on the positive electrode side ( Figure 5 On the left side, refer to Figure 1 ) of the insulating member 280 at the end portion on the liquid injection hole 17 side (at Figure 5 The right end in the middle) has a protrusion 290. In addition, it is arranged on the negative electrode side ( Figure 5 on the right, refer to Figure 1 ) of the insulating member 280 at the end portion on the liquid injection hole 17 side (at Figure 5 The left end portion in the middle is provided with a protrusion 290. In this embodiment, the protrusion 290 is made of an insulating material (e.g., a resin material). Therefore, in addition to the effect of inhibiting the adhesion of the electrolyte to the injection hole 17, the effect of reducing the risk of contact between the electrode body 20 and the sealing plate 14 can also be achieved.

[0073] Hereinafter, regarding the technology disclosed herein, a research example (test example) performed by the inventor will be described. However, the test example is not intended to limit the technology disclosed herein. It should be noted that regarding the reference numerals of the various parts in the following test examples, please refer to the reference numerals of the various parts in the following test examples. Figure 1 to Figure 3 .

[0074] <Design of Evaluation Sample>

[0075] Regarding the protrusion 90 of this test example, the samples shown in the following Table 1 were designed. However, the protrusion 90 designed in this test example is only the protrusion 90 on the side of the first short side 14c, and the protrusion 90 on the side of the second short side 14d is not designed. For each sample, a simulation related to the adhesion of the electrolyte to the injection hole 17 was implemented through CAE (computer aided engineering) analysis. In the CAE analysis, when the test assembly in which the electrode body 20 and the electrolyte are accommodated in the shell body 12 and the sealing plate 14 is installed at the opening 12h is transported from the narrow width 12b corresponding to the first short side 14c to the left and decelerated at a specified timing, it is evaluated whether the electrolyte adheres to the injection hole 17. Here, the electrolyte is accelerated from a stationary state. In a manner that the same result is obtained as when accelerating from the stationary state, it is decelerated from a constant acceleration and analyzed. At this time, the electrolyte is in a stationary state. It should be noted that the conveying speed of the test assembly in the CAE analysis is 1000mm / s. In addition, the acceleration during deceleration (i.e., deceleration) is 1.2×9.8 m / s 2 .

[0076] The dimensional relationship of each sample was designed as follows.

[0077] Long side length of sealing plate 14 (external dimension): 120 mm (internal dimension: 119 mm)

[0078] Height of housing body 12 (external dimensions): 65 mm

[0079] Height of the electrolyte level (distance from the outer surface 141 of the sealing plate 14): 8 mm

[0080] Thickness of protrusion 90: 0.5 mm

[0081] Width of the protrusion 90 (length along the short side of the sealing plate 14): 10.5 mm

[0082] Distance X: as shown in Table 1.

[0083] Distance Z: as shown in Table 1.

[0084] Angle θ: as shown in Table 1.

[0085] It should be noted that "distance X" is equivalent to Figure 3 The shortest distance W3 is shown. Figure 2 As shown in FIG. 1 , “distance Z” is the distance from the inner surface 142 of the sealing plate 14 to the top 90E of the protrusion 90. Figure 2 As shown, "angle θ" is the angle between the line segment LS and the straight line L1.

[0086] <Evaluation>

[0087] The evaluation criteria of each sample are as follows.

[0088] 「○」:

[0089] On the inner surface 142 of the sealing plate 14 , the electrolyte does not adhere to the liquid injection hole 17 (there is an effect of suppressing the adhesion of the electrolyte to the liquid injection hole 17 ).

[0090] "×":

[0091] On the inner surface 142 of the sealing plate 14 , the electrolyte solution adheres to the liquid injection hole 17 (there is no effect of suppressing the adhesion of the electrolyte solution to the liquid injection hole 17 ).

[0092] [Table 1]

[0093] Table 1

[0094] "@

[0095]

[0096] When the protrusion 90 is provided only on the first short side 14c of the sealing plate 14, as shown in Table 1, it can be seen that the smaller the angle θ is, the more the effect of the technology disclosed herein can be achieved. In addition, it can be seen that the smaller the distance Z is, the more the effect of the technology disclosed herein can be achieved. In addition, it can be seen that the closer the protrusion 90 is to the injection hole 17 (that is, the larger the distance X is), the more the effect of the technology disclosed herein can be achieved.

[0097] As described above, specific aspects of the technology disclosed herein include the following items.

[0098] Item 1:

[0099] A power storage device, the power storage device comprising an electrode body, an electrolyte, and a shell for accommodating the electrode body and the electrolyte, the shell comprising: a shell body having a rectangular bottom surface, an opening facing the bottom surface, a pair of facing wide surfaces extending from a pair of facing long sides in the bottom surface, and a pair of facing narrow surfaces extending from a pair of facing short sides in the bottom surface; and a rectangular sealing plate, the sealing plate sealing the opening,

[0100] The sealing plate has a first long side and a second long side facing each other and a first short side and a second short side facing each other.

[0101] The sealing plate has a liquid injection hole for injecting the electrolyte at a position closer to the first short side than a straight line CL passing through a midpoint M1 of the first long side and a midpoint M2 of the second long side,

[0102] Here, the sealing plate has a pair of protrusions protruding from the inner surface of the bottom surface toward the inner side of the housing.

[0103] The pair of protrusions are provided at locations of the inner surface that are symmetrical with respect to the liquid injection hole in the longitudinal direction of the sealing plate.

[0104] Item 2:

[0105] The electric storage device according to claim 1, wherein the protrusion has a flat surface facing a side opposite to the other protrusion.

[0106] Item 3:

[0107] According to the electric storage device according to claim 1 or 2, the protrusion is in a plate shape, has a flat first surface on the other protrusion side, and has a flat second surface on the opposite side to the first surface.

[0108] Item 4:

[0109] According to any one of claims 1 to 3, the protrusion is inclined relative to the inner surface of the sealing plate, and the other of the angles formed between the protrusion and the inner surface is smaller than 90 degrees on the protrusion side.

[0110] Item 5:

[0111] The electrical storage device according to any one of claims 1 to 4, wherein, when the shortest distance between the first short side and the second short side is 1, the shortest distance from the injection hole to the protrusion is 0.06 to 0.13.

[0112] Item 6:

[0113] According to any one of claims 1 to 5, the protrusion is provided continuously and integrally with the sealing plate.

[0114] Item 7:

[0115] According to any one of claims 1 to 5, the sealing plate includes an insulating member extending along the inner surface, and a part of the insulating member constitutes the protrusion.

[0116] The above describes the implementation methods of the technology disclosed herein, but it is not intended to limit the technology disclosed herein to the above implementation methods. The technology disclosed herein can also be implemented in other implementation methods. The technology described in the claims includes technologies obtained by various deformations and changes to the above-mentioned exemplified implementation methods. For example, part of the above-mentioned implementation method can be replaced with other deformation methods, and other deformation methods can be added to the above-mentioned implementation method. In addition, if the technical feature is not described as a necessary feature, it can also be appropriately deleted.

Claims

1. An electrical storage device, comprising an electrode body, an electrolyte, and a shell for accommodating the electrode body and the electrolyte, the shell comprising: a shell body having a rectangular bottom surface, an opening facing the bottom surface, a pair of facing wide surfaces extending from a pair of facing long sides in the bottom surface, and a pair of facing narrow surfaces extending from a pair of facing short sides in the bottom surface; and a rectangular sealing plate, the sealing plate sealing the opening, wherein: The sealing plate has a first long side and a second long side facing each other and a first short side and a second short side facing each other. The sealing plate has a liquid injection hole for injecting the electrolyte at a position closer to the first short side than a straight line (CL) passing through a midpoint (M1) of the first long side and a midpoint (M2) of the second long side, Here, the sealing plate has a pair of protrusions protruding from the inner surface of the bottom surface toward the inner side of the housing. The pair of protrusions are provided at locations of the inner surface that are symmetrical with respect to the liquid injection hole in the longitudinal direction of the sealing plate.

2. The power storage device according to claim 1, wherein The protrusion has a flat surface facing a side opposite to the other protrusion.

3. The power storage device according to claim 1, wherein The protrusion is plate-shaped and has a flat first surface on the other protrusion side and a flat second surface on the side opposite to the first surface.

4. The power storage device according to claim 1, wherein The protrusion is inclined relative to the inner surface of the sealing plate, The other of the angles formed between the protrusion and the inner surface on the protrusion side is smaller than 90 degrees.

5. The power storage device according to claim 1, wherein When the shortest distance between the first short side portion and the second short side portion is 1, the shortest distance from the liquid injection hole to the protrusion portion is greater than or equal to 0.06 and less than or equal to 0.

13.

6. The power storage device according to any one of claims 1 to 5, wherein The protrusion is provided continuously and integrally with the sealing plate.

7. The power storage device according to any one of claims 1 to 5, wherein The sealing plate includes an insulating member extending along the inner surface, and a part of the insulating member constitutes the protruding portion.