Coatings for distal plasma source applications and methods of making same
By using chelating agents and post-treatment technology in remote plasma source applications, the durability and pollution problems of the coating under extreme conditions are solved, and a high-efficiency and low-pollution coating is achieved, which improves the output efficiency and life. It is suitable for In hydrogen-related plasma applications.
Patent Information
- Application Number
- CN202380033577.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-15
- Filing Date
- 2023-04-13
- Publication Date
- 2024-11-22
AI Technical Summary
The coatings in existing remote plasma source applications have durability and pollution problems under extreme operating conditions. The hard anodized coating reacts in fluorine chemicals to form pollution. The PEO coating has metal contamination and low output efficiency. question.
Using chelating agents and electrolytes, the metal content is reduced and the surface is smoothed by combining plasma electrolytic oxidation process and post-treatment technology. .
It significantly reduces metal contamination, improves surface finish and radical output efficiency, extends the service life of the coating, and achieves output performance comparable to HA and PEO coatings in hydrogen-related plasma.
Smart Images

Figure CN119013760A_ABST
Abstract
Description
[0001] CROSS REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of U.S. Provisional Patent No. 63 / 331,735, filed on April 15, 2022, and entitled “Coatings for Use in Remote Plasma Source Applications and Method of Manufacture.” Technical Field
[0003] The present application relates to coatings for remote plasma source applications and a method for making such coatings. Background Art
[0004] Remote plasma sources are commonly used in the manufacture of semiconductors. Historically, remote plasma sources, i.e., remote plasma coaters and products (hereinafter referred to as RPS) have been manufactured from a variety of materials. Typically, the plasma-facing surfaces within the RPS are modified or otherwise coated to meet insulation requirements, extend chamber life, and facilitate chamber cleaning between processing cycles. The choice of plasma-facing materials for aluminum-based plasma coaters in RPS products is largely related to plasma conditions, application requirements, manufacturability, cost, and many other factors. Due to any number of factors, many commercially available materials and coating techniques cannot be used for remote plasma source applications. For example, the geometry and complexity of the coater design (partially enclosed inner surface, narrow plasma channel, and restrictions on overall size) and the extreme operating conditions (high-density plasma, high temperature, chemical attack, and ion bombardment) greatly reduce the number of commercially available materials and coating techniques that can be used for RPS applications.
[0005] Hard anodized (HA) treatment has been used to treat aluminum in RPS coaters for more than two decades. HA oxide coatings offer benefits such as good chemical resistance, suitable manufacturing processes for complex geometries, and good cost effectiveness. In the past, HA coatings for RPS applications have focused on chamber cleaning purposes. Although HA coatings have proven useful in the past, several disadvantages have been identified, especially in NF coatings. 3 For example, although anodized coatings on NF 3The HA coating has relatively good plasma resistance in an environment, but after exposure to fluorine chemicals, amorphous aluminum oxide and hydroxide will react with fluorine to form a thinner flaky layer of aluminum fluoride on top of the anodized layer, which can cause contamination in the RPS. In addition, the anodized layer will degrade over time and reduce the operational service life of the block used for the RPS. In addition, the porous nature and cracks in the HA coating due to thermal mismatch in the anodizing also have a negative impact on its dielectric strength. Arcing problems occur especially in worn surfaces. Figures 1a to 1c illustrate such negative effects on the surface of the anodized layer. More specifically, Figure 1a shows the porous surface of the anodized surface in a plan view, while Figure 1b shows an anodized coating with cracks and defects after plasma exposure in a cross-sectional view, and Figure 1c shows arc marks on a curved anodized surface after plasma exposure.
[0006] In view of the foregoing, a number of alternative processing technologies and materials have been developed. For example, plasma electrolytic oxidation (PEO) coating has been used in some RPS applications for some time. Unlike anodization, the partially crystallized aluminum oxide in the PEO coating is 3 It provides more robust corrosion resistance (at least 2 to 3 times longer life than HA) in plasma and other chemicals. In addition, the denser and less porous structure formed by PEO treatment forms a coating with a dielectric strength about 1.5 to 2 times higher than that of HA treatment. Unfortunately, there are also disadvantages of the PEO process. For example, the high voltage / energy required during the film growth process penetrates the oxide layer and creates an open channel to the base alloy. In addition, trace metals in the base alloy can be transported to the surface over time during the process. These trace metals can be oxidized and solidified after cooling, while the PEO coating process continues until the desired thickness is reached. Therefore, it has been found that some metals in the PEO coating (such as copper, iron and manganese) have extremely uneven distribution due to several factors (including the activity of the trace metals). This high metal concentration feature in the PEO surface can cause potential metal contamination downstream of the RPS after exposure to plasma.
[0007] In some applications, hydrogen can be used to form plasma. In applications of hydrogen-related plasmas (such as H2 and NH3), the output of the PEO-coated RPS can be significantly lower than that of the HA-coated RPS (about 40% to 50% lower). The lower output of the PEO-coated RPS can be caused by any number of factors, including the higher surface recombination rate of the PEO coating and the larger surface area of the PEO coating. As mentioned above, the process of PEO coating can continuously introduce metals into the top surface of the coating, and then oxidize and solidify these metals. When the process is completed, a nodular structure can be formed on the top surface. The layer thickness of the nodular structure is in the range of about 0.25 μm to 35 μm, and the total thickness is up to 50 um. The total surface area is about 3 to 4 times that of HA. Therefore, a larger surface area can significantly increase the chance of free radical adsorption, thereby causing a high recombination rate. In addition, the higher metal concentration in the PEO surface and the relatively low content of hydroxide (known to have a lower H recombination rate than oxide) can also promote a higher recombination rate.
[0008] In view of the foregoing, there is a continuing need for coatings for the plasma-facing surface of RPS that provide the benefits of both HA and PEO coatings while avoiding their disadvantages. Summary of the invention
[0009] The present application discloses various embodiments and methods to provide solutions to the above-mentioned technical needs, as will become apparent in the following description.
[0010] In one embodiment, the present application discloses a method for coating a plasma channel of a plasma source, the method comprising: providing at least one electrolyte having one or more chelating agents therein; treating at least one surface to produce a treated surface; smoothing the surface of the treated surface with at least one post-treatment technique to produce at least one smoothed treated surface; and cleaning the smoothed surface. The surface may be a plasma-facing surface of a plasma source, and treating the surface to produce a treated surface includes treating at least one surface using a plasma electrolytic oxidation process. Alternatively, treating the surface produces a surface treated by plasma electrolytic oxidation. The post-treatment technique includes a dry bead blasting process, and the dry bead blasting process uses high-purity aluminum oxide as a blasting medium. The post-treatment technique may be performed at a pressure of about 10 psi to about 200 psi and at a blasting angle of about 15 degrees to about 90 degrees. The post-treatment technique is configured to remove a layer of about 0.25 μm to about 35 μm of the surface and reduce the surface roughness and surface area by 30% to 50% of its original size. The post-treatment technique includes a steam blasting process. Steam blasting uses pressurized water and at least one abrasive medium to modify a surface. Cleaning involves applying high frequency ultrasonic energy for an extended period of time to remove small particles and embedded process residues from the surface.
[0011] According to another embodiment, the present application discloses a coating for remote plasma source applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] The above and other aspects, features and advantages of the coatings and methods of making the same for remote plasma source applications as disclosed herein will become more apparent from the subsequent description thereof presented in conjunction with the following drawings, in which:
[0013] 1a to 1c illustrate the negative effects of hard anodizing on the surface of the anodized layer;
[0014] 2a and 2b illustrate 3D images of a standard PEO surface (where the inset is in plan view) and a 3D image of a post-treated PEO surface (where the inset is in plan view), respectively;
[0015] Figure 3 A statement of the test results regarding the metal content collected in downstream wafers; and
[0016] Figure 4 is the representation of experimental data, and
[0017] Figure 5 A flow chart showing a method of coating a plasma channel of a plasma source. DETAILED DESCRIPTION
[0018] Exemplary embodiments of methods of coating a plasma channel of a plasma source and coatings for remote plasma source applications are described below with reference to the accompanying drawings. Unless otherwise expressly stated, in the drawings, the size, position, etc. of components, features, elements, etc., and any distances therebetween are not necessarily to scale and may be asymmetric and / or exaggerated for clarity.
[0019] The terms used herein are for the purpose of describing specific exemplary embodiments only and are not intended to be limiting. As used herein, the singular forms "a / an" and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It should be recognized that the term "comprise / comprising" when used in this specification specifies the presence of the stated features, integrals, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, integrals, steps, operations, elements, components and / or groups thereof. Unless otherwise specified, when describing a value range, the value range includes both the upper and lower limits of the range and any sub-ranges therebetween. Unless otherwise indicated, terms such as "first", "second", etc. are only used to distinguish one element from another.
[0020] Unless otherwise indicated, the terms "about," "approximately," and the like mean that amounts, sizes, formulations, parameters, and other quantities and characteristics are not and need not be exact but may be approximate and / or larger or smaller, as necessary, reflecting tolerances, conversion factors, rounding, measurement errors and the like, as well as other factors known to those of ordinary skill in the art.
[0021] Many of the embodiments described in the following description share common components, devices, and / or elements. Similar-named components and elements refer to similarly-named elements throughout. Therefore, the same or similarly-named components or features may be described with reference to other figures, even if such components or features are not mentioned or described in the corresponding figures. In addition, even elements not indicated by reference numbers may be described with reference to other figures.
[0022] Without departing from the spirit and teachings of the present invention, many different forms and embodiments are possible, and therefore, the present disclosure should not be considered limited to the exemplary embodiments set forth herein. Rather, these exemplary embodiments are provided so that the present disclosure will be thorough and complete, and will convey the scope of the present disclosure to those having ordinary knowledge in the art.
[0023] The present application discloses various coatings for use with remote plasma source applications, and methods of applying the coatings to surfaces of remote plasma sources and devices associated therewith. In one specific example, the coatings may be applied to plasma-facing surfaces of remote plasma sources and associated devices, but it should be understood by those skilled in the art that the coatings may be applied to any surface. In addition, it should be understood by those skilled in the art that the methods described herein may be used to coat any type of material. For example, there are two potential sources of metals that may directly affect the metal concentration in the coating. More specifically, as described above with respect to PEO coatings, contamination may originate from trace metals from Al6061-based alloys and the coating environment (e.g., corroded electrodes). Therefore, the present application is particularly concerned with finding solutions to prevent the formation of metal oxides on surfaces.
[0024] Chelating agents are chemical compounds that can bind to metal ions to form stable, water-soluble metal complexes that prevent unwanted precipitation, dissolve scale deposits, and optimize oxidation processes. These materials can be used in different fields, such as medical applications, corrosion control, water treatment, etc. The technology of providing more desirable coatings for plasma-facing surfaces of RPS and related systems involves the use of one or more chelating agents to control and reduce the metal content in the PEO coating. More specifically, the selected chelating agent is added to the electrolyte before coating. During the PEO coating process, the chelating agent couples to the unwanted metal ions in the electrolyte (either from the base alloy or the corroded electrode) and approaches the surface area to prevent the formation of metal oxides in the coating. The metal complex formed is retained in the electrolyte, thereby reducing or preventing the metal from returning to the coating.
[0025] Any of a variety of chelating agents or materials may be used. The selection of an appropriate chelating agent material requires consideration of various factors, such as the type of ions to be removed, the strength of the metal complex formed, the pH of the electrolyte and its possible effect on the coating range and quality. In addition, the electrical range may be adjusted to maintain the coating quality.
[0026] In one embodiment, a post-treatment of the PEO-coated surface is performed to enhance the performance of the RPS. Any of a variety of post-treatment processes configured to smooth the rough surface of the PEO coating may be used, such as a dry bead blasting process. For example, high purity aluminum oxide (e.g., high purity (i.e., greater than 90%) AlO) may be used as a blasting medium. Pressure, blasting angle, and treatment time may be optimized to provide the desired surface smoothness. Exemplarily, the blasting medium comprises 400 mesh particles, having a particle size of about 20 to 40 um, having a large shape with sharp edges. Its delivery is performed by spraying with a nozzle under pressurized air.
[0027] In one embodiment, post-treatment is performed at a certain pressure and blasting angle (about 10 psi to about 200 psi at an angle of about 15 degrees to about 90 degrees), but it should be understood by those of ordinary skill in the art that any type of pressure, blasting angle, and treatment time can be used to remove any amount of material from the coated surface.
[0028] In one embodiment, the pressure, blasting angle, and treatment time of the post-treatment are optimized to remove a layer of coating from about 0.25 μm to about 35 μm thick and reduce the surface roughness and surface area by 30% to 50% or more from the original. Optimization is achieved by treating many different samples at different angles, pressures, treatment times, and media types. The resulting surface area and roughness are then measured using a microscope, and the best conditions are selected.
[0029] The surface produced by the post-treatment described above enhances the surface produced by the PEO process, and the roughness of the surface is similar to the roughness produced by the surface treated by standard PEO. Therefore, the developed bead blasting process described herein can be directly adopted and applied to the surface treated by chelation enhanced PEO to achieve the same finish on the surface. Figures 2a and 2b illustrate the 3D image of the standard PEO surface (wherein the inset is in the plan view) and the 3D image of the post-treated PEO surface (wherein the inset is in the plan view) respectively.
[0030] Alternatively, in another embodiment, steam blasting may be used instead of dry bead blasting. Unlike dry bead blasting, steam blasting uses pressurized water and at least one abrasive medium to modify the surface. In addition, steam blasting is a substantially dust-free process, thereby providing a final surface with less embedded residue while potentially providing a smoother surface than a dry bead blasted surface.
[0031] Optionally, the coated surface may be further treated with an optimized post-cleaning process after the bead blasting step. More specifically, the additional cleaning process includes applying a higher frequency ultrasonic energy cleaning for a longer period of time to remove small particles and embedded process residues. Ultrasonic and UHF ultrasonic cleaning use sound waves propagating in a liquid and produce a cycle of compression and rarefaction. During rarefaction, the liquid is bubbled to produce bubbles filled with steam. The bubbles continue to grow and finally implode to generate local heat and energy. The forces generated by these small implosions can physically remove embedded particles or contamination. Ultrasonic cleaning is conducive to quickly and completely dissolving and replacing particles. The typical frequency range of ultrasonic cleaning is between 25 and 270 kHz, while the frequency range of UHF ultrasonic cleaning is within 360 kHz to 2 MHz or higher. It is envisioned that frequencies above 100 kHz are used for precision cleaning according to the present invention. According to a specific example of the present invention, a frequency of 120 kHz is used. Higher frequency cleaning (such as UHF ultrasonic cleaning) is particularly suitable for removing submicron particles from flat surfaces. The movement of the fluid in this frequency range results in more stable cavitation without implosion, which may cause less damage to the substrate. In one embodiment, the surface may be post-treated using ultrasonic cleaning followed by dry blasting.
[0032] The processes described above provide several advantages over prior art methods and coatings. More specifically, post-PEO process bead blasting and post-bead blasting ultrasonic cleaning performed in combination with a chelating enhanced PEO process produces:
[0033] (1) Clean coating (low metal contamination) - The coating inside the RPS coater is part of the material facing the plasma. After exposure to the plasma, some degree of corrosion and surface reaction is expected. The metal concentration in the coating can directly affect the level of metal contamination outside the RPS. Therefore, reducing the metal content in the coating (source) should be the most direct improvement. Figure 3 The test results in Figure 2 show that the majority of metal content collected downstream on the wafer has been significantly reduced. Metal contamination can be extremely damaging to the wafer during semiconductor manufacturing processes. Applicators with a cleaner coating should increase the chances of RPS being applied to the process on the wafer.
[0034] (2) Lower recombination rate / higher free radical output - Previous tests have shown that standard PEO coatings have a high free radical output in hydrogen and NH 3 The plasma has much lower free radical output (about half) than the HA coating. This can be attributed to the higher free radical recombination rate in the PEO surface. The larger surface area with nodular structure was identified as the potential root cause. The implementation of proper post-treatment and cleaning process has significantly improved the surface finish and cleanliness. Experimental data (see Figure 4 , where PED refers to the thermal output of RPS under PEO, NC-1 and 2 refer to new coatings, and HA refers to H 2 (upper) and NH 3 (Bottom) Coatings in plasma) demonstrate that coatings subjected to such treatments exhibit output performance equivalent to (or better than) PEO and HA in hydrogen-based plasmas. This improvement in radical output further enhances the opportunities of RPS in applications that particularly require hydrogen-based plasmas, such as etching and deposition processes.
[0035] (3) Compared to HA and standard PEO coatings, the coatings and methods described herein have the benefits of standard PEO coatings, such as high corrosion resistance and dielectric strength, with additional significant improvements in metal content and reduction in surface recombination rate. It is expected that the RPS process described herein will be applied to more semi-processes besides chamber cleaning with excellent performance.
[0036] In addition, various other processing steps may be added to the methods described herein, or in the alternative, one or more of the steps described herein may be replaced. For example, extrusion honing may be used to finish the interior surface. More specifically, in one embodiment, a chemically inactive and non-corrosive medium may be flowed through the workpiece. Abrasive particles in the medium may be used to grind away undesirable materials to achieve a desired finish.
[0037] Optionally, atomic layer deposition (hereinafter ALD) may be used to provide a conformal coating on the surface of the RPS and is configured to provide a layer of a selected coating for the desired purpose. For example, an ALD coating of aluminum oxide, aluminum nitride, or silicon oxide may provide less reaction with chlorine or hydrogen radicals.
[0038] According to another embodiment, the ALD treatment is performed after bead blasting the surface, but it should be understood by those of ordinary skill in the art that the ALD coating can be applied to the RPS at any time.
[0039] According to other alternative embodiments, instead of ALD, other deposition methods such as CVD and PVD may be employed, alone or in combination.
[0040] Figure 5 The method of the present invention according to one of the specific examples of the present invention is briefly described.
[0041] Specifically speaking, Figure 5 A method 400 of coating a surface of a plasma source is illustrated. As shown, the method 400 includes the steps of providing 402 at least one electrolyte having one or more chelating agents therein; another step 404 of treating at least one surface to produce a treated surface; another step 406 of smoothing the surface of the treated surface with at least one post-treatment technique to produce at least one smoothed treated surface; and another step 408 of cleaning the smoothed surface.
[0042] The surface may be a surface of a plasma source facing the plasma, and the step 404 of treating the surface to produce a treated surface includes treating at least one surface using a plasma electrolytic oxidation process. Treating at least one surface produces a surface treated by plasma electrolytic oxidation. The post-treatment technique includes a dry bead blasting process, and the dry bead blasting process uses high purity aluminum oxide as a blasting medium.
[0043] The post-treatment technique may be performed at a pressure of about 10 psi to about 200 psi and at a blasting angle of about 15 degrees to about 90 degrees. In one embodiment, the post-treatment technique is configured to remove a layer of about 0.25 μm to about 35 μm of the surface and reduce the surface roughness and surface area by 30% to 50% of its original size.
[0044] Optionally, post-treatment techniques may include a steam blasting process. Steam blasting uses pressurized water and at least one abrasive medium to modify the surface. Cleaning step 408 includes applying high frequency ultrasonic energy cleaning for a longer period of time to remove small particles and embedded process residues from the surface.
[0045] The specific examples disclosed herein illustrate the principles of the present invention. Other modifications that fall within the scope of the present invention may be employed. Therefore, the devices disclosed in this application are not limited to the devices precisely shown and described herein.
Claims
1. A method for coating a plasma channel of a plasma source, comprising: providing at least one electrolyte having one or more chelating agents therein; treating at least one surface of the plasma channel to produce a treated surface; smoothing the surface of the treated surface using at least one post-treatment technique to produce at least one smoothed treated surface; and Clean the smooth surface.
2. The method of claim 1, wherein the surface is a plasma-facing surface of a plasma source.
3. The method of claim 1, wherein treating at least one surface of the plasma channel to produce a treated surface comprises treating the at least one surface using a plasma electrolytic oxidation process.
4. The method of claim 1, wherein the treatment produces a surface treated with plasma electrolytic oxidation.
5. The method of claim 1, wherein the at least one post-processing technique comprises a dry bead blasting process.
6. The method of claim 5, wherein the dry bead blasting process uses high purity alumina as a blasting medium.
7. The method of claim 1, wherein the at least one post-treatment technique is performed at a pressure of about 10 psi to about 200 psi and at a blasting angle of about 15 degrees to about 90 degrees.
8. The method of claim 1, wherein the at least one post-processing technique is configured to remove a layer of about 0.25 μm to about 35 μm of the surface and reduce surface roughness and surface area by 30% to 50% of their original size.
9. The method of claim 1, wherein the at least one post-treatment technique comprises a vapor blasting process.
10. The method of claim 1, wherein the vapor blasting uses pressurized water and at least one abrasive medium to modify the surface.
11. The method of claim 1, wherein the cleaning comprises applying high frequency ultrasonic energy cleaning for an extended period of time to remove small particles and embedded process residues from the surface.
12. A coating for remote plasma source applications, comprising: A surface is obtained by the following steps: providing at least one electrolyte having one or more chelating agents therein; treating at least one surface to produce a treated surface; smoothing the surface of the treated surface using at least one post-treatment technique to produce at least one smoothed treated surface; and Clean the smooth surface.
13. The coating of claim 12, wherein the surface comprises a plasma-facing surface of a plasma source.
14. The coating of claim 12, wherein the surface comprises a surface treated with plasma electrolytic oxidation.