Semiconductor die with metal plate layer
By setting the metal plate layer and bump structure on the back side of the semiconductor die, the warping problem in semiconductor die manufacturing is solved, compensation for the difference in thermal expansion rate and the stability of electrical connection are achieved, and the anti-curve of the die is improved Curvature and bending resistance.
Patent Information
- Application Number
- CN202311750657.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-23
- Filing Date
- 2023-12-19
- Publication Date
- 2024-11-26
AI Technical Summary
In semiconductor die manufacturing processes, semiconductor dies are prone to warping, resulting in bending and layering problems caused by differences in component layering and thermal expansion rates during the manufacturing process.
Using a structural design with a metal plate layer, a first backside metal plate layer and a second backside metal plate layer are provided on the backside of the semiconductor die, and a backside bump structure is provided between the through electrode area and the dummy area. , to compensate and reduce thermal expansion differences between the substrate and the insulating layer, preventing warping and bending.
Effectively prevent and reduce the warping and bending of semiconductor dies, enhance the resistance to warping and bending, ensure stable and electrical connections between components, and improve the reliability of the manufacturing process.
Smart Images

Figure CN119028946A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present disclosure generally provide semiconductor dies, and more particularly, provide semiconductor dies having a metal plate layer. Background Art
[0002] Warping of the semiconductor die occurs during the semiconductor die manufacturing process. Summary of the invention
[0003] An embodiment of the present disclosure provides a semiconductor die, which includes: a substrate having a front side surface and a back side surface; an interlayer insulating layer, which is arranged below the front side surface of the substrate; a horizontal metal interconnect, which is arranged in the interlayer insulating layer; a front side pad, which is arranged below the lower surface of the interlayer insulating layer; a front side bump structure, which is arranged below the lower surface of the front side pad; a through electrode, which vertically passes through the substrate; a back side insulating layer, which is arranged above the back side surface of the substrate; a first back side metal plate layer, which is arranged above the back side insulating layer; a back side passivation layer, which is arranged above the back side insulating layer and covers the first back side metal plate layer; and a back side bump structure, which is arranged above the through electrode and the back side passivation layer. The through electrode has a protruding portion that vertically passes through the back side passivation layer and the first back side metal plate layer. The protruding portion protrudes upward from the back side surface of the substrate.
[0004] An embodiment of the present disclosure provides a semiconductor device, which includes: a substrate having a through-electrode region and a dummy region; an interlayer insulating layer, which is arranged below the active surface of the substrate; a horizontal metal interconnection, which is arranged in the interlayer insulating layer; a front side passivation layer, which is arranged below the lower surface of the interlayer insulating layer; a front side bump structure, which is arranged below the lower surface of the front side passivation layer in the through-electrode region; a dummy front side bump structure, which is arranged below the lower surface of the front side passivation layer in the dummy region; a back side insulating layer, which is arranged above the in-active surface of the substrate; a first back side metal plate layer, which is arranged above the back side insulating layer; the back side passivation layer, which is arranged above the first back side metal plate layer; a through electrode, which vertically passes through the substrate, the back side insulating layer, the first back side metal plate layer and the back side passivation layer in the through-electrode region; the back side bump structure, which is arranged above the through-electrode in the through-electrode region; and a dummy back side bump structure, which is arranged above the back side passivation layer in the dummy region. BRIEF DESCRIPTION OF THE DRAWINGS
[0005] Figure 1 is a top view showing a backside surface of a semiconductor die according to an embodiment of the present disclosure.
[0006] Figure 2A , Figure 2B , Figure 2C , Figure 2D and Figure 2E is a longitudinal cross-sectional view showing a semiconductor die according to an embodiment of the present disclosure.
[0007] Figure 3A , Figure 3B , Figure 4A , Figure 4B , Figure 5A and Figure 5B is a top view of a semiconductor die according to an embodiment of the present disclosure and along Figure 1 A longitudinal cross-sectional view taken along line II'. DETAILED DESCRIPTION
[0008] The embodiments will be described in more detail below with reference to the accompanying drawings. However, the embodiments may be embodied in different forms and should not be construed as being limited to the embodiments set forth herein. Throughout this disclosure, in the various drawings and embodiments of the present invention, the same reference numerals represent the same components.
[0009] It should be understood that although the terms "first" and / or "second" may be used herein to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. For example, without departing from the teachings of the present disclosure, the first element discussed below may be referred to as the second element. Similarly, the second element may also be referred to as the first element.
[0010] Other expressions explaining the relationship between elements (such as “between,” “directly between,” “adjacent to,” or “directly adjacent to”) should be interpreted in the same manner.
[0011] The drawings are not necessarily drawn to scale, and in some cases, the proportions may have been exaggerated in order to clearly illustrate the features of the embodiments. When the first layer is referred to as being "on" the second layer or "on" the substrate, it refers not only to the situation where the first layer is directly formed on the second layer or the substrate, but also to the situation where there is a third layer between the first layer and the second layer or between the first layer and the substrate. For example, it will be understood that when an element or layer, etc. is referred to as "on another element or layer, etc.," "connected to," or "coupled to," another element or layer, etc., it can be directly on another element or layer, etc., directly connected to or coupled to another element or layer, etc., or there can be an intermediate element or layer, etc. On the contrary, when an element or layer, etc. is referred to as "directly on another element or layer, etc.," "directly connected to," or "directly coupled to," another element or layer, etc., there is no intermediate element or layer, etc.
[0012] Embodiments of the present disclosure provide a structure for preventing or reducing warping of a semiconductor die.
[0013] Embodiments of the present disclosure provide a semiconductor die having a metal plate layer.
[0014] Figure 1 is a top view showing the backside surface of the semiconductor die 100 according to an embodiment of the present disclosure. Figure 1 , the semiconductor die 100 according to an embodiment of the present disclosure may include a through-electrode area TA and a dummy area DA. The through-electrode area TA may be disposed between the dummy areas DA. The backside bump structure 50 may be disposed in the through-electrode area TA, and the dummy backside bump structure 50D may be disposed in the dummy area DA. The backside bump structure 50 and the dummy backside bump structure 50D may be arranged in a grid array shape.
[0015] FIG. 2A to FIG. 2E is a longitudinal cross-sectional view showing semiconductor dies 100A to 100E according to an embodiment of the present disclosure. For example, FIG. 2A to FIG. 2E It is along Figure 1 A longitudinal cross-sectional view taken along line II' and / or II-II'. Figure 1 and Figure 2A , the semiconductor die 100A according to the embodiment of the present disclosure may include a substrate 10, a through electrode 13, a front side bump structure 20, a dummy front side bump structure 20D, a first back side metal plate layer 41, a back side bump structure 50 and a dummy back side bump structure 50D. The semiconductor die 100A may also include an interlayer insulating layer 12, a horizontal metal interconnect 15, a vertical via plug 16, a front side passivation layer 17, a front side pad 19, a back side insulating layer 31 and a back side passivation layer 32. The through electrode 13, the front side bump structure 20, the back side bump structure 50, the vertical via plug 16 and the front side pad 19 may be disposed in a through electrode area TA. The dummy front side bump structure 20D and the dummy back side bump structure 50D may be disposed in a dummy area DA. The interlayer insulating layer 12, the horizontal metal interconnection 15, the front side passivation layer 17, the back side passivation layer 32 and the first back side metal plate layer 41 may be disposed in both the through electrode area TA and the dummy area DA. In the through electrode area TA, the through electrode 13, the horizontal metal interconnection 15, the vertical via plug 16, the front side pad 19, the front side bump structure 20 and the back side bump structure 50 may be electrically connected to each other. In the dummy area DA, the horizontal metal interconnection 15, the dummy front side bump structure 20D and the dummy back side bump structure 50D may not be electrically connected to each other.
[0016] The substrate 10 may include a semiconductor layer such as a silicon wafer, a silicon germanium wafer, an epitaxially grown silicon layer, an epitaxially grown silicon germanium layer, or SOI (silicon on insulator). In an embodiment, the substrate 10 may include a silicon wafer. The substrate 10 may have a front surface Sa and a back surface Sb. The front surface Sa may correspond to an active surface of the substrate 10, and the back surface Sb may correspond to an inactive surface of the substrate 10. For example, active circuit elements such as transistors may be provided on the front surface Sa of the substrate 10, and no active circuit elements may be provided on the back surface Sb of the substrate 10. In the accompanying drawings, the front surface Sa of the substrate 10 may face downward, and the back surface Sb of the substrate 10 may face upward.
[0017] Circuit elements such as transistors and metal interconnects may be disposed on the front side surface Sa of the substrate 10. An interlayer insulating layer 12 may be disposed on the front side surface Sa of the substrate 10 to cover the circuit elements. The interlayer insulating layer 12 may include a silicon oxide-based insulating layer and a silicon nitride-based insulating layer.
[0018] The through electrode 13 may vertically pass through the substrate 10. The through electrode 13 may pass through a portion of the interlayer insulating layer 12. The through electrode 13 may include a protruding portion 13p protruding upward from the backside surface Sb of the substrate 10 to be exposed. For example, the top end of the through electrode 13 may protrude upward from the backside surface of the substrate 10 to be exposed. The through electrode 13 may include copper.
[0019] The horizontal metal interconnection 15 may be connected to the end of the through electrode 13 in the interlayer insulating layer 12. Although not shown, the horizontal metal interconnection 15 may include a plurality of metal layers extending in a horizontal direction. The horizontal metal interconnection 15 may include a metal such as copper or tungsten.
[0020] Vertical via plugs 16 may vertically penetrate interlayer insulating layer 12 and electrically connect horizontal metal interconnections 15 to front-side pads 19, respectively, in a vertical direction. In an implementation, vertical via plugs 16 may include a metal such as copper or tungsten.
[0021] The front side passivation layer 17 may be disposed below the lower surface of the interlayer insulating layer 12 disposed below the front side surface Sa of the substrate 10. The front side passivation layer 17 may include an insulating material such as silicon oxide or silicon nitride. The front side passivation layer 17 may surround the side surface of the front side pad 19. The front side passivation layer 17 may expose the lower surface of the front side pad 19.
[0022] In an implementation, front side pad 19 may include metal. For example, front side pad 19 may include aluminum or tungsten. Front side pad 19 may correspond to a top metal layer among a plurality of metal layers of a circuit element of a semiconductor device.
[0023] The front side bump structure 20 may be disposed in the through-electrode area TA under the lower surface of the front side pad 19. In the dummy area DA, the dummy front side bump structure 20D may be disposed under the lower surface of the front side passivation layer 17. The front side bump structure 20 may be electrically connected to the through-electrode 13, and the dummy front side bump structure 20D may not be electrically connected to the through-electrode 13.
[0024] Each front side bump structure 20 may include a front side bump under metallurgy (UBM) layer 21, a front side bump body 23, and a solder layer 25. Each dummy front side bump structure 20D may include a dummy front side bump under metallurgy layer 21D, a dummy front side bump body 23D, and a dummy solder layer 25D. The front side bump under metallurgy layer 21 may be directly disposed below the lower surface of the front side pad 19. The dummy front side bump under metallurgy layer 21D may be directly disposed below the lower surface of the front side passivation layer 17. Each of the front side bump under metallurgy layers 21 and each of the dummy front side bump under metallurgy layers 21D may include a lower bump under metallurgy layer and an upper bump under metallurgy layer. The lower bump under metallurgy layer may include a metal to enhance adhesion to the front side passivation layer 17 and the front side pad 19. For example, the lower bump under metallurgy layer may include a titanium layer or a titanium-tungsten layer. The upper bump under metallurgical layer may include at least one of a copper layer and a nickel layer. In the plating process for forming the front side bump body 23 and the dummy front side bump body 23D, the upper bump under metallurgical layer may be used as a seed layer. The front side bump body 23 and the dummy front side bump body 23D may include a metal with conductivity. For example, the front side bump body 23 and the dummy front side bump body 23D may include at least one of nickel or copper. In an embodiment, the front side bump body 23 and the dummy front side bump body 23D may include nickel with corrosion resistance. The solder layer 25 and the dummy solder layer 25D may include an alloy of metals such as tin (Sn) and silver (Ag).
[0025] The backside insulating layer 31 may be conformally disposed on the backside surface Sb of the substrate 10. A portion of the backside insulating layer 31 may protrude upward to surround the side surface of the protruding portion 13p of the through electrode 13 that protrudes upward from the backside surface Sb of the substrate 10 to be exposed. For example, the backside insulating layer 31 may be conformally disposed on the backside surface Sb of the substrate 10 and disposed on the side surface of the protruding portion 13p of the through electrode 13. The protruding portion of the backside insulating layer 31 may have a cylindrical shape or a tubular shape. The backside insulating layer 31 may include a silicon nitride-based insulating material.
[0026] The first back metal plate layer 41 may be disposed on the back insulating layer 31 in a plate shape. The first back metal plate layer 41 may be disposed to be horizontally spaced apart from the through electrode 13 in the through electrode area TA. The first back metal plate layer 41 may include a double layer having a lower metal layer and an upper metal layer. In an embodiment, the lower metal layer may include a metal adhesion layer to increase the bonding strength between the upper metal layer and the back insulating layer 31. For example, the lower metal layer may include a titanium layer or a titanium tungsten layer. The upper metal layer may include at least one of metals such as copper or nickel. The first back metal plate layer 41 may be formed using a physical vapor deposition (PVD) process such as sputtering. For example, both the lower metal layer and the upper metal layer may be formed using a PVD process.
[0027] The backside passivation layer 32 may be disposed on the backside insulating layer 31 to cover the first backside metal plate layer 41. The backside passivation layer 32 may surround a protruding portion of the backside insulating layer 31 surrounding a side surface of the protruding portion 13p of the through electrode 13. The top end surface of the through electrode 13, the top end surface of the backside insulating layer 31, and the top surface of the backside passivation layer 32 may be coplanar.
[0028] Each backside bump structure 50 may include a backside bump under metallurgical layer 51, a backside bump body 53, and a backside bump capping layer 55. Each dummy backside bump structure 50D may include a dummy backside bump under metallurgical layer 51D, a dummy backside bump body 53D, and a dummy backside bump capping layer 55D. In the through-electrode area TA, the backside bump under metallurgical layer 51 may be disposed on the top surface of the backside passivation layer 32, the top end surface of the backside insulating layer 31, and the top end of the through-electrode 13. In the dummy area DA, the dummy backside bump under metallurgical layer 51D may be disposed on the top surface of the backside passivation layer 32. The backside bump under metallurgical layer 51 and the dummy backside bump under metallurgical layer 51D may include a lower bump under metallurgical layer and an upper bump under metallurgical layer, respectively. The lower bump under metallurgical layer may include a metal layer such as a titanium layer or a titanium-tungsten layer. The upper bump under metallurgical layer may include the same metal as the back bump body 53. The upper bump under metallurgical layer may include at least one of copper and nickel. In the plating process for forming the back bump body 53 and the dummy back bump body 53D, the upper bump under metallurgical layer may be used as a seed layer. The back bump body 53 and the dummy back bump body 53D may include at least one of nickel or copper. The back bump capping layer 55 and the dummy back bump capping layer 55D may include a metal diffusion barrier layer such as nickel or an anti-oxidation metal or anti-corrosion metal such as gold. The back bump structure 50 may be vertically aligned with the through electrode 13 and electrically connected to the through electrode 13, respectively. The dummy back bump structure 50D may not be vertically aligned with the through electrode 13 and may not be electrically connected to the through electrode 13.
[0029] The first back metal plate layer 41 can compensate for thermal expansion of the metal layer and the insulating material layer disposed on the front surface Sa of the substrate 10. Therefore, the first back metal plate layer 41 can prevent, reduce and compensate for warping and bending of the substrate 10, the interlayer insulating layer 12, the horizontal metal interconnection 15, the front passivation layer 17, the back insulating layer 31 and the back passivation layer 32. In addition, the first back metal plate layer 41 can prevent and reduce delamination between elements.
[0030] Reference Figure 2B , the semiconductor die 100B according to the embodiment of the present disclosure may include a substrate 10, a through electrode 13, a front side bump structure 20, a dummy front side bump structure 20D, a first back side metal plate layer 41, a back side bump structure 50 and a dummy back side bump structure 50D. The first back side metal plate layer 41 may be disposed only in the dummy area DA. The first back side metal plate layer 41 may not be disposed in the through electrode area TA. The first back side metal plate layer 41 may be selectively disposed at a selected position. For example, when the operation of the semiconductor die 100B is affected by parasitic capacitance or electrical interference between the first back side metal plate layer 41 and the through electrode 13, the first back side metal plate layer 41 may be omitted in the through electrode area TA.
[0031] Reference Figure 2C , the semiconductor die 100C according to an embodiment of the present disclosure may further include a second backside metal plate layer 42 disposed on the first backside metal plate layer 41. In an embodiment, the second backside metal plate layer 42 may include the same metal as the upper metal layer of the first backside metal plate layer 41. For example, the second backside metal plate layer 42 may include at least one of copper and nickel. The first backside metal plate layer 41 may include a lower metal layer and an upper metal layer formed by a PVD process. The second backside metal plate layer 42 may include a metal layer formed by a plating process.
[0032] In another embodiment, the first back metal plate layer 41 may be a single layer including a titanium layer or a titanium tungsten layer formed by performing a PVD process. The second back metal plate layer 42 may be a double layer including a lower metal layer formed by performing a PVD process and an upper metal layer formed by performing a plating process. In the present embodiment, the lower metal layer and the upper metal layer of the second back metal plate layer 42 may include at least one of copper and nickel. For example, the lower metal layer and the upper metal layer of the second back metal plate layer 42 may include the same metal. The second back metal plate layer 42 may be twice as thick or thicker than the first back metal plate layer 41. The side surface of the first back metal plate layer 41 and the side surface of the second back metal plate layer 42 may be substantially vertically aligned with each other. In an embodiment, the side surface of the first back metal plate layer 41 may be undercut below the lower surface of the second back metal plate layer 42. The second back metal plate layer 42 may be disposed in both the through electrode area TA and the dummy area DA. In another embodiment, the second back metal plate layer 42 may not be disposed in the through electrode area TA. The second back-side metal plate layer 42 may be provided only in the dummy area DA.
[0033] From the viewpoint of the process for forming the first back side metal plate layer 41, in an embodiment, when it is difficult to perform a PVD process and an etching process, a plating process may be used to form the second back side metal plate layer 42 having a sufficient thickness. For example, the second back side metal plate layer 42 may be formed to be twice as thick as or thicker than the first back side metal plate layer 41. In an embodiment, by adding the second back side metal plate layer 42, the warping resistance and the bending resistance may be further enhanced. For example, when the first back side metal plate layer 41 does not sufficiently prevent the warping and the bending of the substrate 10, the second back side metal plate layer 42, which is thicker than the first back side metal plate layer 41, may strengthen the warping resistance and the bending resistance.
[0034] Reference Figure 2D, the semiconductor die 100D according to an embodiment of the present disclosure may include a first backside metal plate layer 41 electrically connected to the backside bump structure 50. A portion of the backside insulating layer 31 may protrude to conformally surround the side surface of the protruding portion 13p of the through electrode 13. The first backside metal plate layer 41 may include a horizontal plate portion 41a and a vertical protruding portion 41b. The horizontal plate portion 41a may have a plate shape between the backside insulating layer 31 and the backside passivation layer 32. The vertical protruding portion 41b may surround the side surface of the protruding portion of the backside insulating layer 31 surrounding the side surface of the protruding portion 13p of the through electrode 13. The vertical protruding portion 41b may protrude upward from the horizontal plate portion 41a to have a cylindrical shape or a tubular shape. Therefore, the first backside metal plate layer 41 and the backside bump under metallurgy layer 51 of the backside bump structure 50 may be physically and electrically connected to each other. When the through-electrode 13 and the backside bump structure 50 transmit a common electrical signal such as a common power supply voltage or a ground voltage, the first backside metal plate layer 41 can act as a power plane or a ground plane to electrically connect the through-electrode 13 to the backside bump structure 50. Therefore, the first backside metal plate layer 41 can provide a stable power supply effect, a decoupling effect, a shielding effect, and other electrical stabilization effects.
[0035] Reference Figure 2E , a semiconductor die 100E according to an embodiment of the present disclosure may include a substrate 10, a through electrode 13, a front side bump structure 20, a first back side metal plate layer 41 and a second back side metal plate layer 42, and a back side bump structure 50. The first back side metal plate layer 41 and the second back side metal plate layer 42 may be disposed on the through electrode 13. The semiconductor die 100E may further include a metal pattern 43 disposed on the second back side metal plate layer 42. The metal pattern 43 may be disposed between the second back side metal plate layer 42 and the back side bump structure 50. The metal pattern 43 may be disposed on a portion of the top surface of the second back side metal plate layer 42 in a shape protruding upward. The second back side metal plate layer 42 and the metal pattern 43 may form a step. The metal pattern 43 may be vertically aligned with the through electrode 13 and / or the back side bump structure 50. The metal pattern 43 may include the same metal as the second back side metal plate layer 42. Therefore, in an embodiment, the interface between the second backside metal plate layer 42 and the metal pattern 43 may exist virtually or may exist. The first backside metal plate layer 41 , the second backside metal plate layer 42 , the metal pattern 43 , and the backside bump structure 50 may be electrically connected to each other.
[0036] In another embodiment, the backside under bump metallurgy layer 51 may be omitted. For example, the metal pattern 43 and the backside bump body 53 may include the same material to be continuous with each other in material.
[0037] In another embodiment, the second backside metal plate layer 42 may be omitted. For example, the metal pattern 43 may be directly disposed on the first backside metal plate layer 41 in a mesa shape protruding upward. Therefore, the metal pattern 43 may be disposed between the first backside metal plate layer 41 and the backside bump structure 50.
[0038] The semiconductor die 100A to 100E according to the embodiment of the present disclosure may include backside metal plate layers 41 and 42 and metal pattern 43 disposed on the backside surface Sb of the substrate 10. Therefore, in the embodiment, warping caused by the difference in thermal expansion rate between the plurality of metal layers and the insulating layer disposed under the frontside surface Sa of the substrate 10 may be prevented, mitigated, and compensated.
[0039] Figure 3A and FIG. 3B to FIG. 5A and Figure 5B is a top view of a semiconductor die according to an embodiment of the present disclosure and along Figure 1 A longitudinal cross-sectional view taken along line II' of FIG. Figure 3A and Figure 3B , the first back metal plate layer 41 may include through-electrode holes Hv each having a circular shape. The first back metal plate layer 41 and the back bump structure 50 may not vertically overlap each other. In an embodiment, the maximum width (or diameter) W1 of the through-electrode hole Hv of the first back metal plate layer 41 and the maximum width (or diameter) W2 of the back bump structure 50 may be substantially the same.
[0040] Reference Figure 4A and Figure 4B , the first back metal plate layer 41 and the back bump structure 50 may partially overlap each other vertically. For example, in the vertical direction, a portion of the first back metal plate layer 41 may be located between the back insulating layer 31 and the back bump structure 50. For example, the maximum width (or diameter) W1 of the through electrode hole Hv of the first back metal plate layer 41 may be smaller than the maximum width (or diameter) W2 of the back bump structure 50. Figure 4A , the side surface of the first backside metal plate layer 41 is indicated by a dotted line. This embodiment may be applied when a decoupling effect or a shielding effect occurs between the through-electrode 13 and the backside bump structure 50 and the first backside metal plate layer 41.
[0041] Reference Figure 5A and Figure 5BIn an embodiment, the first back metal plate layer 41 and the back bump structure 50 may not overlap each other in the vertical direction. For example, the maximum width (or diameter) W1 of the through electrode hole Hv of the first back metal plate layer 41 may be greater than the maximum width (or diameter) W2 of the back bump structure 50. In the top view, the back passivation layer 32 may be exposed between the side of the first back metal plate layer 41 and the side of the back bump structure 50. This embodiment may be applied when signal interference occurs between the through electrode 13 and the back bump structure 50 and the first back metal plate layer 41.
[0042] exist Figure 3A and FIG. 3B to FIG. 5A and Figure 5B In an embodiment, the first back metal plate layer 41 may be replaced by the second back metal plate layer 42. That is, the first back metal plate layer 41 may include the second back metal plate layer 42. Therefore, in an embodiment, a process for manufacturing a semiconductor device may be simplified.
[0043] According to various embodiments of the present disclosure, warpage occurring in a semiconductor die manufacturing process may be prevented and reduced.
[0044] While various embodiments have been described with respect to specific embodiments, it will be apparent to those skilled in the art from this disclosure that various changes and modifications may be made without departing from the spirit and scope of the embodiments as defined in the appended claims.
[0045] CROSS-REFERENCE TO RELATED APPLICATIONS
[0046] This application claims the priority of Korean Patent Application No. 10-2023-0066122 filed on May 23, 2023 in the Korean Intellectual Property Office, the entire contents of which are incorporated herein by reference.
Claims
1. A semiconductor die, the semiconductor die comprising: a substrate having a front surface and a back surface; an interlayer insulating layer, the interlayer insulating layer being disposed below the front surface of the substrate; a horizontal metal interconnection disposed in the interlayer insulating layer; A front side pad, the front side pad being arranged below the lower surface of the interlayer insulating layer; A front side bump structure, the front side bump structure is arranged below the lower surface of the front side pad; A through electrode vertically passing through the substrate; a back insulating layer disposed above the back surface of the substrate; a first back metal plate layer, the first back metal plate layer being disposed above the back insulating layer; a backside passivation layer, the backside passivation layer being disposed above the backside insulating layer and covering the first backside metal plate layer; as well as a backside bump structure, the backside bump structure being arranged above the through electrode and the backside passivation layer, The through electrode has a protruding portion vertically passing through the back passivation layer and the first back metal plate layer, wherein the protruding portion protrudes upward from the back surface of the substrate.
2. The semiconductor die of claim 1 , further comprising: A front side passivation layer is disposed below the lower surface of the interlayer insulating layer to expose the lower surface of the front side pad and surround a side surface of the front side pad.
3. The semiconductor die of claim 2, further comprising: a dummy front bump structure disposed below the front passivation layer and a dummy back bump structure disposed above the back passivation layer, wherein the substrate includes a through-electrode region in which the through-electrode is disposed and a dummy region in which the through-electrode is not disposed, and Wherein, the dummy front-side bump structure and the dummy back-side bump structure are arranged in the dummy region.
4. The semiconductor die according to claim 1, in, The front side bump structure comprises: Metallurgical layer under the front bump; a front-side bump body disposed below a lower surface of the front-side bump lower metallurgical layer; and a solder layer located below the lower surface of the front bump body, and Wherein, the back side bump structure comprises: Back side sub-bump metallurgical layer; a backside bump body disposed above the backside bump lower metallurgical layer; and A backside bump capping layer is disposed above the backside bump body.
5. The semiconductor die according to claim 1, in, The first back metal plate layer comprises multiple layers, Wherein, the multiple layers include: a lower metal layer comprising titanium; and The upper metal layer includes at least one of copper and nickel.
6. The semiconductor die according to claim 1, in, The first back metal plate layer has through electrode holes, and Wherein, the through electrode vertically passes through the through electrode hole.
7. The semiconductor die according to claim 1, in, A portion of the backside insulating layer protrudes to conformally surround the side surface of the protruding portion of the through electrode.
8. The semiconductor die according to claim 7, in, The portion of the back-side insulating layer has a cylindrical shape or a tubular shape.
9. The semiconductor die according to claim 1, in, The first back metal plate layer comprises: a horizontal plate portion disposed between the back-side insulating layer and the back-side passivation layer to have a plate shape; and A vertical protrusion portion surrounds a side surface of the protrusion portion of the backside insulating layer surrounding the through electrode.
10. The semiconductor die according to claim 9, in, The vertical protruding portion of the first backside metal sheet layer is in contact with the backside bump structure.
11. The semiconductor die according to claim 9, in, The vertical protrusion portion of the first back metal sheet layer has a cylindrical shape or a tubular shape.
12. The semiconductor die of claim 1 , further comprising: a metal pattern disposed between the first backside metal plate layer and the backside bump structure, and Wherein, the metal pattern is vertically aligned with the through electrode and the back side bump structure.
13. The semiconductor die of claim 12, in, The metal pattern is disposed over the first backside metal plate layer and has an upwardly protruding shape to contact the through-electrode and the backside bump structure.
14. A semiconductor die, the semiconductor die comprising: A substrate having a through-electrode region and a dummy region; an interlayer insulating layer, the interlayer insulating layer being disposed below the active surface of the substrate; a horizontal metal interconnection disposed in the interlayer insulating layer; A front side passivation layer, the front side passivation layer being disposed below the lower surface of the interlayer insulating layer; a front-side bump structure, the front-side bump structure being arranged below the lower surface of the front-side passivation layer in the through-electrode region; a dummy front side bump structure, the dummy front side bump structure being disposed below the lower surface of the front side passivation layer in the dummy region; a backside insulating layer disposed over the inactive surface of the substrate; a first back metal plate layer, the first back metal plate layer being disposed above the back insulating layer; a backside passivation layer, the backside passivation layer being disposed above the first backside metal plate layer; a through electrode, the through electrode vertically passing through the substrate, the back insulating layer, the first back metal plate layer and the back passivation layer in the through electrode region; a backside bump structure, the backside bump structure being arranged above the through-electrode in the through-electrode region; as well as A dummy backside bump structure is disposed above the backside passivation layer in the dummy region.
15. The semiconductor die of claim 14, in, The through-electrode has a protruding portion protruding upward from the inactive surface of the substrate, and Part of the back-side insulating layer protrudes to surround a side surface of the protruding portion of the through electrode.
16. The semiconductor die of claim 14, in, The first back metal plate layer has through electrode holes, and Wherein, the through electrode vertically passes through the through electrode hole.
17. The semiconductor die of claim 14, in, The first backside metal plate layer includes a lower underbump metallurgy layer including titanium and an upper underbump metallurgy layer including at least one of copper and nickel.
18. The semiconductor die of claim 14, in, The first backside metal plate layer is connected to the backside bump structure.
19. The semiconductor die of claim 14, further comprising: a metal pattern, the metal pattern being arranged between the first back metal plate layer and the back bump structure, wherein the first back metal plate layer extends onto the protruding portion of the through electrode, and The metal pattern is disposed above the first backside metal plate layer to be vertically aligned with the through electrode and the backside bump structure.
20. The semiconductor die of claim 14, in, The first back metal plate layer is disposed in the dummy area.