Electricity storage unit

By setting a recess on the inner peripheral surface of the housing of the power storage unit and filling the outer peripheral surface gap with adhesive materials, the problem of compressing the bulging part of the winding electrode body caused by the thickness of the ear lead is solved, and uniform support of the electrode body is achieved and Improved vibration resistance.

CN119029263APending Publication Date: 2024-11-26TOYOTA JIDOSHA KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410251407.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-26
Filing Date
2024-03-06
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

When the existing power storage unit is provided with the electrode lead, the thickness of the electrode lead causes the bulge to form an outer peripheral surface of the wound electrode body, and then a load is partially applied when the shell is constrained, resulting in uneven pressure on the electrode body.

Method used

The inner peripheral surface of the housing is provided with a recess to increase the distance from the bulging part, reduce the pressure, and fill the outer peripheral surface and the recess to fix the wound electrode body by means of an adhesive material, thereby reducing the anti-electrode body Pressure and improve vibration resistance.

Benefits of technology

The local load applied to the wound electrode body is effectively suppressed, the risk of pressure due to the bulging part is reduced, and the electrode body is fixed by bonding materials, thereby improving the vibration resistance of the battery and the ability to maintain the wound state.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119029263A_ABST
    Figure CN119029263A_ABST
Patent Text Reader

Abstract

The present disclosure relates to a power storage unit. An electricity storage cell is provided with a wound electrode body and a case that houses the wound electrode body. The wound electrode body includes an outer peripheral surface on which a bulging portion is formed. The housing includes an inner peripheral surface opposite to the outer peripheral surface. A groove (recess) is provided on the inner peripheral surface at a position facing the bulge.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a power storage unit. Background Art

[0002] International Publication No. 2020 / 137547 discloses an electricity storage device including a wound electrode body provided with tab leads. Summary of the invention

[0003] The wound electrode body of the International Publication No. 2020 / 137547 is provided with a tab lead. By providing the tab lead, a bulge is sometimes formed on the outer peripheral surface of the wound electrode body due to the thickness of the tab lead. In this case, when the wound electrode body is constrained by a shell or the like, a load is locally applied to the wound electrode body (bulge).

[0004] The present disclosure has been made to solve the above-mentioned problems, and an object of the present disclosure is to provide a power storage unit capable of suppressing the local application of a load to a wound electrode body.

[0005] An electric storage unit according to one aspect of the present disclosure includes:

[0006] A wound electrode body including an electrode sheet and a separator; and

[0007] The casing houses the wound electrode body.

[0008] The wound electrode body is wound so that the electrode sheet and the separator surround the circumference of the winding axis.

[0009] The wound electrode body includes an outer peripheral surface on which a bulge is formed.

[0010] The housing includes an inner peripheral surface opposite to the outer peripheral surface.

[0011] A recessed portion is provided at a position of the inner peripheral surface facing the bulging portion.

[0012] In a storage battery cell according to one aspect of the present disclosure, as described above, a recess is provided on the inner circumferential surface of the shell at a position opposite to the bulge. Thus, the distance between the inner circumferential surface of the shell and the bulge can be increased compared to a case where the recess is not formed. As a result, the pressure on the wound electrode body from the inner circumferential surface of the shell at the location where the bulge is provided can be reduced compared to a case where the recess is not formed. Thus, it is possible to suppress the application of pressure locally to the wound electrode body.

[0013] In the power storage unit according to the above aspect, it is preferred that:

[0014] The bulging portion is formed to extend in the axial direction of the wound electrode body.

[0015] The recessed portion includes a groove portion provided so as to extend along the bulging portion.

[0016] According to this structure, compared with a case where no groove is formed, it is possible to easily reduce the pressure that the bulge portion extending in the axial direction receives from the inner peripheral surface of the case.

[0017] In the power storage unit according to the above aspect, it is preferred that:

[0018] The outer peripheral surface includes a winding terminal end portion of the wound electrode body.

[0019] The wound electrode body includes a tape attached to a terminal end portion so as to maintain the wound state of the wound electrode body.

[0020] The bulge is formed by the belt.

[0021] The recessed portion is provided at a position opposite to the tape. With such a configuration, the pressure on the tape attached to the end portion from the inner circumferential surface of the shell can be reduced compared to a case where the recessed portion is not formed. As a result, the tape can be used to maintain the wound state of the wound electrode body and suppress the application of local pressure to the wound electrode body.

[0022] In the power storage unit according to the above aspect, it is preferred that:

[0023] The bulge is formed by an adhesive material applied between the outer peripheral surface and the recessed portion.

[0024] This configuration can reduce the pressure of the adhesive from the inner peripheral surface of the case compared to a case where no recess is formed. As a result, it is possible to suppress the local pressure on the wound electrode body and improve the vibration resistance of the wound electrode body by fixing the case and the wound electrode body with the adhesive.

[0025] In this case, it is preferred that

[0026] The outer peripheral surface includes a winding terminal end portion of the wound electrode body.

[0027] The adhesive is applied between the recessed portion provided at a position facing the distal end portion and the outer peripheral surface.

[0028] With such a structure, the vibration resistance of the wound electrode body can be improved, and the wound state of the wound electrode body can be maintained by bonding the end portion with the adhesive material. In addition, the wound state of the wound electrode body can be maintained with the adhesive material, so the tape for maintaining the wound state of the wound electrode body can be omitted.

[0029] In the power storage unit according to the above aspect, it is preferred that:

[0030] The electrode sheet includes:

[0031] a sheet-shaped current collector; and

[0032] The tab lead protrudes axially from the current collector.

[0033] The bulge is formed by the tab lead.

[0034] The recessed portion is located radially outside the wound electrode body relative to the tab lead.

[0035] According to this structure, compared with a case where no recess is formed, it is possible to reduce the pressure applied from the inner peripheral surface of the case to the bulge formed by the thickness of the tab lead.

[0036] According to the present disclosure, it is possible to suppress the local application of a load to the wound electrode body having the bulge formed therein. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Features, advantages, and technical and industrial significance of exemplary embodiments of the present invention will be described below with reference to the accompanying drawings, in which like reference numerals represent like elements, and in which:

[0038] Figure 1 is a cross-sectional view showing the structure of the power storage unit according to the first embodiment;

[0039] Figure 2 is a perspective view schematically showing the structure of a wound electrode body according to the first embodiment;

[0040] Figure 3 yes Figure 1 A partial enlarged view of the positive electrode side;

[0041] Figure 4 yes Figure 1 A partial enlarged view of the negative electrode side;

[0042] Figure 5 This is a diagram showing a state in which the wound electrode body and the case of the first embodiment are separated;

[0043] Figure 6 This is a partially enlarged top view of the vicinity of the groove portion of the first embodiment as viewed from the Z1 side;

[0044] Figure 7 This is a partially enlarged top view of the vicinity of the groove portion of the second embodiment as viewed from the Z1 side;

[0045] Figure 8 is a perspective view showing the structure of a wound electrode body according to a second embodiment;

[0046] Fig. 9 is a cross-sectional view showing the structure of a power storage unit according to a third embodiment;

[0047] Fig.10 is a perspective view schematically showing the structure of a wound electrode body according to a third embodiment;

[0048] Fig.11is a plan view showing the structure of a positive electrode plate according to a third embodiment;

[0049] Fig.12 is a plan view showing the structure of a negative electrode plate according to a third embodiment;

[0050] Fig.13 It is along Fig.11 A cross-sectional view of line XIII-XIII;

[0051] Fig.14 It is along Fig.12 A cross-sectional view of line XIV-XIV;

[0052] Fig.15 This is a partially enlarged top view of the vicinity of the groove portion of the third embodiment as viewed from the Z1 side;

[0053] Fig.16 is a partially enlarged top view of the vicinity of the groove portion of the third embodiment as viewed from the Z2 side; and

[0054] Fig.17 This is a diagram showing a state in which a wound electrode body and a case are separated according to a modification of the first embodiment. DETAILED DESCRIPTION

[0055] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that the same or corresponding parts in the drawings are denoted by the same reference numerals, and their description will not be repeated.

[0056] First Embodiment

[0057] Figure 1 1 is a cross-sectional view showing the overall structure of the power storage unit 100 according to the embodiment of the present disclosure. The power storage unit 100 is, for example, a lithium-ion battery mounted on a vehicle. It should be noted that the use and type of the power storage unit 100 are not limited to the above example.

[0058] The electricity storage cell 100 includes a wound electrode body 1 , a case 2 , a positive electrode terminal 3 , a positive electrode current collector plate 4 , an external gasket 5 , an internal gasket 6 , and a negative electrode current collector plate 7 .

[0059] The wound electrode body 1 is accommodated in a case 2. The case 2 has a cylindrical shape. That is, the power storage unit 100 is a cylindrical battery. The case 2 is formed of copper, aluminum, or the like.

[0060] The wound electrode body 1 includes a positive electrode plate 10, a negative electrode plate 20 and a separator 30. The separator 30 is provided between the positive electrode plate 10 and the negative electrode plate 20. The separator 30 enables ions (e.g., lithium ions) to travel back and forth between the positive electrode plate 10 (positive electrode active material) and the negative electrode plate 20 (negative electrode active material), and separates the positive electrode plate 10 from the negative electrode plate 20. The wound electrode body 1 is composed of an electrode plate group in which the positive electrode plate 10 and the negative electrode plate 20 are wound with the separator 30 interposed therebetween. It should be noted that the positive electrode plate 10 and the negative electrode plate 20 are each an example of an "electrode sheet" disclosed herein.

[0061] like Figure 2 As shown in FIG. 1 , the wound electrode body 1 is wound so that the positive electrode plate 10 , the negative electrode plate 20 , and the separator 30 surround the periphery of the winding axis α. Figure 2 In order to facilitate understanding of the wound state of the wound electrode body 1 , the wound electrode body 1 is shown in a state where it is slightly unwound.

[0062] Refer again Figure 1 The positive terminal 3 includes a disk portion 3a and a rivet portion 3b. The rivet portion 3b is connected to the disk portion 3a. The rivet portion 3b is provided in a manner extending from the center of the disk portion 3a toward the Z2 side. It should be noted that the positive terminal 3 is formed of aluminum.

[0063] like Figure 3 As shown, the disk portion 3a is arranged on the upper surface 2a (surface on the Z1 side) of the housing 2. A through hole 2b is provided on the upper surface 2a of the housing 2. The rivet portion 3b extends from the disk portion 3a arranged outside the housing 2 to the inside of the housing 2 through the through hole 2b.

[0064] The positive electrode collector plate 4 is housed in the case 2. The positive electrode collector plate 4 is welded to the positive electrode uncoated portion 11b (described later) of the positive electrode plate 10 on the Z1 side of the wound electrode body 1. Thus, the positive electrode collector plate 4 is positively charged. The positive electrode collector plate 4 is welded to the end portion 3c on the Z2 side of the rivet portion 3b. Thus, the positive electrode terminal 3 is positively charged.

[0065] The external gasket 5 is disposed between the disk portion 3a of the positive electrode terminal 3 and the upper surface 2a of the case 2. Thus, the positive electrode terminal 3 and the case 2 are insulated.

[0066] The internal gasket 6 is disposed between the case 2 and the positive electrode collector plate 4 inside the case 2. Thus, the case 2 is insulated from the positive electrode collector plate 4. It should be noted that the rivet portion 3b penetrates the internal gasket 6 and contacts the positive electrode collector plate 4.

[0067] The positive electrode plate 10 includes a positive current collector 11 and a positive electrode mixture layer 12. The positive electrode mixture layer 12 is applied to both radial (R direction) surfaces of the positive current collector 11 (a positive electrode coating portion 11a described below). The positive electrode mixture layer 12 faces the separator 30 in the R direction.

[0068] The positive electrode current collector 11 uses aluminum, for example. The positive electrode mixture layer 12 is formed by applying positive electrode slurry to the surface of the positive electrode current collector 11 and drying it. The positive electrode slurry refers to a slurry prepared by kneading the material (positive electrode active material, binder, etc.) of the positive electrode mixture layer 12 with a solvent. The positive electrode mixture layer 12 is in close contact with the separator 30. The thickness of the positive electrode mixture layer 12 is, for example, not less than 0.1 μm and not more than 1000 μm.

[0069] The positive electrode current collector 11 includes a positive electrode coating portion 11a and a positive electrode uncoated portion 11b. The positive electrode coating portion 11a is a portion of the positive electrode current collector 11 coated with the positive electrode mixture layer 12. The positive electrode coating portion 11a is sandwiched between separators 30.

[0070] The positive electrode uncoated portion 11b is a portion of the positive electrode current collector 11 not coated with the positive electrode mixture layer 12. The positive electrode uncoated portion 11b is located on the Z1 side of the positive electrode coated portion 11a. Specifically, the positive electrode uncoated portion 11b protrudes from the positive electrode coated portion 11a toward the Z1 side.

[0071] The positive electrode uncoated portion 11b includes a portion 11c extending along the Z direction and a portion 11d extending along the R direction. The positive electrode uncoated portion 11b is bent radially inward. The positive electrode uncoated portion 11b is bent into an L shape. The portion 11d of the positive electrode uncoated portion 11b is in contact with the positive electrode collector plate 4. As a result, the positive electrode collector plate 4 is positively charged. It should be noted that the positive electrode uncoated portion 11b (portion 11d) is joined to the positive electrode collector plate 4 by welding.

[0072] A plurality of positive electrode uncoated portions 11b are arranged in the winding direction. A slit (not shown) is provided between adjacent positive electrode uncoated portions 11b in the winding direction. Adjacent positive electrode uncoated portions 11b in the R direction among the plurality of positive electrode uncoated portions 11b are provided so as to partially overlap each other.

[0073] like Figure 4 As shown, the negative electrode collector plate 7 is housed in the case 2. The negative electrode collector plate 7 is welded to the negative electrode uncoated portion 21b described later of the negative electrode plate 20 on the Z2 side of the wound electrode body 1. As a result, the negative electrode collector plate 7 is negatively charged. It should be noted that the negative electrode collector plate 7 is in contact with the case 2. As a result, the case 2 is negatively charged.

[0074] The negative electrode plate 20 includes a negative electrode collector 21 and a negative electrode mixture layer 22. The negative electrode mixture layer 22 is applied to both radial (R direction) surfaces of the negative electrode collector 21 (negative electrode coating portion 21a described below). The negative electrode mixture layer 22 faces the separator 30 in the R direction.

[0075] The negative electrode current collector 21 uses copper, for example. The negative electrode mixture layer 22 is formed by applying a negative electrode slurry to the surface of the negative electrode current collector 21 and drying it. The negative electrode slurry refers to a slurry prepared by kneading the material of the negative electrode mixture layer 22 (negative electrode active material, binder, etc.) with a solvent. The negative electrode mixture layer 22 is in close contact with the separator 30. The thickness of the negative electrode mixture layer 22 is, for example, 0.1 μm or more and 1000 μm or less.

[0076] The negative electrode current collector 21 includes a negative electrode coating portion 21a and a negative electrode uncoated portion 21b. The negative electrode coating portion 21a is a portion of the negative electrode current collector 21 coated with the negative electrode mixture layer 22. The negative electrode coating portion 21a is sandwiched between separators 30.

[0077] The negative electrode uncoated portion 21b is a portion of the negative electrode current collector 21 not coated with the negative electrode mixture layer 22. The negative electrode uncoated portion 21b is located on the Z2 side of the negative electrode coated portion 21a. Specifically, the negative electrode uncoated portion 21b protrudes from the negative electrode coated portion 21a to the Z2 side.

[0078] The negative electrode uncoated portion 21b includes a portion 21c extending along the Z direction and a portion 21d extending along the R direction. The negative electrode uncoated portion 21b is bent radially inward. The negative electrode uncoated portion 21b is bent into an L shape. The portion 21d of the negative electrode uncoated portion 21b is in contact with the negative electrode collector plate 7. As a result, the negative electrode collector plate 7 is negatively charged. It should be noted that the negative electrode uncoated portion 21b (portion 21d) is joined to the negative electrode collector plate 7 by welding.

[0079] In addition, a plurality of negative electrode uncoated portions 21b are arranged along the winding direction. A slit (not shown) is provided between the negative electrode uncoated portions 21b adjacent to each other in the winding direction. In addition, the negative electrode uncoated portions 21b adjacent to each other in the R direction among the plurality of negative electrode uncoated portions 21b are provided so as to partially overlap each other.

[0080] Figure 5 2 is a schematic perspective view showing a state where the wound electrode body 1 and the case 2 are separated. Figure 5 As shown, the wound electrode body 1 includes an outer peripheral surface 1a and a terminal portion 1b. The terminal portion 1b is a winding terminal portion of the wound electrode body 1. The terminal portion 1b is provided so as to extend in the axial direction (Z direction).

[0081] In addition, the wound electrode body 1 includes a tape 8 attached to the outer peripheral surface 1a. In order to maintain the wound state of the wound electrode body 1, the tape 8 is provided at the terminal portion 1b. The tape 8 is provided so as to extend in the axial direction (Z direction). That is, the tape 8 is provided along the terminal portion 1b extending in the Z direction. The tape 8 is provided so as to cover the terminal portion 1b from the radially outer side (R2 side).

[0082] The belt 8 has a thickness t1 in the radial direction (R direction) (refer to Figure 6 ). Thus, the wound electrode body 1 has a bulging portion 1 c on the outer peripheral surface 1 a because the tape 8 is attached to the outer peripheral surface 1 a. That is, the bulging portion 1 c is formed by the tape 8 .

[0083] In addition, the shell 2 includes an inner peripheral surface 2c. The inner peripheral surface 2c is arranged in a manner opposite to the outer peripheral surface 1a of the wound electrode body 1 in the R direction (radial direction of the wound electrode body 1). It should be noted that the wound electrode body 1 is inserted into the shell 2 from the opening 2d on the Z1 side of the shell 2. In addition, the opening 1d is closed by a cover (not shown) after the wound electrode body 1 is arranged. Thus, the upper surface 2a (see Figure 1 ).

[0084] Here, in conventional storage cells, a tab lead may form a bulge on the outer circumference of the wound electrode body due to the thickness of the tab lead. In this case, when the wound electrode body is restrained by a case or the like, a load is locally applied to the wound electrode body (bulge).

[0085] Therefore, in the first embodiment, a groove portion 2e is provided on the inner peripheral surface 2c of the shell 2 at a position opposite to the bulge portion 1c (belt 8). The groove portion 2e is provided in a manner extending along the bulge portion 1c (belt 8) extending in the Z direction (axial direction). That is, the groove portion 2e extends in the Z direction. The belt 8 has a length L1 in the Z direction. The groove portion 2e has a length L2 in the Z direction. The length L2 of the groove portion 2e is greater than the length L1 of the belt 8. It should be noted that the groove portion 2e is an example of a "recess" disclosed in the present invention.

[0086] Figure 6 FIG. 2 is a plan view of the vicinity of the bulge 1 c as viewed from the Z1 side in a state where the wound electrode body 1 is disposed in the case 2. Figure 6 As shown, the belt 8 has a width W1 in the C direction (circumferential direction). The groove portion 2e has a width W2 in the C direction. The width W1 of the belt 8 is smaller than the width W2 of the groove portion 2e. For example, the width W1 is 0.5 times or more and 0.9 times or less of the width W2.

[0087] Specifically, the end 2f of the groove 2e on the C1 side is arranged closer to the C1 side than the end 8a of the belt 8 on the C1 side. The end 2g of the groove 2e on the C2 side is arranged closer to the C2 side than the end 8b of the belt 8 on the C2 side.

[0088] The belt 8 has a thickness t1 in the R direction. The groove portion 2e has a depth d1 in the R direction. The depth d1 of the groove portion 2e is greater than the thickness t1 of the belt 8. Thus, the entire belt 8 can be accommodated in the groove portion 2e.

[0089] The distance D1 between the outer peripheral surface 1a of the wound electrode body 1 and the inner peripheral surface 2c of the case 2 is smaller than the thickness t1 of the belt 8. Thus, at least a portion of the belt 8 (at least a portion on the case 2 side) is arranged to enter the inner side of the groove 2e. It should be noted that the distance D1 is a distance corresponding to the circumferential position where the bulge 1c and the groove 2e are not provided.

[0090] As described above, in the first embodiment, the groove 2e is provided at a position opposite to the bulging portion 1c (belt 8) on the inner circumferential surface 2c of the case 2. Thus, the bulging portion 1c can be retracted into the groove 2e. As a result, it is possible to suppress the local application of a load from the case 2 to the wound electrode body 1 (bulging portion 1c).

[0091] Second Embodiment

[0092] Next, refer to Figure 7 and Figure 8 , a second embodiment of the present disclosure will be described. In the second embodiment, an adhesive material 18 is used instead of the belt 8 of the first embodiment. The same reference numerals as those of the first embodiment are given to the same structures as those of the first embodiment, and no repeated description will be given.

[0093] Figure 7 It is a partially enlarged plan view showing the structure of the electric storage cell 200. The electric storage cell 200 includes a wound electrode body 31 and a case 2. The wound electrode body 31 includes an outer peripheral surface 31a, a terminal end portion 31b, and a bulging portion 31c.

[0094] In the second embodiment, the bulge 31c is formed by an adhesive material 18 applied between the outer peripheral surface 31a and the groove portion 2e. The adhesive material 18 is configured, for example, by filling the gap S formed between the inner peripheral surface 2c corresponding to the groove portion 2e and the outer peripheral surface 31a with the liquid adhesive material 18 in a state where the wound electrode body 31 is inserted (configured) in the shell 2. That is, the adhesive material 18 is configured to fill the groove portion 2e and the space between the groove portion 2e and the outer peripheral surface 31a. The filled liquid adhesive material 18 is then cured. It should be noted that the wound electrode body 31 can also be combined with the shell in a state where the adhesive material 18 is previously applied to the groove portion 2e or the outer peripheral surface 31a.

[0095] It should be noted that the wound electrode body 31 is structurally different from the wound electrode body 1 of the first embodiment described above only in that an adhesive material 18 is provided instead of the tape 8 .

[0096] The groove 2e is provided at a position opposite to the terminal end 31b in the radial direction (R direction). The terminal end 31b is covered from the radial outer side (R2 side) by the adhesive material 18 provided between the groove 2e and the outer peripheral surface 31a. Thus, the terminal end 31b is fixed by the adhesive material 18.

[0097] The adhesive material 18 is provided so as to extend in the circumferential direction (C direction) from the end 2f on the C1 side of the groove portion 2e to the end 2g on the C2 side.

[0098] Figure 8 3 is a perspective view showing the structure of the wound electrode body 31. Figure 8 As shown, the adhesive material 18 is provided on the outer peripheral surface 31 a of the wound electrode body 31 so as to extend from an end 31 d on the Z1 side of the wound electrode body 31 to an end 31 e on the Z2 side of the wound electrode body 31 .

[0099] Since the other structures are the same as those of the first embodiment described above, the description thereof will not be repeated.

[0100] Third Embodiment

[0101] Next, refer to Figures 9 to 16 , a third embodiment of the present disclosure will be described. In the third embodiment, unlike the first and second embodiments, a bulge is formed by a tab lead.

[0102] Fig. 9 2 is a cross-sectional view showing the overall structure of a power storage unit 300 according to a third embodiment of the present disclosure. The power storage unit 300 is, for example, a lithium-ion battery mounted on a vehicle. It should be noted that the use and type of the power storage unit 300 are not limited to the above example.

[0103] The power storage cell 300 includes a wound electrode body 301 , a case 302 , a current interrupt device (CID) 303 , a positive insulating plate 304 , a negative insulating plate 305 , and an insulating layer 306 .

[0104] The wound electrode body 301 is accommodated in a case 302. The case 302 has a cylindrical shape. That is, the power storage unit 300 is a cylindrical battery. The case 302 is formed of, for example, copper or aluminum.

[0105] The wound electrode body 301 includes a positive electrode plate 310, a negative electrode plate 320 and a separator 330. The separator 330 is disposed between the positive electrode plate 310 and the negative electrode plate 320. The separator 330 enables ions (e.g., lithium ions) to travel back and forth between the positive electrode plate 310 (positive electrode active material) and the negative electrode plate 320 (negative electrode active material), and separates the positive electrode plate 310 from the negative electrode plate 320. The wound electrode body 301 is composed of an electrode plate group in which the positive electrode plate 310 and the negative electrode plate 320 are wound with the separator 330 interposed therebetween. It should be noted that the positive electrode plate 310 and the negative electrode plate 320 are each an example of an “electrode sheet” of the present disclosure.

[0106] like Fig.10As shown in FIG. 1 , the wound electrode body 301 is wound so that the positive electrode plate 310 , the negative electrode plate 320 , and the separator 330 surround the circumference of the winding axis β. Fig.10 In order to facilitate understanding of the wound state of the wound electrode body 301 , the wound electrode body 301 is shown in a state where it is slightly unwound.

[0107] The positive electrode plate 310 includes a sheet-shaped positive electrode collector 311 (see Fig.11 ), positive electrode mixture layer 312 (refer to Fig.11 ) and a positive electrode lead 313. The negative electrode plate 320 includes a sheet-like negative electrode collector 321 (see Fig.12 ), negative electrode mixture layer 322 (refer to Fig.12 ) and the negative electrode tab lead 323. It should be noted that the positive electrode collector 311 and the negative electrode collector 321 are each an example of a "collector" of the present disclosure. In addition, the positive electrode tab lead 313 and the negative electrode tab lead 323 are each an example of a "tab lead" of the present disclosure.

[0108] Refer again Fig. 9 , the positive side insulating plate 304 is housed in the housing 302. The positive side insulating plate 304 is provided in a manner to insulate the wound electrode body 301 (negative electrode plate 320 and separator 330) from the housing 302. The positive side insulating plate 304 is provided in a manner to cover the positive electrode collector 311, the negative electrode plate 320 and the separator 330 from the Z1 side.

[0109] The positive side insulating plate 304 has a through hole 304a. The positive electrode tab lead 313 passes through the through hole 304a and contacts (is welded) with a conductive film 303b described later. Thus, the positive electrode tab lead 313 is electrically connected to the conductive film 303b.

[0110] The negative insulating plate 305 is housed in the case 302. The negative insulating plate 305 is provided to insulate the wound electrode body 301 (positive electrode plate 310 and separator 330) from the case 302. The negative insulating plate 305 is provided to cover the positive electrode plate 310, the negative electrode collector 321, and the separator 330 from the Z2 side.

[0111] The negative side insulating plate 305 has a through hole 305a. The negative electrode tab lead 323 passes through the through hole 305a and contacts the bottom 302a of the shell 302. As a result, the negative electrode tab lead 323 is electrically connected to the bottom 302a of the shell. As a result, the side surface 302b of the shell 302 connected to the bottom 302a of the shell 302 is negatively charged. It should be noted that the side surface 302b is in contact with the negative electrode collector 321 of the negative electrode plate 320 provided on the outermost periphery of the wound electrode body 301.

[0112] The CID 303 is a device that cuts off the current path by utilizing the increase in the cell internal pressure caused by the gas generated by overcharging of the power storage cell 300. The CID 303 is provided to seal the opening on the Z1 side of the case 302. The CID 303 includes an external cover 303a, a conductive film 303b, a gasket 303c, and a chassis 303d.

[0113] The external cover 303a functions as an external terminal by being electrically connected to an external bus bar (not shown). The external cover 303a is provided with a fragile portion 303e (thin wall portion). When the internal pressure of the housing 302 rises, the external cover 303a is easily damaged starting from the fragile portion 303e. As a result, the gas is quickly discharged to the outside of the housing 302.

[0114] The conductive film 303b is arranged in a manner to seal the opening on the Z1 side of the shell 302. The conductive film 303b includes a protrusion 303f protruding toward the wound electrode body 301 side (Z2 side). The protrusion 303f is in contact with the positive electrode tab lead 313. Thus, the conductive film 303b is positively charged. In addition, the conductive film 303b is electrically connected to the external cover 303a. Thus, the external cover 303a is also positively charged. It should be noted that the protrusion 303f is arranged in a manner to penetrate the gasket 303c and the chassis 303d respectively.

[0115] Similar to the outer cover 303a, the conductive film 303b is provided with a fragile portion 303g (thin-walled portion). When the internal pressure of the housing 302 rises, the conductive film 303b is easily damaged starting from the fragile portion 303g. When the conductive film 303b is damaged due to the increase in internal pressure, the contact between the conductive film 303b and the positive electrode tab lead 313 is released. As a result, the positive charge of the conductive film 303b is eliminated, and the positive charge of the outer cover 303a is eliminated. As a result, the charging and discharging of the storage cell 300 is stopped.

[0116] The housing 302 is provided with a caulking portion 302c caulked to the outer peripheral edge of the outer cover 303a. The insulating layer 306 is provided so as to insulate the caulking portion 302c from the outer cover 303a (and the conductive film 303b).

[0117] Fig.11 This is a diagram of the positive electrode plate 310 in a sheet-like state as viewed from the Y1 side. The Y direction is a direction orthogonal to the positive electrode collector 311 that is expanded into a sheet. The positive electrode collector 311 has a rectangular shape consisting of a long side extending in the X direction and a short side extending in the Z direction. It should be noted that the X direction is a direction equivalent to the winding direction of the wound electrode body 301. In addition, the Z direction is an example of the "axial direction" of the present disclosure. It should be noted that the Y direction is a direction equivalent to the Fig. 9The R direction is shown. In addition, the R direction is an example of the "radial direction" of the present disclosure.

[0118] like Fig.11 As shown, the positive electrode mixture layer 312 (hatched portion) is applied to a portion of the positive electrode current collector 311. That is, the positive electrode current collector 311 includes a coated portion 311a coated with the positive electrode mixture layer 312 and an uncoated portion 311b not coated with the positive electrode mixture layer.

[0119] exist Fig.11 In the example shown, the uncoated portion 311b is provided at the end 311c on the X1 side of the positive electrode current collector 311. The uncoated portion 311b is provided so as to extend along the Z direction. In the third embodiment, the X1 side and the X2 side are respectively used as the winding end side and the winding start side of the wound electrode body 301.

[0120] The positive electrode current collector 311 is made of aluminum, for example. The positive electrode mixture layer 312 is formed by applying positive electrode slurry to the surface of the positive electrode current collector 311 and drying it. The positive electrode slurry is a slurry prepared by kneading the materials of the positive electrode mixture layer 312 (positive electrode active material, binder, etc.) with a solvent. The positive electrode mixture layer 312 and the separator 330 (see Fig. 9 The thickness of the positive electrode mixture layer 312 is, for example, not less than 0.1 μm and not more than 1000 μm.

[0121] The positive electrode tab lead 313 is disposed in the uncoated portion 311b. The positive electrode tab lead 313 is provided so as to protrude in the axial direction (Z1 side) from the positive electrode current collector 311. The positive electrode tab lead 313 is provided at the center of the uncoated portion 311b in the X direction.

[0122] Fig.12 3 is a diagram of the negative electrode plate 320 in a sheet-like state as viewed from the Y1 side. Fig.12 As shown, the negative electrode current collector 321 has a rectangular shape including long sides extending in the X direction and short sides extending in the Z direction, similarly to the positive electrode current collector 311 .

[0123] The negative electrode current collector 321 is made of, for example, copper foil. The negative electrode mixture layer 322 is formed by applying negative electrode slurry to the surface of the negative electrode current collector 321 and drying it. The negative electrode slurry is a slurry prepared by kneading the materials of the negative electrode mixture layer 322 (negative electrode active material and binder, etc.) with a solvent. The negative electrode mixture layer 322 and the separator 330 (see Fig. 9 The thickness of the negative electrode mixture layer 322 is, for example, not less than 0.1 μm and not more than 1000 μm.

[0124] The negative electrode mixture layer 322 is applied to a portion of the negative electrode current collector 321. That is, the negative electrode current collector 321 includes a coated portion 321a coated with the negative electrode mixture layer 322 and an uncoated portion 321b not coated with the negative electrode mixture layer 322. The uncoated portion 321b is provided to extend along the Z direction.

[0125] The negative electrode tab lead 323 is disposed in the uncoated portion 321b. The negative electrode tab lead 323 is provided so as to protrude in the axial direction (Z2 side) from the negative electrode current collector 321. The negative electrode tab lead 323 is provided at the center of the uncoated portion 321b in the X direction.

[0126] Fig.13 It is along Fig.11 The cross-sectional view of the XIII-XIII line. Fig.13 As shown, the positive electrode current collector 311 has a thickness t11 in the Y direction. The positive electrode mixture layer 312 has a thickness t12 in the Y direction. The positive electrode tab lead 313 has a thickness t13 in the Y direction.

[0127] The thickness t13 of the positive electrode tab lead 313 is greater than the thickness t12 of the positive electrode mixture layer 312. It should be noted that the thickness t12 of the positive electrode mixture layer 12 and the thickness t13 of the positive electrode tab lead 13 are respectively greater than the thickness t11 of the positive electrode collector 311. In addition, the thickness difference Δt1 (t13-t12) between the thickness t13 of the positive electrode tab lead 313 and the thickness t12 of the positive electrode mixture layer 312 may also be greater than the thickness t11 of the positive electrode collector 311.

[0128] Fig.14 It is along Fig.12 The cross-sectional view of the XIV-XIV line. Fig.14 As shown, the negative electrode current collector 321 has a thickness t21 in the Y direction. The negative electrode mixture layer 322 has a thickness t22 in the Y direction. The negative electrode tab lead 323 has a thickness t23 in the Y direction.

[0129] The thickness t23 of the negative electrode tab lead 323 is greater than the thickness t22 of the negative electrode mixture layer 322. It should be noted that the thickness t22 of the negative electrode mixture layer 322 and the thickness t23 of the negative electrode tab lead 323 are respectively greater than the thickness t21 of the negative electrode collector 321. In addition, the thickness difference Δt2 (t23-t22) between the thickness t23 of the negative electrode tab lead 323 and the thickness t22 of the negative electrode mixture layer 322 may be greater than the thickness t21 of the negative electrode collector 321.

[0130] Fig.15 This is a partially enlarged top view of the wound electrode body 301 as viewed from the Z1 side. Fig.15As shown, in the third embodiment, a bulge 301c is formed on the outer peripheral surface 301a of the wound electrode body 301. The bulge 301c is formed by the positive electrode tab lead 313. Specifically, the bulge 301c is formed by the thickness t13 (see Fig.13 ) and the thickness t12 of the positive electrode mixture layer 312 (see Fig.13 That is, the bulging amount of the bulging portion 301c (the amount of protrusion toward the R2 side) is equal to the thickness difference Δt1.

[0131] The positive electrode tab lead 313 has a width W11 in the C direction. The groove portion 302e has a width W12 in the C direction. The bulge portion 301c has a width W13 in the C direction. The width W13 of the bulge portion 301c is greater than the width W11 of the positive electrode tab lead 313. It should be noted that the groove portion 302e is an example of a "recess" in the present disclosure.

[0132] The groove 302e provided on the inner circumferential surface 302d of the housing 302 is located on the R2 side relative to the positive electrode tab lead 313. The positive electrode tab lead 313 is located at the center of the range in the C direction where the groove 302e is provided. It should be noted that the shape of the groove 302e may be the same as the groove 2e of the first embodiment.

[0133] The width W12 of the groove portion 302e is greater than the width W13 of the bulge portion 301c. The end 302f of the groove portion 302e on the C1 side is located closer to the C1 side than the end 301d of the bulge portion 301c on the C1 side. The end 302g of the groove portion 302e on the C2 side is located closer to the C2 side than the end 301e of the bulge portion 301c on the C2 side. It should be noted that the groove portion 302f is an example of a "recess" disclosed in the present invention.

[0134] The groove portion 302e has a depth d2 in the R direction. The depth d2 of the groove portion 302e is greater than the thickness difference Δt1 described above (see Fig.13 Thus, the entire protrusion 301c can be accommodated in the groove 302e.

[0135] The distance D2 between the outer circumferential surface 301a of the wound electrode body 301 and the inner circumferential surface 302d of the shell 302 is smaller than the above-mentioned thickness difference Δt1. As a result, at least a portion of the bulge 301c (at least a portion of the shell 302 side) is arranged to enter the inner side of the groove 302e. It should be noted that the distance D2 is a distance corresponding to the circumferential position where the bulge 301c and the groove 302e are not provided.

[0136] It should be noted that, in the third embodiment, an example in which only one positive electrode tab lead 313 is provided is shown, but the present disclosure is not limited thereto. A plurality of positive electrode tab leads 313 may also be arranged in the R direction. In this case, the bulging amount of the bulging portion 301c is equal to the value obtained by multiplying the number of positive electrode tab leads 313 arranged in the R direction by the thickness difference Δt1.

[0137] Fig.16 This is a partially enlarged top view of the wound electrode body 301 as viewed from the Z2 side. Fig.16 As shown, a bulge 301f is formed on the outer peripheral surface 301a of the wound electrode body 301. The bulge 301f is formed by the negative electrode tab lead 323. Specifically, the bulge 301f is due to the thickness t23 of the negative electrode tab lead 323 (see Fig.14 ) and the thickness t22 of the negative electrode mixture layer 322 (see Fig.14 That is, the bulging amount of the bulging portion 301f (the amount of protrusion toward the R2 side) is equal to the thickness difference Δt2.

[0138] The groove portion 302h provided in the inner peripheral surface 302d of the case 302 is located on the R2 side with respect to the negative electrode tab lead 323. The negative electrode tab lead 323 is located at the center of the range in the C direction where the groove portion 302h is provided.

[0139] It should be noted that the relationship (size relationship and position relationship, etc.) between the negative electrode tab lead 323, the bulge 301f and the groove 302h is the same as the relationship between the positive electrode tab lead 313, the bulge 301c and the groove 302e described above, and therefore, a repeated description will not be given.

[0140] The distance D2 between the outer circumferential surface 301a of the wound electrode body 301 and the inner circumferential surface 302d of the case 302 is smaller than the thickness difference Δt2. Thus, at least a portion of the bulge 301f (at least a portion on the case 302 side) is disposed so as to enter the inner side of the groove 302h.

[0141] It should be noted that, in the third embodiment, an example in which only one negative electrode tab lead 323 is provided is shown, but the present disclosure is not limited thereto. A plurality of negative electrode tab leads 323 may also be arranged in the R direction. In this case, the bulging amount of the bulging portion 301f is equal to the value obtained by multiplying the number of negative electrode tab leads 323 arranged in the R direction by the thickness difference Δt2.

[0142] In the first to third embodiments, examples are shown in which grooves (2e, 302e, 302h) extending in the Z direction are formed on the inner circumferential surface (2c, 302d) of the housing (2, 302), but the present disclosure is not limited thereto. A recessed portion other than the groove may also be formed. For example, Fig.17 In the example shown, a recess 402b is formed on the inner peripheral surface 402a of the case 402 in a manner corresponding to the bulge 401c formed on the outer peripheral surface 401a of the wound electrode body 401. The recess 402b is formed in a manner corresponding to the bulge 401c so that the width W21 in the Z direction is less than the width W22 in the C direction. Fig.17 In FIG. 4 , an example is shown in which the bulged portion 401 c is formed of the tape 28 , but the bulged portion may be formed of an adhesive material or a tab lead.

[0143] In the first embodiment, the tape 8 is provided at the winding end portion 1b of the wound electrode body 1, but the present disclosure is not limited thereto. The tape 8 may also be provided at a position other than the winding end portion 1b. It should be noted that the position of the adhesive material 18 in the second embodiment is also the same.

[0144] In the first and second embodiments, a wound electrode body without a tab lead is shown as an example, but the present disclosure is not limited thereto. In the first and second embodiments, a wound electrode body with a tab lead may be used as in the third embodiment.

[0145] In the above-mentioned third embodiment, an example in which the tab lead is provided in the uncoated portion is shown, but the present disclosure is not limited to this. The tab lead may also be provided in the coated portion. In this case, the thickness of the tab lead may not be greater than the thickness of the positive electrode (negative electrode) mixture layer. In addition, in the above-mentioned third embodiment, an example in which the thickness difference Δt1 (Δt2) is smaller than the depth d2 of the groove portion and larger than the distance D2 of the gap between the shell 302 and the wound electrode body 301 is shown, but the case in which the tab lead is provided in the coated portion is not limited to this. Regarding the depth d2 and the distance D2, the thickness t13 (t23) of the tab lead may also be smaller than the depth d2 and larger than the distance D2.

[0146] It should be noted that the structures of the above-mentioned embodiment and each of the above-mentioned modifications may be combined with each other.

[0147] The embodiments disclosed this time should be considered as illustrative in all aspects and not restrictive. The scope of the present disclosure is indicated by the claims rather than the description of the embodiments above, and is intended to include all modifications within the meaning and scope equivalent to the claims.

Claims

1. A power storage unit comprising: A wound electrode body comprising an electrode sheet and a separator; and a casing for housing the wound electrode body, The wound electrode body is wound in such a manner that the electrode sheet and the separator surround a winding axis. The wound electrode body includes an outer peripheral surface having a bulge formed thereon, The housing includes an inner peripheral surface opposite to the outer peripheral surface, A recessed portion is provided at a position of the inner peripheral surface facing the bulging portion.

2. The power storage unit according to claim 1, wherein: The bulge is formed to extend in the axial direction of the wound electrode body. The recessed portion includes a groove portion provided so as to extend along the bulging portion.

3. The power storage unit according to claim 1 or 2, wherein: The outer peripheral surface includes a winding terminal end portion of the wound electrode body, The wound electrode body includes a tape attached to the terminal portion so as to maintain the wound state of the wound electrode body. The bulge is formed by the belt, The recessed portion is provided at a position opposing the belt.

4. The power storage unit according to claim 1 or 2, wherein: The protruding portion is formed by an adhesive material applied between the outer peripheral surface and the recessed portion.

5. The power storage unit according to claim 4, wherein: The outer peripheral surface includes a winding terminal end portion of the wound electrode body, The adhesive material is applied between the recessed portion provided at a position opposing the distal end portion and the outer peripheral surface.

6. The power storage unit according to claim 1 or 2, wherein: The electrode sheet comprises: a sheet-shaped current collector; and a tab lead protruding from the current collector in the axial direction of the wound electrode body, The bulge is formed by the tab lead. The recessed portion is located radially outward of the wound electrode body relative to the tab lead.