Substrate and preparation method thereof, display panel and display device

By designing the special connection structure between the active layer and the signal line on the substrate and optimizing the etching process, the problem of too low TFT opening current is solved, and the performance and quality of the display product are improved.

CN119031756APending Publication Date: 2024-11-26BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310594461.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-24
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In display products that use top gate thin film transistors (TFTs), there is a problem that the TFT opening current is too low or even unable to turn on, which affects the quality of the display products.

Method used

A substrate structure is designed in which the active layer is connected to the signal line through the first and second vias, the first and second sub-parts form a recessed surface to improve conductionization, reduce conductionization resistance, and by etching The process optimizes the thickness of the second insulating layer and the size of the channel region to increase the open state current of the TFT.

Benefits of technology

It effectively improves the TFT's open-state current, reduces the conductor resistance, improves the performance and opening performance of the display product, and solves the problem of too low TFT's opening current.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119031756A_ABST
    Figure CN119031756A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a substrate and a preparation method thereof, a display panel and a display device. The substrate comprises a first metal layer, a first insulating layer, an active layer, a second insulating layer and a second metal layer which are sequentially arranged on the substrate, the first metal layer comprises a signal line, the second insulating layer is provided with a first via hole, the first via hole comprises a first sub-hole and a second sub-hole which are communicated with each other, and part of the surface of the active layer is located in the area where the first sub-hole is located. Part of the surface of the signal line is located in the area where the second sub-hole is located, the overlapped part of the active layer and the first sub-hole comprises a first sub-part and a second sub-part close to the second sub-hole, the first sub-part is sunken towards the substrate direction relative to the second sub-part to form a first sunken surface, and the first sunken surface is converted into a preset thickness by a conductor; the second metal layer comprises a first pole, the first pole is in lap joint with the surface of the second sub-part through the first sub-hole, and the first pole is connected with the signal line through the second sub-hole. According to the technical scheme, the conductor resistance of the active layer can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of display technology, and in particular to a substrate and a preparation method thereof, a display panel, and a display device. Background Art

[0002] In the related art, when a top-gate thin film transistor (TFT) is used on a substrate, an insulating layer is disposed above the active layer, a source electrode and a drain electrode are disposed above the insulating layer, and the source electrode and the drain electrode are connected to the active layer through vias penetrating the insulating layer. Display products using top-gate thin film transistors have the problem that the TFT turn-on current is too low or even cannot be turned on, which affects the quality of the display products. Summary of the invention

[0003] The embodiments of the present disclosure provide a substrate and a method for preparing the same, a display panel, and a display device to solve or alleviate one or more technical problems in the prior art.

[0004] As a first aspect of an embodiment of the present disclosure, an embodiment of the present disclosure provides a substrate, comprising

[0005] substrate;

[0006] A first metal layer, located at one side of the substrate, the first metal layer comprising a signal line;

[0007] A first insulating layer, located on a side of the first metal layer facing away from the substrate;

[0008] An active layer, located on a side of the first insulating layer facing away from the substrate;

[0009] a second insulating layer, located on a side of the active layer away from the substrate, the second insulating layer being provided with a first via hole, the first via hole comprising a first sub-hole and a second sub-hole interconnected with each other, the first sub-hole penetrating the second insulating layer, a portion of the surface of the active layer being located in the region where the first sub-hole is located, the second sub-hole penetrating the second insulating layer and the first insulating layer, a portion of the surface of the signal line being located in the region where the second sub-hole is located, an overlapping portion of the active layer and the first sub-hole comprising a first sub-portion and a second sub-portion, the second sub-portion being closer to the second sub-portion relative to the first sub-portion, the first sub-portion being concave relative to the second sub-portion toward the substrate to form a first concave surface, and the first concave surface being conductorized to a preset thickness;

[0010] The second metal layer is located on the side of the second insulating layer away from the substrate. The second metal layer includes a first electrode, which is overlapped with the surface of the second sub-portion through the first sub-hole and connected to the signal line through the second sub-hole.

[0011] In some possible implementations, the second insulating layer is sandwiched between the second metal layer and the first insulating layer, the active layer includes a channel region, and the active layer also includes a fifth sub-portion located between the first pole and the channel region and outside the first via hole, and the thickness of the fifth sub-portion is greater than the thickness of the second sub-portion.

[0012] In some possible implementations, the size of the fifth sub-portion in the first direction is greater than or equal to 100 angstroms, the size of the fifth sub-portion in the first direction is less than or equal to the size of the channel region in the first direction, and / or,

[0013] The size of the second sub-portion in the first direction is greater than or equal to 100 angstroms, and the size of the second sub-portion in the first direction is smaller than the size of the channel region in the first direction. The first direction is a direction perpendicular to the substrate.

[0014] In some possible implementations, the size of the fifth sub-portion in the first direction is greater than or equal to 100 angstroms, the size of the fifth sub-portion in the first direction is less than or equal to the size of the channel region in the first direction, the size of the channel region in the first direction is 200 angstroms-1000 angstroms, and the first direction is a direction perpendicular to the substrate.

[0015] In some possible implementations, the second metal layer also includes a gate and a second electrode, the first electrode and the second electrode are located on both sides of the gate, the second insulating layer is also provided with a second via, the second via penetrates the second insulating layer, a portion of the surface of the active layer is located in the area where the second via is located, the overlapping portion of the active layer and the second via includes a third sub-portion and a fourth sub-portion, the third sub-portion is closer to the gate than the fourth sub-portion, the second electrode is overlapped and connected to the surface of the fourth sub-portion through the second via, the third sub-portion is recessed relative to the fourth sub-portion toward the substrate to form a second recessed surface, and the second recessed surface is conductorized to a preset thickness.

[0016] In some possible implementations, a size of the fourth sub-portion in a first direction is greater than or equal to 100 angstroms, and the first direction is a direction perpendicular to the substrate.

[0017] In some possible implementations, the substrate further includes a third insulating layer, a planar layer, and an electrode layer, which are sequentially arranged on a side of the second metal layer away from the substrate, and the electrode layer is connected to the second electrode.

[0018] In some possible implementations, the material of the active layer includes oxide semiconductor.

[0019] As a second aspect of an embodiment of the present disclosure, an embodiment of the present disclosure provides a method for preparing a substrate, comprising:

[0020] forming a first metal layer on one side of the substrate, the first metal layer comprising a signal line;

[0021] forming a first insulating layer on a side of the first metal layer facing away from the substrate;

[0022] forming an active layer on a side of the first insulating layer facing away from the substrate;

[0023] A second insulating layer is deposited on a side of the active layer away from the substrate, and the second insulating layer is patterned to form a first via hole, wherein the first via hole includes a first sub-hole and a second sub-hole that are interconnected, the first sub-hole penetrates the second insulating layer, a portion of the surface of the active layer is located in the region where the first sub-hole is located, the second sub-hole penetrates the second insulating layer and the first insulating layer, and a portion of the surface of the signal line is located in the region where the second sub-hole is located; the overlapping portion of the active layer and the first sub-hole includes a first sub-portion and a second sub-portion, and the second sub-portion is closer to the second sub-portion than the first sub-portion;

[0024] A second metal layer is formed on a side of the second insulating layer facing away from the substrate, the second metal layer includes a first electrode, the first electrode is overlapped with the surface of the second sub-portion through the first sub-hole, and the first electrode is connected to the signal line through the second sub-hole;

[0025] The method also includes:

[0026] The first sub-portion is etched so that the first sub-portion is recessed relative to the second sub-portion toward the substrate to form a first recessed surface, and the active layer is conductorized, and the first recessed surface is conductorized to a preset thickness.

[0027] In some possible implementations, etching the first sub-portion includes:

[0028] The second metal layer is used as a mask and an etching process is used to remove the second insulating layer outside the second metal layer. Etching damage is formed on the side of the first sub-portion away from the substrate, so that the first sub-portion is recessed toward the substrate relative to the second sub-portion to form a first recessed surface.

[0029] In some possible implementations, the second metal layer further includes a gate and a second electrode, and the method further includes

[0030] The second insulating layer is patterned to form a second via hole, the second via hole penetrates the second insulating layer, a portion of the surface of the active layer is located in the area where the second via hole is located, the overlapping portion of the active layer and the second via hole includes a third sub-portion and a fourth sub-portion, the third sub-portion is closer to the gate than the fourth sub-portion, and the second electrode is overlapped and connected with the surface of the fourth sub-portion through the second via hole;

[0031] In the process of removing the second insulating layer outside the second metal layer by etching, etching damage is formed on the side of the fourth sub-portion away from the substrate, so that the fourth sub-portion is recessed toward the substrate relative to the third sub-portion to form a second recessed surface.

[0032] As a third aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a display panel, comprising a substrate of any disclosed embodiment of the first aspect.

[0033] As a fourth aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a display device, comprising a substrate according to any disclosed embodiment of the first aspect or a display panel according to any disclosed embodiment of the third aspect.

[0034] The technical solution of the embodiment of the present disclosure can achieve the following beneficial effects: the conductor resistance of the active layer can be reduced.

[0035] The above summary is for illustrative purposes only and is not intended to be limiting in any way. In addition to the illustrative aspects, embodiments and features described above, further aspects, embodiments and features of the present disclosure will be readily apparent by reference to the accompanying drawings and the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] In the accompanying drawings, unless otherwise specified, the same reference numerals throughout the multiple drawings represent the same or similar parts or elements. These drawings are not necessarily drawn to scale. It should be understood that these drawings only depict some embodiments according to the present disclosure and should not be regarded as limiting the scope of the present disclosure.

[0037] Figure 1 is a schematic cross-sectional view of a substrate;

[0038] Figure 2 is a schematic cross-sectional view of a substrate in one embodiment of the present disclosure;

[0039] Figure 3 is a partial plan view of a substrate in one embodiment of the present disclosure;

[0040] Figure 4A is a partial schematic diagram of a microscope of the substrate disclosed in the present invention;

[0041] Figure 4B A schematic diagram of a microscope cross section of the first via hole of the substrate disclosed in the present invention

[0042] Figure 4C For this disclosure Figure 4B Microscope magnification of

[0043] Figure 5 is a schematic cross-sectional view of a substrate in another embodiment of the present disclosure;

[0044] Figure 6 is a schematic cross-sectional view of a substrate in another embodiment of the present disclosure;

[0045] Figure 7 is a partial plan view of a substrate in another embodiment of the present disclosure;

[0046] Figure 8 is a schematic cross-sectional view of a substrate in another embodiment of the present disclosure;

[0047] Fig.9A It is a schematic diagram of a plane microscope of a second via hole of the substrate disclosed in the present invention;

[0048] Fig. 9B This is a microscope schematic diagram of a second via cross section of the present disclosure;

[0049] Fig.10 is a cross-sectional schematic diagram of another substrate;

[0050] Fig.11 is a cross-sectional schematic diagram of a substrate in another embodiment of the present disclosure;

[0051] Fig. 12A It is a cross-sectional schematic diagram after a signal line is formed in a substrate according to an embodiment of the present disclosure;

[0052] Fig. 12B It is a plan view schematic diagram of a substrate after an active layer is formed in an embodiment of the present disclosure;

[0053] Fig.13 It is a cross-sectional schematic diagram after a second insulating layer is formed in a substrate according to an embodiment of the present disclosure;

[0054] Fig.14A It is a cross-sectional schematic diagram after a first via hole and a second via hole are formed in a substrate according to an embodiment of the present disclosure;

[0055] Fig. 14B for Fig.14A Schematic diagram of the plane;

[0056] Fig.15 It is a cross-sectional schematic diagram of a substrate after a second metal layer is formed in an embodiment of the present disclosure;

[0057] Fig.16 It is a schematic cross-sectional view after the second insulating layer outside the second metal layer is removed by etching in the substrate.

[0058] Description of reference numerals:

[0059] 10. substrate; 20. first metal layer; 30. first insulating layer; 40. active layer; 50. second insulating layer; 60. second metal layer; 70. third insulating layer; 80. flat layer; 21. signal line; 41. first recessed surface; 42. second recessed surface; 51. first via hole; 51a. first sub-hole; 51b. second sub-hole; 52. second via hole; 61. first pole; 62. second pole; 63. gate; 91. pixel electrode. DETAILED DESCRIPTION

[0060] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present disclosure. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.

[0061] Figure 1 FIG. 1 is a schematic cross-sectional view of a substrate. Figure 1 As shown, the substrate includes a substrate 10, a first metal layer 20, a first insulating layer 30, an active layer 40, a second insulating layer 50 and a second metal layer 60. The first metal layer 20 is located on one side of the substrate 10, and the first metal layer 20 includes a signal line 21. The first insulating layer 30 is located on the side of the first metal layer 20 away from the substrate 10, and the active layer 40 is located on the side of the first insulating layer 30 away from the substrate 10. The second insulating layer 50 is located on the side of the active layer 40 away from the substrate 10. The second insulating layer 50 is provided with a first via 51 and a second via 52, and the second metal layer 60 is located on the side of the second insulating layer 50 away from the substrate 10, and the second metal layer 60 includes a first electrode 61, a second electrode 62 and a gate 63. For example, the first electrode 61 can be a source electrode, and the second electrode 62 can be a drain electrode.

[0062] The first via hole 51 and the second via hole 52 both penetrate the second insulating layer 50. The first via hole 51 includes a first sub-hole 51a and a second sub-hole 51b that are interconnected. The first sub-hole 51a penetrates the second insulating layer 50. Part of the surface of the active layer is located in the area where the first sub-hole 51a is located. The second sub-hole 51b penetrates the second insulating layer 50 and the first insulating layer 30. Part of the surface of the signal line 21 is located in the area where the second sub-hole 51b is located. The first pole 61 can be connected to the active layer 40 through the first sub-hole 51a. The first pole 61 can also be connected to the signal line 21 through the second sub-hole 51b. The second pole 62 can be connected to the active layer 40 through the second via hole 52. Figure 1 The substrate shown also includes a third insulating layer 70, a planar layer 80 and a pixel electrode 91, and the pixel electrode 91 is connected to the second electrode 62. The data signal on the signal line 21 can be transmitted to the active layer 40 through the first electrode 61. When the gate 63 is provided with a gate signal, the data signal is transmitted to the second electrode 62, and then transmitted to the pixel electrode 91. It should be noted that after the second metal layer 60 is formed, the second metal layer 60 is used as a mask to etch away the second insulating layer material outside the second metal layer 60. Therefore, in Figure 1 There is no second insulating layer between the first electrode 61 and the gate 63 , and there is no second insulating layer between the second electrode 64 and the gate 63 .

[0063] Figure 1In the substrate shown, the first pole 61 is overlapped and connected with the overlapping surface of the active layer 14 through the first sub-hole 51a, and the first pole 61 covers the surface of the active layer 40 located in the area where the first sub-hole 51a is located. The second pole 62 is connected to the active layer 40 through the second via hole 52, and the second pole 62 covers the surface of the active layer 40 located in the area where the second via hole 52 is located, that is, the first pole 61 completely covers the first sub-hole 51a, and the second pole 62 completely covers the second via hole 52. This method will cause the first pole 61 and the second pole 62 to block ion injection when the active layer 40 is subjected to the conductorization process, resulting in insufficient conductorization of the active layer 30 below the metal layer.

[0064] Exemplarily, when the active layer is made conductive by an ion implantation process, for example, helium ions or helium-argon ions are implanted to physically bombard the active layer 40, thereby destroying the surface structure of the active layer 40 and making the exposed active layer 40 conductive. Figure 1 The metal covering the active layer 40 of the substrate shown, such as the first electrode 61 and the second electrode 62, will block the ion implantation, which will cause the active layer 40 below the metal to be in a high resistance state.

[0065] Figure 1 The insufficient conductorization of the active layer in the substrate shown can be understood as the active layer in the first via 51 and the second via 52 being in a high resistance state, resulting in excessive contact resistance between the first electrode 61 and the second electrode 62 and the active layer 40, which in turn results in too low TFT on-state current, affecting TFT conduction.

[0066] In order to solve the problem of too low TFT on-state current in the substrate in the related art, an embodiment of the present disclosure provides a substrate, and the technical solution of the substrate is described below with reference to the accompanying drawings.

[0067] Figure 2 is a schematic cross-sectional view of a substrate in one embodiment of the present disclosure, Figure 3 is a partial plan view of a substrate in an embodiment of the present disclosure, Figure 2 Can be Figure 3 AA section diagram of the Figure 2 and Figure 3 As shown, a substrate according to an embodiment of the present disclosure may include a substrate 10, a first metal layer 20, a first insulating layer 30, an active layer 40, a second insulating layer 50, and a second metal layer 60. The first metal layer 20 is located on one side of the substrate 10, and the first metal layer 20 includes a signal line 21, which may be used to transmit a data signal. The first insulating layer 30 is located on a side of the first metal layer 20 that is away from the substrate 10, and the active layer 40 is located on a side of the first insulating layer 30 that is away from the substrate 10. The first insulating layer 30 may also be called a buffer layer.

[0068] The second insulating layer 50 is located on the side of the active layer 40 away from the substrate 10. The second insulating layer 50 is provided with a first via hole 51, and the first via hole 51 includes a first sub-hole 51a and a second sub-hole 51b that are interconnected. The first sub-hole 51 penetrates the second insulating layer 50, and part of the surface of the active layer 40 is located in the area where the first sub-hole 51 is located, that is, the first sub-hole 51a penetrates the second insulating layer 50 to expose part of the surface of the active layer, and the second sub-hole 51b penetrates the second insulating layer 50 and the first insulating layer 30 to expose part of the surface of the signal line 21. The second insulating layer 50 can also be called a gate insulating layer. It should be noted that the K via penetrates the second film layer to expose part of the surface of the first film layer. It should be understood that the first film layer located in the area where the K via is located is not covered by the second film layer, so that before other film layers are formed above the K via, the first film layer in the area where the K via is located is exposed through the K via. Those skilled in the art understand that other film layers can be formed above the K via to cover the first film layer in the area where the K via is located.

[0069] The overlapping portion of the active layer 40 and the first sub-hole 51a includes the first sub-portion 40a and the second sub-portion 40b, and the second sub-portion 40b is closer to the second sub-hole 51b relative to the first sub-portion 40a. The surface of the second sub-portion 40b on the side away from the substrate 10 is overlapped and connected with the first pole 61. The overlapping portion of the active layer 40 and the first sub-hole 51a can be understood as the portion of the active layer 40 exposed through the first sub-hole 51a, that is, the surface of the active layer exposed after etching the first via hole 51a, and an insulating layer can also be provided on the portion of the active layer exposed through the first sub-hole 51a.

[0070] The first sub-portion 40a is recessed relative to the second sub-portion 40b toward the substrate 10 to form a first recessed surface 41. The first recessed surface 41 is conductively conductive to a preset thickness. Figure 2 4 shows the conductive area along the first recessed surface 41. The size of the first sub-portion 40a in the first direction is smaller than the size of the second sub-portion 40b in the first direction, the first direction is a direction perpendicular to the substrate 10, the first sub-portion 40a forms a first recessed portion relative to the second sub-portion 40b and the active layer outside the first via hole, and the exposed surface of the first recessed portion is the first recessed surface.

[0071] The second metal layer 60 is located on the side of the second insulating layer 50 away from the substrate 10, and the second metal layer 60 includes a first electrode 61, the first electrode 61 is overlapped and connected to a part of the exposed surface of the active layer 40 through the first sub-hole 51a, and the first electrode 61 is connected to the signal line 21 through the second sub-hole 51b. Figure 2 As shown, the first pole 61 is overlap-connected with the second sub-portion 40b through the first sub-hole 51a.

[0072] Figure 1In the substrate shown, the orthographic projection of the first sub-hole 51a on the substrate 10 is located within the orthographic projection of the first electrode 61 on the substrate 10, that is, the first electrode 61 covers the first sub-hole 51a, so that when the active layer 40 is conductorized above the second metal layer 60, the metal layer above the active layer 40 will block ion injection or bombardment during conductorization, and the active layer 40 located in the first sub-hole 51a and below the first electrode 61 is in a high-resistance state, which leads to excessive contact resistance of the overlapping portion of the active layer 40 and the first electrode 61, thereby reducing the TFT turn-on current and affecting the TFT conduction performance.

[0073] The overlapping part of the active layer 40 and the first sub-hole 51a includes a first sub-part 40a and a second sub-part 40b, the second sub-part 40b is closer to the second sub-hole 51b relative to the first sub-part 40a, and the first pole 61 is overlapped and connected with the second sub-part 40b through the first sub-hole 51a. In the case where the surface of the first sub-part 40a on the side away from the substrate 10 and the surface of the second sub-part 40b on the side away from the substrate 10 are flush, that is, the surface of the part of the active layer 40 exposed through the first sub-hole 51a is a flat surface, although the conductor can be cut into the area covered by the first pole 61, so that at least a part of the second sub-part 40b is conductorized, such a structure will have a problem of insufficient conductorization of part of the active layer 40 due to metal blocking, resulting in excessively large contact resistance between the first pole 61 and the active layer 40, thereby causing the TFT on-state current to be too low, resulting in failure to turn on, affecting the product yield.

[0074] Figure 2 In the substrate shown in the figure, the first sub-portion 40a is recessed relative to the second sub-portion 40b toward the substrate 10 to form a first recessed surface 41, so that the side wall of the second sub-portion 40b can be exposed through the first recessed portion, so that when the exposed surface of the active layer 30 is conductorized, the side wall of the second sub-portion 40b can be conductorized to a preset thickness, so that the first electrode 61 is electrically connected to the active layer 40 through the conductorized side wall of the second sub-portion 40b. Since the side wall of the second sub-portion 40b is exposed through the first recessed portion, the side wall position of the second sub-portion 40b can be fully conductorized, which greatly reduces the connection resistance between the first electrode 61 and the active layer 40, increases the on-state current of the TFT, and improves the product performance.

[0075] When the active layer 40 is subjected to conductorization treatment, a suitable conductorization process may be selected, such as an ion implantation process or an ion bombardment process, so that when the exposed portion of the active layer 40 is fully conductorized, the exposed side wall of the second sub-portion 40b may be more fully conductorized, thereby reducing the contact resistance of the overlapping portion of the first electrode 61 and the active layer 40 and increasing the on-state current of the TFT.

[0076] In the substrate of the embodiment of the present disclosure, the first via hole 51 simultaneously realizes the overlapping connection between the first pole 61 and the active layer 40 and the connection between the first pole 61 and the signal line. The overlapping part of the active layer 40 and the first sub-hole 51a includes a first sub-part 40a and a second sub-part 40b. The second sub-part 40b is closer to the second sub-hole 51b relative to the first sub-part 40a. The first sub-part 40a is recessed relative to the second sub-part 40b toward the substrate to form a first recessed surface 41. The first recessed surface 41 can expose the side of the second sub-part 40b located below the first pole 61. The first recessed surface 41 is conductorized to a preset thickness. In this way, when the exposed surface of the active layer 40 is conductorized, the conductor will cut into the area covered by the first pole 61 through the side of the first recessed surface 41, so that at least a part of the second sub-part 40b below the first pole 61 is conductorized, so that the first pole 61 can achieve electrical connection with the active layer 40 through the conductorized area. With respect to Figure 1 The display substrate shown in the figure, when being conductive, ions can cut into the second sub-portion 40b from the side through the first recessed portion, preventing metal from blocking ion injection, reducing the conductive resistance inside the TFT and the contact resistance between the first electrode 61 and the active layer 40, and improving the product yield. In addition, the size of the first electrode 61 of the substrate in the direction parallel to the substrate 10 of the embodiment of the present disclosure is relatively Figure 1 The first electrode 61 of the substrate shown has a smaller size in the direction parallel to the substrate 10, which is beneficial to reducing the area of ​​the TFT, further increasing the space utilization of the substrate, and improving the aperture ratio of the display product.

[0077] When the substrate of the present disclosure is applied to a display product, the signal line 21 can be used to transmit a data signal, and the data signal is transmitted to the active layer 40 through the first electrode 61, and the data signal can be transmitted to the pixel electrode 91 through the active layer 40 to realize display. In other embodiments, the signal line 21 can also transmit other signals, so that other signals are transmitted upward through the first electrode 61 and the active layer 40.

[0078] like Figure 2 As shown, the first electrode 61 is connected to the signal line 21 through the second sub-hole 51b. Exemplarily, the orthographic projection of the second sub-hole 51b on the substrate 10 may be located within the orthographic projection of the first electrode 61 on the substrate 10, or the orthographic projection of the second sub-hole 51b on the substrate 10 may partially overlap with the orthographic projection of the first electrode 61 on the substrate 10, both of which can achieve the connection between the first electrode 61 and the signal line 21 through the second sub-hole 51b.

[0079] Figure 4A is a partial schematic diagram of a microscope of the substrate disclosed in the present invention; Figure 4B is a microscope schematic diagram of a first via cross-section of the substrate disclosed in the present invention, Figure 4C For this disclosure Figure 4B Microscope magnification of . Figure 4B for Figure 4A Schematic diagram of the cross section. Figure 4B and Figure 4C In FIG. 4 , the first concave surface formed by the first sub-portion 40a of the active layer 40 can be seen. Figure 4B The active layer (Active) on the right side of the middle is concave to form a first concave surface 41 . In FIG. 4 c , the concave portion of the active layer in the elliptical frame is the first concave surface 41 .

[0080] It should be noted that in Figure 4B and Figure 4C The Gate in represents the gate, source and drain set on the same layer. Figure 4B and Figure 4C The Gate in the gate can be understood as the gate metal layer or the second metal layer. Figure 4B In the figure, the position of Gate is the first pole 61. Figure 4B The Data in represents the signal line 21 in the embodiment of the present disclosure.

[0081] In one embodiment, a single patterning process can be used to form the first recessed surface 41. For example, after forming the second metal layer 60, a photoresist is coated on the second metal layer 60, the photoresist is masked and exposed, the photoresist at the position of the first recessed surface 41 is removed, and the active layer at the position of the first recessed surface 41 is etched to form the first recessed surface 41.

[0082] Figure 5 FIG. 1 is a cross-sectional schematic diagram of a substrate in another embodiment of the present disclosure. In one disclosed embodiment, Figure 5 As shown, the second insulating layer 50 is sandwiched between the second metal layer 60 and the first insulating layer 30. The second insulating layer 50 includes a first sub-insulating portion 53 sandwiched between the first pole 61 and the first insulating layer 30, a second sub-insulating portion 54 sandwiched between the gate 63 and the active layer 40, and a third sub-insulating portion 55 sandwiched between the second pole 62 and the first insulating layer 30. After the second metal layer 60 is formed, the second metal layer 60 is used as a mask, and the second insulating layer 50 located outside the second metal layer 60 is removed by an etching process, and the second insulating layer 50 located in the area where the gate 63, the first pole 61 and the second pole 62 are located is retained to form the second sub-insulating portion 54, the first sub-insulating portion 53 and the third sub-insulating portion 55.

[0083] Reference Figure 5As shown, in a disclosed embodiment, the active layer 40 includes a channel region 40f, and the active layer 40 also includes a fifth sub-portion 40e located between the first pole 61 and the channel region and located outside the first via hole 51. The thickness of the fifth sub-portion 40e is greater than the thickness of the second sub-portion 40b, and the thickness represents the size of the fifth sub-portion 40e and the second sub-portion 40b in a direction perpendicular to the substrate 10. The thickness of the fifth sub-portion 40e is greater than the thickness of the second sub-portion 40b, and the thickness of the second sub-portion 40b is greater than the thickness of the first sub-portion 40a. There is a thickness difference between the various portions of the active layer 40, and steps are formed between the various sub-portions, which can reduce the conductor resistance.

[0084] In the process of preparing the substrate, in the patterning process of forming the first via hole 51, the first sub-hole 51a is formed first, and at this time, the second sub-hole 51b is partially etched, and then the first insulating layer 30 is etched to completely form the second sub-hole 51b. In the process of etching the second sub-hole 51b, the portion of the active layer 40 exposed through the first sub-hole 51a will be exposed to the etching environment, and the active layer 40 will be etched damaged, that is, the first sub-portion 40a and the second sub-portion 40b exposed through the first sub-portion 51a of the active layer 40 will be etched damaged, and the thickness of the first sub-portion 40a and the second sub-portion 40b will be less than the thickness of the fifth sub-portion 40e. After forming the second metal layer 60, an etching process is required to etch the second insulating layer 50 outside the second metal layer 60. In this etching process, the first sub-portion 40a that is not covered by the second metal layer 60 will continue to be exposed to the etching environment and continue to undergo the etching process of the second insulating layer 50. The etching process can be controlled to make the first sub-portion 40a recessed relative to the second sub-portion 40b toward the substrate 10 to form a first recessed surface 41. This can be achieved using the existing mask process without increasing the substrate preparation process steps, thereby reducing costs.

[0085] After the second metal layer 60 is formed, before the second insulating layer 50 outside the second metal layer 60 is etched by the etching process, the fifth sub-portion 40e is covered with the second insulating layer 50, and the second metal layer 60 is used as a mask to remove the second insulating layer 50 on the fifth sub-portion 40e, and the first sub-portion 40a can be recessed relative to the second sub-portion 40b toward the substrate 10 to form a first recessed surface 41 by the etching process at the same time, until the surface of the fifth sub-portion 40e facing away from the substrate 10 is exposed, so that the etching damage to the fifth sub-portion 40e can be reduced. The surface of the fifth sub-portion 40e facing away from the substrate is roughly flush with the surface of the channel region 40f facing away from the substrate 10, so that in the process of conducting the exposed leakage area of ​​the active layer 40, the conductor will cut into the channel region 40f, which can prevent the conductor from cutting too deep into the channel region 40f, reduce the size of the channel region 40f to be conducted, improve the performance of the channel region 40f, and improve the stability of the TFT.

[0086] like Figure 5 As shown, in a disclosed embodiment, the thickness of the channel region 40f is H, the thickness of the first sub-portion 40a is H3, the thickness of the second sub-portion 40b is H3+H2a, the thickness of the fifth sub-portion 40e is H4, and the thickness of the channel region 40f is equal to the thickness of the fifth sub-portion 40e. The thickness of the channel region 40f is greater than the thickness of the second sub-portion 40b, and the thickness difference between the two is H1, and H1 can represent etching damage formed by etching the first insulating layer 30 to form the second sub-hole 51b. The height difference between the first sub-portion 40a and the second sub-portion 40b is H2a, so that the first sub-portion 40a can be cut through the H2a part during conductorization to prevent insufficient conductorization of the first sub-portion 40a. The thickness H of the channel region 40f is equal to the thickness H4 of the fifth sub-portion 40e, which can prevent the conductor from cutting too deep into the channel region 40f and reduce the size of the conductorized channel region 40f.

[0087] In one embodiment, after etching the second insulating layer 50 outside the second metal layer 60 by an etching process, the depth of the first recessed surface 41 may not reach a preset depth. In order to make the first recessed surface 41 reach the preset depth, the first sub-portion 40a may be processed by a patterning process, so that the first sub-portion 40a is recessed relative to the second sub-portion 40b toward the substrate 10 to form the first recessed surface 41, and the first recessed surface reaches the preset depth. In this way, when the first recessed surface 41 is patterned, the fifth sub-portion 40e will not be etched damaged, preventing the conductor from cutting into the depth of the channel region 40f laterally along the boundary of the second sub-insulating portion 54, reducing the size of the channel region 40f to be conductorized, and ensuring the performance of the TFT.

[0088] Figure 6is a cross-sectional schematic diagram of a substrate in another embodiment of the present disclosure, Figure 7 for Figure 5 or Figure 6 A plan view of Figure 6 and Figure 7 As shown, in a disclosed embodiment, the thickness of the channel region 40f is H, the thickness of the first sub-portion 40a is H3, the thickness of the second sub-portion 40b is H3+H2a, the thickness of the fifth sub-portion 40e is H4, and the thickness of the channel region 40f is greater than the thickness of the fifth sub-portion 40e. The thickness difference between the channel region 40f and the second sub-portion 40b is H1, and the thickness difference between the two can represent the etching damage formed on the active layer 40 when the first insulating layer 30 is etched to form the second sub-hole 51b. The thickness difference between the channel region 40f and the fifth sub-portion 40e is H2b, which represents the etching damage formed on the active layer 40 when the second sub-portion 40a is etched.

[0089] In a disclosed embodiment, the size of the fifth sub-portion 40e in the first direction Y is greater than or equal to 100 angstroms. The size of the channel region 40f in the first direction Y is equal to the size of the fifth sub-portion 40e in the first direction Y. The thickness of the first sub-portion 40a and the thickness of the second sub-portion 40b can be set according to the thickness of the active layer 40, which is not limited here. The thickness of the fifth sub-portion 40e is greater than or equal to 100 angstroms. If it is less than this value, it is easy to increase the conductor resistance and reduce the TFT on-state current.

[0090] In a disclosed embodiment, the size of the second sub-portion 40b in the first direction Y is greater than or equal to 100 angstroms, the first direction Y is a direction perpendicular to the substrate 10, and the size of the second sub-portion 40b in the first direction is smaller than the size of the channel region in the first direction. As shown in the figure, the size of the second sub-portion 40b in the first direction Y is H3+H2a, which is greater than 100 angstroms. If it is smaller than this value, it is easy to increase the contact resistance between the second sub-portion 40b and the first electrode 61.

[0091] It should be noted that the thickness H3 of the first sub-portion 40a may be equal to 0, that is, the active layer is partially disposed through. Figure 7 It can be seen from the figure that when the thickness H3 of the first sub-portion 40a can be equal to 0, the second sub-portion 40b can be connected to the fifth sub-portion 40e through the portion outside the first sub-portion 40a.

[0092] Reference Figure 6As shown, in a disclosed embodiment, the size of the channel region 40f in the first direction Y is greater than the size of the fifth sub-portion 40e in the first direction Y, and the thickness difference between the channel region 40f and the fifth sub-portion 40e is H2b. The size of the fifth sub-portion 40e in the first direction Y is greater than or equal to 100 angstroms, and the size of the fifth sub-portion 40e in the first direction Y is smaller than the size of the channel region 40f in the first direction Y. If the size is smaller than this value, the conductor resistance will increase. The size of the channel region 40f in the first direction Y is 200 angstroms-1000 angstroms, and the first direction Y is a direction perpendicular to the substrate 10. The specific thickness values ​​of the first sub-portion 40a and the second sub-portion 40b of the active layer are not limited here, and can be set accordingly according to the thickness of the channel region 40f.

[0093] Exemplarily, the thickness of the channel region 40f may be 275 angstroms, 300 angstroms, 325 angstroms, 350 angstroms, 400 angstroms, 450 angstroms, 500 angstroms, 600 angstroms, 700 angstroms, etc. The thickness of the active layer 40 is not specifically limited here and can be determined according to actual conditions.

[0094] Figure 8 FIG. 1 is a schematic cross-sectional view of a substrate in another embodiment of the present disclosure. Figure 8 As shown, the second metal layer 60 further includes a gate 63 and a second electrode 62, and the first electrode 61 and the second electrode 62 are located on both sides of the gate 63. The second insulating layer 50 is also provided with a second via hole 52, and the second via hole 52 penetrates the second insulating layer 50. Part of the surface of the active layer 40 is located in the area where the second via hole 52 is located. The overlapping part of the active layer 40 and the second via hole 52 includes a third sub-portion 40c and a fourth sub-portion 40d, and the third sub-portion 40c is closer to the gate 63 than the fourth sub-portion 40d. The second electrode 62 is overlapped and connected with the surface of the fourth sub-portion 40d through the second via hole 52, and the third sub-portion 40c is recessed relative to the fourth sub-portion 40d toward the substrate 10 to form a second recessed surface 42, and the second recessed surface 42 is conductively configured to a preset thickness.

[0095] In the process of preparing the substrate, during the process of etching the first sub-hole 51a, the portion of the active layer 40 exposed through the second via hole 52 will be exposed to the etching environment, and the active layer 40 will be etched damaged, that is, the third sub-portion 40c and the fourth sub-portion 40d exposed by the second via hole 52 of the active layer 40 will be etched damaged, and the thickness of the third sub-portion 40c and the fourth sub-portion 40d will be less than the thickness of the fifth sub-portion 40e. When the second insulating layer 50 outside the second metal layer 60 is etched by an etching process, the third sub-portion 40c will be etched damaged, forming a depression relative to the fourth sub-portion 40d toward the substrate 10 to form a second depression surface 42.

[0096] like Figure 8 As shown, the third sub-portion 40c forms a second recessed surface 42 relative to the fourth sub-portion 40d and the fifth sub-portion 40e, and the fourth sub-portion 40d overlaps the second pole 62. When the exposed surface of the active layer 40 is conductorized, ions can cut into the fourth sub-portion 40c through the side of the second recessed portion and the second recessed surface, so that at least a portion of the fourth sub-portion 40d is conductorized, thereby reducing the contact resistance between the fourth sub-portion 40c and the second pole 62.

[0097] It should be noted that the shapes of the first via hole 51 , the second via hole 52 , the first recessed portion, and the second recessed portion may be elliptical, rectangular, or track-shaped, which is not limited here.

[0098] For example, Figure 8 As shown, the gate 63 is located on the surface of the second insulating layer 50 of the first via hole 51 and the second via hole 52. The first electrode 61 is located on the side of the first via hole 151 away from the gate 63, and the second electrode 62 is located on the side of the second via hole 52 away from the gate 63. Therefore, there is a part of the active layer exposed through the first via hole 51 between the gate 63 and the first electrode 61, and there is a part of the active layer exposed through the second via hole 52 between the gate 63 and the second electrode 62. When the active layer is conductorized, the exposed active layer 40 between the gate 63 and the first electrode 61 is conductorized, and the exposed active layer 40 between the gate 63 and the second electrode 62 is conductorized.

[0099] Exemplarily, the first metal layer 20 may further include a shielding portion, and an orthographic projection of the gate 63 on the substrate 10 and an orthographic projection of the active layer 40 on the substrate 10 have an overlapping region, and the orthographic projection of the overlapping region on the substrate 10 is located within the orthographic projection of the shielding portion on the substrate 10. Thus, the shielding portion can shield the channel region 40f of the TFT to prevent the channel region 40f from being affected by external light.

[0100] The active layer 40, the gate electrode 63, the first electrode 61 and the second electrode 62 form a TFT. The data signal on the signal line 21 can be transmitted to the active layer 40 through the first electrode 61. When the gate electrode 63 is provided with a gate signal, the data signal is transmitted to the second electrode 62 through the active layer 40. The second electrode 62 can be connected to the pixel electrode 91, so that the data signal can be transmitted to the pixel electrode 91 through the second electrode 62 to achieve display. It can be understood that in the organic light emitting diode display panel, the pixel electrode 91 can be an anode.

[0101] Fig.9A It is a schematic diagram of a plane microscope of a second via hole of the substrate disclosed in the present invention; Fig. 9B FIG. 1 is a schematic diagram of a microscope cross section of the second via hole disclosed in the present invention. Fig. 9B As shown, the second electrode 62 does not completely cover the second via 52 .

[0102] Fig.10 is a schematic cross-sectional view of another substrate, such as Fig.10 As shown, the gate electrode 63 and the first electrode 61 and the second electrode 62 of the substrate need to be patterned twice, and the embodiment of the present disclosure Figure 8 The substrate shown in FIG. 1 can be patterned to form a gate electrode 63 and a first electrode 61 and a second electrode 62 using a metal film layer. Fig.10 The substrate shown in the embodiment of the present disclosure can also reduce the steps of the substrate preparation process and reduce the cost.

[0103] In a disclosed embodiment, the size of the fourth sub-portion 40d in the first direction Y is greater than or equal to 100 angstroms, and the thickness of the fourth sub-portion 40d and the second sub-portion 40b are substantially equal. This can avoid an increase in the conductor resistance and prevent a decrease in the TFT on-state current.

[0104] Fig.11 FIG. 1 is a schematic cross-sectional view of a substrate in another embodiment of the present disclosure. In one disclosed embodiment, Fig.11 As shown, the substrate may further include a third insulating layer 70, a planar layer 80 and an electrode layer sequentially arranged on the side of the second metal layer 60 away from the substrate 10, and the electrode layer is connected to the second electrode 62. In a liquid crystal display product, the electrode layer may be a pixel electrode 91; in an OLED display product, the electrode layer may be an OLED anode layer.

[0105] In a disclosed embodiment, the material of the active layer 40 includes an oxide semiconductor. The active layer 40 may be a metal oxide such as indium gallium zinc oxide material (IGZO) or amorphous indium gallium zinc oxide material (a-IGZO), indium tin oxide (ITO), etc. The thin film transistor (Oxide TFT) formed by the oxide semiconductor has good uniformity and high mobility. The substrate formed in the disclosed embodiment has a top-gate thin film transistor, which has a high on-state current (Ion) and a stable current, and the substrate can be used in active matrix light emitting diode display products (AMOLED). The substrate formed in the disclosed embodiment has a top-gate thin film transistor, which has a high on-state current and low capacitance, and the substrate can be used in liquid crystal display products.

[0106] The embodiment of the present disclosure also provides a method for preparing a substrate, comprising: forming a first metal layer 20 on one side of a substrate 10, the first metal layer 20 including a signal line 21; forming a first insulating layer 30 on a side of the first metal layer 20 facing away from the substrate 10; forming an active layer 40 on a side of the first insulating layer 30 facing away from the substrate 10; depositing a second insulating layer 50 on a side of the active layer 40 facing away from the substrate 10, patterning the second insulating layer 50 to form a first via hole 51, the first via hole 51 including a first sub-hole 51a and a second sub-hole 51b that are interconnected, the first sub-hole 51a passing through the second insulating layer 50, a portion of the surface of the active layer 40 is located in the area where the first sub-hole 51a is located, the second sub-hole 51b passes through the second insulating layer 50 and the first insulating layer 30, and a portion of the signal line 21 is located in the area where the first sub-hole 51a is located. The sub-surface is located in the area where the second sub-hole 51b is located, and the overlapping part of the active layer 40 and the first sub-hole 51a includes a first sub-section 40a and a second sub-section 40b, and the second sub-section 40b is closer to the second sub-hole 51b relative to the first sub-section 40a; a second metal layer 60 is formed on the side of the second insulating layer 50 away from the substrate 10, and the second metal layer 60 includes a first pole 61, and the first pole 61 overlaps the surface of the first sub-hole 51a and the second sub-section 40b through the first sub-hole 51a, and the first pole 61 is connected to the signal line 21 through the second sub-hole 51b; the first sub-section 40a is etched so that the first sub-section 40a is recessed relative to the second sub-section 40b toward the substrate to form a first recessed surface 41, and the active layer 40 is conductorized, and the first recessed surface 41 is conductorized with a preset thickness.

[0107] In a disclosed embodiment, the first sub-portion 40a is etched, including using the second metal layer 60 as a mask and using an etching process to remove the second insulating layer 50 located outside the second metal layer 60, and etching damage is formed on the side of the first sub-portion 40a away from the substrate 10, so that the first sub-portion 40a is recessed toward the substrate 10 relative to the second sub-portion 40b to form a first recessed surface 41.

[0108] In a disclosed embodiment, the second metal layer 60 also includes a gate 63 and a second pole 62, and the method also includes: patterning the second insulating layer 50 to form a second via 52, the second via 52 penetrates the second insulating layer 50, a portion of the surface of the active layer 40 is located in the area where the second via 52 is located, and the overlapping portion of the active layer 40 and the second via 52 includes a third sub-portion 40c and a fourth sub-portion 40d, the third sub-portion 40c is closer to the gate 63 than the fourth sub-portion 40d, and the second pole 62 is overlapped and connected with the surface of the fourth sub-portion 40d through the second via 52; in the process of removing the second insulating layer 50 located outside the second metal layer 60 by an etching process, etching damage is formed on the side of the fourth sub-portion 40d away from the substrate 10, so that the fourth sub-portion 40d is recessed toward the substrate 10 relative to the third sub-portion 40c to form a second recessed surface 42.

[0109] The technical solution of the embodiment of the present disclosure is further explained below through the preparation process of the substrate in one embodiment of the present disclosure. It can be understood that the "patterning process" in the present disclosure, when the patterned material is an inorganic material or a metal layer, the "patterning process" may include processes such as coating photoresist, mask exposure, development, etching, and stripping photoresist. When the patterned material is an organic material (such as a photoresist or an organic resin), the "patterning process" may include processes such as mask exposure and development. The evaporation, deposition, coating, and coating in the present disclosure are all mature preparation processes in the relevant technology.

[0110] A first metal layer 20 is formed on one side of the substrate 10, and the first metal layer 20 includes a signal line 21. Exemplarily, a first metal film is deposited on one side of the substrate 10, and the first metal film is patterned to form the signal line 21, such as Fig. 12A and Fig. 12B shown. Fig. 12A It is a cross-sectional schematic diagram after a signal line is formed in a substrate according to an embodiment of the present disclosure. Fig. 12B It is a plan view schematically showing an active layer formed in a substrate according to an embodiment of the present disclosure.

[0111] A first insulating film is formed on the side of the first metal layer 20 facing away from the substrate 10. For example, the first insulating film may be deposited on the side of the first metal layer 20 facing away from the substrate 10, such as Fig.13 shown. Fig.13 It is a cross-sectional schematic diagram of depositing a second insulating film in a substrate according to an embodiment of the present disclosure.

[0112] The active layer 40 is formed on the side of the first insulating layer 30 facing away from the substrate 10. For example, an active thin film may be deposited on the side of the first insulating layer 30 facing away from the substrate 10, and the active thin film may be patterned to form the active layer 40, such as Fig.13 shown.

[0113] A second insulating film is deposited on the side of the active layer 40 facing away from the substrate 10, such as Fig.13 The second insulating layer 50 is patterned to form a first via hole 51 and a second via hole 52. The first via hole 51 includes a first sub-hole 51a and a second sub-hole 51b that are interconnected. The first sub-hole 51a penetrates the second insulating layer 50, and a portion of the surface of the active layer 40 is located in the area where the first sub-hole 51a is located. The second sub-hole 51b penetrates the second insulating layer 50 and the first insulating layer 30, and a portion of the surface of the signal line 21 is located in the area where the second sub-hole 51b is located. Fig.14A and Fig. 14B shown. Fig.14A Schematic diagram of a cross section after a first via hole 51 and a second via hole 52 are formed in a substrate according to an embodiment of the present disclosure. Fig. 14B for Fig.14A Schematic diagram of the floor plan.

[0114] Exemplarily, the orthographic projection of the first via hole 51 on the substrate 10 and the orthographic projection of the active layer 40 on the substrate 10 have an overlapping area, the portion of the first via hole 51 located in the overlapping area is the first sub-hole 51a, the portion of the first via hole 51 located outside the overlapping area is the second sub-hole 51b, and the orthographic projection of the second sub-hole 51b on the substrate 10 is located within the orthographic projection of the signal line 21 on the substrate 10. The orthographic projection of the second via hole 52 on the substrate 10 is located within the orthographic projection of the active layer 40 on the substrate 10.

[0115] The formation process of the second insulating layer 50 may include: depositing a second insulating film on the side of the active layer 40 facing away from the substrate 10, coating a photoresist on the side of the second insulating film facing away from the substrate 10, exposing and developing the photoresist, removing the photoresist at the positions of the first via hole 51 and the second via hole 52, retaining the photoresist at other positions, etching the second insulating film at the positions of the first via hole 51 and the second via hole 52, wherein the second via hole 52 penetrates the second insulating film, and a portion of the surface of the active layer 40 is located in the area where the second via hole 52 is located, and the second insulating film is formed. The first sub-hole 51a of a via hole 51 penetrates the second insulating film, a portion of the surface of the active layer 40 is located in the area where the first sub-hole 51a is located, and a portion of the surface of the signal line 21 is not exposed at the position of the second sub-hole 51b. The position of the second sub-hole 51b needs to continue to etch the second insulating layer 50 and the first insulating layer 30 above the signal line 21 after the second via hole 52 and the first sub-hole 51a expose the position of the active layer 40, until the second sub-hole 51b penetrates the second insulating layer 50 and the first insulating layer 30 to expose a portion of the surface of the signal line 21, as shown in FIG. Fig.14A shown.

[0116] Part of the surface of the signal line 21 is located in the area where the second sub-hole 51b is located. The size of the second sub-hole 51b in the direction perpendicular to the substrate 10 is larger than the size of the first sub-hole 51a and the second via hole 52 in the direction perpendicular to the substrate 10. In the subsequent etching process of the second sub-hole 51b, etching damage is formed on one side of the active layer 40 where the first sub-hole 51a and the second via hole 52 overlap, resulting in the upper surface of the active layer located in the area where the first sub-hole 51a is located being lower than the upper surface of the active layer 40 covered by the second insulating layer 50, and the upper surface of the active layer in the area where the second via hole 52 is located being lower than the upper surface of the active layer 40 covered by the second insulating layer 50, as shown in FIG. Fig.14A As shown. Exemplarily, the thickness of the active layer 40 may be 200 angstroms to 1000 angstroms. Fig.14A As shown in the figure, H1 represents the thickness of the active layer 40 damaged during the etching process of the first via hole 51 and the second via hole 52.

[0117] A second metal layer 60 is formed on the side of the second insulating layer 50 facing away from the substrate 10. The second metal layer 60 includes a first electrode 61, a second electrode 62 and a gate 63. Fig.15 shown. Fig.15 It is a cross-sectional schematic diagram after the second metal layer is formed in the substrate of an embodiment of the present disclosure. The first pole 61 is overlapped and connected with the overlapping surface of the active layer 40 through the first sub-hole 51a, and the first pole 61 is connected with the signal line 21 through the second sub-hole 51b. The second pole 62 is overlapped and connected with a part of the overlapping surface of the active layer 40 through the second via 52. The first pole 61 is overlapped and connected with a part of the surface of the active layer overlapped by the first sub-hole 51a. The part of the active layer located in the area where the first sub-hole 51a is located that overlaps with the first pole 61 is the second sub-part 40b, and the part of the active layer located in the area where the first sub-hole 51a is located that does not overlap with the first pole 61 is the first sub-part 40a. The second pole 62 is connected by overlapping a portion of the surface of the active layer overlapping with the second via 52. The portion of the active layer located in the area where the second via 52 is located that overlaps with the second pole 62 is the fourth sub-portion 40d, and the portion of the active layer located in the area where the second via 52 is located that does not overlap with the second pole 62 is the third sub-portion 40c.

[0118] The second metal layer 60 is used as a mask, and the second insulating layer 50 outside the second metal layer 60 is removed by an etching process. The second metal layer 60 is used as a mask, and the second insulating layer 50 is etched by a dry etching process. The second insulating layer 50 located in the area where the gate 63, the first pole 61 and the second pole 62 are located is retained, and the second insulating layer 50 includes a first sub-insulating portion sandwiched between the first pole 61 and the first insulating layer, a second sub-insulating portion sandwiched between the gate 63 and the active layer 40, and a third sub-insulating portion sandwiched between the second pole 62 and the first insulating layer, as shown in FIG. Fig.16 shown. Fig.16The schematic cross-sectional view of the substrate after the second insulating layer outside the second metal layer is removed by etching in one embodiment of the present disclosure. In the process of etching the second insulating layer 50 using a dry etching process, the first sub-portion 40a and the second sub-portion 40d on the side away from the substrate 10 are both exposed to the etching environment. The side of the first sub-portion 40a away from the substrate 10 forms a second etching damage, so that the first sub-portion 40a is recessed relative to the second sub-portion 40b toward the substrate 10 to form a first recessed surface 41, and the side of the fourth sub-portion 40d away from the substrate 10 forms a second etching damage, so that the fourth sub-portion 40d is recessed relative to the third sub-portion 40c toward the substrate 10 to form a second recessed surface 42.

[0119] right Fig.16 The substrate shown is conductorized, the first sub-portion 40a is conductorized, and the active layer 40 is electrically connected to the first pole 61. The fourth sub-portion 40d is conductorized, and the active layer 40 is electrically connected to the second pole 62.

[0120] The method for preparing the substrate may further include: forming a third insulating layer 70, a planar layer 80 and a pixel electrode 91 in sequence on a side of the second metal layer 60 facing away from the substrate 10, such as Fig.11 As shown, the pixel electrode 91 penetrates the planar layer 80 and the third insulating layer 70 and is connected to the second electrode 62 .

[0121] Exemplarily, the first insulating layer 30, the second insulating layer 50, and the third insulating layer 70 may be made of any one or more of silicon oxide (SiOx), silicon nitride (SiNx), and silicon oxynitride (SiON), and may be a single layer, a multilayer, or a composite layer. The first insulating layer 30 may be called a buffer layer, which is used to improve the water and oxygen resistance of the substrate, the second insulating layer 50 may be called a gate insulating (GI) layer, and the third insulating layer 70 may be called an interlayer insulating (ILD) layer.

[0122] Exemplarily, the first metal layer 20 and the second metal layer 60 may be made of metal materials, such as any one or more of silver (Ag), copper (Cu), aluminum (Al), titanium (Ti) and molybdenum (Mo), or alloy materials of the above metals, such as aluminum neodymium alloy (AlNd) or molybdenum niobium alloy (MoNb), and may be a single-layer structure or a multi-layer composite structure, such as Ti / Al / Ti. The flat layer 80 may be made of polyimide, acrylic or polyethylene terephthalate. The active layer 40 may be made of various materials such as amorphous indium gallium zinc oxide (a-IGZO), zinc oxynitride (ZnON), indium zinc tin oxide (IZTO), amorphous silicon (a-Si), polycrystalline silicon (p-Si), sexithiophene, polythiophene, etc., that is, the present disclosure is applicable to transistors manufactured based on oxide technology, silicon technology and organic technology.

[0123] The substrate of the embodiment of the present disclosure can be applied to a liquid crystal display product, and the substrate can be used as an array substrate of the liquid crystal display product.

[0124] The embodiment of the present disclosure further provides a display panel, comprising the substrate in any embodiment of the present disclosure. The display panel may be an organic light emitting diode display panel.

[0125] The present disclosure also provides a display device, which may include the substrate in any embodiment of the present disclosure, or the display device may include the display panel in any embodiment of the present disclosure. The display device may be a liquid crystal display device, an organic light emitting diode display device, or a quantum dot light emitting diode display device.

[0126] The display device provided in the embodiments of the present disclosure may be any product or component with display and touch functions, such as a smart phone, a wearable smart watch, smart glasses, a tablet computer, a television, a monitor, a laptop computer, a digital photo frame, a navigator, a car display, an e-book, a biometric device such as a smart skin device, a soft robot, and a biomedical device.

[0127] The substrate, display panel and other components of the display device in the above-mentioned embodiment may adopt various technical solutions known to ordinary technicians in this field now and in the future, and will not be described in detail here.

[0128] In the description of this specification, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present disclosure.

[0129] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present disclosure, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0130] In the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to specific circumstances.

[0131] In the present disclosure, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being “above”, “above”, and “above” a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0132] The disclosure above provides many different embodiments or examples to implement different structures of the present disclosure. In order to simplify the present disclosure, the components and settings of specific examples are described above. Of course, they are only examples, and the purpose is not to limit the present disclosure. In addition, the present disclosure can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed.

[0133] The above are only specific embodiments of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any technician familiar with the technical field can easily think of various changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. A substrate, characterized in that: include: substrate; A first metal layer, located at one side of the substrate, the first metal layer comprising a signal line; A first insulating layer, located on a side of the first metal layer away from the substrate; an active layer, located on a side of the first insulating layer away from the substrate; a second insulating layer, located at a side of the active layer away from the substrate, the second insulating layer being provided with a first via hole, the first via hole comprising a first sub-hole and a second sub-hole interconnected with each other, the first sub-hole penetrating the second insulating layer, a portion of the surface of the active layer being located in a region where the first sub-hole is located, the second sub-hole penetrating the second insulating layer and the first insulating layer, a portion of the surface of the signal line being located in a region where the second sub-hole is located, an overlapping portion of the active layer and the first sub-hole comprising a first sub-portion and a second sub-portion, the second sub-portion being closer to the second sub-portion relative to the first sub-portion, the first sub-portion being concave relative to the second sub-portion toward the substrate to form a first concave surface, and the first concave surface being conductively conductive with a preset thickness; The second metal layer is located on a side of the second insulating layer away from the substrate, and the second metal layer includes a first electrode, which is overlapped with the surface of the second sub-portion through the first sub-hole and connected to the signal line through the second sub-hole.

2. The substrate according to claim 1, characterized in that The second insulating layer is sandwiched between the second metal layer and the first insulating layer, the active layer includes a channel region, and the active layer also includes a fifth sub-portion located between the first pole and the channel region and outside the first via hole, and the thickness of the fifth sub-portion is greater than the thickness of the second sub-portion.

3. The substrate according to claim 2, characterized in that The size of the fifth sub-portion in the first direction is greater than or equal to 100 angstroms, the size of the fifth sub-portion in the first direction is less than or equal to the size of the channel region in the first direction, and / or, The size of the second sub-portion in the first direction is greater than or equal to 100 angstroms, and the size of the second sub-portion in the first direction is smaller than the size of the channel region in the first direction, and the first direction is a direction perpendicular to the substrate.

4. The substrate according to claim 2, characterized in that The size of the fifth sub-portion in the first direction is greater than or equal to 100 angstroms, the size of the fifth sub-portion in the first direction is less than or equal to the size of the channel region in the first direction, the size of the channel region in the first direction is 200 angstroms-1000 angstroms, and the first direction is a direction perpendicular to the substrate.

5. The substrate according to claim 1, characterized in that The second metal layer also includes a gate and a second electrode, the first electrode and the second electrode are located on both sides of the gate, the second insulating layer is also provided with a second via, the second via penetrates the second insulating layer, part of the surface of the active layer is located in the area where the second via is located, the overlapping part of the active layer and the second via includes a third sub-part and a fourth sub-part, the third sub-part is close to the gate relative to the fourth sub-part, the second electrode is overlapped and connected with the surface of the fourth sub-part through the second via, the third sub-part is recessed relative to the fourth sub-part toward the substrate to form a second recessed surface, and the second recessed surface is conductorized to a preset thickness.

6. The substrate according to claim 5, characterized in that A size of the fourth sub-portion in a first direction is greater than or equal to 100 angstroms, and the first direction is a direction perpendicular to the substrate.

7. The substrate according to claim 5, characterized in that The substrate further includes a third insulating layer, a planar layer, and an electrode layer which are sequentially arranged on a side of the second metal layer away from the substrate, and the electrode layer is connected to the second electrode.

8. The substrate according to claim 1, characterized in that The material of the active layer includes oxide semiconductor.

9. A method for preparing a substrate, characterized in that: include forming a first metal layer on one side of the substrate, wherein the first metal layer includes a signal line; forming a first insulating layer on a side of the first metal layer facing away from the substrate; forming an active layer on a side of the first insulating layer away from the substrate; A second insulating layer is deposited on a side of the active layer away from the substrate, and the second insulating layer is patterned to form a first via hole, wherein the first via hole comprises a first sub-hole and a second sub-hole that are interconnected, the first sub-hole penetrates the second insulating layer, a portion of the surface of the active layer is located in the region where the first sub-hole is located, the second sub-hole penetrates the second insulating layer and the first insulating layer, and a portion of the surface of the signal line is located in the region where the second sub-hole is located; an overlapping portion of the active layer and the first sub-hole comprises a first sub-portion and a second sub-portion, and the second sub-portion is closer to the second sub-portion than the first sub-portion; forming a second metal layer on a side of the second insulating layer away from the substrate, the second metal layer comprising a first electrode, the first electrode overlapping the surface of the second sub-portion through the first sub-hole, and the first electrode connected to the signal line through the second sub-hole; The method further comprises: The first sub-portion is etched so that the first sub-portion is recessed relative to the second sub-portion toward the substrate to form a first recessed surface, and the active layer is conductorized, wherein the first recessed surface is conductorized to a preset thickness.

10. The method for preparing a substrate according to claim 9, characterized in that: The etching of the first sub-portion comprises: The second metal layer is used as a mask and an etching process is adopted to remove the second insulating layer outside the second metal layer, and etching damage is formed on the side of the first sub-portion away from the substrate, so that the first sub-portion is recessed toward the substrate relative to the second sub-portion to form a first recessed surface.

11. The method for preparing a substrate according to claim 10, characterized in that: The second metal layer also includes a gate and a second electrode, and the method also includes The second insulating layer is patterned to form a second via hole, the second via hole penetrates the second insulating layer, a portion of the surface of the active layer is located in the area where the second via hole is located, the overlapping portion of the active layer and the second via hole includes a third sub-portion and a fourth sub-portion, the third sub-portion is closer to the gate than the fourth sub-portion, and the second electrode is overlapped and connected with the surface of the fourth sub-portion through the second via hole; In the process of removing the second insulating layer outside the second metal layer by etching, etching damage is formed on the side of the fourth sub-portion away from the substrate, so that the fourth sub-portion is recessed toward the substrate relative to the third sub-portion to form a second recessed surface.

12. A display panel, characterized in that: A substrate comprising the substrate according to any one of claims 1 to 8.

13. A display device, characterized in that: The invention comprises the substrate according to any one of claims 1 to 8 or the display panel according to claim 12.