Au deposition chiral bismuth oxybromide photocatalytic material as well as preparation method and application thereof

By depositing gold nanoparticles on the surface of bismuth oxybromide and combining them with chiral materials, the problem of photogenerated carrier separation rate of bismuth oxybromide photocatalyst was solved, and a more efficient Rhodamine B degradation effect was achieved.

CN119034817APending Publication Date: 2024-11-29KUNMING UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411340868.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-25
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

Existing bismuth oxybromine photocatalysts have poor photogenerated carrier separation efficiency and slow electron mobility, which limits their application in real life.

Method used

By combining gold nanoparticles with chiral two-dimensional materials, Au-deposited chiral bismuth oxybromine photocatalysts are formed. The photocatalytic degradation efficiency is improved through local surface plasmon resonance effect and chiral-induced electron spin selection effect.

Benefits of technology

The photocatalyst's photoresponse characteristics were enhanced, the degradation efficiency of Rhodamine B was improved, more active sites were provided, and the photocatalytic stability and selectivity of the material were enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119034817A_ABST
    Figure CN119034817A_ABST
Patent Text Reader

Abstract

The invention discloses an Au deposition chiral bismuth oxybromide photocatalytic material as well as a preparation method and application thereof, the Au deposition chiral bismuth oxybromide photocatalytic material is characterized in that the photocatalytic material comprises yY-BiOBr powder and Au nanoparticles loaded on the surface, and the chemical general formula of the photocatalytic material is yY-BiOBr / Aux, wherein x ranges from 0.3 wt% to 0.7 wt%, and y ranges from 2.3 mmol to 4.2 mmol; y is D-sorbitol or D-mannitol; the photocatalytic material is prepared by combining Au nanoparticles and a chiral two-dimensional material, wherein chiral bismuth oxybromide powder is prepared by a hydrothermal method, and then Au is loaded to the chiral bismuth oxybromide powder by an impregnation-reduction method; the photocatalytic material can effectively improve the degradation capability on an organic dye rhodamine B.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The invention relates to the technical field of chiral materials, and in particular to an Au-deposited chiral bismuth oxybromide photocatalytic material and a preparation method and application thereof. Background Art

[0001] Rhodamine B (RhB) is a synthetic water-soluble organic dye with stable physical and chemical properties. It can exist in the natural environment for a long time and is difficult to self-degrade, which not only causes great damage to the environment. At the same time, RhB is highly irritating to the eyes, skin, respiratory tract, etc., and is accompanied by reproductive and developmental, neurological and chronic toxicity to humans and animals. Therefore, photocatalytic technology can be used to utilize ultraviolet light energy to promote the degradation of RhB, which has the advantages of high efficiency and low cost.

[0002] Photocatalytic technology mainly uses sunlight to irradiate and excite photocatalysts, which can catalyze the redox reaction, and the photocatalyst is not lost during the catalytic reaction. Due to its wide band gap, bismuth oxybromide can respond to sunlight and has a high sunlight utilization rate, which can effectively separate photogenerated electrons and holes. However, bismuth oxybromide has problems such as poor photogenerated carrier separation rate and slow electron mobility, which limits its application in real life. The local surface plasmon resonance effect produced by gold nanoparticles can efficiently collect visible light and near-infrared photons and be activated, thereby forming a Schottky barrier on the surface of bismuth oxyhalide, which can quickly inject hot electrons into the conduction band of the semiconductor. At the same time, the addition of chiral molecules gives it a chiral-induced electron spin selection effect, which can effectively inhibit the recombination of photogenerated carriers, and has a stronger chiral light modulation efficiency and a higher CD value (circular dichroism) than natural materials, which will effectively carry out photocatalytic degradation. The plasmon resonance effect produced by gold nanoparticles can be combined with electron spins to form plasma-enhanced electron spin polarization, accelerate the separation of carrier electrons, and inhibit the recombination rate of electron-hole pairs, which will effectively enhance the photocatalytic degradation ability of the material. At the same time, Au nanoparticles provide more active sites, form Schottky barriers with the surface of chiral bismuth oxyhalide, and inject hot electrons into the conduction band of the semiconductor, making the degradation more rapid. Therefore, in order to solve the above problems, this paper proposes an Au-deposited chiral bismuth oxybromide photocatalytic material and its preparation method and application. Summary of the invention The purpose of the present invention is to provide an Au-deposited chiral bismuth oxybromide photocatalytic material, which combines gold nanoparticles with chiral two-dimensional materials and effectively improves the photocatalytic degradation of the organic dye Rhodamine B by the material. In order to achieve the above technical effects, the present invention is implemented through the following technical scheme: an Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that it includes yY-BiOBr powder and surface-loaded Au nanoparticles, and its general chemical formula is yY-BiOBr / Aux; wherein x is 0.3wt%~0.7wt%, y is 2.3mmol~4.2mmol; and Y is D-sorbitol or D-mannitol. Furthermore, the Au-deposited chiral bismuth oxybromide photocatalytic material is a two-dimensional powder material with a particle size of 700nm to 970nm. Furthermore, the particle size of the Au nanoparticles is 3nm to 12nm. Another object of the present invention is to provide a method for preparing Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that it consists of the following steps: S1. Weigh bismuth nitrate: halide: Y in a molar ratio of bismuth nitrate: halide: Y = 1:1:3.5; wherein Y is D-sorbitol or D-mannitol; S2, adding the weighed bismuth nitrate, halide and D-sorbitol or D-mannitol to the solvent, and then transferring to a polytetrafluoroethylene-lined hydrothermal autoclave with a filling degree of 0.4 to 0.8, and performing a solvent thermal reaction at 150 to 170° C. for 12 hours. After the reaction is completed, the reaction product is washed and dried at 65 to 75° C. for 10 hours to obtain chiral bismuth oxybromide powder; S3. Take chiral bismuth oxybromide powder and chloroauric acid trihydrate in a mass ratio of 2:0.001, add the chiral bismuth oxybromide powder and chloroauric acid trihydrate into an aqueous solution, then add a reducing agent, heat at 40-80°C for 0.5-1.5h, and stir during the heating process, wait for it to cool to room temperature, filter the product, wash it, and dry it at 65-75°C for 10h to obtain Au-deposited chiral bismuth oxybromide photocatalytic material. Furthermore, the halide salt is one of sodium bromide or potassium bromide; Furthermore, the solvent is ethylene glycol. Furthermore, the solvent is an aqueous solution of ethylene glycol. Furthermore, the reducing agent is sodium citrate or citric acid. Another object of the present invention is to provide an application of an Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that the Au-deposited chiral bismuth oxybromide photocatalytic material is used in the degradation of rhodamine B. The beneficial effects of the present invention are: (1) The Au-deposited chiral bismuth oxybromide photocatalytic material of the present invention has good light response characteristics, can directly generate circularly polarized light, can produce a higher CD value, has high utilization rate of light in different bands, and has better photocatalytic degradation effect of rhodamine B; (2) The Au-deposited chiral bismuth oxybromide photocatalytic material of the present invention can be prepared by using different Au loading amounts and different chiral materials in combination. The preparation method is easy to operate, the operating conditions are easy to control, and it is easy to prepare two-dimensional materials with various morphologies. (3) The Au-deposited chiral bismuth oxybromide photocatalytic material of the present invention is a two-dimensional inorganic non-metallic semiconductor and information functional material, which is expected to be used as a novel nanomaterial for scientific research in the fields of photocatalytic degradation and direct generation of circularly polarized light, thereby expanding the scope of exploration in the scientific research field of chiral materials. BRIEF DESCRIPTION OF THE DRAWINGS In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work. Figure 1 The XRD spectrum of the 3.5D-BiOBr / Au 0.5% photocatalytic material prepared in Example 1 of the present invention; Figure 2 This is the SEM spectrum of the 3.5D-BiOBr / Au 0.5% photocatalytic material prepared in Example 1 of the present invention; Figure 3 This is the TEM spectrum of the 3.5D-BiOBr / Au 0.5% photocatalytic material prepared in Example 1 of the present invention; Figure 4 is the chiral CD value spectrum of the 3.5D-BiOBr material of the present invention; Figure 5 This is the chiral CD value spectrum of the 3.5D-BiOBr / Au 0.5% photocatalytic material of the present invention; Figure 6 Additional image diagram of the structure of the chiral material of the present invention; Figure 7 The degradation spectrum of rhodamine in the 3.5D-BiOBr material and the 3.5D-BiOBr / Au0.5% photocatalytic material under xenon lamp irradiation of the present invention is compared; Figure 8 The linear fitting spectrum of rhodamine degradation is compared between the 3.5D-BiOBr material of the present invention and the 3.5D-BiOBr / Au 0.5% photocatalytic material; Fig. 9This is a rhodamine degradation cycle diagram of the 3.5D-BiOBr / Au 0.5% photocatalytic material of the present invention; Fig.10 The XRD spectrum of the 3.5L-BiOBr / Au 0.5% photocatalytic material prepared in Example 2 of the present invention; Fig.11 This is the chiral CD value spectrum of the 3.5L-BiOBr / Au 0.5% photocatalytic material of the present invention; Fig.12 The degradation spectra of rhodamine in 3.5L-BiOBr material and 3.5L-BiOBr / Au0.5% material of the present invention are compared under xenon lamp irradiation; Fig.13 The linear fitting spectrum of rhodamine degradation is compared between the 3.5L-BiOBr material of the present invention and the 3.5L-BiOBr / Au 0.5% material. DETAILED DESCRIPTION The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example 1 A method for preparing Au-deposited right-handed chiral bismuth oxybromide photocatalytic material comprises the following steps: (1) Hydrothermal method: Bi(NO 3)3.5H 2O, D-sorbitol (D-SOr) and NaBr were used as raw materials, and the molar ratio of Bi ion: D-SOr: Br ion was 1:3.5:1. All raw materials were dissolved in an aqueous solution of ethylene glycol, and the above solution was added to a container and stirred to mix evenly. Then, it was transferred to a hydrothermal autoclave with a polytetrafluoroethylene liner and the filling degree was 0.8. Then, the temperature was raised to 160°C and kept warm for 12 hours. (2) washing the material obtained in step (1) with deionized water and ethanol three times respectively, drying at 70° C. and keeping the temperature for 10 hours to obtain 3.5D-BiOBr; (3) Impregnation-reduction method: Weigh 0.35 g of 3.5D-BiOBr in a water container, add 50 mL of water, 0.5 wt% chloroauric acid and 10 mg / mL of sodium citrate, heat and stir at 60 ° C for 30 min, and cool to room temperature after 1 hour. Then filter, wash with deionized water and ethanol three times respectively, dry at 70 ° C, keep warm for 10 hours, and finally obtain Au-deposited chiral bismuth oxybromide photocatalytic material. Performance Test 1 Weigh 20 mg of 3.5D-BiOBr / Au 0.5%, 3.5D-BiOBr as a photocatalyst and 50 mL of 20 mg / L Rhodamine B solution, add them to the photocatalytic tube, mix them evenly, and stir them magnetically in a dark environment for 40 minutes to allow Rhodamine B to reach adsorption-desorption equilibrium on the surface of the photocatalyst. Then carry out the photoreaction, take samples every 10 minutes, take samples for a total of 60 minutes, take 4 mL each time, centrifuge them in a centrifuge at a speed of 7000 rpm for 4 minutes, and take the supernatant for absorbance test. In order to test the stability of the photocatalytic material, the 3.5D-BiOBr / Au 0.5% photocatalytic material was subjected to 4 cycles of degradation of Rhodamine B solution. Fig. 9 shown. The prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested by X-ray diffraction, and the XRD spectrum was obtained as follows: Figure 1 As shown, from the XRD results, it can be seen that 3.5D-BiOBr / Au 0.5% doped with 3.5mmol D-sorbitol and deposited with 0.5wt% Au has obvious and sharp diffraction peaks, and the peak position is highly consistent with the layered structure of BiOBr of JCPDS card number. The prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested under a SEM scanning electron microscope. The material showed a sparse and loose right-handed flower ball morphology structure under the SEM scanning electron microscope. A large amount of Au was deposited on the sheet in the form of spherical particles. The SEM morphology is as follows: Figure 2 shown. The prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested under a TEM scanning electron microscope. The material showed a large number of Au nanoparticles deposited around the nanosheets under a TEM scanning electron microscope. The TEM morphology is as follows: Figure 3 shown. When the prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested using a circular dichroism instrument, it was found that the chiral CD value was positive and the peak value was significantly enhanced, proving that Au deposition significantly enhanced the properties and functions of chirality, such as Figure 5 . 3.5 The chiral CD value spectrum of D-BiOBr materials, such as Figure 4 shown. Figure 6 Additional graphic representation of the structure of right-handed chiral materials. After dark adsorption and light irradiation reaction of the photocatalyst, it was found that 3.5D-BiOBr / Au 0.5% degraded faster than 3.5D-BiOBr, with a degradation rate of 88.8%, indicating that the presence of Au nanoparticles provides more active sites, forming a Schottky barrier with the surface of chiral bismuth oxyhalide, and injecting hot electrons into the conduction band of the semiconductor, making the degradation more rapid, such as Figure 7At the same time, the slope of 3.5D-BiOBr / Au 0.5% is larger than that of 3.5D-BiOBr, which also proves that the degradation rate of 3.5D-BiOBr / Au0.5% is faster, proving that electron spin polarization is generated under the action of chiral induced spin selectivity, and a large number of spin electrons are quickly transferred and injected into Au nanoparticles, causing strong plasma resonance in Au nanoparticles, increasing the separation rate of electron-hole pairs, and thus promoting the degradation of RHB by photocatalytic materials. Figure 8 shown. After 4 cycles of degradation, the degradation rates of 3.5D-BiOBr / Au 0.5% photocatalyst for Rhodamine B were 88.8%, 86.0%, 83.0%, and 76.3%, respectively. Although the degradation rate of Rhodamine B decreased to a certain extent, the 3.5D-BiOBr / Au 0.5% photocatalyst still had good photocatalytic stability. Example 2 A method for preparing Au-deposited left-handed chiral bismuth oxybromide photocatalytic material comprises the following steps: (1) Hydrothermal method: Bi(NO 3)3.5H 2O, D-mannitol (L-Man) and NaBr were used as raw materials, and the molar ratio of Bi ion: L-Man: Br ion was 1:3.5:1. All raw materials were dissolved in an aqueous solution of ethylene glycol, and the above solution was added to a container and stirred to mix evenly. Then, it was transferred to a hydrothermal autoclave with a polytetrafluoroethylene liner and the filling degree was 0.8. Then, the temperature was raised to 160°C and kept warm for 12 hours. (2) washing the material obtained in step (1) with deionized water and ethanol three times respectively, drying at 70° C. and keeping the temperature for 10 hours to obtain 3.5L-BiOBr; (3) Impregnation-reduction method: Weigh 0.35 g of 3.5L-BiOBr in a container, add 50 mL of water, 0.5 wt% chloroauric acid and 10 mg / mL of sodium citrate, heat and stir at 60 ° C for 30 min, and cool to room temperature after 1 hour. Then filter, wash with deionized water and ethanol three times respectively, dry at 70 ° C, keep warm for 10 hours, and finally obtain Au-deposited chiral bismuth oxybromide photocatalytic material. Performance Test 2 Weigh 20 mg of 3.5L-BiOBr / Au 0.5%, 3.5L-BiOBr as a photocatalyst and 50 mL of 20 mg / L Rhodamine B solution, add them to the photocatalytic tube, mix them evenly, and stir them magnetically in a dark environment for 40 minutes to allow Rhodamine B to reach adsorption-desorption equilibrium on the surface of the photocatalyst. Then carry out the photoreaction, take samples every 10 minutes, take samples for a total of 60 minutes, take 4 mL each time, centrifuge them on a centrifuge at a speed of 7000 rpm for 4 minutes, and take the supernatant for absorbance test. The prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested by X-ray diffraction, and the XRD spectrum was obtained as follows: Fig.10 As shown, from the XRD results, it can be seen that 3.5L-BiOBr / Au 0.5% doped with 3.5mmol L-mannitol and deposited with 0.5wt% Au has obvious and sharp diffraction peaks, and the peak position is highly consistent with the layered structure of BiOBr of JCPDS card number. When the prepared Au-deposited chiral bismuth oxybromide photocatalytic material was tested using a circular dichroism instrument, it was found that the chiral CD value was positive and the peak was obvious, proving that it has the properties and functions of chirality, such as Fig.11 . After dark adsorption and light irradiation reaction of the photocatalyst, it was found that 3.5L-BiOBr / Au 0.5% degraded faster than 3.5L-BiOBr, with a degradation rate of 73.6%, indicating that the presence of Au nanoparticles provides more active sites, forming a Schottky barrier with the surface of chiral bismuth oxyhalide, and injecting hot electrons into the conduction band of the semiconductor, making the degradation more rapid, such as Fig.12 At the same time, the degradation rate of 3.5L-BiOBr / Au 0.5% is 17.57min-1, which is higher than the degradation rate of 3.5L-BiOBr without gold (k=14.05min-1), proving that electron spin polarization is generated under the action of chiral induced spin selectivity, and a large number of spin electrons are rapidly transferred and injected into Au nanoparticles, resulting in strong plasma resonance in Au nanoparticles, increasing the separation rate of electron-hole pairs, and thus promoting the degradation of RHB by photocatalytic materials; Fig.13 shown. The above implementation examples have been described in detail the different implementation processes of the present invention, but the implementation methods of the present invention are not limited thereto. Ordinary technicians in the relevant technical field can achieve the purpose of the present invention based on the contents disclosed in the present invention. Any improvements and modifications based on the concept of the present invention fall within the protection scope of the present invention, and the specific protection scope shall be subject to the claims.

Claims

1. An Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that: The invention comprises yY-BiOBr powder and Au nanoparticles loaded on the surface, and has a general chemical formula of yY-BiOBr / Aux; wherein x is 0.3wt%-0.7wt%, y is 2.3mmol-4.2mmol; and Y is D-sorbitol or D-mannitol.

2. The Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 1, characterized in that: The Au-deposited chiral bismuth oxybromide photocatalytic material is a two-dimensional powder material with a particle size of 700nm to 970nm.

3. The Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 1, characterized in that: The particle size of the Au nanoparticles is 3nm-12nm.

4. A method for preparing Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that: It consists of the following steps: S1. Weigh bismuth nitrate: halide: Y in a molar ratio of bismuth nitrate: halide: Y = 1:1:3.5; wherein Y is D-sorbitol or D-mannitol; S2, adding the weighed bismuth nitrate, halide and D-sorbitol or D-mannitol to the solvent, and then transferring to a polytetrafluoroethylene-lined hydrothermal autoclave with a filling degree of 0.4 to 0.8, and performing a solvent thermal reaction at 150 to 170° C. for 12 hours. After the reaction is completed, the reaction product is washed and dried at 65 to 75° C. for 10 hours to obtain chiral bismuth oxybromide powder; S3. Take chiral bismuth oxybromide powder and chloroauric acid trihydrate in a mass ratio of 2:0.001, add the chiral bismuth oxybromide powder and chloroauric acid trihydrate into an aqueous solution, then add a reducing agent, heat at 40-80°C for 0.5-1.5h, and stir during the heating process, wait for it to cool to room temperature, filter the product, wash it, and dry it at 65-75°C for 10h to obtain Au-deposited chiral bismuth oxybromide photocatalytic material.

5. The method for preparing an Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 4, characterized in that: The halide salt is one of sodium bromide or potassium bromide.

6. The method for preparing Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 4, characterized in that: The solvent is ethylene glycol.

7. The method for preparing Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 4, characterized in that: The solvent is an aqueous solution of ethylene glycol.

8. The method for preparing Au-deposited chiral bismuth oxybromide photocatalytic material according to claim 4, characterized in that: The reducing agent is sodium citrate or citric acid.

9. An application of Au-deposited chiral bismuth oxybromide photocatalytic material, characterized in that: The Au-deposited chiral bismuth oxybromide photocatalytic material is used in the degradation of rhodamine B.