Wafer thinning processing control method, control system and processing equipment
By calculating the real-time downward shift threshold and displacement correction coefficient of the grinding wheel spindle, the wafer thinning processing is controlled, and the over-grinding problem caused by the failure of the thickness detection device is solved, the processing accuracy and safety are improved, and the scrap rate is reduced.
Patent Information
- Application Number
- CN202411372149.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-09-29
AI Technical Summary
A failure of the thickness detection device of the wafer thinning machine may cause the spindle to move down erroneously, resulting in the wafer being overgrinded and scrapped. It is difficult for the prior art to effectively avoid such failures.
By calculating the real-time downward shift threshold of the grinding wheel spindle, the initial thickness, real-time thickness, downward shift amount at the last processing and thickness change value are used, combined with the displacement correction coefficient, the downward shift amount of the grinding wheel spindle is controlled to prevent overgrinding, and a Alarm signal.
It effectively avoids wafer overgrinding caused by failure of the thickness detection device, improves the accuracy of wafer thinning and the accuracy of displacement correction, and reduces the processing waste rate.
Smart Images

Figure CN119057573A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of wafer thinning processing, and in particular to a wafer thinning processing control method, control system and processing equipment. Background Art
[0002] During the operation of the wafer thinning machine, the spindle with the grinding wheel rotates at a certain speed and gradually descends. The grinding wheel on the spindle contacts the wafer to remove the silicon on the upper layer of the wafer. The spindle is lifted until the built-in wafer thickness measuring device detects that the wafer thickness reaches the set value, and the grinding wheel loses contact with the wafer, and thinning stops.
[0003] The above processing control method determines whether the wafer processing is completed by real-time detection of the wafer thickness, so as to control whether the spindle stops descending. In this process, if the thickness detection device fails (especially the contact thickness detection device in the machine, which has a higher probability of failure), the wafer thickness detection value remains unchanged. If the reported wafer thickness detection value does not reach the target value (i.e., the wafer thickness value used to indicate that the spindle will not move down after the processing is completed), the spindle will continue to move down, which may cause the wafer to be over-grinded due to the incorrect downward movement of the spindle. Since the wafer processing accuracy is high, a small amount of over-grinding will also cause the wafer to be scrapped. Therefore, how to avoid the wafer being scrapped due to a failure of the thickness detection device is an urgent problem to be solved. Summary of the invention
[0004] An object of the first aspect of the present invention is to provide a wafer thinning processing control method, which can avoid the situation where the wafer is over-grinded and scrapped due to a malfunction of a thickness detection device.
[0005] Another object of the present invention is to improve the accuracy of wafer thinning.
[0006] A further object of the present invention is to make the displacement correction coefficient more accurate.
[0007] An object of the second aspect of the present invention is to provide a wafer thinning process control system for executing the above-mentioned wafer thinning process control method.
[0008] An object of the third aspect of the present invention is to provide a processing device including the above-mentioned wafer thinning processing control system.
[0009] An embodiment of the present invention provides a wafer thinning process control method, comprising:
[0010] Obtain the initial thickness and real-time thickness of the wafer being processed;
[0011] Get the downward movement of the grinding wheel spindle when the last processing was completed;
[0012] Calculate the change in the downward displacement of the grinding wheel spindle and the thickness change of the wafer after each processing is completed;
[0013] Calculating a real-time downward movement threshold of the grinding wheel spindle according to the initial thickness, the real-time thickness, the downward movement amount of the grinding wheel spindle when the last processing was completed, each downward movement amount change value and each thickness change value;
[0014] When the real-time downward movement amount of the grinding wheel spindle is greater than or equal to the real-time downward movement threshold, the grinding wheel spindle is controlled to stop.
[0015] Furthermore, the real-time downward shift threshold is calculated according to the following formula:
[0016]
[0017] Where n is the number of processing times, A n is the real-time downward moving threshold during the nth processing, h n-1 is the downward displacement of the grinding wheel spindle when the n-1th processing is completed, h i-1 h is the downward displacement of the grinding wheel spindle when the i-1th processing is completed, i-2 is the downward displacement of the grinding wheel spindle when the i-2th processing is completed, T(i-1) is the thickness of the wafer when the i-1th processing is completed, T0(i-1) is the initial thickness of the wafer before the i-1th processing, h0 is the downward displacement of the grinding wheel spindle when the grinding wheel spindle contacts the wafer during the first processing, T 0n is the initial thickness of the wafer before the nth processing, t n It is the real-time thickness of the wafer during the nth processing.
[0018] Furthermore, when calculating the real-time downward threshold, the displacement correction coefficient is used to correct the formula The displacement correction coefficient is determined according to the wear prediction error of the grinding wheel spindle and the rate of change of the descending displacement difference of the grinding wheel spindle during each processing.
[0019] Furthermore, the displacement correction coefficient is determined according to the following formula:
[0020]
[0021] Among them, α n As The multiplication factor of the term, β1 and β2 are weight coefficients, B′ n-1 is the predicted wear amount of the grinding wheel spindle during the n-1th processing, C n-1 It is the machining displacement change rate of the grinding wheel spindle during the n-1th machining, and the machining displacement is the downward movement of the grinding wheel spindle from the time when the grinding wheel spindle contacts the wafer to the completion of the machining in a single machining.
[0022] Furthermore, the sum of β1 and β2 is 1 and β1 is smaller than β2.
[0023] Furthermore, when the real-time downward movement amount of the grinding wheel spindle is less than the real-time downward movement threshold, the grinding wheel spindle is controlled to descend until the wafer reaches the target thickness.
[0024] Furthermore, when the real-time downward movement amount of the grinding wheel spindle is greater than or equal to the real-time downward movement threshold, an alarm signal is generated and sent to the alarm unit.
[0025] An embodiment of the present invention further provides a wafer thinning processing control system, comprising a memory and a processor, wherein a control program is stored in the memory, and when the control program is executed by the processor, it is used to implement any of the wafer thinning processing control methods described above.
[0026] An embodiment of the present invention further provides a wafer thinning processing device, comprising:
[0027] Wafer thickness detection unit, used to detect the thickness of the wafer;
[0028] A displacement detection unit, used to detect the downward displacement of the grinding wheel spindle; and
[0029] The wafer thinning process control system mentioned above is connected to both the wafer thickness detection unit and the displacement detection unit.
[0030] Furthermore, the wafer thinning processing equipment also includes an alarm unit, which is connected to the wafer thinning processing control system and generates an alarm when an alarm signal is received.
[0031] According to the first aspect of the present invention, the real-time downward displacement threshold of the grinding wheel spindle can be calculated based on the initial thickness and real-time thickness of the wafer being processed this time, the downward displacement of the grinding wheel spindle when the last processing was completed, each downward displacement change value, and each thickness change value, and then the real-time downward displacement threshold is used to compare with the real-time downward displacement of the grinding wheel spindle. Once the real-time downward displacement exceeds the real-time downward displacement threshold, the grinding wheel spindle is immediately controlled to stop. Therefore, in a single processing process, the real-time downward displacement of the grinding wheel spindle always has a threshold for carding, which can ensure that the grinding wheel spindle will not be over-grinded even if a wafer thickness detection failure occurs during the processing, thereby reducing the wafer processing scrap rate.
[0032] According to the second aspect of the invention, the application takes into account the predicted wear change rate and actual displacement change rate of the grinding wheel spindle when calculating the real-time downward movement threshold, wherein the actual displacement change rate can directly reflect the wear change rate of the grinding wheel, and these two factors form a displacement correction coefficient, and the reference value of the current processing grinding wheel wear in the real-time downward movement threshold calculation formula is corrected to make the reference value more accurate and able to reflect the wear change law and the processing displacement change law, thereby making the downward movement control of the grinding wheel spindle more accurate, which is beneficial to improving the accuracy of wafer thinning.
[0033] Furthermore, setting the weight coefficient of the predicted wear change rate to be smaller than the weight coefficient of the actual displacement change rate can avoid over-reliance on the correction of a single prediction error, strengthen the actual displacement change rate that can directly reflect the wear state, and make the displacement correction coefficient more accurate. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 is a flow chart of a wafer thinning process control method according to an embodiment of the present invention;
[0035] Figure 2 The figure is a flow chart of a wafer thinning process control method according to another embodiment of the present invention. DETAILED DESCRIPTION
[0036] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.
[0037] It should be noted that when a component is referred to as being "fixed to" or "disposed on" another component, it may be directly on the other component or there may also be a central component. When a component is considered to be "connected to" another component, it may be directly connected to the other component or there may be a central component at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used in the specification of this application are for illustrative purposes only and do not represent the only implementation method.
[0038] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of this application, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0039] In the present application, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may mean that the first feature is directly in contact with the second feature, or the first feature and the second feature are in contact indirectly through an intermediate medium. Moreover, a first feature being “above”, “above”, or “above” a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being “below”, “below”, or “below” a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0040] Unless otherwise defined, all technical and scientific terms used in the specification of this application have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used in the specification of this application includes any and all combinations of one or more related listed items.
[0041] Figure 1 FIG. 1 is a flow chart of a wafer thinning process control method according to an embodiment of the present invention. Figure 1 As shown, in one embodiment, the wafer thinning process control method includes the following steps:
[0042] Step S100, obtaining the initial thickness and real-time thickness of the wafer being processed;
[0043] Step S200, obtaining the downward movement amount of the grinding wheel spindle when the last processing is completed;
[0044] Step S300, calculating the change value of the downward movement of the grinding wheel spindle and the change value of the thickness of the wafer when each processing is completed;
[0045] Step S400, calculating the real-time downward movement threshold of the grinding wheel spindle according to the initial thickness, the real-time thickness, the downward movement amount of the grinding wheel spindle when the last processing was completed, each downward movement amount change value and each thickness change value;
[0046] Step S500, when the real-time downward movement amount of the grinding wheel spindle is greater than or equal to the real-time downward movement threshold, the grinding wheel spindle is controlled to stop.
[0047] In step S100, the wafer thickness can be collected by a wafer thickness detection unit, such as a non-contact optical thickness meter, a capacitive thickness meter, an ultrasonic thickness meter, etc. In step S200, a grating ruler can be used to measure the downward displacement of the grinding wheel spindle.
[0048] The initial thickness and real-time thickness of the wafer in step S400 are quantities closely related to the downward movement control of the grinding wheel spindle. As the real-time thickness decreases, it means that the downward movement margin of the grinding wheel spindle is gradually reduced. The downward movement amount of the grinding wheel spindle when the last processing is completed can be the basis for the wear amount of the grinding wheel in this processing. Each downward movement amount change value and each thickness change value can reflect the wear law in the historical processing process. Therefore, according to the above values, the limit value when the grinding wheel spindle descends in this processing, that is, the real-time downward movement threshold, can be determined.
[0049] This application can calculate the real-time downward displacement threshold of the grinding wheel spindle according to the initial thickness and real-time thickness of the wafer being processed, the downward displacement of the grinding wheel spindle when the last processing was completed, each downward displacement change value and each thickness change value, and then use the real-time downward displacement threshold to compare with the real-time downward displacement of the grinding wheel spindle. Once the real-time downward displacement exceeds the real-time downward displacement threshold, the grinding wheel spindle is immediately controlled to stop. Therefore, in a single processing process, the real-time downward displacement of the grinding wheel spindle is always limited by a threshold, which can ensure that the grinding wheel spindle will not be over-grinded even if a wafer thickness detection failure occurs during the processing, thereby reducing the wafer processing scrap rate.
[0050] In one embodiment, the real-time downward shift threshold is calculated according to the following formula (1):
[0051]
[0052] Where n is the number of processing times, A n is the real-time downward threshold value during the nth processing, h n-1 is the downward displacement of the grinding wheel spindle when the n-1th processing is completed, h i-1 h is the downward displacement of the grinding wheel spindle when the i-1th processing is completed, i-2 is the downward displacement of the grinding wheel spindle when the i-2th processing is completed, T(i-1) is the thickness of the wafer when the i-1th processing is completed, T0(i-1) is the initial thickness of the wafer before the i-1th processing, h0 is the downward displacement of the grinding wheel spindle when the grinding wheel spindle contacts the wafer during the first processing, T 0n is the initial thickness of the wafer before the nth processing, t n It is the real-time thickness of the wafer during the nth processing.
[0053] The present application provides a specific calculation formula for the real-time downward movement threshold value. The formula takes the downward movement amount of the grinding wheel spindle when the previous processing is completed as the basis, and adds the average value of the difference in the downward movement amount of the grinding wheel spindle when two adjacent processings are completed as a reference value for the grinding wheel wear in this processing, and adds the items related to the real-time thickness of the wafer in the current processing process, so that the real-time downward movement threshold value can change with the real-time thickness change of the wafer, so that the real-time downward movement threshold value can adapt to the entire processing process in real time when the grinding wheel spindle moves downward, play the role of limiting the downward movement amount of the grinding wheel spindle, and effectively prevent the wafer from being over-grinded.
[0054] In a further embodiment, when calculating the real-time downward threshold, the displacement correction coefficient is used to correct the formula The displacement correction coefficient is determined according to the wear prediction error of the grinding wheel spindle and the rate of change of the descending displacement difference of the grinding wheel spindle during each processing. In one embodiment, the displacement correction coefficient is determined according to the following formulas (2) and (3):
[0055]
[0056] Among them, β1 and β2 are weight coefficients, B ′ n-1 is the predicted wear amount of the grinding wheel spindle during the n-1th processing. n-1 It is the rate of change of machining displacement of the grinding wheel spindle during the n-1th machining. The machining displacement is the downward movement of the grinding wheel spindle from the time when the grinding wheel spindle contacts the wafer to the time when the machining is completed during a single machining. For example, when n=6, C5=(X5-X4) / X4, X5 is the downward movement of the grinding wheel spindle from the time when the grinding wheel spindle contacts the wafer to the time when the machining is completed during the 5th machining, and X4 is the downward movement of the grinding wheel spindle from the time when the grinding wheel spindle contacts the wafer to the time when the machining is completed during the 4th machining.
[0057] In this embodiment, the displacement correction coefficient α n As The multiplication factor of the term, so the modified real-time downward threshold is determined according to the following formula (4):
[0058]
[0059] In one embodiment, the sum of β1 and β2 is 1, and β1 is smaller than β2. Optionally, β1 takes a value between 0.1-0.4, and β2 takes a value between 0.5-1, for example, β1 is 0.3 and β2 is 0.7, or β1 is 0.2 and β2 is 0.8.
[0060] The predicted wear change rate and actual displacement change rate of the grinding wheel spindle are taken into account when calculating the real-time downward threshold. The actual displacement change rate can directly reflect the wear change rate of the grinding wheel. These two factors form a displacement correction coefficient, and the reference value of the grinding wheel wear in this processing in the real-time downward threshold calculation formula is corrected to make the reference value more accurate and able to reflect the wear change law and the processing displacement change law, thereby making the downward control of the grinding wheel spindle more accurate, which is beneficial to improving the accuracy of wafer thinning.
[0061] Furthermore, setting the weight coefficient of the predicted wear change rate to be smaller than the weight coefficient of the actual displacement change rate can avoid over-reliance on the correction of a single prediction error, strengthen the actual displacement change rate that can directly reflect the wear state, and make the displacement correction coefficient more accurate.
[0062] Figure 2 FIG. 1 is a flow chart of a wafer thinning process control method according to another embodiment of the present invention. Figure 2 As shown, in another embodiment,
[0063] Step S300 includes:
[0064] Step S310, obtaining the downward movement amount of the abrasive spindle when each processing is completed in the historical processing process;
[0065] Step S320, obtaining the initial thickness of the wafer at the beginning of each processing and the processing thickness of the wafer when the processing is completed in the historical processing process;
[0066] Step S330, calculating the downward displacement change value according to the downward displacement of the abrasive spindle when each processing is completed in the historical processing process, and calculating the thickness change value of the wafer according to the initial thickness of the wafer at the beginning of each processing in the historical processing process and the processing thickness of the wafer when the processing is completed;
[0067] After step S400, the method further includes:
[0068] Step S450, determining whether the real-time downward movement amount of the grinding wheel spindle is less than the real-time downward movement threshold, if so, proceeding to step S600, otherwise proceeding to step S520;
[0069] Step S600, controlling the grinding wheel spindle to descend until the wafer reaches a target thickness.
[0070] Step S520, controlling the grinding wheel spindle to stop, generating an alarm signal, and sending the alarm signal to the alarm unit so that the alarm unit can sound an alarm.
[0071] The present application also provides a wafer thinning processing control system, including a memory and a processor, wherein a control program is stored in the memory, and when the control program is executed by the processor, it is used to implement the wafer thinning processing control method in any of the above-mentioned embodiments.
[0072] The processor may be a central processing unit (CPU). The processor may also be other general control modules, digital signal processors (DSP), application specific integrated circuits (ASIC), field programmable gate arrays (FPGA) or other programmable logic devices, discrete gate or transistor logic devices, discrete hardware components, or a combination of the above chips.
[0073] The memory, as a non-transitory computer-readable storage medium, can be used to store non-transitory software programs, non-transitory computer executable programs and modules, such as the movement trajectory adjustment method in the embodiment of the present invention. The control module executes various functional applications and data processing of the control module, namely, the movement trajectory adjustment method, by running the non-transitory software programs, instructions and modules stored in the memory.
[0074] The memory may include a program storage area and a data storage area, wherein the program storage area may store an operating system, an application required by at least one function; the data storage area may store data created by the control module, etc. In addition, the memory may include a high-speed random access memory, and may also include a non-transitory memory, such as at least one disk storage device, a flash memory device, or other non-transitory solid-state storage device. In some embodiments, the memory may optionally include a memory remotely arranged relative to the control module, and these remote memories may be connected to the control module via a network. Examples of the above-mentioned network include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof.
[0075] Those skilled in the art can understand that all or part of the processes in the above-mentioned embodiments can be implemented by instructing the relevant hardware through a computer program, and the program can be stored in a computer-readable storage medium. When the program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, the storage medium can be a disk, an optical disk, a read-only memory (ROM), a random access memory (RAM), a flash memory, a hard disk drive (HDD) or a solid-state drive (SSD), etc.; the storage medium can also include a combination of the above-mentioned types of memory.
[0076] The present application also provides a wafer thinning processing equipment, including a wafer thickness detection unit, a displacement detection unit, a warning unit and the above-mentioned wafer thinning processing control system. The wafer thickness detection unit is used to detect the thickness of the wafer. The displacement detection unit is used to detect the downward movement of the grinding wheel spindle. The wafer thinning processing control system is connected to both the wafer thickness detection unit and the displacement detection unit. The warning unit is connected to the wafer thinning processing control system and alarms when receiving an alarm signal. The warning unit can be a commonly used warning device such as a display screen, a speaker, a warning light, etc., which is used to prompt the processing personnel that a processing failure has occurred.
[0077] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A wafer thinning process control method, characterized in that: include: Obtain the initial thickness and real-time thickness of the wafer being processed; Get the downward movement of the grinding wheel spindle when the last processing was completed; Calculate the change in the downward displacement of the grinding wheel spindle and the thickness change of the wafer after each processing is completed; Calculating a real-time downward movement threshold of the grinding wheel spindle according to the initial thickness, the real-time thickness, the downward movement amount of the grinding wheel spindle when the last processing was completed, each downward movement amount change value and each thickness change value; When the real-time downward movement amount of the grinding wheel spindle is greater than or equal to the real-time downward movement threshold, the grinding wheel spindle is controlled to stop.
2. The wafer thinning process control method according to claim 1, characterized in that: The real-time downward shift threshold is calculated according to the following formula: Where n is the number of processing times, A n is the real-time downward moving threshold during the nth processing, h n-1 is the downward displacement of the grinding wheel spindle when the n-1th processing is completed, h i-1 h is the downward displacement of the grinding wheel spindle when the i-1th processing is completed, i-2 is the downward displacement of the grinding wheel spindle when the i-2th processing is completed, T(i-1) is the thickness of the wafer when the i-1th processing is completed, T0(i-1) is the initial thickness of the wafer before the i-1th processing, h0 is the downward displacement of the grinding wheel spindle when the grinding wheel spindle contacts the wafer during the first processing, T 0n is the initial thickness of the wafer before the nth processing, t n It is the real-time thickness of the wafer during the nth processing.
3. The wafer thinning process control method according to claim 2, characterized in that: When calculating the real-time downward threshold, the displacement correction coefficient is used to correct the formula The displacement correction coefficient is determined according to the wear prediction error of the grinding wheel spindle and the rate of change of the descending displacement difference of the grinding wheel spindle during each processing.
4. The wafer thinning process control method according to claim 3, characterized in that: The displacement correction coefficient is determined according to the following formula: Among them, α n As The multiplication factor of the term, β1 and β2 are weight coefficients, B′ n-1 is the predicted wear amount of the grinding wheel spindle during the n-1th processing, C n-1 It is the machining displacement change rate of the grinding wheel spindle during the n-1th machining, and the machining displacement is the downward movement of the grinding wheel spindle from the time when the grinding wheel spindle contacts the wafer to the completion of the machining in a single machining.
5. The wafer thinning process control method according to claim 4, characterized in that: The sum of β1 and β2 is 1 and β1 is less than β2.
6. The wafer thinning process control method according to any one of claims 1 to 5, characterized in that: When the real-time downward movement amount of the grinding wheel spindle is less than the real-time downward movement threshold, the grinding wheel spindle is controlled to descend until the wafer reaches the target thickness.
7. The wafer thinning process control method according to any one of claims 1 to 5, characterized in that: When the real-time downward movement amount of the grinding wheel spindle is greater than or equal to the real-time downward movement threshold, an alarm signal is also generated and sent to the alarm unit.
8. A wafer thinning process control system, characterized in that: It comprises a memory and a processor, wherein a control program is stored in the memory, and when the control program is executed by the processor, it is used to implement the wafer thinning processing control method according to any one of claims 1 to 7.
9. A wafer thinning processing equipment, characterized in that: include: Wafer thickness detection unit, used to detect the thickness of the wafer; A displacement detection unit is used to detect the downward displacement of the grinding wheel spindle; as well as The wafer thinning process control system of claim 8, wherein the wafer thinning process control system is connected to both the wafer thickness detection unit and the displacement detection unit.
10. The wafer thinning processing equipment according to claim 9, characterized in that: It also includes an alarm unit, which is connected to the wafer thinning process control system and generates an alarm when an alarm signal is received.
Citation Information
Patent Citations
Polishing apparatus
CN102398210A
Wafer grinding monitoring method and monitoring system
CN114871876A
Thinning method and system and thinning machine
CN117182688A
Wafer thinning method, wafer thinning stage thickness measuring method, wafer thinning stage thickness measuring system and wafer thinning equipment
CN117340778A
Thinning control method and system and thinning equipment
CN117415730A