B1-grade high-flame-retardant cable material extrusion mechanism
By designing a screw barrel and segmented screw structure with multi-annular grooves and oblique grooves in the B1 high flame retardant cable extrusion mechanism, the problems of poor plasticization of the masterbatch and high plasticization temperature are solved, and more stable processing is achieved and high-quality products.
Patent Information
- Application Number
- CN202410602579.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-15
- Publication Date
- 2024-12-03
AI Technical Summary
The poor plasticization properties and high plasticization temperature of the B1 grade high flame retardant cable masterbatch pellets lead to excessive temperatures that are prone to excessive temperature blockage during the extrusion process, affecting processing stability and efficiency.
An extrusion mechanism including a screw barrel and a screw rod is designed. A plurality of annular grooves and oblique grooves are provided in the screw barrel to improve the cooling effect. The screw rod is divided into a cutting section, a melting section, a plasticizing section and a homogenizing section. A secondary thread is added to the plasticizing section, and the depth and volume of the screw groove are distributed in equal parts to increase the diameter of the rod to improve strength and thermal balance.
It improves the plasticization effect and processing stability of the material, extends the mixing time of the material in the screw groove, enhances the thermal balance, and ensures product quality and processing efficiency.
Smart Images

Figure CN119058059A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of extruders, in particular to a B1-level highly flame-retardant cable material extrusion mechanism. Background Art
[0002] An extruder is a device used to heat raw materials and extrude them into a specific shape through a die. It is usually composed of a feeding system, a heating system, an extrusion system, and a die system. The screw and barrel in the extruder are very important components, which basically run through all the processing steps of the entire extruder and are responsible for heating, mixing, compressing and extruding the raw materials. The screw is generally composed of a feeding section, a compression section, and an extrusion section. Each part has a specific pitch and screw tip to achieve continuous heating, compression, and extrusion of the raw materials. The barrel is the outer tube shell that holds the screw, and usually has a heating and cooling system to control the temperature of the raw materials. In the specific working process, the screw is to push the raw materials forward by rotating, and at the same time, it is subjected to the pressure and heating of the barrel to achieve the melting and deformation of the plastic. Therefore, the matching accuracy and processing quality of the screw and barrel will directly affect the production efficiency and product quality of the extruder.
[0003] At present, the masterbatch particles of B1-grade high-flame-retardant cables contain a large amount of flame retardants, such as magnesium oxide, aluminum oxide, flame retardants, etc. Although they can greatly improve the flame retardant properties of the cables, the addition of flame retardants causes the plasticity of the masterbatch particles to become extremely poor, the plasticizing temperature is high, and it is difficult to extrude. The use of ordinary screws and barrels for extrusion will cause problems such as overheating and clogging, which greatly affects the processing stability and efficiency.
[0004] In order to solve the above technical problems, Chinese patent CN116653257A discloses an improved B1-class cable extrusion equipment, including an extruder body, a screw is arranged inside the extruder body, the screw is an equidistant unequal depth single-thread screw, the screw compression ratio is 1.16-1.2, a fuselage protective cover is wrapped on the outside of the extruder body, a frame is fixedly connected to the bottom of the fuselage protective cover, a transmission system and a head are respectively installed at both ends of the extruder body, and a feeding system is connected to one end of the extruder body close to the transmission system. The above patent increases the torque and improves the extrusion effect by setting an equidistant unequal depth single-thread screw and increasing the speed of the main motor, but a single equidistant unequal depth single-thread screw is only suitable for some processes in the extrusion process. For the unloading stage and the plasticizing stage, relying only on a single equidistant unequal depth single-thread screw is not effective and cannot achieve the use effect of conventional equipment.
[0005] Therefore, it is necessary for technical personnel in this field to provide a B1-level high flame retardant cable material extrusion mechanism to improve the plasticizing effect and ensure processing stability and product quality in view of the poor plasticizing properties and high plasticizing temperature of the B1-level high flame retardant cable masterbatch. Summary of the invention
[0006] The present invention aims to provide a B1-class high flame-retardant cable material extrusion mechanism to solve the technical problems in the prior art that the masterbatch particles of the B1-class high flame-retardant cable have poor plasticization, high plasticization temperature and are difficult to extrude.
[0007] The technical solution adopted by the present invention to solve its technical problems is: a B1-level high-flame-retardant cable material extrusion mechanism, comprising a barrel body and a screw body rotatably arranged in the barrel body, an extrusion channel is formed inside the barrel body, a feed opening is arranged on the end of the barrel body, the feed opening penetrates through one wall of the barrel body and is connected to the extrusion channel, a straight groove is arranged on the inner wall of the barrel body near the feed opening; the screw body is divided into a feed opening section, a melting section, a plasticizing section and a homogenizing section, the feed opening section is directly opposite to the feed opening of the barrel body, the screw body comprises a rod body and a main thread spirally arranged on the rod body, the outer diameter of the main thread is uniformly distributed, and the outer diameter of the rod body near the feed opening is smaller than the outer diameter of the end away from the feed opening; a secondary thread is spirally arranged on the screw body at the plasticizing section, and the outer diameter of the secondary thread is lower than the outer diameter of the main thread.
[0008] Furthermore, the barrel body is a circular cylindrical structure, and an annular groove and an oblique groove are provided on the outer wall of the barrel body, and the annular groove and the oblique groove are arranged alternately; the annular groove is evenly arranged on the outer surface of the barrel body along the circumference of the barrel body, and the oblique groove is obliquely arranged on the outer surface of the barrel body and extends from one end of the barrel body to the other end.
[0009] Furthermore, the straight grooves are provided in plurality and are evenly arranged on the inner wall of the barrel body around the axis of the barrel body; the cross section of the straight groove is in the shape of an inverted triangle, one end of the straight groove is flush with the side wall of the feed port, and the other end of the straight groove extends into the extrusion channel.
[0010] Furthermore, an annular water groove is provided on the outer wall of the screw barrel body at the feed outlet, and multiple annular water grooves are provided and evenly arranged around the axis of the screw barrel body. The feed outlet is located in the middle of the multiple annular water grooves, and the annular water grooves are interconnected; an outer cover is provided on the outer wall of the screw barrel body, and the outer cover is located outside the annular water groove.
[0011] Furthermore, the feeding section, melting section, plasticizing section and homogenizing section are divided into four equal parts and are distributed in sequence on the screw body.
[0012] Furthermore, the length of the feeding section is L1, the length of the melting section is L2, the length of the plasticizing section is L3, and the length of the homogenizing section is L4, and L1>L2>L3>L4.
[0013] Furthermore, the diameters of the feeding section and the homogenizing section are uniform, while the diameters of the melting section and the plasticizing section gradually increase from an end close to the feeding port toward an end away from the feeding port.
[0014] Furthermore, a cooling water channel is provided at one end of the rod body, and a feeding head is detachably connected to the other end of the rod body. The cooling water channel is opened inward from the end surface of the rod body and extends to the unloading section. Water is passed through the cooling water channel. The feeding head is bullet-shaped and extends out of the barrel body.
[0015] The beneficial effects of the present invention are as follows: the present invention improves the conveying capacity and shearing capacity by increasing the depth and volume of the screw groove on the material discharge section; increases the diameter of the rod body on the melting section and the plasticizing section to ensure the strength of the rod body and prevent the rod body from being sheared under a large torque; adds a secondary thread on the plasticizing section to extend the plasticizing time of the material, ensure that the material is mixed evenly in the screw groove, improve the thermal balance, and thus improve the plasticizing effect of the material. The present invention sets different screw groove depths and screw groove volumes on the screw body, so that the screw body can process B1 grade materials more adaptably, effectively improving the processing stability and product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a stereoscopic diagram of the barrel body in the B1-level highly flame-retardant cable material extrusion mechanism of the present invention.
[0017] Figure 2 yes Figure 1 A partial enlarged schematic diagram of area A in the middle.
[0018] Figure 3 It is a partial cross-sectional view of the barrel body in the B1-level highly flame-retardant cable material extrusion mechanism of the present invention.
[0019] Figure 4 yes Figure 3 Cross-sectional view along BB.
[0020] Figure 5 It is a stereoscopic diagram of the screw body in the B1-level highly flame-retardant cable material extrusion mechanism of the present invention.
[0021] Figure 6 It is a main cross-sectional view of the screw body in the B1-level high flame-retardant cable material extrusion mechanism of the present invention.
[0022] The markings of the components in the accompanying drawings are as follows: 10, barrel body; 11, discharge port; 12, extrusion channel; 13, straight groove; 14, annular water groove; 15, annular groove; 16, inclined groove; 17, outer cover; 20, screw body; 21, discharge section; 22, melting section; 23, plasticizing section; 24, homogenizing section; 25, cooling water channel; 26, feeding head; 27, rod body; 28, main thread; 29, secondary thread. DETAILED DESCRIPTION
[0023] The present invention will now be described in detail with reference to the accompanying drawings. This figure is a simplified schematic diagram, which only illustrates the basic structure of the present invention in a schematic manner, and therefore only shows the components related to the present invention.
[0024] See also Figure 1 , Figure 5 The present invention provides a B1-level high flame retardant cable material extrusion mechanism, comprising a barrel body 10 and a screw body 20 disposed in the barrel body 10, wherein the screw body 20 is rotatably connected in the barrel body 10. When in use, the material is added into the barrel body 10, and the screw body 20 is used to rotate and extrude the material to achieve plasticization.
[0025] The present invention is further provided with a heating device and a cooling device (not shown) outside the barrel body 10. The heating device is used to heat the barrel body 10, and the cooling device is used to cool the barrel body 10. When in use, the temperature of the barrel body 10 is dynamically monitored, and the temperature of the barrel body 10 is adjusted by turning on or off the heating device and the cooling device, so that the temperature of the barrel body 10 is maintained within a set range, thereby ensuring the stability of the plasticizing process. For the specific operation mode and structure of the heating device and the cooling device, please refer to the intelligent temperature control variable power heating system for an extruder disclosed in patent CN217597771U, and the specific structure will not be described in detail here.
[0026] For further information, see Figure 2 , Figure 3 The barrel body 10 is a circular cylindrical structure, and an extrusion channel 12 is formed inside the barrel body 10, and the extrusion channel 12 penetrates the barrel body 10 along the axis of the barrel body 10. An annular groove 15 and an oblique groove 16 are arranged on the outer wall of the barrel body 10, and the annular groove 15 and the oblique groove 16 are arranged alternately. The annular groove 15 is evenly arranged on the outer surface of the barrel body 10 along the circumference of the barrel body 10, and the oblique groove 16 is obliquely arranged on the outer surface of the barrel body 10 and extends from one end of the barrel body 10 to the other end.
[0027] The present invention effectively increases the contact area between the surface of the barrel body 10 and the air by providing a plurality of annular grooves 15 and an inclined groove 16, thereby achieving the purpose of rapid cooling. The evenly arranged annular grooves 15 and inclined grooves 16 enable the barrel body 10 to be cooled sufficiently in a timely and sufficient manner, thereby avoiding poor quality of extruded products caused by insufficient cooling. At the same time, the plurality of annular grooves 15 and inclined grooves 16 can also improve the heating effect of the heating device on the barrel body 10, thereby ensuring the plasticization effect of the material in the barrel body 10.
[0028] For further information, see Figure 4A feed opening 11 is provided at the end of the barrel body 10, and the feed opening 11 penetrates one wall of the barrel body 10 and is connected to the extrusion channel 12. A straight groove 13 is provided on the inner wall of the barrel body 10 near the feed opening 11. There are multiple straight grooves 13 and they are evenly arranged on the inner wall of the barrel body 10 around the axis of the barrel body 10.
[0029] Specifically, the cross section of the straight groove 13 is in an inverted triangle shape, one end of the straight groove 13 is flush with the side wall of the feed opening 11 , and the other end of the straight groove 13 extends into the extrusion channel 12 .
[0030] The present invention adds the material into the barrel body 10 from the feed port 11, and provides a straight groove 13 on the inner wall of the barrel body 10 near the feed port 11 to increase the friction between the material and the inner wall of the barrel body 10, thereby increasing the feeding speed of the present invention. At the same time, the straight groove 13 can also provide exhaust to prevent gas from being squeezed between materials during the material addition process, thereby improving the uniformity of the material and achieving the purpose of increasing the output.
[0031] Furthermore, an annular water groove 14 is provided on the outer wall of the barrel body 10 at the feed opening 11, and multiple annular water grooves 14 are provided and evenly arranged around the axis of the barrel body 10. The feed opening 11 is located in the middle of the multiple annular water grooves 14, and the annular water grooves 14 are interconnected; an outer cover 17 is sleeved on the outer wall of the barrel body 10, and the outer cover 17 is located outside the annular water groove 14.
[0032] In this embodiment, an upper water inlet is provided on one end of the outer cover 17, and a lower water inlet (not shown) is provided on the other end of the outer cover 17. The upper water inlet and the lower water inlet are connected to a water tank, and water is passed through the annular water groove 14. When in use, the barrel body 10 is cooled by continuously passing water into the annular water groove 14, so as to avoid excessive frictional heat generation between the barrel body 10 and the material at the discharge port 11, thereby ensuring the stability of material discharge.
[0033] In order to adapt to the extrusion of B1 grade materials, the present invention adds an annular groove 15 and an inclined groove 16 on the outer wall of the barrel body 10, which increases the contact area between the surface of the barrel body 10 and the air, thereby achieving the purpose of rapid cooling or rapid heating. At the same time, a straight groove 13 and an annular water groove 14 are added at the discharge port 11 of the barrel body 10. The straight groove 13 can increase the friction between the material and the inner wall of the barrel body 10, improve the feeding speed and mixing effect, and the circulating water in the annular water groove 14 can effectively prevent the high temperature caused by high friction, thereby ensuring the use stability and use effect of the present invention.
[0034] In this embodiment, a flange (not shown) is provided at one end of the barrel body 10 and connected to a motor, and the other end of the barrel body 10 is connected to a die head, and the screw body 20 is fixedly connected to the output shaft of the motor to drive the screw body 20, and the feed opening 11 is close to the flange. When in use, the material is introduced from the feed opening 11, and extrusion is performed by rotating the screw body 20, and finally the plasticized material is extruded from the die head to complete the extrusion operation.
[0035] See also Figure 5 , Figure 6 The screw body 20 is divided into a feeding section 21, a melting section 22, a plasticizing section 23 and a homogenizing section 24. The feeding section 21 of the screw body 20 is directly opposite to the feeding port 11 of the barrel body 10. The material falls from the feeding port 11 into the feeding section 21 of the screw body 20. Under the push of the screw body 20, the material passes through the feeding section 21, the melting section 22, the plasticizing section 23 and the homogenizing section 24 in sequence, completing the feeding, melting, plasticizing and homogenizing steps of the material.
[0036] In this embodiment, the screw body 20 includes a rod body 27 and a main thread 28 spirally arranged on the rod body 27. The feeding section 21, melting section 22, plasticizing section 23 and homogenizing section 24 are divided into four equal parts and distributed in sequence on the screw body 20 to ensure processing stability.
[0037] In another embodiment, the screw body 20 includes a rod body 27 and a main thread 28 spirally arranged on the rod body 27, the length of the material discharge section 21 is L1, the length of the melting section 22 is L2, the length of the plasticizing section 23 is L3, and the length of the homogenizing section 24 is L4, L1>L2>L3>L4, so that different processing effects are provided according to different plasticization degrees of the material.
[0038] Furthermore, the outer diameter of the main thread 28 is uniformly distributed, and the outer diameter of the end of the rod body 27 close to the discharge port 11 is smaller than the outer diameter of the end away from the discharge port 11 .
[0039] Specifically, the diameter of the rod body 27 at the corresponding feeding section 21 is less than the diameter of the rod body 27 at the corresponding melting section 22 is less than the diameter of the rod body 27 at the corresponding plasticizing section 23 is less than the diameter of the rod body 27 at the corresponding homogenizing section 24. At the same time, the diameters of the feeding section 21 and the homogenizing section 24 are uniform, while the diameters of the melting section 22 and the plasticizing section 23 gradually increase from the end close to the feeding port 11 toward the end away from the feeding port 11.
[0040] Since the outer diameter of the main thread 28 is uniform and the outer diameter of one end of the rod body 27 is larger than that of the other end, the screw groove depths (the difference between the outer diameter of the main thread 28 and the outer diameter of the rod body 27) among the feeding section 21, the melting section 22, the plasticizing section 23 and the homogenizing section 24 on the screw body 20 are all different. Specifically, the screw groove depth of the feeding section 21 is greater than that of the melting section 22, the screw groove depth of the melting section 22 is greater than that of the plasticizing section 23, and the screw groove depth of the plasticizing section 23 is greater than that of the homogenizing section 24.
[0041] The rod body 27 and the main thread 28 on the unloading section 21 are equidistant and equal in depth (equal pitches and equal screw groove depths), and the rod body 27 and the main thread 28 on the homogenizing section 24 are also equidistant and equal in depth, that is, the screw groove depths between the pitches on the unloading section 21 are equal, and the screw groove depths between the pitches on the homogenizing section 24 are also equal.
[0042] It can be understood that the ratio of the volume of the first screw groove on the unloading section 21 to the volume of the last screw groove on the homogenizing section 24 is the compression ratio. The larger the compression ratio, the more uniform the plasticizing effect on the material. Therefore, the screw groove depth of the unloading section 21 is greater than the screw groove depth of the homogenizing section 24 to ensure that the compression ratio of the present invention is within a set range. At the same time, the straight groove 13 located on the inner wall of the barrel body 10 is used to increase the volume of the first screw groove on the unloading section 21, thereby further improving the compression ratio and improving the plasticizing effect of the material.
[0043] The rod body 27 and the main thread 28 on the melting section 22 are equidistant from each other but have different depths (the pitches are equal, but the screw groove depths are unequal). Meanwhile, the rod body 27 and the main thread 28 on the plasticizing section 23 are also equidistant from each other but have different depths. That is, on the melting section 22 and the plasticizing section 23, the screw groove depths between the screw pitches decrease from left to right. The plasticizing section 23 is also provided with a secondary thread 29, which is spirally arranged on the rod body 27. The starting end of the secondary thread 29 is tangent to the main thread 28, and the outer diameter of the secondary thread 29 is lower than the outer diameter of the main thread 28. Therefore, in the plasticizing section 23, the screw groove depth between the screw pitches of the secondary thread 29 is lower than the screw groove depth between the screw pitches of the main thread 28.
[0044] It can be understood that a gap is formed between the screw body 20 and the barrel body 10. The larger the gap, the higher the transmission performance, the greater the shear rate, but the greater the heat generation; and the smaller the gap, the slower the material transportation, the better the plasticizing effect, but it is easy to cause material degradation. The present invention adds a secondary thread 29 to the plasticizing section 23, and the outer diameter of the secondary thread 29 is lower than the outer diameter of the main thread 28, so that the gap at the plasticizing section 23 decreases from left to right. When the material passes through the plasticizing section 23, the excessively large particle size cannot pass through the gap between the main thread 28 and the barrel body 10 and accumulates in the screw groove between the secondary thread 29 and the main thread 28, thereby increasing the plasticizing time of the material, reducing the particle size, and thus improving the plasticizing effect.
[0045] The present invention improves the conveying capacity and shearing capacity of the material discharge section 21 by increasing the depth and volume of the screw groove; increases the diameter of the rod body 27 on the melting section 22 and the plasticizing section 23 to ensure the strength of the rod body 27 and prevent the rod body 27 from being sheared under a large torque; and adds a secondary thread 29 to the plasticizing section 23 to extend the plasticizing time of the material, ensure that the material is mixed evenly in the screw groove, improve the thermal balance, and thus improve the plasticizing effect of the material. Therefore, in view of the problem that B1-level materials are difficult to plasticize, the present invention sets different screw groove depths and screw groove volumes on the screw body 20, so that the screw body 20 can process B1-level materials more adaptably, effectively improving the processing stability and product quality.
[0046] In this embodiment, the helix angle of the main thread 28 is 15° to 17°. The helix angle of the secondary thread 29 is 15° to 17°. The working temperature of the feeding section 21 is 120 to 140°C, the working temperature of the melting section 22 is 140 to 160°C, the working temperature of the plasticizing section 23 is 160 to 200°C, and the working temperature of the homogenizing section 24 is 200 to 220°C.
[0047] Furthermore, a cooling water channel 25 is provided at one end of the rod body 27, and a feed head 26 is detachably connected to the other end of the rod body 27. The cooling water channel 25 is provided inwardly from the end surface of the rod body 27 and extends to the unloading section 21. Water is passed through the cooling water channel 25. The feed head 26 is in the shape of a bullet head, and the feed head 26 extends out of the barrel body 10 and into the die head. Preferably, the cooling water channel 25 and the rod body 27 are coaxially arranged.
[0048] The present invention circulates water in the cooling water channel 25 to cool the rod body 27 at the material discharge section 21, reduces the heat generated by the rotational friction of the rod body 27, and thus realizes temperature control of the material discharge section 21 and the material therein. The present invention also provides a feed head 26 at the end of the rod body 27 and installs the feed head 26 into the die head. When in use, the plasticized material enters the die head under the push of the screw body 20, and the feed head 26 is used to ensure the fluidity of the plasticized material and the accuracy of injection, thereby improving the stability of the present invention.
[0049] The specific operation steps of the present invention are: adding the material into the barrel body 10 from the feed port 11, using the heating device to heat the barrel body 10 and the material therein, and then using the screw body 20 to push the material through the feed section 21, the melting section 22, the plasticizing section 23 and the homogenizing section 24 in sequence. When the temperature is too high, start the cooling device to cool the barrel body 10 locally, and the plasticized material flows from the feeding head 26 into the die head to complete the extrusion.
[0050] The present invention improves the conveying capacity and shearing capacity of the unloading section 21 by increasing the depth and volume of the screw groove; increases the diameter of the rod body 27 on the melting section 22 and the plasticizing section 23 to ensure the strength of the rod body 27 and prevent the rod body 27 from being sheared under a large torque; and adds a secondary thread 29 to the plasticizing section 23 to extend the plasticizing time of the material, ensure that the material is mixed evenly in the screw groove, improve the thermal balance, and thus improve the plasticizing effect of the material. The present invention sets different screw groove depths and screw groove volumes on the screw body 20, so that the screw body 20 can process B1 grade materials more adaptively, effectively improving the processing stability and product quality.
[0051] It is to be understood that the present invention is described by some embodiments, and it is known to those skilled in the art that various changes or equivalent substitutions may be made to these features and embodiments without departing from the spirit and scope of the present invention. In addition, under the teachings of the present invention, these features and embodiments may be modified to adapt to specific circumstances and materials without departing from the spirit and scope of the present invention. Therefore, the present invention is not limited by the specific embodiments disclosed herein, and all embodiments falling within the scope of the claims of this application are within the scope of protection of the present invention.
Claims
1. A B1-level highly flame-retardant cable material extrusion mechanism, comprising a barrel body (10) and a screw body (20) rotatably disposed in the barrel body (10), It is characterized in that An extrusion channel (12) is formed inside the barrel body (10), a feed opening (11) is provided at the end of the barrel body (10), the feed opening (11) penetrates one wall of the barrel body (10) and is connected to the extrusion channel (12), and a straight groove (13) is provided on the inner wall of the barrel body (10) near the feed opening (11); the screw body (20) is divided into a feed opening section (21), a melting section (22), a plasticizing section (23) and a homogenizing section (24), and the feed opening section (21) is opposite to the barrel body. The screw body (20) comprises a rod body (27) and a main thread (28) spirally arranged on the rod body (27), the outer diameter of the main thread (28) is uniformly distributed, and the outer diameter of the end of the rod body (27) close to the feeding opening (11) is smaller than the outer diameter of the end away from the feeding opening (11); and a secondary thread (29) is spirally arranged on the screw body (20) at the plasticizing section (23), and the outer diameter of the secondary thread (29) is smaller than the outer diameter of the main thread (28).
2. The B1-level high flame-retardant cable material extrusion mechanism according to claim 1, It is characterized in that The screw barrel body (10) is in a circular cylindrical structure. An annular groove (15) and an oblique groove (16) are provided on the outer wall of the screw barrel body (10). The annular groove (15) and the oblique groove (16) are arranged alternately. The annular groove (15) is evenly arranged on the outer surface of the screw barrel body (10) along the circumference of the screw barrel body (10), and the oblique groove (16) is obliquely arranged on the outer surface of the screw barrel body (10) and extends from one end of the screw barrel body (10) to the other end.
3. The B1-level high flame-retardant cable material extrusion mechanism according to claim 2, It is characterized in that The straight grooves (13) are provided in plurality and are evenly arranged on the inner wall of the barrel body (10) around the axis of the barrel body (10); the cross section of the straight grooves (13) is in the shape of an inverted triangle, one end of the straight grooves (13) is flush with the side wall of the feed opening (11), and the other end of the straight grooves (13) extends into the extrusion channel (12).
4. The B1-level high flame-retardant cable material extrusion mechanism according to claim 3, It is characterized in that An annular water groove (14) is provided on the outer wall of the screw barrel body (10) at the feed opening (11); a plurality of annular water grooves (14) are provided and are evenly arranged around the axis of the screw barrel body (10); the feed opening (11) is located in the middle of the plurality of annular water grooves (14); and the annular water grooves (14) are interconnected; an outer cover (17) is sleeved on the outer wall of the screw barrel body (10); and the outer cover (17) is located outside the annular water grooves (14).
5. The B1-level high flame-retardant cable material extrusion mechanism according to claim 1, It is characterized in that The material discharge section (21), the melting section (22), the plasticizing section (23) and the homogenizing section (24) are divided into four equal parts and are sequentially distributed on the screw body (20).
6. The B1-level high flame-retardant cable material extrusion mechanism according to claim 1, It is characterized in that The length of the material discharge section (21) is L1, the length of the melting section (22) is L2, the length of the plasticizing section (23) is L3, and the length of the homogenizing section (24) is L4, where L1>L2>L3>L4.
7. The B1-level high flame-retardant cable material extrusion mechanism according to claim 6, It is characterized in that The diameters of the feeding section (21) and the homogenizing section (24) are uniform, while the diameters of the melting section (22) and the plasticizing section (23) gradually increase from an end close to the feeding port (11) toward an end away from the feeding port (11).
8. The B1-level high flame-retardant cable material extrusion mechanism according to claim 1, It is characterized in that A cooling water channel (25) is provided at one end of the rod body (27), and a feeding head (26) is detachably connected to the other end of the rod body (27). The cooling water channel (25) is provided inwardly from the end surface of the rod body (27) and extends to the unloading section (21). Water flows through the cooling water channel (25). The feeding head (26) is in the shape of a bullet head and extends out of the screw barrel body (10).